High-strength microcrystalline glass table board

By using glass ceramic material and explosion-proof membrane, elastic membrane, curved edge strips and other designs on the ceramic glass countertop, the insufficient strength of the countertop and the problem of water dripping are solved, achieving higher safety and hygiene.

CN221830260UActive Publication Date: 2024-10-15NANAN SHISHAN HUANGTING GLASS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323425971.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-15
Publication Date
2024-10-15
Estimated Expiration
2033-12-15

AI Technical Summary

Technical Problem

The existing microcrystalline glass countertops are not very strong when used in the kitchen and are prone to expansion and bursting due to external impact or high temperature. Moreover, water stains after cleaning are difficult to deal with, resulting in dirt and affecting kitchen hygiene.

Method used

A high-strength glass-ceramic countertop is designed, using glass-ceramic panels, pipes and edges, adding explosion-proof membranes, elastic membranes and curved edges, and realizing explosion-proof and waterproof functions through pipe slots and isolation pads. , to prevent water dripping.

Benefits of technology

It enhances the mechanical strength and thermal expansion performance of the ceramic glass countertop, reduces the risk of bursting, prevents water from dripping to the ground, and improves the hygiene and cleanliness of the kitchen.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221830260U_ABST
    Figure CN221830260U_ABST
Patent Text Reader

Abstract

The utility model discloses a high-strength glass ceramic table board in the technical field of glass products, which comprises a using plate, a pipeline and an edge strip, the pipeline is integrally formed in the middle of the top of an inner cavity of the using plate and extends downwards, the edge strip is sleeved between the outer side walls of the using plate, an explosion-proof membrane is adhered to the top of the using plate, and the explosion-proof membrane is adhered to the inner cavity of the using plate. The high-strength glass-ceramic table top is reasonable in structural design, when the glass-ceramic table top is used in a kitchen, the strength of the glass-ceramic table top can be enhanced, buffering can be achieved when the glass-ceramic table top is impacted by the outside, the service life of the glass-ceramic table top is prolonged, the service life of the glass-ceramic table top is prolonged, and the service life of the glass-ceramic table top is prolonged. The influence of temperature is less, so that the glass table top is not easy to burst, and the use risk is reduced; when the glass ceramic table top is used in a kitchen, water remaining after articles are cleaned cannot drop to the ground, trampling smudginess cannot be caused, and sanitation and cleaning of the kitchen are facilitated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of glass products, in particular to a high-strength microcrystalline glass table top. Background Art

[0002] Glass is an amorphous inorganic non-metallic material, and microcrystalline glass is a polycrystalline solid phase material containing a glass body that is obtained by controlled nucleation and crystallization of certain basic glasses of specific composition at a certain temperature. The panels made of microcrystalline glass have the advantages of fine texture and excellent performance.

[0003] However, the existing micro-ceramic glass countertops are not strong enough when used in the kitchen. They are easily expanded and cracked by external impact or high temperature, which poses a safety hazard. In addition, when the micro-ceramic glass countertops are used in the kitchen, after washing items, in order to deal with water stains in time, water will drip along the edges to the ground, and then be stepped on by people to cause dirt, making the kitchen unhygienic and unclean. For this reason, we have proposed a high-strength micro-ceramic glass countertop. Utility Model Content

[0004] The purpose of the utility model is to provide a high-strength microcrystalline glass countertop to solve the problem raised in the above-mentioned background technology that the existing microcrystalline glass countertops are not strong enough when used in the kitchen and are easily expanded and cracked by external impact or high temperature; and when the microcrystalline glass countertops are used in the kitchen, after washing items, in order to deal with water stains in time, water drips along the edges to the ground and is then stepped on by people, causing dirt.

[0005] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a high-strength microcrystalline glass table top, comprising a working plate, a pipe and an edge strip, the pipe being integrally formed in the middle of the top of the inner cavity of the working plate and extending downward, the edge strip being sleeved between the outer side walls of the working plate, an explosion-proof film being bonded to the top of the working plate, a decorative film being bonded to the bottom of the working plate, an elastic film being bonded to the bottom of the decorative film, a slot being opened in the middle of the top of the pipe, and a bottom layer being fixedly connected between the lower sides of the inner side walls of the edge strip.

[0006] As a further description of the above technical solution:

[0007] The elastic film is a rubber layer.

[0008] As a further description of the above technical solution:

[0009] The pipeline passes through the decorative film, the elastic film and the middle of the top of the bottom layer in sequence.

[0010] As a further description of the above technical solution:

[0011] An insulating pad is inlaid between the upper sides of the inner side walls of the pipeline.

[0012] As a further description of the above technical solution:

[0013] A groove is provided in the middle of the upper side of the inner side wall of the edge strip, and the outer sides of the decorative film and the elastic film are located in the middle of the inner cavity of the groove.

[0014] As a further description of the above technical solution:

[0015] The use plate, the pipe and the side strip are made of glass ceramic material, and the side strip is in an arc shape.

[0016] Compared with the prior art, the beneficial effects of the utility model are:

[0017] 1. The high-strength microcrystalline glass countertop has an explosion-proof film, an elastic film and side strips added to the use board. The glass ceramic material used in the use board has high mechanical strength, thermal expansion and explosion-proof performance. The explosion-proof effect of the use board is enhanced with the explosion-proof effect of the explosion-proof film. At the same time, the side strips protect the weak parts around the use board, so that the corners of the use board are not easy to burst. At the same time, the addition of the explosion-proof film can effectively prevent the exploded glass fragments from scattering everywhere. The compressibility of the elastic film can make the glass tread expand within a certain range after being affected by temperature. When the microcrystalline glass countertop is used in the kitchen, it can enhance its own strength, be buffered when impacted by the outside world, and be less affected by temperature, so that the glass countertop is not easy to burst, reducing its use risk.

[0018] 2. The high-strength microcrystalline glass countertop can place the sink through the groove on the pipe by adding pipes, grooves, isolation pads and side strips on the use board. With the isolation effect of the isolation pad, the sink fits tightly on the use board. At the same time, the side strips prevent water from dripping. With the arc setting of the side strips, there are no four corners on the use board. The water can be directly discharged into the pipe along the surface of the use board. When the microcrystalline glass countertop is used in the kitchen, the remaining water after washing items cannot drip to the ground, which will not cause trampling and dirt, and is conducive to kitchen hygiene and cleaning. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 This is a schematic diagram of the three-dimensional structure of a high-strength micro-ceramic glass tabletop proposed by the utility model;

[0020] Figure 2 This is a schematic diagram of the main cross-sectional structure of a high-strength micro-ceramic glass tabletop proposed by the utility model;

[0021] Figure 3This is a schematic diagram of the top view of a high-strength micro-ceramic glass tabletop proposed by the utility model;

[0022] Figure 4 A high-strength microcrystalline glass tabletop proposed by the utility model Figure 2 Enlarged structural diagram at A in the middle.

[0023] In the figure: 100, use plate; 110, explosion-proof film; 120, decorative film; 130, elastic film; 200, pipeline; 210, slot; 220, insulation pad; 300, edge strip; 310, groove; 320, bottom layer. DETAILED DESCRIPTION

[0024] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0025] In the description of the present utility model, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present utility model and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present utility model. In addition, features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present utility model, unless otherwise specified, "multiple" means two or more.

[0026] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installation", "connection" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0027] The utility model provides a high-strength microcrystalline glass countertop, which can enhance its own strength when used in the kitchen, can buffer when impacted by the outside world, is less affected by temperature, and is not easy to burst, thereby reducing the danger of use; when the microcrystalline glass countertop is used in the kitchen, the remaining water after washing items cannot drip onto the ground, and will not cause trampling and dirt, which is conducive to kitchen hygiene and cleaning. Please refer to Figure 1-4 , including using a plate 100, a pipe 200 and a side strip 300;

[0028] Please refer again Figure 1-4 The top of the use plate 100 is bonded with an explosion-proof film 110, and the explosion-proof film 110 is used to enhance the explosion-proof effect of the use plate 100. The bottom of the use plate 100 is bonded with a decorative film 120, and the decorative film 120 is used to decorate the explosion-proof glass. The bottom of the decorative film 120 is bonded with an elastic film 130, and the elastic film 130 is used to facilitate the expansion of the use plate 100 after being heated. The use plate 100 is used to install the connecting pipe 200 and the edge strip 300;

[0029] Please refer again Figure 1-4 A slot 210 is provided in the middle of the top of the pipe 200, and the slot 210 is used to buckle the water tank. The pipe 200 is integrally formed in the middle of the top of the inner cavity of the use plate 100 and extends downward. The pipe 200 is used to install the water tank;

[0030] Please refer again Figure 1-3 A bottom layer 320 is fixedly connected between the lower sides of the inner side walls of the edge strip 300 , and the bottom layer 320 is used to reinforce the use plate 100 . The edge strip 300 is sleeved between the outer side walls of the use plate 100 , and the edge strip 300 is used to protect the periphery of the use plate 100 .

[0031] Please refer again Figure 1-4 The elastic film 130 is a rubber layer, and the rubber layer enables the plate 100 to expand.

[0032] Please refer again Figure 1-4 The pipe 200 sequentially penetrates the top middle of the decorative film 120 , the elastic film 130 and the bottom layer 320 , and is installed by penetrating the decorative film 120 , the elastic film 130 and the bottom layer 320 .

[0033] Please refer again Figure 1-4 An isolation pad 220 is embedded between the upper sides of the inner wall of the pipeline 200, and the water tank pool in the pipeline 200 is isolated and installed through the isolation pad 220.

[0034] Please refer again Figure 1-3A groove 310 is opened in the middle of the upper side of the inner wall of the edge strip 300, and the outer sides of the decorative film 120 and the elastic film 130 are located in the middle of the inner cavity of the groove 310, and the decorative film 120 and the elastic film 130 are installed and limited by the groove 310.

[0035] Please refer again Figure 1-4 The plate 100, the pipe 200 and the edge strip 300 are made of glass ceramic material. The edge strip 300 is arc-shaped. The glass ceramic material makes the plate 100, the pipe 200 and the edge strip 300 have explosion-proof effect. There is no dead angle between the arc-shaped edge strip 300 and the plate 100.

[0036] During specific use, a person skilled in the art inserts the sink into the pipe 200 on the use board 100, opens it in the slot 210, and installs it in isolation through the isolation pad 220. The explosion-proof membrane 110 and the material of the use board 100 itself make the table top have the explosion-proof effect. After being heated, the use board 100 expands, so that the use board 100 moves in the groove 310 through the elastic force of the elastic membrane 130 on the bottom layer 320. The protection of the edge strip 300 is used to protect the table top from water dripping and explosion. The use board 100 is decorated with the decorative film 120, and then it can be used.

[0037] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0038] Although the present invention has been described above with reference to the embodiments, various modifications may be made thereto and parts thereof may be replaced with equivalents without departing from the scope of the present invention. In particular, as long as there is no structural conflict, the various features in the embodiments disclosed in the present invention may be used in combination with each other in any manner, and the fact that these combinations are not exhaustively described in this specification is only for the sake of omitting space and saving resources. Therefore, the present invention is not limited to the specific embodiments disclosed herein, but includes all technical solutions falling within the scope of the claims.

Claims

1. A high-strength glass-ceramic table top, characterized by: The utility model comprises a use plate (100), a pipe (200) and a side strip (300), wherein the pipe (200) is integrally formed in the middle of the top of the inner cavity of the use plate (100) and extends downward, the side strip (300) is sleeved between the outer side walls of the use plate (100), an explosion-proof film (110) is bonded to the top of the use plate (100), a decorative film (120) is bonded to the bottom of the use plate (100), an elastic film (130) is bonded to the bottom of the decorative film (120), a slot (210) is opened in the middle of the top of the pipe (200), and a bottom layer (320) is fixedly connected between the lower sides of the inner side walls of the side strip (300).

2. A high-strength microcrystalline glass tabletop according to claim 1, characterized in that: The elastic film (130) is a rubber layer.

3. The high-strength microcrystalline glass tabletop according to claim 1, characterized in that: The pipe (200) sequentially passes through the decorative film (120), the elastic film (130) and the middle of the top of the bottom layer (320).

4. The high-strength microcrystalline glass tabletop according to claim 1, characterized in that: An insulating pad (220) is embedded between the upper sides of the inner side walls of the pipe (200).

5. The high-strength microcrystalline glass tabletop according to claim 1, characterized in that: A groove (310) is provided in the middle of the upper side of the inner wall of the edge strip (300), and the outer sides of the decorative film (120) and the elastic film (130) are located in the middle of the inner cavity of the groove (310).

6. The high-strength microcrystalline glass tabletop according to claim 1, characterized in that: The use plate (100), the pipe (200) and the side strip (300) are made of glass ceramic material, and the side strip (300) is in an arc shape.