Power device and preparation method thereof

Through epitaxial growth technology, the well region and the first region are formed in the SiC power device, which solves the device withstand voltage and on-resistance problems caused by the traditional ion implantation process, and achieves higher electron mobility and stability.

CN119132962AInactive Publication Date: 2024-12-13ANHUI YOFC ADVANCED SEMICONDUCTOR CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411241059.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-05
Publication Date
2024-12-13
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The electron mobility of SiC power devices is greatly affected by the interface state and crystal structure of the material. The traditional ion implantation process leads to the device's voltage withstand voltage limitation, increased on-resistance and material damage, affecting the current channel range.

Method used

The well region and the first region are formed on the semiconductor body through epitaxial growth technology, accurately controlling the film layer thickness and doping concentration, reducing ion implantation damage, and forming a vertical channel structure to improve electron mobility and stability.

Benefits of technology

降低了器件的导通电阻,提升了阈值电压的稳定性,避免了离子注入造成的晶格损伤和导电沟道影响。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119132962A_ABST
    Figure CN119132962A_ABST
Patent Text Reader

Abstract

The invention discloses a power device and a preparation method thereof. The preparation method of the power device comprises the following steps: providing a semiconductor body; the semiconductor body comprises a first surface and a second surface which are oppositely arranged, the semiconductor body further comprises an epitaxial growth well region and an epitaxial growth first region, the first region is arranged on the first surface, and the well region is located on the side, away from the first surface, of the first region; the first region is of a first doping type, and the well region is of a second doping type; forming a gate structure on the first surface of the semiconductor body; the gate structure extends into the semiconductor body from the first surface; forming a source electrode on the first surface of the semiconductor body; and forming a drain electrode on the second surface of the semiconductor body. According to the invention, the ion implantation damage and the on-resistance of the device can be reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of semiconductor devices, and in particular to a power device and a preparation method thereof. Background Art

[0002] The power device may be a silicon carbide (SiC) power device. Compared with silicon (Si) materials, silicon carbide materials have unique performance advantages. They can have higher doping at a thinner epitaxial thickness, and have lower intrinsic carrier concentration. They have excellent withstand voltage characteristics and thermal conductivity. Therefore, silicon carbide devices are more suitable for current and future power electronics applications than traditional silicon devices. However, the process of SiC devices is not yet mature, and the electron mobility is greatly affected by the interface state of the material and the crystal orientation of SiC. At present, in order to achieve higher electron mobility, a trench-type device structure design is usually adopted. Trench-type devices usually use ion implantation to form part of their structure, but the implantation depth of ions in the device is small, which will cause the withstand voltage of the device to be limited. The increase of ion implantation concentration and energy will affect the current channel range, and then affect the on-resistance of the device; and high-energy ion implantation will also cause material defects, increase interface states, and cause ion implantation damage to the material. Summary of the invention

[0003] The invention provides a power device and a preparation method thereof, which can reduce ion implantation damage and the on-resistance of the device.

[0004] According to one aspect of the present invention, there is provided a method for preparing a power device, comprising:

[0005] A semiconductor body is provided; the semiconductor body comprises a first surface and a second surface arranged opposite to each other, the semiconductor body further comprises an epitaxially grown well region and an epitaxially grown first region, the first region is arranged on the first surface, and the well region is located on a side of the first region away from the first surface; the first region is of a first doping type, and the well region is of a second doping type;

[0006] forming a gate structure on a first surface of the semiconductor body; the gate structure extending from the first surface into the semiconductor body;

[0007] forming a source electrode on the first surface of the semiconductor body;

[0008] A drain is formed on the second surface of the semiconductor body.

[0009] Optionally, a semiconductor body is provided, comprising:

[0010] An epitaxial layer is formed on one side of the substrate; the epitaxial layer and the substrate have the same doping type; the substrate is a first doping type;

[0011] forming a well region on a side of the epitaxial layer away from the substrate by epitaxial growth;

[0012] Grinding the surface of the well region away from the epitaxial layer;

[0013] forming a first region on a side of the well region away from the substrate by epitaxial growth;

[0014] A grinding process is performed on a surface of the first region away from the well region.

[0015] Optionally, forming a well region on a side of the epitaxial layer away from the substrate by epitaxial growth includes:

[0016] Silicon and carbon elements are provided, silane and propane are used as reaction gas sources, and boron or aluminum is used as doping element to form a well region on the side of the epitaxial layer away from the substrate.

[0017] Optionally, forming the first region on a side of the well region away from the substrate by epitaxial growth includes:

[0018] Silicon and carbon elements are provided, silane and propane are used as reaction gas sources, and nitrogen, phosphorus or arsenic is used as a doping element to form a first region on a side of the well region away from the substrate.

[0019] Optionally, forming a gate structure on the first surface of the semiconductor body includes:

[0020] A gate groove is formed on the first surface of the semiconductor body; the gate groove extends from the first surface to the inside of the semiconductor body; the gate groove passes through the first region, the well region and a part of the epitaxial layer;

[0021] forming a first insulating layer inside the gate groove;

[0022] A trench gate is formed on a side of the first insulating layer away from the substrate; the trench gate covers the first insulating layer inside the gate groove; the trench gate and the first insulating layer inside the gate groove form a gate structure.

[0023] Optionally, while forming the gate groove on the first surface of the semiconductor body, the method further includes:

[0024] A source groove is formed on the first surface of the semiconductor body; the source groove extends from the first surface to the inside of the semiconductor body; the source groove passes through the first region, the well region and a part of the epitaxial layer;

[0025] After forming a source recess on the first surface of the semiconductor body, the method further includes:

[0026] forming a second region on the sidewall and bottom of the source recess; the second region is of a second doping type;

[0027] While forming the first insulating layer in the gate groove, the method further includes:

[0028] forming a first insulating layer inside the source groove;

[0029] While forming a trench gate on a side of the first insulating layer away from the substrate, the method further comprises:

[0030] A trench source is formed on a side of the first insulating layer away from the substrate, the trench source covers the first insulating layer inside the source groove, and the trench source and the first insulating layer inside the source groove form a source structure.

[0031] Optionally, after forming a gate groove on the first surface of the semiconductor body, the method further includes:

[0032] A second region is formed on the first surface of the semiconductor body; the second region is of a second doping type and extends from the first surface to the inside of the semiconductor body; along the direction from the substrate to the epitaxial layer, the thickness of the second region is greater than or equal to the sum of the thicknesses of the well region and the first region.

[0033] Optionally, after forming the epitaxial layer on one side of the substrate, the method further includes:

[0034] A first sub-region is formed on a surface of the epitaxial layer away from the substrate; the first sub-region extends from the surface of the epitaxial layer away from the substrate to the inside of the epitaxial layer;

[0035] After forming a gate groove on the first surface of the semiconductor body, the method further includes:

[0036] A second sub-region is formed on the first surface of the semiconductor body; a vertical projection of the second sub-region on the substrate coincides with a vertical projection of the first sub-region on the substrate, the first sub-region and the second sub-region are a second area, and the second area is of a second doping type.

[0037] Optionally, after forming a trench gate on a side of the first insulating layer away from the substrate, the method further includes:

[0038] forming a second insulating layer on the first surface of the semiconductor body; the second insulating layer covers the gate structure;

[0039] A source electrode is formed on a first surface of a semiconductor body, comprising:

[0040] A source electrode is formed on a side of the second insulating layer away from the substrate; the source electrode covers the second insulating layer and an area of ​​the first surface of the semiconductor body not covered by the second insulating layer, and the source electrode at least contacts the second area and a part of the first area.

[0041] According to another aspect of the present invention, a power device is provided, which is prepared by the method for preparing a power device according to any embodiment of the present invention.

[0042] The method for preparing a power device provided by the technical solution of the embodiment of the present invention includes: providing a semiconductor body; the semiconductor body includes a first surface and a second surface arranged oppositely, the semiconductor body also includes an epitaxially grown well region and an epitaxially grown first region, the first region is arranged on the first surface, and the well region is located on the side of the first region away from the first surface; the first region is of a first doping type, and the well region is of a second doping type; a gate structure is formed on the first surface of the semiconductor body; the gate structure extends from the first surface into the semiconductor body; a source is formed on the first surface of the semiconductor body; and a drain is formed on the second surface of the semiconductor body. The embodiment of the present invention forms the well region and the first region by epitaxial growth, which can reduce the damage caused by ion implantation, and can accurately control the film thickness and doping concentration of the well region and the first region, which can ensure the stability of the doping concentration, and can also control the channel length, reduce the on-resistance of the device, and improve the stability of the threshold voltage of the device.

[0043] It should be understood that the contents described in this section are not intended to identify the key or important features of the embodiments of the present invention, nor are they intended to limit the scope of the present invention. Other features of the present invention will become easily understood through the following description. BRIEF DESCRIPTION OF THE DRAWINGS

[0044] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0045] Figure 1 It is a flow chart of a method for preparing a power device provided in Example 1 of the present invention.

[0046] Figure 2-Figure 9 It is a schematic diagram of an intermediate structure of a power device provided in Embodiment 1 of the present invention.

[0047] Fig.10 yes Figure 1 A detailed flow chart included in S110.

[0048] Fig.11 yes Figure 1 A detailed flow chart included in S120.

[0049] Figure 12-Figure 17 It is a schematic diagram of an intermediate structure of a power device provided in the second embodiment of the present invention.

[0050] Figure 18-Figure 25 It is a schematic diagram of an intermediate structure of a power device provided in Embodiment 3 of the present invention. DETAILED DESCRIPTION

[0051] In order to enable those skilled in the art to better understand the scheme of the present invention, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.

[0052] It should be noted that the terms "first", "second", etc. in the present invention are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions, for example, a process, method, system, product, or device that includes a series of steps or units is not necessarily limited to those steps or units that are clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products, or devices.

[0053] Embodiment 1

[0054] The embodiment of the present invention provides a method for preparing a power device. Figure 1 is a flow chart of a method for preparing a power device provided in Example 1 of the present invention, with reference to Figure 1 , the preparation method comprises:

[0055] S110. Provide a semiconductor body; the semiconductor body includes a first surface and a second surface arranged opposite to each other, the semiconductor body also includes an epitaxially grown well region and an epitaxially grown first region, the first region is arranged on the first surface, and the well region is located on a side of the first region away from the first surface; the first region is of a first doping type, and the well region is of a second doping type.

[0056] The power device may be a silicon carbide trench metal oxide semiconductor field effect transistor (MOSFET), Figure 2-Figure 9 is a schematic diagram of an intermediate structure of a power device provided in the first embodiment of the present invention, with reference to Figure 2-Figure 9 The semiconductor body 100 may include a substrate 10, an epitaxial layer 20, a well region 30 and a first region 40; the substrate 10 may be a silicon substrate or a silicon carbide substrate, Figure 2If the device is an N-type device, the substrate 10 is an N+ substrate, such as an N+ silicon carbide substrate; the epitaxial layer 20 is an N-epitaxial layer, such as an N-silicon carbide epitaxial layer; if the device is a P-type device, the substrate 10 is a P+ substrate, and the epitaxial layer 20 is a P-epitaxial layer. The epitaxial layer 20 is formed on one side of the substrate 10 by epitaxial growth.

[0057] Specifically, the semiconductor body 100 also includes an epitaxially grown well region 30 and an epitaxially grown first region 40. The well region 30 and the first region 40 are used to form a conductive channel of the power device. The well region 30 can be formed by epitaxial growth on the side of the epitaxial layer 20 away from the substrate 10, and the first region 40 can be formed by epitaxial growth on the side of the well region 30 away from the substrate 10. Compared with the traditional method of forming the well region 30 and the first region 40 by ion implantation, ion implantation is easy to damage the surface where the ions are implanted, causing the device tailing phenomenon and resulting in instability of the threshold voltage of the device; while forming the well region 30 and the first region 40 by epitaxial growth can reduce the damage caused by ion implantation, and can accurately control the film thickness and doping concentration of the well region 30 and the first region 40, which can ensure the stability of the doping concentration, and can also control the channel length, reduce the on-resistance of the device, improve the stability of the threshold voltage of the device, and avoid the lattice damage caused by ion implantation and the influence of injection scattering on the conductive channel.

[0058] S120, forming a gate structure on the first surface of the semiconductor body; the gate structure extends from the first surface into the semiconductor body.

[0059] Among them, reference Figure 7 The gate structure may include a first insulating layer 60 and a trench gate 70. The first insulating layer 60 may be a gate oxide layer, and the gate oxide layer may be a high dielectric constant (K) material; the trench gate 70 may be a polysilicon layer; Figure 4 , a gate groove 31 can be etched on the first surface of the semiconductor body, and the gate groove 31 extends from the first surface to the inside of the semiconductor body; the gate structure extends from the first surface to the inside of the semiconductor body, which can make the device have a larger channel mobility, and the conductive channel is a vertical channel, which can eliminate the junction field-effect transistor (JFET) area and make the device lower in on-resistance. The density of the vertical trench gate is high, which can reduce the cell spacing and increase the current density.

[0060] S130 , forming a source on the first surface of the semiconductor body.

[0061] Among them, reference Fig. 9The source electrode 102 may be formed on the first surface of the semiconductor body by sputtering or the like. The source electrode 102 is a metal conductive layer. Exemplarily, the metal conductive layer may be titanium (Ti), nickel (Ni) or silver (Ag).

[0062] S140, forming a drain on the second surface of the semiconductor body.

[0063] Among them, reference Fig. 9 , a drain electrode 103 can be formed on the first surface of the semiconductor body by sputtering or the like. The drain electrode 103 is a metal conductive layer. For example, the metal conductive layer can be titanium (Ti), nickel (Ni) or silver (Ag). The drain electrode 103 is located on the surface of the substrate 10 away from the epitaxial layer 20. The surface of the substrate 10 away from the epitaxial layer 20 is first thinned, and then the drain electrode 103 is formed by sputtering or the like.

[0064] The method for preparing a power device provided by the technical solution of the embodiment of the present invention includes: providing a semiconductor body; the semiconductor body includes a first surface and a second surface arranged oppositely, the semiconductor body also includes an epitaxially grown well region and an epitaxially grown first region, the first region is arranged on the first surface, and the well region is located on the side of the first region away from the first surface; the first region is of a first doping type, and the well region is of a second doping type; a gate structure is formed on the first surface of the semiconductor body; the gate structure extends from the first surface into the semiconductor body; a source is formed on the first surface of the semiconductor body; and a drain is formed on the second surface of the semiconductor body. The embodiment of the present invention forms the well region and the first region by epitaxial growth, which can reduce the damage caused by ion implantation, and can accurately control the film thickness and doping concentration of the well region and the first region, which can ensure the stability of the doping concentration, and can also control the channel length, reduce the on-resistance of the device, and improve the stability of the threshold voltage of the device.

[0065] Optional, Fig.10 yes Figure 1 A detailed flow chart included in S110, refer to Fig.10 , S110, providing a semiconductor body, including:

[0066] S111, forming an epitaxial layer on one side of a substrate; the epitaxial layer and the substrate have the same doping type; the substrate is of a first doping type.

[0067] Among them, reference Figure 2 , epitaxially grow an epitaxial layer 20 on one side of the substrate 10, and the material of the epitaxial layer 20 can be silicon carbide; the substrate 10 is grown at a high temperature of 1000°C to 1600°C, and the protective gas and etching gas required during the growth process can be argon, nitrogen or hydrogen; the chamber pressure is 10 3 Pa~107 Pa.

[0068] S112, forming a well region on a side of the epitaxial layer away from the substrate by epitaxial growth.

[0069] Among them, reference Figure 3 If the material of the well region 30 is silicon carbide, during the growth process of silicon carbide, silicon and carbon elements are provided, silane and propane are used as reaction gas sources, and boron or aluminum elements are used as doping elements to form the well region 30 on the side of the epitaxial layer away from the substrate. If the power device is an N-type power device, the well region 30 can be a P-type well region.

[0070] S113, grinding the surface of the well region away from the epitaxial layer.

[0071] Among them, by grinding the surface of the well region away from the epitaxial layer through chemical mechanical polishing (CMP), defects on the surface of the well region away from the substrate can be removed, and the thickness of the well region can be thinned to a first preset thickness. The first preset thickness is the thickness of the well region that meets the specification requirements, thereby improving the stability of the threshold voltage.

[0072] S114 , forming a first region on a side of the well region away from the substrate by epitaxial growth.

[0073] Among them, reference Figure 3 If the material of the first region 40 is silicon carbide, during the growth process of silicon carbide, silicon and carbon elements are provided, silane and propane are used as reaction gas sources, and nitrogen, phosphorus or arsenic are used as doping elements to form the first region 40 on the side of the well region 30 away from the substrate 10; if the power device is an N-type power device, the first region 40 can be an N-type region.

[0074] S115, grinding the surface of the first region away from the well region.

[0075] Among them, by grinding the surface of the first region away from the well region through chemical mechanical grinding, defects on the surface of the first region away from the substrate can be removed, and the thickness of the first region can be thinned to a second preset thickness. The second preset thickness is the thickness of the first region that meets the specification requirements, thereby improving the stability of the device threshold voltage.

[0076] Optionally, a well region is formed on a side of the epitaxial layer away from the substrate by epitaxial growth, including: providing silicon and carbon elements, using silane and propane as reaction gas sources, and boron or aluminum as doping elements to form a well region on a side of the epitaxial layer away from the substrate.

[0077] Among them, the embodiment of the present invention provides specific epitaxial process conditions for forming the well region. Forming the well region by epitaxial growth can ensure that the doping concentration of the well region is uniform and stable.

[0078] Optionally, a first region is formed on a side of the well region away from the substrate by epitaxial growth, including: providing silicon and carbon elements, using silane and propane as reaction gas sources, and nitrogen, phosphorus or arsenic as doping elements to form the first region on a side of the well region away from the substrate.

[0079] The embodiment of the present invention provides specific epitaxial process conditions for forming the first region. Forming the first region by epitaxial growth can ensure that the doping concentration of the first region is uniform and stable.

[0080] Optional, Fig.11 yes Figure 1 A detailed flow chart included in S120, refer to Fig.11 , S120, forming a gate structure on the first surface of the semiconductor body, including:

[0081] S121, forming a gate groove on the first surface of the semiconductor body; the gate groove extends from the first surface to the inside of the semiconductor body; the gate groove penetrates the first region, the well region and part of the epitaxial layer.

[0082] Among them, reference Figure 4 , a gate groove is formed on the first surface of the semiconductor body through an etching process.

[0083] S122 , forming a first insulating layer inside the gate groove.

[0084] Among them, reference Figure 6 A first insulating layer 60 is deposited inside the gate groove 31 by atomic layer deposition (ALD) or the like. The first insulating layer 60 inside the gate groove 31 may be a gate oxide layer. The gate oxide layer may be a high-K material, which may improve the electron mobility at the trench gate interface and reduce the on-resistance of the device.

[0085] S123, forming a trench gate on a side of the first insulating layer away from the substrate; the trench gate covers the first insulating layer inside the gate groove; the trench gate and the first insulating layer inside the gate groove constitute a gate structure.

[0086] Among them, reference Figure 7 The trench gate 70 is deposited by low pressure chemical vapor deposition (LPCVD) or the like, and the material of the trench gate 70 may be polysilicon.

[0087] Optionally, S121, while forming a gate groove on the first surface of the semiconductor body, also includes: forming a source groove on the first surface of the semiconductor body; the source groove extends from the first surface to the inside of the semiconductor body; the source groove passes through the first region, the well region and part of the epitaxial layer.

[0088] Among them, reference Figure 4 A source groove 32 can be formed on both sides of the gate groove 31, and the source groove 32 and the gate groove 31 are formed simultaneously by using the same trench etching process. The same process and simultaneous formation can shorten the process time and reduce the process cost.

[0089] After forming a source groove on the first surface of the semiconductor body, the method further includes: forming a second region on the sidewall and bottom of the source groove; the second region is of a second doping type.

[0090] Among them, reference Figure 5 , a second region 50 is formed on the sidewall and bottom of the source groove by ion implantation. If the power device is an N-type power device, the second region is a P-type region. The cavity pressure is 10 3 ~10 7 Pa, the energy of P-type ion implantation is 10Kev~800Kev, and the dose of ion implantation is 1*10 14~30 .

[0091] Optionally, S122, while forming a first insulating layer inside the gate groove, also includes: forming a first insulating layer inside the source groove.

[0092] Among them, reference Figure 6 , and at the same time, a first insulating layer is formed inside the source groove and the gate groove; a whole first insulating layer 60 can be deposited by atomic layer deposition (ALD) and the like, and the whole first insulating layer 60 covers the inside of the gate groove 32, the inside of the gate groove 31 and the surface of the first region away from the substrate, and then the first insulating layer 60 is etched to retain only the first insulating layer 60 inside the source groove 32 and the gate groove 31.

[0093] Optionally, S123, while forming a trench gate on the side of the first insulating layer away from the substrate, also includes: forming a trench source on the side of the first insulating layer away from the substrate, the trench source covers the first insulating layer inside the source groove, and the trench source and the first insulating layer inside the source groove are a source structure.

[0094] Among them, reference Figure 7 A trench source 71 and a trench gate 70 are simultaneously formed on a side of the first insulating layer 60 away from the substrate 10 , and the materials of the trench source 71 and the trench gate 70 are both polysilicon.

[0095] The method for preparing the power device in the embodiment of the present invention specifically comprises: referring to Figure 2 , preparing a substrate 10; growing an epitaxial layer 20 on the substrate 10, referring to Figure 3 , forming a well region 30 on the side of the epitaxial layer 20 away from the substrate 10; removing surface defects of the well region by CMP and thinning to a first preset thickness; forming a first region 40 on the side of the well region 30 away from the substrate 10; removing surface defects of the first region by CMP and thinning to a second preset thickness; referring to Figure 4 , and simultaneously forming a gate groove 31 and a source groove 32; Figure 5 , ion implantation is performed on the sidewall and bottom of the source recess 32 to form a second region 50; Figure 6 , a first insulating layer 60 is formed inside the gate groove 31 and the source groove 32, and the first insulating layer 60 covers the second region 50 inside the source groove 32 and the sidewall and bottom of the gate groove 31; Figure 7 , a trench gate 70 and a trench source 71 are formed on the side of the first insulating layer 60 away from the substrate 10; Figure 8 , and then a second insulating layer 101 is formed on the surface of the first region 40 away from the substrate 10, the second insulating layer 101 is an interlayer dielectric layer (Inter Layer Dielectric, ILD), and the second insulating layer 101 is used to isolate the gate structure and the source; Fig. 9 A source 102 is formed on a surface of the second insulating layer 101 away from the substrate 10 , and a drain 103 is formed on a side of the substrate 10 away from the epitaxial layer 20 .

[0096] Embodiment 2

[0097] The present invention further provides a method for preparing a power device based on the above embodiments. The method also includes S111-S115 and S121-S123 as well as a specific process for forming a well region and a first region.

[0098] The difference from the preparation method of the above embodiment is that:

[0099] Figure 12-Figure 17 is a schematic diagram of an intermediate structure of a power device provided in the second embodiment of the present invention, with reference to Figure 12-Figure 17 Optionally, after forming a gate groove on the first surface of the semiconductor body, the method further includes:

[0100] A second region is formed on the first surface of the semiconductor body; the second region is of a second doping type and extends from the first surface to the inside of the semiconductor body; along the direction from the substrate to the epitaxial layer, the thickness of the second region is greater than or equal to the sum of the thicknesses of the well region and the first region.

[0101] Among them, reference Fig.13, a second region is formed on both sides of the gate groove, the second region is a second doping type, and the second region is formed on the first surface of the semiconductor body by ion implantation; if the power device is an N-type power device, the second region is a P-type region, and the cavity pressure is 10 3 ~10 7 Pa, the energy of P-type ion implantation is 10Kev~800Kev, and the dose of ion implantation is 1*10 14~30 .

[0102] The method for preparing the power device in the embodiment of the present invention specifically comprises: referring to Figure 2 , preparing a substrate 10; growing an epitaxial layer 20 on the substrate 10, referring to Figure 3 , forming a well region 30 on the side of the epitaxial layer 20 away from the substrate 10; removing surface defects of the well region by CMP and thinning to a first preset thickness; forming a first region 40 on the side of the well region 30 away from the substrate 10; removing surface defects of the first region by CMP and thinning to a second preset thickness; referring to Fig.12 , a gate groove 31 is formed by trench etching; Fig.13 , ion implantation is performed on both sides of the gate groove 31 to form a second region 50; Fig.14 , a first insulating layer 60 is formed inside the gate groove 31, and the first insulating layer 60 covers the sidewall and the bottom of the gate groove 31; Fig.15 , a trench gate 70 is formed on a side of the first insulating layer 60 away from the substrate 10; Fig.16 , and then a second insulating layer 101 is formed on the surface of the first region 40 away from the substrate 10, the second insulating layer 101 is an ILD layer, and the second insulating layer 101 is used to isolate the gate structure and the source; Fig.17 , a source electrode 102 is formed on the surface of the second insulating layer 101 away from the substrate 10, the surface of the substrate 10 away from the epitaxial layer 20 is thinned, and a drain electrode 103 is formed on the side of the substrate 10 away from the epitaxial layer 20. The embodiment of the present invention forms the well region and the first region by epitaxial growth, which can reduce the damage caused by ion implantation, and can accurately control the film thickness and doping concentration of the well region and the first region, which can ensure the stability of the doping concentration, and can also control the channel length, reduce the on-resistance of the device, and improve the stability of the threshold voltage of the device.

[0103] Embodiment 3

[0104] The present invention further provides a method for preparing a power device based on the above embodiments. The method also includes S111-S115 and S121-S123 as well as a specific process for forming a well region and a first region.

[0105] The difference from the preparation method of the above embodiment is that:

[0106] Figure 18-Figure 25 is a schematic diagram of an intermediate structure of a power device provided in the third embodiment of the present invention, with reference to Figure 18-Figure 25 Optionally, after forming the epitaxial layer on one side of the substrate, it also includes: forming a first sub-region on the surface of the epitaxial layer away from the substrate; the first sub-region extends from the surface of the epitaxial layer away from the substrate to the inside of the epitaxial layer.

[0107] Among them, reference Fig.18 , a first sub-region 51 is formed on the surface of the epitaxial layer 20 away from the substrate 10 by an ion implantation process. If the power device is an N-type power device, the second region is a P-type region. The cavity pressure is 10 3 ~10 7 Pa, the energy of P-type ion implantation is 10Kev~800Kev, and the dose of ion implantation is 1*10 14~30 .

[0108] After forming a gate groove on the first surface of the semiconductor body, it also includes: forming a second sub-region on the first surface of the semiconductor body; the vertical projection of the second sub-region on the substrate coincides with the vertical projection of the first sub-region on the substrate, the first sub-region and the second sub-region are the second area, and the second area is the second doping type.

[0109] Among them, reference Fig.21 , a second sub-region 52 is formed on the surface of the first region 40 away from the substrate 10 by an ion implantation process. If the power device is an N-type power device, the second region is a P-type region. The chamber pressure is 10 3 ~10 7 Pa, the energy of P-type ion implantation is 10Kev~800Kev, and the dose of ion implantation is 1*10 14~30 .

[0110] Optionally, after forming a trench gate on a side of the first insulating layer away from the substrate, the method further includes: forming a second insulating layer on the first surface of the semiconductor body; and the second insulating layer covers the gate structure.

[0111] The second insulating layer 101 may be deposited by atomic layer deposition (ALD) or the like, and the second insulating layer 101 is an ILD layer for isolating the gate structure and the source.

[0112] A source is formed on the first surface of the semiconductor body, including: forming a source on a side of the second insulating layer away from the substrate; the source covers the second insulating layer and the area of ​​the first surface of the semiconductor body not covered by the second insulating layer, and the source is in contact with at least the second area and part of the first area.

[0113] Among them, reference Fig.25, a source electrode 102 can be formed on the side of the second insulating layer 101 away from the substrate 10 by sputtering or the like. The source electrode 102 is a metal conductive layer. For example, the metal conductive layer can be titanium (Ti), nickel (Ni) or silver (Ag). The drain electrode 103 is located on the surface of the substrate 10 away from the epitaxial layer 20. The surface of the substrate 10 away from the epitaxial layer 20 is first thinned, and then the drain electrode 103 is formed by sputtering or the like.

[0114] The method for preparing the power device in the embodiment of the present invention specifically comprises: referring to Figure 2 , preparing a substrate 10; growing an epitaxial layer 20 on the substrate 10, referring to Fig.18 , a first sub-region 51 is formed on the surface of the epitaxial layer 20 away from the substrate 10 by an ion implantation process; Fig.19 , forming a well region 30 on the side of the epitaxial layer 20 away from the substrate 10; removing surface defects of the well region by CMP and thinning to a first preset thickness; forming a first region 40 on the side of the well region 30 away from the substrate 10; removing surface defects of the first region by CMP and thinning to a second preset thickness; referring to Fig. 20 , a gate groove 31 is formed by trench etching; Fig.21 , ion implantation is performed on a side of the first sub-region 51 away from the substrate to form a second sub-region 52, and the first sub-region 51 and the second sub-region 52 are the second region; Fig. 22 , a first insulating layer 60 is formed inside the gate groove 31, and the first insulating layer 60 covers the sidewall and the bottom of the gate groove 31; Fig.23 , a trench gate 70 is formed on a side of the first insulating layer 60 away from the substrate 10; Fig.24 , a second insulating layer 101 is formed on the surface of the first region 40 away from the substrate 10, the second insulating layer 101 is an ILD layer, and the second insulating layer 101 is used to isolate the gate structure and the source; Fig.25 , a source electrode 102 is formed on the surface of the second insulating layer 101 away from the substrate 10, the surface of the substrate 10 away from the epitaxial layer 20 is thinned, and then a drain electrode 103 is formed on the side of the substrate 10 away from the epitaxial layer 20. The embodiment of the present invention forms the well region and the first region by epitaxial growth, which can reduce the damage caused by ion implantation, and can accurately control the film thickness and doping concentration of the well region and the first region, which can ensure the stability of the doping concentration, and can also control the channel length, reduce the on-resistance of the device, and improve the stability of the threshold voltage of the device.

[0115] An embodiment of the present invention provides a power device based on the above embodiments, which is prepared by using the method for preparing a power device described in any embodiment of the present invention.

[0116] The power device provided by the technical solution of the embodiment of the present invention has the same beneficial effects as the method for preparing the power device described in any embodiment of the present invention.

[0117] It should be understood that the various forms of processes shown above can be used to reorder, add or delete steps. For example, the steps described in the present invention can be executed in parallel, sequentially or in different orders, as long as the desired results of the technical solution of the present invention can be achieved, and this document does not limit this.

[0118] The above specific implementations do not constitute a limitation on the protection scope of the present invention. It should be understood by those skilled in the art that various modifications, combinations, sub-combinations and substitutions can be made according to design requirements and other factors. Any modification, equivalent substitution and improvement made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for preparing a power device, characterized in that: include: A semiconductor body is provided; the semiconductor body comprises a first surface and a second surface arranged opposite to each other, the semiconductor body further comprises an epitaxially grown well region and an epitaxially grown first region, the first region is arranged on the first surface, and the well region is located on a side of the first region away from the first surface; the first region is of a first doping type, and the well region is of a second doping type; forming a gate structure on the first surface of the semiconductor body; the gate structure extending from the first surface into the semiconductor body; forming a source electrode on the first surface of the semiconductor body; A drain is formed on the second surface of the semiconductor body.

2. The preparation method according to claim 1, characterized in that: Provide a semiconductor body, including: An epitaxial layer is formed on one side of a substrate; the epitaxial layer and the substrate have the same doping type; the substrate is a first doping type; forming a well region on a side of the epitaxial layer away from the substrate by epitaxial growth; Grinding the surface of the well region away from the epitaxial layer; forming a first region on a side of the well region away from the substrate by epitaxial growth; A grinding process is performed on a surface of the first region away from the well region.

3. The preparation method according to claim 2, characterized in that: Forming a well region on a side of the epitaxial layer away from the substrate by epitaxial growth, comprising: Silicon and carbon elements are provided, silane and propane are used as reaction gas sources, and boron or aluminum is used as doping element to form a well region on a side of the epitaxial layer away from the substrate.

4. The preparation method according to claim 2, characterized in that: Forming a first region on a side of the well region away from the substrate by epitaxial growth, comprising: Silicon and carbon elements are provided, silane and propane are used as reaction gas sources, and nitrogen, phosphorus or arsenic is used as doping elements to form a first region on a side of the well region away from the substrate.

5. The preparation method according to claim 2, characterized in that: Forming a gate structure on the first surface of the semiconductor body, comprising: A gate groove is formed on the first surface of the semiconductor body; the gate groove extends from the first surface to the inside of the semiconductor body; the gate groove passes through the first region, the well region and a part of the epitaxial layer; forming a first insulating layer inside the gate groove; A trench gate is formed on a side of the first insulating layer away from the substrate; the trench gate covers the first insulating layer inside the gate groove; the trench gate and the first insulating layer inside the gate groove form a gate structure.

6. The preparation method according to claim 5, characterized in that: While forming a gate groove on the first surface of the semiconductor body, the method further includes: A source groove is formed on the first surface of the semiconductor body; the source groove extends from the first surface to the inside of the semiconductor body; the source groove passes through the first region, the well region and a part of the epitaxial layer; After forming a source groove on the first surface of the semiconductor body, the method further includes: forming a second region on the sidewall and bottom of the source groove; the second region is of a second doping type; While forming a first insulating layer inside the gate groove, the method further includes: forming a first insulating layer inside the source groove; While forming a trench gate on a side of the first insulating layer away from the substrate, the method further comprises: A trench source is formed on a side of the first insulating layer away from the substrate, the trench source covers the first insulating layer inside the source groove, and the trench source and the first insulating layer inside the source groove form a source structure.

7. The preparation method according to claim 5, characterized in that: After forming a gate groove on the first surface of the semiconductor body, the method further includes: A second region is formed on the first surface of the semiconductor body; the second region is of a second doping type and extends from the first surface to the inside of the semiconductor body; along the direction from the substrate to the epitaxial layer, the thickness of the second region is greater than or equal to the sum of the thicknesses of the well region and the first region.

8. The preparation method according to claim 5, characterized in that: After forming an epitaxial layer on one side of the substrate, the method further includes: forming a first sub-region on a surface of the epitaxial layer away from the substrate; the first sub-region extends from the surface of the epitaxial layer away from the substrate to the inside of the epitaxial layer; After forming a gate groove on the first surface of the semiconductor body, the method further includes: A second sub-region is formed on the first surface of the semiconductor body; a vertical projection of the second sub-region on the substrate coincides with a vertical projection of the first sub-region on the substrate, the first sub-region and the second sub-region are a second area, and the second area is of a second doping type.

9. The preparation method according to claim 5, characterized in that: After forming a trench gate on a side of the first insulating layer away from the substrate, the method further includes: forming a second insulating layer on the first surface of the semiconductor body; the second insulating layer covers the gate structure; Forming a source electrode on the first surface of the semiconductor body, comprising: A source is formed on a side of the second insulating layer away from the substrate; the source covers the second insulating layer and an area of ​​the first surface of the semiconductor body not covered by the second insulating layer, and the source is in contact with at least the second area and a portion of the first area.

10. A power device, characterized in that: The power device is prepared by the method for preparing the power device according to any one of claims 1 to 9.

Citation Information

Patent Citations

  • Vertical self-align suspending drain MOS audion and its making method

    CN101017823A

  • Source region self-aligned vertical channel metal oxide semiconductor (MOS) integrated circuit unit and implementation method thereof

    CN113013234A

  • Super-self-aligned trench-DMOS structure and method

    US20100032751A1

  • Avalanche capability improvement in power semiconductor devices

    US20110233606A1

  • Silicon Carbide Trench Gate MOSFET and Method for Manufacturing Thereof

    US20230130726A1