Preparation method and application of fuzzing agent containing low aromatic hydrocarbon compound
By emulsifying and preparing with low aromatic compounds, the existing pursing agents have solved the damage and environmental protection of textile fibers and achieved efficient and environmentally friendly pursing agent production, suitable for a variety of textile materials, improving processing convenience and Environmentally friendly performance.
Patent Information
- Application Number
- CN202411316554.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-20
- Publication Date
- 2024-12-03
AI Technical Summary
The existing pursing agents are dimethyl silicone oil as the main raw material, which causes damage to textile fibers, is not hydrophilic and has low production efficiency, and is small in scope of application, which cannot meet the requirements of blue label environmental protection.
Use low aromatic compounds to be used as raw materials, emulsified by emulsifier, combined with precise control of water addition and stirring time, to prepare low aromatic compounds chromic agents, adapt to different textile materials, reduce fiber damage and improve processing convenience and reliability sex.
It improves the affinity and scope of application of purses to various textiles, meets environmental protection standards, simplifies production processes, improves production efficiency, and reduces potential impact on the environment.
Smart Images

Figure CN119061680A_ABST
Abstract
Description
Technical Field
[0001] The invention mainly relates to the field of textile technology, and in particular to a preparation method of a raising agent containing low aromatic compounds and application thereof. Background Art
[0002] Raising agent is one of the commonly used softeners in textile processing. By softening textiles with raising agents, the feel and skin-friendly effect of the finished textiles can be improved.
[0003] Existing raising agents generally use dimethyl silicone oil as the main raw material, and need to be emulsified with an emulsifier to achieve the requirement of soft textiles. Since the raw materials of the raising agent contain silicon, it does not meet the blue label environmental protection requirements and is easy to damage the fibers of textiles. In addition, the silicon-containing raising agent is not hydrophilic to cotton, and the emulsification operation technology requirements are high, resulting in low production efficiency of the raising agent and a small scope of application. Summary of the invention
[0004] The purpose of the present invention is to overcome the shortcomings of the prior art. The present invention provides a method for preparing a raising agent containing low aromatic compounds and an application thereof. By using a raising oil containing low aromatic compounds as a raw material, a raising agent containing low aromatic compounds is prepared, so that the raising agent can be adapted to textiles of different materials, reducing the damage of the raising agent to textile fibers, and at the same time improving the convenience and reliability of the raising agent in the processing and application of textiles.
[0005] The present invention provides a method for preparing a raising agent containing low aromatic compounds, the preparation method comprising:
[0006] Add the hair oil containing low aromatic compounds into the emulsification barrel, start the emulsifier, and make the emulsifier rotate at a preset speed;
[0007] Add water into the emulsification tank at preset time intervals, and continue stirring for a preset time after each water addition;
[0008] Record the amount of water added each time, calculate the total amount of water added, and check whether the total amount of water added reaches the standard value;
[0009] When the total amount of water added reaches the standard value, a bactericide is added into the emulsification barrel, and the raising agent is obtained by filtering after stirring.
[0010] Specifically, the raising agent is prepared by mixing raising oil, fungicide and water, wherein the raising oil accounts for 60% of the total raising agent, the fungicide accounts for 0.2% of the total raising agent, and the water accounts for 39.8% of the total raising agent.
[0011] Further, the step of adding the hair oil into the emulsifying barrel and starting the emulsifying machine so that the emulsifying machine rotates at a preset speed includes:
[0012] The rotation speed of the emulsifier is set to 2000 r / min, and the hair raising oil is rotated at room temperature.
[0013] Specifically, the step of injecting water into the emulsifying tank at a preset time interval and continuously stirring for a preset time after each injection includes:
[0014] Set the water injection volume range for each injection to: 20kg~30kg;
[0015] The preset duration is set to a value range of 3 minutes to 5 minutes.
[0016] Set the preset time interval to 6 minutes.
[0017] Specifically, recording the amount of water added each time the water is injected, calculating the total amount of water added, and detecting whether the total amount of water added reaches the standard value includes:
[0018] The standard value is set to A, the total amount of water involved in the preparation process of the raising agent is B, and the constraint relationship between A and B is: 35%*B≤A≤38%*B.
[0019] The present invention also provides a raising agent, which is prepared based on the method for preparing the raising agent containing low aromatic hydrocarbon compounds.
[0020] The present invention also provides a textile, wherein the textile is treated with the raising agent, and after the textile is dyed, the textile is softened based on the raising agent.
[0021] Furthermore, the material of the textile is one of polyester, polyester-cotton, pure cotton, nylon, and acrylic.
[0022] Further, when the textile is made of polyester or polyester-cotton, the amount of the raising agent used is 1 to 1.5% OWf;
[0023] When the material of the textile is nylon, the amount of the raising agent used is 1.5-5% OWf;
[0024] When the textile is made of pure cotton, the amount of the raising agent used is 3-5% OWf;
[0025] When the textile is made of acrylic fiber, the amount of the raising agent used is 1-3% OWf.
[0026] The present invention mainly relates to a method for preparing a raising agent containing low aromatic compounds and an application thereof. A raising agent containing low aromatic compounds is prepared by taking a raising oil containing low aromatic compounds as a raw material, so that the raising agent can be adapted to textiles of different materials, thereby reducing the damage of the raising agent to textile fibers and improving the convenience and reliability of the raising agent in the processing and application of textiles. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 is a flow chart of a method for preparing a raising agent containing low aromatic compounds in an embodiment of the present invention;
[0028] Figure 2 It is a structural schematic diagram of an emulsifying machine in an embodiment of the present invention. DETAILED DESCRIPTION
[0029] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0030] Embodiment 1:
[0031] Figure 1 The flowchart of the method for preparing a raising agent containing low aromatic compounds in an embodiment of the present invention is shown, and the specific steps are as follows:
[0032] S101: Add the hair oil containing low aromatic compounds into the emulsification barrel, and start the emulsifier to rotate at a preset speed.
[0033] S102: Filling water into the emulsification barrel at preset time intervals, and continuously stirring for a preset time after each water filling.
[0034] S103: Record the amount of water added each time, calculate the total amount of water added, and check whether the total amount of water added reaches the standard value.
[0035] S104: When the total amount of water added reaches the standard value, add the bactericide into the emulsification barrel, and obtain the raising agent by filtering after stirring.
[0036] During the specific implementation, each step was optimized. As for the speed of the emulsifier, after many experiments, it was determined that a speed of about 2000r / min can achieve the best emulsification effect. The speed setting of 2000r / min can provide sufficient shear force to fully disperse the hair oil in the water to form a stable emulsion. The selection of normal temperature conditions can reduce energy consumption and simplify the operation process.
[0037] Taking the production of 1000kg of raising agent as an example, in the step-by-step water addition process, the water injection amount is controlled between 20kg and 30kg each time, and the stirring time after each water injection is set between 3 minutes and 5 minutes. The water injection interval is determined to be about 6 minutes. The total amount of water added is controlled between 35% and 38% of the total amount of raising agent to obtain the best emulsification effect and product performance.
[0038] Specifically, Figure 2 The schematic diagram of the structure of the emulsifier in the embodiment of the present invention is shown, the emulsifier includes an emulsifying barrel 1 and a plurality of driving motors 2, the emulsifying barrel 1 is provided with an agitator 3 and a wall scraper 4, one of the plurality of driving motors 2 is connected to the wall scraper 4, and can scrape off the residue in the barrel wall of the emulsifying barrel 1, reducing the risk of the raw materials of the raising agent sticking to the wall. The emulsifying barrel 1 is provided with a plurality of agitators 3, based on a one-to-one correspondence of a plurality of driving motors 2 to drive a plurality of agitators 3, to meet the stirring and emulsifying operation requirements of the raising agent.
[0039] Furthermore, the emulsification barrel 1 can be made of stainless steel to meet the stirring and emulsification operation requirements of the raising agent.
[0040] In one embodiment, first, 100kg of fluffing oil containing low aromatic compounds is added into a stainless steel emulsifying barrel with a capacity of 200L. Start the emulsifying machine, set the rotating speed to 2000r / min, and stir the fluffing oil at room temperature. According to the preset 6-minute time interval, water is injected into the emulsifying barrel, and each water injection amount is controlled to be about 25kg, and stirring is continued for 4 minutes after water injection. Use an electronic scale to accurately record the amount of water added for each water injection, and calculate the total amount of water added in real time through the control system. When the total amount of water added reaches 66kg, stop water injection. Finally, 0.33kg of bactericide is added into the emulsifying barrel, and stirring is continued for 5 minutes, and then filtered through a 100-mesh filter to obtain a final fluffing agent product. The whole preparation process takes about 90 minutes.
[0041] In another embodiment, 200 kg of low aromatic compound-containing fluffing oil is used, and an emulsifying barrel with a capacity of 500 L is used. The speed of the emulsifying machine is set to 1800 r / min. The water injection amount is 30 kg each time, the water injection interval is 7 minutes, and stirring is performed for 5 minutes after each water injection. When the total amount of water added reaches 132 kg, the water injection is stopped. Finally, 0.66 kg of bactericide is added, and after stirring for 6 minutes, it is filtered through an 80-mesh filter. The whole process takes about 120 minutes.
[0042] The preparation method of the embodiment of the present invention has significant advantages over the traditional method. The use of low aromatic compounds as the main raw materials avoids the potential damage of dimethyl silicone oil to textile fibers and meets strict environmental protection requirements. The step-by-step water addition and continuous stirring method significantly improves the emulsification effect, does not require the addition of additional emulsifiers, and simplifies the production process. The consistency of product quality is ensured by accurately controlling the amount of water added and the stirring time.
[0043] Compared with the traditional method, the preparation method of the embodiment of the present invention improves the production efficiency of the raising agent by about 30%. Since it does not contain silicon, the prepared raising agent has good affinity to various textile materials and its application range is expanded by about 50%. At the same time, since low aromatic compounds are used, the product fully meets the latest environmental protection standards and reduces the potential impact on the environment.
[0044] Embodiment 2:
[0045] In this embodiment, the specific ratio of each component in the raising agent is clarified. The raising agent is prepared by mixing raising oil, fungicide and water, wherein the raising oil accounts for 60% of the total raising agent, the fungicide accounts for 0.2% of the total raising agent, and the water accounts for 39.8% of the total raising agent.
[0046] As the main component, the raising oil accounts for 60%, which can provide a good raising effect. The bactericide accounts for 0.2%, which is a small proportion but can effectively prevent the growth of microorganisms. Water accounts for 39.8%, which is a solvent and dispersion medium, and helps to evenly distribute other ingredients. This ratio design can achieve the antiseptic effect through a small amount of bactericide while ensuring the raising effect, and use an appropriate amount of water to achieve full mixing and dispersion of each component. By accurately controlling the proportion of each component, a raising agent with stable performance, good raising effect and certain antiseptic properties can be obtained. This formula design is conducive to improving the overall performance and use effect of the raising agent.
[0047] In specific implementation, the proportion of the raising oil can be adjusted within the range of 55%-65% to meet the needs of different types of textiles. For example, for coarse fiber fabrics that require a stronger raising effect, the proportion of the raising oil can be increased to 63%-65%. The proportion of the fungicide can be fine-tuned between 0.1%-0.3%, depending on the needs of different seasons and storage environments.
[0048] Specifically, in combination with the preset rotation speed and water injection interval of the emulsifier, it can ensure that each component is fully emulsified during the mixing process to form a stable emulsion state, which not only improves the uniformity of the raising agent, but also enhances its adhesion and permeability on the surface of the textile.
[0049] The preparation method proposed in the embodiment of the present invention solves the problem of how to determine the proportion of each component in the raising agent containing low aromatic compounds to obtain a raising agent with excellent performance by accurately controlling the proportion of each component. The raising oil as the main component, accounting for 60%, ensures good raising effect and softness. The 0.2% bactericide can effectively inhibit the growth of microorganisms while avoiding the interference of the bactericide on the effect of the raising oil. 39.8% of water as a solvent and dispersion medium not only helps the uniform distribution of other components, but also ensures that the raising agent has appropriate fluidity and operability.
[0050] The working principle of this ratio design is that the raising oil provides the main raising and softening functions, water as a medium helps the raising oil to be evenly dispersed to form a stable emulsion state, and the fungicide plays a role in preserving and preserving in the entire system. Through this precise ratio control, the raising agent of the embodiment of the present invention can have excellent stability and antiseptic properties while ensuring a good raising effect.
[0051] Compared with the raising agent with dimethyl silicone oil as the main raw material in the background technology, the technical solution of the embodiment of the present invention has significant advantages. First, the raising oil containing low aromatic compounds is used to replace dimethyl silicone oil, which meets environmental protection requirements and reduces the potential damage to textile fibers. Secondly, the formula of the embodiment of the present invention does not require additional emulsifiers, simplifies the production process, and improves production efficiency. Finally, by accurately controlling the moisture content, the raising agent of the embodiment of the present invention has good affinity for various textiles and expands the scope of application.
[0052] Specifically, add 600 kg of low aromatic compound-containing hair oil into a 2000 L emulsification barrel, start the emulsifier, and set the speed to 2000 r / min. Start stirring at room temperature (about 25°C). Inject 25 kg of water into the emulsification barrel every 6 minutes, and continue stirring for 4 minutes after each water injection. Repeat this process until the total amount of water added reaches 400 kg. At this time, add 2 kg of fungicide into the emulsification barrel and continue stirring for 10 minutes to ensure sufficient mixing. Finally, filter the mixture through a 100-mesh screen to obtain a finished hair raising agent.
[0053] In practical applications, the raising agent with this ratio shows excellent performance. For example, when treating polyester fabrics, using 1.2% OWf can form uniform and dense fluff on the surface of the fabric, which is soft and smooth to the touch and has good washability. At the same time, due to the presence of the fungicide, the raising agent remains stable and has no odor even after being stored in a high temperature and high humidity environment for 3 months.
[0054] Compared with the prior art, the raising agent of the embodiment of the present invention shows obvious advantages in many aspects. First, in terms of environmental performance, since it does not contain silicon, it fully meets the blue label environmental protection requirements and reduces the potential harm to the environment. Secondly, in terms of production efficiency, since no additional emulsifier and complex emulsification process are required, the production process is greatly simplified and the production efficiency is improved. Thirdly, in terms of scope of application, the raising agent of the embodiment of the present invention shows good affinity for various textile materials, especially the hydrophilicity of cotton fiber is significantly better than that of silicon-containing raising agent, so that it can play a good effect in various textile treatments. Finally, in terms of use effect, the raising agent of the embodiment of the present invention can form a more uniform and dense fluff on the surface of the textile, provide a better feel and appearance, and have better washability and durability. These advantages together constitute the innovation and progress of the embodiment of the present invention in the field of raising agents.
[0055] In this embodiment, adding the fluffing oil into the emulsifying barrel and starting the emulsifying machine so that the emulsifying machine rotates at a preset speed includes: setting the speed of the emulsifying machine to 2000 r / min and rotating the fluffing oil at room temperature.
[0056] This technical solution can effectively achieve the emulsification of the hair oil containing low aromatic compounds by setting the speed of the emulsifier to 2000r / min and rotating the hair oil at room temperature. Specifically, the speed setting of 2000r / min can provide sufficient shear force to fully disperse the hair oil in water to form a stable emulsion. The selection of room temperature conditions can reduce energy consumption and simplify the operation process. These two technical features cooperate with each other, which not only ensures the emulsification effect, but also takes into account production efficiency and cost control.
[0057] In the implementation process of the embodiment of the present invention, the speed of the emulsifier can be adjusted between 1800r / min and 2200r / min to adapt to the different viscosities of the hair oil. Normal temperature conditions usually refer to the ambient temperature range of 15°C to 30°C. This setting can be flexibly applied in different seasons and regions without the need for additional heating or cooling equipment.
[0058] The speed and working conditions of the emulsifier are closely related to the water injection process in the previous step. The high-speed rotation of 2000r / min can quickly disperse water into the fluffing oil during the water injection process to form a preliminary emulsion structure. This high-speed shearing action can break the macromolecular structure of the fluffing oil, making it easier to combine with water molecules. At the same time, operation under normal temperature conditions can avoid problems such as denaturation of the fluffing oil components or rapid evaporation of water due to excessive temperature.
[0059] In practical applications, the following specific steps can be adopted: First, add 100kg of low aromatic compound-containing fluffing oil into a 200L stainless steel emulsifying barrel. Start the emulsifier, adjust the speed to 2000r / min, and preliminarily stir the fluffing oil for 2 minutes at room temperature of 20°C. This step can fully preheat the fluffing oil and evenly distribute it in the emulsifying barrel. Subsequently, water is added and stirred in batches according to the above method until the preset water volume standard is reached. During the whole process, the emulsifier maintains a high-speed operation of 2000r / min to ensure that a uniform emulsion can be quickly formed after each water injection.
[0060] The method of combining high-speed emulsification and normal temperature operation adopted in the embodiment of the present invention has significant advantages over the traditional low-speed emulsification or heating methods. First, the high-speed rotation of 2000r / min provides a strong shear force, which can more effectively disperse the hair oil into tiny droplets to form a stable emulsion structure. This not only improves the emulsification efficiency, but also enhances the stability of the final product. Secondly, the operation under normal temperature conditions greatly simplifies the production process, does not require complex temperature control equipment, and reduces energy consumption and equipment investment. At the same time, the normal temperature operation also avoids the problem of hair oil component denaturation that may be caused by high temperature, ensuring the consistency of product quality.
[0061] The preparation method proposed in this embodiment can complete the emulsification process in a short time through the high-speed emulsification method, thereby improving production efficiency. At the same time, the normal temperature operation reduces energy consumption, simplifies the operation process, and makes the entire production process more environmentally friendly and economical. This method is particularly suitable for the fluffing oil containing low aromatic compounds, and can give full play to its environmental protection characteristics while ensuring good emulsification effect and product performance.
[0062] Specifically, the embodiment of the present invention further proposes a solution of injecting water into the emulsification barrel at a preset time interval, and continuously stirring for a preset time after each water injection. Specifically, it includes: setting the water injection amount range of each water injection to 20kg to 30kg; setting the preset time range to 3min to 5min; setting the preset time interval to 6min.
[0063] This technical solution optimizes the emulsification process of the raising agent by setting specific water injection parameters. The water injection volume is controlled between 20kg and 30kg each time to ensure that the water is evenly dispersed in the raising oil and avoid local over-dilution. Stirring is continued for 3 to 5 minutes after each water injection to give enough time for the water and oil to mix fully. Setting a 6-minute water injection interval allows the previous water injection to be fully emulsified before the next water injection to avoid insufficient emulsification.
[0064] This step-by-step water injection and stirring method can gradually and evenly disperse water into the raising oil to form a stable emulsion. By controlling the amount of water injected each time, the stirring time and the interval between water injections, the emulsification process can be optimized and the uniformity and stability of the raising agent can be improved. Compared with adding all the water at once, this precise control method can achieve a better emulsification effect, thereby preparing a raising agent with better performance.
[0065] In specific implementation, the amount of water injected each time can be adjusted according to the capacity of the emulsification barrel and the amount of hair oil used. For example, for a larger capacity emulsification barrel, you can choose a water injection amount of 25kg to 30kg; for a smaller capacity emulsification barrel, you can choose a water injection amount of 20kg to 25kg. This ensures that the water can be evenly dispersed in production of different scales.
[0066] Furthermore, the stirring time involved in the preparation process can also be fine-tuned according to actual conditions. For example, when the ambient temperature is low, a stirring time of 4 to 5 minutes can be selected to ensure sufficient mixing; when the ambient temperature is high, a stirring time of 3 to 4 minutes can be selected to improve production efficiency.
[0067] In practical applications, the following specific embodiments can be used: First, add 60 kg of fluffing oil containing low aromatic compounds into an emulsification barrel with a capacity of 200 L, start the emulsifier, set the speed to 2000 r / min, and pre-stir the fluffing oil for 5 minutes at room temperature. Then, start the step-by-step water injection process. Inject 25 kg of water each time, stir for 4 minutes, and inject water again after an interval of 6 minutes. Repeat this process until the total amount of water added reaches 39.8 kg. Finally, add 0.2 kg of fungicide, stir for 5 minutes, and filter to obtain a fluffing agent with excellent performance.
[0068] This precisely controlled step-by-step water injection method has significant advantages over the traditional one-time water addition method. The traditional method often leads to local over-dilution or insufficient emulsification, affecting the uniformity and stability of the raising agent. The method of the embodiment of the present invention can achieve uniform dispersion and sufficient emulsification of water by controlling the amount of water injected each time, the stirring time and the interval between water injections. This not only improves the quality of the raising agent, but also enhances its applicability on different textile materials.
[0069] In addition, the method of the embodiment of the present invention also has good controllability and flexibility. By adjusting the water injection parameters, it can adapt to the production needs of different scales and different environmental conditions, thereby optimizing production efficiency and product quality. This method not only solves the problem of emulsification effect, but also provides a more scientific and efficient preparation method for the production of raising agents.
[0070] Specifically, the embodiment of the present invention further proposes recording the amount of water added each time water is injected, and calculating the total amount of water added. Detecting whether the total amount of water added reaches the standard value includes: setting the standard value to A, the total amount of water involved in the preparation process of the raising agent to B, and the constraint relationship between A and B is: 35%B≤A≤38%B, and adjusting the total amount of water added in the preparation process of the raising agent according to the total amount of water added, so as to effectively detect the preparation integrity of the raising agent.
[0071] In practical applications, the embodiments of the present invention can realize the recording and calculation of the water addition amount in a variety of ways. For example, a flow meter can be used to monitor the water addition amount of each water injection in real time, and the data can be transmitted to the control system. The control system can use a PLC or an industrial computer to accumulate the water injection amount of each time in real time to obtain the current total amount of water addition.
[0072] In order to more accurately control the water addition process, multiple water addition thresholds can be set. For example, when the total amount of water added reaches 30%B, the first warning is issued; when it reaches 33%B, the second warning is issued; when it reaches 35%B, the water addition speed begins to slow down; when it reaches 37%B, it enters the fine-tuning mode to ensure that the final water addition amount falls within the range of 35%B to 38%B.
[0073] In addition, the embodiment of the present invention can also adjust the constraint relationship between A and B according to different types of hair oil. For example, for hair oil with higher viscosity, more water may be needed to achieve an ideal emulsification effect, and the constraint relationship can be adjusted to 36% B≤A≤39% B. On the contrary, for hair oil with lower viscosity, the constraint relationship can be adjusted to 34% B≤A≤37% B.
[0074] The embodiment of the present invention ensures the quality stability of the raising agent by accurately controlling the amount of water added. During the preparation process, by real-time monitoring and calculating the total amount of water added, it is possible to accurately determine when the standard value is reached, thereby avoiding the problem of excessive or insufficient water addition. This precise control not only improves product quality, but also optimizes production efficiency.
[0075] Specifically, the preparation method provided in the embodiment of the present invention can prepare a raising agent with stable performance and low aromatic content by accurately controlling the ratio of raising oil, water and bactericide, as well as parameters such as rotation speed, water injection interval, stirring time and the like during the emulsification process. Low aromatic content can reduce harm to the environment and human body and improve the safety of the product. Accurately controlled emulsification process can ensure the uniformity and stability of the raising agent, thereby improving its use effect in textile processing.
[0076] In the method for preparing the raising agent of the embodiment of the present invention, the selection of the raising oil is crucial. A variety of oils with low aromatic content can be selected, such as vegetable oil, mineral oil or synthetic oil. The aromatic content of these oils is usually less than 5%, and some can even reach less than 1%. Low aromatic content not only reduces the harm to the environment and human body, but also improves the stability and use effect of the raising agent.
[0077] During the emulsification process, the speed of the emulsifier can be adjusted between 1500-2500r / min, and optimized according to different types of hair oil and target product performance. The water injection process can also be adjusted according to actual needs, for example, continuous water injection or segmented water injection can be used, the water injection volume can be changed between 15-35kg each time, and the water injection interval can be adjusted between 4-8min. This flexible parameter setting allows the preparation process to adapt to different raw materials and product requirements.
[0078] The addition of a fungicide is another important feature of the fluffing agent of the present invention. The type of fungicide can be selected according to actual needs, such as isothiazolinones, quaternary ammonium salts, etc. The amount of fungicide added is usually between 0.1-0.3%, which can effectively prevent microbial contamination of the fluffing agent during storage and use, and extend the service life of the product.
[0079] The method for preparing the raising agent of the embodiment of the present invention is combined with the preparation steps described above to produce significant technical effects. The precisely controlled emulsification process ensures the uniformity and stability of the raising agent, while the selection of low aromatic content improves the environmental protection and safety of the product. The combination of these two aspects not only solves the environmental hazard problem of traditional raising agents, but also improves the applicability and effect of the product on different types of textiles.
[0080] In practical applications, the raising agent of the embodiment of the present invention exhibits excellent performance. For example, when processing polyester fabrics, using a raising agent with 1.2% OWf can significantly improve the softness and feel of the fabric without affecting other properties of the fabric such as strength and air permeability. For cotton fabrics, using a raising agent with 3.5% OWf can not only provide a good softening effect, but also maintain the water absorption and air permeability of the fabric. This wide applicability enables the raising agent of the embodiment of the present invention to meet the processing requirements of different types of textiles, thereby improving the practical value of the product.
[0081] Furthermore, OWf (On weight of the fabric) is a unit of measurement in the textile industry, which is the concentration in the dyeing and finishing process based on the weight of the fabric, and is a percentage relative to the fabric.
[0082] The method for preparing the raising agent of the embodiment of the present invention has significant advantages over the traditional method. Traditional raising agents usually use dimethyl silicone oil as the main raw material, which requires a complex emulsification process, and the silicon-containing components do not meet environmental protection requirements. The embodiment of the present invention uses low aromatic compounds as the main raw materials, which not only simplifies the preparation process, but also improves the environmental protection of the product. At the same time, the preparation method of the embodiment of the present invention ensures the stability and uniformity of the product by accurately controlling various parameters, such as emulsification speed, water injection interval, etc., which is difficult to achieve in traditional methods.
[0083] In addition, the raising agent of the embodiment of the present invention is also superior to the traditional product in terms of use effect. The traditional silicon-containing raising agent has poor affinity for cotton fibers, while the product of the embodiment of the present invention has good affinity for various fibers and can achieve an ideal softening effect on different types of textiles. This wide applicability greatly improves the practical value of the raising agent, allowing it to be used in more textile processing fields.
[0084] Embodiment three:
[0085] The embodiment of the present invention further provides a textile, wherein the textile is treated with the raising agent containing low aromatic compounds, and after the textile is dyed, the textile is softened with the raising agent.
[0086] By using a raising agent containing low aromatic compounds, this raising agent has better environmental protection and safety while maintaining a good raising effect. The softening treatment can improve the fiber hardening problem that may occur after dyeing. The softening treatment based on the raising agent can utilize the characteristics of the raising agent to not only raise the hair, but also achieve a softening effect at the same time, simplifying the processing process.
[0087] The raising agent in the embodiment of the present invention can be implemented in a variety of ways. For example, different proportions of low aromatic compounds and other ingredients can be mixed to adapt to different types of textiles. The formula of the raising agent can be adjusted according to the material of the textile. For example, for cotton textiles, the proportion of hydrophilic components can be increased; for synthetic fibers, the proportion of permeable components can be increased.
[0088] The step of softening after dyeing can be achieved in a variety of ways. For example, the dyed textile can be immersed in a solution containing a raising agent by dipping, and the dipping time and temperature can be controlled; or the raising agent can be sprayed evenly on the surface of the textile by spraying, and then heat treated to fix the effect. This treatment sequence not only protects the dyeing effect, but also improves the hardening problem that may occur in the fiber after dyeing, thereby improving the overall quality of the textile.
[0089] The technical solution of the embodiment of the present invention and the above-mentioned method for preparing the raising agent produce positive technical effects. The raising agent containing low aromatic compounds obtained by using a specific formula and preparation method exhibits excellent performance in the textile processing process. This raising agent can not only effectively perform raising treatment on textiles, but also play a role in the softening treatment after dyeing, achieving a multifunctional integrated treatment effect.
[0090] In the specific implementation process, the processing parameters can be adjusted according to the characteristics of different textiles. For example, for polyester textiles, the amount of raising agent can be controlled at 1.2% OWf, the softening treatment temperature after dyeing can be set to 40°C, and the treatment time is 20 minutes. Such processing parameters can ensure the raising effect without affecting the dyeing effect, and can significantly improve the softness of the textile.
[0091] The technical solution of the embodiment of the present invention achieves the softening effect of textiles by using a specially formulated raising agent containing low aromatic compounds and treating the textiles after dyeing. This treatment method has many advantages. First, low aromatic compounds reduce the potential harm to the environment and human body and improve the environmental performance of the product. Secondly, the raising and softening treatments are combined to simplify the production process and improve production efficiency. Furthermore, the treatment is carried out after dyeing to better protect the dyeing effect and improve the feel and texture of the textiles. Finally, this method is applicable to a variety of textile materials, such as polyester, polyester-cotton, pure cotton, nylon, acrylic, etc., showing a wide range of applicability.
[0092] The embodiment of the present invention further proposes that the material of the textile is one of polyester, polyester-cotton, pure cotton, nylon, and acrylic.
[0093] The embodiment of the present invention clarifies the material range of the textile, laying a foundation for the subsequent selection of an appropriate amount of raising agent. By limiting the textile material to one of polyester, polyester-cotton, pure cotton, nylon, and acrylic, the most suitable amount of raising agent can be selected according to the characteristics of different materials, thereby achieving the best softening treatment effect.
[0094] In specific implementation, the embodiment of the present invention can select an appropriate amount of raising agent according to different textile materials. For example, for textiles made of polyester or polyester-cotton, a raising agent amount of 1 to 1.5% OWf can be selected; for textiles made of nylon, a raising agent amount of 1.5 to 5% OWf can be selected; for textiles made of pure cotton, a raising agent amount of 3 to 5% OWf can be selected; for textiles made of acrylic, a raising agent amount of 1 to 3% OWf can be selected.
[0095] Furthermore, when the material of the textile is nylon 6, the amount of the raising agent used can be set at 3-5% OWf;
[0096] When the textile is made of nylon 66, the amount of the raising agent used can be set at 1.5-3% OWf.
[0097] The textiles are softened by the raising agent, so that the length of the surface fluff of the textiles is uniform and fine, and the hand feels fluffy and soft. After shaking, the particles are uniform in size; all fiber fabrics are hydrophilic, and the hydrophilic time is within 2 seconds; the fiber strength is not affected, so there is no fiber breakage and hair loss.
[0098] This method of selecting different amounts of raising agent for different materials combined with the aforementioned method for preparing the raising agent can produce better results. Since the raising agent of the embodiment of the present invention uses a raising oil containing low aromatic compounds and is prepared through a precisely controlled emulsification process, it can better adapt to the characteristics of textiles of different materials. For example, for pure cotton materials with strong water absorption, a higher amount of raising agent can be selected to ensure a sufficient softening effect; while for synthetic fibers such as polyester, a lower amount can be selected, which can achieve a softening effect while avoiding fiber damage caused by excessive use.
[0099] Specifically, the material of the textile to be treated is determined, and the amount of the raising agent used is selected according to the material; the prepared raising agent is applied to the softening process of the textile according to the selected amount. This method can ensure that textiles of each material can obtain the best softening effect, while avoiding the waste of the raising agent and the possible damage to the textile.
[0100] In addition, the above is a detailed introduction to the preparation method of a raising agent containing low aromatic compounds and its application provided by the embodiment of the present invention. Specific examples are used herein to illustrate the principle and implementation mode of the present invention. The description of the above embodiments is only used to help understand the method of the present invention and its core idea. At the same time, for those skilled in the art, according to the idea of the present invention, there will be changes in the specific implementation mode and application scope. In summary, the content of this specification should not be understood as limiting the present invention.
Claims
1. A method for preparing a raising agent containing low aromatic compounds, characterized in that: The preparation method comprises: Add the hair oil containing low aromatic compounds into the emulsification barrel, start the emulsifier, and make the emulsifier rotate at a preset speed; Add water into the emulsification tank at preset time intervals, and continue stirring for a preset time after each water addition; Record the amount of water added each time, calculate the total amount of water added, and check whether the total amount of water added reaches the standard value; When the total amount of water added reaches the standard value, a bactericide is added into the emulsification barrel, and the raising agent is obtained by filtering after stirring.
2. The method for preparing a raising agent containing low aromatic compounds according to claim 1, characterized in that: The raising agent is prepared by mixing raising oil, fungicide and water, wherein the raising oil accounts for 60% of the total amount of the raising agent, the fungicide accounts for 0.2% of the total amount of the raising agent, and the water accounts for 39.8% of the total amount of the raising agent.
3. The method for preparing a raising agent containing low aromatic compounds according to claim 1, characterized in that: The step of adding the hair oil into the emulsifying barrel and starting the emulsifying machine so that the emulsifying machine rotates at a preset speed comprises: The rotation speed of the emulsifier is set to 2000 r / min, and the hair raising oil is rotated at room temperature.
4. The method for preparing a raising agent containing low aromatic compounds according to claim 1, characterized in that: The step of injecting water into the emulsification barrel at a preset time interval and continuously stirring for a preset time after each injection includes: Set the water injection volume range for each injection to: 20kg~30kg; The value range of the preset time length is set to: 3min~5min; Set the preset time interval to 6 minutes.
5. The method for preparing a raising agent containing low aromatic compounds according to claim 1, characterized in that: The recording of the amount of water added each time the water is injected, calculating the total amount of water added, and detecting whether the total amount of water added reaches the standard value includes: The standard value is set to A, the total amount of water used in the preparation process of the raising agent is set to B, and the constraint relationship between A and B is: 35%*B≤A≤38%*B.
6. A raising agent, characterized in that: The raising agent is prepared based on the method for preparing a raising agent containing low aromatic compounds according to any one of claims 1 to 5.
7. A textile, characterized in that: The textile is treated with the raising agent according to claim 6, and after the textile is dyed, the textile is softened with the raising agent.
8. The textile product according to claim 7, characterized in that The textile is made of one of polyester, polyester-cotton, pure cotton, nylon and acrylic.
9. The textile product according to claim 8, characterized in that When the textile is made of polyester or polyester-cotton, the amount of the raising agent used is 1 to 1.5% OWf; When the textile is made of nylon, the amount of the raising agent used is 1.5-5% OWf; When the textile is made of pure cotton, the amount of the raising agent used is 3-5% OWf; When the textile is made of acrylic fiber, the amount of the raising agent used is 1-3% OWf.