Halogen-free low-smoke low-toxicity polyolefin cable wire

By introducing technical means such as ant-proof layer, galvanized steel belt armor layer and flame retardant layer into the cable, the problem of buried cables being susceptible to mice and termites is solved, the service life and protection performance of the cable are improved, and the Higher insulation and flame retardant properties.

CN222126025UActive Publication Date: 2024-12-06WUHAN XINTIANDI ELECTRICAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420764178.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-15
Publication Date
2024-12-06
Estimated Expiration
2034-04-15

AI Technical Summary

Technical Problem

Traditional cables are susceptible to threats such as mice and termites in buried environments, resulting in damage to the protective layer and affecting service life and safety.

Method used

A halogen-free, low smoke and low toxic polyolefin cable wire is designed, using ant-proof layer, galvanized steel tape armor layer, flame retardant layer and toughness layer, combined with halogen-free flame retardant filler and high-temperature resistant rubber material to enhance the cable protection and insulation performance.

Benefits of technology

It effectively reduces the threat of mice and termites, improves the service life and insulation performance of the cable, enhances the bending, compression and flame retardant properties of the cable, and significantly improves the wear-resistant and protective performance of the cable.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222126025U_ABST
    Figure CN222126025U_ABST
Patent Text Reader

Abstract

The utility model relates to a halogen-free low-smoke low-toxicity polyolefin cable wire, which belongs to the technical field of cables and comprises a cable core arranged in a sheath, and a protection structure and a protection assembly are arranged outside the cable core. The protection structure comprises a shielding layer arranged outside the cable core body and a first insulating layer installed outside the shielding layer. The protection assembly comprises a second insulating layer, a galvanized steel tape armoring layer, a protection layer and an anti-termite layer. The protection structure further comprises a flame-retardant layer and an armoring layer which are arranged outside the sheath. According to the halogen-free low-smoke low-toxicity polyolefin cable wire, threats of rats, termites and the like can be reduced through the anti-termite layer, the service life of the cable core body is prolonged, the influence of external high temperature on the internal wire core can be prevented through the second insulating layer and the protective layer, the insulating performance is improved, and therefore the advantages of being good in protective effect and the like are achieved; the problem that the outside of an underground cable is easily threatened by mice, termites and the like is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of cable technology, and in particular to a halogen-free, low-smoke, low-toxic polyolefin cable wire. Background Art

[0002] Cable is a device for transmitting electric energy or signals, usually composed of several or several groups of wires. Cables include power cables, control cables, compensation cables, shielded cables, high temperature cables, computer cables, signal cables, coaxial cables, fire-resistant cables, marine cables, mining cables, aluminum alloy cables, etc. They are all composed of single or multiple wires and insulation layers, used to connect circuits, electrical appliances, etc.

[0003] At present, with the rapid development of the national economy and the continuous improvement of people's living standards, the social electricity consumption has greatly increased. With the sharp increase in the use of various electrical equipment, electrical fire accidents have also increased dramatically. According to statistics, there are about 100,000 fires in my country every year, with direct property losses of more than 1 billion yuan. Among them, fires caused by electrical reasons such as cable short circuit, overload, and electrical equipment failure account for about 30% of the total number. The number of electrical fires and the losses caused are both the highest among all types of fires. Among electrical fires, fires caused by cables account for about half. Therefore, people pay more and more attention to the flame retardant and fire safety of cables, and the requirements for flame retardant and fire protection of cables are getting higher and higher.

[0004] Traditional fire-resistant cables use copper conductors, and the copper conductors are wrapped with mica tapes to form a fire-resistant layer. The mica tape wrapping layer is insulated with flame-retardant polyvinyl chloride or a low-smoke, halogen-free flame-retardant outer sheath. However, existing cables lack an anti-termite layer. Since the cables are mainly used for underground burial, the outer part of the cables is easily threatened by rats, termites, etc., resulting in damage to the outer protective layer of the cables, which seriously affects the quality of the cables. Therefore, a halogen-free, low-smoke, low-toxic polyolefin cable wire is proposed to solve the above problems. Utility Model Content

[0005] In view of the deficiencies in the prior art, the present application provides a halogen-free, low-smoke, low-toxic polyolefin cable wire, which has the advantages of good protection effect and solves the problem that the outside of the buried cable is easily threatened by rats, termites, etc.

[0006] In summary, the present application provides the following technical solutions: a halogen-free, low-smoke, low-toxic polyolefin cable wire, comprising a cable core disposed inside a sheath, wherein a protective structure and a protective component are disposed outside the cable core;

[0007] The protective structure comprises a shielding layer arranged outside the cable core, and a first insulating layer installed outside the shielding layer;

[0008] The protection assembly includes a second insulating layer, a galvanized steel belt armor layer, a protective layer and an anti-termite layer.

[0009] By adopting the above-mentioned technical solution, the present application can reduce the threat of rats, termites, etc. through the anti-termite layer and increase the service life of the cable core. Through the second insulating layer and the protective layer, it can prevent the external high temperature from affecting the internal core while improving the insulation performance, thereby achieving the advantages of good protection effect, etc., and solving the problem that the outside of the buried cable is easily threatened by rats, termites, etc.

[0010] Furthermore, the protective structure also includes a flame retardant layer and an armor layer arranged outside the sheath, and the shielding layer is made of red copper braided wire.

[0011] The beneficial effect of adopting the above further solution is that the wear resistance and protection performance of the cable is greatly improved by providing the armor layer.

[0012] Furthermore, the flame retardant layer and the armor layer are distributed in sequence from the inside to the outside, the gap inside the sheath is filled with a halogen-free flame retardant filler, and the first insulating layer is formed by extrusion of a halogen-free low-smoke flame retardant cross-linked polyolefin material.

[0013] The beneficial effect of adopting the above further solution is that the flame retardancy of the cable is greatly improved by the halogen-free flame retardant filler and the flame retardant layer.

[0014] Furthermore, a toughness layer is provided between the sheath and the flame retardant layer, and the toughness layer comprises a ceramic silicone rubber layer and a nylon layer.

[0015] The beneficial effect of adopting the above further solution is that the bending resistance and compression resistance of the cable are greatly improved by providing the toughness layer, the ceramic silicone rubber layer and the nylon layer.

[0016] Furthermore, the second insulating layer, the galvanized steel belt armor layer, the protective layer and the anti-termite layer are sequentially arranged inside and outside, and the second insulating layer is made of high temperature resistant rubber material.

[0017] The beneficial effect of adopting the above further scheme is that the wear-resistant protection performance of the cable is greatly improved by setting the galvanized steel belt armor layer and the armor layer.

[0018] Furthermore, the protective layer is fixedly installed on a side of the galvanized steel strip armor layer away from the second insulating layer, and the anti-termite layer is fixedly installed on the outer wall of the protective layer.

[0019] The beneficial effect of adopting the above further scheme is that the first insulating layer, the second insulating layer and the protective layer can prevent the external high temperature from affecting the internal cable core, while improving the insulation performance and achieving good heat resistance.

[0020] Compared with the prior art, the present application provides a halogen-free, low-smoke, low-toxic polyolefin cable and wire, which has the following beneficial effects:

[0021] 1. The halogen-free, low-smoke, low-toxic polyolefin cable and wire can reduce the threat of rats, termites, etc. through the anti-termite layer, and increase the service life of the cable core. The second insulation layer and the protective layer can prevent the external high temperature from affecting the internal core, while improving the insulation performance, thereby achieving the advantages of good protection effect, etc., and solving the problem that the outside of the buried cable is easily threatened by rats, termites, etc.

[0022] 2. The halogen-free, low-smoke, low-toxic polyolefin cable wire has greatly improved the bending and compression resistance of the cable by setting a toughness layer, a ceramic silicone rubber layer and a nylon layer. The flame retardancy of the cable is greatly improved by setting a halogen-free flame retardant filler and a flame retardant layer. The wear resistance of the cable is greatly improved by setting a galvanized steel belt armor layer and an armor layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is a schematic diagram of the structure of this application;

[0024] Figure 2 It is a schematic diagram of the structure of the toughness layer of the present application;

[0025] Figure 3 It is a schematic diagram of the structure of the protection component of this application.

[0026] Description of reference numerals:

[0027] 1. Cable core; 2. Shielding layer; 3. First insulation layer; 4. Sheath; 5. Halogen-free flame retardant filler; 6. Toughness layer; 61. Ceramic silicone rubber layer; 62. Nylon layer; 7. Flame retardant layer; 8. Armor layer; 9. Protection component; 91. Second insulation layer; 92. Galvanized steel tape armor layer; 93. Protection layer; 94. Anti-ant layer. DETAILED DESCRIPTION

[0028] See also Figure 1-3 A halogen-free, low-smoke, low-toxic polyolefin cable wire comprises a cable core 1 arranged inside a sheath 4, a protective structure and a protective component 9 are arranged outside the cable core 1; the protective structure comprises a shielding layer 2 arranged outside the cable core 1, and a first insulating layer 3 installed outside the shielding layer 2;

[0029] The protective structure further includes a flame retardant layer 7 and an armor layer 8 arranged outside the sheath 4, and the shielding layer 2 is made of red copper braided wire.

[0030] It should be noted that the flame retardant layer 7 and the armor layer 8 are distributed from the inside to the outside, the gap inside the sheath 4 is filled with a halogen-free flame retardant filler 5, and the first insulating layer 3 is formed by extrusion of a halogen-free low-smoke flame retardant cross-linked polyolefin material. By providing the halogen-free flame retardant filler 6 and the flame retardant layer 7, the flame retardancy of the cable is greatly improved.

[0031] See also Figure 1 and Figure 2 In this embodiment, a toughness layer 6 is provided between the sheath 4 and the flame retardant layer 7, and the toughness layer 6 includes a ceramic silicone rubber layer 61 and a nylon layer 62. By providing the toughness layer 6, the ceramic silicone rubber layer 61 and the nylon layer 62, the bending resistance and compression resistance of the cable are greatly improved.

[0032] See also Figure 1 and Figure 3 , wherein the protection component 9 includes a second insulating layer 91, a galvanized steel belt armor layer 92, a protective layer 93 and an anti-termite layer 94. The protective layer 93 is fixedly installed on the side of the galvanized steel belt armor layer 92 away from the second insulating layer 91, and the anti-termite layer 94 is fixedly installed on the outer wall of the protective layer 93. The outer surface of the protection component 9 can also be coated with a fluorescent layer, and the light emitted by the fluorescent layer is yellow light, which can be used by the yellow light emitted by the fluorescent layer to facilitate the staff to quickly locate the cable.

[0033] In addition, the second insulating layer 91, the galvanized steel belt armor layer 92, the protective layer 93 and the anti-termite layer 94 are sequentially arranged inside and outside, and the second insulating layer 91 is made of high temperature resistant rubber material. Through the first insulating layer 3, the second insulating layer 91 and the protective layer 93, it is possible to prevent the external high temperature from affecting the internal cable core, while improving the insulation performance and achieving good heat resistance. The anti-termite layer 94 is an insect repellent coating, and the anti-termite layer 94 is coated on the outer surface of the protective layer 93. The anti-termite layer 94 can reduce the threat of rats, termites, etc. and increase the service life of the cable core. The galvanized steel belt armor layer 92 is woven from a single layer of tinned copper wire. By setting the galvanized steel belt armor layer 92 and the armor layer 8, the wear resistance and protection performance of the cable are greatly improved, thereby achieving the advantages of good protection effect, etc., and solving the problem that the outside of the buried cable is easily threatened by rats, termites, etc.

[0034] It should be noted that the second insulating layer 91 is not only made of high temperature resistant rubber material, but also can be made of cross-linked polyethylene material. The insect repellent coating is dieldrin sprayed on the outer wall of the protective layer 93, and can also be sprayed by the following aldrin, lindane, chlordane, heptachlor, etc. Rat repellent can also be sprayed, and rat repellent is a common rat repellent method, which can be sprayed on the area around the cable that is gnawed by rodents or where the cable may be loose. Rat repellent can effectively protect the cable from being gnawed. In addition, it is necessary to spray a rat repellent that is harmless to the human body, but it should be noted that before spraying the agent, the cable trench must be kept dry to ensure the effectiveness of the agent to ensure the safety and integrity of the cable.

[0035] The working principle of the above embodiment is:

[0036] When in use, the anti-ant layer 94 can reduce the threat of rats, termites, etc. and increase the service life of the cable core 1. The second insulating layer 92 and the protective layer 93 can prevent the external high temperature from affecting the internal core while improving the insulation performance and achieving good heat resistance. The toughness layer 6, the ceramic silicone rubber layer 61 and the nylon layer 62 are provided to greatly improve the bending and compression resistance of the cable. The halogen-free flame-retardant filler 6 and the flame-retardant layer 7 are provided to greatly improve the flame retardancy of the cable. The galvanized steel belt armor layer 92 and the armor layer 8 are provided to greatly improve the wear resistance and protection of the cable, thereby achieving the advantages of good protection effect, etc., and solving the problem that the outside of the buried cable is easily threatened by rats, termites, etc.

Claims

1. A halogen-free, low-smoke, low-toxic polyolefin cable wire, comprising a cable core (1) arranged inside a sheath (4), characterized in that: The cable core (1) is provided with a protective structure and a protective component (9) on the outside; The protective structure comprises a shielding layer (2) arranged outside the cable core (1), and a first insulating layer (3) installed outside the shielding layer (2); The protection component (9) comprises a second insulating layer (91), a galvanized steel belt armor layer (92), a protective layer (93) and an anti-termite layer (94).

2. The halogen-free, low-smoke, low-toxic polyolefin cable and wire according to claim 1, characterized in that: The protective structure further comprises a flame retardant layer (7) and an armor layer (8) arranged outside the sheath (4), and the shielding layer (2) is made of red copper braided wire.

3. The halogen-free, low-smoke, low-toxic polyolefin cable and wire according to claim 2, characterized in that: The flame retardant layer (7) and the armor layer (8) are sequentially distributed from the inside to the outside, the gap inside the sheath (4) is filled with a halogen-free flame retardant filler (5), and the first insulating layer (3) is formed by extrusion of a halogen-free low-smoke flame retardant cross-linked polyolefin material.

4. The halogen-free, low-smoke, low-toxic polyolefin cable and wire according to claim 3, characterized in that: A toughness layer (6) is provided between the jacket (4) and the flame retardant layer (7), and the toughness layer (6) comprises a ceramic silicone rubber layer (61) and a nylon layer (62).

5. The halogen-free, low-smoke, low-toxic polyolefin cable and wire according to claim 1, characterized in that: The second insulating layer (91), the galvanized steel belt armor layer (92), the protective layer (93) and the anti-termite layer (94) are arranged in sequence from the inside to the outside, and the second insulating layer (91) is made of a high-temperature resistant rubber material.

6. The halogen-free, low-smoke, low-toxic polyolefin cable and wire according to claim 1, characterized in that: The protective layer (93) is fixedly mounted on a side of the galvanized steel strip armor layer (92) away from the second insulating layer (91), and the anti-termite layer (94) is fixedly mounted on an outer wall of the protective layer (93).