Conductive wear-resistant probe with diamond-like carbon coating
By depositing a cobalt-like carbon thin film and nickel-phosphorus alloy and gold alloy coatings on the probe tip, combined with a sharp rib design, the problem of insufficient probe tip hardness is solved, the wear resistance and conductivity of the probe are improved, and efficient electrical signal detection is achieved.
Patent Information
- Application Number
- CN202420080999.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-12
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2034-01-12
AI Technical Summary
Existing probes, while ensuring conductivity, suffer from insufficient hardness, resulting in poor wear resistance and short service life, making it difficult to meet the needs of high-efficiency electrical signal detection.
A diamond-like carbon film is deposited on the probe tip structure, combined with nickel-phosphorus alloy and gold alloy coatings to form a composite coating to improve hardness and conductivity. The sharp rib structure design is used to pierce the oxide layer to ensure stable electrical contact.
It achieves high hardness, wear resistance and conductivity of the probe tip, reduces loss, avoids soldering, and improves detection accuracy and service life.
Smart Images

Figure CN222070695U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to an electrical signal detection probe, in particular to a conductive wear-resistant probe with a diamond-like carbon coating. Background Art
[0002] In order to ensure smooth signal transmission and electrical correctness of electronic circuits, all kinds of electronic components and electronic devices need to undergo relevant detection procedures for electrical signals during the manufacturing process to ensure the states of various parameters of the components and devices. At this time, probes are often used as detection tools. When detecting electrical signals, the probe head at the front end of the probe is manipulated to contact an object to be tested. Since an oxide layer is generally formed on the surface of the object to be tested, in order to accurately measure the electrical signal, in addition to forming an appropriate contact pressure between the probe head and the object to be tested, the front end of the probe head also needs to properly scrape the oxide layer on the surface of the object to be tested so as to directly contact the surface of the object to be tested and detect electrical signals such as resistance, current or voltage. In this way, the hardness and conductivity of the front end structure of the probe head have a certain required level. Otherwise, if the hardness is insufficient, the service life will be short and the loss cost will be unacceptable.
[0003] However, it is known that the probe head often lowers the hardness requirement when considering conductivity, which makes it difficult to improve the wear resistance and service life. In view of this, how to set a coating on the probe head structure to improve the hardness of the probe head while ensuring high conductivity, so as to improve the above-mentioned shortcomings of the prior art, is the subject that the utility model intends to explore. Utility Model Content
[0004] In view of the above problems, the purpose of the present utility model is to provide a conductive and wear-resistant electrical signal detection probe with a diamond-like carbon coating, so as to achieve the purpose of modifying the surface of the probe head by depositing a layer of diamond-like carbon film on the surface of the probe head, thereby achieving the effect of improving the hardness, wear resistance and conductivity of the probe head.
[0005] To achieve the above-mentioned purpose, the utility model provides a conductive wear-resistant probe with a diamond-like carbon coating, comprising a probe head structure, a modular component and an elastic structure, wherein the modular component has the elastic structure built therein, and the probe head structure is assembled at one end of the modular component and embedded in the elastic structure, and when the modular component is manipulated to detect an object to be detected, the elastic structure reduces the applied force between the object to be detected and the probe head structure, wherein: the probe head structure is arranged in an uneven cylindrical shape and is provided with a front end portion, a middle end portion and a rear end portion, and the two sides of the middle end portion are respectively connected to the front end portion and the rear end portion, The cross-sectional area of the circular surface of the middle end portion is smaller than that of the front end portion but larger than that of the rear end portion; a connecting groove is provided at the middle end portion near the connection with the rear end portion for connecting the modular element, and the rear end of the rear end portion converges toward the center point at an angle to form a cone; the probe head structure is made of an alloy substrate and a plurality of sharp ribs are provided at the front end portion, each of the sharp ribs has at least one chamfered portion so that an angle is formed between each of the sharp ribs, and the probe head structure is provided with a nickel-phosphorus alloy coating, a gold alloy coating and a diamond-like carbon coating in sequence from bottom to top on the surface of the alloy substrate.
[0006] In addition, the front end of the front end portion has a groove and four sharp ribs in the middle, and the four sharp ribs are arranged in a symmetrical ring with the groove as the center, and each sharp rib has two chamfered parts so that the front end of the probe head structure forms a square four-claw arrangement. Each sharp rib has an angle of 50 to 80 degrees.
[0007] In summary, the present invention utilizes the nickel-phosphorus alloy coating, the gold alloy coating, and the diamond-like carbon coating coated on the alloy substrate surface of the probe head structure to enhance the hardness of the probe head, thereby improving the hardness and wear resistance of each of the sharp ribs and reducing the probe loss rate. At the same time, by virtue of the good conductivity of nickel in the nickel-phosphorus alloy, the superior conductivity of gold itself, and the good conductivity of graphite carbon atoms in diamond-like carbon, the probe head structure is ensured to maintain good conductivity and meet high-standard detection requirements. In this way, the present invention enables the conductive wear-resistant probe to have the characteristics of high conductivity, high hardness, high wear resistance, and low loss. Furthermore, since the graphite carbon atoms in the diamond-like carbon coating have the characteristic of good lubricity, the conductive wear-resistant probe has the functional characteristics of anti-sticking, so as to avoid the problem of tinning when contacting the object to be tested during detection, thereby achieving the effect of perfecting practical quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0008] Figure 1 This is a perspective view of a probe according to a preferred embodiment of the present invention.
[0009] Figure 2 This is a cross-sectional view of the probe head structure of a preferred embodiment of the utility model.
[0010] Figure 3This is a schematic diagram of a probe according to another preferred embodiment of the present invention.
[0011] Figure 4 This is an exploded view of a probe according to another preferred embodiment of the present invention.
[0012] Figure 5 This is a cross-sectional view of a probe according to another preferred embodiment of the present invention.
[0013] Explanation of the reference numerals: 1-conductive wear-resistant probe; 10-probe head structure; 100-alloy substrate; 101-nickel-phosphorus alloy coating; 102-gold alloy coating; 103-diamond-like carbon coating; 110-front end; 1100-sharp rib; 111-middle end; 1110-assembly groove; 112-rear end; 11-modular component; 12-elastic structure; 13-connection structure. DETAILED DESCRIPTION
[0014] In order to enable a person skilled in the art with general knowledge in the art to clearly understand the contents of the present invention, the following description is provided with reference to the drawings.
[0015] See also Figure 1 , Figure 2 , which are respectively a perspective view of a probe and a cross-sectional view of a probe head structure of a preferred embodiment of the utility model. As shown in the figure, the conductive wear-resistant probe 1 with a diamond-like carbon coating can include a probe head structure 10, a modular component 11 and an elastic structure 12. The modular component 11 has the elastic structure 12 built therein, and the probe head structure 10 is assembled at one end of the modular component 11 and embedded in the elastic structure 12. When the modular component 11 is manipulated to detect an object to be detected, the elastic structure 12 reduces the applied force between the object to be detected and the probe head structure 10. The probe head structure 10 is made of an alloy substrate 100 and is provided with a plurality of sharp ribs 1100 at one end thereof, each of the sharp ribs 1100 has at least one chamfered portion so that each of the sharp ribs 1100 has an angle, and the probe head structure 10 is provided with a nickel-phosphorus alloy coating 101, a gold alloy coating 102 and a diamond-like carbon coating 103 in order from bottom to top on the surface of the alloy substrate 100. The diamond-like carbon coating 103 is a composite composition of structural elements between sp2 graphite and sp3 diamond, and the three-dimensional composite structure of graphite and diamond components can be controlled by adjusting the target coating power and the substrate bias to form a carbon-based coating with a hardness of 600-1500 Hv and a conductivity of 10-100 S / cm.
[0016] In this way, the outer coating film covering the probe head structure 10 is formed by the good conductivity and lubricity of the graphite carbon atoms in the diamond-like carbon coating 103 and the high hardness and wear resistance of the diamond carbon atoms, so that the probe head structure 10 can have both high hardness and conductivity. Due to the lubricity of the graphite carbon atoms, the probe head structure 10 has anti-sticking properties, avoiding the tinning phenomenon when the probe head structure 10 contacts the object to be tested, thereby achieving the effect of further improving the practical quality of the conductive wear-resistant probe 1.
[0017] See also Figure 3 to Figure 5 , which are respectively a schematic diagram of a probe, an exploded diagram of a probe and a cross-sectional diagram of another preferred embodiment of the utility model. As shown in the figure, the conductive wear-resistant probe 1 with a diamond-like carbon coating comprises a probe head structure 10, a modular element 11, an elastic structure 12 and a connecting structure 13. The modular element 11 is in a hollow cylindrical shape and has the elastic structure 12, such as a metal spring, built therein. The two ends of the modular element 11 are respectively used to assemble the probe head structure 10 and the connecting structure 13 and are respectively inserted into the two ends of the elastic structure 12.
[0018] The probe head structure 10 is arranged in an uneven cylindrical shape and has a front end 110, a middle end 111 and a rear end 112. The two sides of the middle end 111 are respectively connected to the front end 110 and the rear end 112, and the circular cross-sectional area of the middle end 111 is smaller than the front end 110 and larger than the rear end 112. The probe head structure 10 is made of an alloy substrate 100, such as one of copper alloy, iron alloy and palladium alloy or a combination thereof, and is provided with a plurality of sharp ribs 1100 at the front end 110, each of the sharp ribs 1100 has at least one bevel portion so that there is an angle between each of the sharp ribs 1100. For example, the front end of the front end 110 has a groove and four sharp ribs 1100 in the middle, and the four sharp ribs 1100 are arranged around the groove and arranged in a symmetrical ring shape with the groove as the center, and each of the sharp ribs 1100 has two bevel portions so that the front end of the probe head structure 10 forms a square four-claw setting, and the four-claw ribs have an angle of 50 to 80 degrees. It can be seen from this that when each of the sharp ribs 1100 is in contact with the object to be tested, the square four claws cut into the object to be tested most stably without deviation, that is, the area where the multiple sharp ribs 1100 contact the object to be tested is in a non-planar state, so as to increase the multi-directional contact force by utilizing the structure of the beveled portion not cutting straight up or straight down. Furthermore, in order to have better detection performance, the multiple sharp ribs 1100 help to pierce and cut through the oxide layer on the surface of the object to be tested, so that the multiple sharp ribs 1100 and the object to be tested can actually form an electrically conductive state. More specifically, when pressed against the object to be tested, the multiple sharp ribs 1100 can pierce the oxide layer, which can effectively eliminate the influence of the oxide layer on the surface of the object to be tested on electrical conductivity during testing, thereby improving the accuracy of detection. Of course, the plurality of sharp ribs 1100 may also be densely and continuously arranged to facilitate scraping off the oxide layer.
[0019] The middle portion 111 is provided with a connecting groove 1110 near the connection with the rear portion 112 for connecting the modular element 11, and the rear end of the rear portion 112 converges toward the center point at an angle to form a cone shape for connecting to the elastic structure 12 to transmit a test signal. The connecting structure 13 is used to connect an external electronic device (not shown). When the modular element 11 is operated to detect an object to be tested, the elastic structure 12 reduces the applied force between the object to be tested and the probe head structure 10 to ensure that the contact pressure is appropriate, and the elastic structure 12 transmits the test signal obtained from the detection of the probe head structure 10 to the connecting structure 13, and then the connecting structure 13 transmits it to the electronic device.
[0020] Subsequently, since each of the sharp ribs 1100 has the highest impact force and the highest wear when cutting into the metal object to be tested, if the hardness is too high, it is easy to crack and break, and if the hardness is too low, it is easy to wear. Therefore, in order to improve the hardness and conductivity of the probe head structure 10, the probe head structure 10 is provided with a nickel-phosphorus alloy coating 101 with a thickness of 0.5 to 5 um, a gold alloy coating 102 with a thickness of 0.3 to 3 um, and a diamond-like carbon (DLC) coating 103 with a thickness of 0.03 to 1 um from bottom to top on the surface of the alloy substrate 100. The nickel-phosphorus alloy coating 101 is formed by electroplating nickel and phosphorus into an alloy coating under a process parameter of a current density of 0.2-2ASD, so as to form a first-level protective film on the surface of the probe head structure 10 by virtue of the superior corrosion resistance of the nickel-phosphorus alloy. The addition of phosphorus to the nickel-phosphorus alloy can further improve the hardness and wear resistance of the probe head structure 10. In addition, the good electrical conductivity of nickel can ensure that the probe head structure 10 still has high signal sensitivity even when covered by the first-level nickel-phosphorus alloy coating. The gold alloy coating 101 is formed by electroplating gold and other metal elements into an alloy coating under a process parameter of a current density of 0.2-2ASD, so as to form a second-level protective film on the surface of the probe head structure 10 by virtue of the superior corrosion resistance, electrical conductivity and plasticity of gold itself, so as to provide a continuous high signal sensitivity while improving the adhesion of the subsequent diamond-like carbon coating 103.
[0021] In other words, gold plating is a surface electroplating process. This process is to plate a layer of nickel-phosphorus alloy on the surface of the metal substrate, and then plate a layer of gold on the surface of the electroplated nickel, so as to effectively prevent the diffusion of the metal body through the uniform and fine coating of the gold plating, low porosity, low stress and good ductility, so as to prevent nickel oxidation and greatly improve the conductivity and wear resistance. Nickel plating / gold plating is to wrap a layer of nickel-gold alloy with good electrical performance on the surface of the metal body, which can protect the substrate for a long time. It is different from OSP (Organic Solderability Preservative) which is only used as an anti-rust barrier. It is a protective coating that can be used for a long time, achieves good power performance and has environmental tolerance that other surface treatment processes do not have. However, the reason for nickel plating is that gold and copper will diffuse into each other, and nickel can prevent the diffusion between them. If there is no nickel barrier, gold will diffuse into copper within a few hours. Therefore, chemical nickel plating / gold plating can also prevent the dissolution of copper. In addition, another advantage of chemical nickel / gold plating is the strength of nickel. Nickel with a thickness of only 5um can control the expansion in the Z direction at high temperatures.
[0022] Furthermore, the diamond-like carbon coating 103 is a composite composition of structural elements between sp2 graphite and sp3 diamond, and can be formed by a coating technique such as vapor deposition, ion beam assisted deposition, sputtering deposition, magnetic filtered cathode arc or pulsed laser deposition, and can be adjusted at a working pressure of 10 by adjusting the target coating power and the substrate bias. -2 ~10 -5 The three-dimensional composite structure of graphite and diamond components is controlled under the process parameters of 200 to 2000W of operating power to deposit a carbon-based coating with a hardness of 600 to 1500Hv and a conductivity of 10 to 100S / cm. In this way, the outermost coating of the probe head structure 10 is formed by the good conductivity and lubricity of graphite carbon atoms and the high hardness and wear resistance of diamond carbon atoms, so that the probe head structure 10 has both high hardness and conductivity, and at the same time, the probe head structure 10 has anti-sticking properties to avoid the problem of tinning when the probe head structure 10 contacts the object to be tested.
[0023] By the way, in order to avoid the occurrence of cracks, holes and uneven coating in each coating during the coating process, the utility model formulates a precise current density based on multiple experimental data. The current density in each coating process is controlled accordingly to ensure that an appropriate current value is provided and the density of the coating is improved under the premise of an economically efficient coating time, thereby achieving the effect of improving the yield of the probe process.
[0024] The above description is only a preferred embodiment of the present invention and is not intended to limit the scope of implementation of the present invention. Therefore, equivalent changes and modifications made without departing from the spirit and scope of the present invention should be included in the scope of the present invention.
Claims
1. A conductive wear-resistant probe with a diamond-like carbon coating, comprising a probe head structure, a modular element and an elastic structure, wherein the modular element has the elastic structure built therein, and the probe head structure is assembled at one end of the modular element and embedded in the elastic structure, and when the modular element is operated to detect an object to be tested, the elastic structure reduces the applied force between the object to be tested and the probe head structure, characterized in that: The probe head structure is arranged in an uneven cylindrical shape and is provided with a front end, a middle end and a rear end, the two sides of the middle end are respectively connected to the front end and the rear end, and the cross-sectional area of the circular surface of the middle end is smaller than the front end and larger than the rear end; the middle end is provided with a connecting groove near the rear end for connecting the modular element, and the rear end of the rear end converges toward the center point at an angle to form a cone; The probe head structure is made of an alloy substrate and is provided with a plurality of sharp ribs at the front end, each of the sharp ribs has at least one chamfered portion so that an angle is formed between each of the sharp ribs, and the probe head structure is provided with a nickel-phosphorus alloy coating, a gold alloy coating and a diamond-like carbon coating in sequence from bottom to top on the surface of the alloy substrate.
2. The conductive wear-resistant probe with diamond-like carbon coating as claimed in claim 1, characterized in that: The front end of the front end portion has a groove and four sharp ribs in the middle, the four sharp ribs are symmetrically arranged in a ring with the groove as the center, and each sharp rib has two chamfered parts so that the front end of the probe head structure forms a square four-claw configuration.
3. The conductive wear-resistant probe with diamond-like carbon coating as claimed in claim 2, characterized in that: Each of the sharp ribs has an included angle of 50 to 80 degrees.