Low-warpage and high-hardness AG film
By coating the upper and lower layers on the base layer of the AG film, high hardness layers can be printed and added to the upper layer, the warping and high cost problems caused by the thickness of the existing AG hardened layer are solved, and low warping is achieved Its curvature, high hardness and durability reduce production costs and extend service life.
Patent Information
- Application Number
- CN202323230514.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-11-29
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2033-11-29
AI Technical Summary
Due to the thickness requirements of the existing AG hardened layer, the protective film layer structure is thick, not resistant to bending, easy to warp, and high production costs, making it easy to cause cracks in processing.
The high hardness layer can be printed on the substrate layer and the high hardness layer, and the AG scratch-resistant layer can be added to the upper layer can be printed on the high hardness layer. The UV curing resin material is formed to reduce the thickness of the AG scratch-resistant layer to reduce diffusion particles. Use to improve interlayer adhesion and overall hardness.
It realizes a low warping and high hardness AG film, which is resistant to bending and processing, is not prone to cracks, reduces production costs, improves scratch resistance, wear resistance and impact resistance, and extends service life.
Smart Images

Figure CN222024281U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of optical film materials, in particular to an AG film with low warping and high hardness. Background Art
[0002] The current protective film structure of the display panel of electronic products mainly includes a substrate layer made of PET and other materials and an AG hardening layer on the surface of the substrate layer. In order to have sufficient protection effect (hardness 6H, wear-resistant steel wool more than 1000 times), the AG hardening layer usually has to be 15-20um thick, while the PET substrate itself is 50-250um thick, which results in the entire protective film structure being thicker, not resistant to bending, and prone to cracking during processing. In addition, the AG hardening layer is severely warped and difficult to fit. In addition, this type of AG hardening layer needs to be thicker because it needs to achieve the corresponding hardness and wear resistance indicators. However, as the thickness increases, more diffusion particles such as SiO2, TiO2, and acrylic particles need to be added to the hardening liquid to achieve the AG effect, and the production cost is relatively high. Utility Model Content
[0003] The utility model aims to provide an AG film with low warping and high hardness, which is resistant to bending, is not prone to cracking and warping during processing, and has a low preparation cost.
[0004] In order to solve the above technical problems, the utility model adopts the following technical solution: a low-warping and high-hardness AG film, comprising a substrate layer, the upper surface of the substrate layer is coated with an upper printable high-hardness layer, the upper surface of the upper printable high-hardness layer is coated with an AG scratch-resistant layer, and the lower surface of the substrate layer is also coated with a lower printable high-hardness layer.
[0005] Preferably, the upper printable high hardness layer and the AG scratch-resistant layer have an overall hardness of ≥6H (750g), and a scratch resistance of at least 1000 times (500g load).
[0006] More preferably, the thickness of the upper printable high hardness layer is 3-8 um, the thickness of the AG scratch-resistant layer is 1-6 um, and the interlayer adhesion of the two layers is ≥5B.
[0007] More preferably, the thickness of the lower printable high hardness layer is 4-10 um.
[0008] More preferably, the substrate layer is a PET substrate or a PC substrate or a PC+PMMA composite substrate.
[0009] More preferably, the upper printable high hardness layer and the lower printable high hardness layer are both formed by coating a UV curable resin material on the substrate layer and then curing the material through UV light.
[0010] More preferably, the AG scratch-resistant layer is formed by coating a coating with diffusion particles added thereto on an upper printable high-hardness layer.
[0011] Compared with the prior art, the utility model pre-coats an upper printable high hardness layer on the substrate layer, and then coats an AG scratch-resistant layer on the upper printable high hardness layer, so that the AG scratch-resistant layer does not need to be set thicker, while at the same time can cooperate with the printable high hardness layer to achieve the required high hardness protection effect; since the AG scratch-resistant layer does not need to be set too thick, it can withstand bending and is not prone to cracking and warping during processing; in addition, the reduction in the thickness of the AG scratch-resistant layer means that the diffusion particles required in the molding process of this layer of coating are also reduced accordingly, thereby saving production costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Figure 1 It is a schematic diagram of the overall structure of an embodiment of the utility model.
[0013] In the figure:
[0014] 1 - Base material layer 2 - Upper layer can be printed with high hardness layer
[0015] 3——AG scratch-resistant layer 4——The lower layer can be printed with a high hardness layer DETAILED DESCRIPTION
[0016] In order to facilitate the understanding of those skilled in the art, the present invention is further described below in conjunction with embodiments and drawings. The contents mentioned in the implementation modes are not intended to limit the present invention.
[0017] like Figure 1 As shown, a low-warping and high-hardness AG film includes a substrate layer 1, the upper surface of the substrate layer 1 is coated with an upper printable high-hardness layer 2, the upper surface of the upper printable high-hardness layer 2 is coated with an AG scratch-resistant layer 3, and the lower surface of the substrate layer 1 is also coated with a lower printable high-hardness layer 4.
[0018] In the above structure, the upper printable high hardness layer 2 and the AG scratch-resistant layer 3 have an overall hardness of ≥6H (750g), and the scratch resistance is at least 1000 times (500g load).
[0019] The thickness of the upper printable high hardness layer 2 is 3-8um, the thickness of the AG scratch-resistant layer 3 is 1-6um, and the interlayer adhesion of the two layers is ≥5B. The thickness of the lower printable high hardness layer 4 is 4-10um. Those skilled in the art should know that the 1-6um AG scratch-resistant layer 3 is very thin. Since the AG scratch-resistant film 3 achieves the AG effect by protruding the added diffusion particles on the surface of the film layer, the thinner the film layer, the higher the haze. Under the same haze requirement, the required diffusion particle content will be less, which can effectively reduce the cost.
[0020] In this embodiment, the substrate layer 1 is a PET substrate or a PC substrate or an optical film substrate made of a blend of PC and PMMA.
[0021] Those skilled in the art should know that the above-mentioned upper printable high hardness layer 2 and lower printable high hardness layer 4 are formed by coating a UV curable resin material on the substrate layer 1 and then curing it with UV light. In addition, the AG scratch-resistant layer 3 in this embodiment is formed by coating a coating with diffusion particles added on the upper printable high hardness layer 2, and the added diffusion particles are diffusion particles such as SiO2, TiO2, and acrylic particles, and the added amount is 0.1-8%.
[0022] The low-warping and high-hardness AG film provided in the above-mentioned embodiment is manufactured by pre-coating an upper printable high-hardness layer 2 on the substrate layer 1, and then coating an AG scratch-resistant layer 3 on the printable high-hardness layer 2, so that the AG scratch-resistant layer 3 does not need to be set to be thicker, while at the same time can cooperate with the upper printable high-hardness layer 2 to achieve the required high-hardness protection effect; since the AG scratch-resistant layer 3 does not need to be set too thick, it can withstand bending and is not prone to cracking and warping during processing; in addition, the AG scratch-resistant layer 3 itself can also bring about the effect of reducing light reflection, and the reduction in the thickness of the AG scratch-resistant layer 3 means that the diffusion particles required in the molding process of this layer of coating are also reduced accordingly, thereby saving production costs.
[0023] Moreover, by coating the lower printable high-hardness layer 4 on the lower surface of the substrate layer 1, the shrinkage stress on both sides of the optical film can be better offset, thereby achieving a better overall flatness. In addition, the overall hardness is enhanced, so that the AG film can still maintain excellent scratch resistance and wear resistance in more severe environments. At the same time, it also makes the AG film more resistant to external forces and reduces deformation or breakage caused by bending or stress. Of course, the impact resistance of the entire AG film has also been improved, which means that if the device is accidentally impacted or hit, the AG film can better protect the screen and reduce the risk of breakage. Secondly, the durability is also enhanced. An additional printable hardening layer is provided on the lower surface of the substrate layer 1 to further extend the service life of the AG film. This hardening layer can bear part of the external pressure, reduce the erosion and damage to the AG layer and the substrate layer, thereby extending the service life of the film and improving the user experience. These advantages enable the low-warping and high-hardness AG film provided by the utility model to be better applied to screen display protection, and can replace the glass panel to achieve a significant effect of reducing costs.
[0024] In order to make it easier for ordinary technicians in this field to understand the improvements of the present invention over the prior art, some drawings and descriptions of the present invention have been simplified, and the above-mentioned embodiments are better implementation schemes of the present invention. In addition, the present invention can also be implemented in other ways. Any obvious replacement without departing from the concept of the technical solution is within the protection scope of the present invention.
Claims
1. A low-warpage and high-hardness AG film, comprising a substrate layer (1), characterized in that: The upper surface of the substrate layer (1) is coated with an upper printable high hardness layer (2), the upper surface of the upper printable high hardness layer (2) is coated with an AG scratch-resistant layer (3), and the lower surface of the substrate layer (1) is also coated with a lower printable high hardness layer (4).
2. The low-warpage and high-hardness AG film according to claim 1, characterized in that: The upper layer can be printed with a high hardness layer (2) and an AG scratch-resistant layer (3), the overall hardness of which is ≥6H, and the scratch resistance performance is more than 1000 times.
3. The low-warpage and high-hardness AG film according to claim 1, characterized in that: The thickness of the upper printable high hardness layer (2) is 3-8 um, the thickness of the AG scratch-resistant layer (3) is 1-6 um, and the interlayer adhesion between the upper printable high hardness layer (2) and the AG scratch-resistant layer (3) is ≥5B.
4. The low-warpage and high-hardness AG film according to claim 1, characterized in that: The thickness of the lower printable high hardness layer (4) is 4-10 um.
5. The low-warpage and high-hardness AG film according to claim 1, characterized in that: The substrate layer (1) is a PET substrate or a PC substrate.
6. The low-warpage and high-hardness AG film according to claim 1, characterized in that: The upper printable high hardness layer (2) and the lower printable high hardness layer (4) are both formed by coating a UV curable resin material on the substrate layer (1) and then curing it with UV light.