White-edge-free touch screen optical film

By designing a rectangular film body and a frame-like cutting retracted edge in the touch screen optical film, and combining laser trimming technology, the white edge problem is solved, the aesthetics and fault tolerance are improved, and the touch screen optical film without white edges is realized.

CN222189846UActive Publication Date: 2024-12-17TRULY OPTO ELECTRONICS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420039849.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-08
Publication Date
2024-12-17
Estimated Expiration
2034-01-08

AI Technical Summary

Technical Problem

In the prior art, when making touch screens, optical films and touch screens are large, resulting in white edges in a single-side gap, affecting the beauty, and the existing solutions are costly or complex in processes.

Method used

Design a touch screen optical film without white edges, which includes a rectangular film body and a frame-shaped cut inner edge, grab the shape through CCD and use laser technology to perform a single-side 0.1mm retractable cutting on the periphery of the touch screen to eliminate white edges. And optionally set preset arc or inverted trapezoidal shrink grooves to improve aesthetics and fault tolerance.

Benefits of technology

The white-edged touch screen sample has been achieved, which greatly improves the aesthetics. Since the film material is larger than the periphery of the touch screen, the fault tolerance rate during the patch is increased, and the gap after laser trimming is difficult to recognize, which significantly improves the appearance quality of the product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222189846U_ABST
    Figure CN222189846U_ABST
Patent Text Reader

Abstract

The utility model discloses a touch screen optical film without a white edge, which comprises a rectangular film body, the edge of the film body is provided with a square-frame-shaped cutting inner shrinkage edge, and the cutting inner shrinkage edge and the film body are of an integral structure. The width of the cutting inner shrinkage edge ranges from 0.8 mm to 1.2 mm. The single edge of the touch screen optical film without the white edge is expanded outwards by about 1.0 mm on the basis of the periphery of a touch screen, the appearance of the touch screen and the appearance of a film material are grabbed through a CCD, the adhesive face of the film material is attached to the surface of the touch screen, the periphery of the attached film material is larger than that of the touch screen, at the moment, single-edge 0.1 mm inward shrinkage cutting is conducted on the basis of the periphery of the touch screen through a laser technology, and the edge of the touch screen optical film without the white edge extends outwards by about 1.0 mm. And cutting off the membrane material with the excessive touch screen, so as to obtain the touch screen without the white edge. And the sample subjected to laser trimming has a gap of only 0.1 mm, so that the existence of the membrane material is difficult to identify by naked eyes, and the attractiveness of the sample is greatly improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to a touch screen, more specifically, to a touch screen optical film without white edges. Background Art

[0002] When making touch screens, the optical film and the touch screen are almost the same size. The process will allow the film material to shrink inward by 0.5mm on one side based on the periphery of the touch screen. Since this 0.5mm single-sided gap is between the edge of the optical film and the periphery of the touch screen, it creates a white edge phenomenon visually, affecting the appearance.

[0003] Chinese utility model patent document CN206373039U discloses a white edge eliminating liquid smear pen, including a liquid storage capsule, a fiber refill and a pen cap, wherein the liquid storage capsule stores transparent white edge eliminating liquid, the liquid storage capsule has a liquid outlet channel, the fiber refill is inserted into the liquid outlet channel, and one end of the fiber refill is a liquid suction end, and the other end is a liquid outlet end, the liquid suction end extends into the liquid storage capsule, and the liquid outlet end extends out of the liquid outlet channel, and the pen cap covers the outer periphery of the liquid outlet end of the fiber refill. The white edge eliminating liquid smear pen also includes a handle, the handle is fixed to one end of the liquid storage capsule away from the fiber refill, and the length direction of the handle is the same as the length direction of the liquid storage capsule. The handle is flat. The white edge eliminating liquid smear pen also includes a fixing frame, the fixing frame is embedded in the liquid outlet channel, the fiber refill is installed in the liquid outlet channel through the fixing frame, and the outer periphery of the fiber refill and the inner wall of the liquid outlet channel are sealed by the fixing frame. The liquid outlet end of the fiber pen core is tapered. The liquid storage bag is made of soft material.

[0004] Obviously, this patent uses smearing to eliminate white edges, which has limited effect and requires a lot of manual effort.

[0005] Chinese invention patent document CN110568623A discloses a method for eliminating white edges displayed by a 3D-LED module. The 3D-LED module includes n 3D polarizing films, n LED display modules and a light-transmitting layer; the n spliced ​​3D polarizing films are located between the light-transmitting layer and the n spliced ​​LED display modules, and the n 3D polarizing films correspond to the n LED display modules one by one; the method for eliminating white edges is as follows: m light-absorbing grating structures are implanted at the edge of the 3D polarizing film, so that m prism reflection structures are formed along the splicing line at the splicing point of any two 3D polarizing films, each prism reflection structure is formed by combining two light-absorbing grating structures, and the m prism reflection structures on the splicing line are used to reflect the light output by the LED display module through the splicing point to the outside of the field of view on the left and right sides, thereby eliminating white edges. The method of implanting m light-absorbing grating structures at the edge of the 3D polarizing film further includes the following steps: Step 1, setting the 1 / 2 phase difference film 103 on the side of the circular polarizing plate 100 away from the LED display module; Step 2, forming m light-absorbing grating structures 101 in the edge empty lines of the 1 / 2 phase difference film 103, and the right-angle section of the light-absorbing grating structure 101 is flush with the edge of the circular polarizing plate 100; Step 3, splicing n circular polarizing plates 100 with light-absorbing grating structures implanted and 1 / 2 phase difference films attached thereto; Step 4, uniformly flattening the empty lines of the n 1 / 2 phase difference films 103; Step 5, forming an anti-reflection layer 300 to complete the production of the 3D polarizing film. The bottom surface of the light-absorbing grating structure 101 is placed on the circular polarizing plate 100. The light-absorbing grating structure 101 is composed of a mixture of UV polymer and light-absorbing particles. The light-absorbing grating structure 101 is implanted in the edge empty lines of the 1 / 2 phase difference film 103 through a complementary mold. The prism reflection structure is an isosceles triangular prism column or an isosceles quadrangular prism column.

[0006] Obviously, the software control method used by Zhu Ali to pick up different contrast images to debug is particularly cumbersome and solve the problem of poor white edge effect; it solves the problem of white edge caused by light leakage at the joint of 3D-LED modules. The patent uses the refraction and reflection principles of prism columns to further eliminate the white edge problem. The patent uses software control to improve the white edge, which is too costly and has a very complicated structure. Utility Model Content

[0007] Based on this, it is necessary to provide a touch screen optical film without white edges for the above technical problems. The touch screen optical film without white edges comprises a rectangular film body, and the edge of the film body is provided with a square frame-shaped cut inner shrinkage, and the cut inner shrinkage and the film body are an integral structure. The width of the cut inner shrinkage is between 0.8 mm and 1.2 mm. The touch screen optical film without white edges is expanded by about 1.0 mm on one side on the basis of the periphery of the touch screen. The CCD captures the shape of the touch screen and the film material, and the adhesive surface of the film material and the surface of the touch screen are bonded. The periphery of the bonded film material will be larger than the touch screen. At this time, the laser process is used to perform a 0.1 mm unilateral shrinkage cut on the basis of the periphery of the touch screen, and the film material of the extra touch screen is removed, thereby obtaining a touch screen without white edges. Since the sample after laser trimming has only a gap of 0.1 mm, it is difficult for the naked eye to identify whether there is a film material, which greatly improves the aesthetics of the sample. At the same time, since the film material is larger than the periphery of the touch screen, some deviations during patching can also be absorbed by the larger film material, which increases the fault tolerance in the process.

[0008] In order to solve the above technical problems, the utility model adopts the following technical solutions:

[0009] A touch screen optical film without white edges, characterized in that the touch screen optical film without white edges comprises a rectangular film body, the edge of the film body is provided with a square frame-shaped cut inner shrinkage, and the cut inner shrinkage and the film body are an integrated structure.

[0010] As a preferred implementation of the touch screen optical film without white edges provided by the utility model, the width of the cut inner shrinkage edge is between 0.8 mm and 1.2 mm.

[0011] As a preferred implementation of the touch screen optical film without white edges provided by the utility model, the width of the cut inner shrinkage edge is 1 mm.

[0012] As a preferred implementation of the touch screen optical film without white edges provided by the utility model, a preset shrinkage groove is provided between the cut inner shrinkage edge and the film body.

[0013] As a preferred implementation of the touch screen optical film without white edges provided by the utility model, the shrinkage groove is arc-shaped.

[0014] As a preferred implementation of the touch screen optical film without white edges provided by the utility model, the depth of the shrinkage groove is between 0.1 mm and 0.5 mm.

[0015] As a preferred implementation of the touch screen optical film without white edges provided by the utility model, the depth of the shrinkage groove is 0.3 mm.

[0016] As a preferred implementation of the touch screen optical film without white edges provided by the utility model, the shrinkage groove is in an inverted trapezoidal shape.

[0017] As a preferred implementation of the touch screen optical film without white edges provided by the utility model, the depth of the shrinkage groove is between 0.1 mm and 0.5 mm.

[0018] As a preferred implementation of the touch screen optical film without white edges provided by the utility model, the depth of the shrinkage groove is 0.3 mm.

[0019] Compared with the prior art, the utility model has the following beneficial effects:

[0020] The utility model provides a touch screen optical film without white edges. The touch screen optical film without white edges is expanded outward on one side by about 1.0 mm on the basis of the periphery of the touch screen. The appearance of the touch screen and the film material is captured by CCD, and the adhesive surface of the film material and the surface of the touch screen are bonded. The periphery of the bonded film material will be larger than the touch screen. At this time, a laser process is used to perform a 0.1 mm inward cut on one side on the basis of the periphery of the touch screen, and the film material that is extra to the touch screen is removed, thereby obtaining a touch screen without white edges. Since the sample after laser trimming has only a 0.1 mm gap, it is difficult for the naked eye to identify whether there is a film material, which greatly improves the aesthetics of the sample. At the same time, since the film material is larger than the periphery of the touch screen, some deviations during patching can also be absorbed by the larger film material, which increases the fault tolerance rate in the process.

[0021] In addition, a preset shrinkage groove can be provided between the cut inner shrinkage edge and the film body. The shrinkage groove is arc-shaped. The depth of the shrinkage groove is between 0.1 mm and 0.5 mm. Preferably, the depth of the shrinkage groove is 0.3 mm. With the arc-shaped shrinkage groove, the shrinkage groove can automatically shrink into a smooth cutting surface during laser trimming, further improving the aesthetics of the sample.

[0022] In addition, the shrinkage groove can be made into an inverted trapezoid. The depth of the shrinkage groove is between 0.1 mm and 0.5 mm. Preferably, the depth of the shrinkage groove is 0.3 mm. With the inverted trapezoidal shrinkage groove, the shrinkage groove can automatically shrink into a smooth cutting surface during laser trimming, further improving the aesthetics of the sample. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] In order to more clearly illustrate the scheme in the utility model, a brief introduction is given below to the drawings required for use in the description of the embodiments. Obviously, the drawings described below are some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0024] FIG1 is a schematic structural diagram of a touch screen optical film without white edges of the present invention;

[0025] FIG2 is a detailed enlarged schematic diagram of area A of the structural schematic diagram of the touch screen optical film without white edges in FIG1 ;

[0026] FIG3 is a partial cross-sectional schematic diagram of the touch screen optical film without white edges in FIG1 ;

[0027] FIG4 is a detailed enlarged schematic diagram of area B of the partial cross-sectional schematic diagram of the touch screen optical film without white edges in FIG3 ;

[0028] FIG5 is a partial cross-sectional schematic diagram of another embodiment of the touch screen optical film without white edges of FIG1 ;

[0029] FIG6 is a detailed enlarged schematic diagram of area C of the partial cross-sectional schematic diagram of the touch screen optical film without white edges in FIG5 ;

[0030] The markings in the figure are as follows:

[0031] 1. Touch screen optical film; 2. Film body; 3. Cutting inner shrinkage; 4. Shrinkage groove; D. Width. DETAILED DESCRIPTION

[0032] In order to enable those skilled in the art to better understand the solution of the utility model, the technical solution in the embodiment of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiment of the utility model. Obviously, the described embodiment is only a part of the embodiment of the utility model, not all of the embodiments. Based on the embodiment of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the utility model.

[0033] As described in the background technology, with respect to the prior art, when manufacturing a touch screen, the optical film is almost the same size as the touch screen, and the process allows the film material to be shrunk by 0.5 mm on one side based on the periphery of the touch screen. Since this 0.5 mm single-sided gap is between the edge of the optical film and the periphery of the touch screen, a white edge phenomenon is visually produced, affecting the appearance.

[0034] In order to solve this technical problem, the utility model provides a touch screen optical film 1 without white edges, comprising a rectangular film body 2, the edge of the film body 2 is provided with a square frame-shaped cut inner shrink edge 3, and the cut inner shrink edge 3 is an integral structure with the film body 2. The width D of the cut inner shrink edge 3 is between 0.8 mm and 1.2 mm. Preferably, the width D of the cut inner shrink edge 3 is 1 mm.

[0035] Through the above structural design, the touch screen optical film 1 without white edges is expanded about 1.0mm on one side on the basis of the periphery of the touch screen. The CCD captures the shape of the touch screen and the film material, and the adhesive surface of the film material and the surface of the touch screen are bonded. The periphery of the bonded film material will be larger than the touch screen. At this time, the laser process is used to perform a 0.1mm inward cut on one side on the basis of the periphery of the touch screen, and the film material that is extra to the touch screen is removed, thereby obtaining a touch screen without white edges. Since the sample after laser trimming has only a 0.1mm gap, it is difficult to identify the presence of the film material with the naked eye, which greatly improves the aesthetics of the sample. At the same time, since the film material is larger than the periphery of the touch screen, some deviations during patching can also be absorbed by the larger film material, increasing the fault tolerance rate in the process.

[0036] In order to enable those skilled in the art to better understand the present invention, the technical solutions in the embodiments of the present invention will be described in detail below in conjunction with the accompanying drawings, so that the advantages and features of the present invention can be more easily understood by those skilled in the art, thereby making a clearer and more definite definition of the protection scope of the present invention.

[0037] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features and technical solutions in the embodiments may be combined with each other.

[0038] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.

[0039] Example 1

[0040] As shown in FIG. 1 and FIG. 2 , the touch screen optical film 1 without white edges comprises a rectangular film body 2 , the edge of which is provided with a square frame-shaped cut inner shrink edge 3 , and the cut inner shrink edge 3 and the film body 2 are an integral structure.

[0041] It should be noted that the width D of the cut inner shrinkage 3 is between 0.8 mm and 1.2 mm. Preferably, the width D of the cut inner shrinkage 3 is 1 mm.

[0042] The working mode of this embodiment is described below.

[0043] The touch screen optical film 1 without white edges is expanded about 1.0mm on one side on the basis of the periphery of the touch screen. The CCD captures the shape of the touch screen and the film material, and the adhesive surface of the film material and the surface of the touch screen are bonded. The periphery of the bonded film material will be larger than the touch screen. At this time, the laser process is used to perform a 0.1mm inward cut on one side on the basis of the periphery of the touch screen, and the film material that is extra to the touch screen is removed, thereby obtaining a touch screen without white edges. Since the sample after laser trimming has only a 0.1mm gap, it is difficult to identify the presence of the film material with the naked eye, which greatly improves the aesthetics of the sample. At the same time, since the film material is larger than the periphery of the touch screen, some deviations during patching can also be absorbed by the larger film material, increasing the fault tolerance rate in the process.

[0044] Example 2

[0045] As shown in FIG. 3 and FIG. 4 , the touch screen optical film without white edges provided in Example 1 is further optimized. Specifically, a preset shrinkage groove 4 is provided between the cut inner shrinkage edge 3 and the film body 2 .

[0046] It should be noted that the shrinkage groove 4 is arc-shaped. In addition, the depth of the shrinkage groove 4 is between 0.1 mm and 0.5 mm. Preferably, the depth of the shrinkage groove 4 is 0.3 mm.

[0047] The working mode of this embodiment is described below.

[0048] By utilizing the arc-shaped shrinkage groove 4, during laser trimming, the shrinkage groove 4 can automatically shrink into a smooth cutting surface, further improving the aesthetics of the sample.

[0049] Example 3

[0050] As shown in FIG. 5 and FIG. 6 , the touch screen optical film without white edges provided in Example 1 or 2 is further optimized. Specifically, the shrinkage groove 4 is in an inverted trapezoidal shape.

[0051] It should be noted that the depth of the shrinkage groove 4 is between 0.1 mm and 0.5 mm. Preferably, the depth of the shrinkage groove 4 is 0.3 mm.

[0052] The working mode of this embodiment is described below.

[0053] By utilizing the inverted trapezoidal shrinkage groove 4, during laser trimming, the shrinkage groove 4 can automatically shrink into a smooth cutting surface, further improving the aesthetics of the sample.

[0054] The terms "coupling" and "coupling" involved in the embodiments of the present application should be understood in a broad sense. For example, they may refer to a direct physical connection, or an indirect connection achieved through electronic devices, such as a connection achieved through resistors, inductors, capacitors or other electronic devices.

[0055] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection, an electrical connection, or communication with each other; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0056] Obviously, the embodiments described above are only some embodiments of the present application, rather than all embodiments. The preferred embodiments of the present application are given in the accompanying drawings, but they do not limit the patent scope of the present application. The present application can be implemented in many different forms. On the contrary, the purpose of providing these embodiments is to make the understanding of the disclosure of the present application more thorough and comprehensive. Although the present application is described in detail with reference to the aforementioned embodiments, for those skilled in the art, it is still possible to modify the technical solutions recorded in the aforementioned specific implementation methods, or to replace some of the technical features therein with equivalents. Any equivalent structure made using the contents of the specification and drawings of this application, directly or indirectly used in other related technical fields, is similarly within the scope of patent protection of this application.

Claims

1. A touch screen optical film without white edges, characterized in that: The touch screen optical film (1) without white edges comprises a rectangular film body (2), the edge of the film body (2) is provided with a square frame-shaped cut inner shrinkage edge (3), and the cut inner shrinkage edge (3) and the film body (2) are an integral structure.

2. The touch screen optical film without white edges according to claim 1, characterized in that: The width D of the cut inner shrinkage edge (3) is between 0.8 mm and 1.2 mm.

3. The touch screen optical film without white edges according to claim 2, characterized in that: The width D of the cut inner shrinkage edge (3) is 1 mm.

4. The touch screen optical film without white edges according to claim 1, characterized in that: A preset shrinkage groove (4) is provided between the cut inner shrinkage edge (3) and the membrane body (2).

5. The touch screen optical film without white edges according to claim 4, characterized in that: The shrinkage groove (4) is arc-shaped.

6. The touch screen optical film without white edges according to claim 4, characterized in that: The depth of the shrinkage groove (4) is between 0.1 mm and 0.5 mm.

7. The touch screen optical film without white edges according to claim 6, characterized in that: The depth of the shrinkage groove (4) is 0.3 mm.

8. The touch screen optical film without white edges according to claim 4, characterized in that: The shrinkage groove (4) is in the shape of an inverted trapezoid.

9. The touch screen optical film without white edges according to claim 8, characterized in that: The depth of the shrinkage groove (4) is between 0.1 mm and 0.5 mm.

10. The touch screen optical film without white edges according to claim 9, characterized in that: The depth of the shrinkage groove (4) is 0.3 mm.