Novel FOWLP process AOP packaging body and packaging method
Through the new FOWLP process AOP packaging method, the chip offset problem caused by the thermal expansion coefficient of the material during the packaging process is solved, and the signal transmission efficiency and stability are improved through the mosquito-coil copper coil design, achieving high-performance and high-reliability packaging Effect.
Patent Information
- Application Number
- CN202411016153.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-27
- Publication Date
- 2024-12-06
AI Technical Summary
The existing FOWLP process leads to chip offset due to different thermal expansion coefficients of materials during packaging, and the AiP technology has limited packaging size and complex production, making it difficult to meet the needs of efficient and reliable packaging.
The new FOWLP process AOP packaging method is adopted, including first rewiring, electroplating copper needle, degluing crystal, plastic sealing, plastic sealing, plastic sealing and second rewiring, and signal transmission efficiency and stability are improved through the mosquito-coil copper coil design.
It significantly improves the quality of the through hole and packaging yield, increases the signal transmission path, improves the signal transmission efficiency and stability, and achieves high performance and high reliability packaging effects.
Smart Images

Figure CN119092415A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of AOP packaging, and in particular relates to a novel FOWLP process AOP packaging body and a packaging method. Background Art
[0002] The core component of wireless communication and detection technology is the antenna. Antennas can be manufactured independently or in an integrated manner. Independent antennas include metal structures, ceramic chips, and metallized molded parts. Integrated antennas include antenna on chip (AoC) and packaged antenna technology (AiP). AoC technology integrates the antenna with other circuits in the back-end process of the chip, while AiP technology integrates the antenna of the radio or radar module into a standard surface-mounted device.
[0003] Although AoC technology integrates antennas and other circuits in a package, it is limited by the consistency of semiconductor process technology, resulting in cost and performance that are difficult to meet the needs of a wide range of applications. On the other hand, AiP technology improves the integration of the package by placing the chip as close to the antenna as possible, but the package size is still affected and the manufacturing process is more complicated.
[0004] At present, the AiP process mainly uses three technologies: LTCC (low temperature co-fired ceramic), HDI (high density interconnect) and FOWLP (fan-out wafer level packaging). Unlike LTCC and HDI processes, the FOWLP process does not require multiple stacked dielectrics, but is achieved by using molding compounds, redistribution layers (RDL) and dielectric layers. The FOWLP process with TMV (through-hole vertical interconnect) structure can achieve high I / O port density, small pitch and better package size. However, due to the different coefficients of thermal expansion (CTE) of the materials, the chip may be offset during the packaging process. Summary of the invention
[0005] In view of the above situation, in order to overcome the defects of the prior art, the present invention aims to overcome the defects of the prior art through a novel FOWLP process AOP packaging method to achieve a more efficient and reliable packaging effect.
[0006] In order to achieve the above object, the following technical solution is adopted: The present invention provides a novel FOWLP process AOP packaging method, comprising the following steps:
[0007] S1, first rewiring: set the first rewiring layer on the Release layer;
[0008] S2, electroplating copper needles: electroplating copper needles on the first redistribution layer, and coating the surface of the first redistribution layer with photoresist;
[0009] S3, debonding and wafer bonding: removing the photoresist on the surface of the first redistribution layer and bonding the wafer;
[0010] S4, plastic encapsulation: plastic encapsulation is performed on the surface of the first redistribution layer using epoxy resin plastic encapsulation material;
[0011] S5, plastic sealing polishing: polish and thin the plastic sealing material to expose the copper needle;
[0012] S6. Second redistribution: setting a second redistribution layer on the copper needles.
[0013] Furthermore, the step S6 specifically includes: after the copper needle is led out from the second rewiring layer, sputtering is started, photolithography coating, exposure, and development are performed, and after the window is opened, electroplating of the copper coil is started, and after electroplating, the glue is removed, etching is performed, and then a layer of plastic sealing glue is used to encapsulate, and finally polishing is performed to expose the copper coil.
[0014] Furthermore, the copper coil is of mosquito coil type.
[0015] Furthermore, the novel FOWLP process AOP package is packaged according to the novel FOWLP process AOP packaging method.
[0016] The beneficial effects of the present invention are:
[0017] (1) The present invention improves the TMV technology in the AiP package and uses general technology to change the process, effectively reducing the generation of voids in the through-holes, so that the quality of the through-holes is significantly improved, thereby significantly improving the overall yield of the package;
[0018] (2) Changing the antenna layout from the traditional patch type to the mosquito coil type increases the signal transmission path. This design not only amplifies the signal and improves the signal transmission efficiency, but also makes the signal more stable during transmission. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a schematic diagram of the process flow of the novel FOWLP process AOP package and packaging method of the present invention;
[0020] Figure 2 It is a schematic diagram of the specific process flow of the second rewiring of the novel FOWLP process AOP package and packaging method of the present invention.
[0021] The accompanying drawings are used to provide further understanding of the present invention and constitute a part of the specification. They are used to explain the present invention together with the embodiments of the present invention and do not constitute a limitation of the present invention.
[0022] Legend: 1. Substrate layer; 2. Release layer; 3. First redistribution layer; 4. Photoresist; 5. Copper needle; 6. Wafer; 7. Epoxy resin molding compound; 8. Second redistribution layer; 9. Copper pad; 10. Copper coil. DETAILED DESCRIPTION
[0023] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0024] Unless otherwise defined, all professional and scientific terms used herein have the same meanings as those familiar to those skilled in the art. In addition, any methods and materials similar or equivalent to those described herein may be applied to the present invention. The preferred implementation methods and materials described herein are for demonstration purposes only and are not intended to limit the content of this application.
[0025] Example
[0026] New FOWLP process AOP package and packaging method
[0027] According to the attached Figure 1 , the packaging method comprises the following steps:
[0028] S1, first rewiring: set the first rewiring layer on the Release layer;
[0029] First, the circuit pattern needs to be accurately made on the Release layer, and the photoresist is evenly coated on the Release layer. Then, the required circuit pattern is formed through mask alignment and exposure. Subsequently, the unexposed photoresist is removed through development to expose the copper or other conductive materials at the bottom layer. Finally, the exposed conductive material part is removed through the etching process to form the first redistribution layer.
[0030] S2, electroplating copper needles: electroplating copper needles on the first redistribution layer, and coating the surface of the first redistribution layer with photoresist;
[0031] First, the first redistribution layer is cleaned and activated to ensure the uniformity and adhesion of the electroplated layer. Then, the activated redistribution layer is immersed in an electroplating solution containing copper ions. The copper layer is deposited on the redistribution layer through the action of electric current to form the required copper needle structure. After the electroplating is completed, it is cleaned and passivated to prevent the copper needle from oxidation.
[0032] S3, debonding and wafer bonding: removing the photoresist on the surface of the first redistribution layer and bonding the wafer;
[0033] First, use an appropriate solvent or chemical method to remove the photoresist on the surface of the first redistribution layer to expose the copper pins. Then, the wafer is bonded to the copper pins, usually using a heat-curing or light-curing adhesive. During the bonding process, the pressure and temperature need to be precisely controlled to ensure a firm bond between the wafer and the copper pins.
[0034] S4, plastic encapsulation: plastic encapsulation is performed on the surface of the first redistribution layer using epoxy resin plastic encapsulation material;
[0035] Before plastic sealing, the bonded wafers need to be cleaned to remove impurities that may affect the quality of plastic sealing. Then, the epoxy resin plastic sealing material is evenly coated on the surface of the wafer and cured by heating or ultraviolet light to form a solid plastic sealing layer. The plastic sealing layer not only provides mechanical protection, but also has good electrical insulation performance and environmental isolation effect.
[0036] S5, plastic sealing polishing: polish and thin the plastic sealing material to expose the copper needle;
[0037] After the plastic sealing is completed, the plastic sealing polishing operation is carried out. First, the plastic sealing layer is initially polished with coarse abrasives to remove excess plastic sealing materials, gradually approaching the position of the copper needle, and then fine abrasives are used for fine polishing until the copper needle is completely exposed. During the polishing process, the grinding depth and speed need to be precisely controlled to avoid damaging the copper needle and the circuit structure below. After the polishing is completed, cleaning and surface treatment are carried out to remove the debris and damage generated during the polishing process;
[0038] S6. Second redistribution: A second redistribution layer is set on the copper needle to obtain a new FOWLP process AOP package. A second redistribution layer is set on the copper needle to obtain a new FOWLP process AOP package. This step is the final link in the packaging process. Through sophisticated circuit design and wiring, high performance and high reliability of the package are achieved.
[0039] According to the attached Figure 2 The step S6 specifically includes: after the copper needle is led out from the second rewiring layer, sputtering is started, photolithography coating, exposure, and development are performed, and after the window is opened, electroplating of the copper coil is started, and after electroplating, the adhesive is removed, etching is performed, and then a layer of plastic sealing adhesive is used for encapsulation, and finally polishing is performed to expose the copper coil.
[0040] The copper needle lead-out is specifically as follows: the copper needle is led out from the second redistribution layer to prepare for subsequent sputtering and electroplating;
[0041] Sputtering is specifically as follows: sputtering is performed on the surface of the copper needle to increase its conductivity and corrosion resistance;
[0042] Photolithography coating, exposure, and development are specifically: accurately forming circuit patterns through photolithography technology to ensure the accuracy and consistency of the circuit;
[0043] The electroplating copper coil specifically includes: electroplating on the copper needle after the window is opened to form the required copper coil;
[0044] The specific process of photoresist stripping and etching is to remove excess photoresist and form precise circuit patterns through etching technology;
[0045] Plastic encapsulation specifically includes: encapsulating the circuit with a layer of plastic encapsulation to enhance the protection performance of the package;
[0046] Grinding to expose the copper coil is specifically as follows: Grinding is performed at the end to ensure that the copper coil is exposed to facilitate subsequent circuit connection and testing.
[0047] According to the attached Figure 2 The copper coil is mosquito coil type. This unique layout not only increases the signal transmission path and improves the signal transmission efficiency, but also effectively reduces the interference of external signals and improves the reliability of communication. Through these delicate operation steps, the new FOWLP process AOP packaging method achieves high performance and high reliability of the package, providing strong technical support for the development of wireless communication and detection equipment.
[0048] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
[0049] The present invention and its implementation methods are described above, which is not restrictive. The drawings are only one of the implementation methods of the present invention, and the actual application is not limited thereto. In short, if ordinary technicians in the field are inspired by it and design methods and embodiments similar to the technical solution without creativity without departing from the purpose of the invention, they should all fall within the protection scope of the present invention.
Claims
1. A novel FOWLP process AOP packaging method, characterized by: The steps include: S1, first rewiring: set the first rewiring layer on the Release layer; S2, electroplating copper needles: electroplating copper needles on the first redistribution layer, and coating the surface of the first redistribution layer with photoresist; S3, debonding and wafer bonding: removing the photoresist on the surface of the first redistribution layer and bonding the wafer; S4, plastic encapsulation: plastic encapsulation is performed on the surface of the first redistribution layer using epoxy resin plastic encapsulation material; S5, plastic sealing polishing: polish and thin the plastic sealing material to expose the copper needle; S6. Second redistribution: Setting a second redistribution layer on the copper needles.
2. The novel FOWLP process AOP packaging method according to claim 1, characterized in that: The step S6 specifically includes: after the copper needle is led out from the second rewiring layer, sputtering is started, photolithography coating, exposure, and development are performed, and after opening the window, electroplating the copper coil is started, and after electroplating, the adhesive is removed, etching is performed, and then a layer of plastic sealing adhesive is used for encapsulation, and finally polishing is performed to expose the copper coil.
3. The novel FOWLP process AOP packaging method according to claim 2, characterized in that: The copper coil is of mosquito coil type.
4. A novel FOWLP process AOP package, packaged according to the novel FOWLP process AOP packaging method according to claims 1-3.
Citation Information
Patent Citations
Fan-out semiconductor package structure and fabricating method thereof
CN108461455A
Semiconductor Devices and Methods of Manufacture
CN112838078A
Chip fan-out type packaging structure with antenna and packaging method of chip fan-out type packaging structure
CN113192903A
Package structure and method of manufacturing the same
US20210020560A1
Semiconductor package antenna structure and its manufacturing method
US20240195047A1