Polymer-based fracturing fluid and application thereof

By using reflux accelerator and flow synergist in fracturing fluid, the problems of adsorption and retention of polymer thickener and liquid flow resistance are solved, which significantly reduces the damage of low permeability reservoirs and improves the reflux capacity of oil and gas and The overall seepage capacity of the reservoir has achieved effective transformation of low-permeability tight oil and gas reservoirs.

CN119060713AActive Publication Date: 2024-12-03CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202311651794.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-05-30
Filing Date
2023-12-05
Publication Date
2024-12-03
Estimated Expiration
2043-12-05

AI Technical Summary

Technical Problem

In the existing volume fracturing technology, the adsorption and retention of polymer thickeners and high liquid flow resistance lead to serious damage to the low permeability and tight oil and gas reservoirs, and the oil and gas seepage channels are reduced, making it difficult to return oil and gas discharge, and the production increase effect is not significant.

Method used

Using a fracturing fluid including reflux accelerator, polymer thickener, clay stabilizer and discharge aid, the fracturing fluid is enhanced by synergistic action of ammonium chloride, sodium nitrite and flow synergist. Reflow capacity, reduces adsorption and retention of thickener and reduces liquid flow resistance.

Benefits of technology

It significantly reduces the damage of fracturing fluid to the low-permeability reservoir, improves the fracturing transformation effect, enhances the oil and gas re-discharge capacity, improves the overall seepage capacity of the reservoir, and realizes three-dimensional transformation of the reservoir.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119060713A_ABST
    Figure CN119060713A_ABST
Patent Text Reader

Abstract

The invention provides a polymer-based fracturing fluid and application thereof. The fracturing fluid provided by the invention comprises a flowback accelerant, a polymer thickening agent, a clay stabilizer, a cleanup additive and water. Wherein the flowback accelerant comprises ammonium chloride, sodium nitrite and a flow synergist. The flow synergist is a chemical loading product of a compound shown as a structural diagram I on nano silicon dioxide; # imgabs0, wherein A is a naphthalene ring at an optional substitution position; n is an integer from 1 to 10; n R is independently selected from one of a chemical single bond and alkylene of C1 to C10; n X is independently selected from-O-or-NH-, and at least one X is-NH-.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Related Applications

[0002] This application claims the priority of Chinese patent application CN202310621396.0, entitled “A polymer-based fracturing fluid and its application”, filed on May 30, 2023, and the entire contents of CN202310621396.0 are incorporated herein by reference. Technical Field

[0003] The invention belongs to the technical field of oil and gas reservoir transformation, and in particular relates to a polymer-based fracturing fluid and application thereof. Background Art

[0004] Low-permeability tight oil and gas reservoirs are mostly medium- and low-permeability reservoirs, and low-permeability and ultra-low-permeability reservoirs account for a considerable proportion. The reservoirs are obviously heterogeneous, with low porosity, poor connectivity, and strong sensitivity. At home and abroad, attempts have been made to carry out volume fracturing transformation technology in tight sandstone gas reservoirs. Volume fracturing "breaks" the reservoir matrix by fracturing. The cracks obtained are first shear fracture cracks, accompanied by tearing cracks that are both tensile fractures and shear fractures, and the crack morphology is complex. With the increase of construction time, shear fracture cracks and tearing cracks will also transform into tensile fractures. This phenomenon of transformation into tensile fractures is particularly common in cracks near the wellbore, thus forming a network of fractures, which can maximize the contact area between the fracture wall and the reservoir matrix, minimize the seepage distance of oil and gas in the matrix to the fracture, and minimize the seepage resistance of the matrix fluid to the fracture, greatly improving the overall seepage capacity of the reservoir and realizing the "three-dimensional transformation" of the reservoir in the three-dimensional directions of length, width, and height.

[0005] In the polymer fracturing fluid system used in volume fracturing, polymer thickeners (powders, emulsions) are one of the main components. Polymer fracturing fluids cause serious damage to the core matrix of the reservoir, with a damage rate of more than 70% and a gas-tested core permeability recovery rate of no more than 30%. The main factors causing matrix damage include polymer residues in the fracturing fluid, thickener adsorption and retention damage, water lock and water-sensitive effects. In particular, the density of the hydrophilic group of the polymer thickener is large, and its core adsorption and retention damage is greater than that of plant gums such as guar gum, which will directly cause the reduction of oil and gas seepage channels, difficulty in oil and gas backflow in the matrix, and insignificant oil and gas production increase effects.

[0006] In view of the above situation, it is necessary to carry out research on flowback promoters, on this basis to form strong flowback fracturing fluid, which can not only provide additional flowback energy, but also overcome the adsorption and retention problems of thickeners, reduce liquid flow resistance, and improve the fracturing transformation effect. Summary of the invention

[0007] The object of the present invention is to provide a fracturing fluid which can not only overcome the adsorption and retention problem of polymer thickeners, but also reduce the flow resistance of liquid and cause less damage to low-permeability reservoirs.

[0008] The invention provides a fracturing fluid, which comprises a flowback promoter, a polymer thickener, a clay stabilizer, a drainage aid and water.

[0009] According to a specific embodiment of the present invention, the mass of the water is calculated as 100%, the mass concentration of the backflow promoter is 12.4wt% to 18.7%, the mass concentration of the polymer thickener is 0.01wt% to 0.75wt%, the mass concentration of the clay stabilizer is 0.1wt% to 1wt%, and the mass concentration of the drainage aid is 0.1wt% to 1wt%;

[0010] Preferably, taking the mass of the water as 100%, the mass concentration of the flowback promoter is 12.4wt% to 18.7wt%, the mass concentration of the polymer thickener is 0.05wt% to 0.3wt%, the mass concentration of the clay stabilizer is 0.2wt% to 0.3wt%, and the mass concentration of the drainage aid is 0.2wt% to 0.4wt%.

[0011] According to a specific embodiment of the present invention, the flowback promoter includes ammonium chloride, sodium nitrite and a flow enhancer.

[0012] According to a specific embodiment of the present invention, taking the mass of the flowback promoter as 100%, the flowback promoter includes 42.8wt% to 43wt% of ammonium chloride, 55.2wt% to 55.5wt% of sodium nitrite and 1.6wt% to 2wt% of the flow enhancer.

[0013] According to a specific embodiment of the present invention, the flow enhancer is a chemically supported product of a compound having a structural schematic diagram as shown in Formula I on nano-silicon dioxide;

[0014]

[0015] wherein A is a naphthalene ring optionally substituted at a position; n is an integer from 1 to 10; n Rs are independently selected from a chemical single bond and C1 to C 10 n X are independently selected from -O- or -NH-, and at least one X is -NH-.

[0016] According to a specific embodiment of the present invention, the average particle size of the nano-silicon dioxide is 1 nm to 50 nm;

[0017] Preferably, the nano-silica is hydroxylated nano-silica.

[0018] According to a specific embodiment of the present invention, in Formula I, n is an integer from 2 to 6; and / or

[0019] The n Rs are independently selected from one of a chemical single bond and a C1 to C4 alkylene group.

[0020] According to a specific embodiment of the present invention, the compound is hydroxyaminonaphthalene;

[0021] Preferably, the compound is 2,3-dihydroxy-1-methylaminonaphthalene.

[0022] According to a specific embodiment of the present invention, the flow enhancer is prepared by the following method:

[0023] The hydroxylated modified nano silicon dioxide and hydroxyaminonaphthalene are subjected to a first reaction in water to obtain the flow enhancer;

[0024] Preferably, the mass ratio of the hydroxylated modified nano-silicon dioxide to hydroxyaminonaphthalene is 1:2 to 1:4;

[0025] Preferably, the first reaction is carried out at 60°C to 80°C for 20h to 24h;

[0026] Preferably, the hydroxylated modified nano-silica is prepared by the following method:

[0027] Allowing the nano-silicon dioxide to undergo a second reaction in concentrated sulfuric acid to obtain the hydroxylated modified nano-silicon dioxide;

[0028] Preferably, before hydroxylation modification, the particle size of the nano-silica is 1 nm to 50 nm;

[0029] Preferably, the concentration of the concentrated sulfuric acid is 70% to 98%, and the volume / mass ratio of the concentrated sulfuric acid to the nano-silicon dioxide is 1:(0.01 to 0.1);

[0030] Preferably, the second reaction is carried out at 120° C. to 150° C. for 10 to 12 hours.

[0031] According to a specific embodiment of the present invention, the hydroxyaminonaphthalene is prepared by the following method:

[0032] A. subjecting halomethoxynaphthalene and copper cyanide to a third reaction to obtain a first intermediate product;

[0033] B. subjecting the first intermediate product and lithium aluminum tetrahydride to a fourth reaction to obtain a second intermediate product;

[0034] C. subjecting the second intermediate product to a fifth reaction in an acidic environment;

[0035] D. subjecting the reaction product obtained by the fifth reaction and butyllithium to a sixth reaction;

[0036] E. subjecting the reaction product obtained by the sixth reaction to a seventh reaction in a neutral or alkaline environment to obtain the hydroxyaminonaphthalene.

[0037] According to a specific embodiment of the present invention, the halomethoxynaphthalene is 1-bromo-2,3-dimethoxynaphthalene; and / or

[0038] The hydroxyaminonaphthalene is 2,3-dihydroxy-1-methylaminonaphthalene.

[0039] According to a specific embodiment of the present invention, the molar ratio of the halomethoxynaphthalene to copper cyanide is 1:1 to 2:1;

[0040] and / or

[0041] The molar ratio of the halomethoxynaphthalene to the lithium aluminum hydroxide is 1:1 to 2:1; and / or

[0042] The molar ratio of the halomethoxynaphthalene to the butyl lithium is 1:1.

[0043] According to a specific embodiment of the present invention, in step A, the third reaction is carried out in a first organic solvent; and / or

[0044] In step B, the fourth reaction is carried out in a second organic solvent; and / or

[0045] In step C, a carboxylic acid-lower alcohol mixture is added to create the acidic environment; and / or

[0046] In step E, an inorganic base is added to adjust the pH to neutral or alkaline;

[0047] Preferably, the first organic solvent is N-methylpyrrolidone; and / or

[0048] The second organic solvent is diethyl ether; and / or

[0049] The carboxylic acid-lower alcohol mixture is a mixture of formic acid and ethanol; and / or

[0050] The inorganic base is sodium hydroxide;

[0051] Preferably, the total mass of the halomethoxynaphthalene, copper cyanide, lithium aluminum hydroxide and butyl lithium is taken as 100wt%, the amount of the formic acid is 1wt% to 2wt%, and the amount of the ethanol is 3wt% to 5wt%; and / or

[0052] The acidic environment refers to a pH of 3 to 5; and / or

[0053] In step E, the pH is adjusted to between 7 and 9.

[0054] According to a specific embodiment of the present invention, the conditions of the third reaction are to react at 200° C. for 4 to 6 hours;

[0055] and / or

[0056] The fourth reaction is carried out at room temperature (i.e. 25° C.) for 2 to 3 hours; and / or

[0057] The fifth reaction is carried out at 60° C. for 2 h; and / or

[0058] The sixth reaction is carried out at room temperature (i.e. 25° C.) for 1 hour; and / or

[0059] The seventh reaction was carried out at 50° C. for 5 h.

[0060] According to a specific embodiment of the present invention, the clay stabilizer is an alkyl ammonium salt;

[0061] Preferably, the alkylammonium salt is hexadecyltrimethylammonium chloride; and / or

[0062] The polymer thickener is selected from polyacrylamide and / or acrylamide copolymer; and / or

[0063] The drainage aid is polyoxyethylene ether;

[0064] Preferably, the weight average molecular weight of the polymer thickener is not less than 10 million;

[0065] Preferably, the acrylamide copolymer is a 2-acrylamide-2-methylpropanesulfonic acid / acrylamide / maleic anhydride copolymer, an acrylamide / N,N-dimethylacrylamide / 2-acrylamide-2-methylpropanesulfonic acid copolymer, an acrylamide / 2-acrylamide-2-methylpropanesulfonic acid / 2-acrylamide hexadecanesulfonic acid copolymer;

[0066] Preferably, the polymer thickener is polyacrylamide;

[0067] Preferably, the weight average molecular weight of the polyacrylamide is 10 million to 20 million.

[0068] In the present invention, the weight average molecular weight of the polymer thickener can be adjusted according to the target reservoir to be actually fractured.

[0069] Application of the fracturing fluid according to the present invention in fracturing reconstruction of low permeability tight oil and gas reservoirs;

[0070] Preferably, the low-permeability tight sandstone oil and gas reservoir is an oil and gas reservoir with a geopressure coefficient lower than 1 and an average permeability lower than 0.1 mD. Beneficial effects of the present invention:

[0071] In view of the problems of polymer thickener adsorption and retention, high flow resistance of return liquid and high damage to low permeability reservoirs in the fracturing fluid in the existing volume fracturing technology, the present invention provides a polymer-based fracturing fluid and its application. The fracturing fluid includes a return promoter, a polymer thickener, a clay stabilizer, a drainage aid and water. Among them, the return promoter includes ammonium chloride, sodium nitrite and a flow enhancer, and there is a synergistic effect between the three in enhancing the return capacity of the fracturing fluid. The fracturing fluid provided by the present invention can generate additional fluid return energy by spontaneous gas generation at the reservoir temperature, while reducing the adsorption and retention of polymer thickeners on the rock surface, and can reduce the starting pressure of the liquid in the core, reduce the flow resistance of the liquid, improve the return capacity of the fracturing fluid, and finally greatly reduce the damage of the fracturing fluid to the low permeability reservoir. It is a fracturing fluid that can not only overcome the adsorption and retention problem of the polymer thickener, but also reduce the flow resistance of the liquid, and has lower damage to the low permeability reservoir. When the degelling liquid prepared by mixing the fracturing fluid provided by the present invention with a low-temperature degelling agent passes through a powder composed of core particles with an average porosity of 10% and an average permeability of 0.001 mD, the amount of thickener adsorbed on the core particles is 6.8 to 9.1 mg·g -1 ; At 90°C, the confining pressure is fixed at 10MPa and the displacement pressure is slowly increased. The breaking fluid prepared by mixing the fracturing fluid and the low-temperature breaker is displaced with nitrogen. The starting pressure of the breaking fluid containing the fracturing fluid from the experimental rock sample sampled from low-permeability dense sandstone is only 0.32 to 0.56MPa; According to the method specified in 7.7 of SY / T 5107-2016 "Performance Evaluation Method of Water-Based Fracturing Fluid", the breaking fluid prepared by mixing the fracturing fluid and the low-temperature breaker is used as the test medium, and a core displacement experiment is carried out on the experimental rock sample sampled from low-permeability dense sandstone at 90°C. The measured return rate is 71% to 83%, and the damage rate of the fracturing fluid to the matrix permeability of the experimental rock sample is only 20% to 27%. BRIEF DESCRIPTION OF THE DRAWINGS

[0072] Figure 1 The infrared spectrum of 2,3-dihydroxy-1-methylaminonaphthalene prepared in Example 1;

[0073] Figure 2 This is a diagram of a device for measuring the amount of thickener adsorption;

[0074] Figure 3 This is a diagram of the core starting pressure measurement device. DETAILED DESCRIPTION

[0075] The present invention will be further described below in conjunction with examples, but the examples of the present invention are only exemplary descriptions, and the implementation methods do not constitute limitations of the present invention under any circumstances.

[0076] Preparation of flow enhancer

[0077] Example 1

[0078] Preparation of 2,3-dihydroxy-1-methylaminonaphthalene:

[0079] A. 1 mol (i.e. 267 g) of 1-bromo-2,3-dimethoxynaphthalene, 1 mol (i.e. 115.6 g) of copper cyanide and 2 g of N-methylpyrrolidone were mixed and reacted at 200° C. for 4 h to obtain a first intermediate product, which can be directly used in step B without purification;

[0080] B. The obtained first intermediate product, 1 mol (i.e. 38 g) of lithium aluminum tetrahydride and 5 g of ether were mixed and reacted at room temperature (25° C.) for 2 h to obtain a second intermediate product, which can be directly used in step C without purification;

[0081] C. Add a formic acid-ethanol mixture (including 9.69 g of formic acid and 24.2 g of ethanol), adjust the pH of the second intermediate product to 3, react at 60°C for 2 hours, then cool to room temperature (25°C) and add 1 mol (i.e. 64 g) of butyl lithium, react for 1 hour, and finally add sodium hydroxide to adjust the pH to 7, raise the temperature to 50°C and react for 5 hours to obtain 2,3-dihydroxy-1-methylaminonaphthalene.

[0082] 2,3-Dihydroxy-1-methylaminonaphthalene structural characterization:

[0083] The pure 2,3-dihydroxy-1-methylaminonaphthalene product obtained after recrystallization from ethanol was measured with a Fourier transform infrared spectrometer. Figure 1 .

[0084] from Figure 1 It can be seen that the 1-hydroxyl stretching vibration peak, 4-amino stretching vibration peak, 2-naphthalene ring stretching vibration peak, 3-amino bending vibration peak and 5-hydroxyl bending vibration peak appeared in the infrared spectrum. Combined with the preparation process, it was confirmed that 2,3-dihydroxy-1-methylaminonaphthalene was prepared.

[0085] Preparation of hydroxylated modified nano-silica:

[0086] 5 g of nano-silica with a particle size of 1 to 50 nm and 100 mL of 98% concentrated sulfuric acid were mixed and reacted at 150° C. for 12 h to obtain hydroxylated modified nano-silica.

[0087] Preparation of flow enhancer:

[0088] 25 g of hydroxylated modified nano-silica, 50 g of 2,3-dihydroxy-1-methylaminonaphthalene and 25 g of water were mixed and reacted at 80° C. for 24 h to obtain a flow enhancer.

[0089] Preparation of fracturing fluid

[0090] The flow enhancers used in Examples 2 to 8 and Comparative Example 2 are all the flow enhancers prepared in Example 1.

[0091] The polymer thickener used in Examples 2 to 8 and Comparative Examples 1 to 3 is polyacrylamide, which complies with standard Q / SHCG 0149 and is purchased from Dongying Zhongyue Petroleum Technology Co., Ltd. It is determined that the weight average molecular weight thereof is 10 million to 20 million.

[0092] Example 2

[0093] Preparation of fracturing fluid:

[0094] 1) Mix a flowback promoter (specifically comprising 5.35 g of ammonium chloride, 6.9 g of sodium nitrite, and 0.2 g of a flow enhancer), 0.3 g of hexadecyltrimethylammonium chloride, and 100 g of water in a liquid preparation container, and continue stirring until completely dissolved;

[0095] 2) adding 0.05 g of polyacrylamide to the liquid preparation container of step 1), and stirring continuously until the polyacrylamide is completely dissolved;

[0096] 3) Add 0.3 g of polyoxyethylene ether to the liquid preparation container in step 2), continue stirring until the polyoxyethylene ether is completely dissolved, avoid foam overflow during the stirring process, and stir evenly to obtain the fracturing fluid.

[0097] Example 3

[0098] Preparation of fracturing fluid:

[0099] 1) Mix a flowback promoter (specifically comprising 5.35 g of ammonium chloride, 6.9 g of sodium nitrite, and 0.2 g of a flow enhancer), 0.3 g of hexadecyltrimethylammonium chloride, and 100 g of water in a liquid preparation container, and continue stirring until completely dissolved;

[0100] 2) adding 0.1 g of polyacrylamide to the liquid preparation container of step 1), and stirring continuously until the polyacrylamide copolymer is completely dissolved;

[0101] 3) Add 0.3 g of polyoxyethylene ether to the liquid preparation container in step 2), continue stirring until the polyoxyethylene ether is completely dissolved, avoid foam overflow during the stirring process, and stir evenly to obtain the fracturing fluid.

[0102] Example 4

[0103] Preparation of fracturing fluid:

[0104] 1) Mix a flowback promoter (specifically comprising 5.35 g ammonium chloride, 6.9 g sodium nitrite, and 0.2 g flow enhancer), 0.2 g hexadecyltrimethylammonium chloride, and 100 g water in a liquid preparation container, and continue stirring until completely dissolved;

[0105] 2) Add 0.1 g of polyacrylamide to the liquid preparation container of step 1), and continue stirring until the polyacrylamide is completely dissolved;

[0106] 3) Add 0.3 g of polyoxyethylene ether to the liquid preparation container in step 2), continue stirring until the polyoxyethylene ether is completely dissolved, avoid foam overflow during the stirring process, and stir evenly to obtain the fracturing fluid.

[0107] Example 5

[0108] Preparation of fracturing fluid:

[0109] 1) Mix a flowback promoter (specifically comprising 5.35 g of ammonium chloride, 6.9 g of sodium nitrite, and 0.2 g of a flow enhancer), 0.3 g of hexadecyltrimethylammonium chloride, and 100 g of water in a liquid preparation container, and continue stirring until completely dissolved;

[0110] 2) Add 0.1 g of polyacrylamide to the liquid preparation container of step 1), and continue stirring until the polyacrylamide is completely dissolved;

[0111] 3) adding 0.2 g of polyoxyethylene ether to the liquid preparation container in step 2), stirring continuously until the polyoxyethylene ether is completely dissolved, avoiding foam overflow during the stirring process, and stirring evenly to obtain the fracturing fluid.

[0112] Example 6

[0113] Preparation of fracturing fluid:

[0114] 1) Mix a flowback promoter (specifically comprising 6.42 g of ammonium chloride, 8.28 g of sodium nitrite, and 0.3 g of a flow enhancer), 0.3 g of hexadecyltrimethylammonium chloride, and 100 g of water in a liquid preparation container, and continue stirring until completely dissolved;

[0115] 2) adding 0.2 g of polyacrylamide to the liquid preparation container of step 1), and stirring continuously until the polyacrylamide is completely dissolved;

[0116] 3) Add 0.3 g of polyoxyethylene ether to the liquid preparation container in step 2), continue stirring until the polyoxyethylene ether is completely dissolved, avoid foam overflow during the stirring process, and stir evenly to obtain the fracturing fluid.

[0117] Example 7

[0118] Preparation of fracturing fluid:

[0119] 1) Mix a flowback promoter (specifically comprising 6.42 g of ammonium chloride, 8.28 g of sodium nitrite, and 0.3 g of a flow enhancer), 0.3 g of hexadecyltrimethylammonium chloride, and 100 g of water in a liquid preparation container, and continue stirring until completely dissolved;

[0120] 2) adding 0.3 g of polyacrylamide to the liquid preparation container of step 1), and stirring continuously until the polyacrylamide is completely dissolved;

[0121] 3) Add 0.4 g of polyoxyethylene ether to the liquid preparation container in step 2), continue stirring until the polyoxyethylene ether is completely dissolved, avoid foam overflow during the stirring process, and stir evenly to obtain the fracturing fluid.

[0122] Example 8

[0123] Preparation of fracturing fluid:

[0124] 1) Mix a flowback promoter (specifically comprising 8.025 g of ammonium chloride, 10.35 g of sodium nitrite, and 0.3 g of a flow enhancer), 0.3 g of hexadecyltrimethylammonium chloride, and 100 g of water in a liquid preparation container, and continue stirring until completely dissolved;

[0125] 2) adding 0.2 g of polyacrylamide to the liquid preparation container of step 1), and stirring continuously until the polyacrylamide is completely dissolved;

[0126] 3) Add 0.3 g of polyoxyethylene ether to the liquid preparation container in step 2), continue stirring until the polyoxyethylene ether is completely dissolved, avoid foam overflow during the stirring process, and stir evenly to obtain the fracturing fluid.

[0127] Comparative Example 1

[0128] Preparation of fracturing fluid:

[0129] 1) Mix a flowback promoter (specifically comprising 8.025 g of ammonium chloride and 10.35 g of sodium nitrite), 0.3 g of hexadecyltrimethylammonium chloride and 100 g of water in a liquid preparation container, and continue stirring until completely dissolved;

[0130] 2) adding 0.2 g of polyacrylamide to the liquid preparation container of step 1), and stirring continuously until the polyacrylamide is completely dissolved;

[0131] 3) Add 0.3 g of polyoxyethylene ether to the liquid preparation container in step 2), continue stirring until the polyoxyethylene ether is completely dissolved, avoid foam overflow during the stirring process, and stir evenly to obtain the fracturing fluid.

[0132] Comparative Example 2

[0133] Preparation of fracturing fluid:

[0134] 1) Mix a flowback promoter (specifically 0.2 g of flow enhancer), 0.3 g of hexadecyltrimethylammonium chloride and 100 g of water in a liquid preparation container, and continue stirring until completely dissolved;

[0135] 2) adding 0.2 g of polyacrylamide to the liquid preparation container of step 1), and stirring continuously until the polyacrylamide is completely dissolved;

[0136] 3) Add 0.3 g of polyoxyethylene ether to the liquid preparation container in step 2), continue stirring until the polyoxyethylene ether is completely dissolved, avoid foam overflow during the stirring process, and stir evenly to obtain the fracturing fluid.

[0137] Comparative Example 3

[0138] Preparation of fracturing fluid:

[0139] 1) Mix 0.3 g of hexadecyltrimethylammonium chloride and 100 g of water in a liquid preparation container and continue stirring until completely dissolved;

[0140] 2) adding 0.2 g of polyacrylamide to the liquid preparation container of step 1), and stirring continuously until the polyacrylamide is completely dissolved;

[0141] 3) Add 0.3 g of polyoxyethylene ether to the liquid preparation container in step 2), continue stirring until the polyoxyethylene ether is completely dissolved, avoid foam overflow during the stirring process, and stir evenly to obtain the fracturing fluid.

[0142] Fracturing fluid performance evaluation

[0143] 1. Determination of gas volume generated by fracturing fluid reaction

[0144] i. directly placing the fracturing fluids prepared in Examples 2 to 8 and Comparative Examples 1 to 3 in sealed wide-mouth bottles with air guide tubes, and connecting the outlets of the air guide tubes to a gas collecting device;

[0145] ⅱPut the wide-mouth bottle containing the fracturing fluid in a constant temperature water bath, heat it to 90℃ and then keep the temperature constant, collect the gas generated by the fracturing fluid reaction until no more gas is generated, and calculate the amount of gas generated, which is the reaction gas amount of the fracturing fluid.

[0146] The specific results are shown in Table 1.

[0147] Table 1. Gas production from fracturing fluid reaction

[0148]

[0149]

[0150] From the data in Table 1, it can be seen that the fracturing fluids containing ammonium chloride and sodium nitrite prepared in Examples 2 to 8 can react to produce gas at 90°C, and by comparing the data of Example 8 with Comparative Example 1, it can be seen that the addition of the flow enhancer does not significantly affect the reaction gas generation of ammonium chloride and sodium nitrite. The fracturing fluids prepared in Comparative Examples 2 and 3 do not contain sodium nitrite and ammonium chloride, and cannot generate gas. The mass of sodium nitrite and ammonium chloride in the fracturing fluids prepared in Examples 2 to 5 are equal, and the amount of gas generated by the reaction is almost unchanged; the mass of sodium sulfite and ammonium chloride in the fracturing fluids prepared in Examples 6 and 7 are equal, the mass of sodium nitrite and ammonium chloride and the total mass proportion of sodium nitrite and ammonium chloride in the fracturing fluid are greater than those in Examples 2 to 5, and the amount of gas generated by the reaction is greater than that in Examples 2 to 5; the mass of sodium nitrite and ammonium chloride in the fracturing fluid prepared in Example 8 and the total mass proportion of sodium nitrite and ammonium chloride in the fracturing fluid are higher than those in Examples 6 and 7, and the amount of gas generated by the reaction is also higher than that in Examples 6 and 7. Therefore, the total mass proportion of sodium nitrite and ammonium chloride in the fracturing fluid is positively correlated with the amount of reaction gas. The greater the total mass proportion of sodium nitrite and ammonium chloride in the fracturing fluid, the more reaction gas is generated, the stronger the pressure-raising ability of the formation is, which is beneficial to improving the return of the fracturing fluid.

[0151] 2. Determination of thickener adsorption, starting pressure, flowback rate and matrix permeability damage rate

[0152] The low-temperature breakers used in the following experiments were purchased from Dongying Zhongyue Petroleum Technology Co., Ltd.

[0153] A. Determination of Thickener Adsorption

[0154] use Figure 2 The apparatus shown was used to measure the thickener adsorption amount of the fracturing fluids prepared in Examples 2 to 8 and Comparative Examples 1 to 3, and to evaluate the ability of the fracturing fluids to reduce the adsorption damage of the thickener to the core. The specific method is as follows:

[0155] (1) directly adding 600 ppm of low-temperature breaker to the fracturing fluids prepared in Examples 2 to 8 and Comparative Examples 1 to 3, and then aging the fracturing fluids at 35° C. for 24 h until the viscosity of the fracturing fluids after adding the low-temperature breaker is less than 5 mPa.s, and then taking out the fracturing fluids to obtain 10 groups of breaker fluids for standby use;

[0156] (2) firstly, any one of the 10 groups of gel-breaking solutions prepared in step (1) is loaded into an intermediate container; the sand filling tube of the high-temperature and high-pressure filter loss instrument is filled with core particles with a particle size of 0.21 to 0.3 mm (i.e., 70 to 50 meshes), an average porosity of 10%, and an average permeability of 0.001 mD, and then the high-temperature and high-pressure filter loss instrument is preheated to 90° C.;

[0157] (3) Close the valve connecting the nitrogen bottle to the high-temperature and high-pressure filter loss instrument, open the valve connecting the high-temperature and high-pressure filter loss instrument to the intermediate container, and drive the flow pump to allow the debonding liquid in the intermediate container to pass through the high-temperature and high-pressure filter loss instrument preheated to 90°C and filled with core particles at a displacement of 5 mL / min. After all the debonding liquid enters the debonding liquid collector, close the valve connecting the high-temperature and high-pressure filter loss instrument to the intermediate instrument, then open the valve connecting the nitrogen bottle to the high-temperature and high-pressure filter loss instrument, and continue to purge with nitrogen for 10 minutes to prevent the debonding liquid from being mechanically retained in the high-temperature and high-pressure filter loss instrument;

[0158] (4) Obtain a sample of the degelling liquid from the degelling liquid collector, detect the residual thickener content therein by using an ultraviolet spectrophotometer, and calculate the amount of thickener adsorbed by the core particles in the sand filling tube of the high-temperature and high-pressure filter loss instrument by formula (1);

[0159]

[0160] Where, F is the adsorption amount of thickener, g / g;

[0161] m is the mass of thickener in the debonding liquid in the intermediate container without sand filling, g;

[0162] C is the concentration of thickener in the degelling liquid passing through the sand-filled tube in the degelling liquid collector, g / L;

[0163] V is the volume of the degelling liquid that passes through the sand-filled tube in the degelling liquid collector, L.

[0164] According to steps (2) to (4), experiments were carried out using 10 groups of degelling solutions prepared in step (1). The specific results are shown in Table 2.

[0165] B. Start-up pressure measurement

[0166] use Figure 3 The core starting pressure measuring device shown in the figure measures the starting pressure of the fracturing fluid prepared in Examples 2 to 8 and Comparative Examples 1 to 3 when it is discharged from the core. The specific steps are as follows:

[0167] ① Drill multiple cores from the same low-permeability dense sandstone core sample, cut them into samples of equal length, then put the samples into an oven and dry them at 105℃ for 24h, and place them in a drying dish for later use;

[0168] ② Directly add 600 ppm of low-temperature breaker to the fracturing fluids prepared in Examples 2 to 8 and Comparative Examples 1 to 3, respectively, and then age at 35° C. for 24 h until the viscosity of the fracturing fluids after adding the low-temperature breaker is lower than 5 mPa.s, and then take out to obtain 10 groups of breaker fluids for standby use;

[0169] ③ Use the overburden porosimeter to measure the porosity and permeability of the dried rock samples obtained in step ①, select 10 rock samples with basically the same porosity and permeability (average porosity 10%, average permeability 0.001mD) as experimental rock samples, and then use the 10 groups of gel-breaking solutions prepared in step ② to establish 40% initial gel-breaking solution saturation for the 10 experimental rock samples according to 5.1.5 of Q / SH 0501-2013 "Flow Experiment Evaluation Method for Tight Reservoir Sensitivity";

[0170] ④First, select any one of the 10 experimental rock samples with an initial saturation of 40% gel-breaking liquid obtained in step ③ and load it into the core holder, then adjust the confining pressure pump to apply a confining pressure of 10 MPa to the experimental core, heat the core holder and the experimental rock sample clamped therein to 90°C and maintain a constant temperature, slowly adjust the input nitrogen pressure using a pressure reducing valve, observe for 2 minutes each time the pressure is increased by 0.1 MPa, displace the gel-breaking liquid, and nitrogen flows out of the soap foam flowmeter. At this time, the nitrogen pressure is the starting pressure of the experimental rock sample at an initial saturation of 40% gel-breaking liquid;

[0171] According to the method in step ④, the starting pressures of the 10 experimental rock samples with an initial saturation of 40% of the gel-breaking liquid obtained in step ③ were measured respectively. The specific results are shown in Table 2.

[0172] C. Determination of flowback rate and matrix permeability damage rate

[0173] According to 7.7 of SY / T 5107-2016 “Method for evaluating performance of water-based fracturing fluid”, the flowback rate and matrix permeability damage rate were determined.

[0174] In the determination of the flowback rate and matrix permeability damage rate, 10 groups of gel-breaking liquids prepared in step ② of experiment B were used as the test medium.

[0175] a. Determination of flowback rate: For the experimental rock sample with an average porosity of 10% and an average permeability of 0.001 mD, an initial water saturation of 40% is established according to 5.1.5 Initial water saturation establishment method of Q / SH0501-2013 "Flow Experiment Evaluation Method for Tight Reservoir Sensitivity", and the experimental rock sample with an initial water saturation of 40% is placed in the core holder. The confining pressure pump is adjusted to apply a confining pressure of 10 MPa to the experimental rock sample, and then the core holder and the experimental rock sample clamped therein are heated to 90°C and maintained at a constant temperature. One group of gel-breaking liquids is selected from the 10 groups of gel-breaking liquids, and a sufficient amount of gel-breaking liquid (the volume is recorded as V1) is added to the intermediate container at the inlet end. The displacement pressure is maintained at 3.5 MPa to drive the gel-breaking liquid through the core holder, and the gel-breaking liquid passing through the experimental rock sample is collected at the outlet end as the flowback liquid. The displacement time is 30 min, and the collected flowback liquid volume is recorded as V2. The flowback rate is calculated using the following formula (2):

[0176]

[0177] b. Determination of matrix permeability damage rate: For the experimental rock samples with an average porosity of 10% and an average permeability of 0.001 mD, an initial water saturation of 40% is established according to the initial water saturation establishment method in 5.1.5 of Q / SH 0501-2013 "Flow Experiment Evaluation Method for Tight Reservoirs", and the obtained experimental rock samples with a water saturation of 40% are placed in the core holder, and the confining pressure pump is adjusted to apply a confining pressure of 10 MPa to the experimental rock samples, and then the core holder and the experimental rock samples clamped therein are heated to 90°C and maintained at a constant temperature. At a displacement pressure of 3.5 MPa, one group of gel-breaking liquids is selected from 10 groups of gel-breaking liquids to carry out a displacement experiment on the experimental rock samples (i.e., a sufficient amount of gel-breaking liquid is added to the intermediate container at the inlet end, and the displacement pressure is maintained at 3.5 MPa to drive the gel-breaking liquid through the core holder), and the matrix permeability damage rate of the experimental rock samples is analyzed;

[0178] According to the methods described in a and b, 10 groups of debonding solutions were used to measure the flowback rate and matrix permeability damage rate. The specific results are shown in Table 2.

[0179] Table 2. Thickener adsorption, start-up pressure, flowback rate, matrix permeability damage rate

[0180]

[0181]

[0182] The data of thickener adsorption in Table 2 show that when the debonding liquid prepared from the fracturing fluid containing flow enhancer prepared in Examples 2 to 8 and Comparative Example 2 passes through the powder composed of core particles, the thickener adsorption on the core particles is 6.8 to 9.8 mg·g -1 , the thickener adsorption amount is very low; when the degelling liquid prepared by the fracturing fluid without flow enhancer prepared by Comparative Example 1 and Comparative Example 3 passes through the powder composed of core particles, the thickener adsorption amount on the core particles is 15.2 and 19.4 mg·g -1 , the thickener adsorption amount is significantly higher than that of Examples 2 to 8 and Comparative Example 2, specifically 1.9 times and 2.4 times the thickener adsorption amount of Example 8. It is proved that the fracturing fluid containing flow enhancer prepared in Examples 2 to 8 and Comparative Example 2 has obvious thickener adsorption inhibition effect, and the thickener adsorption retention amount generated in the experimental rock sample is small, which can effectively reduce the solid phase damage of the fracturing fluid to the formation in practical application.

[0183] The starting pressure data and flowback rate data in Table 2 show that the starting pressure of the fracturing fluid prepared in Examples 2 to 8 is 0.32 to 0.56 MPa, and the flowback rate is 71% to 83%, while the starting pressure of the fracturing fluid prepared in Comparative Examples 1 to 3 is 1.18 to 2.3 MPa, and the flowback rate is 42% to 63%. The starting pressure of the fracturing fluid prepared in Comparative Examples 1 to 3 is significantly higher than that in Examples 1 to 8, and the flowback rate is significantly lower than that in Examples 2 to 8. The starting pressure of the fracturing fluid prepared in Comparative Examples 1 to 3 is 4.7 times, 3.7 times and 7.2 times the starting pressure of the fracturing fluid prepared in Example 8, and the flowback rate of the fracturing fluid prepared in Example 8 is 1.6 times, 1.3 times and 2 times that of Comparative Examples 1 to 3, respectively. The lower starting pressure and higher flowback rate prove that the fracturing fluid prepared in Examples 2 to 8 is easier to flow back into the formation.

[0184] The matrix permeability damage rate data in Table 2 show that the matrix permeability damage rate of the fracturing fluids prepared in Examples 2 to 8 is 20% to 27%, while the matrix permeability damage rate of the fracturing fluids prepared in Comparative Examples 1 to 3 is 35% to 50%, which proves that the fracturing fluids prepared in Examples 2 to 8 can significantly reduce the matrix permeability damage rate.

[0185] Combined with the data of thickener adsorption, starting pressure, backflow rate and matrix permeability damage rate of the fracturing fluids prepared in Examples 2 to 8 and Comparative Examples 1 to 3 in Table 2 and the formula analysis of the fracturing fluids prepared in Examples 2 to 8 and Comparative Examples 1 to 3: The fracturing fluid prepared in Comparative Example 3 does not contain a backflow promoter (i.e., ammonium chloride, sodium nitrite and flow enhancer), and its thickener adsorption, starting pressure and matrix permeability damage rate are the highest, and the backflow rate is the lowest. It can be seen that in actual application, it causes the highest degree of core damage to the formation, including solid phase damage, and is the least likely to flow back; compared with Comparative Example 3, only the flow enhancer is added to the fracturing fluid prepared in Comparative Example 2, and the thickener adsorption amount of the fracturing fluid prepared in Comparative Example 2 is , starting pressure and matrix permeability damage rate are all reduced compared with those of Comparative Example 3, while the flowback rate is significantly improved; compared with Comparative Example 3, only ammonium chloride and sodium nitrite are added to the fracturing fluid prepared in Comparative Example 1, and the thickener adsorption amount, starting pressure and matrix permeability damage rate of the fracturing fluid prepared in Comparative Example 1 are respectively reduced compared with those of Comparative Example 3, and the flowback rate is improved; compared with Comparative Example 3, a flowback promoter (i.e., ammonium chloride, sodium nitrite and flow enhancer) is added to the fracturing fluid prepared in Example 8, and the thickener adsorption amount, starting pressure and matrix permeability damage rate of the fracturing fluid prepared in Example 8 are respectively reduced by 58%, 86% and 60% compared with those of Comparative Example 3, and the flowback rate is improved by 98%. The above results show that in the fracturing fluid provided by the present invention, the ammonium chloride, sodium nitrite and flow enhancer in the flowback promoter have a synergistic effect in reducing the amount of thickener adsorption of the fracturing fluid, reducing the starting pressure of the fracturing fluid flowback, reducing the matrix permeability damage rate and improving the flowback rate, which can not only improve the flowback capacity of the fracturing fluid, but also further reduce the solid phase damage of the fracturing fluid. It is a fracturing fluid that can overcome the adsorption and retention problem of the polymer thickener and reduce the liquid flow resistance, and has lower damage to low-permeability reservoirs. In addition, the preparation method of the fracturing fluid provided by the present invention is simple, does not change the existing construction process, and is of great significance to reducing reservoir damage and improving oil and gas production efficiency.

[0186] Although the present invention has been described with reference to specific embodiments, it will be appreciated by those skilled in the art that various changes may be made without departing from the true spirit and scope of the present invention. In addition, the subject matter, spirit and scope of the present invention may be varied to accommodate specific situations, materials, material combinations and methods. All of these changes are included within the scope of the claims of the present invention.

Claims

1. A fracturing fluid comprising a flowback promoter, a polymer thickener, a clay stabilizer, a drainage aid and water.

2. The fracturing fluid according to claim 1, characterized in that: Taking the mass of the water as 100%, the mass concentration of the flowback promoter is 12.4wt% to 18.7wt%, the mass concentration of the polymer thickener is 0.01wt% to 0.75wt%, the mass concentration of the clay stabilizer is 0.1wt% to 1wt%, and the mass concentration of the drainage aid is 0.1wt% to 1wt%.

3. The fracturing fluid according to claim 1 or 2, characterized in that: The flowback promoter includes ammonium chloride, sodium nitrite and a flow enhancer.

4. The fracturing fluid according to claim 3, characterized in that: Taking the mass of the flowback promoter as 100%, the flowback promoter includes 42.8 wt % to 43 wt % of ammonium chloride, 55.2 wt % to 55.5 wt % of sodium nitrite and 1.6 wt % to 2 wt % of the flow enhancer.

5. The fracturing fluid according to claim 3 or 4, characterized in that: The flow enhancer is a chemically loaded product of a compound shown in Formula I on nano-silicon dioxide; wherein A is a naphthalene ring optionally substituted at a position; n is an integer from 1 to 10; n Rs are independently selected from a chemical single bond and C1 to C 10 n X are independently selected from -O- or -NH-, and at least one X is -NH-.

6. The fracturing fluid according to claim 5, characterized in that: The average particle size of the nano-silicon dioxide is 1 nm to 50 nm; Preferably, the nano-silica is hydroxylated-modified silica.

7. The fracturing fluid according to claim 5 or 6, characterized in that: In Formula I, n is an integer from 2 to 6; and / or The n Rs are independently selected from one of a chemical single bond and a C1 to C4 alkylene group.

8. The fracturing fluid according to any one of claims 5 to 7, characterized in that: The compound is hydroxyaminonaphthalene; Preferably, the compound is 2,3-dihydroxy-1-methylaminonaphthalene.

9. The fracturing fluid according to any one of claims 1 to 8, characterized in that The clay stabilizer is an alkyl ammonium salt; Preferably, the alkylammonium salt is hexadecyltrimethylammonium chloride; and / or The polymer thickener is selected from polyacrylamide and / or acrylamide copolymer; and / or The drainage aid is polyoxyethylene ether; Preferably, the weight average molecular weight of the polymer thickener is not less than 10 million; Preferably, the polymer thickener is polyacrylamide.

10. Use of the fracturing fluid according to any one of claims 1 to 9 in fracturing reconstruction of low permeability tight oil and gas reservoirs; Preferably, the low-permeability tight sandstone oil and gas reservoir is an oil and gas reservoir with a geopressure coefficient lower than 1 and an average permeability lower than 0.1 mD.

Citation Information

Patent Citations

  • Slickwater fracturing fluid suitable for being used at hypersalinity condition

    CN108559477A

  • Adsorption inhibitor, and preparation method and application thereof

    CN113322057A

  • Inorganic composite gel system

    CN113372899A

  • High-temperature-resistant chemical wall fixing agent for drilling fluid for stabilizing gravel layer well wall as well as preparation method and application of high-temperature-resistant chemical wall fixing agent

    CN114591718A