Device for preparing bilateral gradient metal based on plastic flow forming principle

Through a device based on the principle of plastic flow molding, a gradient structure metal with ultra-fine grains on both sides and coarse grains inside is prepared, which solves the problems of poor performance and low production efficiency in the existing technology, and achieves improved material performance and equipment Simplified, suitable for a variety of metal materials.

CN221909119UInactive Publication Date: 2024-10-29SOUTH CHINA UNIV OF TECH
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202420509790.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-15
Publication Date
2024-10-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing technology for preparing gradient structure materials has problems such as poor performance, low production efficiency, and complex equipment, which limits the promotion and application of materials.

Method used

A device based on the principle of plastic flow molding is used to separate the surface layer of the large workpiece through a controllable lateral extrusion cutting process to form a material with a gradient structure. The material has ultra-fine grains on both sides and coarse grains inside, realizing the material Significant improvement in performance, simplifying equipment and improving production efficiency.

Benefits of technology

It has achieved a significant improvement in material performance, with good strength and plasticity, high processing efficiency, simple equipment, and is suitable for a variety of metal materials to meet diverse needs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221909119U_ABST
    Figure CN221909119U_ABST
Patent Text Reader

Abstract

The utility model discloses a device for preparing bilateral gradient metal based on a plastic flow forming principle, which comprises a main half die, an auxiliary half die, an embedded limiting block, an extrusion block and a punch, and the auxiliary half die is detachably connected with the main half die; the embedded limiting block and the extrusion block are detachably arranged on the main half die, the extrusion block is located below the embedded limiting block, and after the embedded limiting block and the extrusion block are embedded into the main half die, an input channel used for containing a to-be-machined workpiece is formed in the position close to the embedded limiting block. A lower output channel used for conveying redundant materials is formed in the position close to the extrusion block, a transverse output channel used for outputting and flowing out gradient structure metal is formed between the embedded limiting block and the extrusion block, and the input channel communicates with the lower output channel and the transverse output channel. One end of the punch can be inserted into the input channel. The device disclosed by the utility model is wide in application, can be used for processing various metals with better plasticity to manufacture gradient structure metals, and is wide in processing range.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of manufacturing gradient structure metal materials, in particular to a device for preparing bilateral gradient metal based on the plastic flow forming principle. Background Art

[0002] Modern industry, medical equipment, aerospace and other fields are developing rapidly, and processes are needed to manufacture metal materials with better performance. In recent years, many studies have shown that by constructing a multi-level gradient structure of metal materials, the performance shortcomings of nanostructured materials can be effectively overcome, making them present a better match of high strength and high plasticity, and have excellent properties such as good fatigue resistance, wear resistance and adhesion. Gradient structure materials have attracted much attention from researchers and have broad application prospects, so how to prepare excellent gradient structure materials has become a hot topic for researchers.

[0003] Gradient structure material is a material whose component, organization or phase gradually transitions to another component, organization or phase. This material can not only effectively avoid performance mutations caused by size mutations, but also enable the structures of different characteristic sizes to coordinate with each other, greatly optimizing and improving the overall performance and service performance of the material.

[0004] However, the existing technologies for preparing gradient structure materials have some problems, such as poor performance of the prepared gradient structures, and failure to achieve both high strength and high plasticity; some require multiple processes and have low production efficiency; and some require complex equipment and have high production requirements. These problems have limited the promotion and application of gradient structure materials. Utility Model Content

[0005] The purpose of the utility model is to overcome at least one of the shortcomings and deficiencies of the above-mentioned prior art, and to provide a device for preparing bilateral gradient metal. Based on a plastic flow forming principle, the surface layer of a large workpiece is separated through a controllable lateral extrusion cutting process and converted into a material with a gradient structure. The material prepared by the device can present an obvious strain gradient in the thickness direction, and the ultrafine grains on both sides of the material gradually transition to the coarse grains inside. The performance is greatly improved, the required equipment is simple, and the production efficiency is high.

[0006] In order to achieve the above purpose, the utility model adopts the following technical solutions:

[0007] A device for preparing bilateral gradient metal based on the principle of plastic flow forming, comprising a main half-mold, a secondary half-mold, an embedded limiting block, an extrusion block and a punch;

[0008] The secondary half mold and the main half mold are detachably connected;

[0009] The embedded limiting block and the extrusion block are detachably embedded in the main half mold, and the extrusion block is located below the embedded limiting block. When the embedded limiting block and the extrusion block are embedded in the main half mold, an input channel for placing a workpiece to be processed is formed at a position close to the embedded limiting block, a lower output channel for conveying excess material is formed at a position close to the extrusion block, and a lateral output channel for outputting the outflowing gradient structure metal is formed between the embedded limiting block and the extrusion block, and the input channel is communicated with the lower output channel and the lateral output channel.

[0010] One end of the punch is used to insert into the input channel to push the workpiece to be processed toward the output channel below.

[0011] After the workpiece is placed in the device, the punch is placed in, and downward pressure is applied to the punch to press the workpiece down. The workpiece moves downward, and then a gradient structure metal is formed under the principle of plastic flow forming, so that the two sides of the metal are ultrafine-grained materials, and the middle is coarse-grained material. The grains inside the material tend to be refined from the middle to both sides, and there is no performance mutation caused by size mutation.

[0012] Preferably, it also includes a taking-out module, which is used to take out the embedded limiting block and the extrusion block.

[0013] Preferably, the removal module includes a first removal rod and a second removal rod, an upper hole is opened on the main half mold corresponding to the position where the embedded limiting block is set, and a lower hole is opened corresponding to the position where the extrusion block is set, and one end of the first removal rod and the second removal rod can be inserted into the upper hole and the lower hole respectively.

[0014] Preferably, the lower hole is provided on the main half mold and corresponds to the lower output channel and the position where the embedded extrusion block is provided, and one end of the second removal rod can be inserted into the lower hole. After the processing of the gradient structure metal is completed, the embedded limiting block, the extrusion block and the workpiece are ejected from the main half mold.

[0015] Preferably, the first removal rod is cylindrical, and the second removal rod is T-shaped.

[0016] Preferably, the main half mold is provided with a limiting block mounting slot and an extrusion block mounting slot, which are used to embed the limiting block and the extrusion block respectively.

[0017] Preferably, the main half-mold and the auxiliary half-mold are both provided with mounting holes for cooperating with fasteners to realize detachable connection between the main half-mold and the auxiliary half-mold.

[0018] Preferably, the size of the transverse output channel gradually increases from the inlet to the outlet.

[0019] Preferably, the centerline of the input channel and the centerline of the underlying output channel do not coincide.

[0020] Preferably, the embedded limiting block has a sawtooth structure for squeezing the workpiece to be processed during processing. The parameters of the sawtooth structure can be adjusted according to demand, such as the height of the sawtooth can be increased or decreased.

[0021] Preferably, the extrusion block has a cutting edge for extruding and cutting the workpiece to be processed during processing. The geometric parameters of the cutting edge can be adjusted according to demand, such as the slope can be increased or decreased.

[0022] Preferably, before the workpiece to be processed is placed in, a lubricant is applied to the input channel to play a lubricating role and reduce the friction between the workpiece to be processed and the input channel during the processing.

[0023] Preferably, the punch has a clearance fit with the input channel in terms of size, which can reduce the friction between the punch and the input channel during processing and effectively press down the workpiece to be processed.

[0024] Preferably, the workpiece to be processed has a clearance fit with the input channel in terms of size and has the same shape, so that the workpiece to be processed can be easily placed in the input channel, and the generated gradient structure metal material is uniform.

[0025] Compared with the prior art, the beneficial effects of the present invention are at least embodied in:

[0026] 1. The device of the utility model can produce metals with obvious gradient structure, which are ultrafine crystal / nanocrystalline materials on both sides of the material and coarse crystal materials inside. The transition between the materials is uniform, there is no performance mutation caused by size mutation, the overall performance is significantly improved, and it has good strength and plasticity.

[0027] 2. The device of the utility model has high processing efficiency and can produce gradient structure metal in one step with obvious forming effect. Compared with the process that requires multiple steps to process the gradient structure, it has higher processing efficiency and can solve the low efficiency problem of the existing method.

[0028] 3. The device of the utility model has a simple structure, is easy to design and manufacture, and is simple to assemble. The required external processing equipment is simple, and the requirements for the device and equipment are not high, which can solve the problem of complex equipment in the prior art.

[0029] 4. The device of the utility model can realize the manufacture of gradient structure metals with different performance parameters to meet different production needs. During preparation, the performance parameters can be changed by simply modifying the geometric parameters of the sawtooth structure and the cutting edge, such as the sawtooth height of the sawtooth structure and the slope of the cutting edge, to achieve the manufacture of different gradient structure metals to meet diverse needs.

[0030] 5. The device of the utility model has a wide range of applications and can process various metals with good plasticity to produce gradient structure metals with a wide processing range. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Figure 1 This is a schematic diagram of the overall structure of the device for preparing bilateral gradient metal provided in an embodiment of the utility model.

[0032] Figure 2 It is a schematic structural diagram of an embedded limiting block, an extrusion block, a take-out rod, and a T-shaped take-out rod assembled on a main half mold in an embodiment of the utility model.

[0033] Figure 3 This is a partial enlarged view of the processing principle of an embodiment of the utility model.

[0034] Figure 4 It is a cross-sectional view of an embodiment of the utility model during processing.

[0035] Figure 5 It is a three-view drawing of the main half-mold structure of an embodiment of the utility model.

[0036] Figure 6 It is a three-view drawing of the auxiliary half-mold structure of an embodiment of the utility model.

[0037] Figure 7 3 views of the embedded limiting block structure of the embodiment of the utility model.

[0038] Figure 8 Three views of the extrusion block structure of an embodiment of the utility model.

[0039] Fig. 9 Three views of the removal rod structure of an embodiment of the utility model.

[0040] Fig.10 These are three views of the T-shaped removal rod structure of an embodiment of the utility model.

[0041] As shown in the figure: 10-main half mold, 11-upper hole, 12-lower hole, 20-auxiliary half mold, 30-embedded limiting block, 31-serrated structure, 40-extrusion block, 41-cutting edge, 51-removal rod, 52-T-type removal rod, 61~64-bolts, 71~74-nuts, 81-punch, 91-workpiece, 101-input channel, 102-lateral output channel, 103-lower output channel. DETAILED DESCRIPTION

[0042] The present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. The embodiments cannot be described one by one here, but the implementation methods of the present invention are not limited to the following embodiments.

[0043] like Figure 1 to Figure 2 , Figures 5 to 10 As shown, the utility model provides a device for preparing bilateral gradient metal based on the principle of plastic flow forming, which includes a main half mold 10, a secondary half mold 20, an embedding limiting block 30, an extrusion block 40, a removal module and a punch 81.

[0044] The auxiliary half mold 20 is detachably fixed to the main half mold 10 by the cooperation of bolts and nuts. The main half mold 10 is also provided with mounting through holes for receiving a plurality of bolts (61, 62, 63, 64) fixed to the auxiliary half mold 20, and the auxiliary half mold 20 is also provided with mounting through holes for receiving a plurality of bolts (61, 62, 63, 64) fixed to the main half mold 10.

[0045] The main half mold 10 is also provided with a limit block installation slot and an extrusion block installation slot, which are respectively used to install the embedded limit block 30 and the extrusion block 40. After the embedded limit block 30 and the extrusion block 40 are assembled on the main half mold 10, three channels are formed on the main half mold 10, namely, an input channel 101 close to the embedded limit block 30, a lower output channel 103 close to the extrusion block 40, and a transverse output channel 102 located between the embedded limit block 30 and the extrusion block 40. The input channel 101 is connected to the lower output channel 103 and the transverse output channel 102. The input channel 101, the transverse output channel 102 and the lower output channel 103 are respectively used to put in the workpiece to be processed, flow out the gradient structure metal and flow out the excess material.

[0046] One end of the punch 81 is used to insert into the input channel 101 to push the workpiece to be processed toward the output channel 103 below. The punch 81 is used to bear pressure during processing and transmit the pressure to press down the workpiece to be processed so that the workpiece to be processed can be embedded in the limiting block 30 and the extrusion block 40 for processing.

[0047] The removal module includes a first removal rod 51 and a second removal rod 52. An upper hole 11 is opened on the main half mold 10 and corresponds to the position where the embedded limiting block 30 is set. A lower hole 12 (the lower hole 12 is a countersunk hole) is set on the main half mold 10 and corresponds to the lower output channel 103 and the position where the embedded extrusion block 40 is set. The upper hole 11 and the lower hole 12 are used to load the first removal rod 51 and the second removal rod 52 respectively. The first removal rod 51 and the second removal rod 52 can be directly assembled in the upper hole 11 and the lower hole 12 on the main half mold 10, and after the first removal rod 51 and the second removal rod 52 are assembled, a part of them will protrude outside.

[0048] The first removal rod 51 and the second removal rod 52 are used to eject the embedded limiting block 30, the extrusion block 40 and the processed workpiece 91 from the main half mold 10 after processing the gradient structure metal. The second removal rod 52 can simultaneously remove the material in the lower output channel 103 and the extrusion block 40, thereby improving the removal efficiency.

[0049] In some embodiments of the present invention, the first extraction rod 51 is cylindrical, and the second extraction rod 52 is T-shaped. The parameters of the first extraction rod 51 and the second extraction rod 52 can be adjusted according to needs, such as the shape can be changed.

[0050] The portion of the punching device below the punch 81, in some embodiments of the present invention, the cross-sectional shape of the punch 81 is the same as the shape of the input channel 101, both are rectangular, and the dimensions are: length 70mm, width 10mm, thickness 5mm.

[0051] The embedded limiting block 30 has a sawtooth structure 31 for extruding the surface of the workpiece. In some embodiments of the present invention, the sawtooth structure 31 has 4 teeth, a tooth top angle of 120°, a tooth height of 0.3 mm, a tooth shape of an isosceles triangle, and a distance between teeth of 0.3 mm. The sawtooth structure 31 can be adjusted according to demand, such as the top angle of the sawtooth can be increased or decreased, and the shape of the tooth can be changed.

[0052] The extrusion block 40 has a cutting edge 41, which can extrude and cut the workpiece 91. In some embodiments of the present invention, the slope of the cutting edge is 1:4, and the length of the bevel is 1.65 mm. The cutting edge 41 can be adjusted according to needs, such as the slope can be increased or decreased.

[0053] In some embodiments of the present invention, the dimensions of the input channel 101 are 70 mm in length, 10.1 mm in width, and 5.1 mm in thickness. The workpiece to be processed is a pure aluminum workpiece, and the length of the pure aluminum workpiece is 50 mm, the width is 10 mm, and the thickness is 5 mm.

[0054] In some embodiments of the present invention, the dimensions of the lateral output channel 102 are: 2 mm thick, 10.1 mm wide, and the dimensions of the lower output channel 103 are: 2.4 mm thick, 10.1 mm wide, and what finally flows into the lateral output channel 102 is the processed gradient structure metal.

[0055] In some embodiments of the present invention, the cross-sectional size of the transverse output channel 102 gradually increases from the inside to the outside, which can reduce the friction between the processed plate and the mold and reduce the downward force required for processing.

[0056] In some embodiments of the present invention, the cross-sectional size of the lower output channel 103 gradually increases from the inlet to the outlet to reduce the downforce required for processing.

[0057] The geometric or processing parameters of the input channel 101, the lateral output channel 102, the lower output channel 103, the workpiece 91 and the punch 81 can be adjusted according to needs. For example, the length of the workpiece 91 can be increased or decreased, and the pressing speed of the punch 81 can be increased or decreased to meet different production needs.

[0058] The center line of the input channel 101 and the center line of the output channel 103 below do not overlap, so that the material contacts the extrusion block 40 and shears. Figure 2 and Figure 3 , according to the direction shown in the figure, the center line of the input channel 101 is located to the right of the center line of the lower output channel 103. In other embodiments, the center line of the input channel 101 is located to the left of the center line of the lower output channel 103.

[0059] like Figure 3 to Figure 4 As shown, the above embodiment provides a device for preparing bilateral gradient metal based on the principle of plastic flow forming, and the steps of preparing bilateral gradient metal include:

[0060] (1) Install the embedding limiting block 30, the extrusion block 40, the first extraction rod 51 and the second extraction rod 52 on the main half mold 10, and then fix the main half mold 10 and the auxiliary half mold 20 together. The first extraction rod 51 can be assembled to the main half mold 10 at the beginning, or it can be assembled after the metal is prepared later;

[0061] (2) Lubricant, such as molybdenum disulfide, is applied to the input channel 101 to reduce the friction between the workpiece to be processed and the channel. Then, a pure aluminum workpiece is placed in the input channel 101. Then, the punch 81 is pressed into the input channel 101 at a preset speed, such as 1 mm / s, and the pure aluminum workpiece is pressed downward. Figure 3 The partial enlarged diagram of the processing principle shows that the pure aluminum workpiece is firstly subjected to the extrusion effect of the sawtooth structure 31, and then subjected to the extrusion and cutting effect of the cutting edge 41; Figure 4 It can be seen that according to the principle of plastic flow forming, part of the material will flow into the lateral output channel 102, and the rest of the material will flow into the lower output channel 103;

[0062] (3) When the punch 81 is pressed down to almost contact the serrated structure 31, the pressing is stopped and the punch 81 is removed, and then the nuts (71, 72, 73, 74) are screwed off, and the bolts (61, 62, 63, 64) are removed, and the main half mold 10 is separated from the auxiliary half mold 20, and then the protruding parts of the first removal rod 51 and the second removal rod 52 are knocked from the other side, so that the embedded limiting block 30, the extrusion block 40 and the processed pure aluminum workpiece are removed from the main half mold 10, thereby obtaining a metal with a gradient structure.

[0063] In the device provided by the aforementioned embodiment of the present invention, when the surface material flows through the sawtooth structure, it will be squeezed and rubbed by the embedded limiting block 30, and the flow direction and flow rate of the surface material will be changed, resulting in a flow rate difference inside the material, and then a large shear force will be generated between the materials. This shear force will process the coarse crystals into ultrafine crystals / nano crystals. The processed ultrafine crystals / nano crystals flow into the lateral output channel 102 and become the upper side of the metal; when the material flows to the extrusion block 40, it will be blocked by the extrusion block 40, and part of the material will accumulate here, and slowly more material will accumulate here to form Metal dead zone, the material flow rate of the metal dead zone is low, and there is a flow rate difference between the dead zone and the surrounding materials. This flow rate difference will also cause shear force between the materials, and then the coarse crystals are processed into ultrafine crystals / nano crystals. The processed ultrafine crystals / nano crystals flow into the lateral output channel 102 and become the lower side of the metal; the material located between the embedded limiting block 30 and the extrusion block 40 is far away from the two, and there is no large flow rate difference between the original coarse crystals of the material, so it is not subjected to a more intense shearing effect, so the coarse crystals are not processed, and finally flow into the lateral output channel 102 and become the inside of the metal. In this way, a gradient structure metal with ultrafine crystals / nano crystals on both sides and coarse crystals inside can be prepared.

[0064] The device provided by the aforementioned embodiment can manufacture gradient structure metals with uniform material, and the material is uniform, there is no performance mutation caused by sudden size change, the overall performance is significantly improved, and it has good strength and plasticity. Compared with the process that requires multiple steps to process the gradient structure, the utility model can manufacture gradient structure metals in one step, and the forming effect is obvious, with high processing efficiency. In addition, the device of the utility model has a simple structure, is easy to design and manufacture, and is simple to assemble, and the required external processing equipment is simple. Various metals with good plasticity can be processed to manufacture gradient structure metals, and the processing range is wide. The device of the utility model can also process workpieces of various materials, and can process various metals with good plasticity into double-sided gradient structure metal plates, which has the characteristics of a wide processing range.

[0065] As described above, the utility model can be better implemented.

[0066] The above embodiments of the utility model are merely examples for clearly explaining the utility model, and are not intended to limit the implementation methods of the utility model. For ordinary technicians in the relevant field, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the utility model should be included in the protection scope of the claims of the utility model.

Claims

1. A device for preparing bilateral gradient metal based on the principle of plastic flow forming, characterized in that: It comprises a main half mold (10), a secondary half mold (20), an embedding limiting block (30), an extrusion block (40) and a punch (81); The auxiliary half mold (20) and the main half mold (10) are detachably connected; The embedded limiting block (30) and the extrusion block (40) are detachably embedded in the main half mold (10), and the extrusion block (40) is located below the embedded limiting block (30). When the embedded limiting block (30) and the extrusion block (40) are embedded in the main half mold (10), an input channel (101) for placing a workpiece to be processed is formed at a position close to the embedded limiting block (30), a lower output channel (103) for conveying excess material is formed at a position close to the extrusion block (40), and a lateral output channel (102) for outputting the outflowing gradient structure metal is formed between the embedded limiting block (30) and the extrusion block (40), and the input channel (101) is in communication with the lower output channel (103) and the lateral output channel (102); One end of the punch (81) is used to be inserted into the input channel (101) to push the workpiece to be processed toward the output channel (103) below.

2. The device for preparing bilateral gradient metal based on the principle of plastic flow forming according to claim 1, characterized in that: It also includes a taking-out module, which is used to take out the embedded limiting block (30) and the extrusion block (40).

3. The device for preparing bilateral gradient metal based on the principle of plastic flow forming according to claim 2, characterized in that: The removal module comprises a first removal rod (51) and a second removal rod (52). An upper hole (11) is provided on the main half mold (10) at a position corresponding to the position where the embedding limiting block (30) is set, and a lower hole (12) is provided at a position corresponding to the position where the extrusion block (40) is set. One end of the first removal rod (51) and the second removal rod (52) can be inserted into the upper hole (11) and the lower hole (12) respectively.

4. The device for preparing bilateral gradient metal based on the principle of plastic flow forming according to claim 3, characterized in that: The lower hole (12) is arranged on the main half mold (10) and corresponds to the lower output channel (103) and the position where the embedded extrusion block (40) is arranged, and one end of the second removal rod (52) can be inserted into the lower hole (12).

5. The device for preparing bilateral gradient metal based on the principle of plastic flow forming according to claim 1, characterized in that: The main half mold (10) is provided with a limiting block installation slot and an extrusion block installation slot, which are used to embed the limiting block (30) and the extrusion block (40) respectively.

6. The device for preparing bilateral gradient metal based on the principle of plastic flow forming according to claim 1, characterized in that: The main half mold (10) and the auxiliary half mold (20) are both provided with mounting holes for cooperating with fasteners to realize a detachable connection between the main half mold (10) and the auxiliary half mold (20).

7. The device for preparing bilateral gradient metal based on the principle of plastic flow forming according to claim 1, characterized in that: The size of the transverse output channel (102) gradually increases from the inlet to the outlet.

8. The device for preparing bilateral gradient metal based on the principle of plastic flow forming according to claim 1, characterized in that: The centerline of the input channel (101) does not coincide with the centerline of the output channel (103) below.

9. The device for preparing bilateral gradient metal based on the principle of plastic flow forming according to claim 1, characterized in that: The embedded limiting block (30) is provided with a sawtooth structure (31) for pressing the workpiece to be processed during processing.

10. A device for preparing bilateral gradient metal based on the principle of plastic flow forming according to any one of claims 1 to 9, characterized in that: The extrusion block (40) is provided with a cutting edge (41) for extruding and cutting the workpiece to be processed during processing.

Citation Information

Cited By

  • Device and method for preparing surface corrugated array metal heat exchange fin

    CN121339948A