Novel modeling process for reducing weight of belt pulley blank
By reserving annular protrusions in the pulley mold cavity and buckle grooves on the side walls of the cast blank to form a hub and hollow web plate, combined with heat treatment and sandblasting and anti-rust treatment, the problem of excessive weight of the pulley is solved, and the reduction is achieved Energy consumption and the effect of improving transmission efficiency and service life.
Patent Information
- Application Number
- CN202411218994.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-02
- Publication Date
- 2024-12-06
AI Technical Summary
The weight of existing pulleys is large, which leads to an increase in energy consumption, fuel consumption, and cost, and generates centrifugal force and vibration during high-speed rotation, affecting the efficiency and safety of the transmission system.
A new molding process for weight reduction of pulley blanks is adopted. By reserving annular protrusions on the inner wall of the mold cavity to form a belt groove, using gray cast iron or ductile iron materials, and buckle the grooves on the side walls of the cast blanks to form a hub and hollow belly plate , combined with heat treatment and sandblasting and anti-rust treatment, reduce weight and improve transmission efficiency and service life.
Effectively reduce the weight of the pulley, improve transmission efficiency and smooth operation, extend service life, reduce production costs, reduce fuel consumption, meet environmental protection requirements, and improve the practicality and diversity of the pulley.
Smart Images

Figure CN119076893A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of pulleys, and in particular to a new shaping process for reducing the weight of a pulley blank. Background Art
[0002] Pulleys are hub-type parts. They are generally relatively large in size and are manufactured using casting and forging techniques. Pulleys are usually used in transmission systems to transmit power through belts. They are mounted on the motor shaft or the rotating shaft of the machine, and the other pulley that matches it is connected to the load side. The two are connected by an endless belt to achieve the transmission of torque or motion.
[0003] In the prior art, the weight of the pulley, as a core component in the transmission system, has a very important impact on the energy efficiency of the entire system. A heavier pulley requires more energy when operating, which increases the energy consumption of the transmission system and the fuel consumption of the entire transmission system, thereby increasing the cost of the transmission.
[0004] Therefore, those skilled in the art have provided a new shaping process for reducing the weight of a pulley blank to solve the problems raised in the above-mentioned background technology. Summary of the invention
[0005] The purpose of the present invention is to provide a new shaping process for reducing the weight of a pulley blank, so as to solve the problems raised in the above-mentioned background technology.
[0006] To achieve the above object, the present invention provides the following technical solutions:
[0007] The above technical objectives of the present invention are achieved through the following technical solutions:
[0008] A new shaping process for reducing the weight of a pulley blank includes the following steps:
[0009] S101, preparing a mold for casting;
[0010] S102, injecting the casting material into the mold, and waiting for cooling and shaping to be completed to obtain a casting blank;
[0011] S103, taking out the casting blank and mounting it on the chuck of the machine tool;
[0012] S104, machining the surface of the blank by a spindle to obtain a semi-finished pulley;
[0013] S105, removing the semi-finished pulley and performing heat treatment;
[0014] S106, performing surface sandblasting on the heat-treated semi-finished pulley;
[0015] S107, after the sandblasting is completed, the surface of the semi-finished pulley is subjected to rust prevention treatment.
[0016] Further, based on S101, an annular protrusion for forming a belt groove is reserved on the inner wall of the mold cavity at the rim of the pulley.
[0017] Further, based on S102, the casting material is gray cast iron or ductile iron.
[0018] Further, based on S104, machining is performed to groove the side wall of the casting blank with a spindle drive milling cutter, so that a hub for mounting the spindle is formed in the middle of the casting blank, and the web between the hub and the rim is hollowed out.
[0019] Further, based on S105, the heat treatment temperature is controlled at 550° to 650°.
[0020] Further, based on S105, the heat treatment temperature is controlled at 840° to 880°.
[0021] Further, based on S106, the blasting mesh number is 40 mesh to 120 mesh.
[0022] Further, based on S107, the surface anti-rust treatment is phosphating blackening treatment, paint treatment, surface spraying and electroplating.
[0023] In summary, the present invention includes at least one of the following beneficial technical effects:
[0024] 1. The new shaping process of the pulley blank for reducing weight, by using the main shaft to buckle the groove on the side wall of the casting blank, so that the middle part of the casting blank forms a hub for installing the main shaft, and the web between the hub and the rim is hollowed out, which can effectively reduce the weight of the pulley. At the same time, the hollowed-out web can reduce the inertia moment during matrix transmission, improve transmission efficiency and running stability, and further improve the practicality of the pulley;
[0025] 2. The new shaping process of the pulley blank for weight reduction, by making the casting material gray cast iron or ductile iron, can make the pulley select the casting material according to the application environment and use intensity, which can effectively improve the use range of the pulley, thereby enhancing the practicality of the pulley and making the pulley easier to promote;
[0026] 3. The new molding process for reducing the weight of the pulley blank reserves an annular protrusion for forming a belt groove at the rim of the pulley in the casting cavity of the mold. After the casting material is injected into the cavity, it is squeezed by the annular protrusion, and the casting material is cooled and shaped to form a belt groove at the edge of the blank, which can save the subsequent machining steps, thereby further improving the production efficiency of the pulley. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0028] Figure 1 The present invention is a flow chart of a new shaping process for reducing the weight of a pulley blank. DETAILED DESCRIPTION
[0029] The present invention is further described below with reference to the accompanying drawings and specific embodiments:
[0030] Embodiment 1:
[0031] The new shaping process for reducing the weight of a pulley blank disclosed in the present invention comprises the following steps:
[0032] S101, preparing a mold for casting;
[0033] S102, injecting the casting material into the mold, and waiting for cooling and shaping to be completed to obtain a casting blank;
[0034] S103, taking out the casting blank and mounting it on the chuck of the machine tool;
[0035] S104, machining the surface of the blank by a spindle to obtain a semi-finished pulley;
[0036] S105, removing the semi-finished pulley and performing heat treatment;
[0037] S106, performing surface sandblasting on the heat-treated semi-finished pulley;
[0038] S107, after the sandblasting is completed, the surface of the semi-finished pulley is subjected to rust prevention treatment.
[0039] Based on S101, an annular protrusion for forming a belt groove is reserved on the inner wall of the mold cavity at the rim of the pulley.
[0040] Based on S102, the casting material is grey cast iron.
[0041] Based on S104, the spindle drive milling cutter is machined to groove the side wall of the casting blank, so that a hub for mounting the spindle is formed in the middle of the casting blank, and the web between the hub and the rim is hollowed out.
[0042] Based on S105, the heat treatment temperature is controlled at 550°.
[0043] Based on S106, the blasting mesh number is 40 mesh to 120 mesh.
[0044] Based on S107, the surface anti-rust treatment is phosphating blackening treatment.
[0045] In this embodiment, by preparing a mold for casting, the production efficiency of the pulley can be improved, so that the pulley can be produced in large quantities.
[0046] By reserving an annular protrusion for forming a belt groove at the rim of the pulley in the casting cavity of the mold, the casting material can be squeezed by the annular protrusion after being injected into the cavity, and the belt groove is formed at the edge of the blank after the casting material is cooled and shaped, thereby eliminating the subsequent machining steps, thereby further improving the production efficiency of the pulley.
[0047] By using gray cast iron to cast the pulley, the pulley can have good performance in absorbing vibration and impact during use. Gray cast iron also has good wear resistance and self-lubricating properties, which can effectively increase the service life of the pulley. At the same time, the production process of gray cast iron is relatively simple, and its production cost is low, which can effectively reduce the production cost of the pulley.
[0048] A pulley usually refers to a component used in a transmission system to transmit power through a belt. As the core component of the transmission system, the weight of the pulley has a very important impact on the energy efficiency of the entire system. The weight-reduced pulley requires less energy to operate, which directly reduces energy consumption and makes the entire transmission system more energy-efficient. For applications such as automobile engines, weight reduction can reduce fuel consumption, reduce emissions, and meet environmental protection requirements. Weight reduction can also reduce the centrifugal force generated by rotating parts at high speeds, reduce vibration and noise caused by imbalance, and thus improve operational safety. This is especially important for high-speed rotating mechanical equipment.
[0049] Therefore, the casting blank obtained after the gray cast iron is cast and cooled and shaped is installed on the chuck of the machine tool, and then the main shaft is used to buckle the side wall of the casting blank, so that the middle part of the casting blank forms a hub for installing the main shaft, and the web between the hub and the rim is hollowed out, which can effectively reduce the weight of the pulley. Weight reduction can not only reduce the weight of the product, but also reduce the amount of material used, thereby reducing production costs. At the same time, the hollow web can reduce the inertia moment during matrix transmission, improve transmission efficiency and running stability, and further improve the practicality of the pulley.
[0050] After the surface machining is completed, the casting blank already has the shape of a pulley, but its surface still has the remaining parting line during casting and the burrs generated during milling. Therefore, the surface of the semi-finished pulley needs to be sandblasted to facilitate the subsequent surface anti-rust treatment. In order to better improve the effect of sandblasting, the pulley needs to be heat treated first. The main purpose of heat treatment before sandblasting is to improve the performance of the workpiece material, extend its service life, and prepare good surface conditions for thermal spraying. Heat treatment can enhance its high temperature resistance by changing the internal structure of the material, so that it can remain stable during the subsequent thermal spraying process. In addition, heat treatment also helps to remove oxides and impurities on the surface of the material, activate the surface, and thus improve the bonding strength between the subsequent spray coating and the workpiece. This process helps to reduce the risk of coating peeling under harsh working conditions and ensure that the coating is more solid and durable. At the same time, in order to eliminate the residual stress of the casting, stabilize the geometric dimensions, reduce or eliminate the distortion caused by cutting, and improve the effect of sandblasting and subsequent anti-rust treatment, the semi-finished pulley needs to be heat treated first, and the heat treatment temperature is 550°. After the heat treatment is completed, sandblasting can be performed to remove impurities such as burrs and burrs on the surface.
[0051] The mesh number of sandblasting is 40-120 mesh, and the specific mesh number depends on the required surface treatment effect and the type of sandblasting abrasive. For example, 40 mesh is suitable for occasions where thicker coatings, rust need to be removed or surface roughness needs to be increased to improve coating adhesion. The abrasive grain size in this range is larger and has a strong impact force, which can quickly clean the surface, effectively improve the sandblasting efficiency of the pulley, and thus improve the production efficiency of the pulley. At the same time, 40 mesh sandblasting can also improve the coating adhesion, so that the final phosphating blackening treatment has a higher strength, thereby effectively improving the service life of the pulley. At the same time, the protective layer of the pulley after phosphating blackening will not fall off, which can effectively prevent rust, extend the service life, reduce the cost of use, and further improve the quality of the pulley; 80 mesh is a medium mesh number selection, suitable for general surface cleaning and sandblasting, which can remove light dirt, coating or rust on the surface and provide moderate surface roughness; 120 mesh has a smaller abrasive grain size, which is suitable for occasions where fine cleaning or high surface finish is required.
[0052] Embodiment 2:
[0053] The new shaping process for reducing the weight of a pulley blank disclosed in the present invention comprises the following steps:
[0054] S101, preparing a mold for casting;
[0055] S102, injecting the casting material into the mold, and waiting for cooling and shaping to be completed to obtain a casting blank;
[0056] S103, taking out the casting blank and mounting it on the chuck of the machine tool;
[0057] S104, machining the surface of the blank by a spindle to obtain a semi-finished pulley;
[0058] S105, removing the semi-finished pulley and performing heat treatment;
[0059] S106, performing surface sandblasting on the heat-treated semi-finished pulley;
[0060] S107, after the sandblasting is completed, the surface of the semi-finished pulley is subjected to rust prevention treatment.
[0061] Based on S101, an annular protrusion for forming a belt groove is reserved on the inner wall of the mold cavity at the rim of the pulley.
[0062] Based on S102, the casting material is grey cast iron.
[0063] Based on S104, the spindle drive milling cutter is machined to groove the side wall of the casting blank, so that a hub for mounting the spindle is formed in the middle of the casting blank, and the web between the hub and the rim is hollowed out.
[0064] Based on S105, the heat treatment temperature is controlled at 600°.
[0065] Based on S106, the blasting mesh number is 40 mesh to 120 mesh.
[0066] Based on S107, the surface anti-rust treatment is phosphating blackening treatment.
[0067] In this embodiment, since the heat treatment temperature of gray cast iron is different depending on the alloy components contained inside, when the gray cast iron is low-alloy gray cast iron, the mechanical properties of the pulley can be effectively improved, so that it has excellent strength and toughness, and the addition of alloys generally increases the tempering resistance of the material. Therefore, when the gray cast iron is low-alloy gray cast iron, the heat treatment temperature needs to be increased to 600°, which can be used to better ensure the heat treatment effect of the pulley.
[0068] Embodiment three:
[0069] The new shaping process for reducing the weight of a pulley blank disclosed in the present invention comprises the following steps:
[0070] S101, preparing a mold for casting;
[0071] S102, injecting the casting material into the mold, and waiting for cooling and shaping to be completed to obtain a casting blank;
[0072] S103, taking out the casting blank and mounting it on the chuck of the machine tool;
[0073] S104, machining the surface of the blank by a spindle to obtain a semi-finished pulley;
[0074] S105, removing the semi-finished pulley and performing heat treatment;
[0075] S106, performing surface sandblasting on the heat-treated semi-finished pulley;
[0076] S107, after the sandblasting is completed, the surface of the semi-finished pulley is subjected to rust prevention treatment.
[0077] Based on S101, an annular protrusion for forming a belt groove is reserved on the inner wall of the mold cavity at the rim of the pulley.
[0078] Based on S102, the casting material is grey cast iron.
[0079] Based on S104, the spindle drive milling cutter is machined to groove the side wall of the casting blank, so that a hub for mounting the spindle is formed in the middle of the casting blank, and the web between the hub and the rim is hollowed out.
[0080] Based on S105, the heat treatment temperature is controlled at 650°.
[0081] Based on S106, the blasting mesh number is 40 mesh to 120 mesh.
[0082] Based on S107, the surface anti-rust treatment is phosphating blackening treatment.
[0083] In this embodiment, by making the gray cast iron into high-alloy gray cast iron, the pulley can have extremely high strength and good corrosion resistance, so that the pulley can be used normally under some special environments, such as high temperature and high pressure, which can effectively improve the use range of the pulley. However, increasing the alloy content will further increase the heat treatment temperature. Therefore, the heat treatment temperature is controlled at 650° to ensure the heat treatment effect of the pulley.
[0084] Embodiment 4:
[0085] The new shaping process for reducing the weight of a pulley blank disclosed in the present invention comprises the following steps:
[0086] S101, preparing a mold for casting;
[0087] S102, injecting the casting material into the mold, and waiting for cooling and shaping to be completed to obtain a casting blank;
[0088] S103, taking out the casting blank and mounting it on the chuck of the machine tool;
[0089] S104, machining the surface of the blank by a spindle to obtain a semi-finished pulley;
[0090] S105, removing the semi-finished pulley and performing heat treatment;
[0091] S106, performing surface sandblasting on the heat-treated semi-finished pulley;
[0092] S107, after the sandblasting is completed, the surface of the semi-finished pulley is subjected to rust prevention treatment.
[0093] Based on S101, an annular protrusion for forming a belt groove is reserved on the inner wall of the mold cavity at the rim of the pulley.
[0094] Based on S102, the casting material is grey cast iron.
[0095] Based on S104, the spindle drive milling cutter is machined to groove the side wall of the casting blank, so that a hub for mounting the spindle is formed in the middle of the casting blank, and the web between the hub and the rim is hollowed out.
[0096] Based on S105, the heat treatment temperature is controlled at 550°.
[0097] Based on S106, the blasting mesh number is 40 mesh to 120 mesh.
[0098] Based on S107, the surface anti-rust treatment is paint treatment.
[0099] In this embodiment, when selecting the surface treatment method of the cast iron pulley, it is necessary to select the most appropriate method according to the specific use requirements, environmental conditions and cost considerations. Since the phosphating blackening treatment process is relatively complicated, including degreasing and rust removal, water cleaning, surface adjustment, phosphating, water cleaning, chromate treatment, drying, greasing or dyeing treatment and other steps, it will increase the production cost of the pulley to a certain extent and reduce the production efficiency of the pulley. For occasions that require long-term rust prevention and aesthetics, phosphating blackening treatment may be a better choice; for scenes that require short-term use or strict cost control, other more economical treatment methods can be considered. Therefore, the surface rust prevention treatment of the pulley is paint treatment, so that the pulley can effectively prevent rust, and at the same time provide a variety of color options, increase the appearance, and enhance the diversity of the pulley.
[0100] Embodiment five:
[0101] The new shaping process for reducing the weight of a pulley blank disclosed in the present invention comprises the following steps:
[0102] S101, preparing a mold for casting;
[0103] S102, injecting the casting material into the mold, and waiting for cooling and shaping to be completed to obtain a casting blank;
[0104] S103, taking out the casting blank and mounting it on the chuck of the machine tool;
[0105] S104, machining the surface of the blank by a spindle to obtain a semi-finished pulley;
[0106] S105, removing the semi-finished pulley and performing heat treatment;
[0107] S106, performing surface sandblasting on the heat-treated semi-finished pulley;
[0108] S107, after the sandblasting is completed, the surface of the semi-finished pulley is subjected to rust prevention treatment.
[0109] Based on S101, an annular protrusion for forming a belt groove is reserved on the inner wall of the mold cavity at the rim of the pulley.
[0110] Based on S102, the casting material is grey cast iron.
[0111] Based on S104, the spindle drive milling cutter is machined to groove the side wall of the casting blank, so that a hub for mounting the spindle is formed in the middle of the casting blank, and the web between the hub and the rim is hollowed out.
[0112] Based on S105, the heat treatment temperature is controlled at 550°.
[0113] Based on S106, the blasting mesh number is 40 mesh to 120 mesh.
[0114] Based on S107, the surface anti-rust treatment is surface spraying.
[0115] In this embodiment, by spraying the surface of the pulley for rust prevention, the surface of the pulley can be provided with different materials, the properties of the surface of the pulley can be changed, and the rust prevention performance of the pulley can be improved. At the same time, the surface spraying can also increase the friction coefficient of the pulley, improve the corrosion resistance and wear resistance of the pulley, and effectively improve the practicality of the pulley.
[0116] Embodiment six:
[0117] The new shaping process for reducing the weight of a pulley blank disclosed in the present invention comprises the following steps:
[0118] S101, preparing a mold for casting;
[0119] S102, injecting the casting material into the mold, and waiting for cooling and shaping to be completed to obtain a casting blank;
[0120] S103, taking out the casting blank and mounting it on the chuck of the machine tool;
[0121] S104, machining the surface of the blank by a spindle to obtain a semi-finished pulley;
[0122] S105, removing the semi-finished pulley and performing heat treatment;
[0123] S106, performing surface sandblasting on the heat-treated semi-finished pulley;
[0124] S107, after the sandblasting is completed, the surface of the semi-finished pulley is subjected to rust prevention treatment.
[0125] Based on S101, an annular protrusion for forming a belt groove is reserved on the inner wall of the mold cavity at the rim of the pulley.
[0126] Based on S102, the casting material is grey cast iron.
[0127] Based on S104, the spindle drive milling cutter is machined to groove the side wall of the casting blank, so that a hub for mounting the spindle is formed in the middle of the casting blank, and the web between the hub and the rim is hollowed out.
[0128] Based on S105, the heat treatment temperature is controlled at 550°.
[0129] Based on S106, the blasting mesh number is 40 mesh to 120 mesh.
[0130] Based on S107, the surface anti-rust treatment is electroplating.
[0131] In this embodiment, by electroplating the surface of the pulley, a dense metal film can be formed on the surface of the pulley to improve the corrosion resistance of the metal. At the same time, the thickness of the electroplating can be controlled, which is suitable for fields that require precise control of the coating thickness and can improve the specificity of the pulley.
[0132] Embodiment seven:
[0133] The new shaping process for reducing the weight of a pulley blank disclosed in the present invention comprises the following steps:
[0134] S101, preparing a mold for casting;
[0135] S102, injecting the casting material into the mold, and waiting for cooling and shaping to be completed to obtain a casting blank;
[0136] S103, taking out the casting blank and mounting it on the chuck of the machine tool;
[0137] S104, machining the surface of the blank by a spindle to obtain a semi-finished pulley;
[0138] S105, removing the semi-finished pulley and performing heat treatment;
[0139] S106, performing surface sandblasting on the heat-treated semi-finished pulley;
[0140] S107, after the sandblasting is completed, the surface of the semi-finished pulley is subjected to rust prevention treatment.
[0141] Based on S101, an annular protrusion for forming a belt groove is reserved on the inner wall of the mold cavity at the rim of the pulley.
[0142] Based on S102, the casting material is ductile iron.
[0143] Based on S104, the spindle drive milling cutter is machined to groove the side wall of the casting blank, so that a hub for mounting the spindle is formed in the middle of the casting blank, and the web between the hub and the rim is hollowed out.
[0144] Based on S105, the heat treatment temperature is controlled at 840°.
[0145] Based on S106, the blasting mesh number is 40 mesh to 120 mesh.
[0146] Based on S107, the surface anti-rust treatment is electroplating.
[0147] In this embodiment, among the various production materials, there are many materials that are only slightly different in structure but have very different functions and uses. For example, ductile iron is stronger than cast iron, but its corrosion resistance is the same. Compared with cast steel, their strengths are comparable, but ductile iron has better corrosion resistance and oxidation resistance, and its cost is also lower.
[0148] Therefore, using ductile iron as the material of the pulley can make the pulley have better strength and further improve the quality of the pulley. By setting the heat treatment temperature of ductile iron to 840° and the tempering temperature after quenching to 550-600°C, the pulley can obtain tempered troostite structure, improve the comprehensive mechanical properties, further improve the strength of the pulley, and thus further improve the quality of the pulley.
[0149] Embodiment eight:
[0150] The new shaping process for reducing the weight of a pulley blank disclosed in the present invention comprises the following steps:
[0151] S101, preparing a mold for casting;
[0152] S102, injecting the casting material into the mold, and waiting for cooling and shaping to be completed to obtain a casting blank;
[0153] S103, taking out the casting blank and mounting it on the chuck of the machine tool;
[0154] S104, machining the surface of the blank by a spindle to obtain a semi-finished pulley;
[0155] S105, removing the semi-finished pulley and performing heat treatment;
[0156] S106, performing surface sandblasting on the heat-treated semi-finished pulley;
[0157] S107, after the sandblasting is completed, the surface of the semi-finished pulley is subjected to rust prevention treatment.
[0158] Based on S101, an annular protrusion for forming a belt groove is reserved on the inner wall of the mold cavity at the rim of the pulley.
[0159] Based on S102, the casting material is ductile iron.
[0160] Based on S104, the spindle drive milling cutter is machined to groove the side wall of the casting blank, so that a hub for mounting the spindle is formed in the middle of the casting blank, and the web between the hub and the rim is hollowed out.
[0161] Based on S105, the heat treatment temperature is controlled at 860°.
[0162] Based on S106, the blasting mesh number is 40 mesh to 120 mesh.
[0163] Based on S107, the surface anti-rust treatment is electroplating.
[0164] In this embodiment, by setting the heat treatment temperature of the ductile iron pulley to 860° and adding the tempering process at 500-600°C, pearlite + a small amount of dispersed ferrite structure is obtained, thereby obtaining better comprehensive mechanical properties, further improving the strength of the pulley, expanding the range of high-pressure application scenarios of the pulley, and further improving the practicability of the pulley.
[0165] Embodiment nine:
[0166] The new shaping process for reducing the weight of a pulley blank disclosed in the present invention comprises the following steps:
[0167] S101, preparing a mold for casting;
[0168] S102, injecting the casting material into the mold, and waiting for cooling and shaping to be completed to obtain a casting blank;
[0169] S103, taking out the casting blank and mounting it on the chuck of the machine tool;
[0170] S104, machining the surface of the blank by a spindle to obtain a semi-finished pulley;
[0171] S105, removing the semi-finished pulley and performing heat treatment;
[0172] S106, performing surface sandblasting on the heat-treated semi-finished pulley;
[0173] S107, after the sandblasting is completed, the surface of the semi-finished pulley is subjected to rust prevention treatment.
[0174] Based on S101, an annular protrusion for forming a belt groove is reserved on the inner wall of the mold cavity at the rim of the pulley.
[0175] Based on S102, the casting material is ductile iron.
[0176] Based on S104, the spindle drive milling cutter is machined to groove the side wall of the casting blank, so that a hub for mounting the spindle is formed in the middle of the casting blank, and the web between the hub and the rim is hollowed out.
[0177] Based on S105, the heat treatment temperature is controlled at 880°.
[0178] Based on S106, the blasting mesh number is 40 mesh to 120 mesh.
[0179] Based on S107, the surface anti-rust treatment is electroplating.
[0180] In this embodiment, by setting the heat treatment temperature of ductile iron to 880° and the tempering process temperature to 500-600°C, the ductile iron can obtain pearlite + a small amount of ferrite + spheroidal graphite, thereby improving the strength, hardness and wear resistance, further reducing the wear of the pulley during use, and increasing the life of the pulley, thereby further improving the practicability of the pulley.
[0181] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A new process for reducing the weight of a pulley blank includes the following steps: S101, preparing a mold for casting; S102, injecting the casting material into the mold, and waiting for cooling and shaping to be completed to obtain a casting blank; S103, taking out the casting blank and mounting it on the chuck of the machine tool; S104, machining the surface of the blank by a spindle to obtain a semi-finished pulley; S105, removing the semi-finished pulley and performing heat treatment; S106, performing surface sandblasting on the heat-treated semi-finished pulley; S107, after the sandblasting is completed, the surface of the semi-finished pulley is subjected to rust prevention treatment.
2. The new process for reducing the weight of pulley blank according to claim 1 is characterized in that: Based on S101, an annular protrusion for forming a belt groove is reserved on the inner wall of the mold cavity at the rim of the pulley.
3. The new process for reducing the weight of pulley blank according to claim 1 is characterized in that: Based on S102, the casting material is grey cast iron or ductile iron.
4. The new process for reducing the weight of pulley blank according to claim 1 is characterized in that: Based on S104, the spindle drive milling cutter is machined to groove the side wall of the casting blank, so that a hub for mounting the spindle is formed in the middle of the casting blank, and the web between the hub and the rim is hollowed out.
5. The new shaping process for reducing the weight of pulley blank according to claim 3 is characterized in that: Based on S105, the heat treatment temperature is controlled at 550°~650°.
6. The new process for reducing the weight of pulley blank according to claim 3 is characterized in that: Based on S105, the heat treatment temperature is controlled at 840°~880°.
7. The new process for reducing the weight of pulley blank according to claim 1 is characterized in that: Based on S106, the blasting mesh number is 40 mesh to 120 mesh.
8. The new process for reducing the weight of pulley blank according to claim 1 is characterized in that: Based on S107, the surface anti-rust treatment is phosphating blackening treatment, paint treatment, surface spraying and electroplating.