Wear-resistant and corrosion-resistant injection mold

By coating the inner wall of the injection mold with a high-entropy alloy, metal nickel, and chromium-nickel alloy composite coating, the problem of uneven inner walls of the injection mold caused by high glass fiber wear during the injection molding process is solved, and the wear resistance of the mold is significantly improved. Corrosion resistance and service life.

CN221913026UActive Publication Date: 2024-10-29SUZHOU CHAMPION COATING TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323207831.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-11-28
Publication Date
2024-10-29
Estimated Expiration
2033-11-28

AI Technical Summary

Technical Problem

Injection molds are easily abraded by high glass fibers during the injection molding process, resulting in uneven inner walls and insufficient wear and corrosion resistance, affecting their service life.

Method used

A high-entropy alloy coating is used, including aluminum titanium chromium nickel tantalum alloy, which is coated on the inner wall of the mold through magnetron sputtering technology, and a transition layer of metallic nickel and chromium nickel alloy is set on it to form a composite coating to enhance the bonding force. and protection.

Benefits of technology

The wear and corrosion resistance and service life of the injection mold are significantly improved. The wear rate is less than 1.2×10-6mm³/Nm. The electrochemical corrosion current density is extremely low, which can effectively meet the needs of injection molding processing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221913026U_ABST
    Figure CN221913026U_ABST
Patent Text Reader

Abstract

The wear-resistant and corrosion-resistant injection mold comprises a mold body and a functional coating, and the mold body is provided with an inner wall; the functional coating is coated on the inner wall of the mold body; wherein the functional coating comprises a high-entropy alloy coating. And the injection mold can have excellent wear resistance, corrosion resistance and oxidation resistance, and the service life of the injection mold can be effectively prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present application relates to the field of injection molds, and in particular to a wear-resistant and corrosion-resistant injection mold. [Background technology]

[0002] With the rapid development of global industrialization, plastic products play an increasingly important role in contemporary life. As the core process of plastic product production, injection molding technology also needs continuous innovation and development. In order to improve the processability of plastics, high glass fiber fillers such as SiO2 and SiC are usually added to plastic products to increase the hardness of the product. It is precisely because of the presence of these high glass fibers that the injection mold is susceptible to a high degree of wear during the injection molding process, resulting in the destruction of the flatness of the mold cavity surface. Therefore, the inner cavity surface of such injection molds needs to improve its wear resistance and corrosion resistance.

[0003] Therefore, it is necessary to improve the prior art to overcome the above defects in the prior art. [Contents of the utility model]

[0004] The purpose of the present application is to provide a wear-resistant and corrosion-resistant injection mold, aiming to solve the problem that the inner cavity surface of the injection mold is easily affected by high glass fiber during the injection molding process, resulting in uneven inner wall, thereby improving the service life of the injection mold.

[0005] The purpose of this application is to achieve the following technical solution: a wear-resistant and corrosion-resistant injection mold, comprising:

[0006] a mold body having an inner wall; and

[0007] A functional coating is coated on the inner wall of the mold body;

[0008] Wherein, the functional coating comprises a high entropy alloy coating.

[0009] Furthermore, the high entropy alloy coating includes an aluminum-titanium-chromium-nickel-tantalum alloy coating.

[0010] Furthermore, the thickness of the aluminum-titanium-chromium-nickel-tantalum alloy coating is in the range of 5 μm to 7 μm.

[0011] Furthermore, the wear-resistant and corrosion-resistant injection mold also includes an adhesion layer, which is arranged between the inner wall and the functional coating and is used to combine the inner wall of the mold body and the functional coating.

[0012] Furthermore, the adhesion layer includes a metal nickel coating.

[0013] Furthermore, the thickness of the metal nickel coating ranges from 1 μm to 2 μm.

[0014] Furthermore, the wear-resistant and corrosion-resistant injection mold also includes a transition layer, which is arranged between the metal nickel coating and the functional coating, and the transition layer is used to protect the metal nickel coating.

[0015] Furthermore, the transition layer includes a chromium-nickel alloy coating.

[0016] Furthermore, the thickness of the chromium-nickel alloy coating ranges from 1 μm to 2 μm.

[0017] Compared with the prior art, the present application has the following beneficial effects: the present application adopts a high entropy alloy coating to be coated on the inner wall of the mold body. Due to its good thermal stability, high hardness, and excellent wear resistance, corrosion resistance, and oxidation resistance, high entropy alloy is coated on the inner wall of the injection mold, which can effectively improve the service life of the injection mold.

Brief Description of the Drawings

[0018] Figure 1 It is a schematic diagram of a wear-resistant and corrosion-resistant injection mold provided by the present application along a certain angle.

[0019] Explanation of the accompanying figures: 1. Inner wall of the mold body; 2. Aluminum-titanium-chromium-nickel-tantalum alloy coating; 3. Metal nickel coating; 4. Chromium-nickel alloy coating. [Specific implementation method]

[0020] In order to make the above-mentioned purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are described in detail below in conjunction with the accompanying drawings. It is to be understood that the specific embodiments described herein are only used to explain the present application, rather than to limit the present application. It should also be noted that, for ease of description, only some structures related to the present application are shown in the accompanying drawings, rather than all structures. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of this application.

[0021] The terms "including" and "having" and any variations thereof in this application are intended to cover non-exclusive inclusions. For example, a process, method, system, product or device comprising a series of steps or units is not limited to the listed steps or units, but may optionally include steps or units not listed, or may optionally include other steps or units inherent to these processes, methods, products or devices.

[0022] Reference to "embodiments" herein means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.

[0023] See also Figure 1 As shown, the present application proposes a wear-resistant and corrosion-resistant injection mold, including a mold body and a functional coating, wherein the mold body has an inner wall; the functional coating is coated on the inner wall 1 of the mold body; wherein the functional coating includes a high entropy alloy coating.

[0024] A high entropy alloy coating is applied to the inner wall 1 of the mold body. The high entropy alloy has good thermal stability, high hardness, and excellent wear resistance, corrosion resistance, and oxidation resistance. When applied to the inner wall of the injection mold, the service life of the injection mold can be effectively improved.

[0025] It is worth noting that, at present, in order to obtain high-performance high-entropy alloy coating materials, methods that have been developed include spraying, plasma cladding and magnetron sputtering technology. Among them, magnetron sputtering technology has attracted much attention due to its low substrate temperature rise, high deposition rate, uniform and compact film structure, and flexible control of film performance and thickness. It is often used to deposit multilayer coatings composed of different types of coating materials. In this embodiment, magnetron sputtering technology is used to deposit a functional coating on the inner wall 1 of the mold body.

[0026] Specifically, the high entropy alloy coating includes an aluminum-titanium-chromium-nickel-tantalum alloy coating 2. Among a series of high entropy alloys, the aluminum-titanium-chromium-nickel-tantalum (AlTiCrNiTa) series high entropy alloy is a single BCC phase fine nanocrystalline structure. A large number of studies have confirmed that materials with simple phase structures often have stronger wear resistance and corrosion resistance due to their low thermodynamic surface potential difference. Coating them on the inner cavity surface of the injection mold can effectively improve the service life of the injection mold. In this embodiment, the aluminum-titanium-chromium-nickel-tantalum (AlTiCrNiTa) high entropy alloy is prepared by target magnetron sputtering technology, wherein the atomic content ratio of the five metal elements is Al:Ti:Cr:Ni:Ta=1:1:1:1:1.

[0027] Specifically, the thickness of the aluminum-titanium-chromium-nickel-tantalum alloy coating 2 is in the range of 5 μm to 7 μm.

[0028] The wear-resistant and corrosion-resistant injection mold further comprises an adhesive layer, which is arranged between the inner wall and the functional coating and is used to combine the inner wall 1 of the mold body and the functional coating. In this embodiment, the main function of the adhesive layer is to make the combination between the functional coating and the inner wall 1 of the mold body tighter, form a denser structure, and enhance the wear resistance and corrosion resistance.

[0029] The adhesion layer includes a metal nickel coating 3. The metal nickel (Ni) layer 3 is constructed on the surface of the inner cavity of the injection mold by magnetron sputtering technology as an adhesion layer. Specifically, the thickness of the metal nickel coating 3 ranges from 1 μm to 2 μm.

[0030] The wear-resistant and corrosion-resistant injection mold also includes a transition layer, which is arranged between the metal nickel coating 3 and the functional coating, and the transition layer is used to protect the metal nickel coating 3. In order to further improve the bonding force and enhance the wear resistance and corrosion resistance, a transition layer is added. Specifically, the transition layer includes a chromium-nickel alloy coating 4. Most of the existing alloys use titanium (Ti)-based alloys. Compared with traditional cobalt (Co)-based, nickel (Ni)-based high-temperature alloys, titanium (Ti)-based alloys have high strength, high adhesion strength, and high elastic modulus, and are ideal adhesion layer materials. However, the oxidation resistance of Ti-based alloys is poor. Applying a protective coating on the surface of Ti-based alloys is one of the common methods to improve the high-temperature oxidation resistance of titanium alloys. Since the chromium-nickel alloy (Cr-Ni alloy) coating has a similar expansion coefficient to the Ti coating, the two can be well combined. At the same time, the Cr-Ni coating also combines better with the metal nickel coating 3.

[0031] Specifically, the thickness of the chromium-nickel alloy coating 4 is in the range of 1 μm to 2 μm.

[0032] Based on the above description, the present application provides the following embodiments:

[0033] Embodiment 1:

[0034] First, a single-target magnetron sputtering technique was used to deposit a metal Ni coating on the inner surface of the injection mold: the inner surface of the injection mold was pretreated and cleaned as a substrate, and the target material was a metal Ni with a purity of 99.99%. When the vacuum chamber pressure was lower than 1.0×10 -3 After 30 Å, 99.99% argon (Ar) was introduced to make the vacuum pressure of the sputtering chamber 1.8 Pa, the working temperature was room temperature, the sputtering power was 45 W, the bias voltage was 80 V, and the deposition time was 15 min.

[0035] Then, a Cr-Ni alloy coating was deposited on the surface of the metal Ni coating prepared above using a single-target magnetron sputtering technique: the inner wall surface of the injection mold on which the metal Ni coating was deposited was used as a substrate, the target material was a Cr-Ni alloy (Cr content was 10 atom.%), the sputtering power of the Cr-Ni alloy target was 80 W, and after the chamber pressure was lower than 1.0×10-3 Pa, 99.99% argon (Ar) was introduced to make the vacuum pressure of the sputtering chamber 1.0 Pa, the operating temperature was room temperature, the bias voltage was 110 V, and the deposition time was 15 min.

[0036] Finally, a high entropy alloy AlTiCrNiTa coating was deposited on the surface of the metal nickel and chromium-nickel alloy composite coating (Ni / Cr-Ni coating) using a single-target magnetron sputtering technique: the inner cavity surface of the injection mold with the Ni / Cr-Ni coating deposited was mounted on the fixture of the magnetron sputtering equipment, the target material was Al-Ti-Cr-Ni-Ta alloy (previously, five pure metals were mixed and obtained by arc melting, with an atomic content ratio of Al:Ti:Cr:Ni:Ta=1:1:1:1:1), and the vacuum degree was set to 5×10 -4 Pa, and the substrate was heated at 150°C. Argon (Ar) with a purity of 99.99% was introduced, and when the pressure in the chamber reached 0.6 Pa, the bias power was turned on. The bias was maintained at 100V, the sputtering power was 140W, and the deposition time was 60min to obtain a functional coating AlTiCrNiTa layer.

[0037] The thickness of the metal Ni coating is 1 μm, the thickness of the Cr-Ni alloy coating is 1 μm, and the thickness of the AlTiCrNiTa coating is 5 μm.

[0038] Embodiment 2: The difference from Embodiment 1 is that the thickness of the metal Ni coating is 2 μm, the thickness of the Cr-Ni alloy coating is 2 μm, and the thickness of the AlTiCrNiTa coating is 7 μm.

[0039] Embodiment 3: The difference from Embodiment 1 is that the thickness of the metal Ni coating is 2 μm, the thickness of the Cr-Ni alloy coating is 1 μm, and the thickness of the AlTiCrNiTa coating is 6 μm.

[0040] The bonding force between the composite coating of metal Ni, Cr-Ni alloy coating and AlTiCrNiTa coating (Ni / Cr-Ni / AlTiCrNiTa coating) and the inner wall of the injection mold can reach 43-49N, and the wear rate is less than 1.2×10 -6 mm -3 / Nm, electrochemical tests show that the corrosion current density of the inner cavity surface of the injection mold with Ni / Cr-Ni / AlTiCrNiTa composite coating is extremely low. The corrosion current density after immersion in 3.5wt.% NaCl aqueous solution for 72 hours is less than 10 -7 A / cm 2 After the electrochemical corrosion test, the Ni / Cr-Ni / AlTiCrNiTa coating still maintains a complete and dense surface. This shows that the surface of the injection mold cavity with the Ni / Cr-Ni / AlTiCrNiTa composite coating has good wear and corrosion resistance, and can effectively meet the needs of the actual injection molding process.

[0041] The above is only a specific implementation of the present application, and any other improvements made based on the concept of the present application are deemed to be within the protection scope of the present application.

Claims

1. A wear-resistant and corrosion-resistant injection mold, characterized in that: include: A mold body having an inner wall; A functional coating, coated on the inner wall of the mold body, wherein the functional coating comprises a high entropy alloy coating, and the high entropy alloy coating comprises an aluminum-titanium-chromium-nickel-tantalum alloy coating; an adhesive layer, the adhesive layer being disposed between the inner wall and the functional coating and used for bonding the inner wall of the mold body and the functional coating, the adhesive layer comprising a metal nickel coating; and A transition layer is disposed between the metal nickel coating and the functional coating, and is used to protect the metal nickel coating.

2. The wear-resistant and corrosion-resistant injection mold according to claim 1, characterized in that: The thickness of the aluminum-titanium-chromium-nickel-tantalum alloy coating is in the range of 5 μm to 7 μm.

3. The wear-resistant and corrosion-resistant injection mold according to claim 1, characterized in that: The thickness of the metal nickel coating ranges from 1 μm to 2 μm.

4. The wear-resistant and corrosion-resistant injection mold according to claim 1, characterized in that: The transition layer includes a chromium-nickel alloy coating.

5. The wear-resistant and corrosion-resistant injection mold according to claim 4, characterized in that: The thickness of the chromium-nickel alloy coating ranges from 1 μm to 2 μm.