Ecological concrete mix proportion correction mold

By designing an ecological concrete mix correction mold that facilitates disassembly and assembly and collection of excess cement slurry, the problem of inaccurate mix ratio caused by excessive cement slurry is solved, and the accurate correction of mix ratio and improvement of construction quality is achieved.

CN221985369UActive Publication Date: 2024-11-12FUJIAN WATER CONSERVANCY & HYDROPOWER RES INST
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323338188.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-07
Publication Date
2024-11-12
Estimated Expiration
2033-12-07

AI Technical Summary

Technical Problem

The existing ecological concrete molds cannot effectively reflect the problem of holes formed by excessive cement slurry inside the concrete during the concrete mix design stage, resulting in inaccurate mix ratio and affecting the construction quality.

Method used

An ecological concrete mix correction mold including upper mold, lower mold, slurry grating and locking mechanism was designed. The inverted triangular structure of the slurry grating bar allows excess cement slurry to flow from the upper mold into the lower mold, and the locking mechanism is Easy to quickly disassemble and assemble, collect and convert excess cement slurry to correct the mix ratio.

Benefits of technology

Accurate correction of the ecological concrete mix ratio is achieved, the porosity and strength of concrete are improved, and the construction quality is ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221985369U_ABST
    Figure CN221985369U_ABST
Patent Text Reader

Abstract

The utility model belongs to the technical field of ecological concrete construction, and particularly relates to an ecological concrete mix proportion correction mold. An ecological concrete mix proportion correction mold comprises an upper mold, a lower mold, a slurry penetrating grating and a locking mechanism, the upper mold is a frame body, the upper end face of the frame body is a feeding port, the lower end face of the frame body is a discharging port, the lower mold is a groove body with one end closed, the lower mold is arranged below the discharging port of the upper mold, the slurry penetrating grating is arranged between the upper mold and the lower mold, and the locking mechanism is arranged on the upper mold. And the locking mechanism is used for locking and fixing the upper mold, the slurry penetrating grating and the lower mold. According to the ecological concrete mix proportion correction mold, the upper mold body, the lower mold body and the slurry penetrating grating can be rapidly disassembled and assembled through the locking mechanism, redundant cement slurry can be conveniently collected when an ecological concrete test block is manufactured, the collected redundant cement slurry is converted into the mix proportion, the mix proportion is further corrected, and the mix proportion of ecological concrete can be corrected. The ecological concrete mix proportion correction mold is compact in structure, convenient to disassemble and assemble and convenient to move when a test block is manufactured, and the test block is convenient to demold.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of ecological concrete construction, and in particular relates to an ecological concrete mix ratio correction mould. Background Art

[0002] Ecological concrete is a new type of concrete with a continuous pore structure. However, the current ecological concrete specifications have not set standards for the mix ratio of this type of concrete, and the molds currently used more often on the market are cube shapes that are consolidated into a whole by a bottom plate and four vertical plates. In the concrete mix ratio design stage, it is easy to cause slurry to settle at the bottom of the ecological concrete when the concrete test block is formed, which cannot actually reflect the problem of pore blockage caused by excessive cement slurry inside the concrete, resulting in inaccurate concrete mix ratio, which further has an adverse effect on the quality of on-site construction. In order to obtain an ecological concrete mix ratio close to the designed porosity, the collected excess cement slurry can be converted into the mix ratio, and the mix ratio can be further corrected to obtain the relationship between the strength, porosity and water-cement ratio of the ecological concrete, and determine the final practical mix ratio. In this way, the mix ratio of the ecological concrete can be effectively controlled, thereby further controlling the quality of the ecological concrete. For example, the patent application number CN202010619002.4 discloses a high-porosity eco-concrete test block mold, which includes a mold device consisting of a left template, a front template, a wire clip, an inner bottom plate, an outer bottom plate, a wire winder, a right template, a rear template, and a reinforcing wire; the inner bottom plate is a mesh hollow structure; and a water outlet is provided at the bottom of the left template. The existing mold solves the problem of large slurry area, low porosity, and low strength of the test block, but this type of mold is only used for test block molding, and it is impossible to convert and correct the mix ratio of the tested eco-concrete according to the results. Therefore, this case proposes to solve the above problems. Utility Model Content

[0003] In order to overcome the deficiencies in the prior art, the utility model provides an ecological concrete mix ratio correction mold, comprising an upper mold, a lower mold, a slurry-permeable grid, and a locking mechanism. The upper mold is a frame body, the upper end face of the frame body is a feed port, and the lower end face is a discharge port. The lower mold is a trough body closed at one end. The lower mold is arranged below the discharge port of the upper mold. The slurry-permeable grid is arranged between the upper mold and the lower mold. The locking mechanism locks and fixes the upper mold, the slurry-permeable grid, and the lower mold.

[0004] Furthermore, the upper frame includes a plurality of side panels and fastening bolts. The plurality of side panels form a rectangular frame when spliced ​​together, and the fastening bolts fix the side panels when spliced ​​together to form the rectangular frame.

[0005] Furthermore, the side panel is an "L-shaped" structure, and the outer wall of the side panel is provided with bolt holes. When the two side panels are spliced ​​into a rectangular frame body, the bolt holes on the outer walls of the side panels are opposite to each other.

[0006] Furthermore, the grout-permeable grid comprises a frame and grout-permeable grid bars arranged in the frame, and the spacing between the grout-permeable grid bars is 5-9 mm.

[0007] Furthermore, the cross section of the permeable grid bar is triangular, and the side of the permeable grid bar opposite to the upper mold is a plane, and the side opposite to the lower mold is an inclined surface.

[0008] Furthermore, the locking mechanism includes a fastening screw, a fastening screw head and a first locking groove, one end of the fastening screw is hinged to the side wall of the lower mold, the fastening screw head is arranged at the free end of the fastening screw and can be adjusted on the fastening screw, and the first locking groove is connected to the side wall of the upper mold for allowing the fastening screw to pass through.

[0009] Furthermore, the locking mechanism also includes a second locking groove, which is connected to the permeable grid. When the upper mold, the permeable grid and the lower mold are locked and fixed, the second locking groove extends from the lower mold for the fastening screw to pass through.

[0010] Furthermore, it also includes an anti-slip mechanism, which is arranged between the upper mold and the permeable grid and is used to limit the sliding of the upper mold when the upper mold, the permeable grid and the lower mold are locked and fixed.

[0011] Furthermore, the anti-slip mechanism includes a fixed plate, an anti-slip screw and an anti-slip block, the fixed plate is connected to the slurry-permeable grid, the anti-slip screw is arranged on the upper end surface of the fixed plate, and the anti-slip block is penetrated on the anti-slip rod and abuts against the upper mold.

[0012] Furthermore, a strip-shaped hole is formed on the anti-slip block, and the anti-slip block is penetrated on the anti-slip rod through the strip-shaped hole.

[0013] From the above description of the utility model, it can be seen that the ecological concrete mix ratio correction mold provided by the utility model can quickly disassemble and assemble the upper mold, the lower mold, and the grout-permeable grille through the locking mechanism, which is convenient for collecting excess cement slurry when making ecological concrete test blocks, converting the collected excess cement slurry into the mix ratio, and further correcting the mix ratio, so as to correct the mix ratio of ecological concrete. This ecological concrete mix ratio correction mold has a compact structure and is easy to disassemble and assemble. It can also be easily moved when making test blocks, which is convenient for test block demoulding. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 Schematic diagram of the mold for correcting the mix proportion of ecological concrete;

[0015] Figure 2 Schematic diagram of the upper mold for correcting the mix ratio of ecological concrete;

[0016] Figure 3 Schematic diagram of the mold grouting grid for correcting the mix ratio of ecological concrete;

[0017] Figure 4 Schematic diagram of the lower mold for correcting the mix ratio of ecological concrete. DETAILED DESCRIPTION

[0018] The present invention is further described below through specific implementation methods.

[0019] Reference Figures 1 to 4 As shown, an ecological concrete mix ratio correction mold includes an upper mold 1, a lower mold 2, a grout-permeable grid 3, a locking mechanism 4, and an anti-slip mechanism 5;

[0020] The upper mold 1 includes a plurality of side panels 11 and fastening bolts 12. The side panels are of an "L-shaped" structure. When two side panels are spliced ​​together, they form a rectangular frame body. At this time, the upper end surface of the frame body is a feed port 13, and the lower end surface is a discharge port. The outer wall of the side panel 11 is provided with a bolt hole 111. When the two side panels 11 are spliced ​​together, the bolt holes 111 are opposite to each other. The fastening bolts 12 pass through the bolt holes 111 to fix the side panels spliced ​​into the rectangular frame body.

[0021] The lower mold 2 is a trough body with one end closed, and the lower mold 2 is arranged below the discharge port 13 of the upper mold 1;

[0022] The grouting grid 3 is arranged between the upper mold 1 and the lower mold 2. The grouting grid 3 includes a frame 31 and grouting grid bars 32 arranged in the frame. The spacing between the grouting grid bars is 5-9 mm. The spacing is set to 5-9 mm to facilitate the flow of slurry. The cross section of the grouting grid bar 32 is triangular. The side of the grouting grid bar 32 opposite to the upper mold is a plane, and the side opposite to the lower mold is an inclined surface. The inverted triangle structure of the grouting grid bar 32 facilitates the excess cement slurry to flow from the upper mold to the lower mold.

[0023] The locking mechanism 4 includes a fastening screw 41, a fastening screw head 42, a first locking groove 43 and a second locking groove 44. One end of the fastening screw 41 is hinged to the side wall of the lower mold 2. The fastening screw head 42 is arranged at the free end of the fastening screw 41 and can be adjusted on the fastening screw. The first locking groove 43 is arranged on the side wall of the upper mold 1, and the second locking groove 44 is arranged on the frame 31 of the slurry-permeable grid 3. The second locking groove 44 extends out of the lower mold 2. The first locking groove 43 and the second locking groove 44 are U-shaped grooves.

[0024] The anti-slip mechanism 5 includes a fixed plate 51, an anti-slip screw 52 and an anti-slip block 53. The fixed plate 51 is connected to the frame 31 of the slurry-permeable grid 3. The anti-slip screw 52 is arranged on the upper end surface of the fixed plate. The anti-slip block 53 is provided with a strip hole 531. The anti-slip block 53 is passed through the strip hole 531 and is arranged on the anti-slip rod.

[0025] Reference Figure 1-4 As shown, the use process of the above ecological concrete mix ratio correction mold is as follows;

[0026] First, the two side panels 11 are spliced ​​together to form an upper mold 1 of a rectangular frame body, and the fastening bolts 12 pass through the bolt holes 111 to fix the side panels spliced ​​into the rectangular frame body. At this time, the upper end face of the upper mold 1 is the feed port 13, and the lower end face is the discharge port; the upper mold 1, the permeable grid 3, and the lower mold 2 are stacked in order from top to bottom. At this time, the second locking groove 44 and the fixing plate 51 on the permeable grid 3 are both extended out of the lower mold 2, and the openings of the first locking groove 43 and the second locking groove 44 are opposite to each other. The fastening screw 41 is rotated to penetrate into the first locking groove 43 and the second locking groove 44, and the fastening screw head 42 is adjusted to tighten the upper mold 1, the permeable grid 3, and the lower mold 2. The grille 3 and the lower mold 2 are locked and fixed; the anti-slip block 53 is slid on the anti-slip screw 52 until the anti-slip block 53 is tightly pressed against the upper mold, and the anti-slip block 53 is fixed to the anti-slip rod with a nut. At this time, the anti-slip block 53 can limit the sliding of the upper mold. When making ecological concrete test blocks, the well-proportioned ecological concrete is injected into the upper mold 1 from the feed port. The minimum particle size of the injected ecological concrete coarse aggregate is 10 mm. When there is too much cement slurry in the ecological concrete, the excess cement slurry will flow out from the permeable grille bar 32 into the lower mold. By collecting the cement slurry in the lower mold for conversion, the mix ratio of the ecological concrete can be corrected.

[0027] The ecological concrete mix ratio correction mold provided by the utility model can quickly disassemble and assemble the upper mold 1, the lower mold 2, and the slurry-permeable grid 3 through the locking mechanism 4, so that it is convenient to collect excess cement slurry when making ecological concrete test blocks, convert the collected excess cement slurry into the mix ratio, and further correct the mix ratio. The mix ratio of the ecological concrete can be corrected. The ecological concrete mix ratio correction mold has a compact structure and is easy to disassemble and assemble. It can also be convenient to move when making test blocks, so that the test blocks are easy to demold.

[0028] The above are only some specific implementation methods of the utility model, but the design concept of the utility model is not limited to this. Any non-substantial changes to the utility model using this concept shall be deemed as an infringement of the protection scope of the utility model.

Claims

1. An ecological concrete mix ratio correction mold, characterized by: It includes an upper mold, a lower mold, a slurry-permeable grid, and a locking mechanism. The upper mold is a frame body, the upper end face of the frame body is a feed port, and the lower end face is a discharge port. The lower mold is a trough body closed at one end. The lower mold is arranged below the discharge port of the upper mold. The slurry-permeable grid is arranged between the upper mold and the lower mold. The locking mechanism locks and fixes the upper mold, the slurry-permeable grid, and the lower mold.

2. The ecological concrete mix ratio correction mold according to claim 1 is characterized by: The upper mold includes a plurality of side panels and fastening bolts. The plurality of side panels form a rectangular frame body when spliced ​​together, and the fastening bolts fix the side panels when spliced ​​together to form the rectangular frame body.

3. The ecological concrete mix ratio correction mold according to claim 2 is characterized by: The side panels are of an "L-shaped" structure, and bolt holes are arranged on the outer walls of the side panels. When the two side panels are spliced ​​into a rectangular frame body, the bolt holes on the outer walls of the side panels are opposite to each other.

4. The ecological concrete mix ratio correction mold according to claim 1 is characterized by: The grout-permeable grid comprises a frame and grout-permeable grid bars arranged in the frame, and the spacing between the grout-permeable grid bars is 5-9 mm.

5. The ecological concrete mix ratio correction mold according to claim 4 is characterized by: The cross section of the permeable grid bar is a triangle, the side of the permeable grid bar opposite to the upper mold is a plane, and the side opposite to the lower mold is an inclined surface.

6. The ecological concrete mix ratio correction mold according to claim 1 is characterized by: The locking mechanism includes a fastening screw, a fastening screw head and a first locking groove. One end of the fastening screw is hinged to the side wall of the lower mold. The fastening screw head is arranged at the free end of the fastening screw and can be adjusted on the fastening screw. The first locking groove is connected to the side wall of the upper mold for allowing the fastening screw to pass through.

7. The ecological concrete mix ratio correction mold according to claim 6 is characterized by: The locking mechanism also includes a second locking groove, which is connected to the permeable grid. When the upper mold, the permeable grid and the lower mold are locked and fixed, the second locking groove extends from the lower mold for the fastening screw to pass through.

8. The ecological concrete mix ratio correction mold according to claim 1 is characterized by: It also includes an anti-slip mechanism, which is arranged between the upper mold and the permeable grid and is used to limit the sliding of the upper mold when the upper mold, the permeable grid and the lower mold are locked and fixed.

9. The ecological concrete mix ratio correction mold according to claim 8 is characterized by: The anti-slip mechanism includes a fixed plate, an anti-slip screw and an anti-slip block, the fixed plate is connected to the slurry-permeable grid, the anti-slip screw is arranged on the upper surface of the fixed plate, and the anti-slip block is penetrated on the anti-slip rod and abuts against the upper mold.

10. The ecological concrete mix ratio correction mold according to claim 9, characterized in that: The anti-slip block is provided with a strip hole, and the anti-slip block is penetrated on the anti-slip rod through the strip hole.