Tough gas-phase antirust paper containing hydrophobic layer

By introducing a combination of a hydrophobic layer and a flame-retardant layer into the vapor phase rust-preventive paper, the problem of insufficient waterproof and fire-resistant performance is solved, achieving higher waterproof and flame-retardant effects and protecting metal products from damage.

CN222043060UActive Publication Date: 2024-11-22SHUN QIANG STATIONERY (ZJGFTZ) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420065355.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-11
Publication Date
2024-11-22
Estimated Expiration
2034-01-11

AI Technical Summary

Technical Problem

Existing vapor phase rust inhibitors have poor waterproof and fire-resistant properties, which can easily lead to moisture-induced corrosion and fire damage to metal products.

Method used

A tough vapor phase corrosion inhibitor paper with a hydrophobic layer was designed. The paper enhances its waterproof and flame-retardant properties by sequentially coating a vapor phase corrosion inhibitor, a toughening layer, a flame-retardant layer, a waterproof film, and a hydrophobic layer onto the paper layer.

Benefits of technology

The improved waterproof and flame-retardant properties of vapor phase rust inhibitor paper reduce the risk of metal products being damaged by moisture and fire, thus gaining more time for rescue.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222043060U_ABST
    Figure CN222043060U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of anti-rust paper, in particular to tough gas-phase anti-rust paper containing a hydrophobic layer, which comprises a neutral paper layer, and the upper end and the lower end of the neutral paper layer are respectively coated with a gas-phase corrosion inhibitor I and a gas-phase corrosion inhibitor II in a dip-coating mode. A first tough layer, a first flame-retardant layer, a first waterproof film layer and a first hydrophobic layer are sequentially adhered to the lower end of the vapor phase corrosion inhibitor through adhesives from bottom to top, and a second tough layer, a second flame-retardant layer, a second waterproof film layer and a second hydrophobic layer are sequentially adhered to the lower end of the vapor phase corrosion inhibitor through adhesives from top to bottom. According to the utility model, the waterproof and flame-retardant properties of the gas-phase antirust paper can be improved, so that more rescue time can be won for metal products packaged by the gas-phase antirust paper no matter the gas-phase antirust paper encounters fire or rain, and the damage of the metal products is reduced to the greatest extent.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of anti-rust paper, in particular to a tough vapor anti-rust paper containing a hydrophobic layer. Background Art

[0002] Vapor phase anti-rust paper is a special anti-rust packaging material that uses special neutral paper as the base material, is coated with special substances - vapor phase corrosion inhibitors of different formulations, and undergoes a series of post-processing.

[0003] The existing vapor-phase anti-rust paper has poor waterproof and fire-resistant properties. During actual use, external water sources can easily penetrate the vapor-phase anti-rust paper, making the metal products packaged with the vapor-phase anti-rust paper susceptible to moisture and rust. In the event of a fire, the fire will quickly burn the vapor-phase anti-rust paper, which can easily cause damage to the metal products packaged with the vapor-phase packaging paper. Therefore, it is necessary to design a tough vapor-phase anti-rust paper containing a hydrophobic layer. Utility Model Content

[0004] The utility model aims to solve the shortcomings in the prior art and proposes a tough vapor anti-rust paper containing a hydrophobic layer.

[0005] In order to achieve the above-mentioned purpose, the utility model adopts the following technical scheme: a tough vapor phase anti-rust paper containing a hydrophobic layer, comprising a neutral paper layer, the upper and lower ends of the neutral paper layer are respectively dipped with vapor phase corrosion inhibitor 1 and vapor phase corrosion inhibitor 2, the upper end of the vapor phase corrosion inhibitor 1 is sequentially bonded with tough layer 1, flame retardant layer 1, waterproof film layer 1 and hydrophobic layer 1 through an adhesive from bottom to top, and the lower end of the vapor phase corrosion inhibitor is sequentially bonded with tough layer 2, flame retardant layer 2, waterproof film layer 2 and hydrophobic layer 2 through an adhesive from top to bottom.

[0006] Furthermore, an adhesive layer is adhered to the lower end of the second hydrophobic layer, and a release paper layer is adhered to the lower end of the adhesive layer.

[0007] Furthermore, the flame retardant layer 1 and the flame retardant layer 2 are both woven from flame retardant glass fibers.

[0008] Furthermore, the hydrophobic layer is a fluorosilicone acrylic resin layer.

[0009] Furthermore, the toughness layer 1 and the toughness layer 2 are both made of paper reinforcing agent material.

[0010] Furthermore, the waterproof film layer 1 and the waterproof film layer 2 are both made of polyethylene material.

[0011] The utility model has the following beneficial effects:

[0012] 1. Compared with the prior art, the tough VCI paper containing a hydrophobic layer can improve the waterproof performance of the VCI paper through the mutual cooperation of the hydrophobic layer 1, the hydrophobic layer 2, the waterproof film 1 and the waterproof film layer 2. The presence of the hydrophobic layer 1 and the hydrophobic layer 2 enhances the hydrophobic performance of the VCI paper, while the waterproof film 1 and the waterproof film layer 2 can play a good moisture-proof and waterproof effect, so that external water sources are not easy to penetrate the VCI paper, thereby reducing the probability of metal products packaged by the VCI paper being affected by moisture and rust.

[0013] 2. Compared with the prior art, the tough vapor-phase rust-proof paper containing a hydrophobic layer can improve the flame retardant properties of the vapor-phase rust-proof paper through the cooperation of the flame retardant layer one and the flame retardant layer two. Once a fire occurs, the vapor-phase rust-proof paper with excellent flame retardant properties can buy more rescue time for the metal products packaged therein, thereby minimizing the damage to the metal products. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 This is a schematic diagram of the explosion structure of a tough vapor anti-rust paper containing a hydrophobic layer proposed by the utility model;

[0015] Figure 2 This is a schematic diagram of the overall structure of a tough vapor anti-rust paper containing a hydrophobic layer proposed by the utility model when viewed from above.

[0016] Legend:

[0017] 1. Neutral paper layer; 2. Vapor corrosion inhibitor 1; 3. Vapor corrosion inhibitor 2; 4. Tough layer 1; 5. Tough layer 2; 6. Flame retardant layer 1; 7. Flame retardant layer 2; 8. Waterproof film layer 1; 9. Waterproof film layer 2; 10. Hydrophobic layer 1; 11. Hydrophobic layer 2; 12. Release paper layer; 13. Adhesive layer. DETAILED DESCRIPTION

[0018] Reference Figure 1-2 The utility model provides a tough vapor anti-rust paper containing a hydrophobic layer, comprising a neutral paper layer 1, the upper and lower ends of the neutral paper layer 1 are respectively dipped with a vapor corrosion inhibitor 2 and a vapor corrosion inhibitor 3, the upper end of the vapor corrosion inhibitor 2 is sequentially bonded with a tough layer 4, a flame retardant layer 6, a waterproof film layer 8 and a hydrophobic layer 10 through an adhesive from bottom to top, and the lower end of the vapor corrosion inhibitor is sequentially bonded with a tough layer 5, a flame retardant layer 7, a waterproof film layer 9 and a hydrophobic layer 11 through an adhesive from top to bottom.

[0019] During operation, the utility model can improve the waterproof performance of the vapor anti-rust paper through the cooperation of the hydrophobic layer 10, the hydrophobic layer 2 11, the waterproof film 1 and the waterproof film layer 2 9, and can improve the flame retardant performance of the vapor anti-rust paper through the cooperation of the flame retardant layer 1 6 and the flame retardant layer 2 7. In this way, whether it is a fire or rain, more rescue time can be gained for the metal products packaged by the vapor anti-rust paper, thereby minimizing the damage to the metal products.

[0020] Furthermore, an adhesive layer 13 is adhered to the lower end of the second hydrophobic layer 11 , and a release paper layer 12 is adhered to the lower end of the adhesive layer 13 .

[0021] During operation, the release paper can protect the adhesive layer 13. When the vapor-phase anti-rust paper is used to package metal products, the release paper layer 12 can be torn off and the adhesive layer 13 can be adhered to the appropriate position of the vapor-phase anti-rust paper, so that the vapor-phase anti-rust paper can wrap the metal product more tightly.

[0022] Furthermore, the flame retardant layer 1 6 and the flame retardant layer 2 7 are both woven from flame retardant glass fibers.

[0023] During operation, the flame retardant layer 1 6 and the flame retardant layer 2 7 cooperate with each other to improve the flame retardant properties of the vapor-phase anti-rust paper. Once a fire occurs, the vapor-phase anti-rust paper with excellent flame retardant properties can buy more rescue time for the metal products packaged therein, thereby minimizing the damage to the metal products.

[0024] Furthermore, the water-repellent layer is a fluorosilicone acrylic resin layer.

[0025] When working, the fluorosilicone acrylic resin in the hydrophobic layer can optimize the hydrophobic function, thereby greatly reducing the probability of damage to the vapor phase anti-rust paper body.

[0026] Furthermore, the toughness layer 1 4 and the toughness layer 2 5 are both made of paper reinforcing agent material.

[0027] When working, the paper reinforcing agent can improve the moisture resistance, toughness and overall strength of the VCI paper to prevent the wrapped metal products from damaging the VCI paper during transportation.

[0028] Furthermore, the waterproof film layer 1 and the waterproof film layer 2 9 are both made of polyethylene material.

[0029] During operation, the waterproof film layer 1 and the waterproof film layer 2 9 made of polyethylene material can make the vapor phase anti-rust paper have excellent waterproof, moisture-proof and durable functions.

[0030] Working principle:

[0031] When in use, the vapor anti-rust paper composed of neutral paper, vapor corrosion inhibitor 1 2, vapor corrosion inhibitor 2 3, tough layer 1 4, tough layer 2 5, flame retardant layer 1 6, flame retardant layer 2 7, waterproof film 1, waterproof film layer 2 9, hydrophobic layer 1 10 and hydrophobic layer 2 11 can be used to wrap metal products, and the presence of vapor corrosion inhibitor 1 2 and vapor corrosion inhibitor 2 3 here can reduce the probability of corrosion of the vapor anti-rust paper, thereby making the vapor anti-rust paper more durable, and through the mutual cooperation of hydrophobic layer 10, hydrophobic layer 2 11, waterproof film 1 and waterproof film layer 2 9, the waterproof performance of the vapor anti-rust paper can be improved, and through the mutual cooperation of flame retardant layer 1 6 and flame retardant layer 2 7, the flame retardant performance of the vapor anti-rust paper can be improved, so that whether it is a fire or rain, more rescue time can be gained for the metal products packaged by the vapor anti-rust paper, thereby minimizing the damage to the metal products.

[0032] Finally, it should be noted that the above are only preferred embodiments of the present invention and are not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A tough vapor-phase rust-proof paper containing a hydrophobic layer, comprising a neutral paper layer (1), characterized in that: The upper and lower ends of the neutral paper layer (1) are respectively dip-coated with a gas phase corrosion inhibitor 1 (2) and a gas phase corrosion inhibitor 2 (3); the upper end of the gas phase corrosion inhibitor 1 (2) is sequentially bonded with a tough layer 1 (4), a flame retardant layer 1 (6), a waterproof film layer 1 (8) and a hydrophobic layer 1 (10) via an adhesive from bottom to top; the lower end of the gas phase corrosion inhibitor is sequentially bonded with a tough layer 2 (5), a flame retardant layer 2 (7), a waterproof film layer 2 (9) and a hydrophobic layer 2 (11) via an adhesive from top to bottom.

2. The tough VCI paper with a hydrophobic layer according to claim 1, characterized in that: The lower end of the second hydrophobic layer (11) is adhered to an adhesive layer (13), and the lower end of the adhesive layer (13) is adhered to a release paper layer (12).

3. The tough VCI paper with a hydrophobic layer according to claim 1, characterized in that: The flame retardant layer 1 (6) and the flame retardant layer 2 (7) are both woven from flame retardant glass fibers.

4. The tough VCI paper with a hydrophobic layer according to claim 1, characterized in that: The hydrophobic layer is a fluorosilicone acrylic resin layer.

5. The tough VCI paper with a hydrophobic layer according to claim 1, characterized in that: The toughness layer 1 (4) and the toughness layer 2 (5) are both made of paper reinforcing agent material.

6. The tough VCI paper with a hydrophobic layer according to claim 1, characterized in that: The waterproof film layer 1 and the waterproof film layer 2 (9) are both made of polyethylene material.