Cold heading forming die for spline input shaft
By designing the spline input shaft cold heading forming mold, the spline and inner hole molding is achieved using hole needles and clamping components, the problem of lack of molding parts and inner hole processing of spline input shaft molds in the prior art is solved, and the need is achieved High-efficiency molding of machining and heat treatment reduces costs and labor consumption.
Patent Information
- Application Number
- CN202420694217.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-07
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2034-04-07
AI Technical Summary
The lack of molded parts of existing spline input shaft molds leads to increased machining, increasing process and cost. At the same time, the molded parts without holes require machining and heat treatment, making it difficult to improve the strength of the parts.
Design a spline input shaft cold heading mold, including lower mold, mold seat, mold groove and hole needle. The spline and inner hole molding can be achieved through the cylindrical structure of the hole needle and the clamping assembly to avoid machining and improve work Efficiency and part strength.
Cold heading of splines and inner holes is achieved, no need for machining and heat treatment, reducing costs, and improving working efficiency and part strength.
Smart Images

Figure CN222058727U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of automobile manufacturing, and particularly relates to a cold heading forming die for a spline input shaft. Background Art
[0002] The spline input shaft is a common automotive accessory, which is usually used to transfer power from one component to another. The spline shaft achieves this transmission by cooperating with the corresponding spline sleeve. The cooperation between them can be fixed or movable to meet different mechanical requirements.
[0003] The original mold has no spline forming part, and additional machining is required to process the spline, which results in additional processes and waste of costs. In addition, the mold has no inner hole forming part, and the inner hole of the part needs to be machined, and heat treatment is required to improve the strength of the part. Summary of the invention
[0004] The utility model aims to solve the above problems existing in the prior art and provides a cold heading forming die for a spline input shaft which is simple to process and low in cost.
[0005] The purpose of the utility model can be achieved through the following technical solutions: a spline input shaft cold heading forming mold, including a lower mold, a mold base is fixedly installed on the surface of the lower mold, the inner cavity of the mold base is provided with a mold groove, and the inner cavity of the mold groove is provided with a hole needle.
[0006] The cold heading forming die for the spline input shaft increases the spline forming part in the die, and the spline does not need additional machining after cold heading. The inner hole forming part is increased, and the inner hole does not need additional machining after cold heading, thereby improving work efficiency and reducing manpower consumption.
[0007] In the above-mentioned key input shaft cold heading forming die, a stopper is fixedly welded on the left side of the hole needle, and the top and bottom of the stopper are provided with a clamping groove. In actual manufacturing, the use of the stopper can facilitate the positioning and fixing of the hole needle, so that the hole needle can be conveniently fixed in the inner cavity of the die groove, and the leakage of the die material during the processing can be avoided.
[0008] In the above-mentioned key input shaft cold heading forming die, a spline groove is opened inside the die groove, and the hole needle is a cylindrical structure. In practical application, the cylindrical structure of the hole needle can form an internal control after the spline input shaft is formed, without the need for machining, thus saving working time.
[0009] In the above-mentioned key input shaft cold heading forming die, the top and bottom of the left side of the lower die are fixedly installed with a clamping assembly, and the clamping assembly includes a fixing shell. In actual application, the end of the clamping rod away from the spring extends to the inner cavity of the clamping slot. Through the use of the clamping rod and the clamping slot, the stopper can be fixed on the surface of the lower die, so that the hole needle can be stably installed.
[0010] Compared with the prior art, the cold heading forming die for the spline input shaft adds a spline forming part in the die, and the spline does not need additional machining after cold heading. An inner hole forming part is added, and after cold heading, the inner hole does not need additional machining. After the inner hole is formed, the overall strength of the part is improved, and there is no need to add heat treatment process, thereby reducing costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] Figure 1 It is a schematic diagram of the structure of the cold heading forming die for the spline input shaft.
[0012] Figure 2 This is a schematic diagram of the decomposition structure of the cold heading forming die for the spline input shaft.
[0013] Figure 3 It is a schematic diagram of the structure of the spline input shaft cold heading forming die clamping assembly.
[0014] In the figure, 1, lower mold; 2, mold base; 3, mold groove; 4, hole needle; 5, clamping assembly; 51, fixed shell; 52, spring; 53, clamping rod; 6, stop block; 7, clamping groove. DETAILED DESCRIPTION
[0015] The following are specific embodiments of the present invention and the accompanying drawings to further describe the technical solution of the present invention, but the present invention is not limited to these embodiments.
[0016] like Figure 1 , Figure 2 and Figure 3 As shown, the cold heading forming die for the spline input shaft comprises a lower die 1 , a die base 2 is fixedly mounted on the surface of the lower die 1 , a die groove 3 is formed in the inner cavity of the die base 2 , and a hole needle 4 is arranged in the inner cavity of the die groove 3 .
[0017] During actual manufacturing, a stopper 6 is fixedly welded on the left side of the hole needle 4. By using the stopper 6, the hole needle 4 can be conveniently limited and fixed, so that the hole needle 4 can be conveniently fixed in the inner cavity of the mold groove 3, and at the same time, leakage of mold material during processing can be avoided. The top and bottom of the stopper 6 are provided with snap-in grooves 7.
[0018] In actual manufacturing, a spline groove is provided inside the mold groove 3, and the hole needle 4 is a cylindrical structure. A clamping assembly 5 is fixedly installed on the top and bottom of the left side of the lower mold 1, and the clamping assembly 5 includes a fixing shell 51.
[0019] The fixed shell 51 is fixedly welded to the left side of the lower mold 1 , the inner cavity of the fixed shell 51 is fixedly connected with a spring 52 , and the other side of the spring 52 is fixedly connected with a clamping rod 53 .
[0020] During actual manufacturing, the hole needle 4 is placed in the inner cavity of the mold groove 3, the clamping rod 53 is pulled to compress the spring 52, and then the right side of the block 6 is contacted with the left side of the lower mold 1. At this time, the clamping rod 53 is released, and the clamping rod 53 is driven to be clamped into the clamping groove 7 under the reset action of the spring 52 to fix the hole needle 4. Then the mold material is placed in the mold groove 3 for molding, so that the mold material forms the shape of the spline input shaft, and the left side of the spline input shaft is in an open hole state, forming an inner hole with the same specifications as the hole needle 4, so that there is no need for machining, the overall strength is improved, there is no need to increase the heat treatment process, and the cost is reduced.
[0021] The contents not described in detail in this specification belong to the prior art known to the professional and technical personnel in this field. The specific embodiments described in this article are only used to illustrate the spirit of the utility model. The technicians in the technical field of the utility model can make various modifications or supplements to the specific embodiments described or replace them in a similar way, but they will not deviate from the spirit of the utility model or exceed the scope defined by the attached claims.
Claims
1. A cold heading forming die for a spline input shaft, comprising a lower die (1), characterized in that: A mold base (2) is fixedly mounted on the surface of the lower mold (1); a mold groove (3) is provided in the inner cavity of the mold base (2); and a hole needle (4) is provided in the inner cavity of the mold groove (3).
2. According to claim 1, a spline input shaft cold heading forming die, characterized in that: A stopper (6) is fixedly welded to the left side of the hole needle (4), and a clamping groove (7) is provided on the top and the bottom of the stopper (6).
3. According to claim 1, a spline input shaft cold heading forming die, characterized in that: A spline groove is provided inside the mold groove (3), and the hole needle (4) is a cylindrical structure.
4. The cold heading forming die for a spline input shaft according to claim 1, characterized in that: A clamping assembly (5) is fixedly mounted on the top and bottom of the left side of the lower mold (1), and the clamping assembly (5) comprises a fixing shell (51).
5. A spline input shaft cold heading forming die according to claim 4, characterized in that: The fixed shell (51) is fixedly welded to the left side of the lower mold (1); a spring (52) is fixedly connected to the inner cavity of the fixed shell (51); and a clamping rod (53) is fixedly connected to the other side of the spring (52).
