Detection device for visually representing expansion performance of expanding agent
By designing a detection device including steel mold test and characterization components, the problem of large dispersion difference in the detection results of expansion agents in the prior art is solved, and more accurate and efficient expansion performance detection is achieved, reducing the damage to brittle materials .
Patent Information
- Application Number
- CN202420509285.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-15
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2034-03-15
AI Technical Summary
In the prior art, the method for detecting the expansion performance of the expansion agent is simple to operate but is not conducive to the mixing and stirring of cement, expansion agent and water, resulting in a large dispersion of the test results, making it difficult to accurately detect the expansion performance of the concrete at the construction site.
A detection device including steel test mold and characterization components is designed. By first segmenting the test mold cavity with the baffle and sliding wheel, the mixing force of cement, expansion agent and water is increased, and the expansion is recorded using glass or ceramic characterization parts. Performance, reduce damage to brittle materials, and combine with the camera device to monitor the burst time in real time.
It improves the detection accuracy of the expansion agent and the reliability of experimental data, reduces the damage of cement to glass characterization parts, and enhances the efficiency and accuracy of the test.
Smart Images

Figure CN222028032U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of building materials, in particular to a detection device for intuitively characterizing the expansion performance of an expansion agent. Background Art
[0002] Under constrained conditions, the expansive agent can rely on chemical reactions to establish a certain pre-stress in the concrete, which is used to resist the shrinkage of the concrete (mainly drying shrinkage and cold shrinkage), prevent cracking, and improve the durability of the concrete. At present, the expansive agent has been widely used in self-waterproofing of concrete structures, construction of super-long structures, and control of temperature cracks in large-volume concrete. The expansion performance index of the expansive agent and expansive concrete, the limited expansion rate, is obtained by measuring the change in the length of the mortar or concrete specimen cast in the longitudinal limiter.
[0003] This method can quantitatively evaluate its expansion performance, but the test cycle is long. Most construction site conditions and quality inspection personnel are limited, making it difficult to quantitatively detect the limited expansion rate of expansive agents and expansive concrete. For this reason, Appendix C of GB 23439 (Concrete Expansive Agents) provides a rapid test method for the expansion performance of concrete with expansive agents and ring expansive agents, namely the beer bottle method (expansive agent) and the beaker method (expansive concrete). These methods are simple and fast to operate. Although these two methods are simple and feasible, they are not conducive to the mixing and compaction of cement, expansive agent and water, resulting in a large discrete deviation in the test results. Utility Model Content
[0004] In order to solve the deficiencies in the prior art, the utility model provides a detection device for intuitively characterizing the expansion performance of an expansion agent, thereby reducing the damage of cement to brittle characterizing parts such as glass and improving the accuracy of experimental data.
[0005] In order to achieve the above-mentioned purpose, the utility model is realized through the following technical scheme: a detection device for intuitively characterizing the expansion performance of an expansion agent, including a test mold, a characterization component is vertically arranged in the test mold, the characterization component includes a first frame, a second frame, a first baffle plate inserted in the first frame, and a characterization member inserted in the second frame, the first frame and the second frame are closely arranged, and the first baffle plate is rotatably arranged on both sides close to the first frame, and slide grooves compatible with the slide wheels are opened on both sides of the first frame.
[0006] The test mold is a steel test mold, and the steel test mold is vertically provided with a first frame and a second frame connected adjacently. The first frame is used to insert a steel baffle, which divides the steel test mold into two inner cavities. According to the number of characterization components, the steel test mold can be divided into two or more inner cavities for filling cement, expansion agent and water for testing. After the cement and expansion agent are filled, stirred and vibrated, the first baffle is gently pulled out, and the mixed cement and expansion agent are slowly filled into the glass side with tools, which can not only improve the mixing strength of cement, expansion agent and water, so that cement, expansion agent and test mold are fully fitted, but also reduce the damage of cement to brittle characterization parts such as glass, which affects the experimental data. Characterization parts are set on the other side of the first baffle. The characterization parts are made of glass or ceramic materials. The cracking time of brittle materials such as flat glass and ceramics is used to reflect the expansion performance of concrete. The principle of the concrete expansion performance characterization device is that when concrete expands, it generates pressure on the glass plate. When the expansion reaches a certain limit, the greater stress will cause cracks in the flat glass. The quality of the concrete expansion performance can be indirectly judged based on the time when the cracks appear.
[0007] The two sides of the first baffle are slidably connected to the two sides of the first frame through sliding wheels, so that the first baffle can be smoothly and slowly pulled out after filling cement and expansion agent.
[0008] Preferably, the two ends of the first frame are symmetrically arranged, the ends of the first frame are respectively L-shaped, and the sliding groove is arranged on the inner side of the L-shaped end.
[0009] Preferably, the bottom of the first baffle is configured as a downwardly inclined flow guide surface.
[0010] The guide surface is close to the side where cement and expansion agent are filled, so when the first baffle is lifted upward, the cement and expansion agent will slowly fill along the guide surface to the glass side on the first baffle side. The distance between the glass and the first baffle is relatively short, which can be between 0.5 and 2 cm, and the cement and expansion agent mixture is further filled to one side of the glass through tools.
[0011] Preferably, the characterization components are symmetrically arranged in two groups.
[0012] The two sets of characterization components can divide the test mold into three inner cavities, wherein the inner cavities on both sides are used to fill the same type or different types of expansion agents for experiments, thereby improving the test accuracy or test efficiency.
[0013] Preferably, a connecting rod is connected between the second frames of the two groups of characterization components.
[0014] The connecting rod can be connected to the middle or upper part or the upper part and the middle part of the second frames of the two groups of representation components to support the second frames of the two groups of representation components.
[0015] Preferably, a camera device is provided on the connecting rod.
[0016] The monitoring camera of the camera device can monitor the rupture time of the representative parts made of glass or ceramic materials in real time.
[0017] Compared with the prior art, the beneficial effects of the present invention are:
[0018] After the cement and expansion agent are filled, stirred and compacted, the baffle is gently pulled out, and the mixed cement and expansion agent are slowly filled to one side of the glass with tools. This can not only increase the mixing strength of cement, expansion agent and water, so that the cement, expansion agent and test mold are fully fitted, but also reduce the damage of cement to brittle representative parts such as glass, which affects the experimental data;
[0019] The two sets of characterization components can divide the test mold into three cavities, where the cavities on both sides are used to fill the same or different types of expansion agents for experiments, and the middle cavity is used to place connecting rods and camera devices, thereby improving test accuracy and efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Attached Figure 1 It is a schematic diagram of the three-dimensional structure of the utility model;
[0021] Attached Figure 2 It is a top view of the utility model;
[0022] Attached Figure 3 For the utility model Figure 2 The enlarged structural diagram at A in the middle;
[0023] Attached Figure 4 For the utility model Figure 2 Schematic diagram of the cross-sectional structure in CC direction;
[0024] Attached Figure 5 For the utility model Figure 4 Schematic diagram of the enlarged structure at point B in the middle.
[0025] The numbers shown in the accompanying drawings are: 1, test mold; 2, first frame; 201, slide groove; 3, second frame; 4, first baffle; 5, representative part; 6, sliding wheel; 7, guide surface; 8, connecting rod; 9, camera device; 10, handle. DETAILED DESCRIPTION
[0026] The present invention will be further described below in conjunction with specific embodiments. Figures 1 to 5As shown, a detection device for intuitively characterizing the expansion performance of an expansion agent includes a test mold 1, in which two groups of characterization components are vertically arranged, and the characterization components include a first frame 2, a second frame 3, a first baffle plate 4 inserted in the first frame 2, and a characterization member 5 inserted in the second frame 3. The first frame 2 and the second frame 3 are arranged closely, and the first baffle plate 4 is rotatably arranged on both sides close to the first frame 2, and a plurality of sliding wheels 6 are respectively rotatably arranged on both sides of the first frame 2, and sliding grooves 201 adapted to the sliding wheels 6 are opened on both sides of the first frame 2.
[0027] There are two groups of characterization components symmetrically arranged, and the two groups of characterization components can divide the test mold 1 into three inner cavities, wherein the inner cavities on both sides are used to fill the same or different types of expansion agents for experiments, and the material and thickness of the characterization parts 5 are consistent, thereby improving the test accuracy or test efficiency.
[0028] The test mold 1 is a steel test mold 1, and a first frame 2 and a second frame 3 adjacent to each other are vertically arranged inside the steel test mold 1. A first baffle 4 made of steel is inserted into the first frame 2, and the first baffle 4 divides the steel test mold 1 into two inner cavities. According to the number of characterization components, the steel test mold 1 can be divided into two or more inner cavities for filling cement, expansion agent and water for testing. After the cement and expansion agent are filled, stirred and vibrated, the first baffle 4 is gently pulled out, and the mixed cement and expansion agent are slowly filled into one side of the glass with a tool, which can not only improve the mixing strength of the cement, expansion agent and water, so that the cement, expansion agent and the test mold 1 are fully fitted, but also reduce the damage of cement to brittle characterization parts 5 such as glass, which affects the experimental data. A characterizing piece 5 is first set on the other side of the baffle 4. The characterizing piece 5 is made of glass or ceramic material, and its surface is covered with a plastic film. After the concrete specimen is finally set, the plastic film is removed and the specimen is covered with a damp rag for curing. The timing starts when the concrete begins to be stirred with water and ends when the first crack appears on the characterizing piece 5. The rupture time of the glass characterizing piece 5 is recorded. The utility model uses the cracking time of brittle materials such as flat glass and ceramics to reflect the expansion performance of concrete. The principle of the concrete expansion performance characterization device is that when concrete expands, pressure is generated on the glass plate. When the expansion reaches a certain limit, the greater stress will cause cracks in the flat glass. The expansion performance of the concrete can be indirectly judged based on the time when the cracks appear.
[0029] A handle 10 is provided on one side of the first baffle plate 4 near the upper end of the inner cavity. The two sides of the first baffle plate 4 are slidably connected to the two sides of the first frame 2 through the sliding wheels 6, so that after filling with cement and expansion agent, the first baffle plate 4 can be smoothly and slowly pulled out through the handle 10. The bottom of the first baffle plate 4 is set as a downwardly inclined guide surface 7. The guide surface 7 is close to the side where the cement and expansion agent are filled, so that when the first baffle plate 4 is lifted upward, the cement and expansion agent will slowly fill the glass side of one side of the first baffle plate 4 along the guide surface 7. The distance between the glass and the first baffle plate 4 is relatively short, which can be between 0.5 and 2 cm, and the cement and expansion agent mixture is further filled to one side of the glass through tools.
[0030] The two ends of the first frame 2 are symmetrically arranged, and the ends of the first frame 2 are L-shaped, and the slide groove 201 is arranged on the inner side of the L-shaped end. The two ends of the L-shaped shape are integrally formed by a straight plate to form the first frame 2, and the second frame 3 is a U-shaped structure for stably inserting and placing the flat glass.
[0031] A connecting rod 8 is connected between the second frames 3 of the two groups of characterization components. The connecting rod 8 can be connected to the middle or upper part or the upper part and the middle part of the second frames 3 of the two groups of characterization components to support the second frames 3 of the two groups of characterization components. A camera device 9 is provided on the connecting rod 8. The camera device 9 can monitor the cracking of the characterization member 5 made of glass or ceramic material in real time.
[0032] Working principle: The inner cavity of the test mold is used to fill cement, expansion agent and water for testing. After the cement and expansion agent are filled, stirred and vibrated, the first baffle 4 is gently pulled out, and the cement and expansion agent will slowly fill to the glass side of the first baffle 4 along the guide surface 7, and the cement and expansion agent mixture is further filled to the glass side through tools. The surface of the concrete specimen is covered with plastic film. After the concrete specimen is finally set, the plastic film is removed and covered with a damp rag for maintenance. The timing starts when the concrete is started to be stirred with water and ends when the first crack appears on the representative piece 5. The rupture time of the glass material representative piece 5 is recorded.
[0033] It should be understood that these embodiments are only used to illustrate the present invention and are not used to limit the scope of the present invention. In addition, it should be understood that after reading the content taught by the present invention, those skilled in the art can make various changes or modifications to the present invention, and these equivalent forms also fall within the scope defined by the present application.
Claims
1. A detection device for intuitively characterizing the expansion performance of an expansion agent, comprising a test mold (1), characterized in that: A characterization component is vertically arranged in the test mold (1), and the characterization component includes a first frame (2), a second frame (3), a first baffle plate (4) inserted in the first frame (2), and a characterization member (5) inserted in the second frame (3). The first frame (2) and the second frame (3) are arranged closely together, and a plurality of sliding wheels (6) are rotatably arranged on both sides of the first baffle plate (4) close to the first frame (2), and sliding grooves (201) adapted to the sliding wheels (6) are provided on both sides of the first frame (2).
2. A detection device for intuitively characterizing the expansion performance of an expansion agent according to claim 1, characterized in that: The two ends of the first frame (2) are symmetrically arranged, the ends of the first frame (2) are respectively L-shaped, and the sliding groove (201) is arranged on the inner side of the L-shaped end.
3. A device for detecting the expansion performance of an expansion agent according to claim 1, characterized in that: The bottom of the front baffle (4) is arranged as a downwardly inclined flow guide surface (7).
4. A detection device for intuitively characterizing the expansion performance of an expansion agent according to claim 1, characterized in that: The characterization components are symmetrically arranged in two groups.
5. A detection device for intuitively characterizing the expansion performance of an expansion agent according to claim 4, characterized in that: A connecting rod (8) is connected between the second frames (3) of the two groups of the characterization components.
6. A detection device for intuitively characterizing the expansion performance of an expansion agent according to claim 5, characterized in that: A camera device (9) is provided on the connecting rod (8).