Continuous annealing device for multi-unit copper wire
Through multi-unit electromagnetic induction annealing device and nitrogen protection, the problems of ignition, guide wheel wear, high power consumption and oxidation of copper wire continuous annealing device are solved, and low resistance, high efficiency annealing and adaptability of different specifications are achieved.
Patent Information
- Application Number
- CN202420739811.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-11
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2034-04-11
AI Technical Summary
The existing copper wire continuous annealing device has problems such as ignition, large wear of the guide wheel, high power consumption, easy oxidation and inability to adapt to copper wires of different specifications.
The multi-unit electromagnetic induction annealing device is adopted, through the induction annealing mechanism and the nitrogen supply mechanism, combined with the steering wheel box and the swing wheel box, the annealing of copper wires of different specifications is realized, and the electromagnetic induction coil assembly and sealing and supporting assembly are sealed and protected. Avoid oxidation.
It reduces transmission line resistance, reduces annealing power and speed, prevents oxidation, and achieves wide adaptability and high-quality annealing of copper wires of different specifications.
Smart Images

Figure CN222043306U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of copper wire processing equipment for electric wires, in particular to a continuous annealing device for multi-unit copper wires. Background Art
[0002] After cold drawing, the copper conductors of wires and cables are hardened, the tensile strength and yield strength are significantly increased, the plasticity and toughness are generally reduced, and the change in elongation is particularly significant. In order to eliminate the cold drawing hardening phenomenon and increase the elongation, annealing treatment must be carried out to eliminate internal stress and defects.
[0003] The existing continuous annealing devices for copper wire generally use contact-type high-current annealing furnaces. During the production process, sparks will occur between the electrode wheel and the copper wire, affecting the surface quality of the wire. Since the current is transmitted by brushes, the resistance of the electrode wheel is large, and the annealing copper wire will be thinned, so the guide wheel wears a lot and the equipment consumes a lot of power. The annealing chamber is steam-sealed, which is very prone to oxidation. In addition, it cannot adapt to the problem of switching between large, medium and small copper wires of different specifications in the same equipment.
[0004] Therefore, in order to solve the above problems, a continuous annealing device for multi-unit copper wire is proposed. Utility Model Content
[0005] In order to make up for the shortcomings of the existing technology, the present invention solves the problem that the existing copper wire continuous annealing device generally adopts a contact type high current annealing furnace. During the production process, sparks will occur between the electrode wheel and the copper wire, affecting the surface quality of the wire. Since the current is transmitted by the brush, the resistance of the electrode wheel is large, and the annealing copper wire will be thinned, so the guide wheel wears a lot, the equipment power consumption is large, the annealing chamber is steam sealed, oxidation is very likely to occur, and it cannot adapt to the problem of switching between large, medium and small copper wires of different specifications in the same equipment.
[0006] The technical solution adopted by the utility model to solve the technical problem is as follows: a multi-unit copper wire continuous annealing device described in the utility model comprises a steering wheel box body, an induction annealing mechanism is installed on the side of the steering wheel box body, and a swing wheel box body is installed on the other side of the induction annealing mechanism, and a nitrogen supply mechanism is arranged on the outer wall of the swing wheel box body, the steering wheel box body comprises a first stainless steel box body, a wire inlet is arranged on one side of the first stainless steel box body, and three wire inlets are arranged, and a wire outlet is arranged on the other side of the first stainless steel box body;
[0007] The induction annealing mechanism comprises an annealing box, an electromagnetic induction coil assembly, a sealing support assembly, an intermediate support assembly, a sealing water tank, and an air cooling tank;
[0008] The swing wheel housing comprises a second stainless steel housing, a swing wheel body is installed inside the second stainless steel housing, and a swing wheel upper groove is formed on the top of the swing wheel body;
[0009] The nitrogen supply mechanism includes a nitrogen source, a first gas storage tank, a second gas storage tank, a delivery pump, a one-way valve, a two-way solenoid valve, a throttle valve, a three-way solenoid valve, and a pipeline. The two-way solenoid valve, the throttle valve, and the three-way solenoid valve are all provided in plurality.
[0010] Preferably, the first stainless steel box is internally rotatably connected to a copper wire winding steering wheel, and the copper wire winding steering wheel is inclined, and the outer wall of the copper wire winding steering wheel is wrapped with a copper wire body, a steering wheel upper groove is provided on the top of the copper wire winding steering wheel, and the steering wheel upper groove and the wire outlet are located in the same plane, an inlet pipe is provided inside the first stainless steel box, and the inlet pipe is provided in three groups with different specifications, and an inlet sealing assembly is installed inside the inlet pipe.
[0011] Preferably, the inlet sealing assembly includes a fixing seat, which is fixedly connected to the top side of the first stainless steel box body close to the outlet, and the end of the fixing seat is threadedly connected with a connecting sleeve, the other end of the connecting sleeve is connected with an air intake ring, and the other end of the air intake ring is connected with a blowing core, and a sealing gasket is provided on the inner wall of the blowing core, and a circular sealing cover is provided on the side of the sealing gasket, the end of the inlet pipe is fixedly connected to the wire passing pipe, and the outer wall of the wire passing pipe is fixedly connected with the first fixing block.
[0012] Preferably, the electromagnetic induction coil assembly includes a central tube and a copper wire coil, the electromagnetic induction coil assembly and the sealing support assembly are each provided with three groups and have different specifications, and the electromagnetic induction coil assembly is installed on the top of the annealing box, an air inlet is provided inside the sealing support assembly, and a temperature measuring probe is provided on the top of the sealing support assembly.
[0013] Preferably, the sealing support assembly includes a sealing seat, a sealing box, a sealing nut, a square sealing cover, an air inlet hood, a copper wire roller, a roller frame, a temperature measuring probe and a second fixed block. The sealing support assembly is arranged at the inlet end of the electromagnetic induction coil assembly. The sealing support assembly is made of high temperature resistant and wear-resistant materials. The bottom of the sealing box is provided with an air inlet and an exhaust port in sequence. The top of the sealing box is provided with a square sealing cover, and the outside of the square sealing cover is fixedly connected with a temperature measuring probe. The air inlet hood is arranged at the outlet end of the sealing box, and two sealing nuts are provided.
[0014] Preferably, the intermediate support assembly is arranged inside the electromagnetic induction coil assembly, a sealed water tank is arranged at the bottom of the annealing box, a porous nozzle is arranged inside the sealed water tank, a temperature sensor is installed on the top of the porous nozzle, and a main interface is arranged at the bottom of the porous nozzle, the porous nozzle is externally connected to cooling water and cooling air, the air cooling tank is arranged at the top of the annealing box, and the air cooling tank includes an air tank, the air tank and the upper tank of the steering wheel are located in the same plane, and a small blowing hole is arranged outside the air tank.
[0015] Preferably, a temperature sensor is provided inside the sealed water tank, the air cooling tank is connected to a compressed air source, flanges with holes are provided on both sides of the annealing box, a sealing support assembly is provided at the line inlet end of the swing wheel box, and the swing wheel body is hinged inside the second stainless steel box.
[0016] Preferably, one side of the nitrogen source is connected to a first gas tank, and the other end of the nitrogen source is connected to a second gas tank, a delivery pump is installed on the top of the second gas tank, and a one-way valve is installed on the top of the delivery pump, a side of the first gas tank is connected to a two-way solenoid valve, and a throttle valve is installed at the bottom of the two-way solenoid valve, a side of the second gas tank is connected to a three-way solenoid valve, and the end of the second gas tank is connected to a pipeline.
[0017] The utility model is beneficial in that:
[0018] 1. The multi-unit copper wire continuous annealing device adopts a multi-unit electromagnetic induction annealing method, which does not require brushes to transmit current, so the transmission line resistance is small and the annealed copper wire is not easy to be drawn thin; at the same time, it has the characteristics of low annealing power and fast annealing speed;
[0019] 2. The multi-unit copper wire continuous annealing device is connected to the nitrogen supply mechanism through the air inlet of the rotary box and the internal sealing support assembly of the annealing box, which can effectively prevent the annealing copper wire from being oxidized by air at high temperature;
[0020] 3. The multi-unit copper wire continuous annealing device realizes the annealing production of copper wires with different wire diameters through three different specifications of inlet pipes and three different specifications of sealing components set in the steering wheel box, three different specifications of large, medium and small electromagnetic induction coils and three groups of sealing support components with different specifications set in the induction annealing mechanism, with a wide production range and the function of one machine with multiple uses. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0022] Figure 1 It is a schematic diagram of the structure of the utility model;
[0023] Figure 2 This is a side view of the steering wheel box of the utility model;
[0024] Figure 3 This is a schematic diagram of the structure of the inlet pipe sealing assembly of the utility model;
[0025] Figure 4 This is a schematic diagram of the structure of the induction annealing mechanism of the utility model;
[0026] Figure 5 It is a side view of the induction annealing mechanism of the utility model;
[0027] Figure 6 This is a schematic diagram of the structure of the sealing support assembly of the utility model;
[0028] Figure 7 It is a side view of the swing wheel box of the utility model.
[0029] In the figure: 1, steering wheel housing; 2, induction annealing mechanism; 3, swing wheel housing; 4, nitrogen supply mechanism; 5, copper wire body; 11, first stainless steel housing; 12, wire inlet; 13, wire outlet; 14, copper wire rotating steering wheel; 15, steering wheel upper groove; 16, wire inlet pipe; 17, wire inlet sealing assembly; 171, fixed seat; 172, connecting sleeve; 173, air inlet ring; 174, air blowing core; 175, sealing pad; 176, circular sealing cover; 177, wire passing pipe; 178, first fixed block; 21, annealing housing; 22, electromagnetic induction coil assembly; 221, center tube; 222, copper wire coil; 23, sealing support assembly; 230, sealing seat; 231, sealing box; 232, Sealing nut; 233, square sealing cover; 234, air inlet hood; 235, copper wire support wheel; 236, support wheel frame; 237, temperature probe; 238, second fixed block; 239, air inlet; 240, exhaust port; 24, intermediate support assembly; 25, sealed water tank; 251, multi-hole nozzle; 252, temperature sensor; 253, main interface; 26, air cooling tank; 261, air tank; 27, flange with holes; 31, second stainless steel box; 32, swing wheel body; 33, swing wheel upper groove; 41, nitrogen source; 42, first gas tank; 43, second gas tank; 44, delivery pump; 45, one-way valve; 46, two-way solenoid valve; 47, throttle valve; 48, three-way solenoid valve; 49, pipeline. DETAILED DESCRIPTION
[0030] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0031] Embodiment 1
[0032] See also Figure 1As shown, a continuous annealing device for multi-unit copper wire includes a steering wheel box 1, an induction annealing mechanism 2 is installed on the side of the steering wheel box 1, and a swing wheel box 3 is installed on the other side of the induction annealing mechanism 2, and a nitrogen supply mechanism 4 is arranged on the outer wall of the swing wheel box 3, the steering wheel box 1 includes a first stainless steel box 11, one side of the first stainless steel box 11 is provided with a wire inlet 12, and the wire inlet 12 is provided with three, and the other side of the first stainless steel box 11 is provided with a wire outlet 13, the induction annealing mechanism 2 includes an annealing box 21, an electromagnetic induction coil assembly 22, A sealing support assembly 23, an intermediate support assembly 24, a sealing water tank 25, and an air cooling tank 26. The swing wheel box 3 includes a second stainless steel box 31. A swing wheel body 32 is installed inside the second stainless steel box 31, and a swing wheel upper groove 33 is opened on the top of the swing wheel body 32. The nitrogen supply mechanism 4 includes a nitrogen source 41, a first gas storage tank 42, a second gas storage tank 43, a delivery pump 44, a one-way valve 45, a two-way solenoid valve 46, a throttle valve 47, a three-way solenoid valve 48, and a pipeline 49. A plurality of two-way solenoid valves 46, throttle valves 47 and three-way solenoid valves 48 are provided.
[0033] See also Figure 1 As shown, a continuous annealing device for multi-unit copper wire is provided, wherein a copper wire winding steering wheel 14 is rotatably connected inside a first stainless steel box body 11, and the copper wire winding steering wheel 14 is inclined, and a copper wire body 5 is wound around the outer wall of the copper wire winding steering wheel 14, and a steering wheel upper groove 15 is provided on the top of the copper wire winding steering wheel 14, and the steering wheel upper groove 15 and the wire outlet 13 are located in the same plane, an inlet pipe 16 is provided inside the first stainless steel box body 11, and the inlet pipe 16 is provided in three groups with different specifications, and an inlet sealing assembly 17 is installed inside the inlet pipe 16.
[0034] See also Figure 3 As shown, a continuous annealing device for multi-unit copper wires, the inlet sealing assembly 17 includes a fixed seat 171, the fixed seat 171 is fixedly connected to the top of the first stainless steel box 11 near the side of the outlet 13, and the end of the fixed seat 171 is threadedly connected with a connecting sleeve 172, the other end of the connecting sleeve 172 is connected to an air intake ring 173, and the other end of the air intake ring 173 is connected to a blowing core 174, and a sealing gasket 175 is provided on the inner wall of the blowing core 174, and a circular sealing cover 176 is provided on the side of the sealing gasket 175, the end of the inlet pipe 16 is fixedly connected to a wire passing pipe 177, and the outer wall of the wire passing pipe 177 is fixedly connected to a first fixed block 178.
[0035] See also Figure 4As shown, a continuous annealing device for multi-unit copper wire, the electromagnetic induction coil assembly 22 includes a central tube 221 and a copper wire coil 222, the electromagnetic induction coil assembly 22 and the sealing support assembly 23 are provided in three groups with different specifications, and the electromagnetic induction coil assembly 22 is installed on the top of the annealing box 21, the sealing support assembly 23 is provided with an air inlet 239, and the top of the sealing support assembly 23 is provided with a temperature measuring probe 237.
[0036] See also Figure 6 As shown, a continuous annealing device for multi-unit copper wire is provided, wherein a sealing support assembly 23 comprises a sealing seat 230, a sealing box 231, a sealing nut 232, a square sealing cover 233, an air inlet hood 234, a copper wire supporting roller 235, a supporting roller frame 236, a temperature measuring probe 237 and a second fixed block 238, and the sealing support assembly 23 is arranged at the inlet end of the electromagnetic induction coil assembly 22, and the sealing support assembly 23 is made of high temperature resistant and wear-resistant materials, an air inlet port 239 and an exhaust port 240 are sequentially arranged at the bottom of the sealing box 231, a square sealing cover 233 is arranged at the top of the sealing box 231, and a temperature measuring probe 237 is fixedly connected to the outside of the square sealing cover 233, an air inlet hood 234 is arranged at the outlet end of the sealing box 231, and two sealing nuts 232 are provided.
[0037] See also Figure 4 and Figure 5 As shown, a continuous annealing device for multi-unit copper wire is provided, wherein the intermediate support assembly 24 is arranged inside the electromagnetic induction coil assembly 22, a sealed water tank 25 is arranged at the bottom of the annealing box 21, a porous nozzle 251 is arranged inside the sealed water tank 25, a temperature sensor 252 is installed on the top of the porous nozzle 251, and a main interface 253 is arranged at the bottom of the porous nozzle 251, the porous nozzle 251 is externally connected to cooling water and cooling air, an air cooling groove 26 is arranged at the top of the annealing box 21, and the air cooling groove 26 includes an air groove 261, the air groove 261 and the upper groove 15 of the steering wheel are located in the same plane, and a small blowing hole is arranged outside the air groove 261.
[0038] See also Figure 4 , Figure 5 and Figure 7 As shown, a continuous annealing device for multi-unit copper wire is provided, a temperature sensor 252 is arranged inside the sealed water tank 25, an air cooling tank 26 is externally connected to a compressed air source, flanges 27 with holes are provided on both sides of the annealing box 21, a sealing support assembly 23 is arranged at the wire inlet end of the swing wheel box 3, and the swing wheel body 32 is hinged inside the second stainless steel box 31.
[0039] See also Figure 1As shown, a continuous annealing device for a multi-unit copper wire is provided, wherein one side of a nitrogen source 41 is connected to a first gas tank 42, and the other end of the nitrogen source 41 is connected to a second gas tank 43, a delivery pump 44 is installed on the top of the second gas tank 43, and a one-way valve 45 is installed on the top of the delivery pump 44, a two-way solenoid valve 46 is connected to the side of the first gas tank 42, and a throttle valve 47 is installed at the bottom of the two-way solenoid valve 46, a three-way solenoid valve 48 is connected to the side of the second gas tank 43, and a pipeline 49 is connected to the end of the second gas tank 43.
[0040] Working principle: When the copper wire body 5 is introduced from any inlet 12 of the steering wheel housing 1 during annealing operation, the copper wire body 5 first passes through the corresponding inlet pipe 16, passes through the wire pipe 177 of the inlet sealing assembly 17, and then passes through the corresponding central pipes 221 of the three sets of electromagnetic induction annealing mechanisms 2 in sequence, enters the swing wheel upper groove 33 in the swing wheel housing 3, bypasses 180 degrees and enters the sealed water tank 25, and then is led out from the sealed water tank 25 and returns to the steering wheel housing 1 again, bypasses 180 degrees along the copper wire around the steering wheel 14, and then is led out from the steering wheel upper groove 15, enters the air cooling tank 26 through the outlet 13, and completes the annealing operation after being cooled by air, and enters the next production process;
[0041] Since the steering wheel housing 1, the induction annealing mechanism 2 and the swing wheel housing 3 are respectively provided with three different specifications of the inlet pipe 16, the center pipe 221, the wire passing pipe 177 and the electromagnetic induction coil assembly 22, they can adapt to the annealing operation production of copper wires of various specifications.
[0042] Since the copper wire does not pass through the guide wheel for winding and steering in the annealing preheating section, the heat preservation section and the slow cooling section, the copper wire is not easy to be stretched and deformed. Electromagnetic induction heating is adopted, and the heat source is generated in the copper wire, the heating efficiency is high, and the energy loss is small. Different sealing components are arranged in the steering wheel box 1, the electromagnetic induction annealing mechanism 2 and the swing wheel box 3, and nitrogen can be filled for protection, so that the copper wire is not easy to be oxidized during the annealing process, and high-quality production is guaranteed. In the latter section of the annealing operation, multiple sections of sealed water tanks 25 and multiple sections of air cooling tanks 26 are arranged, which can ensure the rapid cooling of the copper wire and are conducive to further improving the production speed.
[0043] The above shows and describes the basic principle, main features and advantages of the utility model. Those skilled in the art should understand that the utility model is not limited by the above embodiments, and the above embodiments and descriptions are only for explaining the principle of the utility model. Without departing from the spirit and scope of the utility model, the utility model may have various changes and improvements, and these changes and improvements fall within the scope of the utility model to be protected.
Claims
1. A continuous annealing device for multi-unit copper wire, characterized in that: The invention comprises a steering wheel housing (1), an induction annealing mechanism (2) is installed on the side of the steering wheel housing (1), and an oscillating wheel housing (3) is installed on the other side of the induction annealing mechanism (2), and a nitrogen supply mechanism (4) is arranged on the outer wall of the oscillating wheel housing (3), the steering wheel housing (1) comprises a first stainless steel housing (11), one side of the first stainless steel housing (11) is provided with a wire inlet (12), and three wire inlets (12) are arranged, and the other side of the first stainless steel housing (11) is provided with a wire outlet (13); The induction annealing mechanism (2) comprises an annealing box (21), an electromagnetic induction coil assembly (22), a sealing support assembly (23), an intermediate support assembly (24), a sealing water tank (25), and an air cooling tank (26); The swing wheel housing (3) comprises a second stainless steel housing (31), a swing wheel body (32) is installed inside the second stainless steel housing (31), and a swing wheel upper groove (33) is provided on the top of the swing wheel body (32); The nitrogen supply mechanism (4) comprises a nitrogen source (41), a first gas storage tank (42), a second gas storage tank (43), a delivery pump (44), a one-way valve (45), a two-way solenoid valve (46), a throttle valve (47), a three-way solenoid valve (48), and a pipeline (49), wherein a plurality of the two-way solenoid valve (46), the throttle valve (47), and the three-way solenoid valve (48) are provided.
2. A continuous annealing device for multi-unit copper wire according to claim 1, characterized in that: The first stainless steel box (11) is rotatably connected to a copper wire revolving steering wheel (14), and the copper wire revolving steering wheel (14) is arranged obliquely, and the outer wall of the copper wire revolving steering wheel (14) is wound with a copper wire body (5), and the top of the copper wire revolving steering wheel (14) is provided with a steering wheel upper groove (15), and the steering wheel upper groove (15) and the outlet (13) are located in the same plane, and the first stainless steel box (11) is provided with an inlet pipe (16), and the inlet pipe (16) is provided in three groups with different specifications, and an inlet sealing assembly (17) is installed inside the inlet pipe (16).
3. A continuous annealing device for multi-unit copper wire according to claim 2, characterized in that: The inlet sealing assembly (17) comprises a fixing seat (171), the fixing seat (171) is fixedly connected to the top of the first stainless steel box (11) on one side close to the outlet (13), and the end of the fixing seat (171) is threadedly connected to a connecting sleeve (172), the other end of the connecting sleeve (172) is connected to an air intake ring (173), and the other end of the air intake ring (173) is connected to a blowing core (174), and a sealing gasket (175) is provided on the inner wall of the blowing core (174), and a circular sealing cover (176) is provided on the side of the sealing gasket (175), and the end of the inlet pipe (16) is fixedly connected to a wire passing pipe (177), and the outer wall of the wire passing pipe (177) is fixedly connected to a first fixing block (178).
4. A continuous annealing device for a multi-unit copper wire according to claim 1, characterized in that: The electromagnetic induction coil assembly (22) comprises a central tube (221) and a copper wire coil (222); the electromagnetic induction coil assembly (22) and the sealing support assembly (23) are both provided in three groups and have different specifications; the electromagnetic induction coil assembly (22) is installed on the top of the annealing box (21); an air inlet (239) is provided inside the sealing support assembly (23); and a temperature measuring probe (237) is provided on the top of the sealing support assembly (23).
5. The continuous annealing device for multi-unit copper wire according to claim 1, characterized in that: The sealing support assembly (23) comprises a sealing seat (230), a sealing box (231), a sealing nut (232), a square sealing cover (233), an air inlet cover (234), a copper wire support wheel (235), a support wheel frame (236), a temperature measuring probe (237) and a second fixed block (238); the sealing support assembly (23) is arranged at the inlet end of the electromagnetic induction coil assembly (22); the sealing support assembly (23) is made of high temperature resistant and wear resistant material; an air inlet (239) and an air outlet (240) are arranged at the bottom of the sealing box (231) in sequence; a square sealing cover (233) is arranged at the top of the sealing box (231); and the outside of the square sealing cover (233) is fixedly connected to the temperature measuring probe (237); the air inlet cover (234) is arranged at the outlet end of the sealing box (231); and two sealing nuts (232) are arranged.
6. A continuous annealing device for a multi-unit copper wire according to claim 1, characterized in that: The intermediate support component (24) is arranged inside the electromagnetic induction coil component (22); a sealed water tank (25) is arranged at the bottom of the annealing box (21); a multi-hole nozzle (251) is arranged inside the sealed water tank (25); a temperature sensor (252) is installed on the top of the multi-hole nozzle (251); a main interface (253) is arranged at the bottom of the multi-hole nozzle (251); the multi-hole nozzle (251) is externally connected to cooling water and cooling air; the air cooling groove (26) is arranged at the top of the annealing box (21); the air cooling groove (26) comprises an air groove (261); the air groove (261) and the upper groove (15) of the steering wheel are located in the same plane; and a small blowing hole is arranged outside the air groove (261).
7. A continuous annealing device for multi-unit copper wire according to claim 1, characterized in that: A temperature sensor (252) is arranged inside the sealed water tank (25), the air cooling tank (26) is externally connected to a compressed air source, flanges (27) with holes are provided on both sides of the annealing box (21), a sealing support assembly (23) is arranged at the line inlet end of the swing wheel box (3), and the swing wheel body (32) is hinged inside the second stainless steel box (31).
8. The continuous annealing device for multi-unit copper wire according to claim 1, characterized in that: One side of the nitrogen source (41) is connected to a first gas storage tank (42), and the other end of the nitrogen source (41) is connected to a second gas storage tank (43); a delivery pump (44) is installed on the top of the second gas storage tank (43), and a one-way valve (45) is installed on the top of the delivery pump (44); a side of the first gas storage tank (42) is connected to a two-way solenoid valve (46), and a throttle valve (47) is installed at the bottom of the two-way solenoid valve (46); a side of the second gas storage tank (43) is connected to a three-way solenoid valve (48), and an end of the second gas storage tank (43) is connected to a pipeline (49).