Hard AF film

By using a combination of carbon mixture and indirect layer in the hard AF film, the problem of lack of hard materials and easy falling off of the hard film in the existing technology is solved, and high hardness, wear resistance and good optical properties are achieved, which is suitable for for various glass panels.

CN221917818UActive Publication Date: 2024-10-29ANHUI JINGZHUO OPTICAL DISPLAY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420242032.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-01
Publication Date
2024-10-29
Estimated Expiration
2034-02-01

AI Technical Summary

Technical Problem

The existing hard film lacks hard materials, which causes the display screen to be easily scratched, and the AF film layer is easy to fall off during friction.

Method used

A carbon mixture is used as the hard layer, and an indirect layer of metal or non-metal coating material is set between the substrate and the AF layer. The hard layer and indirect layer are formed through magnetron sputtering or evaporation processes to ensure the thickness and thickness of the hard layer. Stability of indirection layers.

Benefits of technology

It improves the hardness and scratch resistance of the hard film, maintains the optical benchmark, enhances the wear resistance and waterproof performance of the film body, and extends the service life of the AF film layer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221917818U_ABST
    Figure CN221917818U_ABST
Patent Text Reader

Abstract

The utility model discloses a hard AF film, which belongs to the field of protective films and comprises a substrate and an AF layer opposite to the substrate, and a hard layer is stacked between the substrate and the AF layer and is made of carbon mixture. According to the invention, the carbon mixture is used as the hard layer, so that the hard layer has the characteristic of high hardness; the hardness of the whole film body is high, the Mohs hardness of the film body is larger than or equal to 6, the nanoindentation is larger than or equal to 15, and the Vickers hardness is larger than or equal to 1500. The original optical standard can be kept, the film body has a good rubber friction effect, and the hard film is suitable for front and rear glass panels of mobile phones, vehicles, televisions, wears, cameras and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to a protective film, in particular to a hard AF film. Background Art

[0002] Display screens are prone to scratches during use. For example, the glass panels on mobile phones, cars, TVs and other objects rub against sharp objects, causing scratches on the glass panels and affecting the appearance. To this end, R&D personnel coat the surface of the display screen to form an AF film layer, but with the frequent friction between the display screen (glass panels on mobile phones, cars, TVs and other objects) and objects (pockets, fingers), the AF film layer on the glass cover will eventually fall off.

[0003] In order to prevent the AF film from falling off, SiO2 or Al2O3 is often used as a primer, combined with AF waterproof pills to produce better waterproof and anti-scratch effects. However, this film layer structure lacks hard materials, and the display screen is prone to scratches. For example, the Chinese patent with application number 2023106464278 discloses a hard film and a method for making it. The technical solution disclosed therein is to use SiO2 or Al2O3 as a primer, and then set an AF layer on the top, lacking a hard material layer. In order to obtain better test results and optical effects, this application has been improved and optimized based on the prior art, thereby obtaining a better hard film.

[0004] Therefore, those skilled in the art provide a hard AF film to solve the problems raised in the above background technology. Utility Model Content

[0005] The purpose of the utility model is to provide a hard AF film, which can effectively resist scratches and avoid scratches on the display screen by using a carbon mixture as a hard layer, so as to solve the problems raised in the above background technology.

[0006] In order to achieve the above purpose, the utility model provides the following technical solutions:

[0007] A hard AF film comprises a substrate and an AF layer arranged opposite to the substrate, wherein a hard layer is stacked between the substrate and the AF layer, and the hard layer is a carbon mixed layer, which is a carbon mixture produced by synchronous sputtering or synchronous evaporation of carbon and a metal film or a non-metal film.

[0008] As a further solution of the utility model: an indirect layer is provided between the hard layer and the substrate or between the hard layer and the AF layer.

[0009] As a further solution of the utility model: the indirect layer is a metal or non-metallic coating material;

[0010] If it is a metal coating material, the indirect layer can be Al2O3;

[0011] If it is a non-metallic coating material, the indirect layer can be SiO2 / Si.

[0012] As a further solution of the present invention: the metal film in the carbon mixture can be any one of aluminum, chromium or titanium, and the non-metal film can be silicon dioxide or silicon nitride.

[0013] As a further solution of the utility model: the number of stacked layers of the carbon mixture is at least 2, and the thickness of the hard layer after stacking is ≤3000nm.

[0014] As a further solution of the present invention: the thickness of the indirect layer is ≥2nm.

[0015] As a further solution of the utility model: the hard layer and the indirect layer are both arranged on the substrate by using magnetron sputtering or evaporation process.

[0016] As a further solution of the utility model: the AF layer is deposited on the surface of the hard layer or the indirect layer by evaporating or spraying AF.

[0017] As a further solution of the utility model: the thickness of the indirect layer is less than the thickness of the hard layer.

[0018] Compared with the prior art, the beneficial effects of the utility model are:

[0019] 1. In this application, a carbon mixture is used as a hard layer, which has a high hardness characteristic; the overall film hardness is high, the Mohs hardness of the film is ≥6, the nanoindentation is ≥15, and the Vickers hardness is ≥1500;

[0020] 2. Able to maintain the original optical benchmark, haze ≤ 0.18%, B value ≤ 1.2 (CM3600), transmittance 550nm ≥ 89%;

[0021] 3. The membrane has good rubber friction effect and can withstand the following test: rubber friction ≥ 4200 times (load 1kg, ) Water drop angle ≥100°, steel wool friction ≥4200 times (load 1kg, 1*1cm) Water drop angle ≥90°, alkali sweat resistance 24H ≥100°;

[0022] 4. This hard film is suitable for front and rear glass panels of mobile phones, cars, TVs, wearables, cameras, etc. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is a schematic diagram of the structure of the hard AF film with an intermediate layer below the hard layer in the utility model.

[0024] Figure 2It is a schematic diagram of the structure of the hard AF film in which the intermediate layer is above the hard layer in the utility model.

[0025] In the figure: 1, substrate; 2, indirect layer; 3, hard layer; 4, AF layer. DETAILED DESCRIPTION

[0026] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0027] In the present application, the terms "upper", "lower", "left", "right", "front", "back", "top", "bottom", "inner", "outer", "vertical", "horizontal", "lateral", "longitudinal" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings. These terms are mainly used to better describe the present application and its embodiments, and are not used to limit the indicated devices, elements or components to have a specific orientation, or to be constructed and operated in a specific orientation.

[0028] In addition, some of the above terms may be used to express other meanings in addition to indicating orientation or positional relationship. For example, the term "on" may also be used to express a certain dependency or connection relationship in some cases. For those of ordinary skill in the art, the specific meanings of these terms in this application can be understood according to specific circumstances.

[0029] In addition, the terms "installed", "set", "provided with", "connected", and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral structure; it can be a mechanical connection, or an electrical connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be an internal connection between two devices, elements, or components. For those of ordinary skill in the art, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0030] In addition, the terms "first", "second", etc. are mainly used to distinguish different devices, elements or components (the specific types and structures may be the same or different), and are not used to indicate or imply the relative importance and quantity of the indicated devices, elements or components. Unless otherwise specified, "plurality" means two or more.

[0031] As mentioned in the background technology of this application, the inventors have discovered through research that the existing AF film coating method is to use SiO2 or Al2O3 as a base and combine it with AF waterproof pills. Although this coating method produces better waterproof and anti-scratch effects, this film layer structure lacks hard materials and the display screen is prone to scratches.

[0032] In order to solve the above defects, the present application discloses a hard AF film, which uses a carbon mixture as a hard layer with a Mohs hardness ≥ 6, can effectively resist scratches and avoid scratches on the display screen, thereby effectively solving the above defects.

[0033] The following will describe in detail how the solution of the present application solves the above technical problems in conjunction with the accompanying drawings.

[0034] See also Figure 1-2 As shown, in the embodiment of the utility model, a hard AF film includes a substrate 1 and an AF layer 4 arranged opposite thereto, a hard layer 3 is stacked between the substrate 1 and the AF layer 4, and the hard layer 3 is a carbon mixed layer, which is a carbon mixture produced by synchronous sputtering or synchronous evaporation of carbon and a metal film or a non-metal film. Using a carbon mixture as the hard layer 3 has a higher Mohs hardness and a stronger scratch resistance, and the formed film body is not easily scratched during use. The carbon mixture has the advantages of wear resistance and resistance to cold and hot shocks.

[0035] In this embodiment, an indirect layer 2 is provided between the hard layer 3 and the substrate 1 or between the hard layer 3 and the AF layer 4 .

[0036] In this embodiment: the indirect layer 2 is a metal or non-metallic coating material;

[0037] If it is a metal coating material, the indirect layer 2 can be Al2O3;

[0038] If it is a non-metallic coating material, the indirect layer 2 can be SiO2 / Si.

[0039] Using metal or non-metallic coating materials as the indirect layer 2 makes the film structure more solid, and the AF layer 4 is not easy to fall off during use. The chemical properties of SiO2 and AL2O3 are relatively stable, do not react with water, have high fire resistance, high temperature resistance, small thermal expansion coefficient, corrosion resistance and unique optical properties. Si has a high melting point (1410℃), high hardness, and relatively stable physical properties.

[0040] In this embodiment: the metal film in the carbon mixture can be any one of aluminum, chromium or titanium, and the non-metal film can be silicon dioxide or silicon nitride. The formed carbon mixture is one of aluminum carbide, chromium carbide, titanium carbide or silicon carbide, all of which have high hardness and scratch resistance.

[0041] In this embodiment: the number of stacked layers of the carbon mixture is at least 2, and the thickness of the hard layer 3 after stacking is ≤3000nm. If the thickness of the hard layer 3 is too small, the hardness and scratch resistance of the final film will be affected. If the thickness is too large, the stress on the substrate 1 will be too large, affecting the flatness of the substrate 1, resulting in the film being affected. The thickness of the hard layer 3 is preferably 50nm.

[0042] In this embodiment: the thickness of the indirect layer 2 is ≥ 2 nm. In order to keep the film body ultra-thin, the thickness of the indirect layer 2 is preferably 30 nm.

[0043] In this embodiment, the hard layer 3 and the indirect layer 2 are both disposed on the substrate 1 by using a magnetron sputtering or evaporation process.

[0044] In this embodiment, the AF layer 4 is deposited on the surface of the hard layer 3 or the indirect layer 2 by evaporating or spraying AF.

[0045] In this embodiment, the thickness of the indirect layer 2 is smaller than the thickness of the hard layer 3 .

[0046] The working principle of the utility model is: when preparing the hard AF film, if the indirect layer 2 is set between the hard layer 3 and the AF layer 4, a carbon mixture is sputtered or evaporated on a preset substrate 1 by a magnetron sputtering or evaporation process to form a hard layer 3, and then a metal or non-metallic coating material is sputtered or evaporated on the hard layer 3 by a magnetron sputtering or evaporation process to form an indirect layer 2. Finally, AF is deposited on the indirect layer 2 by evaporation or spraying to form an AF layer 4.

[0047] If the indirect layer 2 is disposed between the hard layer 3 and the substrate 1, a metal or non-metallic coating material is sputtered or evaporated on the preset substrate 1 by magnetron sputtering or evaporation process to form the indirect layer 2, and then a carbon mixture is sputtered or evaporated on the indirect layer 2 by magnetron sputtering or evaporation process to form the hard layer 3. Finally, AF is deposited on the hard layer 3 by evaporation or spraying to form an AF layer 4.

[0048] The finished hard film formed by the above two methods not only has high hardness and good wear resistance, but also can maintain the original optical reference. The final glass panel has better quality and is suitable for mobile phone cover plates, car cover plates, TV cover plates and other glass panels, with a wide range of applicability.

[0049] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.

[0050] What is described above is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes within the technical scope disclosed by the present invention according to the technical scheme and the utility model concept of the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A hard AF film, comprising a substrate (1) and an AF layer (4) arranged opposite to the substrate, characterized in that: A hard layer (3) is stacked between the substrate (1) and the AF layer (4), the hard layer (3) being a carbon mixed layer, the carbon mixed layer being a carbon mixture produced by synchronous sputtering or synchronous evaporation of carbon and a metal film or a non-metal film.

2. A hard AF film according to claim 1, characterized in that: An indirect layer (2) is provided between the hard layer (3) and the substrate (1) or between the hard layer (3) and the AF layer (4).

3. A hard AF film according to claim 2, characterized in that: The indirect layer (2) is a metal or non-metal coating material; If it is a metal coating material, the indirect layer (2) can be Al2O3; If it is a non-metallic coating material, the indirect layer (2) can be SiO2 / Si.

4. The hard AF film according to claim 1, characterized in that: The metal film in the carbon mixture may be any one of aluminum, chromium or titanium, and the non-metal film may be silicon dioxide or silicon nitride.

5. A hard AF film according to any one of claims 1 to 4, characterized in that: The number of layers of the carbon mixture stacked is at least 2, and the thickness of the hard layer (3) after stacking is ≤3000nm.

6. A hard AF film according to claim 2 or 3, characterized in that: The thickness of the indirect layer (2) is ≥2 nm.

7. The hard AF film according to claim 2, characterized in that: The hard layer (3) and the indirect layer (2) are both arranged on the substrate (1) by using a magnetron sputtering or evaporation process.

8. A hard AF film according to claim 2 or 7, characterized in that: The AF layer (4) is deposited on the surface of the hard layer (3) or the indirect layer (2) by evaporating or spraying AF.

9. The hard AF film according to claim 2, characterized in that: The thickness of the indirect layer (2) is smaller than the thickness of the hard layer (3).