Solder strip soldering flux coating mechanism
By designing the welding tape flux coating mechanism, and automatically applying flux using the siphon function of non-woven fabrics or sponge sheets, the problem of inconvenient flux coating in welding tape processing is solved, and the welding continuity and production efficiency are improved .
Patent Information
- Application Number
- CN202323560832.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-26
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2033-12-26
AI Technical Summary
During the welding tape processing process, how to effectively and conveniently apply flux to meet production needs is a technical challenge, especially in automatic processing production lines, it is difficult for the existing technology to achieve effective flux coating, resulting in discontinuity of welding.
A welding tape flux coating mechanism is designed, which uses a rectangular main box body and a transverse circular box body to connect, and a built-in non-woven fabric or sponge sheet is used as a siphon material. The welding tape slides through the upper end of the non-woven fabric or sponge sheet to Automatically apply flux and achieve complementary two sets of structures through the communication tube and the shut-off valve to ensure that the coating is in place.
It realizes uniform coating of automated flux for welding tape, meets long-term production needs, ensures welding continuity, and improves production efficiency.
Smart Images

Figure CN222000501U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of welding strip processing, in particular to a welding strip soldering flux coating mechanism. Background Art
[0002] During the processing of the soldering ribbon, the surface needs to be coated with flux so that the surface can be effectively tinned later. However, the soldering ribbon is a continuous linear body. How to effectively and conveniently apply the flux is a technical problem that needs to be solved. Now all automatic processing production lines are used. If the flux cannot be applied effectively and conveniently, the line cannot be effectively connected and production needs cannot be met. Summary of the invention
[0003] In order to solve the above technical problems, the utility model proposes a soldering flux coating mechanism for a soldering strip, which has an ingenious design, a reasonable and compact structure and meets production needs.
[0004] The technical solution of this utility model:
[0005] A soldering ribbon flux coating mechanism comprises a rectangular main box body and a transverse circular box body. A transverse circular box body is respectively installed on one side or both sides of the rectangular main box body, the transverse circular box body is connected with the rectangular main box body, an upper opening is opened at the upper end of the transverse circular box body, a non-woven fabric or a sponge sheet with a siphon function is installed in the upper opening, the lower end of the non-woven fabric or the sponge sheet is located at the bottom of the transverse circular box body, the upper end of the non-woven fabric or the sponge sheet extends a certain length from the upper opening, and the soldering ribbon slides through the inner part of the upper end of the non-woven fabric or the sponge sheet; the rectangular main box body and the transverse circular box body are filled with soldering flux, and the soldering flux is in contact with the lower end of the non-woven fabric or the sponge sheet.
[0006] A connecting pipe is installed at the lower end of the rectangular main box body. The connecting pipe is connected to the lower end of the rectangular main box body through a vertical pipe. Stop valves are installed at both ends of the connecting pipe.
[0007] The soldering ribbon flux coating mechanism is designed with two sets, and a second set is designed on the rear side of the first set. The design height of the second set is lower than that of the first set. The connecting pipe at the lower end of the first set is connected to the rectangular main box body of the second set and is separated by a stop valve; the soldering ribbon passes through the interior of the upper end of the non-woven fabric or sponge sheet of the higher set, and then slides through the interior of the upper end of the non-woven fabric or sponge sheet on the corresponding side of the lower set.
[0008] The rectangular main box body and the transverse circular box body are made of transparent plastic.
[0009] The connecting pipe and the vertical pipe are also made of transparent plastic.
[0010] A cover plate is designed on the upper end of the rectangular main box body.
[0011] The utility model has the advantages of ingenious design and reasonable and compact structure. The welding belt automatically slides through the non-woven fabric or sponge sheet. The siphon function of the non-woven fabric or sponge sheet transfers the flux to the welding belt. The rectangular main box body and the horizontal circular box body can accommodate a certain amount of flux, which meets the long-term coating requirements of the welding belt and meets the production needs. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Figure 1 It is a main schematic diagram of the utility model.
[0013] Figure 2 It is a top view of the utility model. DETAILED DESCRIPTION
[0014] See attached Figure 1-2 , a soldering ribbon flux coating mechanism comprises a rectangular main box body 1 and a transverse circular box body 2. A transverse circular box body 2 is respectively installed on one side or both sides of the rectangular main box body 1, and the transverse circular box body 2 is connected to the rectangular main box body 1. An upper opening 6 is opened at the upper end of the transverse circular box body 2, and a non-woven fabric or sponge sheet 3 with a siphon function is installed in the upper opening 6. The lower end of the non-woven fabric or sponge sheet 3 is located at the bottom of the transverse circular box body 2, and the upper end of the non-woven fabric or sponge sheet 3 extends a certain length from the upper opening 6, and a soldering ribbon 7 slides through the upper end of the non-woven fabric or sponge sheet 3; the rectangular main box body 1 and the transverse circular box body 2 are filled with soldering flux, and the soldering flux is in contact with the lower end of the non-woven fabric or sponge sheet 3.
[0015] A connecting pipe 4 is installed at the lower end of the rectangular main box body 1. The connecting pipe 4 is connected to the lower end of the rectangular main box body 1 through a vertical pipe. Stop valves are installed at both ends of the connecting pipe 4.
[0016] The soldering ribbon flux coating mechanism is designed with two sets, and a second set is designed on the rear side of the first set. The design height of the second set is lower than that of the first set. The connecting pipe 4 at the lower end of the first set is connected to the rectangular main box body of the second set and is isolated by a stop valve; the soldering ribbon 7 passes through the upper end of the non-woven fabric or sponge sheet 3 of the higher set, and then slides through the upper end of the non-woven fabric or sponge sheet 3 on the corresponding side of the lower set.
[0017] The rectangular main box body 1 and the transverse circular box body 2 are made of transparent plastic.
[0018] The connecting pipe 4 and the vertical pipe are also made of transparent plastic.
[0019] A cover plate 5 is designed on the upper end of the rectangular main box body 1 .
[0020] When the utility model is used, the rectangular main box body is designed with horizontal circular boxes on both sides to provide two workstations. Both sides can be used, one side is used and the other side is spare. The two sets of designs prevent problems such as one set not being coated in place, ensuring that the coating is in place. The transparent material design facilitates observation of the internal situation and can replenish the flux in time.
Claims
1. A soldering flux coating mechanism, characterized in that: It comprises a rectangular main box body and a transverse circular box body. A transverse circular box body is respectively installed on one side or both sides of the rectangular main box body, the transverse circular box body is connected with the rectangular main box body, an upper opening is opened at the upper end of the transverse circular box body, a non-woven fabric or a sponge sheet with a siphon function is installed in the upper opening, the lower end of the non-woven fabric or the sponge sheet is located at the bottom of the transverse circular box body, the upper end of the non-woven fabric or the sponge sheet extends a certain length from the upper opening, and the welding belt slides through the inner part of the upper end of the non-woven fabric or the sponge sheet; soldering flux is installed in the rectangular main box body and the transverse circular box body, and the soldering flux is in contact with the lower end of the non-woven fabric or the sponge sheet.
2. The soldering flux coating mechanism according to claim 1, characterized in that: A connecting pipe is installed at the lower end of the rectangular main box body. The connecting pipe is connected to the lower end of the rectangular main box body through a vertical pipe. Stop valves are installed at both ends of the connecting pipe.
3. The soldering ribbon flux coating mechanism according to claim 2, characterized in that: The soldering ribbon flux coating mechanism is designed with two sets, and a second set is designed on the rear side of the first set. The design height of the second set is lower than that of the first set. The connecting pipe at the lower end of the first set is connected to the rectangular main box body of the second set and is separated by a stop valve; the soldering ribbon passes through the interior of the upper end of the non-woven fabric or sponge sheet of the higher set, and then slides through the interior of the upper end of the non-woven fabric or sponge sheet on the corresponding side of the lower set.
4. The soldering flux coating mechanism according to claim 1, characterized in that: The rectangular main box body and the transverse circular box body are made of transparent plastic.
5. The soldering ribbon flux coating mechanism according to claim 2, characterized in that: The connecting pipe and the vertical pipe are also made of transparent plastic.
6. The soldering ribbon flux coating mechanism according to claim 1, characterized in that: A cover plate is designed on the upper end of the rectangular main box body.