Double-sided multi-layer lead-free tin spraying plate

By designing electromagnetic shielding layer, insulation protection layer, corrosion-resistant layer and heat dissipation layer in lead-free tin spray plate, the electromagnetic interference and corrosion problems of lead-free tin spray plate in complex environments is solved, and the durability of the circuit board is improved. Stability extends service life.

CN222053444UActive Publication Date: 2024-11-22HUAIAN KAIMEI ELECTRONIC TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420306940.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-20
Publication Date
2024-11-22
Estimated Expiration
2034-02-20

AI Technical Summary

Technical Problem

The existing lead-free tin spray plates are susceptible to interference and corrosion in complex electromagnetic environments and harsh environments, and cannot effectively prevent electromagnetic interference and signal leakage, resulting in the impact of the performance and stability of electronic equipment, and are susceptible to corrosive media such as acid and alkali. erosion shortens service life.

Method used

A double-sided multi-layer lead-free tin spray plate is designed, including electromagnetic shielding layer, insulation protection layer, corrosion-resistant layer, and heat dissipation layer. The combination of these layers improves the conductivity and corrosion resistance, enhances the electromagnetic shielding performance, and prevents electromagnetic Interference and signal leakage, and improve heat dissipation performance and extend service life.

Benefits of technology

Effectively improve the electromagnetic shielding performance, corrosion resistance and heat dissipation performance of lead-free tin spray plate, extend the service life, enhance the anti-interference ability and durability of the circuit board, prevent oxidation and corrosion, and ensure the stability of the circuit board and reliability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222053444U_ABST
    Figure CN222053444U_ABST
Patent Text Reader

Abstract

The utility model discloses a double-sided multi-layer lead-free tin spraying plate which comprises a lead-free tin spraying plate main body, the top of the lead-free tin spraying plate main body is fixedly connected with a top end layer, the bottom of the lead-free tin spraying plate main body is fixedly connected with a bottom end layer, and the two sides of the lead-free tin spraying plate main body are fixedly connected with metal protection plates. The interior of the top end layer comprises a first electromagnetic shielding layer, and the top of the first electromagnetic shielding layer is fixedly connected with an insulating protection layer. According to the double-sided multi-layer lead-free tin spraying plate, through the design of the first electromagnetic shielding layer, the insulation protection layer, the first corrosion-resistant layer, the second electromagnetic shielding layer, the heat dissipation layer and the second corrosion-resistant layer, the conductivity and corrosion resistance of the lead-free tin spraying plate can be effectively improved, and then the service life of the lead-free tin spraying plate is prolonged; the electromagnetic shielding performance of the lead-free tin-sprayed plate can be effectively enhanced, electromagnetic interference and signal leakage can be effectively prevented, and the anti-interference capability of the circuit board is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of lead-free tin-spraying plates, in particular to a double-sided multi-layer lead-free tin-spraying plate. Background Art

[0002] Lead-free tin-spraying board refers to a circuit board with a layer of tin film on the surface of the metal plate substrate treated by lead-free tin-spraying process in the production process of electronic circuit boards. This treatment method can prevent oxidation, corrosion and degradation of welding performance of the copper surface, and at the same time, it can also isolate the metal from the air and protect the substrate from being corroded by oxides in the environment.

[0003] Existing lead-free tin-sprayed boards are easily interfered with and corroded in complex electromagnetic environments and harsh environments, which affects their service life. Lead-free tin-sprayed boards cannot effectively prevent electromagnetic interference and signal leakage, which may have an adverse effect on the performance and stability of electronic equipment. At the same time, lead-free tin-sprayed boards are easily corroded by corrosive media such as acids and alkalis, resulting in oxidation, corrosion and other problems on the surface of the circuit board, thereby shortening its service life. Utility Model Content

[0004] The purpose of the utility model is to provide a double-sided multi-layer lead-free tin-spraying board to solve the problem mentioned in the above background technology that the existing lead-free tin-spraying board is easily interfered and corroded in complex electromagnetic environments and harsh environments, thereby affecting its service life. The lead-free tin-spraying board cannot effectively prevent electromagnetic interference and signal leakage, which may have an adverse effect on the performance and stability of electronic equipment. At the same time, the lead-free tin-spraying board is easily corroded by corrosive media such as acids and alkalis, resulting in oxidation, corrosion and other problems on the surface of the circuit board, thereby shortening its service life.

[0005] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a double-sided multi-layer lead-free tin-sprayed board, comprising a lead-free tin-sprayed board main body, the top of the lead-free tin-sprayed board main body is fixedly connected with a top layer, the bottom of the lead-free tin-sprayed board main body is fixedly connected with a bottom layer, both sides of the lead-free tin-sprayed board main body are fixedly connected with metal protective plates, the interior of the top layer includes an electromagnetic shielding layer 1, the top of the electromagnetic shielding layer 1 is fixedly connected with an insulating protective layer, the top of the insulating protective layer is fixedly connected with a corrosion-resistant layer 1, the interior of the bottom layer includes an electromagnetic shielding layer 2, the bottom of the electromagnetic shielding layer 2 is fixedly connected with a heat dissipation layer, and the bottom of the heat dissipation layer is fixedly connected with the corrosion-resistant layer 2.

[0006] Compared with the prior art, the beneficial effects of the utility model are:

[0007] The double-sided multi-layer lead-free tin-spraying board can effectively improve the conductivity and corrosion resistance of the lead-free tin-spraying board through the design of the electromagnetic shielding layer one, the insulating protection layer, the corrosion-resistant layer one, the electromagnetic shielding layer two, the heat dissipation layer and the corrosion-resistant layer two, thereby improving the service life of the lead-free tin-spraying board. The design of the electromagnetic shielding layer one and the electromagnetic shielding layer two can effectively enhance the electromagnetic shielding performance of the lead-free tin-spraying board, can effectively prevent electromagnetic interference and signal leakage, and improve the anti-interference ability of the circuit board. At the same time, the electromagnetic shielding layer can also effectively reduce the possibility of oxidation and corrosion on the surface of the circuit board, and improve the durability of the circuit board. The design of the insulating protection layer can effectively protect the circuit board surface of the lead-free tin-spraying board from static electricity, electromagnetic fields, etc. Interference, ensure the normal operation of the circuit board, can effectively prevent the surface of the circuit board from being damaged and deformed, and improve the stability and reliability of the circuit board. The design of the corrosion-resistant layer one and the corrosion-resistant layer two can effectively improve the corrosion resistance of the lead-free tin-spraying board, and can effectively prevent corrosive media such as acids and alkalis from damaging the circuit board. At the same time, the corrosion-resistant layer can also effectively reduce the possibility of oxidation and corrosion on the surface of the circuit board, and improve the durability of the circuit board. The design of the heat dissipation layer can effectively improve the heat dissipation performance of the lead-free tin-spraying board, and can effectively conduct the heat inside the circuit board to prevent overheating and thermal failure. At the same time, the heat dissipation layer can also effectively reduce the possibility of oxidation and corrosion on the surface of the circuit board, and improve the durability of the circuit board. BRIEF DESCRIPTION OF THE DRAWINGS

[0008] Figure 1 It is a schematic diagram of the structure of the utility model;

[0009] Figure 2 This is a cross-sectional view of the structure of the utility model;

[0010] Figure 3 This is a structural cross-sectional view of the top layer of the utility model;

[0011] Figure 4 It is the structural section layer of the bottom layer of the utility model.

[0012] In the figure: 1. Lead-free tin-spraying board body; 2. Metal protective plate; 3. Reinforcement plate; 4. Heat-conducting plate; 5. Heat-conducting rod; 6. Metal frame; 7. Heat dissipation plate; 8. Heat dissipation strip; 9. Top layer; 10. Bottom layer; 11. Electromagnetic shielding layer one; 12. Insulation protection layer; 13. Corrosion-resistant layer one; 14. Electromagnetic shielding layer two; 15. Heat dissipation layer; 16. Corrosion-resistant layer two. DETAILED DESCRIPTION

[0013] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0014] See also Figure 1-4 The utility model provides a technical solution: a double-sided multi-layer lead-free tin-spraying board, including a lead-free tin-spraying board main body 1, a top layer 9 is fixedly connected to the top of the lead-free tin-spraying board main body 1, a bottom layer 10 is fixedly connected to the bottom of the lead-free tin-spraying board main body 1, and metal protective plates 2 are fixedly connected to both sides of the lead-free tin-spraying board main body 1. The top layer 9 includes an electromagnetic shielding layer 11 inside, an insulating protection layer 12 is fixedly connected to the top of the electromagnetic shielding layer 11, and a corrosion-resistant layer 13 is fixedly connected to the top of the insulating protection layer 12. The bottom layer 10 includes an electromagnetic shielding layer 2 14 inside, a heat dissipation layer 15 is fixedly connected to the bottom of the electromagnetic shielding layer 14, and a corrosion-resistant layer 2 16 is fixedly connected to the bottom of the heat dissipation layer 15.

[0015] Two reinforcing plates 3 are fixedly connected to opposite sides of the two metal protection plates 2 , and one side of the reinforcing plates 3 is fixedly connected to one side of the lead-free tin-spraying plate body 1 , which can improve the strength of the lead-free tin-spraying plate body 1 .

[0016] The electromagnetic shielding layer 11 and the electromagnetic shielding layer 2 14 are both made of copper material, which can enhance the electromagnetic shielding performance of the lead-free tin-spraying board and reduce electromagnetic interference and signal leakage.

[0017] The insulating protective layer 12 is made of insulating adhesive material, which can prevent the lead-free tin-spraying board from being disturbed by static electricity, electromagnetic fields, etc. during the manufacturing and use process, thereby ensuring the normal operation of the lead-free tin-spraying board.

[0018] The first corrosion-resistant layer 13 and the second corrosion-resistant layer 16 are both made of precious metal alloy materials, which can effectively improve the corrosion resistance of the lead-free tin-spraying plate.

[0019] The heat dissipation layer 15 is made of metal oxide material, which can effectively improve the heat dissipation performance of the lead-free tin-spraying board.

[0020] A heat conducting plate 4 is fixedly connected to the inside of the lead-free tin-spraying board body 1, a metal frame 6 is fixedly connected to the outside of the heat conducting plate 4, a heat conducting rod 5 is fixedly connected to the front and rear sides of the heat conducting plate 4, a side of the heat conducting rod 5 away from the heat conducting plate 4 penetrates to the outside of the lead-free tin-spraying board body 1 and is fixedly connected to a heat sink 7, a side of the heat sink 7 away from the heat conducting rod 5 is fixedly connected to a heat dissipation bar 8, which can effectively improve the heat dissipation performance of the lead-free tin-spraying board.

[0021] In summary: the double-sided multi-layer lead-free tin-spraying board can effectively improve the electrical conductivity and corrosion resistance of the lead-free tin-spraying board through the design of the electromagnetic shielding layer 11, the insulating protective layer 12, the corrosion-resistant layer 13, the electromagnetic shielding layer 2 14, the heat dissipation layer 15 and the corrosion-resistant layer 2 16, thereby improving the service life of the lead-free tin-spraying board. The design of the electromagnetic shielding layer 11 and the electromagnetic shielding layer 2 14 can effectively enhance the electromagnetic shielding performance of the lead-free tin-spraying board, can effectively prevent electromagnetic interference and signal leakage, and improve the anti-interference ability of the circuit board. At the same time, the electromagnetic shielding layer can also effectively reduce the possibility of oxidation and corrosion on the surface of the circuit board, and improve the durability of the circuit board. The design of the insulating protective layer 12 can effectively protect the surface of the circuit board of the lead-free tin-spraying board from Interference from static electricity, electromagnetic fields, etc. can ensure the normal operation of the circuit board, can effectively prevent the surface of the circuit board from being damaged and deformed, and improve the stability and reliability of the circuit board. The design of the corrosion-resistant layer 13 and the corrosion-resistant layer 2 16 can effectively improve the corrosion resistance of the lead-free tin-spraying board, and can effectively prevent corrosive media such as acids and alkalis from damaging the circuit board. At the same time, the corrosion-resistant layer can also effectively reduce the possibility of oxidation and corrosion on the surface of the circuit board, and improve the durability of the circuit board. The design of the heat dissipation layer 15 can effectively improve the heat dissipation performance of the lead-free tin-spraying board, and can effectively conduct the heat inside the circuit board to prevent overheating and thermal failure. At the same time, the heat dissipation layer 15 can also effectively reduce the possibility of oxidation and corrosion on the surface of the circuit board, and improve the durability of the circuit board.

[0022] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0023] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A double-sided multi-layer lead-free tin-spraying board, comprising a lead-free tin-spraying board body (1), characterized in that: The top of the lead-free tin-spraying board body (1) is fixedly connected to a top layer (9), the bottom of the lead-free tin-spraying board body (1) is fixedly connected to a bottom layer (10), both sides of the lead-free tin-spraying board body (1) are fixedly connected to metal protective plates (2), the top layer (9) includes an electromagnetic shielding layer (11) inside, the top of the electromagnetic shielding layer (11) is fixedly connected to an insulating protective layer (12), the top of the insulating protective layer (12) is fixedly connected to a corrosion-resistant layer (13), the bottom layer (10) includes an electromagnetic shielding layer (14) inside, the bottom of the electromagnetic shielding layer (14) is fixedly connected to a heat dissipation layer (15), and the bottom of the heat dissipation layer (15) is fixedly connected to a corrosion-resistant layer (16).

2. A double-sided multi-layer lead-free tin-spraying board according to claim 1, characterized in that: Two reinforcing plates (3) are fixedly connected to opposite sides of the two metal protection plates (2), and one side of the reinforcing plates (3) is fixedly connected to one side of the lead-free tin-spraying plate body (1).

3. A double-sided multi-layer lead-free tin-spraying board according to claim 1, characterized in that: The electromagnetic shielding layer 1 (11) and the electromagnetic shielding layer 2 (14) are both made of copper material.

4. A double-sided multi-layer lead-free tin-spraying board according to claim 1, characterized in that: The insulating protective layer (12) is made of insulating glue material.

5. The double-sided multi-layer lead-free tin-spraying board according to claim 1, characterized in that: The corrosion-resistant layer 1 (13) and the corrosion-resistant layer 2 (16) are both made of precious metal alloy materials.

6. A double-sided multi-layer lead-free tin-spraying board according to claim 1, characterized in that: The heat dissipation layer (15) is made of metal oxide material.

7. The double-sided multi-layer lead-free tin-spraying board according to claim 1, characterized in that: A heat conducting plate (4) is fixedly connected to the interior of the lead-free tin-spraying plate body (1), a metal frame (6) is fixedly connected to the exterior of the heat conducting plate (4), a heat conducting rod (5) is fixedly connected to the front and rear sides of the heat conducting plate (4), a side of the heat conducting rod (5) away from the heat conducting plate (4) penetrates to the exterior of the lead-free tin-spraying plate body (1) and is fixedly connected to a heat dissipation plate (7), and a side of the heat dissipation plate (7) away from the heat conducting rod (5) is fixedly connected to a heat dissipation bar (8).