Stamping device

By setting stamping channels and stops in the die base of the stamping device, the elastic deformation of the stop is used to introduce waste and block the punch when the punch exits, the problem of waste is solved and the service life of the stamping device is improved. The accuracy of stamping holes improves production efficiency.

CN222113246UActive Publication Date: 2024-12-06GUANGDONG MIDEA KITCHEN APPLIANCES MFG CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420627850.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-28
Publication Date
2024-12-06
Estimated Expiration
2034-03-28

AI Technical Summary

Technical Problem

During the stamping process, the waste material of the plate is easily adsorbed on the mould and brought out with the mould, resulting in damage to the mould and the stamping device during the subsequent stamping process, affecting product quality and production efficiency.

Method used

Design a stamping device, by setting a stamping port and stamping channel in the base of the die, and using the elastic deformation of the stop during the stamping process, waste material is introduced to the other side of the stamping channel, and the deformation is restored when the punch exits. Block the waste and prevent it from being taken out.

Benefits of technology

Effectively prevent waste from jumping out, reduce damage to plates and stamping devices, improve the service life of stamping devices and the accuracy of stamping holes, reduce the accuracy during subsequent stamping processes, reduce risks, and improve production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222113246U_ABST
    Figure CN222113246U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of stamping, and provides a stamping device which comprises a plate, a male die and a female die. The female die comprises a base and a stopping piece, a stamping channel and a stamping opening are formed in the base, the stamping opening is communicated with the stamping opening, the stamping opening is covered with the plate, the stopping piece is arranged in the base so as to separate the stamping channel in the stamping direction, a stopping hole penetrating through the two side faces in the stamping direction is formed in the stopping piece, and the stopping hole is communicated with the stamping channel. The hydraulic diameter of the stamping opening is larger than that of the stop hole; the male die is configured to punch the plate, and in the punching process, the male die can make the stop piece generate elastic deformation, so that waste of the plate enters the other side of the punching channel from one side of the punching channel through the stop hole; and in the process that the male die retreats from the stop hole, the stop piece recovers deformation so as to stop waste materials of the plate. The stamping device is good in waste jumping prevention effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of stamping technology, and in particular to a stamping device. Background Art

[0002] In the related art, the stamping device includes a punch and a die. When the punch is stamping the sheet, the waste material of the sheet will be carried out with the rise of the punch after breaking and separation, which will cause damage to the sheet and the stamping device in the subsequent stamping process. Utility Model Content

[0003] In view of this, an embodiment of the present application hopes to provide a punching device that prevents waste from bouncing.

[0004] In order to achieve the above-mentioned purpose, the technical solution of the embodiment of the present application is implemented as follows:

[0005] The present application embodiment discloses a stamping device, comprising:

[0006] Plates;

[0007] The die comprises a base and a stopper, wherein the base is formed with a punching channel and a punching opening, wherein the punching opening is communicated with the punching channel, wherein the plate cover is arranged on the punching opening, wherein the stopper is arranged in the base to separate the punching channel along the punching direction, wherein the stopper is formed with a stopper hole penetrating through two side surfaces in the punching direction, wherein the stopper hole is communicated with the punching channel, and wherein the hydraulic diameter of the punching opening is greater than the aperture of the stopper hole;

[0008] A punch is configured to punch the sheet material. During the punching process, the punch can cause the stopper to undergo elastic deformation to move the waste material of the sheet material from one side of the punching channel through the stop hole into the other side of the punching channel; when the punch exits the stop hole, the stopper resumes its deformation to block the waste material of the sheet material.

[0009] In one embodiment, the thickness of the plate is between 0.4 mm and 0.6 mm, and the diameter of the punching hole of the plate is between 1.5 mm and 5 mm.

[0010] In one embodiment, the stamping channel includes a first channel and a second channel, the first channel is connected to the second channel, the first channel is located on the side of the second channel close to the punch along the stamping direction, the first channel is connected to the stamping port, the stopper is arranged in the second channel, and the hydraulic diameter of the first channel is smaller than the hydraulic diameter of the second channel.

[0011] In one embodiment, during the punching process, a gap between the punch and the first channel along a first direction is between 0.5 mm and 1 mm, wherein the first direction is perpendicular to the punching direction.

[0012] In one embodiment, the stopper is formed with an exhaust groove running through the stamping direction, and the exhaust groove is located at the outer periphery of the stop hole.

[0013] In one embodiment, there are multiple exhaust grooves, and the multiple exhaust grooves are arranged at intervals along the circumference of the stop hole.

[0014] In one embodiment, the exhaust groove is connected to the stop hole.

[0015] In one embodiment, a dimension of the stopper along the stamping direction is between 0.3 mm and 0.8 mm.

[0016] In one embodiment, the punching opening, the stop hole and the punching channel are coaxially arranged.

[0017] In one embodiment, the die is formed with a slot and a socket connected to the slot, the opening direction of the socket is a first direction, and the stopper is inserted into the slot through the socket, wherein the first direction is perpendicular to the stamping direction.

[0018] The embodiment of the present application discloses a stamping device, which is provided with a stamping port and a stamping channel on a base, a plate is provided at the stamping port, and a punch is used to stamp the plate against the stamping port and the stamping channel along the stamping direction, so that the waste material of the plate can be broken and separated to present a stamping hole that matches the shape of the stamping port. A stopper is provided in the base, and the stopper is formed with a stopper hole along the stamping direction, and the stopper hole is connected to the stamping channel, and the hydraulic diameter of the stamping port is greater than the aperture of the stopper hole, that is, the hydraulic diameter of the waste material is greater than the aperture of the stopper hole, so that when the punch pushes the waste material to contact the periphery of the stopper hole, the stopper will undergo elastic deformation, so that the aperture of the stopper hole will expand, so that the waste material and the punch can enter the other side of the stamping channel through the stopper hole; after the stamping is completed, the punch withdraws from the stopper hole, and at this time, the stopper will restore its deformation due to the absence of the extrusion of the punch, so that the aperture of the stopper hole is restored, so that due to the adhesion Waste materials adsorbed on the punch due to adhesion, magnetism and vacuum will contact the periphery of the stop hole during the withdrawal of the punch to block the waste materials and prevent them from being brought out of the punching port. On the one hand, it has a good effect in preventing waste materials from jumping, which can reduce damage to the sheet and the punching device and increase the service life of the punching device; on the other hand, it can reduce the risk of reduced dimensional accuracy of the punching holes in the subsequent punching process and improve the quality and production efficiency of sheet processing; on the other hand, the punching device of the present application has a simpler structure than the prior art and has low processing difficulty and cost for the punching holes. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 A schematic cross-sectional view of a punching device provided in an embodiment of the present application, wherein the punch punches and breaks the waste material of the plate;

[0020] Figure 2 A cross-sectional schematic diagram of a stamping device provided in another embodiment of the present application, wherein the stopper is elastically deformed and the punch pushes the waste material through the stop hole;

[0021] Figure 3 A cross-sectional schematic diagram of a punching device provided in yet another embodiment of the present application, wherein the punch exits the stop hole and the stopper recovers its deformation;

[0022] Figure 4 A schematic structural diagram of a stopper provided in yet another embodiment of the present application.

[0023] Description of Reference Numerals

[0024] Punching device 100; plate 1; punching hole 1a; die 2; base 21; punching channel 21a; first channel 21a1; second channel 21a2; punching port 21b; stopper 22; stop hole 22a; exhaust groove 22b; punch 3; connecting seat 31; punch 32; waste material A. DETAILED DESCRIPTION

[0025] It should be noted that, in the absence of conflict, the embodiments and technical features in the embodiments of the present application can be combined with each other, and the detailed description in the specific implementation method should be understood as an explanation of the purpose of the present application and should not be regarded as an improper limitation on the present application.

[0026] The present application is further described in detail below in conjunction with the accompanying drawings and specific embodiments. The descriptions of "first", "second", etc. in the embodiments of the present application are only for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly including at least one feature. In the description of the embodiments of the present application, the meaning of "multiple" is at least two, such as two, three, etc., unless otherwise clearly and specifically limited.

[0027] In the related art, the stamping device includes a punch and a die. When stamping the sheet, the waste of the sheet is easily adsorbed on the punch due to the oil, magnetism and vacuum on the punch. After the punch rises, the waste will be brought out with the rise of the punch, and then fall on the stamping device, causing damage to the sheet and the stamping device in the subsequent stamping process, and may even affect the dimensional accuracy of the stamping holes of the sheet, seriously affecting the quality of the product and production efficiency.

[0028] A stamping device provided in the embodiment of the present application is shown in FIG. Figures 1 to 4The punching device 100 includes a plate 1, a die 2 and a punch 3. The die 2 includes a base 21 and a stopper 22. The base 21 is formed with a punching channel 21a and a punching port 21b. The punching port 21b is connected to the punching channel 21a. The plate 1 is covered with the punching port 21b. The stopper 22 is arranged in the base 21 to separate the punching channel 21a along the punching direction. The stopper 22 is formed with a stop hole 22a penetrating the two sides in the punching direction. The stop hole 22a is connected to the punching channel 21a. The hydraulic diameter of the punching port 21b is larger than the aperture of the stop hole 22a. The punch 3 is configured to punch the sheet 1. During the punching process, the punch 3 can cause the stopper 22 to undergo elastic deformation to move the waste material A of the sheet 1 from one side of the punching channel 21a through the stop hole 22a into the other side of the punching channel 21a; during the process of the punch 3 exiting the stop hole 22a, the stopper 22 restores its deformation to block the waste material A of the sheet 1.

[0029] The stamping device 100 provided in the present application is configured by setting a stamping port 21b and a stamping channel 21a on a base 21, and a plate 1 is set at the stamping port 21b. The punch 3 stamps the plate 1 against the stamping port 21b and the stamping channel 21a along the stamping direction. In this way, the waste material A of the plate 1 can be broken and separated to present a stamping hole 1a that is adapted to the shape of the stamping port 21b. By arranging a stopper 22 in the base 21, the stopper 22 is formed with a stop hole 22a along the stamping direction, the stop hole 22a is connected to the stamping channel 21a, and the hydraulic diameter of the stamping port 21b is larger than the aperture of the stop hole 22a, that is, the hydraulic diameter of the waste material A is larger than the aperture of the stop hole 22a. In this way, when the punch 3 pushes the waste material A to contact the periphery of the stop hole 22a, the stopper 22 will undergo elastic deformation, so that the aperture of the stop hole 22a will expand, so that the waste material A and the punch 3 can enter the other side of the stamping channel 21a through the stop hole 22a; after the stamping is completed, the punch 3 withdraws from the stop hole 22a, and at this time, the stopper 22 will restore its deformation due to the absence of the extrusion of the punch 3, so that the stop hole 2 The aperture of 2a is restored. In this way, the waste A adsorbed on the punch 3 due to adhesion, magnetism and vacuum will contact the periphery of the stop hole 22a during the withdrawal of the punch 3, so as to block the waste A and prevent it from being brought out of the punching port 21b. On the one hand, the waste A can be prevented from jumping out, which can reduce the damage to the plate 1 and the punching device 100 and increase the service life of the punching device 100; on the other hand, the risk of reducing the dimensional accuracy of the punching hole 1a in the subsequent punching process can be reduced, and the processing quality and production efficiency of the plate 1 can be improved; on the other hand, the punching device 100 of the present application is simpler in structure than that in the prior art, and the processing difficulty and cost of the punching hole 1a are low.

[0030] It should be noted that the stamping direction may be a downward direction, and the upward direction refers to the direction toward the ceiling, and the downward direction is opposite to the upward direction.

[0031] It should be noted that Figure 2 The R1 in can be in the up and down directions.

[0032] It should be noted that the hydraulic diameter refers to the ratio of four times the cross-sectional area of ​​the flow passage to the perimeter. The flow passage refers to the cross-section taken by the streamline cluster perpendicular to the fluid. For example, if the cross-sectional shape of the central channel is a regular quadrilateral, the hydraulic diameter is the ratio of four times the cross-sectional area of ​​the central channel of the regular quadrilateral to the perimeter of the regular quadrilateral. For another example, if the cross-sectional shape of the central channel is a circle, the hydraulic diameter is the diameter of the circular central channel.

[0033] Exemplarily, in one embodiment, the shape of the punching opening 21b may be circular.

[0034] For example, in one embodiment, please refer to Figures 1 to 3 The punch 3 includes a connecting seat 31 and a punch 32. The connecting seat 31 is connected to the side of the punch 32 away from the die 2. The projection along the stamping direction, the projection area of ​​the stamping port 21b and the projection area of ​​the punch 32 are both located within the projection area of ​​the connecting seat 31. In this way, when the punch 32 is inserted into the stamping channel 21a, the connecting seat 31 can abut against the surface of the die 2 where the stamping port 21b is set to prevent the punch 32 from being difficult to retract.

[0035] Exemplarily, in one embodiment, the shape of the plate 1 is not limited. For example, in the projection along the stamping direction, the plate 1 can be round, square or other shapes.

[0036] Exemplarily, in one embodiment, the plate 1 may be a sheet metal part.

[0037] Exemplarily, in one embodiment, the shape of the punching channel 21 a is not limited. For example, the shape of the punching channel 21 a can be circular when projected along the punching direction.

[0038] For example, in one embodiment, please refer to Figures 1 to 3 The punching channel 21a can penetrate the die 2 along the punching direction, so that the waste A of the plate 1 can be discharged from the side of the punching channel 21a away from the punching port 21b to avoid blocking the punching channel 21a.

[0039] In one embodiment, the thickness of the plate 1 is between 0.4 mm and 0.6 mm, and the diameter of the punching hole 1a of the plate 1 is between 1.5 mm and 5 mm. For example, the thickness of the plate 1 can be 0.4 mm, 0.45 mm, 0.5 mm, 0.55 mm or 0.6 mm, etc., and the diameter of the punching hole 1a can be 1.5 mm, 2 mm, 2.5 mm, 3 mm, 3.5 mm, 4 mm, 4.5 mm, 5 mm, 5.5 mm or 6 mm, etc. It should be noted that when punching holes in such thin plates, some related technologies adopt solutions to reduce the contact area with the waste, such as setting protrusions, pits and reinforcing ribs at the bottom of the punch, etc. However, due to the size and light weight of such plates, the punched waste is easily affected by magnetic force, adhesion force and vacuum negative pressure and is carried out by the punch, and the effect of preventing waste from jumping is poor; in other related technologies, a punching pin and a spring are set in the punch, and the punching pin will be pressed into the punch when the plate contacts. After the stamping is completed, the punching pin will be ejected by the spring to push the waste adsorbed on the punch away, and the processing of the stamping hole is difficult and the structure is complex; in some other related technologies, a processing air hole is formed in the center of the punch, and the air hole is connected to the high-pressure gas. After the stamping is completed, the waste needs to be blown off by high-pressure air, which makes the processing cost of the stamping hole high. In the present application, a stopper is provided in the die, and the waste material can be blocked under the stopper through the formed stop hole to prevent it from being carried out. The processing cost and difficulty of the punching hole are low and easy to realize.

[0040] In one embodiment, please refer to Figures 1 to 3 The punching channel 21a includes a first channel 21a1 and a second channel 21a2. The first channel 21a1 is connected to the second channel 21a2. The first channel 21a1 is located on the side of the second channel 21a2 close to the punch 3 along the punching direction. The first channel 21a1 is connected to the punching port 21b. The stopper 22 is arranged in the second channel 21a2. The hydraulic diameter of the first channel 21a1 is smaller than the hydraulic diameter of the second channel 21a2. Exemplarily, the first channel 21a1 can be a punching channel, and the second channel 21a2 can be a chip removal channel. The first channel 21a1 can avoid and cooperate with the punch 3 to better process the punching hole 1a of the required size with high processing accuracy. The hydraulic diameter of the first channel 21a1 can be equal to the hydraulic diameter of the punching port 21b. In this way, the processing accuracy of the punching hole 1a can be improved. The hydraulic diameter of the second channel 21a2 is larger than the hydraulic diameter of the first channel 21a1, and the stopper 22 is arranged in the second channel 21a2. In this way, when the punch 3 punches the plate 1, the broken and separated waste A can pass through the stop hole 22a under the push of the punch 3, and can fall freely when entering the second channel 21a2 without the continuous push of the punch 3.

[0041] Exemplarily, in one embodiment, the stopper 22 may also be disposed at the first channel 21a1.

[0042] In one embodiment, please refer to Figure 1 and Figure 2 , during the punching process of the punch 3, the gap between the punch 3 and the first channel 21a1 along the first direction is between 0.5mm and 1mm, wherein the first direction is perpendicular to the punching direction. Exemplarily, the gap between the punch 3 and the first channel 21a1 can be 0.3mm, 0.4mm, 0.5mm, 0.6mm, 0.7mm or 0.8mm, etc. By setting a suitable gap, on the one hand, the suitable gap can reduce the generation of burrs on the sheet 1 during the punching process, making the edge of the punching hole 1a smoother and neater, and the processing accuracy of the punching hole 1a is high; on the other hand, the suitable gap can reduce the friction between the punch 3 and the punching channel 21a, thereby reducing the wear of the punching device 100 and increasing the life of the punching device 100.

[0043] It should be noted that the first direction may be the front-to-back direction, the left-to-right direction, or the radial direction of the stop hole.

[0044] It should be noted that Figure 2 R2 can be in the front-to-back direction, the left-to-right direction, or the radial direction of the stop hole.

[0045] In one embodiment, please refer to Figure 1 and Figure 4 The stopper 22 is formed with an exhaust groove 22b that runs through the stamping direction, and the exhaust groove 22b is located at the periphery of the stop hole 22a. Here, when the punch 3 pushes the waste material A to contact the stopper 22 along the stamping direction, since the waste material A will cover the stop hole 22a at this time, and the gap between the punch 3 and the stamping channel 21a is small, the pressure of the space between the stopper 22 and the stamping port 21b in the stamping channel 21a is high, and it is difficult for the punch 3 to push the waste material A to continue to move. By setting the exhaust groove 22b on the periphery of the stopper 22 at the stop hole 22a, the gas in the space between the stopper 22 and the stamping port 21b in the stamping channel 21a can be discharged to the side of the stamping channel 21a located on the stopper 22 away from the stamping port 21b through the exhaust groove 22b, so that the punch 3 can easily push the waste material A through the stop hole 22a.

[0046] In one embodiment, please refer to Figure 4 , the number of the exhaust grooves 22b is multiple, and the multiple exhaust grooves 22b are arranged at intervals along the circumference of the stop hole 22a. Exemplarily, the number of the exhaust grooves 22b can be 8, and the 8 exhaust grooves 22b are arranged at 45° intervals along the circumference of the stop hole 22a to form a "plum blossom" shape. In this way, not only the exhaust volume is further increased, so that the punch 3 can more easily push the waste A through the stop hole 22a, but also the appearance is beautiful.

[0047] In one embodiment, please refer to Figure 4 In this way, not only is it easy to discharge the gas in the space between the stopper 22 and the punching port 21b in the punching channel 21a, but also the exhaust groove 22b is connected to the stop hole 22a, which can reduce the structural strength of the periphery of the stop hole 22a, so as to further enable the punch 3 to push the waste material A through the stop hole 22a.

[0048] For example, in one embodiment, the specific size of the diameter of the stop hole 22a can be adjusted according to the diameter, material thickness, material and other properties of the punching hole 1a to ensure that the deformation of the stopper 22 during the deformation process does not exceed the elastic limit, thereby avoiding failure due to plastic deformation. For example, the diameter of the stop hole 22a can be between 2 mm and 3 mm, and specifically, the diameter of the stop hole 22a can be 2.6 mm.

[0049] Exemplarily, in one embodiment, the shape of the exhaust groove 22b may be a rectangle. For example, the width of the exhaust groove 22b may be 0.2 mm, and the length of the exhaust groove 22b may be 0.7 mm.

[0050] In one embodiment, the size of the stopper 22 along the stamping direction is between 0.3 mm and 0.8 mm. Exemplarily, the size of the stopper 22 along the stamping direction can be 0.3 mm, 0.4 mm, 0.5 mm, 0.6 mm, 0.7 mm or 0.8 mm, etc. In this way, by setting the stopper 22 of appropriate size, on the one hand, the stopper 22 can have better elasticity. In the process of the punch 3 pushing the waste A through the stop hole 22a, the punch 3 can easily cause the periphery of the stop hole 22a to elastically deform, so that the aperture of the stop hole 22a is expanded, so that the waste A can pass through the stop hole 22a more easily; on the other hand, setting the stopper 22 of appropriate size can improve the structural strength of the stopper 22 to a certain extent, so that when the punch 3 withdraws from the stop hole 22a, it can better resist the waste A and prevent it from being taken out by the punch 3.

[0051] In one embodiment, the punching opening 21b, the stop hole 22a and the punching channel 21a are coaxially arranged. On the one hand, the coaxial arrangement can improve the alignment accuracy during the punching process, reduce deviation, and thus improve the qualified rate of the sheet 1 processing; on the other hand, the punching opening 21b, the stop hole 22a and the punching channel 21a are coaxially arranged, which can ensure the stability during the punching process and the pushing process of the waste material A, reduce the impact of vibration and impact on the punching device 100, and improve the service life of the punching device 100; on the other hand, since the punching opening 21b, the stop hole 22a and the punching channel 21a are coaxially arranged, the operator can more easily observe and timely adjust the punching process, so as to more accurately punch the sheet 1 and pass the waste material A through the stop hole 22a.

[0052] In one embodiment, the die 2 is formed with a slot and a socket connected to the slot, the opening direction of the socket is a first direction, and the stopper 22 is inserted into the slot through the socket, wherein the first direction is perpendicular to the stamping direction.

[0053] In this way, on the one hand, when it is necessary to block the waste A, the stopper 22 can be inserted into the slot from the socket along the first direction. Since the stamping direction is perpendicular to the first direction, the stopper 22 arranged perpendicular to the stamping direction can enable the punch 3 to push the waste A through the stop hole 22a to maintain a stable posture, reduce the possibility of deviation and tilt, and the punching hole 1a of the plate 1 has high accuracy and pass rate; on the other hand, the stopper 22 can be easily replaced and repaired with high efficiency.

[0054] The above is only a preferred embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. All modifications, equivalent substitutions, improvements, etc. within the spirit and principles of the present application are included in the protection scope of the present application.

Claims

1. A punching device, It is characterized in that include: Plates; The die comprises a base and a stopper, wherein the base is formed with a punching channel and a punching opening, wherein the punching opening is communicated with the punching channel, wherein the plate cover is arranged on the punching opening, wherein the stopper is arranged in the base to separate the punching channel along the punching direction, wherein the stopper is formed with a stopper hole penetrating through two side surfaces in the punching direction, wherein the stopper hole is communicated with the punching channel, and wherein the hydraulic diameter of the punching opening is greater than the aperture of the stopper hole; A punch is configured to punch the sheet material. During the punching process, the punch can cause the stopper to undergo elastic deformation to move the waste material of the sheet material from one side of the punching channel through the stop hole into the other side of the punching channel; when the punch exits the stop hole, the stopper resumes its deformation to block the waste material of the sheet material.

2. The punching device according to claim 1, It is characterized in that The thickness of the plate is between 0.4 mm and 0.6 mm, and the diameter of the punching hole of the plate is between 1.5 mm and 5 mm.

3. The punching device according to claim 1, It is characterized in that The stamping channel includes a first channel and a second channel, the first channel is connected to the second channel, the first channel is located on a side of the second channel close to the punch along the stamping direction, the first channel is connected to the stamping port, the stopper is arranged in the second channel, and the hydraulic diameter of the first channel is smaller than the hydraulic diameter of the second channel.

4. The punching device according to claim 3, It is characterized in that During the punching process, a gap between the punch and the first channel along a first direction is between 0.5 mm and 1 mm, wherein the first direction is perpendicular to the punching direction.

5. The punching device according to claim 1, It is characterized in that The stopper is formed with an exhaust groove penetrating the punching direction, and the exhaust groove is located at the outer periphery of the stop hole.

6. The punching device according to claim 5, It is characterized in that There are multiple exhaust grooves, and the multiple exhaust grooves are arranged at intervals along the circumference of the stop hole.

7. The punching device according to claim 5, It is characterized in that The exhaust groove is communicated with the stop hole.

8. The punching device according to claim 1, It is characterized in that The dimension of the stopper along the stamping direction is between 0.3 mm and 0.8 mm.

9. The punching device according to claim 1, It is characterized in that The punching opening, the stop hole and the punching channel are coaxially arranged.

10. The punching device according to claim 1, It is characterized in that The die is formed with a slot and a socket connected to the slot, the opening direction of the socket is a first direction, and the stopper is inserted into the slot through the socket, wherein the first direction is perpendicular to the stamping direction.