Anti-warping insulating film assembly
By introducing a nylon filling layer and an anti-curl assembly of iron wire into the insulating film assembly, combining multi-layer insulation and thermal insulation structure, the problem of curling edges during insulating film is solved, and the stable adhesion and long-term use of the insulating film are achieved.
Patent Information
- Application Number
- CN202420754252.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-12
- Publication Date
- 2025-01-17
- Estimated Expiration
- 2034-04-12
AI Technical Summary
The insulating film is prone to curling edges when attached, which leads to easy falling off and affects the electrical insulation effect.
Design an anti-warping insulating film assembly, including the main insulating film, heat insulation layer, moisture-proof layer, secondary insulating film and anti-warping assembly. The inner cavity of the anti-warping assembly is filled with nylon filling layer and wire, and the top and bottom are provided with adhesives. The layer and release paper are shaped and positioned through nylon filling layers and wire to prevent curling edges, while using a multi-layer structure to provide insulation, heat insulation and moisture-proof effects.
Effectively prevent the insulating film assembly from curling, improve the adhesion stability and electrical insulation performance, extend the service life, and improve the efficiency of the insulating film assembly.
Smart Images

Figure CN222365434U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of insulating film components, in particular to an insulating film component that resists warping. Background Art
[0002] Insulating film is a thin film that can ensure good electrical insulation. This film should have very high resistivity and breakdown field strength, and the electronic structure is characterized by a large bandgap. In order to be used for high-frequency insulation, the material is also required to have low dielectric loss. There are two types of insulating films: inorganic and organic. Inorganic insulators are usually called dielectrics, and commonly used ones are silicon oxide, silicon nitride, aluminum oxide, and aluminum nitride; commonly used organic insulating film materials are polyimide, polyethylene, polyvinylidene fluoride, and polytetrafluoroethylene. Whether inorganic or organic insulators, they generally have the ability to polarize under the action of an external electric field. When used as an electrical insulating film, it is hoped that its dielectric constant is low to reduce dielectric loss.
[0003] When the insulating film is attached, it is easy to cause the edge to warp, which can easily cause the insulating film to fall off, thereby affecting the insulation effect.
[0004] Therefore, it is necessary to propose an anti-warping insulating film assembly to solve the above problems. Utility Model Content
[0005] The main purpose of the utility model is to provide an anti-warping insulating film component, which can effectively solve the problems in the background technology.
[0006] In order to achieve the above purpose, the technical solution adopted by the utility model is:
[0007] A warping-resistant insulating film assembly comprises an insulating film assembly body, wherein anti-warping assemblies are symmetrically fixedly connected in the middle of left and right sides of the insulating film assembly body, and the insulating film assembly body comprises a main insulating film, a first thermal insulation layer, a first moisture-proof layer, a first auxiliary insulating film, a second thermal insulation layer, a second moisture-proof layer and a second auxiliary insulating film.
[0008] Preferably, the inner cavities of the two anti-warping components are filled with a nylon filling layer, and iron wires are symmetrically fixedly connected in the middle of the inner cavities of the two anti-warping components.
[0009] Preferably, adhesive layers are symmetrically fixedly connected to the top and bottom of the insulating film assembly body, a first release paper is pasted to the top of the top adhesive layer, and a second release paper is pasted to the bottom of the bottom adhesive layer.
[0010] Preferably, the main insulating film is fixedly connected to the center of the inner cavity of the insulating film assembly body, the first thermal insulation layer is fixedly connected to the top of the main insulating film, the first moisture-proof layer is fixedly connected to the top of the first thermal insulation layer, and the first auxiliary insulating film is fixedly connected to the top of the first moisture-proof layer.
[0011] Preferably, the bottom of the main insulating film is fixedly connected to the top of the second thermal insulation layer, the bottom of the second thermal insulation layer is fixedly connected to the top of the second moisture-proof layer, and the bottom of the second moisture-proof layer is fixedly connected to the top of the second secondary insulating film.
[0012] Preferably, the thickness of the main insulating film is 0.6-0.9 mm, the thickness of the first thermal insulation layer and the second thermal insulation layer is 0.1-0.3 mm, the thickness of the first moisture-proof layer and the second moisture-proof layer is 0.1-0.3 mm, and the thickness of the first secondary insulating film and the second secondary insulating film is 0.2-0.5 mm.
[0013] Beneficial Effects
[0014] Compared with the prior art, the utility model has the following beneficial effects:
[0015] 1. The anti-warping insulating film component can have a certain shaping effect on the anti-warping component through the nylon filling layer and iron wire. At the same time, the iron wire and the nylon filling layer can also have a certain bending effect. When the insulating film component body is attached, the nylon filling layer and the iron wire can have a certain positioning effect on the insulating film component body, which can adapt to the shape of the attached object while preventing the insulating film component body from warping.
[0016] 2. The anti-warping insulating film assembly can tear off the first release paper and the second release paper so that the insulating film assembly body can be normally attached through the adhesive layer, and the main insulating film, the first auxiliary insulating film and the second auxiliary insulating film can achieve an insulating effect.
[0017] 3. The anti-warping insulating film assembly can achieve a certain thermal insulation effect on the insulating film assembly body by providing the first thermal insulation layer and the second thermal insulation layer, and can achieve a certain moisture-proof effect on the insulating film assembly body by providing the first moisture-proof layer and the second moisture-proof layer, thereby improving the use efficiency and service life of the insulating film assembly body. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a structural schematic diagram of the front side of the utility model;
[0019] Figure 2 It is a cross-sectional view of the anti-warping component of the utility model;
[0020] Figure 3 This is a schematic diagram of the structure of the inner cavity of the insulating film assembly body of the utility model;
[0021] Figure 4 This utility model Figure 3 Enlarged view of point A in the middle.
[0022] In the figure: 1. Insulating film component body; 2. Anti-warping component; 3. First release paper; 4. Nylon filling layer; 5. Iron wire; 6. Second release paper; 7. Adhesive layer; 8. Main insulating film; 9. First thermal insulation layer; 10. First moisture-proof layer; 11. First secondary insulating film; 12. Second thermal insulation layer; 13. Second moisture-proof layer; 14. Second secondary insulating film. DETAILED DESCRIPTION
[0023] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further described below in conjunction with specific implementation methods.
[0024] like Figure 1-4As shown, an anti-warping insulating film component comprises an insulating film component body 1, anti-warping components 2 are symmetrically fixedly connected in the middle of the left and right sides of the insulating film component body 1, the insulating film component body 1 comprises a main insulating film 8, a first heat insulation layer 9, a first moisture-proof layer 10, a first auxiliary insulating film 11, a second heat insulation layer 12, a second moisture-proof layer 13 and a second auxiliary insulating film 14, the inner cavities of the two anti-warping components 2 are filled with nylon filling layers 4, iron wires 5 are symmetrically fixedly connected in the middle of the inner cavities of the two anti-warping components 2, adhesive layers 7 are symmetrically fixedly connected to the top and bottom of the insulating film component body 1, and a first release paper 3 is pasted on the top of the top adhesive layer 7, The bottom of the bottom adhesive layer 7 is pasted with a second release paper 6, the main insulating film 8 is fixedly connected to the center of the inner cavity of the insulating film assembly body 1, the first thermal insulation layer 9 is fixedly connected to the top of the main insulating film 8, the first moisture-proof layer 10 is fixedly connected to the top of the first thermal insulation layer 9, the first auxiliary insulating film 11 is fixedly connected to the top of the first moisture-proof layer 10, the bottom of the main insulating film 8 is fixedly connected to the top of the second thermal insulation layer 12, the bottom of the second thermal insulation layer 12 is fixedly connected to the top of the second moisture-proof layer 13, the bottom of the second moisture-proof layer 13 is fixedly connected to the top of the second auxiliary insulating film 14, the thickness of the main insulating film 8 is 0.6-0.9mm, the first thermal insulation layer 9 is fixedly connected to the top of the main insulating film 8, the first moisture-proof layer 10 is fixedly connected to the top of the first moisture-proof layer 10 ... moisture-proof layer 11 is fixedly connected to the top of the first moisture-proof layer 10, the first moisture-proof layer 11 is fixedly connected to the top of the first moisture-proof layer 10, the first moisture-proof layer The thickness of the first layer 9 and the second heat insulation layer 12 is 0.1-0.3mm, the thickness of the first moisture-proof layer 10 and the second moisture-proof layer 13 is 0.1-0.3mm, and the thickness of the first secondary insulating film 11 and the second secondary insulating film 14 is 0.2-0.5mm. The nylon filling layer 4 and the iron wire 5 can be set to prevent the anti-warping component 2 from having a certain shaping effect. At the same time, the iron wire 5 and the nylon filling layer 4 can also have a certain bending effect. When the insulating film component body 1 is attached, the nylon filling layer 4 and the iron wire 5 can have a certain positioning effect on the insulating film component body 1, which can adapt to the shape of the attached object and prevent the insulating film component from warping. The main body 1 has a warping phenomenon. By tearing off the first release paper 3 and the second release paper 6, the insulating film component main body 1 can be normally attached through the adhesive layer 7. The main insulating film 8, the first auxiliary insulating film 11 and the second auxiliary insulating film 14 can achieve an insulation effect. The first thermal insulation layer 9 and the second thermal insulation layer 12 can achieve a certain thermal insulation effect on the insulating film component main body 1. The first moisture-proof layer 10 and the second moisture-proof layer 13 can achieve a certain moisture-proof effect on the insulating film component main body 1, thereby improving the use efficiency and service life of the insulating film component main body 1.
[0025] It should be noted that the utility model is an anti-warping insulating film component. When in use, the first release paper 3 and the second release paper 6 are removed, and the insulating film component body 1 is attached to the object through the adhesive layer 7. After attachment, the insulating film component body 1 is fit-treated according to the shape of the object. At this time, the nylon filling layer 4 and the iron wire 5 in the inner cavity of the anti-warping component 2 will adapt to the shape of the object and move, so that the insulating film component body 1 can be positioned to prevent it from warping. When using the insulating film component body 1, it can have an insulating effect through the first secondary insulating film 11, the second secondary insulating film 14 and the main insulating film 8, can have a heat insulating effect through the first thermal insulation layer 9 and the second thermal insulation layer 12, and can have a moisture-proof effect through the first secondary insulating film 11 and the second moisture-proof layer 13.
[0026] The above shows and describes the basic principle and main features of the utility model and the advantages of the utility model. Those skilled in the art should understand that the utility model is not limited by the above embodiments. The above embodiments and descriptions are only for explaining the principle of the utility model. Without departing from the spirit and scope of the utility model, the utility model may have various changes and improvements, which fall within the scope of the utility model to be protected. The scope of protection claimed by the utility model is defined by the attached claims and their equivalents.
Claims
1. An anti-warping insulating film assembly, comprising an insulating film assembly body (1), characterized in that: The anti-warping components (2) are symmetrically fixedly connected in the middle of the left and right sides of the insulating film component body (1), and the insulating film component body (1) comprises a main insulating film (8), a first heat insulation layer (9), a first moisture-proof layer (10), a first auxiliary insulating film (11), a second heat insulation layer (12), a second moisture-proof layer (13) and a second auxiliary insulating film (14).
2. The anti-warping insulating film assembly according to claim 1, characterized in that: The inner cavities of the two anti-warping components (2) are both filled with a nylon filling layer (4), and iron wires (5) are symmetrically fixedly connected in the middle of the inner cavities of the two anti-warping components (2).
3. The anti-warping insulating film assembly according to claim 1, characterized in that: The top and bottom of the insulating film assembly body (1) are symmetrically fixedly connected with an adhesive layer (7), the top of the adhesive layer (7) is adhered with a first release paper (3), and the bottom of the adhesive layer (7) is adhered with a second release paper (6).
4. The anti-warping insulating film assembly according to claim 1, characterized in that: The main insulating film (8) is fixedly connected to the center of the inner cavity of the insulating film assembly body (1), the first thermal insulation layer (9) is fixedly connected to the top of the main insulating film (8), the first moisture-proof layer (10) is fixedly connected to the top of the first thermal insulation layer (9), and the first auxiliary insulating film (11) is fixedly connected to the top of the first moisture-proof layer (10).
5. The anti-warping insulating film assembly according to claim 1, characterized in that: The bottom of the main insulating film (8) is fixedly connected to the top of the second thermal insulation layer (12), the bottom of the second thermal insulation layer (12) is fixedly connected to the top of the second moisture-proof layer (13), and the bottom of the second moisture-proof layer (13) is fixedly connected to the top of the second auxiliary insulating film (14).
6. The anti-warping insulating film assembly according to claim 1, characterized in that: The thickness of the main insulating film (8) is 0.6-0.9 mm, the thickness of the first thermal insulation layer (9) and the second thermal insulation layer (12) is 0.1-0.3 mm, the thickness of the first moisture-proof layer (10) and the second moisture-proof layer (13) is 0.1-0.3 mm, and the thickness of the first secondary insulating film (11) and the second secondary insulating film (14) is 0.2-0.5 mm.