Method for efficiently extracting 2-phenyl propylene from rectified heavy components
By preparing catalysts containing aluminum chloride, iron chloride, zinc chloride and vanadium sulfate, and optimizing reaction conditions in fixed bed reactors, the conversion of 2-phenyl isopropanol to 2-benzene in the distilled heavy component was solved by preparing the catalysts containing aluminum chloride, iron chloride, zinc chloride and vanadium sulfate, and optimizing the reaction conditions in the fixed bed reactor. The low yield problem of plasmopropylene achieves efficient extraction of 2-phenylpropylene, which significantly improves the conversion rate and economic value.
Patent Information
- Application Number
- CN202411242411.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-05
- Publication Date
- 2024-12-06
AI Technical Summary
Prior Art In the production process of industrial peroxide, the yield of dehydration of 2-phenyl isopropyl alcohol in the distilled heavy component is not high, and the residual 2-phenyl isopropyl isopropyl The difficulty in separation of alcohols leads to difficulty in separation of acetophenone in subsequent distillation. The catalytic yield of traditional catalysts does not exceed 90%, which poses waste of resources and safety risks.
The fixed mixture of aluminum chloride, iron chloride, zinc chloride and vanadium sulfate is mixed with dilute sulfuric acid, and the catalyst is prepared by evaporation and dryness, crushing, extrusion molding and low-temperature sintering to improve the proportion and acidity of the catalyst, and the reaction is carried out by fixed bed. The device carries out catalytic dehydration reaction to optimize temperature, time and empty bed speed.
The conversion rate of 2-phenyl isopropanol is achieved by more than 98% to 2-phenyl propylene, which significantly improves the yield, reduces the cost of waste liquid treatment, and obtains high economic value products.
Abstract
Description
Technical Field
[0001] The invention relates to the field of extraction and utilization of distillation heavy components containing 2-phenylisopropanol generated in the production process of industrial cumene peroxide (DCP), in particular to a method for efficiently extracting 2-phenylpropylene from the distillation heavy components. Background Art
[0002] When the isopropylbenzene oxidation method is used to produce products such as diisopropylbenzene peroxide, by-products such as acetophenone, 2-phenylpropylene and 2-phenylisopropanol are generated. In the distillation process of diisopropylbenzene peroxide, distillation heavy components are produced, which are generally called heavy aromatic waste liquid in industry. This waste liquid is a hazardous waste, but contains high-value chemical products such as acetophenone, 2-phenylpropylene and 2-phenylisopropanol in high concentrations. Since the heavy components are flammable hazardous chemical wastes with acute toxicity and flammability, their random discharge will cause ecological pollution and serious safety hazards. Such hazardous wastes must be harmlessly treated by enterprises with corresponding hazardous waste disposal qualifications. Traditionally, incineration is the main method, but there are disadvantages such as high third-party entrusted disposal costs, waste of resources, and increased carbon emissions.
[0003] In the process of extracting chemicals such as acetophenone and 2-phenylpropylene from heavy components, the 2-phenylisopropanol in the heavy components needs to be dehydrated and converted into 2-phenylpropylene, and then produced by distillation process. In theory, a mixed liquid containing about 75% by mass of 2-phenylpropylene and about 20% by mass of acetophenone can be obtained; the conventional process uses dilute sulfuric acid, water, ferric sulfate, and other organic acids for catalytic dehydration, and the yield generally does not exceed 90%; at the same time, the residual unreacted 2-phenylisopropanol will cause difficulty in separation during the subsequent distillation of acetophenone because its boiling point is close to that of acetophenone. Summary of the invention
[0004] The technical problem to be solved by the present invention is to overcome the disadvantages of the prior art and provide a method for efficiently extracting 2-phenylpropylene from a distillation heavy component.
[0005] In order to solve the above technical problems, the technical solution of the present invention is as follows: a method for preparing a catalyst, comprising the following steps: Step 1: mixing a fixed mixture of aluminum chloride, ferric chloride, zinc chloride and vanadium sulfate with dilute sulfuric acid to obtain a mixed solution; Step 2: The mixed solution is evaporated and then crushed, and then dilute sulfuric acid and other solvents are added, extruded into strips, and then dried to constant weight to obtain a pre-finished product; Step 3: Sinter the pre-finished product at low temperature to obtain the desired catalyst.
[0006] In step 1, the mass components of the fixed mixture are: aluminum chloride 45-48%, ferric chloride 20-25%, zinc chloride 28-30%, and vanadium sulfate 4.5-10%.
[0007] In the catalyst ratio, increasing the content of aluminum chloride and ferric chloride can make the target hydroxyl group in 2-phenylisopropanol positively charged, so that it is easier to remove the hydroxyl group under heating conditions. However, too high a content of ferric chloride will cause 2-phenylisopropanol to be oxidized. Appropriate content of zinc chloride and vanadium sulfate can accelerate the catalytic reaction rate.
[0008] The concentration of dilute sulfuric acid in step 1 is 15-45%.
[0009] Adding dilute sulfuric acid can increase the acidity of the mixed solution. After contacting with 2-phenylisopropanol, the protons can quickly react with the hydroxyl groups, making it easier to remove the hydroxyl groups and form water. Excessively high concentrations of sulfuric acid can cause the catalyst to be oxidized and turn black during the preparation process.
[0010] The concentration of dilute sulfuric acid in step 1 is 20-30%.
[0011] The concentration of dilute sulfuric acid in step 1 is 25%.
[0012] In step 1, the ratio of the added mass of the dilute sulfuric acid to the total mass of the solid mixture is 1.05-1.80:1.
[0013] An appropriate amount of dilute sulfuric acid can increase the acidity of the mixed solution, while excessive sulfuric acid will result in failure to sinter the catalyst during preparation.
[0014] The ratio of the added mass of the dilute sulfuric acid to the total mass of the solid mixture in step 1 is 1.35-1.73:1.
[0015] The ratio of the added mass of the dilute sulfuric acid to the total mass of the solid mixture in step 1 is 1.43:1.
[0016] The temperature during mixing in step 1 is 40-70° C.; the mixing method is preferably stirring.
[0017] The appropriate mixing temperature can fully dissolve the salt substances.
[0018] The temperature during mixing in step 1 is 45-60° C.; the mixing method is preferably stirring.
[0019] The temperature during mixing in step 1 is 55° C.; the mixing method is preferably stirring.
[0020] In step 2, the mixed solution is evaporated to constant weight; the evaporation temperature is 95-110°C.
[0021] If the evaporation temperature is too low, the preparation speed will be too slow; if the temperature is too high, the solution will be locally overheated, resulting in catalyst poisoning.
[0022] In step 2, the mixed solution is evaporated to constant weight; the evaporation temperature is 98-105°C.
[0023] In step 2, the mixed solution is evaporated to constant weight; the evaporation temperature is 102°C.
[0024] The particle size after crushing in step 2 is 0.5-2.5 mm.
[0025] Appropriate particle size can reduce the loss of catalyst during the reaction and increase the specific surface area of the material.
[0026] The particle size after crushing in step 2 is 0.95-2.0 mm.
[0027] The particle size after crushing in step 2 is 1.2 mm.
[0028] The concentration of dilute sulfuric acid in step 2 is 15-45%, and the mass of added dilute sulfuric acid is 30% of the mass after drying to constant weight in step 1.
[0029] An appropriate amount of dilute sulfuric acid can increase the acidity of the mixed solution, while excessive sulfuric acid will result in failure to sinter the catalyst during preparation.
[0030] Too high or too low a concentration of sulfuric acid will cause the subsequent extruded strips to change in shape.
[0031] The concentration of dilute sulfuric acid in step 2 is 20-30%, and the mass of added dilute sulfuric acid is 30% of the mass after drying to constant weight in step 1.
[0032] The concentration of dilute sulfuric acid in step 2 is 25%, and the mass of dilute sulfuric acid added is 30% of the mass after drying to constant weight in step 1.
[0033] The other solvent in step 2 is a mixed solvent of nitromethane and triphenylphosphine; the mass ratio of nitromethane to triphenylphosphine is 0.15-0.40:1, and the total mass of the two solvents is 15.5% of the mass after drying to constant weight in step 1.
[0034] Both nitromethane and triphenylphosphine are good phase transfer solvents, and appropriate amounts are helpful for the subsequent catalytic dehydration.
[0035] The other solvent in step 2 is a mixed solvent of nitromethane and triphenylphosphine; the mass ratio of nitromethane to triphenylphosphine is 0.25-0.35:1, and the total mass of the two solvents is 15.5% of the mass after drying to constant weight in step 1.
[0036] The other solvent in step 2 is a mixed solvent of nitromethane and triphenylphosphine; the mass ratio of nitromethane to triphenylphosphine is 0.3:1, and the total mass of the two solvents is 15.5% of the mass after drying to constant weight in step 1.
[0037] The drying temperature in step 2 is 80-105°C.
[0038] Too low a drying temperature will result in slow catalyst preparation; too high a temperature will cause the catalyst to fail to form and become scattered.
[0039] The drying temperature in step 2 is 90-100°C.
[0040] The drying temperature in step 2 is 95°C.
[0041] The sintering temperature in step 3 is 100-150°C.
[0042] If the sintering temperature is too low, the catalyst preparation speed will be too slow; if the temperature is too high, the catalyst will not be able to form and will become scattered.
[0043] The sintering temperature in step 3 is 110-140°C.
[0044] The sintering temperature in step 3 is 120°C.
[0045] The sintering time in step 3 is 3-6h.
[0046] If the sintering time is too low, the catalyst preparation speed will be too slow; if the temperature is too high, the catalyst will not be able to form and will become scattered.
[0047] The sintering time in step 3 is 3.5-5h.
[0048] The sintering time in step 3 is 4 h.
[0049] The heating rate of sintering in step 3 is 2-5°C / min.
[0050] Increasing the temperature too quickly during sintering can cause the catalyst to crack and can also cause the catalyst to be unable to form after sintering.
[0051] The heating rate of sintering in step 3 is 3.1-4.7°C / min.
[0052] The heating rate of sintering in step 3 is 3.5°C / min.
[0053] The method is applied in a fixed bed reactor. The specific method is as follows: the distilled heavy component is introduced into a microchannel fixed bed reactor equipped with a catalyst for reaction to obtain a crude 2-phenylpropylene liquid with a concentration of 75%.
[0054] The temperature of the fixed bed reactor is 90-160°C.
[0055] Too low a temperature will result in a slow reaction rate, while too high a temperature will cause the catalyst to crack and fail.
[0056] The temperature of the fixed bed reactor is 110-130°C.
[0057] The temperature of the fixed bed reactor was 125°C.
[0058] The reaction time is 3-10h.
[0059] If the reaction time is too short, the reactants will not be able to receive enough activation energy, resulting in a significant decrease in yield; if the reaction time is too long, side effects such as increased impurities will occur.
[0060] The reaction time is 4-8h.
[0061] The reaction time is 6h.
[0062] The empty bed velocity of the distillation heavy component is 0.1-10h -1 .
[0063] If the empty bed velocity is too high, the catalyst will not be able to fully contact the reactants during the reaction, resulting in a significant decrease in yield; if the velocity is too slow, the reaction time will be increased, resulting in side effects such as an increase in impurities.
[0064] The empty bed velocity of the distillation heavy component is 0.9-3.8h -1 .
[0065] The empty bed velocity of the distillation heavy component is 1.8h -1 .
[0066] The beneficial effects of the present invention are: The present invention can convert 2-phenylisopropanol in heavy aromatic waste liquid into target product 2-phenylpropylene with a conversion rate exceeding 98%. The catalyst formulation of the present invention can achieve a conversion rate under appropriate reaction conditions that is much higher than conventional catalytic reactions on the market; it can significantly reduce waste liquid treatment costs, and the high-concentration product obtained has greater economic value. DETAILED DESCRIPTION
[0067] In order to make the content of the present invention more clearly understood, the present invention is further described in detail below according to specific implementation methods. Example 1
[0068] Preparation of catalyst: Step 1: At 52° C., add 33.4 g of aluminum chloride, 16.64 g of ferric chloride, 21.77 g of zinc chloride and 3.89 g of vanadium sulfate to 106.4 g of sulfuric acid (concentration 25%), stir and mix well to obtain a mixed solution; Step 2: evaporate the mixed solution to constant weight at 102°C, crush it to a particle size of 1.2 mm, sieve it, add 9.0g triphenylphosphine, 24.1g 25% sulfuric acid and 2.7g nitromethane, disperse it evenly at high speed, and then put it into a mold for extrusion molding, and dry it at 105°C to constant weight to obtain a pre-finished product; Step 3: The pre-finished product is heated from room temperature to 120°C at a heating rate of 3.5°C / min and sintered for 4 hours to obtain a finished catalyst.
[0069] Extraction of 2-phenylpropene: 300 g of catalyst was placed in a fixed bed reactor, the reaction temperature was set to 120 °C, and the distilled heavy components were introduced at a space velocity of 1.85 h -1 After 6 hours of reaction, the conversion rate of 2-phenylisopropanol was 99.21%, and the yield of 2-phenylpropylene was 98.74%. Example 2
[0070] Preparation of catalyst: Step 1: At 52° C., add 25 g of aluminum chloride, 12.2 g of ferric chloride, 15.6 g of zinc chloride and 2.7 g of vanadium sulfate to 79.5 g of sulfuric acid (concentration 25%), stir and mix well to obtain a mixed solution; Step 2: The mixed solution is evaporated to constant weight at 102°C, then crushed to a particle size of 1.3 mm, sieved, and then 6.7 g of triphenylphosphine, 16.7 g of 25% sulfuric acid and 2.0 g of nitromethane are added, and after high-speed dispersion, it is put into a mold for extrusion molding, and dried at 105°C to constant weight to obtain a pre-finished product; Step 3: The pre-finished product is heated from room temperature to 120°C at a heating rate of 3.5°C / min and sintered for 4 hours to obtain a finished catalyst.
[0071] Extraction of 2-phenylpropene: 200 g of catalyst was placed in a fixed bed reactor, the reaction temperature was set to 120 °C, and the distilled heavy components were introduced at a space velocity of 1.83 h -1 After 6.2 h of reaction, the conversion rate of 2-phenylisopropanol was 98.61%, and the yield of 2-phenylpropylene was 98.11%. Example 3
[0072] Preparation of catalyst: Step 1: At 55° C., add 37.5 g of aluminum chloride, 18.3 g of ferric chloride, 23.4 g of zinc chloride and 4.05 g of vanadium sulfate to 119 g of sulfuric acid (concentration 25%), stir and mix well to obtain a mixed solution; Step 2: evaporate the mixed solution to constant weight at 102°C, crush it to a particle size of 1.2 mm, sieve it, add 10.1g triphenylphosphine, 25g 25% sulfuric acid and 3.0g nitromethane, disperse it evenly at high speed, and then put it into a mold for extrusion molding, and dry it at 105°C to constant weight to obtain a pre-finished product; Step 3: The pre-finished product is heated from room temperature to 120°C at a heating rate of 3.5°C / min and sintered for 4 hours to obtain a finished catalyst.
[0073] Extraction of 2-phenylpropene: 200 g of catalyst was placed in a fixed bed reactor, the reaction temperature was set to 120 °C, and the distilled heavy components were introduced at a space velocity of 1.8 h -1 After 6 hours of reaction, the conversion rate of 2-phenylisopropanol was 99.31%, and the yield of 2-phenylpropylene was 99.12%.
[0074] In addition to the above embodiments, the present invention may also have other implementation modes; any technical solutions formed by equivalent replacement or equivalent transformation shall fall within the protection scope required by the present invention.
Claims
1. A method for preparing a catalyst, It is characterized in that The following steps are involved: Step 1: mixing a fixed mixture of aluminum chloride, ferric chloride, zinc chloride and vanadium sulfate with dilute sulfuric acid to obtain a mixed solution; Step 2: The mixed solution is evaporated and then crushed, and then dilute sulfuric acid and other solvents are added, extruded into strips, and then dried to constant weight to obtain a pre-finished product; Step 3: Sinter the pre-finished product at low temperature to obtain the desired catalyst.
2. The method for preparing the catalyst according to claim 1, It is characterized in that The mass components of the fixed mixture in step 1 are: 45-48% aluminum chloride, 20-25% ferric chloride, 28-30% zinc chloride, and 4.5-10% vanadium sulfate.
3. The method for preparing the catalyst according to claim 2, It is characterized in that The concentration of the dilute sulfuric acid in step 1 is 15-45%; the ratio of the added mass of the dilute sulfuric acid to the total mass of the solid mixture in step 1 is 1.05-1.80:1; the temperature during mixing in step 1 is 40-70° C.; the mixing method is preferably stirring.
4. The method for preparing the catalyst according to claim 2, It is characterized in that In the step 2, the mixed solution is evaporated to constant weight; the evaporation temperature is 95-110° C.; the particle size after crushing in the step 2 is 0.5-2.5 mm; the concentration of dilute sulfuric acid in the step 2 is 15-45%, and the mass of the added dilute sulfuric acid is 30% of the mass after drying to constant weight in the step 1; the other solvent in the step 2 is a mixed solvent of nitromethane and triphenylphosphine; the mass ratio of nitromethane to triphenylphosphine is 0.15-0.40:1, and the total mass of the two solvents is 15.5% of the mass after drying to constant weight in the step 1; the drying temperature in the step 2 is 80-105° C.
5. The method for preparing the catalyst according to claim 2, It is characterized in that The sintering time in step 3 is 3-6 hours; the heating rate of sintering in step 3 is 2-5°C / min.
6. Use of the catalyst according to any one of claims 1 to 5 in extracting 2-phenylpropylene from a distillation heavy component containing 2-phenylisopropanol, It is characterized in that The application in a fixed bed reactor is specifically as follows: the distilled heavy component is introduced into a microchannel fixed bed reactor equipped with a catalyst for reaction to obtain a crude 2-phenylpropylene liquid with a concentration of 75%.
7. Use of the catalyst according to claim 6 in extracting 2-phenylpropylene from a distillation heavy component containing 2-phenylisopropanol, It is characterized in that The temperature of the fixed bed reactor is 90-160°C.
8. Use of the catalyst according to claim 6 in extracting 2-phenylpropylene from a distillation heavy component containing 2-phenylisopropanol, It is characterized in that The reaction time is 3-10h.
9. Use of the catalyst according to claim 6 in extracting 2-phenylpropylene from a distillation heavy component containing 2-phenylisopropanol, It is characterized in that Empty bed velocity of heavy component is 0.1-10h -1 .