METHOD FOR SEMICONDUCER MANUFACTURING
Patent Information
- Application Number
- DE102017120571
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2017-08-30
- Filing Date
- 2017-09-07
- Publication Date
- 2024-10-02
- Estimated Expiration
- 2037-09-07
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
backgroundFinFET devices have become mainstream in semiconductor manufacturing to achieve ever smaller device structures and higher circuit performance. There are many challenges in manufacturing these small FinFET devices in an integrated circuit (IC). For example, when manufacturing contact elements in FinFET devices, contact depth variation due to topography on the wafer has become a problem. In particular, semiconductor fins are mostly higher than isolation structures that insulate the fins. When contact elements (which have metals) are manufactured on top of the fins as well as on the isolation structures, some of the contact elements are higher than others. Over time, these non-uniform contact elements can skew and push adjacent circuit elements (e.g., gate structures) causing them to bend, which could lead to circuit defects. Another problem associated with contact manufacturing is that some vias are deep and narrow, and it may be difficult for the contact elements to completely fill these vias, leaving voids under the contact elements. These voids may be difficult to detect at the manufacturing stage, but they can cause the circuit to short or open over time. Therefore, improvements in the contact manufacturing process are desirable.US 2016 / 0 064 327 A1 discloses a semiconductor device comprising: a substrate; a first metal gate on the substrate; a first hard mask on the first metal gate; an interlayer dielectric (ILD) layer on and around the first metal gate; and a patterned metal layer embedded in the ILD layer, wherein the upper surface of the patterned metal layer is lower than the upper surface of the first hard mask. Further prior art is known from US 2014 / 0 239 354 A1 and US 2002 / 0 081 852 A1.The invention is defined in the claims.Short description of the drawingsAspects of the present invention can best be understood by reference to the following detailed description when taken in conjunction with the accompanying drawings. It should be noted that, in accordance with standard practice in the industry, various elements are not drawn to scale. Rather, for the sake of clarity of discussion, the dimensions of the various elements may be increased or decreased as desired.1A, 1B, 1C and 1D are flow diagrams of a method of manufacturing a semiconductor device according to various aspects of the present invention. 2 is a perspective view of a portion of a semiconductor device fabricated according to the method of FIGS. 1A-1D, according to one embodiment.3, 4, 5, 6, 7, 8, 9 and 10 are cross-sectional views of a portion of the semiconductor device of FIG. 2 at intermediate stages of fabrication according to the method of FIGS. 1A, 1B and 1C, according to one embodiment.11, 12, 13, 14, 15, 16 and 17 are cross-sectional views of a portion of the semiconductor device of FIG. 2 at intermediate stages of fabrication according to the method of FIGS. 1A and 1D, according to one embodiment.Detailed descriptionThe present invention relates generally to semiconductor devices and methods of manufacturing the same. More particularly, the present invention relates to contact manufacturing methods in semiconductor manufacturing, particularly in the manufacture of FinFET devices. In accordance with some aspects of the present invention, contact elements such as source / drain (S / D) contacts, local via contacts, and dome contacts are manufactured to have approximately the same depth across a large area of a wafer. These contact elements tend to maintain their shape and location over time, thereby increasing circuit reliability. In addition, the provided article reduces the aspect ratio (ratio of depth to width) of contact holes, effectively reducing the risk of voids forming beneath the contact elements.1A, 1B, 1C, and 1D show flow diagrams of a method 10 for manufacturing a semiconductor device 100 according to various aspects of the present invention. In particular, FIGS. 1A and 1C show one embodiment of the method 10, and FIGS. 1A and 1D show an alternative embodiment of the method 10. FIG. 1B shows a flow diagram of a method that may be part of the method 10. The method 10 is merely an example and is not intended to limit the present invention beyond what is expressly set forth in the claims. Additional steps may be provided before, during, and after the method 10, and some of the steps described may be replaced, omitted, or shifted in other embodiments of the method. In the following discussion, the method 10 will first be described with reference to FIGS. 1A, 1B, 1C and 2 through 10 and will then be described with reference to FIGS. 1A, 1D and 11 through 17. FIG. 2 shows the semiconductor device 100 at an intermediate stage of manufacture in a perspective view, and FIGS. 3 through 17 show the semiconductor device 100 at intermediate stages of manufacture in a cross-sectional side view of FIG. 2.The semiconductor device 100 is illustrative and does not necessarily limit embodiments of the present invention to a number of devices, a number of regions, or a configuration of structures or regions. Moreover, the semiconductor device 100 shown in FIGS. 2 to 17 may be an intermediate device manufactured during processing of an IC or a portion thereof and may include: SRAM and / or logic circuits (SRAM: static random access memory), passive components such as resistors, capacitors and inductors, and active components such as p-type field effect transistors (PFETs), n-type FETs (NFETs), multi-gate FETs such as FinFETs, metal oxide semiconductor field effect transistors (MOSFETs), CMOS transistors (CMOS: complementary metal oxide semiconductor), bipolar transistors, high voltage transistors, high frequency transistors, other memory cells, and combinations thereof.In step 12, the method 10 (FIG. 1A) provides a device structure (or device) 100 shown in FIGS. 2 and 3. In FIG. 2, the device 110 includes a substrate 102, one or more fins 104 extending from the substrate 102, an isolation structure 106 separating the fins 104 from each other, and various gate structures 108a, 108b, 108c, 108d, and 108e.Substrate 102 is a silicon substrate in the present embodiment. In alternative embodiments, substrate 102 comprises another elemental semiconductor such as germanium; a compound semiconductor such as silicon carbide, gallium arsenide, indium arsenide, and indium phosphide; or an alloy semiconductor such as silicon germanium carbide, gallium arsenophosphide, and gallium indium phosphide. In some embodiments, substrate 102 may be a silicon-on-insulator (SOI) substrate, may be strained to improve performance, and may include epitaxial regions, isolation regions, doped regions, and / or other suitable features and layers.The fins 104 comprise one or more semiconductor materials, such as silicon, germanium, silicon germanium, silicon carbide, gallium arsenide, indium arsenide, indium phosphide, silicon germanium carbide, gallium arsenophosphide, and gallium indium phosphide. The fins 104 are doped with dopants suitable for fabricating FinFETs. For example, the fins 104 may be doped with one or more p-dopants, such as boron or indium, or with one or more n-dopants, such as phosphorus or arsenic. The fins 104 may include doped regions, such as lightly doped regions and heavily doped regions, and may include epitaxially grown materials.In the present embodiment, the device 100 further comprises S / D features 120 (FIG. 3). In one embodiment, the S / D features 120 are fully embedded in the fin 104, such as heavily doped S / D regions. In another embodiment, the S / D features 120 are partially embedded in the fin 104 and protrude beyond the fin 104, such as epitaxially grown semiconductor material with suitable dopants. The S / D features 120 may be silicided or germanosilicided. In the present embodiment, two S / D features 120 are shown adjacent to the gate structure 108c (FIG. 3).The fins 104 may be formed using suitable processes, such as photolithographic and etching processes. For example, the photolithographic process may include the steps of: forming a photoresist layer (resist) over the substrate 102; exposing the resist to form a pattern; performing a post-exposure bake; and developing the resist to form a masking member comprising the resist. The masking member is then used to etch recesses into the substrate 102 such that the fins 104 remain on the substrate 102. The etching process may include dry etching, wet etching, reactive ion etching (RIE), and / or other suitable processes. For the dry etching process, oxygen-containing gases, fluorine-containing gases (e.g. CF4, SF6, CH2F2, CHF3and / or C2F6), chlorine-containing gases (e.g. Cl2, CHCl3, CCl4and / or BCl3), bromine-containing gases (e.g. HBr and / or CHBr3), iodine-containing gases, other suitable gases and / or plasmas and / or combinations thereof can be used. The wet etching process can, for example, involve etching in dilute hydrofluoric acid (DHF); potassium hydroxide (KOH) solution; ammonia; a solution containing hydrofluoric acid (HF), nitric acid (HNO3) and / or acetic acid (CH3COOH); or in another suitable wet etching medium. The fins 104 may also be formed using double-patterning lithography (DPL) processes. Numerous other embodiments of methods for forming the fins 104 may be suitable.The isolation structure 106 may comprise silicon oxide, silicon nitride, silicon oxynitride, fluorosilicate glass (FSG), a low-k dielectric material, and / or another suitable isolation material. The isolation structure 106 may comprise shallow trench isolation (STI) features in some embodiments. The isolation structure 106 may be formed by etching trenches in the substrate 102, e.g., as part of the manufacturing process for the fins 104. The trenches are then filled with isolation material, followed by chemical mechanical planarization (CMP). Other isolation structures are also possible, such as field oxide, local oxidation of silicon (LOCOS), and / or other suitable structures. The isolation structure 106 may be a multi-layer structure and may, for example, have one or more thermal oxide capping layers.In the present embodiment, the fins 104 are higher than the isolation structure 106. In other words, the top of the fins 104 is higher than the top of the isolation structure 106 along the Z direction. This can be manufactured, for example, by etching back the isolation structure 106 after the fins 104 are manufactured or by epitaxially growing the fins 104 from the trenches in the isolation structure 106.The gate structures 108a-108e are each a multilayer structure (FIG. 3). In the present embodiment, the gate structures 108a-108e each include a dielectric layer 110, a gate electrode layer 112, a first hard mask (HM) layer 114, a second HM layer 116, and a spacer layer 118 as the sidewall of the respective gate structure. The dielectric layer 110 may comprise silicon oxide or silicon oxynitride and may be formed by chemical oxidation, thermal oxidation, atomic layer deposition (ALD), chemical vapor deposition (CVD), and / or other suitable methods. The gate electrode layer 112 may be a polysilicon layer that may be formed by suitable deposition methods such as low pressure chemical vapor deposition (LPCVD) and plasma enhanced chemical vapor deposition (PECVD). The HM layer 114 may comprise a nitride such as silicon nitride, silicon carbonitride, silicon oxynitride, and silicon oxycarbonitride. The HM layer 116 may comprise an oxide such as silicon oxide. The HM layers 114 and 116 may each be formed by CVD, PVD, or ALD. The spacer layer 118 may have a single layer or a multilayer structure. The spacer layer 118 may comprise a dielectric material such as silicon oxide, silicon nitride, silicon oxynitride, another dielectric material, or a combination thereof. In one example, the spacer layer 118 is formed by performing a protective deposition of a first dielectric layer (e.g., a SiO2 layer having a consistent thickness) as a cap layer over the device 100 and a second dielectric layer (e.g., a SiN layer) as a main D-shaped spacer over the first dielectric layer, and then performing an anisotropic etch to remove portions of the dielectric layers to form the spacer layer 118.The gate structures 108a to 108e may have different widths depending on their respective function. For example, the gate structure 108b is wider (along the X direction) than the other gate structures. In addition, some gate structures (e.g., 108b and 108c) are arranged above the fins 104, and some other gate structures (e.g., 108a, 108d, and 108e) are arranged above the isolation structure 106. The gate structures 108a to 108e may be designed to have different functions. For example, the gate structure 108c is designed to be a gate terminal (or a placeholder for a gate terminal) of a FinFET. For example, the gate structure 108b may be designed as a local interconnect by connecting the S / D feature 120 to another S / D feature or a gate (not shown) using a dome contact. For example, the gate structures 108a, 108d, and 108e may each be designed as an interconnect or simply as a dummy gate for device uniformity. When a gate structure is disposed over the fin 104, it encloses the fin 104 on three sides, i.e., on the top and sidewalls of the fin 104. FIG. 2 shows the gate structures 108b and 108c enclosing the top and one sidewall of the fin 104, with the other sidewall of the fin 104 cut out and not shown.Various trenches in the device 100 are provided (or defined) by the various structures 104, 106, and 108a-108e. In the illustrated embodiment, trenches 109a, 109b, 109c, and 109d are provided. In particular, adjacent sidewalls of the gate structures 108a-108e (and in the case of trench 109a, together with sidewalls of the fin 104) provide sidewalls for the trenches 109a-d, while the top of the fins 104 and the top of the isolation structure 106 provide the bottom for the trenches 109a-d. Note that the trenches 109a-d have different depths in the present embodiment because the fins 104 are higher than the isolation structure 106. As the feature size of the transistors decreases, the aspect ratio of the trenches 109a-d, which is defined by the ratio of their height (along the Z direction) to their width (along the X direction), becomes larger, making these trenches deep and narrow. This is particularly evident in the trenches 109a-d having the isolation structure 106 as their bottom.These trenches 109a-d may present two problems for subsequent processing that involves fabricating contact elements that extend into the bottom of the trenches. First, the contact elements in the trenches would have different depths while their tops are at the same level. For example, a contact element in trench 109d would have a greater depth (or be longer) than a contact element in trench 109c. Over time, the longer contact elements may tilt and may press against adjacent gate structures, causing circuit failure. Second, a deep and narrow trench, such as trenches 109a and 109d, may be difficult to fill with metal materials, creating voids in the trench. These voids may cause the circuit to open or short over time. The present invention provides methods for addressing these problems.In step 14, in the method 10 (FIG. 1A), a contact etch stop layer (CESL) 122 is formed over the various structures of the device 100. In FIG. 4, the CESL 122 is formed over the tops of the fin 104, the isolation structure 106, the gate structures 108a-108e, and the S / D features 120. In one embodiment, the CESL 122 comprises a dielectric material such as silicon nitride (SiN), silicon oxide (SiO2), silicon oxynitride (SiON), and / or other materials. The CESL 122 may be formed using one or more processes such as plasma enhanced chemical vapor deposition (PECVD) and ALD, and / or other suitable deposition or oxidation processes. In the present embodiment, a top portion 122a of the CESL 122 on the gate structures 108a-108e is fabricated to be thicker than another portion 122b of the CESL 122 on sidewalls of the gate structures 108a-108e. In an alternative embodiment (shown in FIG. 11, discussed later), the CESL 122 is fabricated to be conformal, i.e., to have approximately the same thickness throughout the device 100. Other thickness profiles are also intended to be within the scope of the present invention.1B shows a flow diagram of an embodiment of step 14 in which the top portion 122a is formed which is thicker than the sidewall portion 122b. In FIG. 1B, step 14 in this embodiment comprises steps 14a, 14b, and 14c. In step 14a, a conformal layer 122 of a dielectric material is deposited, for example by ALD. The dielectric material is deposited substantially uniformly over the top and sidewalls of the gate structures 108a-108e, the top and sidewalls of the fins 104, and the top of the isolation structure 106. In step 14b, the conformal layer is treated with a plasma, such as argon plasma and / or nitrogen plasma. In a specific example, the plasma treatment is directed, i.e. i.e., the top portion 122a of the conformal layer 122 receives a stronger plasma treatment than the sidewall portion 122b of the conformal layer 122. In step 14c, a chemical solution is applied to the plasma treated conformal layer 122. The chemical solution dissolves or etches the sidewall portion 122b at a higher rate than the top portion 122a. This makes the top portion 122a thicker than the sidewall portion 122b. In one example, the chemical solution is dilute hydrofluoric acid (DHF). The special profile (the top is thicker than the sidewall) of the CESL 122 offers several advantages. First, the top portion 122a serves as a CMP stop in a subsequent CMP process. If it is too thin, it is not effective. In some embodiments, the top portion 122a is at least 4 nm thick. Second, the existing sidewall portion 122b further increases the aspect ratio of the trenches 109a-d, which is undesirable. Therefore, the sidewall portion 122b should be as thin as possible. In some embodiments, the sidewall portion 122b (or a portion thereof) is removed and the spacer layer 118 is exposed.In step 16, in the method 10 (FIG. 1A), an interlayer dielectric (ILD) layer 124 is deposited over the first CESL 122. In FIG. 5, the ILD layer 124 fills the various trenches and covers the gate structures 108a-108e, the fins 104, and the isolation structure 106. In one embodiment, the ILD layer 124 is deposited using flowable chemical vapor deposition (FCVD). For example, a flowable material (such as a liquid compound) is deposited on the device 100 and fills the trenches 109a-d (FIG. 4). Then, one or more annealing processes are performed to convert the flowable material to a solid material. In an alternative embodiment, the ILD layer 124 may be deposited using other deposition techniques, such as PECVD. The ILD layer 124 may comprise materials such as tetraethyl orthosilicate (TEOS) oxide, undoped silicate glass, or doped silicon oxide such as borophosphosilicate glass (BPSG), silica glass (FSG), phosphosilicate glass (PSG), borosilicate glass (BSG), a low-k dielectric material, and / or other suitable dielectric materials. In the present embodiment, in step 16, an oxide layer 126 is further deposited over the ILD layer 124, for example by PECVD.In step 17, in method 10 (FIG. 1A), a CMP process is performed on the ILD layer 124. In the present embodiment, the CMP process first removes the oxide layer 126 and then recesses the ILD layer 124 until a top surface of the CESL 122 is exposed, for example, as shown in FIG. 6. The top portion 122a serves as a CMP stop in the present embodiment.In step 18, in the method 10 (FIG. 1A), the ILD layer 124 is recessed with an etch process. The etch process is a dry etch in one embodiment. The etch process is adapted to selectively etch the ILD layer 124 but not (or only insignificantly) etch the CESL 122. In FIG. 7, the ILD layer 124 above the fins 104 is removed, and the ILD layer 124 above the isolation structure 106 is recessed such that its top surface 124' is approximately at the same level as the top surface 104' of the fins 104. One purpose of providing the ILD layer 124 is to provide approximately the same depth in the trenches 109a-d so that contact elements formed in the trenches, if any, have approximately the same depths. Therefore, the top surface 124' should be approximately level with (approximately at the same level as) the top surface 104'. In one embodiment, the etching process is timed to achieve the specific depth of etching. In the present embodiment, the method 10 includes forming some contact elements that extend into the S / D features 120. By providing the ILD layer 124 over the S / D features 120, the contact elements may be prevented from properly electrically contacting the S / D features 120. Therefore, in the present embodiment, the ILD layer 124 in the trenches 109a-d is completely removed, for example by performing an overetch on the ILD layer 124. This overetch also recesses the ILD layer 124 in the trenches 109a and 109d, so that the top surface 124' may be slightly below the top surface 104'. In some embodiments, the top surface 124' may be a few nanometers, such as less than or equal to 15 nm, below the top surface 104'.In step 20, in method 10 ( FIG. 1C ), a second CESL 128 is formed over the first CESL 122 and the ILD layer 124. In FIG. 8, in the present embodiment, the CESL 128 is formed to be a conformal layer and to cover the topography of the device 100. The CESL 128 comprises a dielectric material, such as silicon nitride (SiN), silicon oxide (SiO2), silicon oxynitride (SiON), and / or other materials. The CESL 128 may be formed using one or more processes, such as plasma enhanced chemical vapor deposition (PECVD) and ALD, and / or other suitable deposition or oxidation processes. In various embodiments, the CESL 122 and the CESL 128 may comprise the same or different dielectric materials. In the present embodiment, the combined thickness of the CESL 122 and the CESL 128 on the sidewalls of the gate structures 108a-108e is designed to be as small as possible so that the aspect ratio of the trenches 109a-d is in a desired range.In step 22, in the method 10 (FIG. 1C), a second ILD layer 130 is deposited over the second CESL 128. In FIG. 9, the ILD layer 130 fills the trenches and covers the topography of the device 100. In one embodiment, the ILD layer 130 is deposited using the FCVD process, which includes depositing a flowable material and annealing the flowable material. In another embodiment, the ILD layer 130 may be deposited using other deposition techniques, such as PECVD. The ILD layer 130 may comprise materials such as tetraethyl orthosilicate (TEOS) oxide, undoped silicate glass, or doped silicon oxide such as borophosphosilicate glass (BPSG), silica glass (FSG), phosphosilicate glass (PSG), borosilicate glass (BSG), a low-k dielectric material, and / or other suitable dielectric materials. Moreover, the ILD layers 124 and 130 may comprise the same or different dielectric materials.In step 24, the method 10 (FIG. 1C) forms contact elements 136a, 136b, 136c, and 136d that extend into the second ILD layer 130, as shown in FIG. 10. This includes various processes in the present embodiment, which are discussed below.First, in step 24, one or more CMP processes are performed to recess the ILD layer 130, the CESL 128, the CESL 122, and the spacer layer 118 and remove the HM layers 114 and 116. The one or more CMP processes expose the gate electrode layer 112.Second, in step 24, one or more etch processes are performed to selectively remove the gate electrode layer 112 without etching the ILD layer 130, the CESL 128, the CESL 122, and the spacer layer 118. In some embodiments, the one or more etch processes also remove the dielectric layer 110. This creates trenches between each pair of spacer layers 118. Then, in step 24, a gate dielectric layer 110' and a gate electrode layer 112' are deposited into the trenches. The gate dielectric layer 110' may be a high-k dielectric layer and may be comprised of, for example, hafnium oxide (HfO2), zirconium oxide (ZrO2), lanthanum oxide (La2O3), titanium oxide (TiO2), yttrium oxide (Y2O3), strontium titanate (SrTiO3), other suitable metal oxides, or combinations thereof, and may be formed by ALD and / or other suitable methods. The gate electrode layer 112' may be a p-work function metal layer or an n-work function metal layer. The p-work function metal layer comprises a metal selected from the group consisting of titanium nitride (TiN), tantalum nitride (TaN), ruthenium (Ru), molybdenum (Mo), tungsten (W), and platinum (Pt), or combinations thereof, among others. The n-type work function metal layer comprises a metal selected from the group consisting of titanium (Ti), aluminum (Al), tantalum carbide (TaC), tantalum carbide nitride (TaCN), and tantalum silicon nitride (TaSiN), among others, or combinations thereof. The p-type or n-type work function metal layer may comprise a plurality of layers and may be deposited by CVD, PVD, and / or another suitable method. The gate electrode layer 112' may be a metal fill layer (or a bulk metal layer) comprising aluminum (Al), tungsten (W), cobalt (Co), copper (Cu), and / or other suitable materials, and may be formed by CVD, PVD, plating, and / or other suitable method. In step 24, a CMP process may also be performed to remove excess material of the gate electrode layer 112'.Third, in step 24, a third CESL 132 is deposited on the ILD layer 130, the CESL 128, the CESL 122, the spacer layer 118, and the gate electrode 112'. The CESL 132 may comprise silicon nitride (SiN), silicon oxide (SiO2), silicon oxynitride (SiON), and / or other materials, and may be formed using one or more processes, such as PECVD and ALD, and / or other suitable processes. Then, in step 24, another ILD layer 134 is deposited over the CESL 132. The ILD layer 134 may comprise materials such as tetraethyl orthosilicate (TEOS) oxide, undoped silicate glass, or doped silicon oxide such as borophosphosilicate glass (BPSG), silica glass (FSG), phosphosilicate glass (PSG), borosilicate glass (BSG), a low-k dielectric material, and / or other suitable dielectric materials. The ILD layer 134 may be deposited using FCVD, PECVD, or other suitable methods.Fourth, in step 24, contact holes are formed that pass through the ILD layer 134, the CESL 132, the ILD layer 130, the CESL 128, and the CESL 122. Above the top of the fins 104, the contact holes expose a portion of the S / D features 120. Above the top of the isolation structure 106, the contact holes expose an upper portion of the ILD layer 124. Since the top 124' is approximately level with or top 104' ( FIG. 7 ), the contact holes above the fins 104 and above the isolation structure 106 have approximately the same depth as measured from the top of the ILD layer 134.Finally, in step 24, one or more conductive materials are deposited into the contact holes to form the contact elements 136a-136d. The contact elements 136a-136d each include a barrier layer and a metal fill layer above the barrier layer. The barrier layer may include a conductive nitride such as TaN or TiN, and the metal fill layer may include aluminum (Al), tungsten (W), copper (Cu), cobalt (Co), combinations thereof, or other suitable material. The barrier layer and the metal fill layer may each be formed using CVD, PVD, plating, or other suitable methods. In one embodiment, silicidation or germanosilicidation may be performed below the barrier layer and above the S / D features 120. Advantageously, since the contact elements 136a-136d have approximately the same depth and size, they tend to maintain their shapes and positions over time without tilting. And because the contact holes above the isolation structure 106 are relatively shallower than they would be without the ILD layer 124, they can be relatively more easily completely filled with the contact elements 136a-136d, reducing the risk of voids forming under the contact elements.The method 10 may proceed to further steps to complete the fabrication of the device 100. For example, in the method 10, one or more dielectric layers may be formed on the ILD layer 134, gate pins (vias) may be formed over the gate electrodes 112', and metal interconnects may be formed for connecting terminals of various transistors to form an IC.1A and 1D show a flow diagram of another embodiment of the method 10, which is described below in connection with FIGS. 11 to 17.In step 12, the method 10 (Fig. 1A) provides a device structure (or device) 100 shown in Figs. 2 and 3. This has already been described above.In step 14, in the method 10 (FIG. 1A), a contact etch stop layer (CESL) 122 is formed over the various structures of the device 100, as shown in FIG. 11. In contrast to the embodiment shown in FIG. 4, the CESL 122 in FIG. 11 is substantially conformal, i.e., its top portion 122a has approximately the same thickness as its sidewall portion 122b, and it may be formed by ALD. The other aspects of the CESL 122 have already been described with reference to FIG. 4.In step 16, the process 10 (FIG. 1A) deposits an interlayer dielectric (ILD) layer 124 over the CESL 122, as shown in FIG. 12. In step 16, an oxide layer 126 may further be deposited over the ILD layer 124. The materials and deposition methods for layers 124 and 126 have already been described with reference to FIG. 5.In step 17, the method 10 (FIG. 1A) performs a CMP process to remove the oxide layer 126 and recess the ILD layer 124, thereby exposing the CESL 122.In step 18, in the method 10 (FIG. 1A), the ILD layer 124 is recessed using an etching process, such as a dry etching process. The etching process is adapted to selectively etch the ILD layer 124, but not (or only insignificantly) etch the CESL 122. In FIG. 13, the ILD layer 124 above the fins 104 is removed, and the ILD layer 124 above the isolation structure 106 is recessed such that its top surface 124' is approximately at the same level as the top surface 104' of the fins 104. The top surface 124' may be slightly lower than the top surface 104' in some embodiments by overetching, as already explained with reference to FIG. 7.In step 19, in method 10 (FIG. 1D), the CESL 122 is recessed. In FIG. 14, in step 19, the CESL 122 is removed from the trenches 109b and 109c, and the CESL 122 is removed from the trenches 109a and 109d until it is at or below the top surface 124'. Step 19 includes an etch process adapted to selectively remove the material of the CESL 122 without substantially removing the HM layer 116, the spacer layer 118, the fins 104, the S / D features 120, and the ILD layer 124. In one embodiment, the CESL 122 comprises silicon nitride, the HM layer 116 comprises silicon oxide, the spacer layer 118 comprises silicon oxynitride, silicon carbonitride, silicon oxycarbonitride, or silicon nitride (different from the material of the CESL 122), and the S / D features 120 comprise silicon doped with phosphorus. Furthermore, in this embodiment, in step 19, an etchant comprising phosphoric acid (H3PO4) is applied. The phosphoric acid etches the CESL 122 much faster than the HM layer 116, the spacer layer 118, the ILD layer 124, the fins 104, and the S / D features 120. In some embodiments, some loss of the various features 116, 118, 124, 104, and 120 during the etching process is acceptable.In step 20, the method 10 (FIG. 1D) forms a CESL 128 over the gate structures 108a-108e, the fins 104, the S / D features 120, the CESL 122, and the ILD layer 124, as shown in FIG. 15. The other aspects of step 20 have already been described with reference to FIG. 8.In step 22, in the method 10 (FIG. 1D), an ILD layer 130 is deposited over the CESL 128, and the ILD layer 130 fills the trenches 109a-d (FIG. 15), as shown in FIG. 16. The other aspects of step 22 have already been described with reference to FIG. 9.In step 24, the method 10 (FIG. 1D) forms contact elements 136a, 136b, 136c and 136d that extend into the second ILD layer 130, as shown in FIG. 17. In FIG. 17, the contact elements 136a through 136d pass through the ILD layer 134, the CESL 132, the ILD layer 130 and the CESL 128. The contact elements 136b and 136c electrically contact the S / D structure elements 120 via the fins 104. In this embodiment, the contact elements 136a and 136d come into contact with the ILD layer 124 via the isolation structure 106. The other aspects of step 24 have already been discussed with reference to FIG. 10.Some or more embodiments of the present invention, which are not intended to be limiting, provide numerous advantages for a semiconductor device and its manufacturing method. For example, embodiments of the present invention produce contact elements that have approximately the same depth (and height) above a fin and above an isolation structure, even though the fin and the isolation structure have different heights. As a result, these contact elements do not have as severe tilt and bend defects as contact elements with very different heights. In addition, embodiments of the present invention reduce the aspect ratio of trenches located above an isolation structure, which effectively reduces the risk of voids forming at the bottom of the trenches after contact is made. In addition, embodiments of the present invention can be easily integrated into existing semiconductor manufacturing processes.In an exemplary aspect, the present invention is directed to a method of semiconductor fabrication. The method includes providing a device structure having an isolation structure, a fin adjacent to the isolation structure and higher than the isolation structure, and gate structures over the fin and the isolation structure, wherein the isolation structure, the fin, and the gate structures define a first trench over the fin and a second trench over the isolation structure. The method further includes the steps of: forming a first contact etch stop layer (CESL) over the gate structures, the fin, and the isolation structure; depositing a first interlayer dielectric (ILD) layer over the first CESL and filling the first and second trenches; and recessing the first ILD layer such that it is removed in the first trench and recessed in the second trench to a level approximately level with a top surface of the fin.In one embodiment of the method, the first CESL is thicker on top of the gate structures than on sidewalls of the gate structures. In one embodiment, the method further comprises the steps of: forming a second CESL over the first CESL in the first trench and over the first CESL and the first ILD layer in the second trench after recessing the first ILD layer; and depositing the second ILD layer over the second CESL and filling remaining gaps of the first and second trenches. In another embodiment, the method comprises forming a first contact element extending into the second ILD layer in the first trench and a second contact element extending into the second ILD layer in the second trench. In one embodiment of the method, the second CESL is conformal.In one embodiment, fabricating the first CESL includes the steps of: depositing a conformal layer comprising a dielectric material over the gate structures, the fin, and the isolation structure; treating the conformal layer with a plasma such that first portions of the conformal layer on top of the gate structures receive a stronger plasma treatment than second portions of the conformal layer on the sidewalls of the gate structures; and applying to the conformal layer a chemical solution that dissolves the second portions faster than the first portions. In another embodiment, the dielectric material comprises silicon nitride, the plasma uses argon gas or nitrogen gas, and the chemical solution comprises dilute hydrofluoric acid (DHF).In one embodiment, the method further comprises, after recessing the first ILD layer, recessing the first CESL so that it is removed from the first trench and removed from the second trench above the first ILD layer. In another embodiment, the method further comprises the steps of: forming a second CESL on sidewalls of the first and second trenches after recessing the first CESL; and depositing a second ILD layer above the second CESL and filling remaining gaps of the first and second trenches. Furthermore, the method may comprise forming a first contact element extending into the second ILD layer in the first trench and a second contact element extending into the second ILD layer in the second trench.In another exemplary aspect, the present invention is directed to a method of semiconductor manufacturing. The method includes providing a device structure having a substrate, a fin extending from the substrate, an isolation structure over the substrate adjacent to the fin and lower than the fin, and gate structures over the fin and the isolation structure. The fin, the isolation structure, and the gate structures define a first trench over the fin and a second trench over the isolation structure. The method further includes forming a first contact etch stop layer (CESL) over the gate structures, the fin, and the isolation structure, wherein the first CESL is thicker on top of the gate structures than on sidewalls of the gate structures. The method further includes the steps of: depositing a first interlayer dielectric (ILD) layer over the first CESL and filling the first and second trenches; and recessing the first ILD layer such that it is removed in the first trench and recessed in the second trench to a level approximately as low as a top surface of the fin.In one embodiment, the method further comprises forming a second CESL over the first CESL in the first trench and over the first CESL and the first ILD layer in the second trench after recessing the first ILD layer. The second CESL is conformal. The method further comprises depositing a second ILD layer over the second CESL and filling remaining gaps of the first and second trenches. In another embodiment, the method further comprises forming a first contact element passing through the second CESL in the first trench and a second contact element passing through the second CESL in the second trench.In one embodiment of the method, fabricating the first CESL comprises the steps of: depositing a conformal layer comprising silicon nitride over the gate structures, the fin, and the isolation structure; treating the conformal layer with a plasma such that first portions of the conformal layer on the top of the gate structures receive a stronger plasma treatment than second portions of the conformal layer on the sidewalls of the gate structures; and applying, to the conformal layer, a chemical solution comprising hydrofluoric acid that dissolves the second portions faster than the first portions.In yet another aspect, the present invention is directed to a method of semiconductor fabrication. The method includes providing a device structure having an isolation structure, a fin laterally adjacent to the isolation structure and higher than the isolation structure, and gate structures over the fin and the isolation structure. The isolation structure, the fin, and the gate structures define a first trench over the fin and a second trench over the isolation structure. The method further includes the steps of: depositing a first contact etch stop layer (CESL) over the gate structures, the fin, and the isolation structure; depositing a first interlayer dielectric (ILD) layer over the first CESL and filling the first and second trenches; recessing the first ILD layer such that it is removed in the first trench and recessed in the second trench to a level approximately level with a top surface of the fin; and recessing the first CESL so that it is removed from the first trench and removed from the second trench above the first ILD layer.In one embodiment, the method further comprises depositing a second CESL over sidewalls of the first and second trenches. In one embodiment, the first CESL and the second CESL are each conformal. In another embodiment, the method further comprises depositing a second ILD layer over the second CESL and forming two contact elements passing through the second ILD layer in the first and second trenches, respectively.In another exemplary aspect, the present invention is directed to a semiconductor device. The semiconductor device includes: an isolation structure; a fin adjacent to the isolation structure and higher than the isolation structure; gate structures over the isolation structure and the fin defining a first gap between a first pair of adjacent sidewalls of the gate structures and a top surface of the fin and defining a second gap between a pair of adjacent sidewalls of the gate structures and a top surface of the isolation structure; a first dielectric layer on the second pair of adjacent sidewalls and the top surface of the isolation structure; a second dielectric layer filling a lower portion of the second gap, over the first dielectric layer, the first and second dielectric layers comprising different materials; a first contact element over the top surface of the fin and between the first pair of adjacent sidewalls; and a second contact element above the top surface of the second dielectric layer and between the second pair of adjacent sidewalls, the top surface of the fin being approximately level with the top surface of the second dielectric layer.In one embodiment, the semiconductor device further comprises a third dielectric layer over the first pair of adjacent sidewalls and over portions of the second pair of adjacent sidewalls that are above the second dielectric layer. In one embodiment, the first dielectric layer is further deposited between the third dielectric layer and the respective sidewall of the first pair of adjacent sidewalls. In another embodiment, the first dielectric layer is further deposited between the third dielectric layer and the respective sidewall of the second pair of adjacent sidewalls.In yet another exemplary aspect, the present invention is directed to a semiconductor device. The semiconductor device includes: an isolation structure; a fin adjacent to the isolation structure; gate structures over the isolation structure and the fin; a first dielectric layer over a top surface of the isolation structure, a top surface of the fin, and sidewalls of the gate structures; a second dielectric layer over a portion of the first dielectric layer directly over the isolation structure, the first and second dielectric layers comprising different materials; a third dielectric layer that is in physical contact with another portion of the first dielectric layer directly over the fin, is in physical contact with the fin, and is in physical contact with the first and second dielectric layers directly over the isolation structure; and a fourth dielectric layer over the third dielectric layer.In one embodiment, the semiconductor device further comprises: a first conductive feature over the top of the fin that passes through the first, third, and fourth dielectric layers; and a second conductive feature over the top of the isolation structure that passes through the third and fourth dielectric layers but not through the second dielectric layer. The semiconductor device may also comprise a source / drain feature that is in physical contact with the first conductive feature.In yet another aspect, the present invention is directed to a semiconductor device. The semiconductor device includes: an isolation structure; a fin adjacent to the isolation structure; gate structures over the isolation structure and the fin; a first dielectric layer over a top of the isolation structure and on sidewalls of the gate structures that are directly above the isolation structure; a second dielectric layer over the first dielectric layer; a third dielectric layer that is in physical contact with sidewalls of the gate structures, is in physical contact with the fin, and is in physical contact with the second dielectric layer, the second dielectric layer comprising a material that is different from the materials that are part of the first and third dielectric layers; and a fourth dielectric layer over the third dielectric layer.In some embodiments, the semiconductor device further comprises: a first conductive feature over the fin that passes through the third and fourth dielectric layers; and a second conductive feature over the second dielectric layer that passes through the third and fourth dielectric layers. In some embodiments of the semiconductor device, a top surface of the second dielectric layer is below a top surface of the fin.
Claims
A method of semiconductor manufacturing comprising the steps of: providing a device structure (100) having an isolation structure (106), a fin (104) adjacent to the isolation structure (106) and higher than the isolation structure (106), and gate structures (108) over the fin (104) and the isolation structure (106), the isolation structure (106), the fin (104), and the gate structures (108) defining a first trench (109b-c) over the fin (104) and a second trench (109d) over the isolation structure (106); forming a first contact etch stop layer over the gate structures (108), the fin (104), and the isolation structure (106); Depositing a first ILD layer (124) over the first contact etch stop layer (122) and filling the first and second trenches (109b, 109c, 109d); and recessing the first ILD layer (124) such that it is removed in the first trench (109b-c) and recessed in the second trench (109d) to a level approximately level with a top surface of the fin (104); wherein forming the first contact etch stop layer (122) comprises: depositing a conformal layer (122) comprising a dielectric material over the gate structures (108), the fin (104), and the isolation structure (106); Treating the conformal layer (122) with a plasma such that first portions (122a) of the conformal layer on the top of the gate structures (108) receive a stronger plasma treatment than second portions (122b) of the conformal layer on the sidewalls of the gate structures (108); and applying, to the conformal layer, a chemical solution that dissolves the second portions faster than the first portions.The method of claim 1, further comprising the steps of: after recessing the first ILD layer (124), forming a second contact etch stop layer (128) over the first contact etch stop layer (122) in the first trench and over the first contact etch stop layer (122) and the first ILD layer (124) in the second trench; and depositing a second ILD layer (130) over the second contact etch stop layer (128) and filling remaining gaps between the first and second trenches.The method of claim 2, further comprising: forming a first contact element extending into the second ILD layer (130) in the first trench and a second contact element extending into the second ILD layer (130) in the second trench.The method of claim 2 or 3, wherein the second contact etch stop layer (128) is conformal.A method according to any preceding claim, wherein the first contact etch stop layer (122) is thicker on top of the gate structures (108) than on sidewalls of the gate structures (108).The method of claim 5, wherein the dielectric material comprises silicon nitride.A method according to claim 5 or 6, wherein argon gas or nitrogen gas is used for the plasma.A method according to claim 5, 6 or 7, wherein the chemical solution comprises dilute hydrofluoric acid (DHF).Method according to one of claims 5 to 8, wherein the first parts (122a) are at least 4 nm thickThe method of claim 1, further comprising: after recessing the first ILD layer (124), recessing the first contact etch stop layer (122) such that it is removed from the first trench and removed from the second trench above the first ILD layer (124).The method of claim 10, further comprising: after recessing the first contact etch stop layer (122), forming a second contact etch stop layer (128) on sidewalls of the first and second trenches; and depositing a second ILD layer (130) over the second contact etch stop layer (128) and filling remaining gaps of the first and second trenches.The method of claim 11, further comprising: forming a first contact element extending into the second ILD layer (130) in the first trench and a second contact element extending into the second ILD layer (130) in the second trench.A method according to any one of the preceding claims, wherein the plasma treatment is directed.A method according to any one of the preceding claims, wherein the ILD layer (124) is deposited by an FCVD process or a PECVD process.
Citation Information
Patent Citations
Method to form etch and / or CMP stop layers
US20020081852A1
FinFETs and Methods for Forming the Same
US20140239354A1
Semiconductor device and method for fabricating the same
US20160064327A1