Car cover film pasting liquid as well as preparation method and use method thereof
By using the combination of components A and components B in the car coat film solution, the lubrication effect of glycerol and the water absorption effect of high molecular weight polyvinyl alcohol and alumina powder are solved, and the problem of unsolid pasting and bubbles of the car coat is solved. It realizes stable pasting of car clothes and stability in long-term use.
Patent Information
- Application Number
- CN202411056901.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-02
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2044-08-02
AI Technical Summary
During the installation of existing car coat film liquid, the car coat is not sticky and is prone to bubbles and incompatibility.
A combination of component A and component B, wherein component A includes triethanolamine, carbomer, resin, sodium silicate, glycerol, preservatives and thickeners, and component B includes high molecular weight polyvinyl alcohol and oxidation Aluminum powder is easy to spread and scrape the car clothes during installation through the lubricating effect of glycerol, and reduces the concentration of lubricant through the water absorption of high molecular weight polyvinyl alcohol and alumina powder to prevent bubbles or displacement after pasting.
It realizes convenient pasting and stability during long-term use of the car clothes, avoids bubbles and incompatibility on the adhesive surface, and ensures that the car clothes are not prone to bubbles or displacement during use.
Smart Images

Figure BDA0004976704690000131 
Figure BDA0004976704690000141 
Figure HDA0004976704710000011
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of car cover film liquid, and more specifically, it relates to a car cover film liquid and a preparation method and a use method thereof. Background Art
[0002] Car cover requires the cover itself, film liquid and installation tools. A car cover with good installation quality can protect the car paint surface and prevent damage caused by external factors such as scratches and stone impacts that may be encountered in daily use. It can also reduce oxidation and corrosion caused by natural factors such as ultraviolet rays and acid rain. Therefore, the installation quality of car cover is extremely important, and it can be improved mainly from three aspects: the quality of the car cover, the quality of the film liquid and the installation workers.
[0003] In the prior art, a Chinese invention patent with publication number CN115368973A discloses a foam type invisible car cover installation liquid, the weight composition of raw materials includes 80-100 parts of deionized water, 1-10 parts of surfactant, 6-10 parts of foaming agent, 5-10 parts of foam stabilizer, 1-3 parts of antioxidant, 1-2 parts of preservative, 0.1-0.3 parts of chelating agent. By mixing deionized water, surfactant, foaming agent, foam stabilizer, antioxidant, preservative, and chelating agent, it has good antioxidant properties and can facilitate the pasting of car covers.
[0004] The above-mentioned traditional car cover installation liquid is used to replace shower gel. In order to play a lubricating role during installation, a foaming agent is still added, so that micro-bubbles are present between the car cover and the surface of the car shell. There are disadvantages that the adhesive surface has bubbles and is not adhered after long-term use of the car cover. Summary of the invention
[0005] In order to solve the problem that the car cover is not firmly adhered and does not fit well in order to improve the lubrication when installing the car cover, the present application provides a car cover film liquid and a preparation method and use method thereof.
[0006] In the first aspect, the present application provides a car cover film liquid, which adopts the following technical solution:
[0007] A car cover film liquid comprises component A and component B, wherein component A comprises triethanolamine, carbomer, resin, sodium silicate, glycerol, a preservative, a defoaming agent and a thickener; and component B comprises high molecular weight polyvinyl alcohol and aluminum oxide powder.
[0008] By adopting the above technical solution, the glycerol in the A component plays a lubricating role, which facilitates the spreading and leveling of the car cover when the car cover is applied. The principle of the lubricating effect of glycerol is the water absorption and moisture retention of glycerol. After the car cover is applied, if the glycerol continues to play a lubricating role, it may cause bubbles or displacement between the car cover and the car surface. Therefore, since the high molecular weight polyvinyl alcohol and alumina powder in the B component of the present application both have a water absorption effect, the high molecular weight polyvinyl alcohol and alumina powder can compete for the moisture around the glycerol and the moisture concentrated and overflowed by the glycerol, resulting in a reduction in the lubricating effect of the glycerol, and it is difficult for the applied car cover to generate bubbles or displacement.
[0009] After absorbing water, high molecular weight polyvinyl alcohol will swell slightly and fill the gaps left by the concentrated glycerol. The good water retention performance of high molecular weight polyvinyl alcohol makes the car cover still have good toughness and elasticity after being installed for a long time, and it is difficult to cause damage to the car surface when it is torn.
[0010] Component B contains high molecular weight polyvinyl alcohol and alumina powder, and the water-absorbing component is an organic-inorganic compound. The water absorption rate of the organic-inorganic compound is higher than that of a single component of the same weight, and the stability is good;
[0011] The sodium silicate in component A is used to adjust the temperature of the film liquid. The car may experience rapid temperature changes at different times and locations, so that the composition of the car film liquid also changes with the temperature change of the car surface. The addition of sodium silicate increases the adaptability of the car film liquid to temperature, so that the elasticity and viscosity of the organic-inorganic compound of component B will not change dramatically in a short time. Therefore, even after several years of use, the car cover using the car film liquid of the present application is still unlikely to have bubbles and displacement.
[0012] The car cover film liquid of the present application has the advantages of being easy to move when installing the car cover, quickly adhering to the surface of the car shell after being pasted, and no bubbling or looseness on the pasted surface during long-term use.
[0013] Preferably, the component A comprises the following substances in parts by weight: 3-5 parts of triethanolamine, 0.5-1 parts of carbomer, 30-50 parts of resin, 5-10 parts of sodium silicate, 3-7 parts of glycerol, 0.1-0.5 parts of preservative, 0.5-1 parts of defoamer and 0.6-1.5 parts of thickener.
[0014] By adopting the above technical scheme, the resin which is an important component of the above film-sticking liquid is the main binder, triethanolamine plays an emulsifying role, and triethanolamine plays a role of thickening and moisturizing the resin by cooperating with carbomer; sodium silicate is mainly used to adjust the temperature of component B and component A to avoid the influence of sudden changes in external temperature on the components of the film-sticking liquid; propylene glycol mainly plays a lubricating role to facilitate the movement of the car cover when sticking the car cover; preservatives, defoaming agents and thickeners are common additives, and the added amount is relatively small.
[0015] Preferably, the mass ratio of high molecular weight polyvinyl alcohol to alumina powder in the B component is 1:(0.1-0.3).
[0016] By adopting the above technical solution, the appropriate ratio of high molecular weight polyvinyl alcohol and alumina powder can maximize the water absorption effect of the organic-inorganic composite and maintain the long-term stability of component B to the greatest extent.
[0017] Preferably, the alumina powder is nano-β-alumina powder; the high molecular weight polyvinyl alcohol solution is a high molecular weight polyvinyl alcohol aqueous solution with a mass fraction of 0.45%-0.55%.
[0018] By adopting the above technical scheme, the volume of the nano β-alumina powder will not change after absorbing water. Therefore, the only substance in component B whose volume increases after absorbing water is high molecular weight polyvinyl alcohol, and the high molecular weight polyvinyl alcohol solution is viscous and can flow by itself to fill the remaining gaps after the glycerol is concentrated, so as to keep the surface of the car cover smooth; the high molecular weight polyvinyl alcohol solution with a mass fraction of 0.45%-0.55% is between Newtonian fluid and non-Newtonian fluid, so that the high molecular weight polyvinyl alcohol solution itself carries less water and has sufficient water absorption space, and it is viscous itself and can firmly grasp the surface of the car.
[0019] Preferably, the sodium silicate is Na2O·2SiO2.
[0020] By adopting the above technical solution, Na2O·2SiO2 type sodium silicate has a better temperature adjustment effect and does not have a side reaction with high molecular weight polyvinyl alcohol and alumina powder.
[0021] Preferably, the resin is one of liquid epoxy resin, polyurethane resin or acrylic resin.
[0022] By adopting the above technical solution, epoxy resin, polyurethane resin or acrylic resin can all be used as the main components of the film liquid. However, due to the different components of the three resins, their mutual adhesion and water retention are different, so they cannot be mixed. If mixed for a long time, bubbles or cracks will form on the surface of the car cover and the surface of the car.
[0023] In a second aspect, the present application provides a method for preparing a car cover film liquid, using the following technical solution:
[0024] A method for preparing a car cover film liquid, wherein the preparation method of component A comprises the following steps: triethanolamine, carbomer, resin, sodium silicate, glycerol, a preservative, a defoaming agent and a thickener are mixed, and a defoaming stirrer is used to stir the mixture at a speed of 100-300 rpm for 0.5-1h to obtain component A; and the preparation method of component B comprises the following steps: aluminum oxide powder is added to a high molecular weight polyvinyl alcohol solution, and a defoaming stirrer is used to stir the mixture at a speed of 500-800 rpm for 0.5-1h to obtain component B.
[0025] By adopting the above technical scheme, a simple preparation method can quickly and conveniently prepare component A and component B, and a defoaming mixer is used to avoid bubbles during the stirring process. The final components A and B are free of bubbles, meeting the requirement that the car cover film liquid is free of bubbles.
[0026] In a third aspect, the present application provides a method for using a car cover film liquid, using the following technical solution:
[0027] A method for using a car cover film liquid comprises the following steps:
[0028] Step 1, diluting the component A with deionized water, wherein the weight ratio of the component A to the deionized water is 1:(80-150);
[0029] Step 2, when applying the car cover, first spray component B on the car surface, then spray component A on the car surface, and finally apply the car cover.
[0030] By adopting the above technical scheme, component A is diluted in step 1, and the volume is expanded by 80-150 times. The user only needs to purchase the car cover film liquid of the present application once, and can use it for many times, which is economical and practical. In step 2, component B is first sprayed on the surface of the car shell. Component B is viscous, which can not only firmly grasp the surface of the car shell, but also has good viscoelasticity, and it is difficult to cause damage to the car surface when tearing. Component A is then sprayed, and the car cover is attached after spraying component A. The lubricity of glycerol in component A enables the user to smoothly adjust the position of the car cover and scrape the car cover flat with a scraper when attaching the car cover. The moment component A contacts component B, component B begins to absorb the moisture in component A, so the lubricating effect of glycerol is continuously reduced until the car cover is firmly adhered to the surface of the car.
[0031] Preferably, the mass ratio of the B component to the A component sprayed on the surface of the car is 1:(5-10).
[0032] By adopting the above technical solution, the appropriate mass ratio of component B and component A sprayed on the car surface can reserve enough time for the constructor to move the car cover when applying the car cover. After the car cover is applied, the car cover can be firmly adhered to the car surface within an appropriate time range.
[0033] Preferably, after the B component is sprayed on the surface of the car, the A component is sprayed within 0-5 minutes; after the A component is sprayed, the car cover is applied within 0-10 minutes.
[0034] By adopting the above technical scheme, within the time range of spraying component A, the time when component B is exposed to the air will not cause changes in the physical or chemical properties of component B; within the time range of applying the car cover, the time when component B is exposed to the air will not cause changes in the physical or chemical properties of component B; within this time range, component A and component B of the present application can both perform their respective functions, and bubbles and displacement are unlikely to occur after the car cover is applied.
[0035] In summary, this application has the following beneficial effects:
[0036] 1. In the present application, the glycerol in component A plays a lubricating role, and the high molecular weight polyvinyl alcohol and alumina powder in component B both have a water-absorbing effect. After the car cover is applied, the high molecular weight polyvinyl alcohol and alumina powder can compete for the water around the glycerol and the water concentrated and overflowed by the glycerol, which reduces the lubricating effect of the glycerol, and the applied car cover is difficult to generate bubbles or shift; the car cover film-applying liquid of the present application is easy to shift when used for the car cover installation, and quickly adheres to the surface of the car shell after installation;
[0037] 2. The sodium silicate in component A of the present application is used to adjust the temperature of the film liquid. The car shell may experience rapid temperature changes at different times and locations, so that the composition of the car film liquid also changes with the temperature change of the car shell surface. The addition of sodium silicate increases the adaptability of the car film liquid to temperature, so that the elasticity and viscosity of the organic-inorganic compound of component B will not change dramatically in a short time. Therefore, even after several years of use, the car cover using the car film liquid of the present application is still unlikely to have bubbles or displacement;
[0038] 3. In the method of use of the present application, component B is sprayed first and then component A. The moment component A comes into contact with component B, component B begins to absorb the moisture in component A. Therefore, the lubricating effect of glycerol is continuously reduced until the car cover is firmly adhered to the surface of the car. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] Figure 1 The purpose is to demonstrate the adhesion of the car cover film liquid of the present application at different times when the car cover is installed. DETAILED DESCRIPTION
[0040] The raw materials of the examples and comparative examples of the present application can all be purchased commercially;
[0041] High molecular weight polyvinyl alcohol, analytical grade, molecular weight: 20w, brand: Fangxin Biology; car cover, model: XH7240ZU0DXG; brand: UPPF; triethanolamine, model: AR500mL, brand, Xilong; carbomer, model: 971P, brand: Yamade; Na2O·2SiO2, model: MDS-A, brand: Tongli; propylene glycol, analytical grade, brand: Sinopharm; preservative is BIT-10, purchased from Foshan Liyuan Chemical; defoaming agent is polyvinyl alcohol defoaming agent, model: PR6339, purchased from Tianjin Ruike Chemical Trading Co., Ltd.; thickener is polyacrylamide, analytical grade, brand: Hengju; nano-β-alumina powder, analytical grade, brand, Hefei Kejing;
[0042] The present application is further described in detail below in conjunction with embodiments and comparative examples.
[0043] Example
[0044] Example 1
[0045] A method for preparing a car cover film liquid comprises the following steps:
[0046] The preparation method of component A comprises the following steps: 3 g of triethanolamine, 1 g of carbomer, 30 g of epoxy resin, 10 g of Na2O·2SiO2, 3 g of propylene glycol, 0.5 g of preservative, 0.5 g of defoamer and 1.5 g of thickener are mixed, and stirred at room temperature for 1 hour at a speed of 100 rpm using a defoaming stirrer to obtain component A;
[0047] The preparation method of component B comprises the following steps: adding 0.2 g of nano-β-alumina powder to 1 g of a high molecular weight polyvinyl alcohol solution with a mass fraction of 0.5%, stirring at room temperature for 1 hour at a speed of 500 rpm using a defoaming stirrer to obtain component B.
[0048] A method for using a car cover film liquid comprises the following steps:
[0049] Step 1, diluting component A with deionized water, the weight ratio of component A to deionized water being 1:80;
[0050] Step 2, when applying the car cover, first spray 1g of component B on the car surface, and then spray 7g of component A on the surface of the 10cm*10cm car shell template after 5 minutes. After 10 minutes, apply the car cover, reserve the tension angle, and prepare the car cover film liquid sample.
[0051] Example 2
[0052] A method for preparing a car cover film liquid comprises the following steps:
[0053] The preparation method of component A comprises the following steps: 5 g of triethanolamine, 0.5 g of carbomer, 50 g of polyurethane resin, 5 g of Na2O·2SiO2, 7 g of propylene glycol, 0.1 g of preservative, 1 g of defoamer and 0.6 g of thickener are mixed, and stirred at room temperature for 0.5 h at a speed of 300 rpm using a defoaming stirrer to obtain component A;
[0054] The preparation method of component B comprises the following steps: adding 0.2 g of nano-β-alumina powder to 1 g of a high molecular weight polyvinyl alcohol solution with a mass fraction of 0.5%, stirring at room temperature for 0.5 h at a speed of 800 rpm using a defoaming stirrer to obtain component B.
[0055] A method for using a car cover film liquid comprises the following steps:
[0056] Step 1, diluting component A with deionized water, wherein the weight ratio of component A to deionized water is 1:150;
[0057] Step 2, when applying the car cover, first spray 1g of component B on the car surface, and then spray 7g of component A on the surface of the 10cm*10cm car shell template after 1 minute, and apply the car cover after 1 minute, leaving a tension angle to prepare a car cover film liquid sample.
[0058] Example 3
[0059] A method for preparing a car cover film liquid comprises the following steps:
[0060] The preparation method of component A comprises the following steps: 4 g of triethanolamine, 0.8 g of carbomer, 40 g of acrylic resin, 8 g of Na2O·2SiO2, 5 g of propylene glycol, 0.3 g of preservative, 0.7 g of defoamer and 1 g of thickener are mixed, and stirred at room temperature for 0.7 h at a speed of 200 rpm using a defoaming stirrer to obtain component A;
[0061] The preparation method of component B comprises the following steps: adding 0.2 g of nano-β-alumina powder to 1 g of a high molecular weight polyvinyl alcohol solution with a mass fraction of 0.5%, stirring at room temperature for 0.7 h at a speed of 650 rpm using a defoaming stirrer, and obtaining component B.
[0062] A method for using a car cover film liquid comprises the following steps:
[0063] Step 1, diluting component A with deionized water, wherein the weight ratio of component A to deionized water is 1:110;
[0064] Step 2, when applying the car cover, first spray 1g of component B on the car surface, and then spray 7g of component A on the surface of the 10cm*10cm car shell template after 3 minutes, and apply the car cover after 6 minutes, leaving a tension angle to prepare a car cover film liquid sample.
[0065] Example 4
[0066] The difference from Example 3 is that the amount of raw materials in component B is different. The specific preparation steps of component B are as follows:
[0067] The preparation method of component B comprises the following steps: adding 0.5 g of nano-β-alumina powder to 1 g of a high molecular weight polyvinyl alcohol solution with a mass fraction of 0.5%, stirring at room temperature for 0.7 h at a speed of 650 rpm using a defoaming stirrer, and obtaining component B.
[0068] Example 5
[0069] The difference from Example 3 is that the mass fraction of the high molecular weight polyvinyl alcohol solution is 0.3%.
[0070] Example 6
[0071] The difference from Example 3 is that the mass fraction of the high molecular weight polyvinyl alcohol solution is 0.6%.
[0072] Example 7
[0073] The difference from Example 3 is that Na2O·2SiO2 in component A is replaced by an equal weight of water glass.
[0074] Example 8
[0075] The difference from Example 3 is that the amount of raw materials used in step 2 of the method for using the car cover film liquid is different. Step 2 is specifically as follows:
[0076] Step 2, when applying the car cover, first spray 1g of component B on the car surface, and then spray 5g of component A on the surface of the 10cm*10cm car shell template after 3 minutes, and apply the car cover after 6 minutes, leaving a pulling angle to prepare a car cover film liquid sample.
[0077] Example 9
[0078] The difference from Example 3 is that the amount of raw materials used in step 2 of the method for using the car cover film liquid is different. Step 2 is specifically as follows:
[0079] Step 2, when applying the car cover, first spray 1g of component B on the car surface, then spray 10g of component A on the surface of the 10cm*10cm car shell template 3 minutes later, and apply the car cover 6 minutes later, leaving a pulling angle to prepare a car cover film liquid sample.
[0080] Example 10
[0081] The difference from Example 3 is that the amount of raw materials used in step 2 of the method for using the car cover film liquid is different. Step 2 is specifically as follows:
[0082] Step 2, when applying the car cover, first spray 1g of component B on the car surface, and then spray 3g of component A on the surface of the 10cm*10cm car shell template after 3 minutes, and apply the car cover after 6 minutes, leaving a pulling angle to prepare a car cover film liquid sample.
[0083] Embodiment 11
[0084] The difference from Example 3 is that the amount of raw materials used in step 2 of the method for using the car cover film liquid is different. Step 2 is specifically as follows:
[0085] Step 2, when applying the car cover, first spray 1g of component B on the car surface, and then spray 12g of component A on the surface of the 10cm*10cm car shell template after 3 minutes, and apply the car cover after 6 minutes, leaving a pulling angle to prepare a car cover film liquid sample.
[0086] Example 12
[0087] The difference from Example 3 is that the film application time of step 2 in the method of using the car cover film application liquid is different, and step 2 is specifically as follows:
[0088] Step 2, when applying the car cover, first spray 1g of component B on the car surface, and then spray 7g of component A on the surface of the 10cm*10cm car shell template after 8 minutes. After 15 minutes, apply the car cover, leaving a pulling angle, and prepare a car cover film liquid sample.
[0089] Comparative Example
[0090] Comparative Example 1
[0091] The difference from Example 3 is that no carbomer is added to component A.
[0092] Comparative Example 2
[0093] The difference from Example 3 is that no triethanolamine is added to the A component.
[0094] Comparative Example 3
[0095] The difference from Example 3 is that no Na2O·2SiO2 is added to component A.
[0096] Comparative Example 4
[0097] The difference from Example 3 is that glycerol is not added to the A component.
[0098] Comparative Example 5
[0099] The difference from Example 3 is that high molecular weight polyvinyl alcohol solution is not added to component B, but the added mass of nano β-alumina powder is 1.2 g.
[0100] Comparative Example 6
[0101] The difference from Example 3 is that no nano β-alumina powder is added to component B, but the added mass of high molecular weight polyvinyl alcohol solution is 1.2 g.
[0102] Comparative Example 7
[0103] The difference from Example 3 is that the method of using the car cover film liquid is different, and the specific method is as follows:
[0104] A method for using a car cover film liquid comprises the following steps:
[0105] Step 1, diluting component A with deionized water, wherein the weight ratio of component A to deionized water is 1:110;
[0106] Step 2: Before applying the car cover, mix 1g of component B with 7g of component A, and then spray it on the surface of a 10cm*10cm car shell template. After 6 minutes, apply the car cover, leaving a pulling angle, and prepare a car cover film liquid sample.
[0107] Comparative Example 8
[0108] The commercially available film liquid used was named "Car Cover Installation Glue"; series was M-X1QC35L; model was 8026; brand was Henkel.
[0109] Performance testing
[0110] Adhesion time test: Use the car cover film liquid samples of Example 3, Example 12, Comparative Example 4, Comparative Example 5, and Comparative Example 6 of the present application, use the XLW-L intelligent electronic tensile testing machine to pull the car cover, and record the tensile force of the car cover being pulled away from the car shell template 0.5min, 1min, 3min, and 5min after the car cover is applied; the test results are shown in the attached manual Figure 1 ;
[0111] Durability test
[0112] 80°C UV irradiation blistering test: The car cover film liquid samples prepared in the examples of the present application and the comparative examples were subjected to UV irradiation for 72 hours at 37°C using a Deliang DL-0209 UV aging box, and the blistering phenomenon on the car cover surface was observed after the irradiation;
[0113] 80℃ sustained adhesion tensile test: The car cover film liquid samples prepared in the examples of the present application and the comparative examples were baked in a vacuum oven at 80℃ for 7 days, and then the car cover was pulled by an XLW-L intelligent electronic tensile testing machine to record the tensile force required to pull the car cover away from the car shell template;
[0114] 37℃ electrolyte immersion test: refer to the standard ASTM G71-1981 (2009) "Implementation and Evaluation of Current Corrosion Tests in Electrolyte", and conduct an electrolysis test for 72 hours; after the electrolysis, take out the car cover film liquid sample, soak it in deionized water for 1 hour, and then observe the phenomenon.
[0115] The test results are in Table 1 below;
[0116] Table 1 Car cover film liquid sample durability test table
[0117]
[0118]
[0119] In conjunction with the instruction manual Figure 1 It can be seen that the car cover film liquid sample prepared in Example 3 of the present application has a small pulling force within 1 minute after preparation, and has good lubricity; the pulling force increases rapidly after 3 minutes, proving that the adhesion increases rapidly after 3 minutes, and the car cover is firmly attached to the car shell; the spraying time and film application time of component A in Example 12 are both extended, resulting in the pulling force of the car cover film liquid sample prepared in Example 12 increasing to 1N 0.5 minutes after preparation, making it difficult to move and adjust the car cover again, and the subsequent adhesion continues to increase; Comparative Example 4 does not add propylene glycol, and the car cover is attached 0.5 minutes after being attached , the pulling force has increased to 4N, and the car cover is difficult to move after it is applied; the high molecular weight polyvinyl alcohol in Comparative Example 5 is replaced by aluminum oxide powder, and the aluminum oxide powder in Comparative Example 6 is replaced by high molecular weight polyvinyl alcohol. The car cover film liquid samples prepared in Comparative Examples 5 and 6 have small pulling force within 1 minute after the preparation, and the car cover can be moved, but the pulling force of the car cover is still small within the subsequent 5 minutes, and the car cover is not firmly adhered to the car shell, and there is a risk of displacement of the car cover; therefore, the car cover film liquid sample prepared in Example 3 of the present application is the most convenient to use when installing the car cover and has the strongest adhesion.
[0120] Combining the data of Examples 1, 2, and 3, it can be seen that the only difference between Examples 1, 2, and 3 is the different raw material composition ratios. The car cover film liquid of Example 3 does not turn yellow after being immersed in a 37°C electrolyte for 72 hours, while the car cover film liquids of Examples 1 and 2 turn slightly yellow after being immersed in a 37°C electrolyte for 72 hours. Therefore, the raw material ratio of Example 3 becomes the optimal ratio for preparing the car cover film liquid.
[0121] Combining the data of Examples 3 and 4, it can be seen that the difference between Example 4 and Example 3 is that the ratio of high molecular weight polyvinyl alcohol to alumina powder in Example 4 is different. Under the conditions of 80°C ultraviolet irradiation for 72 hours and 37°C electrolyte immersion for 72 hours, the car cover film liquid samples obtained in Example 4 and Example 3 do not bubble or turn yellow, but the car cover film liquid sample obtained in Example 4 after baking at 80°C for 7 days has a much greater adhesive tension than the car cover film liquid sample obtained in Example 3 after baking at 80°C for 7 days, and there is slight residual glue, which proves that the car cover film liquid sample obtained in Example 4 is greatly affected by high temperature, and the optimal range of the ratio of high molecular weight polyvinyl alcohol to alumina powder is 1:(0.1-0.3).
[0122] Combining the data of Examples 3, 5, and 6, it can be seen that the difference between Examples 5 and 6 and Example 3 is that the mass fraction of the high molecular weight polyvinyl alcohol aqueous solution in Example 5 and Example 6 is different. The results show that the car cover film liquid samples prepared in Examples 5 and 6 both turned slightly yellow after being immersed in 37°C electrolyte for 72 hours. Therefore, the optimal mass fraction of the polyvinyl alcohol aqueous solution in this application is 0.45%-0.55%.
[0123] Combining the data of Examples 3 and 7, it can be seen that the difference between Example 7 and Example 3 is that Example 7 uses water glass to prepare component A, while Example 3 uses pure Na2O·2SiO2. The results show that the car cover film liquid sample prepared in Example 7 slightly bubbles after being exposed to ultraviolet light at 80°C for 72 hours, and slightly turns yellow and has residual glue after being immersed in 37°C electrolyte for 72 hours, which proves that using water glass directly to replace Na2O·2SiO2 will have a great impact on the car cover film liquid of the present application, and the car cover film liquid of the present application can only use Na2O·2SiO2.
[0124] Combining the data of Examples 3, 8, 9, 10, and 11, it can be seen that the difference between Examples 8, 9, 10, and 11 and Example 3 is that when using the car cover film liquid, the ratio of component A to component B is different. The car cover film liquid samples prepared in Examples 8 and 9 have a greater adhesive tensile strength after baking at 80°C for 7 days than the car cover film liquid sample prepared in Example 3, and other parameters are the same as those in Example 3; the car cover film liquid samples prepared in Examples 10 and 11 have a greater adhesive tensile strength after baking at 80°C for 7 days than the car cover film liquid sample prepared in Example 3, and both of them turn slightly yellow after being immersed in 37°C electrolyte for 72 hours; therefore, the optimal mass ratio of component B to component A when used in this application is 1:(5-10).
[0125] Combining the data of Examples 3 and 12, it can be seen that the difference between Example 12 and Example 3 is that when the car cover film liquid of Example 12 is used, the spraying time of component A and the pasting time of the car cover are different. The car cover film liquid sample prepared in Example 12 turns slightly yellow after being soaked in 37°C electrolyte for 72 hours, which proves that when the car cover film liquid of this application is used, it is necessary to follow the time range of this application "after spraying component B on the car surface, spray component A within 0-5 minutes; after spraying component A, stick the car cover within 0-10 minutes" to achieve the best effect of pasting the car cover.
[0126] Combining the data of Example 3 and Comparative Examples 1 and 2, it can be seen that the difference between Comparative Examples 1 and 2 and Example 3 is that carbomer and triethanolamine are not added in Comparative Examples 1 and 2, respectively. The results show that the car cover film liquid samples prepared in Comparative Examples 1 and 2 have a greater adhesive tensile strength after baking at 80°C for 7 days than the car cover film liquid samples prepared in Example 3, and turn slightly yellow after immersion in 37°C electrolyte for 72 hours; this proves that carbomer and triethanolamine are indispensable in the preparation of component A.
[0127] Combining the data of Example 3 and Comparative Example 3, it can be seen that the difference between Comparative Example 3 and Example 3 is that Na2O·2SiO2 is not added in Comparative Example 3. The results show that the car cover film liquid sample prepared in Comparative Example 3 slightly bubbles after being irradiated with ultraviolet light at 80°C for 72 hours, and slightly turns yellow and has residual glue after being immersed in 37°C electrolyte for 72 hours. The adhesion tension after baking at 80°C for 7 days is greater than the adhesion tension of the car cover film liquid sample prepared in Example 3 after baking at 80°C for 7 days, which proves that Na2O·2SiO2 must be added when preparing component A.
[0128] Combining the data of Example 3 and Comparative Example 4, it can be seen that the difference between Comparative Example 4 and Example 3 is that propylene glycol is not added in Comparative Example 4. The results show that the car cover film liquid sample prepared in Comparative Example 4 slightly bubbles after being irradiated with ultraviolet light at 80°C for 72 hours, and slightly turns yellow and has residual glue after being immersed in 37°C electrolyte for 72 hours. The adhesion tension after baking at 80°C for 7 days is greater than the adhesion tension after baking at 80°C for 7 days prepared in Example 3, which proves that propylene glycol must be added as a lubricant.
[0129] Combining the data of Example 3 and Comparative Examples 5 and 6, it can be seen that the difference between Comparative Examples 5 and 6 and Example 3 is that the high molecular weight polyvinyl alcohol in Comparative Example 5 is replaced by alumina powder, and the alumina powder in Comparative Example 6 is replaced by high molecular weight polyvinyl alcohol. The car cover film liquid samples prepared in Comparative Examples 5 and 6 slightly bubbled after ultraviolet irradiation at 80°C for 72 hours, and turned slightly yellow and had residual glue after being immersed in 37°C electrolyte for 72 hours. The adhesion tension after baking at 80°C for 7 days was greater than the adhesion tension after baking at 80°C for 7 days prepared in Example 3, which proves that high molecular weight polyvinyl alcohol and alumina powder cannot replace each other, and only when used together can they play a synergistic role.
[0130] Combining the data of Example 3 and Comparative Example 7, it can be seen that the difference between Comparative Example 7 and Example 3 is that when using the car cover film liquid, Comparative Example 7 mixes component A and component B and sprays them at the same time. The results show that the car cover film liquid sample prepared in Comparative Example 7 slightly bubbles after being irradiated with ultraviolet light at 80°C for 72 hours, turns yellow and has residual glue after being soaked in 37°C electrolyte for 72 hours, and has a greater stickiness and tension after baking at 80°C for 7 days than the car cover film liquid sample prepared in Example 3 after baking at 80°C for 7 days, which proves that the use steps of component A and component B are very important to the final effect of the car cover film liquid of this application.
[0131] Combining the data of Example 3 and Comparative Example 8, it can be seen that the difference between Comparative Example 8 and Example 3 is that Comparative Example 8 is a commercially available car cover film liquid, and the car cover film liquid sample prepared in Comparative Example 8 has a slightly greater adhesive tension after being baked at 80°C for 7 days than the car cover film liquid sample prepared in Example 3 has a slightly greater adhesive tension after being baked at 80°C for 7 days, and both samples turn slightly yellow after being immersed in 37°C electrolyte for 72 hours, which proves that the performance of the commercially available car cover film liquid samples is not as good as the car cover film liquid samples prepared under the optimal conditions of the present application.
[0132] This specific embodiment is merely an explanation of the present application and is not a limitation of the present application. After reading this specification, those skilled in the art may make modifications to the present embodiment without any creative contribution as needed. However, as long as it is within the scope of the claims of the present application, it shall be protected by the patent law.
Claims
1. A car cover film liquid, characterized in that: The invention comprises component A and component B. Component A comprises triethanolamine, carbomer, resin, sodium silicate, propylene glycol, preservative, defoaming agent and thickener; and component B comprises high molecular weight polyvinyl alcohol and aluminum oxide powder.
2. The car cover film liquid according to claim 1, characterized in that: The component A comprises the following substances in parts by weight: 3-5 parts of triethanolamine, 0.5-1 parts of carbomer, 30-50 parts of resin, 5-10 parts of sodium silicate, 3-7 parts of glycerol, 0.1-0.5 parts of preservative, 0.5-1 parts of defoamer and 0.6-1.5 parts of thickener.
3. The car cover film liquid according to claim 1, characterized in that: The mass ratio of high molecular weight polyvinyl alcohol to aluminum oxide in the B component is 1:(0.1-0.3).
4. The car cover film liquid according to claim 1, characterized in that: The alumina powder is nanometer beta-type alumina powder; the high molecular weight polyvinyl alcohol is a high molecular weight polyvinyl alcohol aqueous solution with a mass fraction of 0.45%-0.55%.
5. The car cover film liquid according to claim 1, characterized in that: The sodium silicate is Na2O·2SiO2.
6. The car cover film liquid according to claim 1, characterized in that: The resin is one of liquid epoxy resin, polyurethane resin or acrylic resin.
7. A method for preparing the car cover film liquid according to any one of claims 1 to 5, characterized in that: The preparation method of component A comprises the following steps: triethanolamine, carbomer, resin, sodium silicate, glycerol, preservative, defoamer and thickener are mixed, and a defoaming stirrer is used to stir the mixture at a speed of 100-300 rpm for 0.5-1 h to obtain component A; the preparation method of component B comprises the following steps: alumina powder is added to a high molecular weight polyvinyl alcohol solution, and a defoaming stirrer is used to stir the mixture at a speed of 500-800 rpm for 0.5-1 h to obtain component B.
8. A method for using the car cover film liquid according to any one of claims 1 to 5, characterized in that: The method for using the car cover film liquid comprises the following steps: Step 1, diluting the component A with deionized water, wherein the weight ratio of the component A to the deionized water is 1:(80-150); Step 2, when applying the car cover, first spray component B on the car surface, then spray component A on the car surface, and finally apply the car cover.
9. The method for using the car cover film liquid according to claim 8, characterized in that: The mass ratio of the B component to the A component sprayed on the surface of the car is 1:(5-10).
10. The method for using the car cover film liquid according to claim 8, characterized in that: After the B component is sprayed on the surface of the car, the A component is sprayed within 0-5 minutes; after the A component is sprayed, the car cover is applied within 0-10 minutes.
Citation Information
Patent Citations
Car solar film cutting tool, cutting method and mounting method
CN105600041A
Method suitable for automotive glass suspension bubble-cutting pasting
CN110682658A
Foam type invisible car cover mounting liquid
CN115368973A