Riveting die for frame rivets of electronic products

By using two sets of molds for stretching and secondary stamping, the problem of surface deformation caused by existing stamping methods has been solved, achieving stable riveting and efficient production, reducing costs and energy consumption, and improving the strength and appearance quality of the frame.

CN222036697UActive Publication Date: 2024-11-22DONGGUAN PINYANG HARDWARE TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420782160.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-15
Publication Date
2024-11-22
Estimated Expiration
2034-04-15

AI Technical Summary

Technical Problem

Existing stamping methods cause deformation of the electronic product frame's appearance, affecting product yield and resulting in unstable riveting.

Method used

Two sets of molds are used for riveting, including a first upper mold and a second upper mold. Through stretching and secondary stamping steps, the solid riveting head body and the rivet post of the central shaft hole are used for precise positioning and stable connection, decomposing the stress support points and reducing the deformation of the appearance surface.

Benefits of technology

It improves production efficiency and product stability, reduces production costs and energy consumption, meets environmental protection requirements, enhances assembly precision and appearance integrity, and strengthens the frame.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222036697U_ABST
    Figure CN222036697U_ABST
Patent Text Reader

Abstract

The utility model discloses a riveting die for electronic product frame rivets, which comprises a lower die for positioning an aluminum alloy frame and an upper die arranged above the lower die, the upper die comprises two sets of dies including a first upper die and a second upper die, the first upper die comprises a first forming punch rod provided with a first hollow cavity and a first punch pin arranged in the first hollow cavity, a first forming interval matched with the wall thickness of a riveting column is defined by the first punch pin and the first punch rod, the second upper die comprises a second forming punch rod provided with a second hollow cavity and a second punch pin arranged in the second hollow cavity, and a second forming interval matched with the wall thickness of the riveting column is defined by the second forming punch rod and the second punch pin. And a second forming space matched with the wall thickness of the riveting column is defined by the second punching needle and the second forming punching rod. The rivet head main body and the aluminum alloy frame are completely combined through the secondary punching step, and under the pressure action of the second forming punching rod and the second punching needle, the deformation part serves as a fulcrum for decomposing downward pressure, so that the downward pressure of the rivet head main body part is converted into deformation pressure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of electronic product processing methods, and in particular to a riveting die for electronic product frame rivets. Background Art

[0002] In the processing of metal electronic products (such as laptops, tablets, all-in-one computers, etc.), it is generally necessary to set plastic structural parts on the frame to form studs, so as to achieve mutual connection and fixation between the shells (such as C shell (i.e. keyboard frame) + D shell).

[0003] However, when stamping a special rivet, if the existing stamping method is used, it will cause a large deformation of the appearance surface, which will affect the qualification rate of the product. Therefore, how to design a mold that can reduce the stability of the appearance surface and ensure the stability of the riveting is the key to the design. Summary of the invention

[0004] The main purpose of the present invention is to provide a riveting die for electronic product frame rivets, aiming to improve the existing die structure, so that the rivets can be stably installed on the electronic frame and the damage to the appearance surface can be reduced.

[0005] To achieve the above-mentioned purpose, the present invention provides a riveting die for electronic product frame rivets, comprising a lower die for positioning an aluminum alloy frame and an upper die arranged above the lower die, the upper die comprising two sets of dies, including a first upper die and a second upper die, the first upper die comprising a first forming punch provided with a first hollow cavity and a first punch needle arranged in the first hollow cavity, the first punch needle and the first punch rod form a first forming spacing suitable for the wall thickness of the rivet column, the second upper die (21) comprising a second forming punch rod (23) provided with a second hollow cavity and a second punch needle (24) arranged in the second hollow cavity, the second punch needle (24) and the second forming punch rod (23) form a second forming spacing (25) suitable for the wall thickness of the rivet column (202).

[0006] The technical effect is as follows: through the solid structure of the rivet head body and the rivet column of the central axis hole, the aluminum alloy frame is firstly placed in the fixture of the lower mold after being shaped, and accurate positioning is achieved. Then, the rivet is stretched to achieve preliminary positioning of the deformation part and the aluminum alloy frame. At the same time, the force fulcrum can be decomposed through the deformation and stretching of the rivet column, so that the combination of the rivet column part and the aluminum alloy frame is more stable.

[0007] After the secondary stamping step is performed to completely combine the rivet head body with the aluminum alloy frame, under the pressure of the second forming punch and the second punch needle, the deformation part serves as a fulcrum for decomposing the downward pressure, so that the downward pressure of the rivet head body is converted into deformation pressure;

[0008] By using two sets of molds with the same structure, the production efficiency is effectively improved. Of course, in actual design, the predetermined processing requirements can also be achieved by using one set of molds. BRIEF DESCRIPTION OF THE DRAWINGS

[0009] Figure 1 This is a view of the clamping rod of the present invention clamping a rivet;

[0010] Figure 2 A schematic diagram of the cooperation between the first upper die and the first lower die in the stretching step;

[0011] Figure 3 A schematic diagram of the cooperation between the second upper die and the second lower die in the secondary stamping step;

[0012] Figure 4 Schematic diagram of the mold

[0013] Figure 5 This is a schematic diagram of the rivet before processing;

[0014] Figure 6 It is a schematic diagram after the rivet stretching step;

[0015] Figure 7 This is a schematic diagram of the rivet after the secondary stamping step;

[0016] Figure 8 It is a schematic diagram of the aluminum alloy frame;

[0017] Fig. 9 This is a processing diagram of a 1.2 mm aluminum alloy frame in the fourth embodiment;

[0018] Fig.10 This is a processing diagram of a 1.6 mm aluminum alloy frame in the third embodiment.

[0019] In the figure, 100 is an aluminum alloy frame, 101 is an exterior surface,

[0020] 200 is a rivet, 201 is a rivet head body, 202 is a rivet column, 203 is a central axis hole, 204 is an annular groove, 2041 is a first side wall, 2042 is a second side wall, 205 is a first closed-loop groove, 206 is a second closed-loop groove, 207 is a guide inclination, 208 is a deformation portion, 209 is a flat surface,

[0021] 300 is a positioning hole, 301 is a riveting layer, and 302 is a protrusion with a predetermined height.

[0022] 400 is a second rivet column, 401 is a stepped portion, 402 is a second central axis hole,

[0023] 11 is the first upper die, 12 is the first lower die, 13 is the first forming punch, 14 is the first punch needle, 15 is the first forming distance,

[0024] 21 is the second upper die, 22 is the second lower die, 23 is the second forming punch, 24 is the second punch needle, 25 is the second forming distance,

[0025] 3 is the punch body, 31 is the first chamfer, 32 is the first end,

[0026] 4 is a straight wall, 41 is a second chamfer,

[0027] 5 is a notch, 51 is a pressure part,

[0028] 6 is a clamping rod, and 61 is a limiting surface. DETAILED DESCRIPTION

[0029] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0030] It should be noted that if the embodiments of the present invention involve directional indications (such as up, down, left, right, front, back, top, bottom, inside, outside, vertical, horizontal, longitudinal, counterclockwise, clockwise, circumferential, radial, axial...), then the directional indication is only used to explain the relative position relationship, movement status, etc. between the components in a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.

[0031] In addition, if there are descriptions involving "first" or "second" etc. in the embodiments of the present invention, the descriptions of "first" or "second" etc. are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" or "second" may explicitly or implicitly include at least one of the features. In addition, the technical solutions between the various embodiments can be combined with each other, but they must be based on the ability of ordinary technicians in the field to implement them. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such combination of technical solutions does not exist and is not within the scope of protection required by the present invention.

[0032] like Figures 1 to 8 As shown, a riveting method for an electronic product frame with special-shaped rivets comprises:

[0033] The rivet 200 is applied to the installation of the thin-walled aluminum alloy frame 100 of the electronic product, and the aluminum alloy frame 100 has a thickness within a predetermined range (the conventional aluminum alloy frame thickness is 5-8 mm);

[0034] The rivet 200 includes a rivet head body 201 and a rivet column 202 extending upward from the rivet head body 201, wherein the rivet column 202 has a central axis hole 203 or a solid structure, and the rivet head body 201, the rivet column 202 and the central axis hole 203 are coaxially arranged, and the bottom of the central axis hole is a solid rivet head body;

[0035] The aluminum alloy frame 100 is provided with a positioning hole 300 for accommodating the rivet head body 201. The positioning hole 300 is recessed in the aluminum alloy frame 100, and the thickness of the positioning hole 300 is greater than the thickness of the aluminum alloy frame 100. The thickness of the positioning hole is 0.8 mm-3 mm. Of course, it can also be applied to products with a thickness of about 3 mm or more. That is, the greater the thickness, the less difficult it is to process, and the positioning hole will not even be deformed.

[0036] An annular groove 204 is provided between the connecting ends of the rivet head body 201 and the rivet column 202. The annular groove 204 is provided on the radial inner side of the rivet head body 201. The annular groove 204 is provided on the upper wall of the rivet head body 201. The annular groove 204 includes a first side wall 2041 away from the rivet column 202 and a second side wall 2042 close to the rivet column 202. The annular groove 204 is provided with a guide inclination angle 207 of a predetermined range between the first side wall 2041 and the second side wall 2042.

[0037] The rivet head body 201 is provided with a deformation portion 208 of a predetermined thickness at the lower wall of the rivet column 202;

[0038] The riveting die comprises a lower die for positioning the aluminum alloy frame 100 and an upper die arranged above the lower die, the upper die comprises two sets of dies, including a first upper die 11 and a second upper die 21, the first upper die 11 comprises a first forming punch rod 13 provided with a first hollow cavity and a first punch needle 14 arranged in the first hollow cavity, the first punch needle 14 and the first punch rod form a first forming spacing 15 suitable for the wall thickness of the rivet column 202,

[0039] The second upper die 21 includes a second forming punch 23 with a second hollow cavity and a second punch pin 24 disposed in the second hollow cavity. The second punch pin 24 and the second forming punch 23 form a second forming interval 25 suitable for the wall thickness of the rivet column 202.

[0040] A stretching step, in which the first upper die 11 and the lower die are closed, and the first punch 14 and the first forming punch 13 apply a predetermined pressure, so that the rivet column 202 is stretched to a predetermined height under the extrusion force. At the same time, the guide angle 207 is deformed into a flat surface 209 under pressure, and the rivet head body 201 is forced to partially fit with the positioning hole 300 or non-stacked positioning, that is, partially embedded or not embedded but only positioned;

[0041] Secondary stamping step, in which the second upper mold 21 and the lower mold are closed, and then the second forming punch 23 and the second punch needle 24 apply secondary pressure to deform the deformation portion 208 and the bottom of the rivet head body 201. At the same time, the height of the central axis hole 203 continues to stretch, thereby riveting the rivet head body 201 and the positioning hole 300 to form a riveting layer 301.

[0042] In the aluminum alloy frame 100 of the electronic product, one of the factors for checking whether the product is qualified is the deformation degree of the appearance and whether there are defects. Therefore, the structure cannot be used for welding, which will cause the deformation of the aluminum alloy material and the local strength reduction, and welding lines will appear. Conventional perforated rivets 200 and other structures will also have rivet lines even after grinding, otherwise it will affect the appearance of the product, and there will also be problems of uneven frame strength.

[0043] In the processing method, the aluminum alloy frame 100 is firstly placed in the jig of the lower mold through the solid rivet head body 201 and the rivet column 202 of the central axis hole 203 to achieve precise positioning. Then, the rivet 200 is stretched to achieve preliminary positioning of the deformation part 208 and the aluminum alloy frame 100. At the same time, the force fulcrum can be decomposed through the deformation and stretching of the rivet column 202, so that the rivet column 202 is more stably combined with the aluminum alloy frame 100.

[0044] The rivet head body 201 is completely combined with the aluminum alloy frame 100 through the secondary stamping step. Under the pressure of the second forming punch 23 and the second punch needle 24, the deformation part 208 acts as a fulcrum to decompose the downward pressure, so that the downward pressure of the rivet head body 201 is partially converted into deformation pressure, and the sinking of the central rivet hole is achieved. In the secondary stamping step, the rivet column body is not further stretched, but the central axis hole sinks, thereby combining the rivet head body and the aluminum alloy frame to form a riveted layer 301.

[0045] Compared with the existing technology, 1. Compared with the existing technology, the overall processing cost and processing time are shorter, the structural strength is higher, the strength of the plastic frame + aluminum alloy is different from the strength of a single aluminum alloy frame of the same thickness, and the production cost is lower, the use of plastic materials and glue is reduced, and the environmental protection is effectively improved. Especially for some areas with strict control over plastic products, plastic products are white pollution, so their green environmental protection is poor, and the recycling cost is high, reducing carbon emissions, while the production mold and production cost, the unit price is lower, and its unit price can be comparable to that of plastic with aluminum alloy frame, and the processing time is 20-35 minutes;

[0046] 2. Compared with a single thick aluminum alloy frame directly processed by CNC, the side wall is also processed by CNC, which takes less processing time, has lower energy consumption and less material waste, that is, less electricity consumption and aluminum alloy consumables.

[0047] The two sets of molds can be of the same structure, or the same mold, to achieve the processing of two sets of processes;

[0048] 3. Meeting the environmental protection requirements of ESG effectively improves the market competitiveness of producers and increases market recognition.

[0049] 4. The assembly accuracy is higher, that is, the position of the rivet column can remain basically unchanged during the processing of the mold, and the tolerance can be controlled to ±0.05mm (i.e. 5 wires);

[0050] 5. The product appearance can be improved twice, that is, it does not affect the integrity of the appearance, and achieves an effect close to one-piece molding.

[0051] In the first embodiment, if Figure 1-7 The thickness of the positioning hole of the aluminum alloy frame is 0.8mm, the height of the central axis hole of the rivet column before riveting is 1.5mm, and the punching machine with a die tonnage of 110T~160T is used. The height of the central axis hole of the rivet column after the first upper die riveting is 2.6mm. The punching machine with a die tonnage of 110T~160T is used. The height of the central axis hole of the rivet column after the second upper die riveting is 2.9mm, and then the appearance surface is trimmed by about 0.3mm. Its tensile strength is 50kg;

[0052] In the second embodiment, if Figure 1-7 In the process, the thickness of the positioning hole of the aluminum alloy frame is 2mm, the height of the central axis hole of the rivet column before riveting is 2.6mm, and the punching machine with the mold tonnage controlled at 110T~160T is adopted. The height of the central axis hole of the rivet column after the first upper die riveting is 3.4mm. The punching machine with the mold tonnage controlled at 110T~160T is adopted. The height of the central axis hole of the rivet column after the second upper die riveting is 3.6mm, and then the appearance surface is trimmed by about 0.5mm, and its tensile strength is 80kg;

[0053] In the third embodiment, Fig.10In the embodiment, the thickness of the positioning hole of the aluminum alloy frame is 1.6mm, the rivet column before riveting is a solid structure with a thickness of 1.6mm, the annular groove is provided with a guide inclination angle of the predetermined range, ① the punching machine with a die tonnage controlled at 110T to 160T is used to punch a 3.7mm chamfer, at which time the aluminum alloy frame and the rivet head body 201 are initially positioned, ② then a 3.55mm central rivet hole is formed, and the aluminum alloy frame and the rivet head body are initially riveted; ③ and then the stepped portion 401 of the second rivet column 400 is riveted and embedded into the central axis hole through the second upper die (of course, it can also be the third upper die); ④ the second rivet column is provided with a second central axis hole 402, and in the second riveting, the second axis axis hole continues to sink and the height of the second central axis hole 402 is increased by 0.2mm, and the bottom of the rivet head body continues to be riveted with the aluminum alloy frame, and the riveting thickness of the riveted layer is increased, and finally the mold print of the appearance surface is cut by CNC (reshaping step), and its tensile strength is 50kg.

[0054] In the fourth embodiment, Fig. 9 In the embodiment, the thickness of the positioning hole of the aluminum alloy frame position is 1.2mm, the rivet column before riveting is a solid structure with a thickness of 1.2mm, the annular groove is provided with a guide inclination angle specifically having the predetermined range, ① the punching machine with a die tonnage controlled at 110T to 160T is used to punch a 3.7mm chamfer, at which time the aluminum alloy frame and the rivet head body 201 are initially positioned, ② then a 3.55mm central rivet hole is formed, and the aluminum alloy frame and the rivet head body are initially riveted; ③ and then the stepped portion of the second rivet column is riveted and embedded into the central axis hole through the second upper die (of course, it can also be the third upper die); ④ the second rivet column is provided with a second central axis hole, and in the second riveting, the second axis axis hole continues to sink and the height of the second central axis hole is increased by 0.2mm, and the bottom of the rivet head body continues to be riveted with the aluminum alloy frame, and the riveting thickness of the riveted layer is increased, and finally the mold print of the appearance surface is cut by CNC (reshaping step), and its tensile strength is 50kg.

[0055] In the third and fourth embodiments, a different processing method is adopted from that of the first and second embodiments, that is, a second rivet column structure is adopted, which can achieve more stringent processing requirements and reduce the deformation of the appearance surface to 0.2mm. The tensile strength is 50kg.

[0056] It can be seen from the processing embodiment with the minimum positioning hole thickness of 0.8 mm that the predetermined two-punching structure can effectively ensure the bonding degree between the rivet and the thin plate. Of course, the deformation of the thin plate is ignored during the test of this structure, and the tensile force stretches the rivet stud upward at a speed of 50.0 mm / min until a crack appears between the thin plate and the rivet stud;

[0057] The 2mm positioning hole is mainly the size of most thin plate structures, so longer rivet columns are used. At the same time, thicker thin plates can still achieve good tensile test results.

[0058] Therefore, in the actual use of electronic products, the shell's drop resistance can be guaranteed and the problem of rivet post breakage can be avoided. The one-piece molded rivet post has a much higher breakage rate than the rivet post structure of the present application because it does not undergo secondary stamping.

[0059] Specifically, a side of the aluminum alloy frame 100 away from the positioning hole 300 is an appearance surface 101 .

[0060] More specifically, the annular groove 204 includes a first closed-loop groove 205 and a second closed-loop groove 205 spaced apart from the first side wall 2041 toward the second side wall 2042, the thickness of the second closed-loop groove 205 is greater than the thickness of the first closed-loop groove 205, and the first closed-loop groove 205 is provided with the guide inclination angle 207;

[0061] After the secondary stamping step, the second closed-loop groove 205 is deformed to bulge upward.

[0062] In the embodiment of the present invention, the angle of the guide inclination 207 from the lowest point to the axis is 15 degrees to 35 degrees, and the bottom end of the central axis hole is a conical surface.

[0063] Therefore, the rivet head body 201 can be smoothly combined during riveting and fixing, avoiding deformation of the appearance surface 101 of the aluminum alloy frame 100 caused by direct extrusion force, and avoiding deformation of the riveting column caused by the stretching step.

[0064] In the stretching step, the guide inclination angle 207 also achieves the effect of stretching the rivet column 202, so that the rivet column 202 is stretched toward the first forming interval 15;

[0065] The setting of the conical surface can realize the stretching of the central axis hole and at the same time play a role of stamping guide, so that the rivet column is stretched.

[0066] There is a vertical clamping step before the stretching step. A lowest point is provided at the lower end of the clamping rod 6 . An inclined limiting surface 61 is extended upwardly toward the central axis hole 203 from the lowest point. The limiting surface is structurally compatible with the guide inclination angle 207 .

[0067] Through the cooperation of the limiting surface and the guide inclination angle 207 , the vertical clamping of the rivet column 202 is achieved.

[0068] Furthermore, the first punch needle 14 and the second punch needle 24 have the same structure, including a punch rod body 3, a first end portion 32 arranged at the bottom end of the punch rod body 3, and a first chamfer 31 arranged at the upper end of the punch rod body 3, and the first end portion 32 is arranged to gradually reduce in diameter from the punch rod body 3 downward.

[0069] The first end portion 32 can be used to apply force to the lower end, thereby preventing the radial pressure of the punch body 3 from causing deformation of the rivet column 202 during mold closing, and achieving a consistent thickness of the rivet column 202, that is, decomposing the downward pressure into downward and deformation extrusion forces.

[0070] In the embodiment of the present invention, the first forming punch 13 and the second forming punch 23 have the same structure. A straight wall 4 is provided at the lower end of the forming punch, and a second chamfer 41 is provided at the inner end of the straight wall 4 .

[0071] By setting the second chamfer 41, the first closed-loop groove 205 is formed into a straight surface suitable for the straight wall 4 under pressure guidance, wherein the setting of the straight wall 4 can reduce the later processing time.

[0072] At the same time, the first closed-loop groove 205 is deformed under the action of pressure, thereby avoiding deformation of the appearance surface 101 of the aluminum alloy frame 100 caused by the vertical force, thereby improving production stability.

[0073] After the secondary stamping step, a trimming step is also included. After the riveting layer is formed, the appearance surface is partially protruded by a predetermined height, and after CNC processing, a 100mm-150mm flying cutter is used to trim the appearance surface to a predetermined value of 0.1mm-0.5mm, and the appearance surface is made flat. The deformation tolerance of the processed appearance surface can be controlled within the range of plus or minus 0.05mm, and the tolerance of the prior art is generally ±0.15mm.

[0074] The shaping step also includes a tapping step, wherein the tapping step is used to form a threaded hole in the central axis hole 203 of the rivet column 202 .

[0075] The second closed-loop groove 205 is used to decompose the vertical pressure. The first forming punch 13 and the second forming punch 23 are respectively provided with a notch 5 that avoids the second closed-loop groove 205. The first forming punch 13 and the second forming punch 23 are respectively provided with a pressing portion 51 that matches the rivet head body 201.

[0076] In another embodiment, the central axis hole is embedded with a second rivet column, the second rivet column has a predetermined height, and the bottom of the second rivet column has a stepped portion.

[0077] First, the stepped portion is riveted and formed into the central shaft hole;

[0078] The second rivet column is provided with a second central axis hole. During the second riveting, the second central axis hole continues to sink and the height of the second central axis hole is increased, and the bottom of the rivet head body continues to be riveted with the aluminum alloy frame, and the riveting thickness of the riveted layer is increased.

[0079] By providing the notch 5 and the pressing portion 51 , the second closed-loop groove 205 can further reduce the frame deformation caused by the vertical pressure, that is, the pressure is partially decomposed to the second closed-loop groove 205 , and at the same time, part of the pressure of the rivet head body 201 is also decomposed radially.

[0080] Compared with the second production method, it reduces the cost of making molds for rubber parts, reduces the number of assembly steps for rubber parts, effectively avoids the risk of studs or rubber surfaces coming apart, and provides high strength for the entire machine (according to the purchaser's needs, there are requirements for weight and actual thickness, such as requiring the maximum wall thickness not to exceed 5mm), reducing costs by more than 20%.

[0081] The rivet stud is punched into the desired shape of the preformed product by a punch of a predetermined shape, and the preformed shape is a solid cylinder. The rivet stud is punched, so its structural toughness is better.

[0082] Its main feature is that it uses the strong plasticity of aluminum and adopts a special strong extrusion multi-step process to form a rivet column of a certain height.

[0083] The above description is only a preferred embodiment of the present invention, and does not limit the patent scope of the present invention. All equivalent structural changes made by using the contents of the present invention specification and drawings under the inventive concept of the present invention, or directly / indirectly applied in other related technical fields are included in the patent protection scope of the present invention.

Claims

1. A riveting die for electronic product frame rivets, It is characterized in that It comprises a lower die for positioning an aluminum alloy frame (100) and an upper die arranged above the lower die, The upper die comprises two sets of dies, including a first upper die (11) and a second upper die (21); the first upper die (11) comprises a first forming punch (13) provided with a first hollow cavity, and a first punch needle (14) provided in the first hollow cavity; the first punch needle (14) and the first punch form a first forming spacing (15) suitable for the wall thickness of the rivet column (202); The second upper die (21) comprises a second forming punch rod (23) provided with a second hollow cavity and a second punch needle (24) provided in the second hollow cavity, wherein the second punch needle (24) and the second forming punch rod (23) form a second forming spacing (25) suitable for the wall thickness of the rivet column (202).

2. The riveting die for electronic product frame rivets according to claim 1, Features: The mold also includes a vertical clamping mold, the upper mold of the clamping mold is provided with a clamping rod (6), and the lower end of the clamping rod is provided with a lowest point.

3. The riveting die for electronic product frame rivets as claimed in claim 2, Features: The lowest point is provided with an inclined limiting surface (61) extending obliquely upward toward the central axis hole (203), and the limiting surface is structurally compatible with the guide inclination angle (207).

4. The riveting die for electronic product frame rivets according to claim 1, Features: The first punch needle (14) and the second punch needle (24) have the same structure, comprising a punch rod body (3), a first end portion (32) arranged at the bottom end of the punch rod body (3), and a first chamfer (31) arranged at the upper end of the punch rod body (3).

5. The riveting die for electronic product frame rivets as claimed in claim 4, Features: The first end portion (32) is arranged to gradually reduce in diameter downward from the punch rod body (3).

6. The riveting die for electronic product frame rivets according to claim 1, Features: The first forming punch (13) and the second forming punch (23) have the same structure. The lower end of the forming punch is provided with a straight wall (4), and the inner side end of the straight wall (4) is provided with a second chamfer (41).

7. The riveting die for electronic product frame rivets as claimed in claim 3, Features: The first forming punch (13) and the second forming punch (23) are respectively provided with a notch (5) for avoiding the second closed-loop groove (205).

8. The riveting die for electronic product frame rivets as claimed in claim 3, Features: The first forming punch (13) and the second forming punch (23) are respectively provided with a pressing portion (51) that matches the rivet head body (201).