Crude oil demetallization method, and pre-removal agent and demetallization agent used in method

Through the combination of pre-removing agent A and demetallic agent B, the chelation reaction and electrodesalting reaction are used to solve the problems of low removal efficiency and equipment corrosion of different types of metals and existing forms in the prior art, and achieve high efficiency, Low-cost crude oil metal removal.

CN119081731APending Publication Date: 2024-12-06NANJING PETRO-CHEM CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
CN202411452688.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-17
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

The existing crude oil demetalization technology is difficult to efficiently remove different types of metals and their existing forms, and it is easy to cause equipment corrosion and low removal efficiency.

Method used

Using the combination method of pre-removing agent A and demetallic agent B, the pre-removing agent A consists of a chelating agent and acrylic maleic acid copolymer. Through the chelating reaction and electrodesalting reaction, stable chelating and acidification washing are formed. Detachment, inhibits metal precipitation and conversion into water-soluble metals, and surfactants increase contact between water and oil, promotes metals to enter the aqueous phase, and achieves efficient removal.

Benefits of technology

It improves the removal efficiency of metals such as calcium and iron, improves the electrodesalting environment, reduces equipment corrosion, and achieves efficient removal of different types of metals.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

The invention discloses a crude oil demetallization method which comprises the following steps: (1) pretreating crude oil to remove moisture in the crude oil; (2) a pre-removal agent A is added into the crude oil with moisture removed in the step (1), mixing and heating are carried out, a reaction is carried out, and the pre-removal agent A is composed of a chelating agent and an acrylic acid-maleic acid copolymer; and (3) after the reaction in the step (2) is finished, a demetallization agent B and electro-desalting water are added, the temperature is raised, an electro-desalting reaction is carried out, crude oil with metal removed is obtained, and the demetallization agent B is composed of water-soluble organic acid and a surfactant. By adopting the method, various metals can be removed, the demetallization rate is improved, and the problem of equipment corrosion in the demetallization process is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of petroleum demetallization, in particular to a method for demetallizing crude oil and a pre-demetallizing agent and a demetallizing agent used in the method. Background Art

[0002] Chelation demetallization technology primarily removes petroleum salts dissolved in the oil phase, including a range of carboxylates such as fatty acids, cyclohexane salts, and aromatic salts. Chelation demetallization technology removes metal elements originally dissolved in the oil phase by adding a suitable demetallizing agent, displacing them in the aqueous phase. Appropriate methods are then employed to separate the oil and water to achieve the desired metal removal. Chelation demetallization is often used in conjunction with electro-desalting demetallization methods, effectively removing water-soluble inorganic and oil-soluble organic salts from oil samples with minimal changes to experimental equipment. This technology, with its low investment and high effectiveness, has attracted widespread attention from researchers.

[0003] Crude oil contains a high content of metal elements and their occurrence states vary. Any single removal technology has certain limitations. Therefore, for crude oil, the multiple demetallization technologies introduced above can be used in combination according to its properties to remove metal elements efficiently, environmentally friendly and at low cost, providing crude oil raw materials that meet the requirements for subsequent processing.

[0004] Existing crude oil demetallization agents and their use methods are difficult to target different types of metals in their different forms, and the removal efficiency is low. Therefore, for the crude oil demetallization process, it is very necessary to develop an efficient, low-cost removal method that can target different types of metals and their different forms. Summary of the Invention

[0005] In order to solve the problems of low demetallization efficiency in crude oil demetallization technology, the existing crude oil demetallization technology can only remove a single type of metal and is prone to corrosion of equipment, the present invention provides a method for crude oil demetallization and a pre-demetallization agent and a demetallization agent used in the method.

[0006] The technical solution adopted by the present invention is: a method for demetallizing crude oil, comprising the following steps: (1) Pre-treat the crude oil to remove water from it; (2) adding a pre-removal agent A to the crude oil from which water has been removed in step (1), mixing and heating, and reacting, wherein the pre-removal agent A is composed of a chelating agent and an acrylic acid-maleic acid copolymer; (3) After the reaction in step (2) is completed, a demetallizing agent B and electro-desalting water are added, and the temperature is raised to carry out electro-desalting reaction to obtain crude oil after metal removal, wherein the demetallizing agent B is composed of a water-soluble organic acid and a surfactant.

[0007] The above technical solution pre-treats the crude oil to remove most of the water-soluble calcium and iron in the crude oil, thereby preventing the water-soluble metal salts in the crude oil from excessively consuming the chelating agent component in the pre-removal agent A, resulting in low metal removal efficiency. Then, the pre-removal agent A containing a chelating agent is added at an appropriate temperature to carry out a chelation reaction with the metal petroleum salt and porphyrin metal to form a strong chelate, inhibiting metal precipitation in the crude oil, thereby removing metal substances in the crude oil and improving the electro-desalting environment. In addition, the acrylic acid maleic acid copolymer in the pre-removal agent A also has a certain corrosion inhibition effect and can also effectively reduce equipment corrosion. Finally, the demetallizing agent B and electro-desalting water are added, and the organic acid and surfactant in the demetallizing agent B are acidified and eluted under an electric field to further remove the metal substances in the crude oil. The demetallizing agent B can acidify the chelate before heating to convert it into water-soluble metal. The surfactant can increase the contact between water and oil and perform a certain degree of phase transfer on the water-soluble metal, helping the metal to enter the water phase. Finally, under the electro-desalting reaction, the water-soluble metal is eluted and discharged with the electro-desalting water to achieve the metal removal effect.

[0008] Preferably, the pretreatment step in step (1) is specifically as follows: adding a demulsifier with a mass concentration of 20 ppm to the crude oil, specifically using a demulsifier model NS-80 from Jinpu New Materials Company, mixing and standing for 24 hours to allow the crude oil and water to separate.

[0009] Preferably, the ratio of the pre-removal agent A in step (2) to the sum of the mass of calcium and iron in the crude oil is 1-1.5:1.

[0010] Preferably, in step (2), after adding the pre-removing agent A, the temperature is raised to 50-60° C. and the reaction is carried out for 30 minutes.

[0011] Since the chelating agent and its chelate product in the pre-removing agent A have poor stability at high temperatures, setting the above temperature can prevent the chelating agent component from directly entering the high temperature environment of the electric desalting tank, and setting the above reaction time can allow it to fully mix and react.

[0012] Preferably, the ratio of the demetallizing agent B in step (3) to the sum of the mass of calcium and iron in the crude oil is 1.2-1.5:1.

[0013] Preferably, the temperature of the electrical desalination reaction in step (3) is 130-140° C., and the reaction time is 20 minutes.

[0014] The present application also provides a pre-removal agent A used in a method for demetallizing crude oil, comprising the following components in parts by weight: 60 parts of a chelating agent, 40 parts of an acrylic acid-maleic acid copolymer; Among them, the chelating agent is selected from one or more mixtures of ethylenediaminetetraacetic acid, nitrilotriacetic acid, diethylenetriaminepentaacetic acid, hydroxyethylidene diphosphonic acid or aminotrimethylenephosphonic acid; the acrylic acid maleic acid copolymer is a copolymerization product of acrylic acid and maleic acid, wherein the mass fraction of maleic acid is 30%.

[0015] Preferably, the preparation method is as follows: dissolving the chelating agent and acrylic acid-maleic acid copolymer in an alkaline solution free of metal elements, and mixing the mixture under alkaline conditions.

[0016] The present application also provides a demetallization agent B used in a method for demetallization of crude oil, comprising the following components in parts by weight: 85-90 parts of a water-soluble organic acid, 10-15 parts of a surfactant; The water-soluble organic acid is selected from one or more mixtures of acetic acid, glycolic acid, citric acid, malic acid or lactic acid; and the surfactant is selected from one or a mixture of sulfonated polybutadiene or dodecylbenzenesulfonic acid.

[0017] Preferably, the preparation method is: dissolving a water-soluble organic acid and a surfactant in deionized water.

[0018] Beneficial effects of the present invention: The crude oil demetallization method of the present application can simultaneously chelate and remove calcium and iron, which are difficult to remove from crude oil, with high removal efficiency. At the same time, it can improve the electro-desalting environment and reduce equipment corrosion. The chelating agent in the pre-removal agent A can react with the metal ions in the crude oil to form a chelate complex, inhibiting metal precipitation in the crude oil and improving the electro-desalting environment. The acrylic acid-maleic acid copolymer in the pre-removal agent A has a certain corrosion inhibition effect and can also effectively reduce equipment corrosion. The organic acid in the demetallization agent B is used to acidify the chelate product and convert it into a water-soluble metal. The surfactant increases the contact between water and oil and can perform a certain degree of phase transfer, helping the metal enter the water phase and be removed with the water. DETAILED DESCRIPTION

[0019] In order to make the purpose, technical solutions and advantages of the present invention more clear, the technical solutions of the present invention will be clearly and completely described below in conjunction with preferred implementation methods.

[0020] The crude oil in the following examples was demetallized using a crude oil having a calcium content of 15 ppm and an iron content of 12 ppm; the mass fraction of the maleic acid copolymer in the acrylic acid-maleic acid copolymer used in the following pre-removal agent was 30%. Example 1.

[0021] The components of pre-stripping agent A are as follows: 60 parts of ethylenediaminetetraacetic acid 40 parts of acrylic acid maleic acid copolymer The components of demetallizing agent B are as follows: 35 parts of acetic acid 55 parts of lactic acid 10 parts of dodecylbenzenesulfonic acid The preparation method of pre-removal agent A is as follows: ethylenediaminetetraacetic acid and acrylic acid maleic acid copolymer are mixed and stirred, ammonia water is slowly added to the pH value to 7, and stirred until completely dissolved; The preparation method of demetallizing agent B is as follows: first add deionized water, start stirring, then add acetic acid, lactic acid and dodecylbenzenesulfonic acid, and stir until completely dissolved.

[0022] The steps for crude oil demetallization are as follows: (1) Pretreatment step: Add 20 ppm of Jinpu New Material NS-80 to the crude oil, mix and let it stand for 24 hours to allow the crude oil and water to separate.

[0023] (2) Add pre-removal agent A to the pretreated crude oil, heat the mixture to 55°C, and keep warm for 30 minutes; (3) After the reaction is completed, demetallization agent B and electro-desalting water are added, and electro-desalting is carried out at 135°C with a residence time of 20 minutes to obtain the crude oil after metal removal.

[0024] The ratio of the mass of the pre-removal agent A to the sum of the mass of calcium and iron in the crude oil is 1.2:1, and the ratio of the mass of the demetallization agent B to the sum of the mass of calcium and iron in the crude oil is 1.3:1. The metal removal rates are shown in Table 1.

[0025] Example 2: Compared with Example 1, the differences are that the mixing temperature in step (2) is 50°C, and the temperature of the electrical desalting reaction in step (3) is reduced to 130°C; the ratio of the mass of the pre-removing agent A to the sum of the mass of calcium and iron in the crude oil is 1:1, and the ratio of the mass of the demetallizing agent B to the sum of the mass of calcium and iron in the crude oil is 1.2:1. The metal removal rates are shown in Table 1.

[0026] Example 3: Compared with Example 1, the difference is that the mixing temperature in step (2) is 60°C, and the electro-desalting reaction temperature in step (3) is 140°C. The ratio of the mass of the pre-removal agent A to the sum of the mass of calcium and iron in the crude oil is 1.5:1, and the ratio of the mass of the demetallization agent B to the sum of the mass of calcium and iron in the crude oil is also 1.5:1. The metal removal rates are shown in Table 1.

[0027] Example 4: The components of pre-stripping agent A are as follows: 40 parts of ethylenediaminetetraacetic acid 20 parts of hydroxyethylidene diphosphonic acid 40 parts of acrylic acid maleic acid copolymer The components of demetallizing agent B are as follows: 35 parts of acetic acid 55 parts of lactic acid 10 parts of dodecylbenzenesulfonic acid Compared with Example 1, only the composition of the pre-removing agent A and the demetallizing agent B is different. The metal removal rates are shown in Table 1.

[0028] Example 5: The components of pre-stripping agent A are as follows: 20 parts of ethylenediaminetetraacetic acid 20 parts of nitrilotriacetic acid 20 parts of diethylenetriaminepentaacetic acid 40 parts of acrylic acid maleic acid copolymer The components of demetallizing agent B are as follows: 35 parts of acetic acid 55 parts of lactic acid 10 parts of dodecylbenzenesulfonic acid Compared with Example 1, only the composition of the pre-removing agent A and the demetallizing agent B is different. The metal removal rates are shown in Table 1.

[0029] Example 6: The components of pre-stripping agent A are as follows: 20 parts of ethylenediaminetetraacetic acid 20 parts of nitrilotriacetic acid 20 parts of diethylenetriaminepentaacetic acid 40 parts of acrylic acid maleic acid copolymer The components of demetallizing agent B are as follows: 15 parts of glycolic acid 35 parts of citric acid 35 parts of malic acid 8 parts of dodecylbenzenesulfonic acid 7 parts of sulfonated polybutadiene Compared with Example 1, only the composition of the pre-removing agent A and the demetallizing agent B is different. The metal removal rates are shown in Table 1.

[0030] Example 7: The components of pre-stripping agent A are as follows: 40 parts of hydroxyethylidene diphosphonic acid 20 parts of aminotrimethylenephosphonic acid 40 parts of acrylic acid maleic acid copolymer The components of demetallizing agent B are as follows: 35 parts of acetic acid 55 parts of lactic acid 10 parts of dodecylbenzenesulfonic acid Compared with Example 1, only the composition of the pre-removing agent A and the demetallizing agent B is different. The metal removal rates are shown in Table 1.

[0031] Comparative Example 1 Compared with Example 1, the difference is that the pre-removal agent A is not added. The metal removal rate is shown in Table 1.

[0032] Table 1 shows the metal removal rates of the examples and comparative examples.

[0033] It can be seen from the data of Example 1 and Comparative Example 1 in Table 1 that the iron removal rate and calcium removal rate are significantly reduced without the addition of pre-removal agent A. Therefore, the addition of pre-removal agent A is very important for improving the efficiency of iron removal and calcium removal. It can be seen from the data of the embodiment in Table 1 that the method of the present application has high removal efficiency and can remove calcium and iron elements at the same time.

[0034] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principles of the present invention. These improvements and modifications are also within the scope of protection of the present invention.

Claims

1. A method for demetallizing crude oil, characterized in that: The following steps are involved: (1) Pre-treat the crude oil to remove water from it; (2) adding a pre-removal agent A to the crude oil from which water is removed in step (1), mixing and heating, and reacting, wherein the pre-removal agent A is composed of a chelating agent and an acrylic acid-maleic acid copolymer; (3) After the reaction in step (2) is completed, a demetallizing agent B and electro-desalting water are added, and the temperature is raised to carry out electro-desalting reaction to obtain crude oil after metal removal, wherein the demetallizing agent B is composed of a water-soluble organic acid and a surfactant.

2. The method for demetallizing crude oil according to claim 1, characterized in that: The pretreatment step in step (1) is specifically as follows: adding a demulsifier with a mass concentration of 20 ppm to the crude oil, mixing and standing for 24 hours to allow the crude oil and water to separate.

3. The method for demetallizing crude oil according to claim 1, characterized in that: The ratio of the pre-removal agent A in step (2) to the sum of the mass of calcium and iron in the crude oil is 1-1.5:

1.

4. The method for demetallizing crude oil according to claim 1, characterized in that: After adding the pre-removing agent A in step (2), the temperature is raised to 50-60°C and the reaction is carried out for 30 minutes.

5. The method for demetallizing crude oil according to claim 1, characterized in that: The ratio of the demetallizing agent B in step (3) to the sum of the mass of calcium and iron in the crude oil is 1.2-1.5:

1.

6. The method for demetallizing crude oil according to claim 1, characterized in that: The temperature of the electrical desalination reaction in step (3) is 130-140°C and the reaction time is 20 minutes.

7. A pre-removal agent A used in the method according to claim 1, characterized in that: The invention comprises the following components in parts by weight: 60 parts of a chelating agent, 40 parts of an acrylic acid-maleic acid copolymer; The chelating agent is selected from one or more mixtures of ethylenediaminetetraacetic acid, nitrilotriacetic acid, diethylenetriaminepentaacetic acid, hydroxyethylidene diphosphonic acid or aminotrimethylenephosphonic acid; the acrylic acid maleic acid copolymer is composed of the copolymerization product of acrylic acid and maleic acid, wherein the mass fraction of the maleic acid copolymer is 30%.

8. The pre-removal agent A according to claim 7, characterized in that The preparation method is as follows: a chelating agent and an acrylic acid-maleic acid copolymer are added into an alkaline solution without metal elements to dissolve the mixture, and the mixture is mixed under alkaline conditions.

9. A demetallizing agent B used in the method according to claim 1, characterized in that: The invention comprises the following components in parts by weight: 85-90 parts of a water-soluble organic acid, and 10-15 parts of a surfactant; The water-soluble organic acid is selected from one or more mixtures of acetic acid, glycolic acid, citric acid, malic acid or lactic acid; the surfactant is selected from one or a mixture of sulfonated polybutadiene or dodecylbenzene sulfonic acid.

10. The demetallizing agent B according to claim 7, characterized in that: The preparation method is as follows: water-soluble organic acid and surfactant are added into deionized water and dissolved.

Citation Information

Patent Citations

  • Composite metal remover used for hydrocarbon oil and method for removing metal

    CN101085932A

  • Method for removing metal in hydrocarbon oil

    CN102443422A

  • Composite demetalization agent and preparation method thereof

    CN103146417A

  • Method for removing metals from crude oil

    CN103146421A

  • Processing method of acid-containing crude oil

    CN103320160A