Package and electronic device

By designing the convex structure and coating of the heat dissipation cover in the package to prevent the soldering material from overflowing, the problem of welding material overflowing during the assembly of the chip and the heat dissipating cover is solved, the heat dissipation effect and product yield are improved, and the weight of the package is reduced .

CN221805502UActive Publication Date: 2024-10-01SUZHOU TF AMD SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323546410.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-25
Publication Date
2024-10-01
Estimated Expiration
2033-12-25

AI Technical Summary

Technical Problem

When assembling the chip with the heat dissipation cover, the product yield is low, mainly due to the high probability of solder material overflow, resulting in poor heat dissipation and short circuits between the chip and external components.

Method used

Design a package. The heat dissipation cover is provided with protrusions toward the surface of the substrate. The protrusions are located on the orthogonal projection periphery of the substrate. The welding part is a concave curved surface. The density of the peripheral part is smaller than that of the welding part. It is protected by a nickel-plated gold layer. The surface of the welding part is rough. The thickness is larger than that of the peripheral part, and the protrusion height is 200 microns to 300 microns, which is used to prevent the flow of soldering materials and reduce the weight of the package.

Benefits of technology

It effectively reduces the probability of solder material overflow, improves heat dissipation, avoids short circuits between chips and external components, improves product yield, and improves product quality by reducing the weight of the package.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221805502U_ABST
    Figure CN221805502U_ABST
Patent Text Reader

Abstract

The utility model discloses a packaging body and electronic equipment. The packaging body comprises a substrate, a heat dissipation cover, a chip and a welding layer, the heat dissipation cover is arranged on the substrate, and an accommodating space is formed between the heat dissipation cover and the substrate; the chip is arranged on the substrate and located in the containing space, the functional surface of the chip faces the substrate, and the non-functional surface of the chip faces the heat dissipation cover; the welding layer is positioned between the heat dissipation cover and the chip and is used for connecting the heat dissipation cover and the chip; the surface, facing the substrate, of the heat dissipation cover is provided with a protrusion, the protrusion is located in the containing space, and the orthographic projection, on the substrate, of the protrusion is located on the periphery of the orthographic projection, on the substrate, of the chip. Wherein the heat dissipation cover comprises a welding part and a peripheral part, the welding part is connected with the chip through a welding layer, and the peripheral part is arranged on the periphery of the welding part and connected with the welding part; wherein the surface, facing the substrate, of the welding part is a concave curved surface, and the density of the peripheral part is smaller than that of the welding part. In this way, the product yield can be guaranteed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor technology, and in particular to a package and an electronic device. Background Art

[0002] Chip heat dissipation has always been an important topic in the semiconductor industry. Chips with high heat dissipation requirements often use a combination of thermal interface materials and heat dissipation covers to ensure heat dissipation. However, the inventors of this application have found that when assembling a chip and a heat dissipation cover together, there is a defect of low product yield. Utility Model Content

[0003] The main technical problem solved by the present application is to provide a package and an electronic device, which can reduce the probability of welding material overflow during the packaging process, and at the same time reduce the weight of the package to ensure product yield.

[0004] In order to solve the above technical problems, a technical solution adopted in the present application is: to provide a package, the package includes a substrate, a heat dissipation cover, a chip and a welding layer; the heat dissipation cover is arranged on the substrate and forms a containing space between the heat dissipation cover and the substrate; the chip is arranged on the substrate and located in the containing space, the functional surface of the chip faces the substrate, and the non-functional surface faces the heat dissipation cover; the welding layer is located between the heat dissipation cover and the chip, connecting the heat dissipation cover and the chip; wherein, a protrusion is arranged on the surface of the heat dissipation cover facing the substrate, the protrusion is located in the containing space, and the orthographic projection of the protrusion on the substrate is located at the periphery of the orthographic projection of the chip on the substrate; wherein, the heat dissipation cover includes a welding part and a peripheral part, the welding part is connected to the chip through the welding layer; the peripheral part is arranged at the periphery of the welding part and connected to the welding part; wherein, the surface of the welding part facing the substrate is a concave curved surface, and\or the density of the peripheral part is less than the density of the welding part.

[0005] The protrusion is in a ring structure, and the orthographic projection of the protrusion on the substrate surrounds the orthographic projection of the chip on the substrate.

[0006] Wherein, a surface of the protrusion facing the substrate is flush with a surface of the welding layer facing the substrate.

[0007] The package body further includes a first bump and a second bump, wherein the first bump is arranged between the substrate and the chip, and the second bump is arranged on a side of the substrate away from the heat dissipation cover.

[0008] Wherein, the roughness of the welding portion facing the substrate surface is greater than the roughness of the protruding surface.

[0009] The roughness of the surface of the welding portion facing the chip is in a range of 2.0 microns to 3.5 microns.

[0010] Wherein, the protrusion is integrally formed with the peripheral portion; and / or, a groove is formed on the surface of the peripheral portion and the welding portion, and a portion of the welding portion extends into the groove.

[0011] A plating layer is formed on the surface of the welding part, and the plating layer includes: a nickel layer covering the entire surface of the welding part; and a gold layer formed on the nickel layer located in the accommodating space.

[0012] Wherein, the height of the protrusion ranges from 200 microns to 300 microns.

[0013] In order to solve the above technical problem, another technical solution adopted in the present application is: to provide an electronic device, including a circuit board and a packaging body as described above welded on the circuit board.

[0014] The beneficial effect of the present application is as follows: different from the prior art, the heat dissipation cover of the present application is provided with a protrusion on the surface facing the substrate, and the orthographic projection of the protrusion on the substrate is located at the periphery of the orthographic projection of the chip on the substrate. During the packaging process, when the welding material used for the welding layer is in a molten state, the protrusion will prevent the flow of the welding material, which can reduce the probability of welding material overflow, thereby reducing the porosity of the welding layer, thereby improving the heat dissipation effect of the heat dissipation cover, and preventing the welding material from overflowing and causing a bridge short circuit between the chip and the external components. At the same time, the density of the outer portion of the package body is less than the density of the welding portion, which reduces the quality of the package body relative to the situation where the outer portion and the welding portion have the same density, and can improve the yield of the product. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work. Among them:

[0016] Figure 1 It is a structural schematic diagram of an implementation method of a package body of the present application;

[0017] Figure 2 yes Figure 1 A schematic structural diagram of an embodiment of a heat dissipation cover;

[0018] Figure 3 It is a schematic structural diagram of an embodiment of an electronic device of the present application. DETAILED DESCRIPTION

[0019] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0020] See also Figure 1 The package body 100 includes a substrate 1, a heat dissipation cover 2, a chip 3 and a welding layer 4.

[0021] The heat dissipation cover 2 is fixed to the substrate 1 by adhesive, and a containing space 11 is formed between the heat dissipation cover 2 and the substrate 1. The chip 3 is arranged on the substrate 1 and is located in the containing space 11. Specifically, the substrate 1 plays a supporting role in the package body 100, and it can be one of a BGA package substrate, a CSP package substrate, an FC package substrate and an MCM package substrate. At the same time, various circuits (not shown) are formed on the substrate 1 for signal transmission with the chip 3. At the same time, the material of the heat dissipation cover 2 includes one of silver, copper, aluminum and iron, which plays a role in quickly conducting the heat generated by the chip 3.

[0022] The chip 3 is disposed on the substrate 1 and is located in the accommodating space 11, and the functional surface 31 of the chip 3 faces the substrate 1, and the non-functional surface 32 faces the heat dissipation cover 2. Specifically, the chip 3 outputs or inputs signals through the functional surface 31, and the non-functional surface 32 is disposed opposite to the functional surface 31. The functional surface 31 of the chip 3 is electrically connected to the substrate 1 for inputting or outputting signals to the substrate 1, and the non-functional surface 32 of the chip 3 is connected to the heat dissipation cover 2 for fixing the position between the heat dissipation cover 2 and the chip 3, and for heat dissipation of the chip 3.

[0023] The welding layer 4 is located between the heat dissipation cover 2 and the chip 3, and connects the heat dissipation cover 2 and the chip 3. Specifically, the welding layer 4 is used to realize the electrical connection between the heat dissipation cover 2 and the chip 3, and fix the heat dissipation cover 2 and the chip 3. The material of the welding layer 4 includes at least one of indium and solder, which is not limited here.

[0024] A protrusion 21 is disposed on the surface of the heat dissipation cover 2 facing the substrate 1 . The protrusion 21 is located in the accommodating space 11 , and the orthographic projection of the protrusion 21 on the substrate 1 is located at the periphery of the orthographic projection of the chip 3 on the substrate 1 .

[0025] Specifically, the protrusion 21 is arranged on the heat dissipation cover 2 and is located at the periphery of the chip 3, so that during the package reflow soldering process, Figure 1As shown, the package body 100 is inverted and enters the reflow furnace, that is, the substrate 1 is on the top and the heat dissipation cover 2 is on the bottom. When the welding material used for the welding layer 4 is in a molten state due to heat, the protrusion 21 will prevent the flow of the welding material, which can reduce the probability of the welding material overflowing, thereby reducing the porosity of the welding layer 4, thereby improving the heat dissipation effect of the heat dissipation cover 2, and preventing the welding material from splashing onto the surface of the capacitor 7 on the substrate 1 and causing the solder on the surface of the capacitor 7 to short-circuit and fail.

[0026] Continue reading Figure 1 The heat dissipation cover 2 includes a welding portion 22 and a peripheral portion 23. The welding portion 22 is connected to the chip 3 through the welding layer 4; the peripheral portion 23 is arranged at the periphery of the welding portion 22 and connected to the welding portion 22, wherein the surface of the welding portion 22 facing the substrate 1 is a concave curved surface.

[0027] Specifically, the heat dissipation cover 2 includes a welding portion 22 and a peripheral portion 23. The welding portion 22 is connected to the chip 3, and the peripheral portion 23 is not connected to the chip 3 and the substrate 1 through an adhesive. At the same time, the surface of the welding portion 22 facing the substrate 1, that is, the surface where the welding portion 22 is connected to the chip 3 is a concave curved surface, so that during the packaging process, when the package body 100 is Figure 1 When the soldering material is placed in the reflow oven in the inverted state, the soldering material will flow to the lowest point of the curved surface of the soldering portion 22 in the molten state (the flow direction is Figure 1 In the direction indicated by the arrow in the figure), the welding material can be further prevented from overflowing the area outside the welding portion 22.

[0028] In one embodiment, the density of the peripheral portion 23 is less than the density of the soldering portion 22. Specifically, the material of the peripheral portion 23 is selected to be a material with a lower density than the material of the soldering portion 22, which can reduce the weight of the heat dissipation cover 2. When the size of the chip 3 is larger, the size of the required heat dissipation cover 2 is also larger, and the weight of the package 100 is also heavier. When the package 100 is soldered on the PCB board, selecting a heat dissipation cover 2 with a lower density of the peripheral portion 23 can reduce the weight of the heat dissipation cover 2, thereby reducing the weight of the package 100 and reducing the probability of the second bump 52 collapsing.

[0029] In one application scenario, the material of the welding portion 22 is copper, and the material of the peripheral portion 23 is a resin material. Compared with copper, the resin material has a lower density and can reduce the overall weight of the heat dissipation cover 2. In other application scenarios, graphene, plastic composite materials or other lightweight materials can also be selected as the material of the peripheral portion 23.

[0030] Continue reading Figure 1 The protrusion 21 is in a ring structure, and the orthographic projection of the protrusion 21 on the substrate 1 surrounds the orthographic projection of the chip 3 on the substrate 1 .

[0031] Specifically, the protrusion 21 is an annular structure, that is, a fully enclosed structure, which surrounds the chip 3. Therefore, during the packaging reflow process, the protrusion 21 can prevent the overflow of the welding material 360°, so that the welding material forms a welding layer 4 within the range of the protrusion 21, and further prevents the welding material from splashing onto the surface of the capacitor 7, causing the solder on the surface of the capacitor 7 to short-circuit and fail.

[0032] Of course, in other embodiments, the protrusion 21 may also be a semi-enclosed structure, which can also prevent the overflow of the welding material to a certain extent. For example, in one application scenario, there are multiple protrusions 21, and the multiple protrusions 21 are arranged at intervals along the periphery of the chip 3.

[0033] Continue reading Figure 1 The package body 100 further includes a first bump 51 and a second bump 52 .

[0034] The first bump 51 is arranged between the substrate 1 and the chip 3, and is used for the electrical connection between the substrate 1 and the chip 3. A bottom filling glue 6 wrapping the first bump 51 is also arranged between the substrate 1 and the chip 3 to protect the first bump 51 and strengthen the fixation between the substrate 1 and the chip 3; the second bump 52 is arranged on the side of the substrate 1 away from the heat dissipation cover 2, and is used for the electrical connection between the substrate 1 and other electronic devices. Among them, the materials of the first bump 51 and the second bump 52 can be the same or different. In an application scenario, the materials of the first bump 51 and the second bump 52 include at least one of copper, steel, and tin.

[0035] See also Figure 2 In one embodiment, the protrusion 21 and the peripheral portion 23 are integrally formed. That is, the protrusion 21 and the peripheral portion 23 are formed by simultaneous processing and cannot be disassembled and assembled from each other. In the process of processing the peripheral portion 23, a mold of a corresponding shape is selected to form the peripheral portion 23 and the protrusion 21 as an integral whole. Integrating the peripheral portion 23 by a mold can reduce the waste of materials and energy, reduce production costs, and can also further reduce the weight of the heat dissipation cover 2.

[0036] Of course, in other embodiments, the protrusion 21 may also be integrally formed with the welding portion 22 .

[0037] Continue reading Figure 2 In one embodiment, a groove 24 is formed in the contact area between the peripheral portion 23 and the welding portion 22, and a portion of the welding portion 22 extends into the groove 24. Specifically, the peripheral portion 23 and the welding portion 22 are in a detachable combination, and the groove 24 is provided in the peripheral portion 23, and a portion of the welding portion 22 can extend into the groove 24, which can ensure the connection strength between the peripheral portion 23 and the welding portion 22 and prevent the two from being separated.

[0038] Of course, in other embodiments, the outer portion 23 may not be provided with the groove 24. In this case, the outer portion 23 and the welding portion 22 may be connected by gluing or other methods.

[0039] In this embodiment, a plating layer is formed on the surface of the welding portion 22, and the plating layer includes a nickel layer and a gold layer. The nickel layer covers the entire surface of the welding portion 22; and the gold layer is formed on the nickel layer located in the accommodating space 11.

[0040] Specifically, the heat dissipation cover 2 is usually made of copper, which reacts with oxygen and water in the air to form copper oxide and carbonate, which cannot be well welded with other materials. Therefore, a nickel layer is plated on the outside of the copper to form a protective layer to prevent oxidation of the copper surface, thereby improving welding performance. Therefore, plating a nickel layer on the surface of the welding portion 22 can be used to protect the welding portion 22, isolate water and oxygen in the air, and prevent oxidation of the welding portion 22.

[0041] Considering that the material of the welding layer 4 is generally indium, the thermal conductivity of indium is as high as 87W / (m·K), and the ductility of metal indium itself is good, the reliability of the package 100 after welding is good. However, the weldability of indium and nickel is poor, so indium is used as the welding layer material for welding with the heat dissipation cover 2, and a layer of gold is plated on the welding portion 22 of the nickel-plated layer to better meet the welding requirements of the heat dissipation cover 2.

[0042] Of course, in other implementations, the plating layer may include a nickel layer, may only include a gold layer, or may include neither a nickel layer nor a gold layer, which is not limited here.

[0043] In this embodiment, the roughness of the surface of the welding portion 22 facing the substrate 1 is greater than the roughness of the surface of the protrusion 21. Specifically, a surface with a large roughness can enhance the wetting performance of an object, because a surface with a large roughness can provide more contact points and microscopic gaps, so that the wetting liquid can better enter and contact and expand with the surface. Therefore, during the welding process, the welding layer 4 will tend to better wet and contact the welding portion 22 relative to the protrusion 21, thereby improving the welding effect.

[0044] In one application scenario, the roughness of the surface of the welding portion 22 facing the chip 3 is set in the range of 2.0 microns to 3.5 microns. For example, the roughness of the welding portion 22 can be selected to be 2.0 microns, 2.5 microns, 3.0 microns or 3.5 microns. The specific selection can be made according to actual needs and is not limited here.

[0045] Continue reading Figure 1, the height of the protrusion 21 ranges from 200 microns to 300 microns. For example, the height of the protrusion 21 can be 200 microns, 220 microns, 240 microns, 260 microns, 280 microns or 300 microns. The height of the protrusion 21 can be adjusted according to the size of the chip 3 and the size of the heat dissipation cover 2, and the present application does not limit the height of the protrusion 21.

[0046] Continue reading Figure 1 , the surface of the protrusion 21 facing the substrate 1 is flush with the surface of the welding layer 4 facing the substrate 1 .

[0047] Specifically, the height of the protrusion 21 is substantially consistent with the height of the welding layer 4, which can limit the overflow of the welding material to the greatest extent. For example, the height of the protrusion 21 and the welding layer 4 can be 200 microns, 225 microns, 250 microns, 275 microns or 300 microns. In one application scenario, the material of the welding layer 4 is an indium sheet, the height of the indium sheet is consistent with the height of the protrusion 21, and the heat dissipation cover 2 and the chip 3 are welded in a molten state.

[0048] Of course, in other embodiments, the height of the protrusion 21 may also be greater than or less than the height of the welding layer 4 , and the specific selection can be made according to actual needs, and is not limited here.

[0049] See also Figure 3 The electronic device 200 includes a circuit board 210 and a package 100 as any of the above embodiments welded on the circuit board. The electronic device 200 may be a mobile phone, a tablet computer, an e-book, a computer, etc., which are not limited here. By arranging the package 100 in the electronic device 200, a better heat dissipation effect can be achieved for the electronic device 200, and it is conducive to the miniaturization design of the electronic device 200.

[0050] The above description is only an implementation method of the present application, and does not limit the patent scope of the present application. Any equivalent structure or equivalent process transformation made using the contents of the present application specification and drawings, or directly or indirectly used in other related technical fields, are also included in the patent protection scope of the present application.

Claims

1. A package, characterized in that: The package comprises: substrate; A heat dissipation cover, disposed on the substrate and forming an accommodation space between the heat dissipation cover and the substrate; A chip is arranged on the substrate and located in the accommodating space, wherein a functional surface of the chip faces the substrate and a non-functional surface faces the heat dissipation cover; A welding layer, located between the heat dissipation cover and the chip, connecting the heat dissipation cover and the chip; Wherein, a protrusion is arranged on the surface of the heat dissipation cover facing the substrate, the protrusion is located in the accommodating space, and the orthographic projection of the protrusion on the substrate is located at the periphery of the orthographic projection of the chip on the substrate; Among them, the heat dissipation cover includes a welding part and a peripheral part, the welding part is connected to the chip through the welding layer; the peripheral part is arranged on the periphery of the welding part and is connected to the welding part, the surface of the welding part facing the substrate is a concave surface, and the density of the peripheral part is less than the density of the welding part.

2. The package according to claim 1, characterized in that: The protrusion is in a ring structure, and the orthographic projection of the protrusion on the substrate surrounds the orthographic projection of the chip on the substrate.

3. The package according to claim 1, characterized in that: A surface of the protrusion facing the substrate is flush with a surface of the welding layer facing the substrate.

4. The package according to claim 1, characterized in that: The package body further includes a first bump and a second bump, wherein the first bump is arranged between the substrate and the chip, and the second bump is arranged on a side of the substrate away from the heat dissipation cover.

5. The package according to claim 4, characterized in that: The roughness of the surface of the welding portion facing the substrate is greater than the roughness of the protruding surface.

6. The package according to claim 1, characterized in that: The roughness of the surface of the welding portion facing the chip ranges from 2.0 microns to 3.5 microns.

7. The package according to claim 1, characterized in that: The protrusion is integrally formed with the peripheral portion; and / or, a groove is formed on the surface of the peripheral portion and the welding portion, and a portion of the welding portion extends into the groove.

8. The package according to claim 6, characterized in that: A plating layer is formed on the surface of the welding portion, and the plating layer includes: A nickel layer covering the entire surface of the welding portion; A gold layer is formed on the nickel layer in the accommodating space.

9. The package according to claim 1, characterized in that: The height of the protrusions ranges from 200 microns to 300 microns.

10. An electronic device, characterized in that: The invention comprises a circuit board and a package body as claimed in any one of claims 1 to 9 which is welded on the circuit board.