Flaky composite material
By designing the stacking of rubber coat layer and glass fiber layer in the composite material and filling the glass fiber layer with resin, the problems of low elastic modulus and poor temperature difference in composite material are solved, and the interlayer shear strength and anti-aging are improved performance.
Patent Information
- Application Number
- CN202323602113.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-28
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2033-12-28
AI Technical Summary
The existing composite materials have problems such as low elastic modulus, poor long-term temperature difference resistance, easy aging and low interlayer shear strength.
A structure that includes a rubber coat layer, a resin layer bonded to the surface of the rubber coat layer, and a glass fiber layer bonded to the surface of the resin layer, is filled with resin in the glass fiber layer, and is laid and connected and stacked with rubber coat layer. design.
The elastic modulus, long-term temperature difference resistance and interlayer shear strength of the composite material are improved, bubbles and wrinkles are avoided in the rubber coat layer, and the temperature difference and anti-aging properties are improved.
Smart Images

Figure CN222097225U_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the technical field of composite materials, and specifically relates to a sheet-like composite material. Background Art
[0002] Composite material FRP is also called GRP or GFRP, and its scientific name is glass fiber reinforced plastic. It is a composite material made of glass fiber and its products as reinforcing materials and synthetic resin as matrix material through a certain molding process. The concept of composite material means that one material cannot meet the use requirements, and two or more materials need to be combined together to form another material that can meet people's requirements, that is, composite materials.
[0003] However, existing composite materials have defects such as low elastic modulus, poor long-term temperature difference resistance, easy aging and low interlaminar shear strength. Utility Model Content
[0004] The purpose of the embodiments of the present application is to provide a sheet-like composite material with a high elastic modulus, good long-term temperature difference resistance, not prone to aging and high interlaminar shear strength, thereby solving at least one technical problem involved in the background technology.
[0005] In order to solve the above technical problems, this application provides the following technical solutions:
[0006] The embodiment of the present application provides a sheet-like composite material, including a gel coat layer, a resin layer bonded and fixed to the surface of the gel coat layer, and a glass fiber layer bonded and fixed to the surface of the resin layer, wherein the glass fiber layer is filled with resin.
[0007] As a limitation of the present invention, the glass fiber layer includes a plurality of glass fiber blocks, and adjacent glass fiber blocks are overlapped and connected.
[0008] As a limitation of the present invention, the overlap width is 45-55 mm.
[0009] As a limitation of the present invention, the overlap is compacted by a roller.
[0010] As a limitation of the present invention, the gel coat layer includes a first gel coat layer and a second gel coat layer stacked together, wherein the gel coat dosage of the first gel coat layer is 0.55±0. kg / m2 and the thickness is 0.4-0.6 mm; the gel coat dosage of the second gel coat layer is 0.8±0.1 kg / m2 and the thickness is 0.5-0.8 mm.
[0011] As a limitation of the present invention, the resin layer is made of unsaturated polyester resin or vinyl resin material.
[0012] The beneficial effects of the embodiments of the present application are as follows:
[0013] 1. The gel coat layer is configured as a first gel coat layer and a second gel coat layer stacked together, which can not only avoid bubbles and wrinkles in the gel coat layer, but also improve the temperature difference resistance and anti-aging performance of the composite material;
[0014] 2. By filling the glass fiber layer with resin, the elastic modulus and interlaminar shear strength of the composite material can be improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for describing the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative work, among which:
[0016] Figure 1 It is a schematic diagram of the structure of the sheet-like composite material provided in the embodiment of the present application. DETAILED DESCRIPTION
[0017] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments, and the embodiments can be arranged horizontally or vertically, and can respectively realize the application of horizontal excitation loads and vertical excitation loads. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present application.
[0018] The terms "first", "second", etc. in the specification and claims of the present application are used to distinguish similar objects, and are not used to describe a specific order or sequence. It should be understood that the data used in this way can be interchangeable under appropriate circumstances, so that the embodiments of the present application can be implemented in an order other than those illustrated or described here, and the objects distinguished by "first", "second", etc. are generally of one type, and the number of objects is not limited. For example, the first object can be one or more. In addition, "and / or" in the specification and claims represents at least one of the connected objects, and the character " / " generally indicates that the objects associated with each other are in an "or" relationship.
[0019] See also Figure 1 As shown, the embodiment of the present application provides a sheet-like composite material, including a gel coat layer 1, a resin layer 2 bonded and fixed to the surface of the gel coat layer 1, and a glass fiber layer 3 bonded and fixed to the surface of the resin layer 2, wherein the glass fiber layer 3 is filled with resin.
[0020] It should be noted that the resin filled in the glass fiber layer 3 is the same as the resin used in the resin layer 2 .
[0021] The gel coat layer 1 comprises a first gel coat layer 11 and a second gel coat layer 12 stacked together, wherein the gel coat dosage of the first gel coat layer 11 is 0.55±0.1 kg / m2 and the thickness is 0.4-0.6 mm; the gel coat dosage of the second gel coat layer 12 is 0.8±0.1 kg / m2 and the thickness is 0.5-0.8 mm.
[0022] The resin layer 2 is made of unsaturated polyester resin or vinyl resin material.
[0023] The glass fiber layer 3 includes a plurality of glass fiber blocks, and the adjacent glass fiber blocks are overlapped and connected, wherein the overlap width is 50±10 mm, and the overlap is compacted by a roller.
[0024] The beneficial effects of the embodiments of the present application are as follows:
[0025] 1. The gel coat layer is configured as a first gel coat layer and a second gel coat layer stacked together, which can not only avoid bubbles and wrinkles in the gel coat layer, but also improve the temperature difference resistance and anti-aging performance of the composite material;
[0026] 2. By filling the glass fiber layer with resin, the elastic modulus and interlaminar shear strength of the composite material can be improved.
[0027] The embodiments of the present application are described above in conjunction with the accompanying drawings, but the present application is not limited to the above-mentioned specific implementation methods. The above-mentioned specific implementation methods are merely illustrative and not restrictive. Under the guidance of the present application, ordinary technicians in this field can make many forms of changes without departing from the purpose of the present application and the scope of protection of the claims, but all of them are within the protection of the present application.
Claims
1. A sheet-like composite material, characterized in that: The invention comprises a gel coat layer, a resin layer bonded and fixed to the surface of the gel coat layer, and a glass fiber layer bonded and fixed to the surface of the resin layer, wherein the glass fiber layer is filled with resin, and the resin filled in the glass fiber layer is the same as the resin used in the resin layer; the glass fiber layer comprises a plurality of glass fiber blocks, and adjacent glass fiber blocks are overlapped and connected, and the gel coat layer comprises a first gel coat layer and a second gel coat layer stacked.
2. The sheet-like composite material according to claim 1, characterized in that: The overlap width is 45-55mm.
3. The sheet-like composite material according to claim 2, characterized in that: The overlap is compacted with a roller.
4. The sheet-like composite material according to claim 1, characterized in that: The gel coat dosage of the first gel coat layer is 0.55±0.1 kg / m2, and the thickness is 0.4-0.6 mm; the gel coat dosage of the second gel coat layer is 0.8±0.1 kg / m2, and the thickness is 0.5-0.8 mm.
5. The sheet-like composite material according to claim 1, characterized in that: The resin layer is made of unsaturated polyester resin or vinyl resin material.