Lining pot for metal plating crucible
By designing a lining pot for metal plating crucibles and using the combined structure of a thick-walled lining pot and a thermal conductive ring, the problem of low coating rate in the traditional evaporation process is solved, cost reduction and production efficiency are improved, and product quality is improved. .
Patent Information
- Application Number
- CN202420433885.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-06
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2034-03-06
AI Technical Summary
The metal coating rate in the traditional evaporation process is low, resulting in high production costs, heavy equipment load, high energy consumption and poor product quality.
Design a lining pot for metal-plated crucibles, including a thick-walled lining pot and a heat-conducting ring. The outer wall of the lining pot is provided with an inward arc. The bottom of the lining pot has a heat-conducting ring and a spherical inner hole. The lining pot and the heat-conducting ring are made of heat-conducting materials. into an arc-shaped gap to improve thermal conductivity.
It significantly reduces the amount of metal pre-melting, reduces production costs, increases the coating rate, shortens production time, reduces the splash of large particles, and improves product quality.
Smart Images

Figure CN221877155U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of evaporation equipment, and in particular relates to a lining pot for a metal plating crucible. Background Art
[0002] The four basic processes of chip manufacturing include: chip design, FPGA verification, wafer lithography development, etching, chip packaging, etc. The chip production process is the most complicated and requires wet cleaning, lithography, ion implantation, dry etching, plasma washing, heat treatment, chemical vapor deposition, physical vapor deposition, electroplating, chemical / mechanical surface treatment, wafer testing and other processes. The electron beam evaporation method of metal is usually used in the physical vapor deposition process.
[0003] In the traditional evaporation process, the first method is to pre-melt the metal directly in the crucible, and the second method is to pre-melt the metal in a conventional liner crucible. Both of these methods have two major defects: one is that the evaporation pre-melted metal material uses a lot of materials, and the amount used each time is relatively small. Most of the metals used in semiconductors are precious metals, which invisibly increases the production input cost. Another aspect is that whether it is directly in the crucible or in the ordinary liner crucible, it requires a large evaporation power and a low evaporation rate. The low rate leads to a long evaporation time. Excessive power will cause equipment load and high energy consumption. In addition, excessive power will cause large particles of material to splash, resulting in an increase in spots on the product surface and reduced product quality. Utility Model Content
[0004] The utility model aims to provide a lining pot for a metal plating crucible, which solves the problem of low coating rate of existing metal evaporation.
[0005] The technical scheme adopted by the utility model is a lining pot for a metal-plated crucible, comprising a crucible body and a lining pot arranged inside the crucible body, the lining pot wall thickness is 10mm-16mm, an inner arc is arranged on the outer side wall of the lining pot, so that an arc-shaped gap is formed between the lining pot and the crucible body, a heat conduction ring is also arranged at the bottom of the lining pot, and a spherical lining pot inner hole is milled downwardly at the top of the lining pot.
[0006] The utility model is also characterized in that:
[0007] The inner arc is arranged along the circumference of the outer side wall of the liner pot, the diameter of the inner arc is 15mm-20mm, and the curvature ratio of the inner arc is 1.1-1.5.
[0008] The diameter of the inner hole of the liner pot is 10mm to 15mm.
[0009] The overall height of the heat-conducting ring is 0.8 mm to 1.2 mm, and the inner ring diameter of the heat-conducting ring is 22 mm to 30 mm.
[0010] The lining pot and the heat conducting ring are both made of heat conducting materials.
[0011] The beneficial effects of the utility model are:
[0012] The utility model reduces the weight of the metal pre-melting crucible liner used in the metal plating crucible, and greatly reduces the investment of the initial production cost for precious metals. The designed liner only needs about 30g of Au to meet the original production needs. The evaporation rate of the same evaporation power can be increased by 200% to 300% by using the utility model liner crucible, thereby increasing the metal coating rate and shortening the coating time. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 The utility model is a schematic structural diagram of a lining pot for a metal plating crucible.
[0014] In the figure, 1. crucible body, 2. lining pot, 3. heat transfer ring, 4. inner arc, 5. inner hole of lining pot. DETAILED DESCRIPTION
[0015] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0016] Example 1
[0017] like Figure 1 As shown, the lining pot for metal plating crucible of the utility model comprises a crucible body 1 and a lining pot 2 arranged inside the crucible body 1, the wall thickness of the lining pot 2 is 10mm-16mm, and the outer wall of the lining pot 2 is provided with an inward arc 4, so that an arc-shaped gap is formed between the lining pot 2 and the crucible body 1, and a heat conduction ring 3 is also provided at the bottom of the lining pot 2, and a spherical lining pot inner hole 5 is milled downward from the top of the lining pot 2.
[0018] The inner arc 4 is arranged along the circumferential direction of the outer side wall of the liner pot 2, the diameter of the inner arc 4 is 15 mm to 20 mm, and the curvature ratio of the inner arc 4 is 1.1 to 1.5.
[0019] Example 2
[0020] The utility model is used for a metal plating crucible lining pot, comprising a crucible body 1 and a lining pot 2 arranged inside the crucible body 1, wherein the lining pot 2 has a wall thickness of 10 mm to 16 mm, and an inner arc 4 is arranged on the outer side wall of the lining pot 2. The inner arc 4 is arranged along the circumference of the outer side wall of the lining pot 2.
[0021] Specifically, the diameter of the inner arc 4 is 15 mm to 20 mm, and the arc ratio of the inner arc 4 is 1.1 to 1.5, so that an arc-shaped gap is formed between the liner 2 and the crucible body 1 .
[0022] A heat-conducting ring 3 with a height of 0.8 mm to 1.2 mm and an inner ring diameter of 22 mm to 30 mm is also provided at the bottom of the liner pot 2.
[0023] A spherical inner hole 5 is milled downwardly from the top of the liner pot 2, and the diameter of the inner hole 5 is 10 mm to 15 mm.
[0024] The purpose of the inner hole 5 of the liner crucible having a diameter of 10mm-15mm is to allow the metal pre-melting to only require a little more metal than the required amount, thereby reducing the amount of metal pre-melting and ensuring that the metal material condition is basically consistent during each production, thereby reducing the difference in product consistency caused by differences in material height.
[0025] Example 3
[0026] On the basis of Example 2, the liner pot 2 and the heat-conducting ring 3 of the utility model are both made of heat-conducting materials.
[0027] The thermal conductive material is any one of molybdenum, tungsten copper and graphite.
[0028] The utility model has an arc gap of 15mm-20mm in diameter between the outer wall of the lining pot 2 and the inner wall of the crucible body 1, a heat conductive ring 3 with a height of 0.8mm-1.2mm, an inner ring with a diameter of 22mm-30mm, and a lining crucible wall thickness of 10mm-16mm, so as to make the heat conduction effect between the lining pot 2 and the crucible body 1 worse. Due to the obvious heat accumulation effect, the power of the electron gun will be reduced during film coating, the corresponding radiant heat will also be reduced, the substrate temperature will also be reduced, and the coating rate can also be increased, which can reduce the production time of the product.
[0029] In actual production, when evaporating AU, only 10%-20% of the previous power is needed to reach 300% of the previous rate. The power reduction reduces the splashing of large particles, reduces spots on the product surface, and improves product quality.
[0030] The utility model is used for the lining pot of the metal plating crucible. Under the premise of not affecting the coating quality, the lining pot 2 is added to the crucible body 1. In production practice, it is found that the size of the lining pot must follow a certain rule to meet the requirements of both increasing the metal coating rate and reducing the coating power. Advantages of adding the lining pot:
[0031] 1. Reduce the weight of metal pre-melt, greatly reduce the investment of early production costs, the designed liner crucible, AU only needs about 30g to meet the original production needs.
[0032] 2. Compared with the commonly used liner crucible, the evaporation rate of the liner pot of the utility model can be increased by 200% to 300% at the same evaporation power, and the production time can be shortened at the same thickness.
[0033] It will be clear to those skilled in the art that the scope of the present invention is not limited to the examples discussed above, and that several changes and modifications may be made thereto without departing from the scope of the present invention as defined by the appended claims. Although the present invention has been illustrated and described in detail in the drawings and the specification, such illustration and description are merely illustrative or schematic, and not restrictive. The present invention is not limited to the disclosed embodiments.
Claims
1. A lining pot for a metal-plated crucible, comprising a crucible body (1) and a lining pot (2) arranged inside the crucible body (1), characterized in that: The wall thickness of the lining pot (2) is 10 mm to 16 mm, and the outer wall of the lining pot (2) is provided with an inward arc (4), so that an arc-shaped gap is formed between the lining pot (2) and the crucible body (1). A heat conduction ring (3) is also provided at the bottom of the lining pot (2), and a spherical lining pot inner hole (5) is milled downward at the top of the lining pot (2).
2. The liner pot for metal plating crucible according to claim 1, characterized in that: The inner arc (4) is arranged along the circumference of the outer wall of the liner pot (2), the diameter of the inner arc (4) is 15 mm to 20 mm, and the curvature ratio of the inner arc (4) is 1.1 to 1.
5.
3. The liner pot for metal plating crucible according to claim 1, characterized in that: The diameter of the inner hole (5) of the liner pot is 10 mm to 15 mm.
4. The liner pot for metal plating crucible according to claim 1, characterized in that: The overall height of the heat-conducting ring (3) is 0.8 mm to 1.2 mm, and the inner ring diameter of the heat-conducting ring (3) is 22 mm to 30 mm.
5. The liner pot for metal plating crucible according to claim 4, characterized in that: The lining pot (2) and the heat-conducting ring (3) are both made of heat-conducting materials.