Semiconductor refrigeration or thermoelectric power generation device and preparation method thereof

By forming through holes on the ceramic substrate of semiconductor cooling or temperature difference power generation devices and releasing stress, the problems of lifting and welding layer cracks caused by temperature difference of ceramic substrate are solved, the stability and life of the device are improved, and the number of semiconductor particles is increased. The situation.

CN119095462APending Publication Date: 2024-12-06DONGGUAN PILOT ADVANCED TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411010630.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-26
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

In semiconductor cooling or temperature difference power generation devices, the temperature difference of the ceramic substrate leads to thermal expansion and contraction differences, forming internal stresses, causing substrate lift and welding layer cracks, affecting device stability and life.

Method used

By forming through holes in the thickness direction on the ceramic substrate, avoiding the deflector, and place solder and semiconductor particles, forming a series electrical connection, and releasing internal stress through the through holes to prevent the substrate from rising up and cracking of the solder layer.

Benefits of technology

Effectively release stress generated by temperature difference, avoid the rise of ceramic substrates and cracks in the welding layer, improve the working stability and life of the device, and is suitable for increasing the number of semiconductor particles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119095462A_ABST
    Figure CN119095462A_ABST
Patent Text Reader

Abstract

The invention provides a semiconductor refrigeration or thermoelectric power generation device and a preparation method thereof. The semiconductor refrigeration or thermoelectric power generation device comprises a first ceramic substrate, a second ceramic substrate, a plurality of first flow deflectors, a second flow deflector, a first solder, a second solder, N particles, P particles and two output electrode wires. The first ceramic substrate and the second ceramic substrate are opposite to each other; the plurality of first flow deflectors are arranged on the first ceramic substrate, and the plurality of second flow deflectors are arranged on the second ceramic substrate; the first solder is arranged on the first flow deflectors, and the second solder is arranged on the second flow deflectors; the N particles and the P particles are placed between the corresponding first solder and the corresponding second solder; the first flow deflector, the second flow deflector, the N particles and the P particles are welded through the first welding flux and the second welding flux to form series electric connection; the two output electrode wires are electrically connected to the head and the tail of the series electric connection respectively; a through first through hole is formed in the first ceramic substrate, and a through second through hole is formed in the second ceramic substrate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the field of thermoelectricity, and more specifically to a semiconductor refrigeration or temperature difference power generation device and a preparation method thereof. Background Art

[0002] Both semiconductor coolers (TEC) and semiconductor thermoelectric generators (TEG) are devices based on the thermoelectric effect, which can be collectively referred to as semiconductor cooling or thermoelectric power generation devices. They are widely used in electronic equipment, household appliances, medical equipment, aerospace, automotive industry, renewable energy, micro power sources, etc. With the continuous advancement of technology, the scope of application will be further expanded, and it has broad development prospects.

[0003] In the field of semiconductor refrigeration or temperature difference power generation, there are currently the following technical challenges and problems.

[0004] Whether it is thermoelectric cooling or thermoelectric power generation, during the operation of semiconductor cooling or thermoelectric power generation devices, there is a temperature difference between the ceramic substrate at the cold end and the ceramic substrate at the hot end. The greater the temperature difference, the higher the cooling capacity of thermoelectric cooling or the power generation efficiency of thermoelectric power generation. As far as the current technical level is concerned, the degree of temperature difference that can be achieved by thermoelectric power generation is higher than that of thermoelectric cooling. In order to increase the cooling capacity and power generation efficiency, it is necessary to increase the number of semiconductor particles of N particles and P particles, which usually means using a larger ceramic substrate in semiconductor cooling or thermoelectric power generation devices. Because the increased number of semiconductor particles of N particles and P particles will increase the temperature difference between the ceramic substrate at the cold end and the ceramic substrate at the hot end of the semiconductor cooling or thermoelectric power generation device during operation, this increased temperature difference will increase the difference in thermal expansion and contraction between the ceramic substrate at the cold end and the ceramic substrate at the hot end during operation. Because the ceramic substrate at the cold end and the ceramic substrate at the hot end are connected together via the N particles and P particles that are electrically connected to each other, the increased difference in thermal expansion and contraction between the ceramic substrate at the cold end and the ceramic substrate at the hot end causes the ceramic substrate at the cold end and the ceramic substrate at the hot end to interact with each other to form internal stress, and this internal stress cannot be released, thereby causing the ceramic substrate at the hot end and / or the ceramic substrate at the cold end to warp. The warping of the ceramic substrate will have a negative impact on the working stability of the semiconductor cooling or thermoelectric power generation device, and may cause cracks in the welding layer formed by the N particles / P particles or solder, which will directly affect the life of the semiconductor cooling or thermoelectric power generation device. Summary of the invention

[0005] In view of the problems existing in the background technology, an object of the present disclosure is to provide a semiconductor refrigeration or temperature difference power generation device and a preparation method thereof, which can release the stress caused by temperature difference, thereby avoiding the warping of the ceramic substrate and further avoiding cracks in the welding layer formed by N particles / P particles or solder.

[0006] Another object of the present disclosure is to provide a semiconductor cooling or temperature difference power generation device and a method for manufacturing the same, which is suitable for the case where the ceramic substrate is adaptively enlarged due to the increase in the number of semiconductor particles of N particles and P particles.

[0007] Thus, in a first embodiment, a method for preparing a semiconductor refrigeration or temperature difference power generation device includes the following steps: S1, providing a first ceramic substrate provided with a plurality of first guide plates and a second ceramic substrate provided with a plurality of second guide plates; S2, providing a first solder on each first guide plate of the first ceramic substrate, and providing a second solder on each second guide plate of the second ceramic substrate; S3, placing N particles and P particles on the first solder of the corresponding first guide plates; S4, clamping the second ceramic substrate provided with the second solder on each second guide plate on the N particles and P particles placed on the first solder of the corresponding first guide plate to form a clamping assembly; S5, welding the clamping assembly so that the plurality of first guide plates and the plurality of second guide plates are electrically connected in series with all the N particles and P particles through all the first solders and the second solders; S6, welding the formed series electrical connection The two output electrode lines are welded to corresponding two of the multiple first guide plates and the multiple second guide plates at both ends of the connection respectively to form an initial product; S7, a welding effect test is performed on the initial product to determine whether the welding effect of the initial product is within the standard; S8, after determining that the welding effect of the initial product is within the standard, a first through hole is formed on the first ceramic substrate of the initial product along the thickness direction of the first ceramic substrate and a second through hole is formed on the second ceramic substrate of the initial product along the thickness direction of the second ceramic substrate to obtain a product device, the first through hole avoids the multiple first guide plates, extends to and opens at the first periphery of the first ceramic substrate, and the first through hole does not divide the first ceramic substrate into multiple independent parts, the second through hole avoids the multiple second guide plates, extends to and opens at the second periphery of the second ceramic substrate, and the second through hole does not divide the second ceramic substrate into multiple independent parts.

[0008] In a second embodiment, a method for preparing a semiconductor refrigeration or temperature difference power generation device comprises the following steps: Sa, providing a first ceramic substrate provided with a plurality of first guide plates and a second ceramic substrate provided with a plurality of second guide plates; Sb, forming a first through hole penetrating along the thickness direction of the first ceramic substrate on the first ceramic substrate and forming a second through hole penetrating along the thickness direction of the second ceramic substrate on the second ceramic substrate, the first through hole avoiding the plurality of first guide plates and being spaced apart from the first periphery of the first ceramic substrate, the first through hole not dividing the first ceramic substrate into a plurality of independent parts, the second through hole avoiding the plurality of second guide plates and being spaced apart from the second periphery of the second ceramic substrate, the second through hole not dividing the second ceramic substrate into a plurality of independent parts; Sc, providing a first solder on each of the first guide plates of the first ceramic substrate, and providing a second solder on each of the second guide plates of the second ceramic substrate; Sd, placing N particles and P particles on the first solder of the corresponding first guide plate; Se, clamping the second ceramic substrate with the second solder on each second guide plate on the N particles and P particles placed on the first solder of the corresponding first guide plate to form a clamping assembly; Sf, welding the clamping assembly to make a plurality of first guide plates and a plurality of second guide plates form a series electrical connection with all the N particles and P particles through all the first solders and the second solders; Sg, respectively welding two output electrode lines to the corresponding two of the plurality of first guide plates and the plurality of second guide plates at the head and tail ends of the series electrical connection to form a product device; Sh, performing a welding effect test on the product device to determine whether the welding effect of the product device is within the standard. If the welding effect of the product device is within the standard, the product device is used as a semiconductor refrigeration or temperature difference power generation device.

[0009] Provided is a semiconductor cooling or temperature difference power generation device, comprising a first ceramic substrate, a second ceramic substrate, a plurality of first guide plates, a second guide plate, a first solder, a second solder, N particles, P particles and two output electrode lines; the first ceramic substrate and the second ceramic substrate are opposite to each other; a plurality of first guide plates are arranged on the surface of the first ceramic substrate facing the second ceramic substrate, and a plurality of second guide plates are arranged on the surface of the second ceramic substrate facing the first ceramic substrate; a first solder is arranged on each first guide plate, and a second solder is arranged on each second guide plate; N particles and P particles are placed between the corresponding first solder and the corresponding second solder; a plurality of first guide plates are arranged on the surface of the second ceramic substrate facing the first ceramic substrate; A guide plate, a plurality of second guide plates, and all N particles and P particles are welded through all first solders and second solders to form a series electrical connection; two output electrode lines are respectively electrically connected to corresponding two of the plurality of first guide plates and the plurality of second guide plates at the head and tail ends of the series electrical connection; the first ceramic substrate is formed with a first through hole penetrating along the thickness direction of the first ceramic substrate, the first through hole avoids the plurality of first guide plates, and the first through hole does not divide the first ceramic substrate into a plurality of independent parts; the second ceramic substrate is formed with a second through hole penetrating along the thickness direction of the second ceramic substrate, the second through hole avoids the plurality of second guide plates, and the second through hole does not divide the second ceramic substrate into a plurality of independent parts.

[0010] The beneficial effects of the present disclosure are as follows.

[0011] In the first and second embodiments of the method for preparing the semiconductor cooling or thermoelectric power generation device according to the present disclosure and the semiconductor cooling or thermoelectric power generation device according to the present disclosure, the first through hole and the second through hole, during the operation of the semiconductor cooling or thermoelectric power generation device, there is a temperature difference between the first ceramic substrate and the second ceramic substrate, which are respectively the cold end and the hot end, and a difference in the degree of thermal expansion and contraction caused by the temperature difference. This difference in the degree of thermal expansion and contraction will cause the first ceramic substrate and the second ceramic substrate to interact with each other to form internal stress due to the connection of the first ceramic substrate and the second ceramic substrate via the N particles and the P particles electrically connected to each other. This internal stress can be released through the first through hole and the second through hole. In short, the stress generated by the temperature difference is released, thereby avoiding the first ceramic substrate and the second ceramic substrate from warping, and then avoiding cracks in the welding layer formed by the N particles / P particles or the first solder and the second solder, thereby avoiding affecting the life of the semiconductor cooling or thermoelectric power generation device. This is particularly suitable for the case where the first ceramic substrate and the second ceramic substrate are adaptively enlarged due to the increase in the number of semiconductor particles of the N particles and the P particles (i.e., the case where the cooling capacity and power generation efficiency are improved and the corresponding temperature difference is larger). BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1It is a process diagram of the first embodiment of the method for preparing a semiconductor refrigeration or temperature difference power generation device according to the present disclosure, wherein the second ceramic substrate and multiple second guide plates during mold closing in step S4, welding of two output electrode wires in step S6 and packaging of colloid are shown with dotted lines.

[0013] Figure 2 yes Figure 1 An enlarged view of a first ceramic substrate, a plurality of first guide plates and a first through hole in a product device, wherein the first through hole is in a straight line shape.

[0014] Figure 3 yes Figure 1 An enlarged view of the second ceramic substrate, multiple second guide plates and second through holes in the product device.

[0015] Figure 4 yes Figure 2 A variation of the present invention, wherein the first through hole is L-shaped.

[0016] Figure 5 yes Figure 3 A variation of , wherein the second through hole is L-shaped.

[0017] Figure 6 yes Figure 2 Another variation of the present invention is that the first through hole is T-shaped.

[0018] Figure 7 yes Figure 3 Another variation of the present invention is that the second through hole is T-shaped.

[0019] Figure 8 yes Figure 2 In yet another variation of the present invention, the first through hole is cross-shaped.

[0020] Fig. 9 yes Figure 3 In yet another variation of the present invention, the second through hole is cross-shaped.

[0021] Fig.10 It is a process diagram of the second embodiment of the method for preparing a semiconductor refrigeration or temperature difference power generation device according to the present disclosure, wherein the second ceramic substrate, multiple second guide plates and the first through hole during mold closing in step Se and welding of two output electrode wires in step Sg are shown with dotted lines, and the first through hole during encapsulation of the colloid is shown with a dotted line.

[0022] Fig.11 yes Fig.10 An enlarged view of the first ceramic substrate, the plurality of first guide plates and the first through hole in step Sb, wherein the first through hole is in a straight line shape.

[0023] Fig.12 yes Fig.10An enlarged view of the second ceramic substrate, the plurality of second guide plates and the second through holes in step Sb.

[0024] Fig.13 yes Fig.11 A variation of the present invention, wherein the first through hole is L-shaped.

[0025] Fig.14 yes Fig.12 A variation of , wherein the second through hole is L-shaped.

[0026] Fig.15 yes Fig.11 Another variation of the present invention is that the first through hole is T-shaped.

[0027] Fig.16 yes Fig.12 Another variation of the present invention is that the second through hole is T-shaped.

[0028] Fig.17 yes Fig.11 In yet another variation of the present invention, the first through hole is cross-shaped.

[0029] Fig.18 yes Fig.12 In yet another variation of the present invention, the second through hole is cross-shaped.

[0030] The reference numerals are described as follows:

[0031] 1 first ceramic substrate 6 second solder

[0032] 11 First through hole 7N particles

[0033] 12 First peripheral 8P particles

[0034] 2 second ceramic substrate 9 output electrode line

[0035] 21 second through hole 10 colloid

[0036] 22 second periphery 100 mold clamping component

[0037] 3First guide vane 200 initial product

[0038] 4 Second guide plate 300 product device

[0039] 5. First Solder DETAILED DESCRIPTION

[0040] The accompanying drawings show embodiments of the present disclosure, and it will be understood that the disclosed embodiments are merely examples of the present disclosure, and the present disclosure can be implemented in various forms. Therefore, the specific details disclosed herein should not be interpreted as limiting, but merely as the basis for the claims and as a representative basis for teaching ordinary technicians in the field to implement the present disclosure in various ways.

[0041] [First embodiment of the method for manufacturing a semiconductor cooling or temperature difference power generation device]

[0042] Reference Figure 1 According to the first embodiment of the method for preparing the semiconductor refrigeration or temperature difference power generation device disclosed in the present invention, the steps include:

[0043] S1, providing a first ceramic substrate 1 provided with a plurality of first guide plates 3 and a second ceramic substrate 2 provided with a plurality of second guide plates 4;

[0044] S2, disposing a first solder 5 on each first guide plate 3 of the first ceramic substrate 1, and disposing a second solder 6 on each second guide plate 4 of the second ceramic substrate 2;

[0045] S3, placing N particles 7 and P particles 8 on the first solder 5 of the corresponding first guide plate 3;

[0046] S4, the second ceramic substrate 2 with the second solder 6 disposed on each second guide plate 4 is molded onto the N particles 7 and the P particles 8 that have been placed on the first solder 5 of the corresponding first guide plate 3 to form a mold assembly 100;

[0047] S5, welding the mold assembly 100, so that the plurality of first guide plates 3, the plurality of second guide plates 4 are electrically connected in series with all the N particles 7 and the P particles 8 through all the first solders 5 and the second solders 6;

[0048] S6, welding two output electrode wires 9 to form a primary product 200 by respectively welding two corresponding ones of the plurality of first guide plates 3 and the plurality of second guide plates 4 at both ends of the series electrical connection;

[0049] S7, performing welding effect detection on the primary product 200 to determine whether the welding effect of the primary product 200 is within the standard;

[0050] S8, after determining that the welding effect of the primary product 200 is within the standard, a first through hole 11 penetrating along the thickness direction of the first ceramic substrate 1 is formed on the first ceramic substrate 1 of the primary product 200, and a second through hole 21 penetrating along the thickness direction of the second ceramic substrate 2 is formed on the second ceramic substrate 2 of the primary product 200, so as to obtain a product device 300, wherein the first through hole 11 avoids the plurality of first guide plates 3, extends to and opens at the first periphery 12 of the first ceramic substrate 1, and the first through hole 11 does not divide the first ceramic substrate 1 into a plurality of independent parts, and the second through hole 21 avoids the plurality of second guide plates 4, extends to and opens at the second periphery 22 of the second ceramic substrate 2, and the second through hole 21 does not divide the second ceramic substrate 2 into a plurality of independent parts.

[0051] In the first embodiment of the method for preparing a semiconductor refrigeration or thermoelectric power generation device according to the present disclosure, the first through hole 11 formed by step S8, which avoids the plurality of first guide plates 3 and extends to and opens at the first periphery 12 of the first ceramic substrate 1, and the second through hole 21 which avoids the plurality of second guide plates 4 and extends to and opens at the second periphery 22 of the second ceramic substrate 2, during the operation of the semiconductor refrigeration or thermoelectric power generation device, the first ceramic substrate 1 and the second ceramic substrate 2, which serve as the cold end and the hot end, respectively (for example, the first ceramic substrate 1 is the cold end ceramic substrate, and the second ceramic substrate 2 is the hot end ceramic substrate; or the first ceramic substrate 1 is the hot end ceramic substrate, and the second ceramic substrate 2 is the cold end second ceramic substrate). There is a temperature difference between the first ceramic substrate 1 and the second ceramic substrate 2 and a difference in the degree of thermal expansion and contraction caused by the temperature difference. The difference in the degree of thermal expansion and contraction will cause the first ceramic substrate 1 and the second ceramic substrate 2 to interact with each other to form internal stress due to the connection of the first ceramic substrate 1 and the second ceramic substrate 2 via the N particles 7 and the P particles 8 electrically connected to each other. This internal stress can be released through the first through hole 11 and the second through hole 21. In short, the stress caused by the temperature difference is released, thereby preventing the first ceramic substrate 1 and the second ceramic substrate 2 from warping, and further preventing the welding layer formed by the N particles 7 / P particles 8 or the first solder 5 and the second solder 6 from cracking, thereby avoiding affecting the life of the semiconductor refrigeration or temperature difference power generation device. This is particularly suitable for the case where the first ceramic substrate 1 and the second ceramic substrate 2 are adaptively enlarged due to the increase in the number of semiconductor particles of the N particles 7 and the P particles 8 (i.e., the case where the cooling capacity and power generation efficiency are improved and the corresponding temperature difference is larger).

[0052] In step S1, for example, the first ceramic substrate 1 and the second ceramic substrate 2 are aluminum oxide or aluminum nitride ceramic substrates. In step S1, for example, a plurality of first guide plates 3 are sintered or electroplated on the first ceramic substrate 1, and a plurality of second guide plates 4 are sintered or electroplated on the second ceramic substrate 2.

[0053] In step S2, for example, the first solder 5 and the second solder 6 are both solder pastes, preferably tin pastes. In step S2, for example, the first solder 5 and the second solder 6 are screen printed using a steel screen printing process. Further, in step S2, for example, the steel screen has a thickness of 0.1-0.3 mm, and the length and width of the mesh are the same as the corresponding sizes of the first guide plate 3 and the second guide plate 4.

[0054] In step S3, generally, the N particles 7 and P particles 8 are first cut into wafers of designed thickness, and then the wafers are electroplated with, for example, Ni+Au or Ni+Sn, and finally the wafers are cut into N particles 7 / P particles 8 according to the particle size required by the product. In step S3, the N particles 7 and P particles 8 are placed on the first solder 5 of the corresponding first guide plate 3 through a screen or DB (Die Bond) process.

[0055] In step S4 , for example, the second ceramic substrate 2 on which the second solder 6 is provided on each second guide plate 4 is clamped by using a clamping jig for clamping.

[0056] In step S5, the mold assembly 100 is welded by reflow welding, pulse welding or vacuum reflow welding, preferably reflow welding.

[0057] In step S6, the two output electrode wires 9 are welded by soldering iron welding, reflow welding or laser welding, preferably soldering iron welding.

[0058] In step S7, the welding effect is detected by connecting an internal resistance detection device to the two output electrode lines 9 to detect the internal resistance and determine the welding effect. Further, the internal resistance detection device is a bridge or an LCR bridge.

[0059] In step S8, the first through hole 11 and the second through hole 21 are realized by laser cutting, water jet cutting or mechanical cutting, preferably water jet cutting. Further, the first through hole 11 is made by a pattern preset on the surface of the first ceramic substrate 1 away from the first guide plate 3; the second through hole 21 is made by a pattern preset on the surface of the second ceramic substrate 2 away from the second guide plate 4. The pattern can be pre-set based on the layout of the multiple first guide plates 3 on the first ceramic substrate 1 and the multiple second guide plates 4 on the second ceramic substrate 2 after step S1 is completed, for example, a sticker with a pre-set pattern is attached or a marking line is made in advance.

[0060] like Figures 2 to 9 As shown, in step S8, the first through hole 11 and the second through hole 21 are in, but not limited to, a straight shape, an L shape, a T shape, or a cross shape.

[0061] like Figures 2 to 9 As shown, in step S8, there are multiple first through holes 11 and they are spaced apart from each other, there are multiple second through holes 21 and they are spaced apart from each other, one first through hole 11 is provided between two adjacent first guide plates 3, and one second through hole 21 is provided between two adjacent second guide plates 4. When multiple first through holes 11 are provided, the shapes of the multiple first through holes 11 may be the same or different; similarly, when multiple second through holes 21 are provided, the shapes of the multiple second through holes 21 may be the same or different.

[0062] In one example, the first embodiment of the method for preparing a semiconductor cooling or temperature difference power generation device according to the present disclosure further includes the steps: S9, performing an internal resistance test on the product device 300; S10, after the internal resistance test is qualified, performing non-destructive testing on the product device 300 to determine whether the product device 300 has microcracks. If there are no microcracks, the product device 300 is qualified, that is, the product device 300 is used as a semiconductor cooling or temperature difference power generation device. Further, in step S9, the internal resistance of the product device 300 is measured by connecting an internal resistance detection device to the two output electrode lines 9. For example, the internal resistance detection device is a bridge or an LCR bridge. Further, in step S10, for example, X-ray non-destructive testing is used.

[0063] Reference Figure 1 In one example, the first embodiment of the method for preparing a semiconductor refrigeration or thermoelectric power generation device according to the present disclosure further includes a step between step S7 and step S8: packaging. After determining in step S7 that the welding effect of the initial product 200 is within the standard, the first ceramic substrate 1 and the second ceramic substrate 2 are packaged with a colloid 10 around them; step S8 is performed after the packaging step. By packaging, condensation at the cold end of the product device 300 during operation / or foreign matter entering the interior to cause a short circuit is prevented. Specifically, the colloid 10 is an epoxy resin. Further, in step S8, after forming the first through hole 11 and the second through hole 21, a sealant is formed in the first through hole 11 and the second through hole 21, so that the first ceramic substrate 1, the second ceramic substrate 2, the colloid 10, and the sealant in the first through hole 11 and the second through hole 21 achieve full sealing of the product device 300. The sealant can also be an epoxy resin.

[0064] In addition, in one example, the first embodiment of the method for preparing a semiconductor refrigeration or temperature difference power generation device according to the present disclosure also includes the following steps: after step S8 (if there are the aforementioned steps S9 and S10, it can be after step S10), after forming the first through hole 11, a whole sheet of thermal pad / thermal grease is affixed to the entire surface of the first ceramic substrate 1 facing away from the first guide plate 3, and after forming the second through hole 21, a whole sheet of thermal pad / thermal grease is affixed to the entire surface of the second ceramic substrate 2 facing away from the second guide plate 4, which not only improves the thermal conductivity of the first ceramic substrate 1 and the second ceramic substrate 2, but also improves the sealing effect of the first ceramic substrate 1 and the second ceramic substrate 2.

[0065] In addition, in one example, the first embodiment of the method for preparing a semiconductor cooling or temperature difference power generation device according to the present disclosure includes the step of packaging and shipping after step S10. If there is the aforementioned step of setting a thermal pad / thermal grease, packaging and shipping is performed after the aforementioned step of setting a thermal pad / thermal grease.

[0066] [Second embodiment of the method for manufacturing a semiconductor cooling or temperature difference power generation device]

[0067] Reference Fig.10 According to the second embodiment of the method for preparing the semiconductor refrigeration or temperature difference power generation device disclosed in the present invention, the steps include:

[0068] Sa, providing a first ceramic substrate 1 provided with a plurality of first guide plates 3 and a second ceramic substrate 2 provided with a plurality of second guide plates 4;

[0069] Sb, a first through hole 11 penetrating along the thickness direction of the first ceramic substrate 1 is formed on the first ceramic substrate 1, and a second through hole 21 penetrating along the thickness direction of the second ceramic substrate 2 is formed on the second ceramic substrate 2, the first through hole 11 avoids the plurality of first guide plates 3 and is spaced apart from the first peripheral edge 12 of the first ceramic substrate 1, the first through hole 11 does not divide the first ceramic substrate 1 into a plurality of independent parts, the second through hole 21 avoids the plurality of second guide plates 4 and is spaced apart from the second peripheral edge 22 of the second ceramic substrate 2, the second through hole 21 does not divide the second ceramic substrate 2 into a plurality of independent parts;

[0070] Sc, a first solder 5 is disposed on each first guide plate 3 of the first ceramic substrate 1, and a second solder 6 is disposed on each second guide plate 4 of the second ceramic substrate 2;

[0071] Sd, placing N particles 7 and P particles 8 on the first solder 5 of the corresponding first guide plate 3;

[0072] Se, the second ceramic substrate 2 with the second solder 6 disposed on each second guide plate 4 is molded onto the N particles 7 and the P particles 8 that have been placed on the first solder 5 of the corresponding first guide plate 3 to form a mold assembly 100;

[0073] Sf, welding the mold assembly 100 so that the plurality of first guide plates 3 and the plurality of second guide plates 4 are electrically connected in series with all the N particles 7 and the P particles 8 through all the first solders 5 and the second solders 6;

[0074] Sg, welding two output electrode wires 9 to form a product device 300 by respectively welding two corresponding ones of the plurality of first guide plates 3 and the plurality of second guide plates 4 at both ends of the series electrical connection;

[0075] Sh, the welding effect detection is performed through the product device 300 to determine whether the welding effect of the product device 300 is within the standard. If the welding effect of the product device 300 is within the standard, the product device 300 is used as a semiconductor cooling or temperature difference power generation device.

[0076] The second embodiment of the method for preparing a semiconductor cooling or thermoelectric power generation device according to the present disclosure is different from the first embodiment of the method for preparing a semiconductor cooling or thermoelectric power generation device according to the present disclosure in that the first through hole 11 does not extend to the periphery 12 of the first ceramic substrate 1, and the second through hole 21 does not extend to the periphery 22 of the second ceramic substrate 2, and the first through hole 11 and the second through hole 21 are made before the product device 300 is formed (specifically, before the step Sc of setting the first solder 5 and the second solder 6). In particular, the first embodiment of the method for preparing a semiconductor cooling or thermoelectric power generation device according to the present disclosure can be performed centrally after the batch product devices 300 are formed.

[0077] In the second embodiment of the method for preparing a semiconductor refrigeration or thermoelectric power generation device according to the present disclosure, similarly, the first through hole 11 avoiding the plurality of first guide plates 3 and spaced apart from the first periphery 12 of the first ceramic substrate 1 and the second through hole 21 avoiding the plurality of second guide plates 4 and spaced apart from the second periphery 22 of the second ceramic substrate 2 formed by step Sb, during the operation of the semiconductor refrigeration or thermoelectric power generation device, the first ceramic substrate 1 and the second ceramic substrate 2 serving as the cold end and the hot end, respectively (for example, the first ceramic substrate 1 is the cold end ceramic substrate, and the second ceramic substrate 2 is the hot end ceramic substrate; or the first ceramic substrate 1 is the hot end ceramic substrate, and the second ceramic substrate 2 is the cold end ceramic substrate There is a temperature difference between the first ceramic substrate 1 and the second ceramic substrate 2 and a difference in the degree of thermal expansion and contraction caused by the temperature difference. The difference in the degree of thermal expansion and contraction will cause the first ceramic substrate 1 and the second ceramic substrate 2 to interact with each other to form internal stress due to the connection of the first ceramic substrate 1 and the second ceramic substrate 2 via the N particles 7 and the P particles 8 electrically connected to each other. This internal stress can be released through the first through hole 11 and the second through hole 21. In short, the stress caused by the temperature difference is released, thereby preventing the first ceramic substrate 1 and the second ceramic substrate 2 from warping, and further preventing the welding layer formed by the N particles 7 / P particles 8 or the first solder 5 and the second solder 6 from cracking, thereby avoiding affecting the life of the semiconductor refrigeration or temperature difference power generation device. This is particularly suitable for the case where the first ceramic substrate 1 and the second ceramic substrate 2 are adaptively enlarged due to the increase in the number of semiconductor particles of the N particles 7 and the P particles 8 (i.e., the case where the cooling capacity and power generation efficiency are improved and the corresponding temperature difference is larger).

[0078] Similarly, in step Sa, for example, the first ceramic substrate 1 and the second ceramic substrate 2 are aluminum oxide or aluminum nitride ceramic substrates. Similarly, in step Sa, for example, a plurality of first guide plates 3 are sintered or electroplated on the first ceramic substrate 1, and a plurality of second guide plates 4 are sintered or electroplated on the second ceramic substrate 2.

[0079] Similarly, in step Sb, the first through hole 11 and the second through hole 21 are realized by laser cutting, water jet cutting or mechanical cutting, preferably water jet cutting. Further, in step Sb, similarly, the first through hole 11 is made by presetting a pattern on the surface of the first ceramic substrate 1 away from the first guide plate 3; the second through hole 21 is made by presetting a pattern on the surface of the second ceramic substrate 2 away from the second guide plate 4. Similarly, the pattern can be pre-set based on the layout of the multiple first guide plates 3 on the first ceramic substrate 1 and the multiple second guide plates 4 on the second ceramic substrate 2 after step S1 is completed, such as affixing a sticker with a pre-set pattern or pre-marking lines.

[0080] like Figures 11 to 18 As shown, in step Sb, the first through hole 11 and the second through hole 21 are in a straight shape, an L shape, a T shape or a cross shape, but are not limited to. In one example, in step Sb, there are multiple first through holes 11 and they are spaced apart from each other, there are multiple second through holes 21 and they are spaced apart from each other, one first through hole 11 is provided between two adjacent first guide plates 3, and one second through hole 21 is provided between two adjacent second guide plates 4. When multiple first through holes 11 are provided, the shapes of the multiple first through holes 11 may be the same or different; similarly, when multiple second through holes 21 are provided, the shapes of the multiple second through holes 21 may be the same or different.

[0081] Similarly, in step Sc, for example, the first solder 5 and the second solder 6 are both solder pastes, preferably tin pastes. Similarly, in step Sc, for example, the first solder 5 and the second solder 6 are screen printed using a steel screen printing process. Further, in step Sc, for example, the steel screen has a thickness of 0.1-0.3 mm, and the length and width of the mesh are the same as the corresponding sizes of the first guide plate 3 and the second guide plate 4.

[0082] Similarly, in step Sd, generally, the N particles 7 and P particles 8 are first cut into wafers of designed thickness, and then the wafers are electroplated with, for example, Ni+Au or Ni+Sn, and finally the wafers are cut into N particles 7 / P particles 8 according to the particle size required by the product. Similarly, in step Sd, the N particles 7 and P particles 8 are placed on the first solder 5 of the corresponding first guide plate 3 through a screen or DB (Die Bond) process.

[0083] Similarly, in step Se, the second ceramic substrate 2 on which the second solder 6 is provided on each second guide plate 4 is clamped by using a clamping jig for clamping.

[0084] Likewise, in step Sf, the mold assembly 100 is welded by reflow welding, pulse welding or vacuum reflow welding, preferably reflow welding.

[0085] Similarly, in step Sg, the two output electrode wires 9 are welded by soldering iron welding, reflow soldering or laser welding, preferably soldering iron welding.

[0086] Similarly, in step Sh, the welding effect is detected by connecting the internal resistance detection device to the two output electrode lines 9 to detect the internal resistance and determine the welding effect. Further, similarly, the internal resistance detection device is a bridge or an LCR bridge.

[0087] Similarly, in one example, the second embodiment of the method for preparing a semiconductor cooling or temperature difference power generation device according to the present disclosure further includes step: S1, performing nondestructive testing on the product device 300 to determine whether the product device 300 has microcracks, and if there are no microcracks, the product device 300 is qualified. Further, in step S1, similarly, for example, X-ray nondestructive testing is used.

[0088] Likewise, in one example, referring to Fig.10 According to the second embodiment of the method for preparing a semiconductor refrigeration or temperature difference power generation device disclosed in the present invention, the step Sh also includes the following steps: packaging. After determining in step Sh that the welding effect of the product device 300 is within the standard, the first ceramic substrate 1 and the second ceramic substrate 2 are packaged with a colloid 10 around them. By packaging, condensation at the cold end of the product device 300 during operation and / or foreign matter entering the interior to cause a short circuit are prevented. Specifically, the colloid 10 is an epoxy resin. Further, in the packaging step, a sealant is formed in the first through hole 11 and the second through hole 21. Thus, the first ceramic substrate 1, the second ceramic substrate 2, the colloid 10, and the sealant in the first through hole 11 and the second through hole 21 achieve full sealing of the product device 300. The sealant can also be an epoxy resin.

[0089] Similarly, in one example, the second embodiment of the method for preparing a semiconductor refrigeration or temperature difference power generation device according to the present disclosure also includes the steps of: after the packaging step, a whole sheet of thermal pad / thermal grease is affixed on the entire surface of the first ceramic substrate 1 facing away from the first guide plate 3, and a whole sheet of thermal pad / thermal grease is affixed on the entire surface of the second ceramic substrate 2 facing away from the second guide plate 4, which not only improves the thermal conductivity of the first ceramic substrate 1 and the second ceramic substrate 2, but also improves the sealing effect of the first ceramic substrate 1 and the second ceramic substrate 2.

[0090] Similarly, in one example, the second embodiment of the method for preparing a semiconductor cooling or temperature difference power generation device according to the present disclosure further includes the step of packaging and shipping after step Sh. If there is the aforementioned step of setting a thermal pad / thermal grease, packaging and shipping is performed after the aforementioned step of setting a thermal pad / thermal grease.

[0091] [Semiconductor cooling or temperature difference power generation device]

[0092] Reference Figures 1 to 18 According to the present disclosure, the semiconductor refrigeration or temperature difference power generation device includes a first ceramic substrate 1, a second ceramic substrate 2, a plurality of first guide plates 3, a second guide plate 4, a first solder 5, a second solder 6, N particles 7, P particles 8 and two output electrode wires 9.

[0093] The first ceramic substrate 1 and the second ceramic substrate 2 are opposite to each other. A plurality of first guide plates 3 are arranged on the surface of the first ceramic substrate 1 facing the second ceramic substrate 2, and a plurality of second guide plates 4 are arranged on the surface of the second ceramic substrate 2 facing the first ceramic substrate 1. A first solder 5 is arranged on each first guide plate 3, and a second solder 6 is arranged on each second guide plate 4. N particles 7 and P particles 8 are placed between the corresponding first solder 5 and the corresponding second solder 6. A plurality of first guide plates 3, a plurality of second guide plates 4 and all N particles 7 and P particles 8 are welded through all first solders 5 and second solders 6 to form a series electrical connection. Two output electrode lines 9 are respectively electrically connected to corresponding two of the plurality of first guide plates 3 and the plurality of second guide plates 4 at the head and tail ends of the series electrical connection. The first ceramic substrate 1 is formed with a first through hole 11 extending along the thickness direction of the first ceramic substrate 1, the first through hole 11 avoids the plurality of first guide plates 3, and the first through hole 11 does not divide the first ceramic substrate 1 into a plurality of independent parts, and the second ceramic substrate 2 is formed with a second through hole 21 extending along the thickness direction of the second ceramic substrate 2, the second through hole 21 avoids the plurality of second guide plates 4, and the second through hole 21 does not divide the second ceramic substrate 2 into a plurality of independent parts.

[0094] The method for preparing the semiconductor cooling or temperature difference power generation device according to the present disclosure can be referred to the first embodiment and the second embodiment of the method for preparing the semiconductor cooling or temperature difference power generation device according to the present disclosure, and will not be repeated here.

[0095] For details on the features, effects, implementation, etc. of the various components of the semiconductor cooling or temperature difference power generation device according to the present disclosure, please refer to the first and second embodiments of the preparation method of the semiconductor cooling or temperature difference power generation device according to the present disclosure, and will not be repeated here.

[0096] As described in the first embodiment of the method for preparing a semiconductor cooling or temperature difference power generation device according to the present disclosure, in one example, referring to Figures 1 to 9 The first through hole 11 extends to and opens at the first peripheral edge 12 of the first ceramic substrate 1 ; the second through hole 21 extends to and opens at the second peripheral edge 22 of the second ceramic substrate 2 .

[0097] As described in the second embodiment of the method for preparing a semiconductor cooling or temperature difference power generation device according to the present disclosure, in one example, referring to Figures 10 to 18The first through hole 11 is spaced apart from the first peripheral edge 12 of the first ceramic substrate 1 , and the second through hole 21 is spaced apart from the second peripheral edge 22 of the second ceramic substrate 2 .

[0098] As described in the first and second embodiments of the method for preparing a semiconductor cooling or temperature difference power generation device according to the present disclosure, referring to Figures 2 to 9 and Figures 11 to 18 , the first through hole 11 and the second through hole 21 are in a straight line shape, an L shape, a T shape or a cross shape. There are multiple first through holes 11 and they are spaced apart from each other, there are multiple second through holes 21 and they are spaced apart from each other, one first through hole 11 is provided between two adjacent first guide plates 3, and one second through hole 21 is provided between two adjacent second guide plates 4. When multiple first through holes 11 are provided, the shapes of the multiple first through holes 11 can be the same or different; similarly, when multiple second through holes 21 are provided, the shapes of the multiple second through holes 21 can be the same or different.

[0099] The above detailed description is used to describe multiple exemplary embodiments, but this document is not intended to be limited to the explicitly disclosed combinations. Therefore, unless otherwise stated, the various features disclosed herein can be combined together to form multiple additional combinations that are not shown for the sake of simplicity.

Claims

1. A method for preparing a semiconductor refrigeration or temperature difference power generation device, characterized in that: Includes steps: S1, providing a first ceramic substrate (1) provided with a plurality of first guide plates (3) and a second ceramic substrate (2) provided with a plurality of second guide plates (4); S2, arranging a first solder (5) on each first guide plate (3) of the first ceramic substrate (1), and arranging a second solder (6) on each second guide plate (4) of the second ceramic substrate (2); S3, placing N particles (7) and P particles (8) on the first solder (5) of the corresponding first guide plate (3); S4, clamping the second ceramic substrate (2) on which the second solder (6) is arranged on each second guide plate (4) onto the N particles (7) and the P particles (8) which have been placed on the first solder (5) of the corresponding first guide plate (3) to form a clamping assembly (100); S5, welding the mold assembly (100) so that the plurality of first guide plates (3) and the plurality of second guide plates (4) are electrically connected in series with all the N particles (7) and the P particles (8) through all the first solders (5) and the second solders (6); S6, welding two output electrode wires (9) to corresponding two of the plurality of first guide plates (3) and the plurality of second guide plates (4) at both ends of the series electrical connection, respectively, to form a primary product (200); S7, performing welding effect testing on the primary product (200) to determine whether the welding effect of the primary product (200) is within the standard; S8, after determining that the welding effect of the primary product (200) is within the standard, a first through hole (11) is formed on the first ceramic substrate (1) of the primary product (200) and is penetrated along the thickness direction of the first ceramic substrate (1), and a second through hole (21) is formed on the second ceramic substrate (2) of the primary product (200) and is penetrated along the thickness direction of the second ceramic substrate (2), so as to obtain a product device (300), wherein the first through hole (11) avoids the plurality of first guide plates (3), extends to and opens at the first peripheral edge (12) of the first ceramic substrate (1), and the first through hole (11) does not divide the first ceramic substrate (1) into a plurality of independent parts, and the second through hole (21) avoids the plurality of second guide plates (4), extends to and opens at the second peripheral edge (22) of the second ceramic substrate (2), and the second through hole (21) does not divide the second ceramic substrate (2) into a plurality of independent parts.

2. The method for preparing a semiconductor cooling or temperature difference power generation device according to claim 1, characterized in that: In step S8, the first through hole (11) and the second through hole (21) are in a straight line shape, an L shape, a T shape or a cross shape.

3. The method for preparing a semiconductor cooling or temperature difference power generation device according to claim 1, characterized in that: In step S8, there are a plurality of first through holes (11) spaced apart from each other, there are a plurality of second through holes (21) spaced apart from each other, one first through hole (11) is provided between two adjacent first guide plates (3), and one second through hole (21) is provided between two adjacent second guide plates (4).

4. A method for preparing a semiconductor refrigeration or temperature difference power generation device, characterized in that: Includes steps: Sa, providing a first ceramic substrate (1) provided with a plurality of first guide plates (3) and a second ceramic substrate (2) provided with a plurality of second guide plates (4); Sb, forming a first through hole (11) penetrating along the thickness direction of the first ceramic substrate (1) on the first ceramic substrate (1), and forming a second through hole (21) penetrating along the thickness direction of the second ceramic substrate (2) on the second ceramic substrate (2), the first through hole (11) avoiding the plurality of first guide plates (3) and being spaced apart from the first peripheral edge (12) of the first ceramic substrate (1), the first through hole (11) not dividing the first ceramic substrate (1) into a plurality of independent parts, the second through hole (21) avoiding the plurality of second guide plates (4) and being spaced apart from the second peripheral edge (22) of the second ceramic substrate (2), the second through hole (21) not dividing the second ceramic substrate (2) into a plurality of independent parts; Sc, a first solder (5) is arranged on each first guide plate (3) of the first ceramic substrate (1), and a second solder (6) is arranged on each second guide plate (4) of the second ceramic substrate (2); Sd, placing N particles (7) and P particles (8) on the first solder (5) of the corresponding first guide plate (3); Se, a second ceramic substrate (2) on which a second solder (6) is arranged on each second guide plate (4) is molded onto N particles (7) and P particles (8) which have been placed on the first solder (5) of the corresponding first guide plate (3) to form a mold assembly (100); Sf, welding the mold assembly (100) so that the plurality of first guide plates (3) and the plurality of second guide plates (4) are electrically connected in series with all the N particles (7) and the P particles (8) through all the first solders (5) and the second solders (6); Sg, welding two output electrode wires (9) to corresponding two of the plurality of first guide plates (3) and the plurality of second guide plates (4) at both ends of the series electrical connection, so as to form a product device (300); Sh, a welding effect test is performed on the product device (300) to determine whether the welding effect of the product device (300) is within the standard. If the welding effect of the product device (300) is within the standard, the product device (300) is used as a semiconductor cooling or temperature difference power generation device.

5. The method for preparing a semiconductor cooling or temperature difference power generation device according to claim 4, characterized in that: In step Sb, the first through hole (11) and the second through hole (21) are in a straight line shape, an L shape, a T shape or a cross shape.

6. The method for preparing a semiconductor cooling or temperature difference power generation device according to claim 4, characterized in that: In step Sb, there are a plurality of first through holes (11) spaced apart from each other, there are a plurality of second through holes (21) spaced apart from each other, one first through hole (11) is provided between two adjacent first guide plates (3), and one second through hole (21) is provided between two adjacent second guide plates (4).

7. A semiconductor cooling or temperature difference power generation device, characterized in that: The semiconductor cooling or temperature difference power generation device comprises a first ceramic substrate (1), a second ceramic substrate (2), a plurality of first guide plates (3), a second guide plate (4), a first solder (5), a second solder (6), N particles (7), P particles (8) and two output electrode lines (9); The first ceramic substrate (1) and the second ceramic substrate (2) are opposite to each other; A plurality of first guide plates (3) are arranged on a surface of the first ceramic substrate (1) facing the second ceramic substrate (2), and a plurality of second guide plates (4) are arranged on a surface of the second ceramic substrate (2) facing the first ceramic substrate (1); The first solder (5) is arranged on each first guide plate (3), and the second solder (6) is arranged on each second guide plate (4); N particles (7) and P particles (8) are placed between the corresponding first solder (5) and the corresponding second solder (6); A plurality of first guide plates (3), a plurality of second guide plates (4), and all N particles (7) and P particles (8) are welded via all first solders (5) and second solders (6) to form a series electrical connection; The two output electrode lines (9) are respectively electrically connected to corresponding two of the plurality of first guide plates (3) and the plurality of second guide plates (4) at the head and tail ends of the series electrical connection; The first ceramic substrate (1) is formed with a first through hole (11) penetrating along the thickness direction of the first ceramic substrate (1), the first through hole (11) avoids the plurality of first guide plates (3), and the first through hole (11) does not divide the first ceramic substrate (1) into a plurality of independent parts. The second ceramic substrate (2) is formed with a second through hole (21) penetrating along the thickness direction of the second ceramic substrate (2), the second through hole (21) avoids the plurality of second guide plates (4), and the second through hole (21) does not divide the second ceramic substrate (2) into a plurality of independent parts.

8. The semiconductor cooling or temperature difference power generation device according to claim 7, characterized in that: The first through hole (11) extends to and opens at a first peripheral edge (12) of the first ceramic substrate (1), and the second through hole (21) extends to and opens at a second peripheral edge (22) of the second ceramic substrate (2); or The first through hole (11) is spaced apart from a first peripheral edge (12) of the first ceramic substrate (1), and the second through hole (21) is spaced apart from a second peripheral edge (22) of the second ceramic substrate (2).

9. The semiconductor cooling or temperature difference power generation device according to claim 7, characterized in that: The first through hole (11) and the second through hole (21) are in a straight line shape, an L shape, a T shape or a cross shape.

10. The semiconductor cooling or temperature difference power generation device according to claim 7, characterized in that: There are a plurality of first through holes (11) spaced apart from each other, there are a plurality of second through holes (21) spaced apart from each other, one first through hole (11) is provided between two adjacent first guide plates (3), and one second through hole (21) is provided between two adjacent second guide plates (4).