Moisture-absorption quick-dry comfortable polyamide fabric, spinning melt and preparation method of spinning melt
By adding silk fibroin and polyvinylpyrrolidone to the nylon yarn and using a specific spinning process to form a cross-shaped or non-circular cross-section, the problem of poor moisture absorption and quick drying of nylon fiber fabrics is solved, significantly reducing the sultry feeling and improving the Comfortable.
Patent Information
- Application Number
- CN202411385271.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-30
- Publication Date
- 2024-12-03
AI Technical Summary
Nylon fiber fabrics have poor moisture absorption and quick drying properties when sweating during exercise, resulting in the fabric being easily sticky and unable to keep the body dry, causing a stuffy feeling.
Use moisture-absorbing and quick-drying comfort polyamide fabric woven from nylon yarn and spandex yarn. The nylon yarn components include 1% to 8% silk fibroin and 0.9% to 6% polyvinylpyrrolidone, and pass specific Methods for preparing spinning melts include heating melt plasticization, water-cooled pelletization and vacuum drying to form nylon fibers with cross-shaped or non-circular cross-sections to improve the moisture absorption and moisture conduction properties of the fabric.
It significantly improves the moisture absorption and moisture conduction properties of the fabric, reduces the stuffy feeling when wearing, improves comfort, and improves the quality and stability of the fibers through dispersants.
Smart Images

Figure CN119061556A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of fabrics, and in particular to a moisture-absorbing, quick-drying, comfortable polyamide fabric, a spinning melt, and a method for preparing the spinning melt. Background Art
[0002] The moisture absorption and perspiration wicking performance of fibers plays a vital role in textiles, which is directly related to the comfort of wearing and the functionality of products. Since nylon fibers have a natural cool feeling and a relatively low modulus, fabrics made from them are soft and elastic. However, since the moisture regain of nylon fibers is as high as 4.5%, sweat will be locked in the inner layer of the fibers, resulting in poor moisture absorption and quick-drying properties of nylon fibers. Therefore, when wearing fabrics made of nylon fibers during exercise and sweating, the fabrics are easy to stick to the body, cannot keep the body dry, and are easy to feel stuffy when worn. Summary of the invention
[0003] The purpose of the present application is to provide a moisture-absorbing quick-drying comfortable polyamide fabric, a spinning melt, and a method for preparing the spinning melt, which are helpful in reducing the feeling of stuffiness when wearing.
[0004] In order to achieve the above purpose, the following technical solutions are adopted:
[0005] The first technical solution relates to a moisture-absorbing quick-drying comfortable polyamide fabric, which is woven from nylon yarn and spandex yarn. The composition of the nylon yarn includes 1% to 8% silk fibroin and 0.9% to 6% polyvinyl pyrrolidone by mass percentage.
[0006] The second technical solution is based on the first technical solution, wherein the composition of the nylon yarn further includes 0.1% to 0.8% of a dispersant by mass percentage.
[0007] The third technical solution is based on the second technical solution, wherein the molecular weight of the silk fibroin is 5000-10000, the K value of the polyvinyl pyrrolidone is 20-60, and the dispersant is a polyether ester polymer and / or an amide polymer.
[0008] The fourth technical solution is based on the third technical solution, wherein the nylon yarn and the spandex yarn are 40D and 20D respectively.
[0009] The fifth technical solution is based on the fourth technical solution, wherein the nylon yarn is made of nylon fiber, and the cross-section of the nylon fiber is circular or non-circular.
[0010] The sixth technical solution is based on the fifth technical solution, wherein the cross-section of the nylon fiber is cross-shaped, octagonal, or I-shaped.
[0011] The seventh technical solution relates to a spinning melt for preparing nylon fibers, which are used to spin nylon yarns, and the nylon yarns are used to manufacture the moisture-absorbing, quick-drying, comfortable polyamide fabrics as described in claims 1 to 4, characterized in that the composition of the spinning melt includes 1% to 8% of silk fibroin and 0.9% to 6% of polyvinyl pyrrolidone by mass percentage.
[0012] The eighth technical scheme relates to a method for preparing a spinning melt, which is used to prepare the spinning melt as described in the seventh technical scheme, and is characterized in that it includes the following steps: S1: in percentage, 68% to 80% polyamide 6, 10% to 20% silk fibroin, 9% to 15% polyvinyl pyrrolidone and 1% to 2% dispersant are mixed and heated to 220 to 260°C for melt plasticization, and then sequentially subjected to water cooling and pelletizing, and vacuum drying steps to obtain hygroscopic masterbatch; S2: the dried polyamide 6 and hygroscopic masterbatch are fed into a screw extruder, heated to 230 to 280°C, and then melt-extruded to obtain a spinning melt, in percentage, the proportion of polyamide 6 is 60%-90%, and the proportion of hygroscopic masterbatch is 10%-40%.
[0013] The ninth technical solution is based on the eighth technical solution, wherein the relative viscosity of the polyamide 6 is 2.5 to 2.8.
[0014] The tenth technical solution is based on the ninth technical solution, wherein the preparation method of the hygroscopic masterbatch is as follows: first preheat the high-speed mixer to 220-260°C, and then divide the polyamide 6 into two equal parts, first add one part of polyamide 6 to the high-speed mixer, then add all the silk fibroin and all the polyvinyl pyrrolidone, and finally add the other part of polyamide 6.
[0015] Compared with the prior art, the above solution has the following beneficial effects:
[0016] In the first technical solution, the moisture-absorbing, quick-drying and comfortable polyamide fabric is woven from nylon yarn and spandex yarn. The composition of the nylon yarn includes 1% to 8% silk fibroin and 0.9% to 6% polyvinyl pyrrolidone by mass. Silk fibroin and polyvinyl pyrrolidone have good hygroscopicity. Compared with the nylon yarn without silk fibroin and polyvinyl pyrrolidone, the nylon yarn with silk fibroin and polyvinyl pyrrolidone added has stronger water absorption, which is beneficial to reduce the stuffiness when worn.
[0017] In the second technical solution, the composition of the nylon yarn also includes 0.1% to 0.8% of a dispersant by mass, and the dispersant improves the quality and stability of the nylon fiber during the preparation process.
[0018] In the third technical solution, the molecular weight of silk fibroin is 5000-10000, and the K value of polyvinyl pyrrolidone is 20-60. When the molecular weight of silk fibroin is lower than 5000-10000 and the K value of polyvinyl pyrrolidone is lower than 20-60, the cross-shaped cross-section of the nylon fiber is distorted and not three-dimensional, and yellowing and hairiness occur, and the fabric turns yellow.
[0019] In the third technical solution, when the molecular weight of silk fibroin is higher than 5000-10000 and the K value of polyvinyl pyrrolidone is higher than 20-60, the nylon fiber has poor forming performance and poor quality. There are undesirable phenomena such as broken yarn and strong strength during spinning, and the yarn is seriously broken during fabric weaving.
[0020] In the fifth technical solution, the cross section of the nylon yarn is circular, and the nylon yarn with a circular cross section is easier to manufacture and has a simple process.
[0021] In the fifth technical solution, the cross-section of the nylon yarn is non-circular. Compared with the circular cross-section, the non-circular specific surface area is larger than the circular specific surface area, the moisture conduction efficiency is higher, the quick-drying effect is better, and it is beneficial to reduce the feeling of stuffiness when wearing.
[0022] In the sixth technical solution, the cross-section of the nylon fiber is cross-shaped, octagonal and I-shaped. Compared with the circular shape, the cross-shaped, octagonal and I-shaped shapes not only have a larger surface area, but also improve their capillary effect and air permeability, have higher moisture conduction efficiency, and better quick-drying effect, which is conducive to reducing the feeling of stuffiness when wearing.
[0023] In the eighth technical solution, a hygroscopic masterbatch is first prepared, and then the dried polyamide 6 and the hygroscopic masterbatch are sent to a screw extruder and heated to obtain a spinning melt, in order to better mix the polyamide 6, silk fibroin, polyvinyl pyrrolidone and the dispersant.
[0024] In the tenth technical solution, polyamide 6 is divided into two parts in order to better mix polyamide 6, silk fibroin, polyvinyl pyrrolidone and dispersant. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] In order to more clearly illustrate the technical solution of the embodiment, the following briefly introduces the drawings required for use:
[0026] Figure 1 This is a schematic diagram of a cross-section of a nylon fiber in Example 1;
[0027] Figure 2 It is a schematic diagram of the cross-section of the nylon fiber in Example 2.
[0028] Description of main reference numerals:
[0029] 1. The first cross-shaped section; 2. The second cross-shaped section. DETAILED DESCRIPTION
[0030] In the claims and the description, unless otherwise defined, the terms "first", "second" or "third", etc. are intended to distinguish different objects rather than to describe a specific order.
[0031] In the claims and the specification, unless otherwise defined, terms such as "center", "lateral", "longitudinal", "horizontal", "vertical", "top", "bottom", "inside", "outside", "up", "down", "front", "back", "left", "right", "clockwise", "counterclockwise" and the like indicating directions or positional relationships are based on the directions and positional relationships shown in the drawings and are only for the convenience of simplifying the description and do not imply that the device or element referred to must have a specific direction or be constructed and operated in a specific direction.
[0032] In the claims and the specification, unless otherwise defined, the term "fixed connection" or "fixed connection" should be understood in a broad sense, that is, any connection method in which there is no displacement relationship and relative rotation relationship between the two parties, that is to say, including non-detachable fixed connection, detachable fixed connection, integral connection and fixed connection through other devices or elements.
[0033] In the claims and the description, unless otherwise defined, the terms "includes", "has" and their variations mean "including but not limited to".
[0034] In the claims and the specification, unless otherwise defined, the term "provided with" means that the technical feature located thereafter is a part of the technical feature located therefor.
[0035] The technical solutions in the embodiments will be described clearly and completely below in conjunction with the accompanying drawings.
[0036] Embodiment 1
[0037] This embodiment provides a moisture-absorbing, quick-drying, comfortable polyamide fabric, which is woven from nylon yarn and sprocket yarn, wherein the nylon yarn is made of nylon fiber, see Figure 1 , Figure 1 The cross section of the nylon fiber in this embodiment is shown. In this embodiment, the cross section of the nylon fiber is cross-shaped, and in other embodiments, the cross section of the nylon fiber can also be circular, octagonal, and I-shaped. In this embodiment, the components of the nylon yarn include fibroin and polyvinyl pyrrolidone. Fibroin and polyvinyl pyrrolidone are water-absorbent, and the fabric woven from the nylon yarn is more moisture-absorbent and quick-drying than ordinary nylon fabrics, which is conducive to reducing the stuffiness when wearing and improving the comfort when wearing.
[0038] The preparation of the moisture-absorbing quick-drying comfortable polyamide fabric in this embodiment requires the preparation of a moisture-absorbing masterbatch, which includes, by mass percentage, 70% polyamide 6, 15% silk fibroin, 13% polyvinyl pyrrolidone, and 2% dispersant. The relative viscosity of spinning-grade polyamide 6 is 2.5; the relative molecular weight of silk fibroin is 6000; the K value of polyvinyl pyrrolidone is 30; the dispersant is a polyether ester polymer;
[0039] The preparation method of hygroscopic masterbatch is as follows:
[0040] Step 1: Preheat the high-speed mixer. Adjust the temperature of the high-speed mixer to 240°C.
[0041] Step 2: Melt mixing. Divide the polyamide 6 into two equal parts, add the first part of the polyamide 6 into the high-speed mixer, then add all the silk fibroin and polyvinyl pyrrolidone, and finally add the remaining polyamide 6.
[0042] Step 3: Water-cooling pelletizing: The melted and plasticized product mixed in the high-speed mixer is water-cooled and pelletized.
[0043] Step 4: vacuum drying: The product treated in step 3 is vacuum dried to obtain a hygroscopic masterbatch.
[0044] After the hygroscopic masterbatch is prepared, the nylon fiber can be prepared.
[0045] The preparation method of nylon fiber is as follows:
[0046] Step 1: Preheat the screw extruder. Adjust the temperature of the screw extruder to 260°C.
[0047] Step 2: Preparation of spinning melt: The dried polyamide 6 and the hygroscopic masterbatch are fed into a screw extruder for melt extrusion, wherein the ratio of the silk fibroin and polyvinyl pyrrolidone mixture is 7 wt%.
[0048] Step 3: Preparation of nylon fiber. The spinning melt obtained in the second step is metered by a metering pump and sent to the composite spinning box, passed through the composite spinning assembly, and finally spun using a special-shaped spinneret to adjust the shape of the fiber. The spinning temperature is 260°C, the spinning speed is 1600m / min, the draft ratio is 3.5, the stretching temperature is 130°C, and the cold air temperature is 22°C.
[0049] The cross section of the nylon fiber obtained in this embodiment is cross-shaped, as shown in the figure, and the first cross-shaped cross section 1 can be seen. The specific surface area of the cross-shaped cross section 1 is larger than that of the circular cross section, and the air permeability and capillary effect are also greater, so that its moisture conduction efficiency is higher and the quick-drying effect is also stronger.
[0050] After the nylon fiber is prepared, the moisture-absorbing quick-drying comfortable polyamide fabric can be prepared. The preparation method of the moisture-absorbing quick-drying comfortable polyamide fabric is as follows: the nylon fiber is made into 40D nylon yarn, and then it is woven, dyed and formed with 20D spandex to obtain the moisture-absorbing quick-drying comfortable polyamide fabric.
[0051] The moisture-absorbing, quick-drying and comfortable polyamide fabric in this embodiment uses nylon fibers with a cross-shaped cross-section 1, so its specific surface area is larger than that of a circular cross-section, and its air permeability and capillary effect are also greater, making it more efficient in moisture conduction and more quick-drying, thereby reducing the feeling of stuffiness when worn. In addition, the nylon fabric itself has the characteristic of a cool feeling, which further improves comfort.
[0052] In this embodiment, the moisture-absorbing, quick-drying and comfortable polyamide fabric is woven from nylon yarn and spandex yarn. The components of the nylon yarn are silk fibroin and polyvinyl pyrrolidone. Silk fibroin and polyvinyl pyrrolidone have good hygroscopicity. Compared with the nylon yarn without silk fibroin and polyvinyl pyrrolidone, the nylon yarn with silk fibroin and polyvinyl pyrrolidone added has stronger water absorption, which is beneficial to reduce the feeling of stuffiness when worn.
[0053] In this embodiment, the components of the nylon yarn also include a dispersant, which improves the quality and stability of the nylon fiber during the preparation process.
[0054] In this embodiment, the cross-section of the nylon fiber is cross-shaped, which not only has a larger surface area than a circle, but also improves its capillary effect and air permeability, has a higher moisture conduction efficiency, and has a better quick-drying effect, which is beneficial to reducing the feeling of stuffiness when worn.
[0055] In this embodiment, the hygroscopic masterbatch is first prepared, and then the dried polyamide 6 and the hygroscopic masterbatch are sent to a screw extruder for heating to obtain a spinning melt, in order to better mix the polyamide 6, silk fibroin, polyvinyl pyrrolidone and the dispersant.
[0056] In this embodiment, polyamide 6 is divided into two parts in order to better mix polyamide 6, silk fibroin, polyvinyl pyrrolidone and dispersant.
[0057] Embodiment 2
[0058] The composition of the moisture-absorbing quick-drying comfortable polyamide fabric of this embodiment is substantially the same as that of the first embodiment, except that the relative molecular weight of the silk fibroin is 4000, and the K value of the polyvinyl pyrrolidone is 10.
[0059] The method of making the moisture absorbing and quick-drying comfortable polyamide fabric in this embodiment is exactly the same as that in the first embodiment.
[0060] Figure 2 FIG. 4 shows a cross section of the nylon fiber in this embodiment. Figure 2As shown, compared with the first cross-shaped cross-section 1, the second cross-shaped cross-section 2 is distorted and not three-dimensional, and has yellowing, fuzziness, etc., and the fabric has yellowing.
[0061] Embodiment 3
[0062] The composition of the moisture-absorbing, quick-drying and comfortable polyamide fabric of this embodiment is substantially the same as that of the first embodiment, except that the relative molecular weight of the silk fibroin is 12,000, and the K value of the polyvinyl pyrrolidone is 80.
[0063] The method of making the moisture absorbing and quick-drying comfortable polyamide fabric in this embodiment is exactly the same as that in the first embodiment.
[0064] In this embodiment, the nylon fiber has poor forming performance and very poor quality. There are undesirable phenomena such as broken yarns and strong strength during spinning, and serious yarn breakage during fabric weaving.
[0065] As shown in Table 1, the fabrics obtained in Example 1, Example 2, and Example 3 were compared with blank sample 1 (comparison with ordinary nylon-ammonia fabric) according to the amino acid content test method: breaking strength test method: GB / T 14344-2022 "Test method for tensile properties of chemical fiber filaments", FZ / T 50049-2020 "Test method for amino acid content of chemical fibers", coolness test: GB / T35263-2017 "Detection and evaluation of instantaneous coolness of textiles at contact", drying rate test: GB / T 21655.1-2023 "Evaluation of moisture absorption and quick-drying properties of textiles" and moisture resistance: GB / T 11048-2018 "Determination of thermal resistance and moisture resistance of textiles under steady-state conditions of physiological comfort (evaporative hot plate method) and were compared.
[0066] Table 1 Comparison of test results of fabrics obtained in Example 1, Example 2 and Example 3
[0067]
[0068] Table 2 Comparison of test results of Example 1 and Blank Sample 1
[0069]
[0070] The above specification and description of the embodiments are used to explain the protection scope of the present application, but do not constitute a limitation on the protection scope of the present application.
Claims
1. A moisture-absorbing, quick-drying, comfortable polyamide fabric, characterized in that: The moisture-absorbing quick-drying comfortable polyamide fabric is woven from nylon yarn and spandex yarn. The nylon yarn comprises 1% to 8% of silk fibroin and 0.9% to 6% of polyvinyl pyrrolidone by mass percentage.
2. The moisture-absorbing, quick-drying, comfortable polyamide fabric according to claim 1, characterized in that: The composition of the nylon yarn also includes 0.1% to 0.8% of a dispersant by mass percentage.
3. The moisture-absorbing, quick-drying, comfortable polyamide fabric according to claim 2, characterized in that: The molecular weight of the silk fibroin is 5000-10000, the K value of the polyvinyl pyrrolidone is 20-60, and the dispersant is a polyether ester macromolecular polymer and / or an amide macromolecular polymer.
4. The moisture-absorbing, quick-drying, comfortable polyamide fabric according to claim 3, characterized in that: The nylon yarn and the spandex yarn are 40D and 20D respectively.
5. The moisture-absorbing, quick-drying, comfortable polyamide fabric according to claim 4, characterized in that: The nylon yarn is made of nylon fiber, and the cross section of the nylon fiber is circular or non-circular.
6. The moisture-absorbing quick-drying comfortable polyamide fabric according to claim 5, characterized in that: The cross section of the nylon fiber is cross-shaped, octagonal or I-shaped.
7. A spinning melt for preparing nylon fiber, characterized in that: The nylon fiber is used to spin into nylon yarn, and the nylon yarn is used to manufacture the moisture-absorbing, quick-drying, comfortable polyamide fabric as described in claims 1 to 4, characterized in that the composition of the spinning melt includes 1% to 8% silk fibroin and 0.9% to 6% polyvinyl pyrrolidone by mass percentage.
8. A method for preparing a spinning melt, for preparing the spinning melt as claimed in claim 7, characterized in that: The steps include: S1: In percentage, 68% to 80% polyamide 6, 10% to 20% silk fibroin, 9% to 15% polyvinyl pyrrolidone and 1% to 2% dispersant are mixed and heated to 220 to 260° C. for melt plasticization, and then water-cooled pelletizing and vacuum drying are performed in sequence to obtain a hygroscopic masterbatch; S2: The dried polyamide 6 and hygroscopic masterbatch are fed into a screw extruder, heated to 230-280°C, and then melt-extruded to obtain a spinning melt. In percentage, the proportion of the polyamide 6 is 60%-90%, and the proportion of the hygroscopic masterbatch is 10%-40%.
9. A method for preparing a spinning melt according to claim 8, characterized in that: The relative viscosity of the polyamide 6 is 2.5-2.
8.
10. A method for preparing a spinning melt according to claim 9, characterized in that: The preparation method of the hygroscopic masterbatch is as follows: first preheat the high-speed mixer to 220-260° C., then divide the polyamide 6 into two equal parts, first add one part of the polyamide 6 to the high-speed mixer, then add all the silk fibroin and all the polyvinyl pyrrolidone, and finally add the other part of the polyamide 6.
Citation Information
Patent Citations
Silk fibroin and polybutylene terephthalate blended fiber and preparation method thereof
CN104790062A
Modified chemical fiber using natural protein fiber superfine powder and production process thereof
CN1594682A
Highly hygroscopic polyamide fiber and its production
JP1997188917A
Moisture-absorbing polyamide fiber and method of melt spinning thereof
JP2004225190A
Cited By
Moisture-absorbing and quick-drying polypropylene fiber with gradient structure and preparation method of moisture-absorbing and quick-drying polypropylene fiber
CN120026401A
A moisture-absorbing and quick-drying polypropylene fiber with a gradient structure and its preparation method
CN120026401B