Chassis with anti-ablation structure
By using internally cooled iron, heat conducting pipes and high-temperature ablation silicon carbide particle filler in the steel ingot mold chassis, the short life problem caused by thermal shock during the mold casting process is solved, and the long life use and production cost of the chassis is achieved The reduction.
Patent Information
- Application Number
- CN202323667799.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-31
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2033-12-31
AI Technical Summary
During the mold casting process, the chassis of the steel ingot mold has a short service life due to long-term high-temperature thermal shock, resulting in large consumption and increased production costs.
An anti-ablation structural chassis was designed, using multiple internally cooled iron, heat conducting pipes and high-temperature ablated silicon carbide particle fillers, combining chromium ore sand and refractory bricks to form a step hole structure to quickly solidify the steel and improve the service life of the chassis.
It effectively solves the ablation problem in the runner area, extends the service life of the chassis, and reaches more than 22 furnaces per piece, and reduces production costs.
Smart Images

Figure CN222113461U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the field of steel ingot die casting devices, and in particular relates to an anti-ablation structural chassis. Background Art
[0002] When using die casting to produce steel ingots, the chassis and the ingot mold are generally combined into a casting mold, and bottom pouring is adopted. The center hole of the chassis is used as the inner runner. During pouring, more than 10 tons of molten steel at 1560-1590℃ are all poured into the ingot mold through it. During this period, the molten steel flows continuously from its center hole. The center hole of the chassis is strongly subjected to the thermal shock of the molten steel during the pouring process. Until the entire ingot mold is poured, the flushing time is long. Under this working environment, the chassis requires the material of the center hole of the chassis to have high strength.
[0003] Since no special measures were taken during the casting process, the chassis of the steel ingot mold had a short service life and was scrapped after less than 10 uses, resulting in high chassis consumption, reduced continuity of die casting production, and increased production costs of die casting steel ingots. Utility Model Content
[0004] The utility model aims to provide an anti-ablation structural chassis, which can make molten steel solidify quickly and refine grains at the pouring channel of the chassis, thereby increasing the service life of the chassis.
[0005] The technical solution is as follows:
[0006] The anti-ablation structural chassis comprises: a chassis body, a runner is arranged in the middle of the chassis body, a plurality of risers are arranged on the top surface of the chassis body, the upper opening of the runner is located on the top surface of the chassis body, the lower opening of the runner is located on the bottom surface of the chassis body, a plurality of hangers are arranged on the side wall of the chassis body, and a plurality of internal chillers are arranged inside the chassis body; the runner is a stepped hole with an inner diameter increasing downward, the stepped hole comprises: a first runner section, a second runner section, and a third runner section, the first runner section, the second runner section, and the third runner section are connected in sequence from top to bottom; chromium ore sand is arranged in the second runner section; heat conduction pipes are arranged in the first runner section and the second runner section, ablative fillers and refractory bricks are arranged in the heat conduction pipes, the ablative fillers are located on the upper part of the refractory bricks, and the heat conduction pipes are inserted into the chromium ore sand.
[0007] Furthermore, the second runner section and the third runner section are four-sided trapezoids.
[0008] Furthermore, the two ends of the refractory bricks are respectively connected with ablative fillers and chromium ore sand; the ablative fillers are made of high-temperature ablative silicon carbide particles.
[0009] Furthermore, the bottom surface of the chassis body is circular, and the top surface is provided with four risers, each of which has a diameter of 100 mm.
[0010] Furthermore, the riser is located on a concentric circle with a radius of 1 / 2 of the bottom surface of the chassis body.
[0011] Furthermore, a groove is arranged at the front end of the hanging handle.
[0012] Compared with the prior art, the utility model has the following advantages:
[0013] The invention aims to make molten steel solidify quickly and refine grains in the center of the chassis by adopting measures such as cold iron, hanging handle, filling silicon carbide, adding heat conduction pipes, etc., so as to improve the service life of the chassis.
[0014] By adopting the anti-ablation process, the problem of sintering and sand sticking in the runner is solved, and the sand mold in the runner 5 can be removed during rough cleaning without processing or using strong impact to remove it.
[0015] The chassis has been used through ingot casting, and the service life of each piece is more than 22 furnaces, and all chassis can continue to be used. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a schematic diagram of the structure of the anti-ablation structural chassis in the utility model;
[0017] Figure 2 It is a schematic cross-sectional structure diagram of the anti-ablation structural chassis in the utility model. DETAILED DESCRIPTION
[0018] The following description sufficiently illustrates specific embodiments of the present invention to enable those skilled in the art to practice and reproduce the same.
[0019] like Figure 1 As shown, it is a schematic diagram of the structure of the anti-ablation structure chassis in the utility model; Figure 2 The figure is a schematic diagram of the cross-sectional structure of the anti-ablation structural chassis in the utility model.
[0020] The anti-ablation structural chassis comprises: a chassis body 1, a runner 5 is arranged in the middle of the chassis body 1, a plurality of risers 2 are arranged on the top surface of the chassis body 1, an upper opening of the runner 5 is located on the top surface of the chassis body 1, a lower opening of the runner 5 is located on the bottom surface of the chassis body 1, a plurality of hangers 3 are arranged on the side wall of the chassis body 1, and a plurality of internal chillers 4 are arranged inside the chassis body 1; the runner 5 is a stepped hole with an inner diameter increasing downward, and the stepped hole comprises: a first runner section, a second runner section, and a third runner section, and the first runner section, the second runner section, and the third runner section are connected in sequence from top to bottom; chromium ore sand 9 is arranged in the second runner section; heat pipes 7 are arranged in the first runner section and the second runner section, and ablation fillers 8 and refractory bricks 6 are arranged in the heat pipes 7, and the heat pipes 7 are inserted into the chromium ore sand 9.
[0021] The two ends of the refractory brick 6 are respectively connected to the ablative filler 8 and the chrome ore sand 9; the ablative filler 8 is made of high temperature ablative silicon carbide particles. The second runner section and the third runner section are four-sided trapezoids.
[0022] The bottom surface of the chassis body 1 is used as the parting surface, which is circular. The casting is arranged as a whole in the lower mold, and the upper mold is a riser 2 (4 locations) with a diameter of Φ100mm. The runner 5 is cast by top pouring. The cross-sectional area ratio of the pouring system is: vertical: horizontal: internal = 2:1.5:1.2. The riser 2 adopts the open riser method, and the riser (4 locations) with a diameter of Φ100mm is placed on the concentric circle of 1 / 2 the bottom radius of the chassis body 1. The 4 risers are evenly distributed. The runner 5 adopts top pouring, and the thickness of the inner runner is 20mm, and the thickness of the horizontal runner is 35mm.
[0023] The chassis body 1 is molded with furan resin sand. The molding sand is continuously vibrated during the molding process. Internal and external chillers 4 are placed. Refractory bricks 6 (high-aluminum refractory bricks) with a thickness of 45 mm are placed in the heat pipe 7 at the bottom hole. The surface bricks of the refractory bricks 6 are thickened with zircon powder coating. Heat pipes 7 are added to the sand tire of the chrome ore sand 9 in the second runner section to enable the central part to solidify quickly and refine the grains in the center of the ingot mold chassis.
[0024] Use inner cooling iron 4 and chromium ore sand for quenching; place two inner cooling irons 4 with a distance of 80 mm around the bottom hole inside; fill the second runner section with chromium ore sand 9 with a thickness of 100 mm.
[0025] The hanging handle 3 is changed to an inner-inserted 35# steel handle; the hanging handle uses 4 35# steel handles with a diameter of 80mm and a length of 300mm, which are embedded in the casting mold, and three grooves with a width of 10mm and a depth of 15mm are opened at the front end of the steel handle.
[0026] In order to obtain high-strength gray iron structure, it is necessary to change the organization of ferrite and cementite to make the cast iron structure in the center excellent. The smelting plan uses ductile iron with high purity and low phosphorus and sulfur content as raw material, medium frequency electric furnace smelting, appropriate amount of Si and Mn alloy elements, 1400℃ molten iron, and silicon-barium-iron alloy inoculation, slag removal, and then pouring, the pouring temperature is 1320℃-1380℃; BaSiFe (high barium ferrosilicon Ba≥10%) is selected as the inoculant; the proportion of scrap steel is increased by 1% to 5% to 15%, and the carbon equivalent and silicon-carbon ratio are reduced; the carbon element is close to the lower limit of 3.5%, and the chemical composition is controlled within the range of the following Table 1. The rest is still implemented according to the general molding, core making and smelting process codes.
[0027] Table 1
[0028] element C Si Mn P S CE content / % 3.5-3.9 1.5-1.9 0.5-1.0 ≤0.15 ≤0.10 4.2-4.4
[0029] The terms used in the present invention are illustrative and exemplary, rather than restrictive. Since the present invention can be implemented in various forms without departing from the spirit or essence of the technical solution, it should be understood that the above embodiments are not limited to any of the aforementioned details, but should be widely interpreted within the spirit and scope defined by the attached claims, so all changes and modifications falling within the scope of the claims or their equivalents should be covered by the attached claims.
Claims
1. An anti-ablation structural chassis, characterized in that: include: A chassis body, a runner is arranged in the middle of the chassis body, a plurality of risers are arranged on the top surface of the chassis body, an upper opening of the runner is located on the top surface of the chassis body, a lower opening of the runner is located on the bottom surface of the chassis body, a plurality of hangers are arranged on the side wall of the chassis body, and a plurality of internal chillers are arranged inside the chassis body; the runner is a stepped hole with an increasing inner diameter downward, the stepped hole comprises: a first runner section, a second runner section, and a third runner section, the first runner section, the second runner section, and the third runner section are sequentially connected from top to bottom; chromium ore sand is arranged in the second runner section; heat conduction pipes are arranged in the first runner section and the second runner section, ablative fillers and refractory bricks are arranged in the heat conduction pipes, the ablative fillers are located on the upper part of the refractory bricks, and the heat conduction pipes are inserted into the chromium ore sand.
2. The anti-ablation structural chassis according to claim 1, characterized in that: The second runner section and the third runner section are four-sided trapezoids.
3. The anti-ablation structural chassis according to claim 1, characterized in that: The two ends of the refractory bricks are respectively connected with ablative fillers and chromium ore sand; the ablative fillers are made of high-temperature ablative silicon carbide particles.
4. The anti-ablation structural chassis according to claim 1, characterized in that: The bottom surface of the chassis body is circular, and the top surface is provided with four risers, each with a riser diameter of 100 mm.
5. The anti-ablation structural chassis according to claim 4, characterized in that: The riser is located on a concentric circle with a radius of 1 / 2 of the bottom surface of the chassis body.
6. The anti-ablation structural chassis according to claim 1, characterized in that: A groove is arranged at the front end of the hanging handle.