Method for testing bonding strength of gravel and impurity base in conglomerate

Through the methods of sample preparation, fracture strength testing and whole rock fault surface analysis, the cementation strength of gravel and heterogeneous foundations in conglomerate was calculated, which solved the problems of inaccurate and complex testing results in the existing technology, and realized the gravel and gravel in conglomerate and The rapid and accurate measurement of heterobase cementing strength improves the effectiveness of reservoir development process.

CN119064261APending Publication Date: 2024-12-03PETROCHINA CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310644827.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-06-01
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The prior art cannot accurately and simply test the cementation strength of gravel and heterogeneous substrates in conglomerates, resulting in inaccurate test results and complex methods, making it difficult to obtain the engineering mechanical properties of the reservoir, affecting the effectiveness of the reservoir development process.

Method used

The cementing strength of gravel and heterogeneous substrates is calculated by formulas using sample preparation, fracture strength test, whole rock fracture surface analysis and cementing strength calculation methods. The cementing strength of gravel and heterogeneous substrates is calculated by using Brazilian splitting standard samples or three-point bending samples for experiments, and the fracture is analyzed in combination with ImageJ software. Area, simplify the testing process and improve accuracy.

Benefits of technology

It realizes rapid and accurate measurement of the cementation strength of gravel and miscellaneous foundations in conglomerates, avoids the problem of inaccurate cementation and cementation surface testing, simplifies sample processing and testing operations, reduces equipment demand, and improves the accuracy of test results. sex.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119064261A_ABST
    Figure CN119064261A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of conglomerate oil and gas development and research, in particular to a method for testing the bonding strength of gravels and miscellaneous bases in conglomerate. The testing method comprises the steps of sample preparation, breaking strength testing, total rock fracture surface analysis and cementing strength calculation. Wherein the bonding strength Kgm of the gravel and the impurity base is calculated through a formula (I), # imgabs0 # K0, Kg and Km are the total rock breaking strength, the gravel breaking strength and the impurity base breaking strength respectively, and the unit is MPa; sg, Sgm and Sm are respectively the gravel fracture surface area, the gravel peeling surface area and the miscellaneous base fracture surface area, and the unit is m2. The test method solves the problems of difficult sample preparation, inaccurate test result, complex test method and the like in the existing test method, and has the advantages of simple test process and accurate test result.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of conglomerate oil and gas development research, and in particular to a method for testing the bonding strength of gravel and matrix in conglomerate. Background Art

[0002] my country has the world's largest distribution area and the richest reserves of gravel reservoirs, which is a new growth point for my country's future unconventional oil and gas exploration and development. Gravel reservoirs are different from existing unconventional oil and gas reservoirs such as shale, tight sandstone, and coal seams. They have the characteristics of strong rock heterogeneity caused by the development of gravel. In the process of drilling, fracturing, and oil production, it is found that the bonding strength between gravel and matrix directly affects the engineering mechanical properties of the reservoir and is the key to the optimization of reservoir development technology, especially the influence on the morphology of hydraulic fracturing fractures. This parameter cannot be accurately obtained, which restricts the effectiveness of engineering construction technology. However, the existing test methods cannot accurately and simply test the key parameter of the bonding strength between gravel and matrix, and it is urgent to develop new methods to improve the shortcomings of existing technical solutions.

[0003] CN201310632690.8 discloses a simple shear test method for rock and concrete bonding surface, which is used to detect the shear strength of the bonding surface of two media. The method includes: vertically setting the rock-concrete bonding specimen to be tested, applying horizontal shear force at the bonding surface of the two media through a force transmission screw, and collecting the maximum strain of the sensor during the shear process by a strain sensor placed on the force transmission screw; the force transmission screw and the sensor axis are on the same horizontal line, and the bottom of the sensor has an arc surface that fits the force transmission screw.

[0004] CN201710744761.1 discloses a device and method for testing the strength of cemented particles under different loads in a high-temperature environment, wherein the device includes a stress field loading device, a temperature field loading device, and a data acquisition and processing device; wherein, the stress field loading device can be used to perform compression, shear, bending and torsion, and other mechanical property tests on the cemented particles; the temperature field loading device can be used to create a high-temperature environment for the test, which is closer to the deep formation and increases the authenticity of the test results; the data acquisition and processing device can be used to quantitatively obtain and record the changes in various parameters of the cemented particles during the test, measure and record the stress-strain process of the cemented particles under various loading conditions, and describe the fracture characteristics of the rock from the perspective of the microscopic basic particle unit.

[0005] CN201910369299.0 discloses a gravel bond strength testing device, method and process, the gravel bond strength testing device comprises: a fixed seat, the fixed seat comprises a first mounting surface and a second mounting surface arranged opposite to the first mounting surface; a support assembly, the support assembly is arranged on the first mounting surface, the support assembly is used to fix the gravel; a test assembly, the test assembly is arranged on the second mounting surface, the test assembly comprises a sensor and a pressure head, the pressure head is arranged on the side of the sensor away from the second mounting surface, and the pressure head is used to be pressed on the gravel; wherein, at least a part of the support assembly is movably arranged relative to the fixed seat, so that when the gravel moves relative to the pressure head, the sensor obtains the real-time pressure value of the pressure head acting on the gravel.

[0006] The above patents cannot solve the problem of testing the bonding properties of gravel and matrix. The bonding surface between gravel and matrix in conglomerate is generally a weaker surface. The first two methods need to be made by cutting. The bonding surface required in the test is exactly the fracture surface during the test. The sample preparation is complicated, difficult and has low accuracy. Although the third test method can directly test the bonding surface between gravel and matrix, its bonding strength is tested by peeling the gravel and the matrix that wraps the gravel with a pressure needle. Since gravel and matrix are in a wrapping and wrapped relationship, the bonding surface is concave, which easily leads to inaccurate estimation of the bonding surface area between gravel and matrix. In addition, the force obtained from the test includes not only the bonding force, but also the force of gravel destroying the edge of the bonding concave surface, which leads to the problem of excessive bonding force, and the bonding strength parameter cannot be accurately obtained.

[0007] Therefore, there is an urgent need for a method to quickly and accurately test the bonding strength between gravel and matrix in conglomerate. Summary of the invention

[0008] The purpose of the present invention is to overcome the problems that the existing testing method for the bonding strength of gravel and matrix in gravel cannot accurately and simply test the bonding strength, requires the use of specific testing equipment, and is easy to break during the processing process. A new testing method for the bonding strength of gravel and matrix in gravel is provided, and the testing method can quickly and accurately measure the bonding strength of gravel and matrix in gravel.

[0009] In order to achieve the above object, the present invention provides a method for testing the bonding strength of gravel and matrix in conglomerate, the testing method comprising: sample preparation, fracture strength test, whole rock fracture surface analysis and bonding strength calculation;

[0010] The bonding strength K between the gravel and the matrix is gm It is calculated by formula (I), where:

[0011]

[0012] Among them, K0, Kg and K m are the whole rock fracture strength, gravel fracture strength and matrix fracture strength, all in MPa; S g , S gm and S m They are the gravel fracture surface area, gravel peeling surface area and base fracture surface area, all in m 2 .

[0013] Preferably, in the sample preparation, the samples include whole rock samples, gravel samples and matrix samples.

[0014] Preferably, the whole rock sample, gravel sample and matrix sample are each independently selected from Brazilian splitting standard samples and three-point bending samples.

[0015] Preferably, when the sample is a Brazilian splitting standard sample, the shapes of the whole rock sample, gravel sample and miscellaneous matrix sample are each independently regular shapes, preferably selected from cylinders, and the ratio of the thickness to the diameter of the cylinder is preferably 0.5-1; or, when the sample is a three-point bending sample, the shapes of the whole rock sample, gravel sample and miscellaneous matrix sample are each independently regular shapes, preferably selected from cuboids, and the ratio of the length to the height of the cuboid is preferably 4.

[0016] Preferably, the process of the breaking strength test includes:

[0017] (1) When the sample is selected from the Brazilian splitting standard sample, the sample is tested according to the Brazilian splitting test method, the low displacement-load curve is tested, and the load peak value P is read in N; wherein the load peak value P includes the load peak value P0 of the Brazilian splitting standard sample of whole rock, the load peak value P of the Brazilian splitting standard sample of gravel g The peak load P of the Brazilian cleavage standard sample of the impurity base m ;

[0018] (2) According to formula (II), the whole rock fracture strength K0 and gravel fracture strength K0 are calculated respectively. g and base breaking strength K m ,in,

[0019]

[0020] Wherein, i is selected from 0, g and m; K i K0, K g and K m , the unit is MPa; P i They are P0, P g and P m , the unit is N; D i D0, D g and Dm , the unit is m; L i L0, L g and L m , the unit is m; π is 3.14.

[0021] Preferably, the process of the breaking strength test includes:

[0022] (1) When the sample is selected from a three-point bending sample, the sample is subjected to a three-point bending test method to test the low displacement-load curve and read the load peak value P ’ , unit is N;

[0023] The load peak value P' includes the load peak value P'0 of the three-point bending sample of the whole rock, the load peak value P' of the three-point bending sample of the gravel g The peak load P' of the three-point bending sample of the impurity base m ;

[0024] (2) The whole rock fracture strength K0 and gravel fracture strength K0 are calculated by formula (III) respectively. g and base breaking strength K m ,

[0025]

[0026] Wherein, i is selected from 0, g and m; K i K0, K g and K m , the unit is MPa; l i are l0, l g and l m , the unit is m; P' i P'0, P' g and P' m , the unit is N; t i are t0 and t g and t m , the unit is m; h i are h0 and h g and h m , the unit is m; a i a0, a g and a m , the unit is m.

[0027] Preferably, the whole rock fracture surface analysis process includes:

[0028] (1) After the whole rock sample is subjected to the whole rock fracture test, a fracture surface of the whole rock sample is obtained;

[0029] (2) collecting photos of the fracture surface of the whole rock sample, and using ImageJ software to identify and calculate the fracture surface area S on the fracture surface of the whole rock sample;

[0030] Wherein, the fracture surface area S includes: the gravel fracture surface area S g , gravel peeling surface area S gm and the fracture surface area S m .

[0031] Compared with the prior art, the present invention has the following advantages:

[0032] (1) The test method provided by the present invention adopts a specific formula (I) to calculate the bonding strength value of gravel and matrix in conglomerate with high precision, thus avoiding the problem of inaccurate bonding strength and bonding surface testing in the existing test method; at the same time, the test method is simple and easy to operate and execute;

[0033] (2) The test method provided by the present invention is easy to process the sample, and adopts a regular shape that is easy to realize (for example, a cylinder or a cuboid, etc.), thereby avoiding the problem of easy breakage during processing due to weak conglomerate cementation;

[0034] (3) The testing method provided by the present invention does not require any special experimental equipment and can be implemented using an ordinary rock mechanics experimental device. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] Figure 1 It is a process flow chart of a method for testing the bonding strength between gravel and matrix in conglomerate provided by the present invention;

[0036] Figure 2a It is a force diagram of a Brazilian splitting standard sample of a whole rock provided by the present invention;

[0037] Figure 2b It is a schematic diagram of a fracture surface of a whole-rock Brazilian splitting standard sample provided by the present invention, wherein the fracture surface of the whole-rock Brazilian splitting standard sample includes: a gravel fracture surface, a gravel peeling surface and a matrix fracture surface;

[0038] Figure 3a It is a force diagram of a three-point bending sample of a whole rock provided by the present invention;

[0039] Figure 3b It is a schematic diagram of a fracture surface of a whole-rock three-point bending sample provided by the present invention, wherein the fracture surface of the whole-rock three-point bending sample includes: a gravel fracture surface, a gravel peeling surface and a matrix fracture surface. DETAILED DESCRIPTION

[0040] The endpoints and any values ​​of the ranges disclosed in this article are not limited to the precise ranges or values, and these ranges or values ​​should be understood to include values ​​close to these ranges or values. For numerical ranges, the endpoint values ​​of each range, the endpoint values ​​of each range and the individual point values, and the individual point values ​​can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed in this article.

[0041] The present invention provides a method for testing the bonding strength of gravel and matrix in conglomerate, the testing method comprising: sample preparation, fracture strength test, whole rock fracture surface analysis and bonding strength calculation;

[0042] The bonding strength K between the gravel and the matrix is gm It is calculated by formula (I), where:

[0043]

[0044] Among them, K0, K g and K m are the whole rock fracture strength, gravel fracture strength and matrix fracture strength, all in MPa; S g , S gm and S m They are the gravel fracture surface area, gravel peeling surface area and base fracture surface area, all in m 2 .

[0045] The inventor of the present invention has found that: based on the problem that the existing rock bonding strength test method cannot test the bonding strength value of gravel and matrix, the present invention designs a gravel bonding strength test method based on the principle of testing bonding strength by the rock three-point bending method. During the test, the bonding strength test of gravel and matrix in the gravel is divided into three parts: whole rock fracture strength, matrix fracture strength and gravel fracture strength. The bonding strength of gravel and matrix is ​​calculated by the weighted method according to the proportion of the bonding area of ​​the matrix and gravel and matrix in the whole rock fracture strength of the gravel. This method solves the problems of difficult sample preparation, inaccurate test results, and complex test methods of the existing test methods, and has the advantages of simple test process and accurate test results.

[0046] A schematic diagram of a method for testing the bonding strength of gravel and matrix in conglomerate provided by the present invention is shown in FIG. Figure 1 As shown, the test method includes: step 1, sample preparation; step 2, fracture strength test; step 3, whole rock fracture surface analysis; step 4, cementation strength calculation.

[0047] In some embodiments of the present invention, preferably, in the sample preparation, the sample includes a whole rock sample, a gravel sample and a matrix sample. In the present invention, the whole rock sample refers to a sample whose fracture surface of the test sample is composed of gravel and matrix, and is a sample prepared from an actual natural core, and the ratio of gravel to matrix is ​​an actual volume ratio, that is, (5%-70%): (95%-30%); the gravel sample refers to a sample whose fracture surface of the test sample is composed of gravel; the matrix sample refers to a sample whose fracture surface of the test sample is composed of matrix.

[0048] In the present invention, the preparation method of the sample (i.e., whole rock sample, gravel sample and matrix sample) has a wide range of selection. Preferably, the preparation method of the sample is selected from the Brazilian splitting method (Technical Specifications for Testing Mechanical Properties of Oil and Gas Reservoirs Part 1: Conglomerate SY / T 7491.1-2020), the three-point bending method (Reference: Three-point bending test study on rock tensile strength and fracture toughness).

[0049] In some embodiments of the present invention, preferably, the whole rock sample, gravel sample and matrix sample are each independently selected from Brazilian splitting standard samples and three-point bending samples.

[0050] In a specific embodiment of the present invention, the sample preparation process includes: selecting gravel and matrix in conglomerate, and preparing a whole rock Brazilian splitting standard sample, a gravel Brazilian splitting standard sample and a matrix Brazilian splitting standard sample, respectively, wherein the volume ratio of gravel and matrix in the whole rock Brazilian splitting standard sample is (5%-70%): (95%-30%) after the actual natural core preparation sample test.

[0051] In another specific embodiment of the present invention, the sample preparation process also includes: selecting gravel and matrix in conglomerate to prepare three-point bending samples of whole rock, three-point bending samples of gravel and three-point bending samples of matrix respectively, wherein the volume ratio of gravel to matrix in the three-point bending sample of whole rock is the volume content of gravel and matrix obtained after testing the actual natural core preparation sample, which is (5%-70%): (95%-30%).

[0052] In some embodiments of the present invention, preferably, when the sample is a Brazilian splitting standard sample, the shapes of the whole rock sample, gravel sample and matrix sample are each independently regular shapes, preferably selected from cylinders, and further preferably, the ratio of the thickness to the diameter of the cylinder is 0.5-1, for example, 0.5, 0.8, 1, and any value in the range consisting of any two numerical values; or, when the sample is a three-point bending sample, the shapes of the whole rock sample, gravel sample and matrix sample are each independently regular shapes, preferably selected from cuboids, and further preferably, the ratio of the length to the height of the cuboid is 4.

[0053] In a specific embodiment of the present invention, the shapes of the Brazilian cleavage standard sample of whole rock, the Brazilian cleavage standard sample of gravel and the Brazilian cleavage standard sample of matrix are each independently a regular round cake shape.

[0054] In another specific embodiment of the present invention, the shapes of the three-point bending samples of whole rock, the three-point bending samples of gravel and the three-point bending samples of matrix are each independently a regular rectangular parallelepiped shape.

[0055] In some embodiments of the present invention, preferably, in the sample preparation, when the sample is selected from the Brazilian splitting standard sample, the diameter D0 of the whole rock Brazilian splitting standard sample is 50 mm and the thickness L0 is 25 mm; the diameter D0 of the gravel Brazilian splitting standard sample is 50 mm and the thickness L0 is 25 mm; g 50mm, thickness L g The diameter of the Brazilian cleavage standard sample of the impurity base is D m 50mm, thickness L m 25mm. (For the same type of conglomerate, considering the size effect of the mechanical properties of the conglomerate, it is advisable to select samples of two or more specifications for mechanical parameter determination, and the conglomerate sample size should be 2-5 times the maximum gravel diameter.)

[0056] In the present invention, unless otherwise specified, the diameter D parameter and the thickness L parameter are measured using the method in "Technical Specifications for Testing Mechanical Properties of Oil and Gas Reservoir Rocks Part 1: Conglomerate SY / T 7491.1-2020".

[0057] In some embodiments of the present invention, preferably, in the sample preparation, when the sample is selected from the three-point bending sample, the span l0 of the three-point bending sample of the whole rock is 100 mm, the width t0 is 40 mm, the height h0 is 25 mm, and the incision depth a0 is 12.5 mm; the l0 of the three-point bending sample of the gravel is g 100mm, width t g 40mm, height h g is 25mm, the incision depth a g is 12.5 mm; the l of the three-point bending sample of the impurity base m 100mm, width t m 40mm, height h m is 25mm, the incision depth a m For the same kind of conglomerate, considering the size effect of the mechanical properties of the conglomerate, it is advisable to select samples of two or more specifications for mechanical parameter determination, and the conglomerate sample size should be 2-5 times the gravel diameter.

[0058] In the present invention, unless otherwise specified, the span l parameter, width t parameter, height h parameter and cut depth a parameter are all measured using the method in the document "Three-point bending test study on rock tensile strength and fracture toughness".

[0059] In some embodiments of the present invention, preferably, Figure 1 As shown, the fracture strength test includes: whole rock fracture strength test, gravel fracture strength test, and matrix fracture strength test.

[0060] In some embodiments of the present invention, preferably, the process of the breaking strength test includes:

[0061] (1) When the sample is selected from the Brazilian splitting standard sample, the sample is tested according to the Brazilian splitting test method, and the displacement-load curve is tested, and the load peak value P is read in N; wherein the load peak value P includes the load peak value P0 of the Brazilian splitting standard sample of whole rock, the load peak value P of the Brazilian splitting standard sample of gravel g The peak load P of the Brazilian cleavage standard sample of the impurity base m ;

[0062] (2) According to formula (II), the whole rock fracture strength K0 and gravel fracture strength K0 are calculated respectively. g and base breaking strength K m ,in,

[0063]

[0064] Wherein, i is selected from 0, g and m; K i K0, K g and K m , the unit is MPa; P i They are P0, P g and P m , the unit is N; D i D0, D g and D m , the unit is m; L i L0, L g and L m , the unit is m; π is 3.14.

[0065] In the present invention, unless otherwise specified, in formula (II), when K i When i is selected from 0, P i and D i where i is also selected from 0; similarly, when K i When i is selected from g, P i and D i i is also selected from g; when K iWhen i is selected from m, P i and D i Here i is also selected from m.

[0066] In a specific embodiment of the present invention, the Brazilian splitting standard sample of whole rock, the Brazilian splitting standard sample of gravel and the Brazilian splitting standard sample of impurities are respectively subjected to the Brazilian splitting test method to test the low displacement-load curve, and the load peak value P0 of the Brazilian splitting standard sample of whole rock, the load peak value P0 of the Brazilian splitting standard sample of gravel and the load peak value P0 of the Brazilian splitting standard sample of gravel are respectively read. g The peak load P of the Brazilian cleavage standard sample of the impurity base m ;according to and The whole rock fracture strength K0 and gravel fracture strength K g and base breaking strength K m , where π is 3.14.

[0067] In some embodiments of the present invention, preferably, the process of the breaking strength test includes:

[0068] (1) When the sample is selected from a three-point bending sample, the sample is subjected to a three-point bending test method to test the low displacement-load curve and read the load peak value P ’ , unit is N;

[0069] The load peak value P' includes the load peak value P'0 of the three-point bending sample of the whole rock, the load peak value P' of the three-point bending sample of the gravel g The peak load P' of the three-point bending sample of the impurity base m ;

[0070] (2) The whole rock fracture strength K0 and gravel fracture strength K0 are calculated by formula (III) respectively. g and base breaking strength K m ,

[0071]

[0072] Wherein, i is selected from 0, g and m; K i K0, K g and K m , the unit is MPa; l i are l0, l g and l m , the unit is m; P' i P'0, P' g and P' m , the unit is N; t i are t0 and t g and t m, the unit is m; h i are h0 and h g and h m , the unit is m; a i a0, a g and a m , the unit is m.

[0073] In the present invention, unless otherwise specified, in formula (III), when K i When i is selected from 0, l i , P' i ,t i 、h i and a i where i is also selected from 0; similarly, when K i When i is selected from g, l i , P' i ,t i 、h i and a i i is also selected from g; when K i When i is selected from m, l i , P' i ,t i 、h i and a i Here i is also selected from m.

[0074] In another specific embodiment of the present invention, the three-point bending sample of the whole rock, the three-point bending sample of the gravel and the three-point bending sample of the matrix are respectively subjected to the three-point bending test method to test the low displacement-load curve, and the load peak value P'0 of the Brazilian splitting standard sample of the whole rock, the load peak value P' of the Brazilian splitting standard sample of the gravel, and the load peak value P' g The peak load P' of the Brazilian cleavage standard sample of the impurity base m ;according to and The whole rock fracture strength K0 and gravel fracture strength K g and base breaking strength K m .

[0075] In the present invention, unless otherwise specified, the whole rock fracture strength K0 and gravel fracture strength K1 measured by the above two fracture strength test processes are g and base breaking strength K m That is to say, when the sample is selected from the Brazilian splitting standard sample, the fracture strength test is conducted by using the Brazilian splitting test method to obtain the load peak value P, and combined with formula (II), the whole rock fracture strength K0 and gravel fracture strength K g and base breaking strength K mWhen the sample is selected from the three-point bending sample, the fracture strength test is carried out by the three-point bending test method to obtain the load peak value P', and combined with formula (III), the whole rock fracture strength K0 and gravel fracture strength K g and base breaking strength K m .

[0076] In some embodiments of the present invention, preferably, the whole rock fracture surface analysis process includes:

[0077] (1) After the whole rock sample is subjected to the whole rock fracture test, a fracture surface of the whole rock sample is obtained;

[0078] (2) collecting photos of the fracture surface of the whole rock sample, and using ImageJ software to identify and calculate the fracture surface area S on the fracture surface of the whole rock sample;

[0079] Wherein, the fracture surface area S includes: the gravel fracture surface area S g , gravel peeling surface area S gm and the fracture surface area S m .

[0080] In the present invention, the specific test method of using ImageJ software to identify and calculate the fracture surface area S on the fracture surface of the whole rock sample includes: splicing the fracture surface images through CT scanning, and then using PHotoshop software to analyze and extract the gravel fracture surface, gravel peeling surface and matrix fracture surface on the fracture surface, and then using ImageJ software to identify and analyze the identified fracture surface area.

[0081] In one embodiment of the present invention, Figure 2a-2b As shown, when the whole rock sample is selected from the Brazilian splitting standard sample of the whole rock, the whole rock sample has a cylindrical shape, a diameter D and a thickness L of the whole rock sample; after the whole rock fracture test, the two fracture surfaces on both sides of the crack of the whole rock sample are obtained, and one of the fracture surfaces is selected, which includes: gravel fracture surface, gravel peeling surface and matrix fracture surface, and the gravel fracture surface area S is identified and calculated using ImageJ software g , gravel peeling surface area S gm and the fracture surface area S m .

[0082] In another embodiment of the present invention, Figure 3a-3bAs shown, when the whole rock sample is selected from the three-point bending sample of the whole rock, the whole rock sample has a rectangular parallelepiped, and the span of the whole rock sample is l, the width is t, the height is h, and the incision depth is a; after the whole rock sample is subjected to the whole rock fracture test, two fracture surfaces on both sides of the crack of the whole rock sample are obtained, and one of the fracture surfaces is selected, which includes: gravel fracture surface, gravel peeling surface and matrix fracture surface, and the gravel fracture surface area S is identified and calculated using ImageJ software g , gravel peeling surface area S gm and the fracture surface area S m .

[0083] In some embodiments of the present invention, Figure 1 As shown, a method for testing the bonding strength between gravel and matrix in conglomerate comprises the following steps:

[0084] S1. Sample preparation: gravel and matrix in conglomerate are selected to prepare Brazilian splitting standard samples or three-point bending samples respectively; wherein, Brazilian splitting standard samples include: Brazilian splitting standard samples of whole rock, Brazilian splitting standard samples of gravel and Brazilian splitting standard samples of matrix; three-point bending samples include: three-point bending samples of whole rock, three-point bending samples of gravel and three-point bending samples of matrix;

[0085] S2. Fracture strength test includes: gravel fracture strength test, matrix fracture strength test and whole rock fracture strength test;

[0086] The process of the breaking strength test includes:

[0087] The Brazilian splitting standard samples of whole rock, gravel and mixed matrix were tested according to the Brazilian splitting test method, and the low displacement-load curve was tested. The load peak values ​​P0 of the Brazilian splitting standard sample of whole rock, the load peak values ​​P0 of the Brazilian splitting standard sample of gravel and the load peak values ​​P0 of the Brazilian splitting standard sample of gravel were read respectively. g The peak load P of the Brazilian cleavage standard sample of the impurity base m ;according to The whole rock fracture strength K0 and gravel fracture strength K g and base breaking strength K m , wherein, in formula (II), i is selected from 0, g and m; K i K0, K g and K m , the unit is MPa; P i They are P0, P g and P m , the unit is N; D i D0, D g and D m, the unit is m; L i L0, L g and L m , all in m; π is 3.14; or,

[0088] The three-point bending samples of whole rock, gravel and matrix were tested according to the three-point bending test method, and the low displacement-load curve was tested. The load peak values ​​P'0 of the Brazilian splitting standard sample of whole rock, the load peak values ​​P' of the Brazilian splitting standard sample of gravel and the load peak values ​​P' of the Brazilian splitting standard sample of gravel were read respectively. g The peak load P' of the Brazilian cleavage standard sample of the impurity base m ;according to The whole rock fracture strength K0 and gravel fracture strength K g and base breaking strength K m , wherein, in (III), i is selected from 0, g and m; K i K0, K g and K m , the unit is MPa; l i are l0, l g and l m , the unit is m; P' i P'0, P' g and P' m , the unit is N; t i are t0 and t g and t m , the unit is m; h i are h0 and h g and h m , the unit is m; a i a0, a g and a m , the unit is m;

[0089] S3, whole rock fracture surface analysis, when the whole rock Brazilian splitting standard sample or the whole rock three-point bending sample is subjected to the above whole rock fracture test, the whole rock sample fracture surface is obtained; collect photos of the whole rock sample fracture surface, and use ImageJ software to identify and calculate the fracture surface area S on the whole rock sample fracture surface, wherein the fracture surface area S includes: the gravel fracture surface area S g , gravel peeling surface area S gm and the fracture surface area S m ;

[0090] S4. Calculation of bonding strength, bonding strength K between gravel and base gm It is calculated by formula (I), where:

[0091] In a specific embodiment of the present invention, a method for testing the bonding strength between gravel and matrix in conglomerate comprises the following steps:

[0092] S1. Sample preparation: gravel and matrix in conglomerate are selected to prepare Brazilian splitting standard samples of whole rock, Brazilian splitting standard samples of gravel and Brazilian splitting standard samples of matrix respectively;

[0093] S2. Fracture strength test includes: gravel fracture strength test, matrix fracture strength test and whole rock fracture strength test;

[0094] The fracture strength test process includes: testing the Brazilian splitting standard sample of whole rock, the Brazilian splitting standard sample of gravel and the Brazilian splitting standard sample of impurities according to the Brazilian splitting test method, testing the low displacement-load curve, reading the load peak value P0 of the Brazilian splitting standard sample of whole rock, the load peak value P0 of the Brazilian splitting standard sample of gravel, and the load peak value P0 of the Brazilian splitting standard sample of gravel. g The peak load P of the Brazilian cleavage standard sample of the impurity base m ;according to The whole rock fracture strength K0 and gravel fracture strength K g and base breaking strength K m , wherein, in formula (II), i is selected from 0, g and m; K i K0, K g and K m , the unit is MPa; P i They are P0, P g and P m , the unit is N; D i D0, D g and D m , the unit is m; L i L0, L g and L m , the unit is m; π is 3.14;

[0095] S3, whole rock fracture surface analysis, when the whole rock Brazilian splitting standard sample is subjected to the whole rock fracture test, the whole rock sample fracture surface is obtained; collect photos of the whole rock sample fracture surface, and use ImageJ software to identify and calculate the fracture surface area S on the whole rock sample fracture surface, wherein the fracture surface area S includes: the gravel fracture surface area S g , gravel peeling surface area S gm and the fracture surface area S m ;

[0096] S4. Calculation of bonding strength, bonding strength K between gravel and base gm It is calculated by formula (I), where:

[0097] In another specific embodiment of the present invention, a method for testing the bonding strength between gravel and matrix in conglomerate comprises the following steps:

[0098] S1. Sample preparation: gravel and matrix in conglomerate are selected to prepare three-point bending samples of whole rock, three-point bending samples of gravel and three-point bending samples of matrix respectively;

[0099] S2. Fracture strength test includes: gravel fracture strength test, matrix fracture strength test and whole rock fracture strength test;

[0100] The fracture strength test process includes: conducting experiments on the three-point bending samples of whole rock, gravel and matrix respectively according to the three-point bending test method, testing the low displacement-load curve, and reading the load peak value P'0 of the Brazilian splitting standard sample of whole rock, the load peak value P' of the Brazilian splitting standard sample of gravel, and the load peak value P' g The peak load P' of the Brazilian cleavage standard sample of the impurity base m ;according to The whole rock fracture strength K0 and gravel fracture strength K g and base breaking strength K m , wherein, in (III), i is selected from 0, g and m; K i K0, K g and K m , the unit is MPa; l i are l0, l g and l m , the unit is m; P' i P'0, P' g and P' m , the unit is N; t i are t0 and t g and t m , the unit is m; h i are h0 and h g and h m , the unit is m; a i a0, a g and a m , the unit is m;

[0101] S3, whole rock fracture surface analysis, when the whole rock three-point bending sample is subjected to the whole rock fracture test, the whole rock sample fracture surface is obtained; collect photos of the whole rock sample fracture surface, and use ImageJ software to identify and calculate the fracture surface area S on the whole rock sample fracture surface, wherein the fracture surface area S includes: the gravel fracture surface area S g, gravel peeling surface area S gm and the fracture surface area S m ;

[0102] S4. Calculation of bonding strength, bonding strength K between gravel and base gm It is calculated by formula (I), where:

[0103] In some embodiments of the present invention, preferably, the bonding strength K of the gravel and the matrix is gm The theoretical bonding strength K between gravel and matrix satisfies formula (IV): The theoretical bonding strength K of the gravel and the matrix is ​​measured by directly peeling off the bonding surface of the gravel and the matrix, that is, by dividing the peak force of completely peeling off the gravel and the matrix by the area of ​​the gravel peeling off.

[0104] In some embodiments of the present invention, preferably, in formula (IV), Any value selected from the range consisting of ±5%, ±4%, ±3%, ±2%, ±1% and 0, and any two values.

[0105] The present invention will be described in detail below through examples.

[0106] The theoretical bonding strength K of gravel and matrix is ​​measured by directly peeling off the bonding surface of gravel and matrix, that is, K = 1.44 MPa.

[0107] Example 1

[0108] S1. Select gravel and matrix from the above conglomerate to prepare cylindrical Brazilian splitting standard samples of whole rock, Brazilian splitting standard samples of gravel and Brazilian splitting standard samples of matrix respectively;

[0109] The diameter D0 of the Brazilian splitting standard sample of whole rock is 50mm and the thickness L0 is 25mm; the diameter D0 of the Brazilian splitting standard sample of gravel is g 50mm, thickness L g The diameter of the Brazilian cleavage standard sample of the impurity base is D m 50mm, thickness L m 25mm;

[0110] S2. The Brazilian splitting standard samples of whole rock, gravel and mixed matrix are respectively subjected to the Brazilian splitting test method to test the low displacement-load curve, and the load peak values ​​P0 of the Brazilian splitting standard sample of whole rock are 1000N, the load peak values ​​P0 of the Brazilian splitting standard sample of gravel are 1000N, and the load peak values ​​P0 of the Brazilian splitting standard sample of gravel are 1000N. g The peak load P of the Brazilian cleavage standard sample with a base of 500N ism is 200N; according to The whole rock fracture strength K0 and gravel fracture strength K g and base breaking strength K m ,Right now,

[0111]

[0112]

[0113]

[0114] S3. After the whole-rock Brazilian splitting standard sample is subjected to the whole-rock fracture test, a whole-rock sample fracture surface is obtained; a photo of the whole-rock sample fracture surface is collected, and the gravel fracture surface area S on the fracture surface is identified and calculated using ImageJ software. g 0.0006875m 2 , gravel peeling surface area S gm 0.0003125m 2 and the fracture surface area S m 0.00025m 2 ;

[0115] S4, bond strength K between gravel and base gm It is calculated by formula (I), where:

[0116]

[0117] Among them, the bonding strength K between gravel and matrix is gm The theoretical bonding strength K between gravel and matrix satisfies: Error ≤±5%.

[0118] Example 2

[0119] S1. Sample preparation: gravel and matrix in conglomerate are selected to prepare rectangular three-point bending samples of whole rock, three-point bending samples of gravel and three-point bending samples of matrix respectively;

[0120] The span l0 of the three-point bending sample of whole rock is 100 mm, the width t0 is 40 mm, the height h0 is 25 mm, and the cut depth a0 is 12.5 mm; the l0 of the three-point bending sample of gravel is g 100mm, width t g 40m, high h g is 25m, the cutting depth a g is 12.5 mm; the l of the three-point bending sample of the impurity base m 100mm, width t m 40mm, height h mis 25mm, the incision depth a m 12.5mm;

[0121] S2. The three-point bending samples of the whole rock, the three-point bending samples of the gravel and the three-point bending samples of the matrix are respectively subjected to the three-point bending test method to test the low displacement-load curve, and the load peak values ​​P'0 of the three-point bending standard sample of the whole rock are read as 30N, the load peak values ​​P'0 of the three-point bending standard sample of the gravel are read as 30N, and the load peak values ​​P'1 of the three-point bending standard sample of the gravel are read as 30N. g The peak load P' of the three-point bending standard sample is 19N and impurity m is 10N; according to The whole rock fracture strength K0 and gravel fracture strength K g and base breaking strength K m ,Right now

[0122]

[0123]

[0124]

[0125] S3. After the three-point bending sample of the whole rock is subjected to the whole rock fracture test, the fracture surface of the whole rock sample is obtained; a photo of the fracture surface of the whole rock sample is collected, and the gravel fracture surface area S on the fracture surface is identified and calculated using ImageJ software. g 0.00025m 2 , gravel peeling surface area S gm 0.00015m 2 and the fracture surface area S m 0.0001m 2 ;

[0126] S4, bond strength K between gravel and base gm It is calculated by formula (I), where:

[0127]

[0128] Among them, the bonding strength K between gravel and matrix is gm The theoretical bonding strength K between gravel and matrix satisfies: Error ≤±5%.

[0129] Comparative Example

[0130] The micrometer pressure head was used to peel off the gravel and the cementing surface of the matrix. The gravel peeling area was 0.0004m 2 The peak force of the instrument is 540N, and the corresponding bonding strength value is 540N / 0.0004m 2 =1.44MPa.

[0131] The preferred embodiments of the present invention are described in detail above, but the present invention is not limited thereto. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications, including the combination of various technical features in any other suitable manner, and these simple modifications and combinations should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.

Claims

1. A method for testing the bonding strength between gravel and matrix in conglomerate, characterized in that: The test method includes: sample preparation, fracture strength test, whole rock fracture surface analysis and cementation strength calculation; The bonding strength K between the gravel and the matrix is gm It is calculated by formula (I), where: Among them, K0, K g and K m are the whole rock fracture strength, gravel fracture strength and matrix fracture strength, all in MPa; S g , S gm and S m They are the gravel fracture surface area, gravel peeling surface area and base fracture surface area, all in m 2 .

2. The testing method according to claim 1, wherein: In the sample preparation, the samples include whole rock samples, gravel samples and matrix samples; Preferably, the whole rock sample, gravel sample and matrix sample are each independently selected from Brazilian splitting standard samples and three-point bending samples.

3. The testing method according to claim 2, wherein: When the sample is a Brazilian splitting standard sample, the shapes of the whole rock sample, the gravel sample and the matrix sample are each independently regular, preferably selected from a cylinder, and the ratio of the thickness to the diameter of the cylinder is preferably 0.5-1; When the sample is a three-point bending sample, the shapes of the whole rock sample, gravel sample and matrix sample are each independently regular shapes, preferably selected from a cuboid, and the ratio of the length to the height of the cuboid is preferably 4.

4. The testing method according to claim 3, wherein: In the sample preparation, when the sample is selected from the Brazilian splitting standard sample, the diameter D0 of the Brazilian splitting standard sample of the whole rock is 50 mm and the thickness L0 is 25 mm; the diameter D0 of the Brazilian splitting standard sample of the gravel is 50 mm and the thickness L0 is 25 mm. g 50mm, thickness L g The diameter of the Brazilian cleavage standard sample of the impurity base is D m 50mm, thickness L m is 25mm.

5. The testing method according to claim 3, wherein: In the sample preparation, when the sample is selected from the three-point bending sample, the span l0 of the three-point bending sample of the whole rock is 100 mm, the width t0 is 40 mm, the height h0 is 25 mm, and the incision depth a0 is 12.5 mm; the l0 of the three-point bending sample of the gravel is g 100mm, width t g 40mm, height h g is 25mm, the incision depth a g is 12.5 mm; the l of the three-point bending sample of the impurity base m 100mm, width t m 40mm, height h m is 25mm, the incision depth a m It is 12.5mm.

6. The test method according to claim 4 or 5, wherein: The fracture strength test includes: whole rock fracture strength test, gravel fracture strength test and matrix fracture strength test.

7. The testing method according to claim 6, wherein: The process of the breaking strength test includes: (1) When the sample is selected from the Brazilian splitting standard sample, the sample is tested according to the Brazilian splitting test method, the low displacement-load curve is tested, and the load peak value P is read in N; wherein the load peak value P includes the load peak value P0 of the Brazilian splitting standard sample of whole rock, the load peak value P of the Brazilian splitting standard sample of gravel g The peak load P of the Brazilian cleavage standard sample of the impurity base m ; (2) According to formula (II), the whole rock fracture strength K0 and gravel fracture strength K0 are calculated respectively. g and base breaking strength K m ,in, Wherein, i is selected from 0, g and m; K i K0 and K g and K m , the unit is MPa; P i They are P0, P g and P m , the unit is N; D i D0, D g and D m , the unit is m; L i L0, L g and L m , the unit is m; π is 3.

14.

8. The testing method according to claim 6, wherein: The process of the breaking strength test includes: (1) When the sample is selected from a three-point bending sample, the sample is subjected to a three-point bending test method to test the low displacement-load curve and read the load peak value P ’ , unit is N; The load peak value P' includes the load peak value P'0 of the three-point bending sample of the whole rock, the load peak value P' of the three-point bending sample of the gravel g The peak load P' of the three-point bending sample of the impurity base m ; (2) The whole rock fracture strength K0 and gravel fracture strength K0 are calculated by formula (III) respectively. g and base breaking strength K m , Wherein, i is selected from 0, g and m; K i K0, K g and K m , the unit is MPa; l i are l0, l g and l m , the unit is m; P' i P'0, P' g and P' m , the unit is N; t i are t0 and t g and t m , the unit is m; h i are h0 and h g and h m , the unit is m; a i a0, a g and a m , the unit is m.

9. The testing method according to claim 6, wherein: The whole rock fracture surface analysis process includes: (1) After the whole rock sample is subjected to the whole rock fracture test, a fracture surface of the whole rock sample is obtained; (2) collecting photos of the fracture surface of the whole rock sample, and using ImageJ software to identify and calculate the fracture surface area S on the fracture surface of the whole rock sample; Wherein, the fracture surface area S includes: the gravel fracture surface area S g , gravel peeling surface area S gm and the fracture surface area S m .

10. The test method according to any one of claims 1 to 9, wherein: The bonding strength K between the gravel and the base gm The theoretical bonding strength K between gravel and matrix satisfies formula (IV): The theoretical bonding strength K between the gravel and the matrix is ​​measured by directly peeling off the bonding surface between the gravel and the matrix.