Silicon-based capacitor structure
By forming conductive contact areas through chemical mechanical polishing and etching processes, the problems of excessive use of photomasks and low capacitor area utilization in traditional deep trench capacitors are solved, thereby achieving cost reduction and improved capacitor area utilization.
Patent Information
- Application Number
- CN202323286397.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-04
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2033-12-04
AI Technical Summary
Traditional deep trench capacitors require the addition of a photomask during the stacking of conductive and dielectric layers, resulting in high process costs, low capacitor area utilization, and difficulty in etching contact vias.
The conductive contact area is formed by chemical mechanical polishing and etching back, reducing the use of photomasks, eliminating conductive layer steps, and bringing the electrodes out through sidewalls and metallization processes, resulting in a uniform height between the conductive and dielectric layers.
It reduces process costs, improves capacitor area utilization, simplifies the contact via etching process, and is suitable for deep trench capacitors with thick conductive and dielectric layers.
Smart Images

Figure CN221977932U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a capacitor, in particular to a silicon-based capacitor structure. Background Art
[0002] Driven by the terminal market, the integration of integrated circuits continues to increase, and there is a demand for miniaturization of various modules and components. Capacitors are the most widely used passive devices in integrated circuits. They can be used in circuits for DC isolation, AC bypass, filtering, coupling, tuning loops, energy conversion and storage. Commonly used capacitors in integrated circuits include: MOS tube capacitors, polysilicon-insulator-polysilicon capacitors, metal-insulator-metal capacitors, etc. The miniaturization of capacitors can be achieved using integrated passive device (IPD) technology, or by increasing the capacitance value of the capacitor per unit area. Deep trench capacitors (DTC) are three-dimensional vertical capacitors formed by etching deep trenches into a silicon substrate, which can provide ultra-high capacitance value per unit area. Methods for increasing capacitance density include increasing the depth of the trench, increasing the number of stacked layers of conductive and dielectric layers, reducing the thickness of the dielectric layer, and selecting high dielectric constant dielectric materials.
[0003] It should be pointed out that the conductive layer of the traditional deep trench capacitor is formed by patterning the conductive layer steps, and then led out through the contact through-holes. When the number of stacked layers of the conductive layer and the dielectric layer increases, the method needs to increase the photomask to realize the patterning of the conductive layer steps, which increases the process cost; on the other hand, the conductive layer steps will occupy too much non-groove area, reducing the utilization rate of the capacitor area; on the other hand, the height difference of the contact through-holes placed in different conductive layers is large, which increases the difficulty of etching the contact through-holes. Summary of the invention
[0004] In order to solve the above problems, the utility model proposes a silicon-based capacitor structure, which reduces the number of masks used, reduces the process cost, and improves the utilization rate of the capacitor area.
[0005] The technical solution of this utility model:
[0006] A silicon-based capacitor structure, which is a deep trench capacitor, consists of a semiconductor substrate, a hard mask layer, a plurality of deep trenches, an insulating layer, an m-periodic stacked conductive layer and dielectric layer, a top conductive layer, a metal silicide, an interlayer dielectric layer, a contact through hole, and a metal interconnection structure; the insulating layer, the m-periodic stacked conductive layer and dielectric layer, and the top conductive layer of the silicon-based capacitor structure are located inside the deep trench of the silicon-based capacitor structure.
[0007] The insulating layer, m-periodically stacked conductive layer and dielectric layer, and top conductive layer of the silicon-based capacitor structure have concave-convex structures at their tops, and the heights of the conductive layer and top conductive layer of the silicon-based capacitor structure are lower than those of the insulating layer and dielectric layer.
[0008] The top sidewalls of the insulating layer and the dielectric layer of the silicon-based capacitor structure are provided with sidewalls, and the sidewalls are ON structures formed by low-pressure chemical vapor deposition.
[0009] The conductive layer and the top conductive layer of the silicon-based capacitor structure are flush, and the contact through-holes of the silicon-based capacitor structure are located above the deep trenches and have the same height; thus, the etching load effect of the contact through-holes is reduced, and the process is suitable for deep trench capacitors with thicker conductive layers and dielectric layers.
[0010] The hard mask layer of the silicon-based capacitor structure is silicon nitride.
[0011] The method for forming the above silicon-based capacitor structure is as follows:
[0012] 1) Providing a semiconductor substrate;
[0013] 2) forming a first hard mask layer and a second hard mask layer on a semiconductor substrate;
[0014] 3) forming a plurality of deep trenches in the semiconductor substrate, the first hard mask layer, and the second hard mask layer, and removing the second hard mask layer to expose the first hard mask layer;
[0015] 4) forming an insulating layer, an m-periodic stacked conductive layer and a dielectric layer, and a top conductive layer above the first hard mask layer and inside the deep trench;
[0016] 5) Chemical mechanical polishing to the first hard mask layer, etching back the conductive layer and the top conductive layer, exposing the dielectric layer and the insulating layer, and forming a concave-convex structure on the top of the insulating layer, the m-periodic stacked conductive layer and the dielectric layer, and the top conductive layer;
[0017] 6) forming sidewalls on the top sidewalls of the dielectric layer and the insulating layer;
[0018] 7) Implementing a metallization process on top of the conductive layer to form metal silicide;
[0019] 8) Forming an interlayer dielectric layer and performing chemical mechanical polishing;
[0020] 9) forming a contact through hole in the interlayer dielectric layer, wherein the contact through hole is connected to the metal silicide;
[0021] 10) Forming metal interconnection structure.
[0022] When the deposited state of the conductive layer and the top conductive layer is polysilicon or amorphous silicon, a rapid thermal annealing process at 1000-1150° C. is performed.
[0023] When a plurality of deep trenches are formed in the stack structure by photolithography and etching processes in step 3), a photoresist layer is also formed on the semiconductor substrate in step 2).
[0024] The advantages of the utility model are reasonable design and ingenious conception. A conductive contact area is formed by chemical mechanical grinding and etching back process, and the electrode is derived through side wall, metallization and contact through-hole process. There is no conductive layer step of traditional trench capacitor. During the formation process, the number of masks used is greatly reduced, the process cost is reduced, and the utilization rate of the capacitor area is improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] The drawings show only preferred embodiments. Various features in the drawings are not drawn to scale, and the dimensions of each feature may be changed arbitrarily, which is not considered to be a limitation of the present invention.
[0026] Figure 1 It is a schematic diagram of the stacking structure of a hard mask and a photoresist according to an embodiment of the present application.
[0027] Figure 2 Schematic diagram of the groove structure of an embodiment of the present application.
[0028] Figure 3 It is a schematic diagram of the stacking structure of an insulating layer, a conductive layer and a dielectric layer according to an embodiment of the present application.
[0029] Figure 4 It is a schematic diagram of the stacking structure of the insulating layer, the conductive layer and the dielectric layer after chemical mechanical polishing according to an embodiment of the present application.
[0030] Figure 5 It is a schematic diagram of the stacking structure of the insulating layer, the conductive layer and the dielectric layer after the etch-back process in one embodiment of the present application.
[0031] Figure 6 It is a schematic diagram of forming a dielectric layer according to an embodiment of the present application.
[0032] Figure 7 It is a schematic diagram of forming sidewall spacers and metal silicide according to an embodiment of the present application.
[0033] Figure 8 It is a schematic diagram of forming an interlayer dielectric layer and a contact through hole according to an embodiment of the present application.
[0034] Fig. 9 It is a schematic diagram of the interconnection structure of a conductive layer, a contact through hole and a back-end metal in a MIMIM capacitor with a strip-shaped groove according to an embodiment of the present application. DETAILED DESCRIPTION
[0035] In order to make the content and technical advantages of the utility model clearer and easier to understand, the content of the utility model will be described more clearly and more completely in conjunction with the drawings in the embodiments. It should be understood that the utility model is not limited to some specific embodiments, that is, some of the specific embodiments described are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, general replacements known to those skilled in the art are also included in the protection scope of the utility model.
[0036] Figures 1 to 9 The figure shows a cross-sectional view of the manufacturing process of a silicon-based capacitor according to a preferred embodiment of the utility model. To further describe the manufacturing method of the utility model, the manufacturing steps will be described in detail in conjunction with the schematic diagram as follows:
[0037] like Figure 1 As shown, a semiconductor substrate 100 is first provided, and the semiconductor substrate 100 is made of semiconductor-related materials such as silicon (Si), germanium (Ge), silicon germanium (GeSi), silicon on insulator (SOI), germanium on insulator (GOI), gallium arsenide (GaAs), indium phosphide (InP), gallium nitride (GaN), silicon carbide (SiC), zinc oxide (ZnO), etc. The structure of the semiconductor substrate 100 can be one of single crystal, polycrystalline, and amorphous, and the structure of the semiconductor substrate 100 can have or not have an epitaxial layer. The semiconductor substrate 100 can be an initial wafer, or a wafer integrated with semiconductor devices such as CMOS and Flash.
[0038] Further, a first hard mask layer 101 is deposited on the semiconductor substrate 100, a second hard mask layer 102 is deposited on the first hard mask layer 101, and a photoresist layer 103 is formed on the second hard mask layer 102. In some embodiments, the material of the first hard mask layer 101 is, for example, silicon oxide or silicon nitride, and the thickness of the first hard mask layer 101 is 100nm to 300nm. In some embodiments, the material of the second hard mask layer 102 is, for example, silicon oxide or silicon nitride, and the thickness of the second hard mask layer 102 is 300nm to 600nm. In some embodiments, the formation method of the first hard mask layer 101 and the second hard mask layer 102 is, for example, atomic layer deposition (ALD) or chemical vapor deposition (CVD).
[0039] In the structure, the first hard mask layer 101 has a higher etching selectivity to the semiconductor substrate 100 than the second hard mask layer 102. The second hard mask layer 102 is mainly used to protect the first hard mask layer 101, ensure that the trench opening in the first hard mask layer is perpendicular to the semiconductor substrate 100, and ensure that when the subsequent conductive layer and dielectric layer are filled, a thin film with an approximate right angle is formed at the top corner, which can reduce the unfilled inverted triangle groove located above the trench sealing, and reduce the load effect of the subsequent chemical mechanical polishing process. The first hard mask layer 101 also serves as a stop layer for the chemical mechanical polishing of the subsequent conductive layer and dielectric layer.
[0040] Further, a photoresist layer 103 is formed, and the thickness of the photoresist layer 103 is in the range of 2 μm to 6 μm. In some embodiments, the thickness of the second hard mask layer 102 and the photoresist layer 103 can be adjusted according to the depth requirement of the groove, that is, as the groove depth becomes shallower, the thickness of the second hard mask layer 102 and the photoresist layer 103 can become thinner, and vice versa.
[0041] A photolithography process is performed to transfer the pattern of the groove mask to the photoresist layer 103, and an etching process is performed to form a groove 104 with a high aspect ratio on the stacked structure of the semiconductor substrate 100, the first hard mask layer 101 and the second hard mask layer 102. The etching process is, for example, a wet etching process, a dry etching process, a BOSCH etching process, etc. In some embodiments, a BOSCH etching process is preferably used for deep silicon etching. The BOSCH etching process realizes etching and sidewall passivation by alternately switching etching gas and passivation gas, wherein the etching gas is SF6 and the passivation gas is C4F8. The unique etching process characteristics make the etching aspect ratio of the BOSCH etching process as high as 50:1.
[0042] Furthermore, a wet etching process is used to remove the photoresist 103 and the second hard mask layer 102 to expose the first hard mask layer 101. The aspect ratio of the groove 104 is between 10:1 and 50:1, the width of the groove 104 is between 500nm and 1.5μm, and the depth of the groove 104 is between 100nm and 50μm. The specific implementation of the width and depth of the groove 104 is set according to the requirements of the capacitor withstand voltage and capacitance density. It should be pointed out that multiple groove 104 arrays are connected in parallel to form capacitors with different capacitance values, but in order to clearly describe the capacitor structure, only one groove is selected for illustration, such as Figure 2 shown.
[0043] Further, stacked layer deposition is performed on the surface of the first hard mask layer 101 and the sidewall and bottom of the trench 104. The stacked layer is a stack structure of an insulating layer, a conductive layer and a dielectric layer stacked in an m-period, and a top conductive layer. In some embodiments, the stacked layers are, from bottom to top, an insulating layer 105, a first conductive layer 106, a first dielectric layer 107, a second conductive layer 108, a second dielectric layer 109, and a third conductive layer 110. The stacked layers are briefly described as a MIMIM structure, such as Figure 3 The combination of the conductive layer and the dielectric layer in the present invention is not limited thereto, and can be adjusted according to the specific requirements of capacitance density, such as MIM, MIMIMIM, etc. That is, when the number of dielectric layers is m, the number of conductive layers is m+1.
[0044] In some embodiments, the semiconductor substrate 100 may be doped to serve as a conductive layer. In this case, the insulating layer 105 needs to be removed, and a dielectric layer and a conductive layer are continuously stacked.
[0045] In some embodiments, the material of the insulating layer 105 may be silicon nitride or silicon oxide, the insulating layer 105 may be formed by atomic layer deposition or low pressure chemical vapor deposition (LPCVD), and the thickness of the insulating layer 105 is between 15 and 50 nm.
[0046] In some embodiments, the insulating layer 105 can inhibit the diffusion of doping elements in the polysilicon conductive layer and maintain the conductivity of the polysilicon conductive layer. In some embodiments, when the silicon-based capacitor is integrated into a substrate containing a through silicon via (TSV) structure, the insulating layer 105 can block metal ions from the substrate to ensure that the dielectric layer is not damaged.
[0047] In some embodiments, the conductive layers 106 , 108 , 110 may be made of conductive materials such as doped polysilicon, metals, and metal compounds. The conductive layers 106 , 108 , 110 may be formed by, for example, low-pressure chemical vapor deposition or physical vapor deposition (PVD).
[0048] In a specific embodiment of the present application, preferably, the conductive layers 106, 108, and 110 are n-type phosphorus-doped polysilicon formed by low-pressure chemical vapor deposition, the reaction gases are silane and phosphine, the growth temperature is 580~630°C, and the doping concentration is 1.5E20~3E20cm-3. In another embodiment, the growth temperature is 500~530°C, and the deposited film is amorphous silicon. It should be noted that, regardless of whether the deposited film is polycrystalline silicon or amorphous silicon, in order to further improve the conductivity of the conductive layer, the conductive layers 106, 108, and 110 need to perform a high-temperature annealing process to activate impurity atoms and increase the crystallization rate of the film. In some embodiments, the high-temperature annealing process is rapid thermal annealing (RTA), the annealing temperature is 1000~1150°C, and the annealing time is 10~30s.
[0049] The thickness of the conductive layers 106, 108, and 110 is adjusted based on the characteristic width of the groove and the combination of the stacked layers, for example, 100~200nm. It is worth noting that the stacked layer needs to close the opening of the groove 110 to prevent liquid from entering the groove gap in the subsequent wet process and causing damage to the conductive layer or the dielectric layer.
[0050] In some embodiments, the material of the dielectric layers 107 and 109 may be nitride, oxide, nitride-oxygen compound, etc., such as SiO2, Si3N4, HfO2, Al2O3, ZrO2 and compound thereof. The structure of the dielectric layers 107 and 109 may be a nitride or oxide single layer structure, a multilayer stacked structure of nitride and oxide, or a composite structure of nitride and oxide. The formation method of the dielectric layers 107 and 109 may be, for example, atomic layer deposition, low pressure chemical vapor deposition, and physical vapor deposition.
[0051] In a specific embodiment of the present application, preferably, the dielectric layers 107 and 109 are multilayer stacked structures of silicon oxide / silicon nitride / silicon oxide (Oxide-Nitride-Oxide, ONO) deposited by low-pressure chemical vapor deposition. The multilayer stacked structure combines the high stability of silicon oxide and the high dielectric properties of silicon nitride, and the capacitor prepared by the multilayer stacked structure has the characteristics of low leakage and high density. The thickness of the multilayer stacked structure and the ratio of the thickness of each stacked layer are adjusted according to the capacitance density and the withstand voltage requirements. The thickness of the multilayer stacked structure is 5~500nm, and the ratio of the thickness of each stacked layer can be 1:1:1, 1:2:1, 1:3:1, etc.
[0052] In some other embodiments, the dielectric layers 107 and 109 are stacked structures of silicon oxide / silicon nitride (Oxide-Nitride, ON) or silicon nitride / silicon oxide (Nitride-Oxide, NO) deposited by low pressure chemical vapor deposition.
[0053] In some other embodiments, the dielectric layers 107 and 109 are nitrogen and silicon oxide composites (SiOxNy) deposited by atomic layer deposition. The composites utilize the characteristics of atomic layer deposition to adjust the number of cycles of silicon oxide and silicon nitride in each cycle to obtain composites with different silicon, oxygen and nitrogen ratios. The composites also have the stability of silicon oxide and the high dielectric properties of silicon nitride.
[0054] Further, a chemical mechanical polishing process is performed to complete the polishing of the third conductive layer 110, the second dielectric layer 109, the second conductive layer 108, the first dielectric layer 107, the first conductive layer 106, and the insulating layer 105 on the aforementioned surface. In some embodiments, by adjusting the selectivity of the chemical mechanical polishing and detecting the signal of the relevant substance in the polishing liquid, the polishing can be stopped on the first hard mask layer 101. Subsequently, a cleaning process after chemical mechanical polishing is performed to form Figure 4 The structure shown.
[0055] Furthermore, a selective etching back process is performed to make the height of the conductive layer lower than the height of the dielectric layer, thereby forming a concave-convex structure, such as Figure 5 As shown, the height of the conductive layer is 10-20 nm lower than the dielectric layer, and the height difference can be adjusted based on the thickness of the dielectric layer to avoid the problem of the dielectric layer splitting. It should be noted that the etching process is an overall etching process without patterning. The etching process is, for example, a wet etching process with a high selectivity ratio, or a dry etching process with a high selectivity ratio.
[0056] In a specific embodiment of the present application, preferably, a high selectivity dry etching process is adopted. Specifically, a pre-etching is performed first to remove the natural oxide layer on the surface of the conductive layer; then a main etching is performed to etch the polysilicon of the conductive layer without damaging the dielectric layer. The main etching uses Cl2 and HBr gases, and the time of the main etching is determined based on the etching rate and the height difference.
[0057] Furthermore, a dielectric layer 111 is deposited, such as Figure 6As shown, the dielectric layer 111 may be silicon oxide, silicon nitride, and a combination thereof, etc. The structure of the dielectric layer 111 may be a single-layer structure or a multi-layer stacked structure. The dielectric layer 111 may be formed by atomic layer deposition, low-pressure chemical vapor deposition, physical vapor deposition, etc. The thickness of the dielectric layer 111 is between 30 and 60 nm. In a specific embodiment of the present application, preferably, the dielectric layer 111 is a stacked structure of silicon oxide / silicon nitride, and the silicon oxide / silicon nitride is formed by low-pressure chemical vapor deposition. It is worth noting that during the dry etching process, high-energy plasma will damage the dielectric layer on both sides of the top of the conductive layer, thereby weakening the withstand voltage and leakage performance of the capacitor. The deposition of silicon oxide by low-pressure chemical vapor deposition can repair the dielectric layer damage, thereby improving the stability of the capacitor.
[0058] refer to Figure 7 , an anisotropic dry etching process is performed to form a sidewall 112 on the sidewall of the conductive layer and expose the conductive layers 106, 108, and 110. In some embodiments, in order to further reduce the contact resistance, a metal silicide process is performed on the top conductive contact area of the conductive layers 106, 108, and 110. Specifically, a physical vapor deposition method is performed to form a layer of metal on the surface, and the metal can be Ti, Co, NiPt, etc. Then, a physical vapor deposition method is performed to form a cap layer TiN on the metal, and the cap layer TiN can prevent the metal from flowing during the rapid thermal annealing process. Then, a low-temperature rapid thermal annealing is performed to form a high-resistance metal silicide. Then, a selective wet etching process is performed to remove the TiN on the surface and the unreacted metal. Finally, a high-temperature rapid thermal annealing is performed to form a low-resistance metal silicide 113. The silicide is, for example, TiSi2, CoSi2, NiPtSi, etc.
[0059] like Figure 8As shown, the interlayer dielectric layer 114 (ILD) is deposited. The interlayer dielectric layer 114 may be formed by high density plasma chemical vapor deposition (HDP CVD), sub-atmospheric pressure chemical vapor deposition (SACVD), etc. The material of the interlayer dielectric layer 114 may be tetra ethyl ortho silicate (TEOS), fluorine or carbon doped silicon oxide, etc. The thickness of the interlayer dielectric layer 114 is in the range of 0.5 to 1 μm. Then, a chemical mechanical polishing process is performed to eliminate the surface undulations of the interlayer dielectric layer 114, so that the interlayer dielectric layer 114 is flattened, and the thickness of the interlayer dielectric layer 114 is reduced to the range of 0.3 to 0.8 μm.
[0060] In some embodiments, before performing the deposition of the interlayer dielectric layer 114, a chemical vapor deposition method is first used to form an etching stop layer. The material of the stop layer is, for example, silicon nitride. The thickness of the stop layer is between 100 and 200 nm. The stop layer can be used to reduce the load effect of contact hole etching.
[0061] Further, a photolithography process and an etching process are performed to transfer the contact hole pattern to the interlayer dielectric layer 114, so as to form a contact hole 115 connected to the metal silicide 113. A metal is filled in the contact hole, and the metal may be a conductive material such as copper, aluminum, tungsten, etc. The metal may be formed by electroplating, physical vapor deposition, etc. In a specific embodiment of the present application, a physical vapor deposition method is implemented to fill the barrier layer titanium nitride (not shown) and metal tungsten in the contact hole, and a chemical mechanical planarization process is performed to remove the barrier layer titanium nitride and metal tungsten on the surface. The contact hole 115 includes a contact hole 115a connected to the first conductive layer 106, a contact hole 115b connected to the second conductive layer 108, and a contact hole 115c connected to the third conductive layer 110.
[0062] It should be noted that in the embodiments of the present application, the conventional stepped conductive contact steps are abandoned, and conductive contact areas placed at the same level are used, so that the heights of the contact holes of different conductive layers can be kept consistent. Since there is no etching load effect of the contact holes, the height of the contact holes can be further reduced to reduce the equivalent series resistance generated by the contact holes.
[0063] Finally, a back-end metal interconnection structure of the capacitor is formed. The metal interconnection structure is, for example, an aluminum wire interconnection, a copper wire interconnection, etc. The metal interconnection structure is composed of at least two layers of metal to reduce the equivalent series resistance. Fig. 9 The interconnection structure of the conductive layer, contact vias and back-end metal in a MIMIM capacitor with a strip groove is shown. The contact vias 115a and 115c are derived from one port of the capacitor by the first layer of metal 116, and the contact via 115b is derived from the other port of the capacitor by the first layer of metal 117. The first layer of metal 116 and 117 are led to the aluminum pad via the second layer of metal.
[0064] In summary, the utility model adopts chemical mechanical grinding and etch-back process to form a conductive contact area, which greatly reduces the number of masks used, abandons the conductive layer steps of traditional trench capacitors, eliminates the area occupied by the steps, improves the utilization rate of the capacitor area, and makes the contact through-hole height consistent, reducing the difficulty of etching the contact through-hole. The utility model is particularly suitable for the process implementation of deep trench capacitors with thicker conductive layers and dielectric layers.
[0065] It should be noted that in the above-mentioned specific embodiments, the terms used in detailing the specific implementation scheme of the utility model, such as "above", "below", "horizontal", "vertical" and other terms describing the orientation or position relationship, only refer to the orientation or position relationship in the drawings, and do not indicate or imply that the device or component must have a specific orientation, or be constructed and operated in a specific orientation. In addition, when detailing the implementation scheme of the utility model, in order to clearly represent the structure of the utility model for the convenience of explanation, the structure in the drawings is not drawn according to the general scale, and is partially enlarged, deformed and simplified. Therefore, it should be avoided to be understood as a limitation of the utility model.
Claims
1. A silicon-based capacitor structure, wherein the silicon-based capacitor is a deep trench capacitor; characterized in that: The insulating layer, the m-periodically stacked conductive layer and dielectric layer, and the top conductive layer of the silicon-based capacitor structure are located inside the deep trench of the silicon-based capacitor structure.
2. A silicon-based capacitor structure according to claim 1, characterized in that: The insulating layer, m-periodically stacked conductive layer and dielectric layer, and top conductive layer of the silicon-based capacitor structure have concave-convex structures at their tops, and the heights of the conductive layer and top conductive layer of the silicon-based capacitor structure are lower than those of the insulating layer and dielectric layer.
3. A silicon-based capacitor structure according to claim 2, characterized in that: The top sidewalls of the insulating layer and the dielectric layer of the silicon-based capacitor structure are provided with sidewalls, and the sidewalls are ON structures formed by low-pressure chemical vapor deposition.
4. The silicon-based capacitor structure according to claim 1, characterized in that: The tops of the conductive layer and the top conductive layer of the silicon-based capacitor structure are flush with each other, and the contact through-holes of the silicon-based capacitor structure are located above the deep trenches and have the same height.
5. The silicon-based capacitor structure according to claim 1, characterized in that: The hard mask layer of the silicon-based capacitor structure is silicon nitride.