Carbon dioxide removal method
By employing a cation exchange membrane to separate anode and cathode compartments and using non-chlorine electrolyzed sodium sulfate solutions, the method enhances magnesium hydroxide production efficiency and purity while minimizing costs and chlorine gas generation.
Patent Information
- Application Number
- JP2024122963
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2039-11-01
AI Technical Summary
The existing magnesium recovery methods, such as those described in Patent Document 1, suffer from reduced production efficiency due to hydroxide ions passing through the diaphragm from the cathode to the anode side, leading to inefficient magnesium hydroxide production.
The method involves using a cation exchange membrane to divide the electrolytic cell into an anode and cathode compartments, restricting the movement of anions from the cathode side to the anode side, and employing non-chlorine electrolyzed water with sodium sulfate solutions to prevent chlorine gas generation and enhance magnesium hydroxide production efficiency.
This approach significantly improves the production efficiency of magnesium hydroxide by maintaining high hydroxide ion concentrations in the cathode compartment, reduces costs by using inexpensive sodium sulfate, and prevents harmful chlorine gas generation, resulting in high-purity magnesium recovery.
Smart Images

Figure 2024152742000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method and an apparatus for recovering magnesium. [Background technology]
[0002] Conventionally, there has been a method and device for recovering magnesium, in which an electrolytic treatment vessel having an inlet, an outlet, an anode and a cathode on the upper and lower wall surfaces, and a partition and a diaphragm separating the upper and lower sides, is immersed in the sea to perform electrolysis (electrolysis), and magnesium is recovered by precipitating it as magnesium hydroxide in the cathode electrolyzed water (see, for example, Patent Document 1). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2012-57230 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, in Patent Document 1, hydroxide ions, which are anions generated in the cathodic electrolyzed water by electrolysis, can pass through the diaphragm and migrate to the anodic electrolyzed water, so there is a problem that the efficiency of generating magnesium hydroxide is low.
[0005] The present invention has been made in consideration of such problems, and has an object to provide a magnesium recovery method and magnesium recovery apparatus capable of improving the efficiency of producing magnesium hydroxide. [Means for solving the problem]
[0006] In order to solve the above problems, the magnesium recovery method according to claim 1 of the present invention comprises the steps of: A method for recovering magnesium, comprising electrolyzing an aqueous solution containing at least magnesium ions to generate and recover magnesium hydroxide, which is poorly soluble in water, the method comprising the steps of: An electrolytic cell having an anode and a cathode is partitioned by a cation exchange membrane into an anode-side cell having the anode and a cathode-side cell having the cathode, and the aqueous solution is introduced into the cathode-side cell to perform electrolysis in a state in which the movement of anions from the cathode-side cell to the anode-side cell is restricted. It is characterized by the following. According to this feature, the hydroxide ions generated in the cathode side tank are prevented from migrating to the anode side tank, and the hydroxide ion concentration in the cathode side tank can be efficiently increased, thereby improving the efficiency of magnesium hydroxide production.
[0007] The magnesium recovery method according to claim 2 of the present invention is the magnesium recovery method according to claim 1, The aqueous solution is seawater. It is characterized by the following. This feature allows magnesium to be recovered from seawater at low cost.
[0008] The magnesium recovery method according to claim 3 of the present invention is the magnesium recovery method according to claim 1 or 2, A non-chlorine-based electrolytic water not containing chlorine ions is introduced into the anode side tank, and the aqueous solution is introduced into the cathode side tank. It is characterized by the following. According to this feature, it is possible to prevent harmful chlorine gas from being generated on the anode side due to electrolysis, and therefore it is possible to suppress an increase in the cost of recovering magnesium due to the cost of treating chlorine gas.
[0009] The magnesium recovery method according to claim 4 of the present invention is the magnesium recovery method according to claim 3, The non-chlorine electrolytic water is a sodium sulfate aqueous solution. It is characterized by the following. According to this feature, by using sodium sulfate, which is easily available and inexpensive, it is possible to suppress an increase in the cost of recovering magnesium that would otherwise be caused by using non-chlorine-based electrolytic water.
[0010] The magnesium recovery method according to claim 5 of the present invention is the magnesium recovery method according to claim 3 or 4, The method includes a regeneration step of introducing an aqueous regeneration solution containing cations transferred from the non-chlorine electrolyzed water in the anode side tank to the cathode side tank by electrolysis for recovering the magnesium hydroxide into one compartment of a regeneration tank partitioned by a cation exchange membrane, and introducing the non-chlorine electrolyzed water after electrolysis for recovering the magnesium hydroxide into the other compartment of the regeneration tank, thereby transferring the cations from the aqueous regeneration solution to the non-chlorine electrolyzed water and regenerating the water. It is characterized by the following. According to this feature, the non-chlorine electrolytic water can be regenerated and reused, and the cost of recovering magnesium can be reduced.
[0011] The magnesium recovery method according to claim 6 of the present invention is the magnesium recovery method according to any one of claims 1 to 5, The method includes a carbon dioxide gas removal step of reducing the concentration of carbon dioxide gas dissolved in the aqueous solution, and electrolyzing the aqueous solution in which the concentration of carbon dioxide gas has been reduced in the carbon dioxide gas removal step to recover magnesium. It is characterized by the following. According to this feature, the amount of calcium, which is an impurity, contained in the recovered magnesium can be reduced, and the purity of the magnesium can be increased.
[0012] The magnesium recovery method according to claim 7 of the present invention is the magnesium recovery method according to claim 6, The carbon dioxide gas removing step includes a heating step of heating the aqueous solution. It is characterized by the following. According to this feature, the dissolved carbon dioxide gas can be easily removed.
[0013] The magnesium recovery method according to claim 8 of the present invention is the magnesium recovery method according to claim 6 or claim 7, The carbon dioxide gas removing step includes a step of producing calcium carbonate by electrolyzing the aqueous solution. It is characterized by the following. This feature allows the dissolved carbon dioxide gas to be removed.
[0014] The magnesium recovery method according to claim 9 of the present invention is the magnesium recovery method according to any one of claims 1 to 8, The aqueous solution is seawater, and the amount of electricity applied per liter of seawater in the electrolysis for recovering magnesium is 12,000 coulombs or less. It is characterized by the following. According to this feature, it is possible to prevent the calcium hydroxide contained in the aqueous solution from being recovered together with the magnesium hydroxide, which would result in a decrease in the purity of magnesium.
[0015] The magnesium recovery method according to claim 10 of the present invention is the magnesium recovery method according to any one of claims 1 to 9, The electrode constituting the anode is an insoluble electrode having a material with a smaller ionization tendency than silver. It is characterized by the following. According to this feature, it is possible to prevent ions of the material constituting the electrode from being contained in the aqueous solution after magnesium recovery, which would have a significant impact on the environment.
[0016] The magnesium recovery apparatus according to claim 11 of the present invention comprises: an electrolytic cell having an anode and a cathode; A power supply means capable of supplying power for electrolysis to the anode and the cathode; A recovery means capable of recovering magnesium hydroxide which is sparingly soluble in water produced by electrolysis; A magnesium recovery apparatus comprising: the electrolytic cell is partitioned by a cation exchange membrane into an anode-side cell having the anode and a cathode-side cell having the cathode, A supply means is provided for supplying an aqueous solution containing at least magnesium ions to the cathode side tank. It is characterized by the following. According to this feature, the hydroxide ions generated in the cathode side tank are prevented from migrating to the anode side tank, and the hydroxide ion concentration in the cathode side tank can be efficiently increased, thereby improving the efficiency of magnesium hydroxide production.
[0017] Furthermore, the present invention may have only the invention-specific matters described in the claims of the present invention, or may have the invention-specific matters described in the claims of the present invention as well as configurations other than the invention-specific matters. [Brief description of the drawings]
[0018] [Figure 1] FIG. 1 is a configuration diagram of a magnesium recovery device in a first embodiment of the present invention. [Diagram 2] FIG. 1 is a diagram showing a configuration of an electrolytic cell in a magnesium recovery device according to a first embodiment of the present invention. [Diagram 3] FIG. 2 is a diagram showing flow paths used in the electrolysis stack 2 in the first embodiment of the present invention. [Figure 4] 4 is a table showing test conditions in the first embodiment of the present invention. [Diagram 5] 1 is a graph showing the relationship between current and magnesium ion concentration. [Figure 6] 1 is a graph showing the relationship between current and calcium ion concentration. [Figure 7] 1 is a graph showing the relationship between magnesium ion concentration and unit volume charge. [Figure 8] 1 is a graph showing the relationship between calcium ion concentration and electrical charge per unit volume. [Figure 9] 11 is a table showing measured concentrations of magnesium ions and calcium ions at each flow rate and each unit volume charge. [Figure 10] 4 is a graph showing changes in pH value in the anode side chamber 20a and the cathode side chamber 20b. [Figure 11] (a) is a mapping SEM image of a precipitate with a unit volume electrical charge of 3600 C / L, and (b) is a mapping SEM image of a precipitate with a unit volume electrical charge of 14400 C / L. [Figure 12] (a) is the result of EDS analysis of a precipitate with a unit volume electrical charge of 3600 C / L, and (b) is the result of EDS analysis of a precipitate with a unit volume electrical charge of 14400 C / L. [Figure 13] 1 is a graph showing the relationship between magnesium ions and unit volume electricity in each deaerated seawater and non-deaerated seawater. [Figure 14] 1 is a graph showing the relationship between calcium ions and unit volume electricity in each deaerated seawater and non-deaerated seawater. [Figure 15] 1 is a table showing the measured values of magnesium ions and calcium ions at each unit volume of electricity during electrolysis of each degassed seawater. [Figure 16] (a) is a mapping SEM image of sediment from seawater that has been degassed by boiling, (b) is a mapping SEM image of sediment from seawater that has been degassed by adding acid, and (c) is a mapping SEM image of sediment from non-degassed seawater. [Figure 17] (a) is the EDS analysis result of sediment from boiling degassed seawater, (b) is the EDS analysis result of sediment from seawater degassed with added acid, and (c) is the EDS analysis result of sediment from non-degassed seawater. [Figure 18] FIG. 11 is a configuration diagram of a magnesium recovery device in a second embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] Examples of the present invention are described below.
[0020] FIG. 1 is a diagram showing the configuration of an example of a magnesium recovery apparatus to which the magnesium recovery method of the present invention is applied.
[0021] As shown in FIG. 1, the magnesium recovery device of the present embodiment 1 is mainly composed of an electrolysis stack 2 which is an electrolysis tank (electrolysis tank) for performing electrolysis, a DC power supply device (power supply means) 1 for supplying power for electrolysis (electrolysis power) to an anode 2a and a cathode 2c provided in the electrolysis stack 2, a seawater tank 7 and a sodium sulfate aqueous solution tank 8 for storing seawater (deep ocean water) and a 5% by weight aqueous sodium sulfate solution to be supplied to the electrolysis stack 2, a cathode solution tank 10 and an anode solution tank 9 for storing treated seawater and aqueous sodium sulfate solution electrolyzed in the electrolysis stack 2, and a filtration device 16 for filtering the treated seawater stored in the cathode solution tank 10 and recovering magnesium hydroxide, which is magnesium hydroxide contained in the treated seawater without settling. The device is capable of performing electrolysis continuously.
[0022] The lower part of the electrolysis stack 2 is connected to the sodium sulfate aqueous solution tank 8 and the seawater tank 7 by inlet pipes 13a and 13c, and the sodium sulfate aqueous solution and seawater stored in the sodium sulfate aqueous solution tank 8 and the seawater tank 7 are introduced into the electrolysis stack 2 from the lower part of the electrolysis stack 2 and discharged from the upper part of the electrolysis stack 2.
[0023] As shown in FIG. 1, pumps 14a and 14c capable of varying the flow rate are provided on the paths of the inlet pipes 13a and 13c corresponding to the respective inlet pipes 13a and 13c, and the flow rates of the aqueous sodium sulfate solution and seawater supplied to the electrolysis stack 2 by the pumps 14a and 14c can be individually adjusted by inverter power sources 6a and 6c for operating the pumps 14a and 14c. In the first embodiment, as described later, for example, MG204XPD17-10S, MAGPON GEAR (product name of Nikkiso Eiko Co., Ltd.) is used as the pumps 14a and 14c capable of varying the flow rate because it is necessary to change the flow rate to consider the recovery conditions, but the present invention is not limited to this, and a pump that cannot vary the flow rate may be used. The inverter power sources 6a and 6c may be appropriately selected depending on the pumps to be used.
[0024] 1, flowmeters 3a and 3c for measuring the flow rates of the aqueous sodium sulfate solution and seawater supplied to the electrolysis stack 2 via the inlet pipes 13a and 13a are provided on the paths of the inlet pipes 13a and 13c, and valves 4a and 4c are also provided on the paths of the inlet pipes 13a and 13c. Note that, for example, a Handy Logger GL200A (trade name manufactured by Graphtec Corporation) can be used as the flowmeters 3a and 3c.
[0025] In this embodiment 1, as shown in FIG. 1, a spare seawater tank 11 capable of storing deep-sea water is connected to the seawater tank 7, and a degassing treatment device 12 for degassing carbon dioxide contained in the deep-sea water is provided between the seawater tank 7 and the spare tank 11.
[0026] The degassing treatment device 12 of this embodiment 1 has two degassing treatment systems inside: a boiling degassing system that heats and boils deep-ocean water (seawater) to degasify carbon dioxide, and an acid addition degassing system that adds acid to deep-ocean water (seawater) to degasify carbon dioxide, and these can be used by switching between them.
[0027] Meanwhile, the upper part of the electrolytic stack 2 is connected to the anode solution tank 9 and the cathode solution tank 10 by discharge pipes 15a and 15c, and the treated sodium sulfate aqueous solution and seawater that have been electrolyzed in the electrolytic stack 2 and discharged are stored in the anode solution tank 9 and the cathode solution tank 10.
[0028] As described above, the catholyte solution tank 10 is connected to the filtration device 16, so that magnesium hydroxide contained in the treated seawater without settling in the catholyte solution tank 10 is filtered.
[0029] Fig. 2 is a diagram showing the configuration of the electrolysis stack 2 of the present embodiment 1. As shown in Fig. 2, the electrolysis stack 2 of the present embodiment 1 is an electrolysis cell (electrolysis cell) that includes an anode 2a and a cathode 2c and is partitioned by an ion exchange membrane 2b provided between the anode 2a and the cathode 2c.
[0030] Specifically, the cation exchange membrane 2b is arranged in the center of the electrolytic cell by pressing it with silicone rubber, and the electrolytic cell is divided into an anode side cell 20a and a cathode side cell 20b. In this embodiment, a CMB (product name manufactured by Astom Corporation) capable of exchanging sodium ions, which are monovalent cations, is used as the cation exchange membrane, but the present invention is not limited to this, and an appropriate membrane may be selected depending on the electrolyte dissolved in the aqueous solution introduced into the anode side cell 20a, particularly the valence of the cations.
[0031] Moreover, the concentration of the aqueous sodium sulfate solution supplied from the aqueous sodium sulfate solution tank 8 to the anode side tank 20a of the electrolysis stack 2 is preferably a concentration sufficient to prevent a neutralization reaction caused by hydrogen ions transported from the anode side to the cathode side. Specifically, as a result of an investigation by measuring the pH value in the solution obtained at the outlet of the electrolysis stack 2, a high concentration aqueous sodium sulfate solution with a weight concentration of 5% may be used.
[0032] The anode 2a and the cathode 2c provided in the electrolytic stack 2 are platinum-plated titanium plates, which are titanium plates plated with platinum, because they are not corroded by the aqueous solution by electrolysis, have high electrical conductivity, are excellent in mechanical strength, and are preferably inexpensive. The platinum electrodes have high chemical stability, and platinum does not dissolve in the aqueous solution even by electrolysis. The thickness of the platinum plating layer may be an appropriate thickness that does not have missing parts (defects) in the plating layer. In the first embodiment, the electrodes have a platinum layer formed on the surface by plating, but the present invention is not limited to this. If there are no problems with the cost or mechanical strength, the electrodes themselves may be platinum plates or may be made of a carbon material. In this case, it is preferable that the surface of the carbon material is coated with a conductive material such as a nanoporous metal. In this embodiment, a platinum-plated titanium plate is used as the anode 2a provided in the electrolytic stack 2, but the present invention is not limited to this. If the anode 2a has an ionization tendency equal to or greater than that of silver (Ag), the electrode will be oxidized and dissolved. Therefore, as long as the ionization tendency of the material is smaller than that of silver (Ag), the electrode may have a material other than platinum, such as gold (Au) or carbon (C), on at least the surface. In addition, since a reduction reaction occurs on the cathode side, the cathode 2c provided in the electrolysis stack 2 can be made of any metal.
[0033] Here, the flow path used in the electrolysis stack 2 in the present embodiment 1 is shown in Fig. 3. The flow path was made by hollowing out the center of a 5 mm-thick plate-shaped silicone rubber as shown in Fig. 3, with electrodes disposed on one side and a cation exchange membrane disposed on the other side.
[0034] Specifically, two silicone rubber plates with platinum-plated titanium arranged in the center of one side are prepared, and a cation exchange membrane 2b is sandwiched between the other sides of the two silicone rubber plates and pressure-bonded to form the electrolytic stack 2 shown in FIG. 2.
[0035] Therefore, by disposing the electrodes on one side of the central part of the flow channel, the area where the electrodes are disposed becomes the area where a chemical reaction occurs by electrolysis. The dimensions of the area where the chemical reaction occurs are 600 mm in length, 5 mm in depth, and 20 mm in width.
[0036] In addition, while FIG. 3 illustrates the flow paths as being horizontal, in the first embodiment, the flow paths are arranged so as to be approximately vertical to the ground, and each aqueous solution is supplied from below in the direction opposite to the force of gravity. In this way, it is possible to prevent clogging of the flow paths caused by the production of magnesium hydroxide in the cathode-side tank 20b when the flow paths are arranged horizontally.
[0037] When an aqueous sodium sulfate solution is introduced into the anode tank 20a of the electrolysis stack 2 made of silicone rubber formed as described above and seawater is introduced into the cathode tank 20b, an electrolysis reaction occurs when a current is passed between the anode 2a and the cathode 2c. Hydroxide ions generated at the cathode 2c by the electrolysis of water react with magnesium ions in the seawater, and magnesium hydroxide is precipitated.
[0038] Furthermore, since the cation exchange membrane 2b is used in the first embodiment, hydroxide ions, which are anions generated at the cathode 2c, cannot pass through the cation exchange membrane 2b and cannot move to the anode side tank 20a. This makes it possible to efficiently increase the pH value of the cathode side tank 20b with a small amount of power, and efficiently generate magnesium hydroxide. Similarly to hydroxide ions, chloride ions, which are anions contained in seawater introduced into the cathode side tank 20b, cannot pass through the cation exchange membrane 2b and cannot move to the anode side tank 20a. Therefore, electrolysis is performed without chloride ions being contained in the anode side tank 20a. Therefore, chlorine gas is not generated at the anode 2a, and oxygen gas is generated at the anode 2a. Hydrogen gas is generated at the cathode 2c.
[0039] Next, the magnesium recovery conditions were tested using the device of the first embodiment described above. In this test, the flow rates of seawater and the sodium sulfate aqueous solution were set to be the same, and three sets of flow rates of 20 ml / min, 40 ml / min, and 60 ml / min were selected as shown in FIG. 4. Furthermore, the test was performed by changing the amount of electricity per unit volume of seawater according to each flow rate. In this test, the amount of electricity was set so as not to exceed the limit current density, so that dissociation of water does not occur in the boundary layer of the cation exchange membrane 2b. Details of the test conditions are shown in FIG. 4. The amount of electricity per unit volume of seawater (hereinafter referred to as the amount of electricity per unit volume) was selected to be 3600 C (coulomb) / L (liter), 7200 C / L, 10800 C / L, and 14400 C / L.
[0040] In addition, in order to clarify the effect of the degassing device 16 in the comparison described below, the test was carried out using non-degassed seawater without operating the degassing device 16.
[0041] In the test, the electrolytic seawater containing the precipitate was collected in a glass beaker from the outlet of the electrolytic stack 2 after the electrolysis reached a steady state. The beaker was sealed and left for 30 minutes until the chemical reaction in the electrolytic seawater had fully reacted. After that, the fully reacted solution was filtered with filter paper to separate the precipitate from the aqueous solution. The precipitate was washed three times with pure water to prevent water-soluble compounds such as sodium chloride in the seawater from adhering to the precipitate. Next, the precipitate was dried and then analyzed for its surface condition and constituent elements using a scanning electron microscope (SEM) and energy dispersive X-ray spectrometry (EDS). The filtered aqueous solution was diluted to an appropriate ratio using ultrapure water according to each ion in a dilution device. The diluted solution was analyzed for the concentration of each element using inductively coupled plasma (ICP).
[0042] Fig. 5 is a graph showing the relationship between current and magnesium ion concentration. As shown in Fig. 5, the magnesium ion concentration decreases as the flow rate decreases. This is because, when the amount of electricity is the same, the amount of hydroxide ions generated at the cathode 2c is also the same, so when the flow rate is decreased, more hydroxide ions are contained in a unit volume. On the other hand, the magnesium ion concentration decreases as the applied current increases. This is because, when the applied current is increased, the amount of hydroxide ions generated by the electrode reaction also increases, and the amount of magnesium ions that react with hydroxide ions to become magnesium hydroxide also increases.
[0043] FIG. 6 is a graph showing the relationship between the current and the calcium ion concentration. The relationship between the calcium concentration and the flow rate decreased with a decrease in the flow rate, just like the magnesium ion. Furthermore, the calcium production reaction is divided into two stages as shown in FIG. 6. In the first stage, the concentration slightly decreases at the same time as the production of magnesium hydroxide. This is because the pH value of the seawater in the cathode side tank 20b increases as electrolysis is performed, and the carbonate ions present in the seawater are converted to carbonate ions, which then react with the calcium ions and precipitate as calcium carbonate. In the second stage, the concentration of calcium decreases after the magnesium ions are consumed due to the reaction between the magnesium ions and the hydroxide ions. This is because as the reaction of magnesium hydroxide progresses, the magnesium ions in the seawater decrease proportionally, and the proportion of calcium ions increases, so a chemical reaction between the calcium ions and the hydroxide ions begins, and the calcium ions precipitate as calcium hydroxide, thereby decreasing the concentration of calcium ions.
[0044] FIG. 9 is a table showing measured concentrations of magnesium ions and calcium ions at each flow rate and each unit volume charge, and graphs based on the measured values are shown in FIGS.
[0045] FIG. 7 is a graph showing the relationship between the measured magnesium ion concentration and the unit volume charge. With the unit volume charge on the horizontal axis, the ion concentration is consistent at the same unit volume charge regardless of the flow rate. This shows that the generation of hydroxide ions at the cathode 2c is proportional to the current, so that the change in magnesium ion concentration depends on the volume charge. On the other hand, in the case of non-deaerated seawater, it can be seen that the magnesium ions in the seawater can be almost completely recovered at a unit volume charge between 10,000 C / L and 14,400 C / L, more specifically, at about 12,000 C / L, calculated from the slope of the graph.
[0046] Fig. 8 is a graph showing the relationship between the measured calcium ion concentration and the unit volume charge. Unlike magnesium ions, calcium ions have a small unit volume charge, and the concentration slightly decreases in the early stage of electrolysis, but there is almost no change between 3600 C / L and 7200 C / L, and there is a large decrease from 10000 C / L (more specifically, 10800 C / L). This is because, in the early stage of electrolysis, in parallel with the generation of magnesium hydroxide, the pH value increases due to the generation of hydroxide ions, causing the carbon dioxide contained in seawater to react with calcium, resulting in the precipitation of calcium carbonate, and the concentration of calcium ions slightly decreases, as described later. After all the carbon dioxide contained in seawater has been consumed, calcium carbonate does not precipitate, so the calcium ions do not decrease, and magnesium hydroxide precipitates. Up to approximately 10,000 C / L (more specifically, 10,800 C / L), at which point the magnesium ions are almost all consumed, the concentration of calcium ions does not decrease much, and it can be seen that after almost all the magnesium ions in the seawater have been consumed, the calcium ions decrease as they are consumed as calcium hydroxide.
[0047] Next, the changes in pH value in the anode side tank 20a and the cathode side tank 20b are shown in Fig. 10. As the quantity of electricity per unit volume increases, hydrogen ions are generated in the anode 2a, so the pH value of the sodium sulfate aqueous solution in the anode side tank 20a decreases. On the other hand, as the quantity of electricity per unit volume increases in the cathode 2c, hydroxide ions are generated, so the pH value of the seawater in the cathode side tank 20b increases.
[0048] As shown in Fig. 10, it can be seen that the pH value depends on the unit volume charge (C / L) input to the electrolysis stack 2. Furthermore, since the solubility products of magnesium hydroxide and calcium hydroxide are different and the pH environment required for the reaction is also different, the pH value of the seawater in the cathode side tank 20b changes in two stages. The pH value of the seawater in the cathode side tank 20b remains at 9.8 under conditions between unit volume charges of 3600 C / L and 10000 C / L, and increases again when the unit volume charge exceeds 10000 C / L (more specifically, 10800 C / L). This is because hydroxide ions are consumed by the production of magnesium hydroxide in the range of 3600 C / L to 10000 C / L (more specifically, 10800 C / L), so the pH value of the seawater in the cathode side tank 20b remains at 9.8. When the pH exceeds 10000 C / L, calcium hydroxide begins to be produced as magnesium ions decrease, and the pH value rises.
[0049] Next, the analysis results of the collected precipitate are shown. In order to verify the composition of the precipitate, the surface state of the precipitate generated in the cathode side tank 20b during electrolysis was observed by a scanning electron microscope (SEM), and at the same time, the composition of the constituent elements was analyzed by energy dispersive X-ray analysis (EDS). Based on the results of energy dispersive X-ray analysis (EDS), mapping of the SEM image was performed.
[0050] Figure 11(a) is a mapping SEM image of a precipitate with a unit volume charge of 3600 C / L at a flow rate of 40 ml / min, and Figure 11(b) is a mapping SEM image of a precipitate with a unit volume charge of 14400 C / L at a flow rate of 40 ml / min. In the mapping SEM image, the light grey areas that are smooth are magnesium compounds, and the dark grey areas that are relatively large crystals and not smooth are calcium compounds.
[0051] From Figures 7 and 8, and Figures 12, 13, and 14, which are the test results after degassing, it is believed that the calcium compound in Figure 11(a) is calcium carbonate, and the calcium compound in Figure 11(b) is calcium hydroxide. Also, as shown in Figure 8, there is almost no decrease in calcium ion concentration when comparing the unit volume charge of 3600 C / L and the unit volume charge of 7200 C / L, so it is believed that a mapping SEM image of the precipitate similar to that of Figure 11(a) for the unit volume charge of 3600 C / L can be obtained even in the case of the unit volume charge of 7200 C / L. With a unit volume electrical charge of 12,000C / L, magnesium can be completely recovered. However, not only magnesium but also calcium in seawater precipitates, resulting in low purity of the recovered magnesium. Therefore, magnesium needs to be purified in a post-process. Furthermore, at a unit volume electrical charge of 10800C / L, almost all of the magnesium can be recovered. Although not only magnesium but also calcium precipitates in seawater, the amount of precipitated calcium is small, and the purity of magnesium is high. Therefore, near this unit volume electrical charge, the magnesium recovery rate is high and calcium precipitation is small, so that magnesium of high purity can be recovered with high efficiency, and this unit volume electrical charge is sufficient to obtain magnesium that is practical for industrial magnesium applications. In addition, in the range of unit volume electrical charge of 3600C / L to 7200C / L, the recovery rate of magnesium is lower than that of the unit volume electrical charge of 10800C / L, but there is almost no calcium precipitation and the purity of magnesium is the highest. This is an effective unit volume electrical charge when magnesium purity is required for applications such as pharmaceuticals and reagents.
[0052] Next, the results of the component analysis by energy dispersive X-ray analysis (EDS) are shown in Figure 12. Note that the carbon content in the precipitate was not measured because the energy dispersive X-ray analysis (EDS) measurement requires a seal containing carbon. Therefore, the percentages in the EDS analysis results show values excluding carbon.
[0053] FIG. 12(a) shows the results of EDS analysis of a precipitate with a unit volume charge of 3600 C / L at a flow rate of 40 ml / min, and FIG. 12(b) shows the results of EDS analysis of a precipitate with a unit volume charge of 14400 C / L at a flow rate of 40 ml / min.
[0054] As can be seen from Fig. 12, only the cations calcium ions and magnesium ions were detected in the EDS analysis results. This is because highly soluble compounds such as sodium chloride and potassium chloride present in the seawater in the cathode side tank 20b were washed away by the pure water during filtration. In addition, as shown in Fig. 10, there was no increase in the pH value of the seawater between the unit volume electrical quantities of 3600 C / L and 10000 C / L (more specifically, 10800 C / L), which can be considered to be because the hydroxide ions generated by electrolysis were consumed in the chemical reaction generating magnesium hydroxide.
[0055] Furthermore, since the calcium ions begin to decrease after the magnesium ions have been almost completely recovered, it can be determined that the calcium compound produced in the two steps is calcium hydroxide.
[0056] Next, it will be explained below how the purity of the recovered magnesium hydroxide can be improved by degassing the carbon dioxide in the seawater.
[0057] As described above, when hydroxide ions are generated by electrolysis in the cathode side tank 20b and the pH value rises, magnesium carbonate precipitates in parallel with the precipitation of magnesium ions in the seawater, and the magnesium ions are contaminated with the magnesium carbonate to reduce the purity of the magnesium hydroxide.
[0058] Therefore, in order to prevent magnesium carbonate from being mixed in, it is effective to carry out a degassing process to remove carbonate ions, which are carbon dioxide, from seawater.
[0059] As for these degassing processes, because the solubility of carbon dioxide, which is a gas, decreases as the liquid temperature increases according to Henry's law, we carried out a boiling degassing process in which the seawater is heated to boil before being supplied to the electrolysis stack 2 to degas the carbon dioxide, and because the abundance ratio of carbonate ions varies depending on the pH value in the solution, we carried out an acid addition degassing process in which the pH value of the seawater is changed to acidic by adding an acid, thereby degassing the carbonate ions as carbon dioxide.
[0060] Therefore, in this embodiment 1, as described above, the degassing treatment device 12 is provided with two degassing treatment systems: a boiling degassing system that performs boiling degassing treatment, and an acid addition degassing system that performs acid addition degassing treatment, and it is possible to switch between each degassing treatment.
[0061] In addition, although the degassing treatment device 12 of this embodiment 1 is exemplified as having two systems, the present invention is not limited to this, and the device may have only one of these systems, or may be capable of performing both processes of the two systems in an overlapping manner.
[0062] In the boiling degassing process, seawater is heated to 100°C for 5 minutes. In the acid degassing process, the pH value of seawater is lowered to 3 by adding hydrochloric acid, and bicarbonate ions are converted to carbon dioxide and removed from the seawater. In the case of adding acid, the bicarbonate ions are neutralized by hydroxide ions generated by electrolysis.
[0063] In the first embodiment, the seawater degassed by the degassing device 12 was stored in the seawater tank 7 for about 24 hours (one day) and then supplied to the electrolysis stack 2 for electrolysis.
[0064] For electrolysis, the aqueous solution collected from the outlet of the cathode side tank 20b of the electrolysis stack 2 at a flow rate of 40 ml / min was filtered to separate the precipitate from the aqueous solution, after which the aqueous solution was subjected to component analysis using inductively coupled plasma (ICP). The precipitate was also subjected to surface analysis and elemental analysis using a scanning electron microscope (SEM) and energy dispersive X-ray spectrometry (EDS).
[0065] Fig. 15 is a table showing the measured values of magnesium ion and calcium ion at each unit volume of electricity in the electrolysis of each degassed seawater, Fig. 13 is a graph showing the relationship between magnesium ion and unit volume of electricity in each degassed seawater and non-degassed seawater, and Fig. 14 is a graph showing the relationship between calcium ion and unit volume of electricity in each degassed seawater and non-degassed seawater. For non-degassed seawater, the measurement data at a flow rate of 40 ml / min in Fig. 9 is used.
[0066] From the graph in Figure 13, it can be seen that the rate of magnesium hydroxide formation in boiled and degassed seawater is slightly faster than in non-degassed seawater. Furthermore, from the graph in Figure 14, it can be seen that in boiled and degassed seawater, calcium ions do not decrease between unit volume electrical quantities of 0 C / L and 7200 C / L. Therefore, it can be seen that the calcium compound formed in the first stage in non-degassed seawater is calcium carbonate formed due to the increase in the pH value of the seawater.
[0067] Therefore, the graph in Figure 13 can be understood to indicate that the amount of electricity is being used to recover only the magnesium ions in the seawater, with almost no effect of calcium carbonate due to the calcium ions contained in the seawater.From this graph in Figure 13, it can be seen that by keeping the amount of electricity per unit volume in the electrolysis of magnesium in seawater to around 10,000 C / L (more specifically, 10,800 C / L), it is possible to recover almost all of the magnesium in the seawater while recovering high-purity magnesium hydroxide with significantly little loss of purity due to the precipitation of calcium hydroxide.
[0068] On the other hand, as shown in the graph in Figure 14, in the case of acid-added degassing treatment, the amount of calcium carbonate produced in the first stage was slightly reduced. Adding acid to seawater increases the abundance of carbon dioxide. However, although some carbon dioxide was released to the outside due to its solubility, it is not possible to remove all of the carbon dioxide. Therefore, when electrolysis is performed, the pH value of the solution rises again due to the electrolysis of water, so it is thought that carbon dioxide returns to carbonate ions, reacts with calcium ions, and precipitates as calcium carbonate.
[0069] Thus, although the boiling degassing process is superior as a degassing process for preventing calcium carbonate from being mixed in, boiling seawater requires a lot of energy and the equipment is large, which may increase the processing cost, whereas the acid addition degassing process only involves adding acid, which can suppress the increase in processing cost, and therefore which degassing process should be selected appropriately based on the balance between the purity of the magnesium hydroxide to be recovered and the acceptable processing cost. Moreover, the degassing process is not limited to the boiling degassing process or the acid addition degassing process, and other degassing methods may be used.
[0070] Next, mapping SEM images of sediments from degassed seawater are shown in Figure 16. Figure 16(a) is a mapping SEM image of sediments from boiling degassed seawater, Figure 16(b) is a mapping SEM image of sediments from seawater degassed with acid added, and Figure 16(c) is a mapping SEM image of sediments from non-degassed seawater, which are the same images as Figure 11(a). Note that the unit volume electrical charge of each mapping SEM image shown in Figure 16 is 3600 C / L, and similar mapping SEM images would be obtained even if the unit volume electrical charge was 7200 C / L.
[0071] As shown in Figure 16(c), calcium compounds are scattered on the surface of the sediment from seawater that has not been degassed, but there are almost no dark gray areas in Figures 16(a) and (b), which shows that the amount of calcium compounds has clearly decreased in the sediment from seawater that has been degassed by boiling or additive degassing.
[0072] Moreover, the results of energy dispersive X-ray analysis (EDS) of components of sediment from degassed seawater are shown in Figure 17. Figure 17(a) shows the results of EDS analysis of sediment from boiling degassed seawater, Figure 17(b) shows the results of EDS analysis of sediment from seawater degassed with acid, and Figure 17(c) shows the results of EDS analysis of sediment from non-degassed seawater.
[0073] Comparing the EDS analysis results of the sediment of seawater without degassing shown in FIG. 17(c) with the EDS analysis results of the sediment of seawater subjected to boiling degassing shown in FIG. 17(a) and the EDS analysis results of the sediment of seawater subjected to acid-addition degassing shown in FIG. 17(b), the abundance ratio of calcium element in the sediment of the degassed seawater was significantly reduced. This proved that the boiling method and the acid-addition method are effective for generating calcium carbonate. In addition, the EDS analysis results show that the molar ratio of magnesium ion to calcium ion in the sediment subjected to degassing treatment is 30.54:0.41 in the boiling degassing treatment and 31.23:0.28 in the acid-addition method. Therefore, it is understood that a magnesium compound with a purity of 99% can be recovered by the degassing treatment. Furthermore, since the molar ratio of magnesium to oxygen is 1:2 in the magnesium compound not containing calcium carbonate, it is understood that the magnesium compound is magnesium hydroxide. Embodiment 2
[0074] 18 is a diagram showing the configuration of the magnesium recovery device of the embodiment 2. The magnesium recovery device of the embodiment 2 is mainly characterized by the following two points.
[0075] The first point is that in the above-mentioned embodiment 1, in order to reduce calcium carbonate mixed in the magnesium hydroxide precipitate, the carbon dioxide contained as bicarbonate ions in seawater is degassed to reduce calcium carbonate, whereas in the embodiment 2, the carbon dioxide contained as bicarbonate ions in seawater is removed as calcium carbonate by the first stage of electrolysis.
[0076] The second advantage is that the aqueous sodium sulfate solution used in the anode-side tank 20a during electrolysis is regenerated and reused.
[0077] As shown in Fig. 18, the magnesium recovery apparatus of the second embodiment is mainly composed of two electrolysis stacks (electrolysis tanks) 21, 22 and one regeneration tank 30. In Fig. 18, "P" indicates a pump and "FM" indicates a flow meter. In Fig. 18, due to space limitations, the DC power supply device 1 shown in Fig. 1 and the inverter power supplies 6a, 6c that drive the pumps are omitted.
[0078] The two electrolysis stacks 21 and 22 have the same configuration as the electrolysis stack 2 used in the first embodiment, which is partitioned into an anode-side chamber 20a and a cathode-side chamber 20b by a cation exchange membrane 2b, as shown in FIGS. 2 and 3.
[0079] The first electrolysis stack 21 performing the first electrolysis and the second electrolysis stack 22 performing the second electrolysis are connected in series by piping, as shown in Figure 18, so that the sodium sulfate aqueous solution in the anode side tank 20a of the first electrolysis stack 21 is introduced into the anode side tank 20a of the second electrolysis stack 22, and seawater in the cathode side tank 20b of the first electrolysis stack 21 is introduced into the cathode side tank 20b of the second electrolysis stack 22.
[0080] In addition, a first filtration device 40 is provided on the piping path connecting the cathode side tank 20b of the first electrolysis stack 21 and the cathode side tank 20b of the second electrolysis stack 22. Calcium hydroxide and magnesium hydroxide precipitated by electrolysis in the first electrolysis stack 21 are filtered by the first filtration device 40, and the filtered seawater is supplied to the cathode side tank 20b of the second electrolysis stack 22.
[0081] Furthermore, as shown in FIG. 18 , the magnesium recovery apparatus of the second embodiment is provided with a configuration in which the electrodes are removed from the electrolytic stack 2 shown in FIG. 2 , that is, a regeneration tank 30 having two compartments separated by a cation exchange membrane, and is connected so that the aqueous sodium sulfate solution discharged from the anode side tank 20 a of the second electrolytic stack 22 is supplied to one compartment of the regeneration tank 30, and seawater discharged from the cathode side tank 20 b of the second electrolytic stack 22 is supplied to the other compartment of the regeneration tank 30.
[0082] Then, as shown in FIG. 18, the aqueous sodium sulfate solution regenerated in one compartment of the regeneration tank 30 is supplied to the anode side tank 20a of the first electrolysis stack 21 and reused, while the seawater discharged from the other compartment of the regeneration tank 30 is discharged into the sea.
[0083] Next, the flow of the process in the magnesium recovery apparatus of the second embodiment will be described. Undeaerated seawater (deep ocean water) stored in a seawater tank is supplied by a pump to the cathode side tank 20b of the first electrolysis stack 21, and a regenerated aqueous sodium sulfate solution is supplied to the anode side tank 20a of the first electrolysis stack 21. Note that, in the regenerated aqueous sodium sulfate solution, the sodium sulfate concentration is measured, and if the concentration is insufficient, that is, does not reach a weight concentration of 5%, sodium sulfate may be added to adjust the concentration to a sufficient level.
[0084] Then, in the first electrolysis stack 21, primary electrolysis is performed at a unit volume electrical quantity of 3600 C / L as shown in Fig. 18. The reason for electrolysis at 3600 C / L is that, as described above in the first embodiment, the calcium ion concentration hardly changes in the period from 3600 to 7200 C / L in the graph of Fig. 8 showing the change in calcium ion concentration, and therefore precipitation of calcium carbonate by bicarbonate ions (carbon dioxide) contained in seawater is considered to be already completed by the time the unit volume electrical quantity reaches 3600 C / L.
[0085] That is, by performing primary electrolysis with a unit volume electrical quantity of 3600 C / L, almost all of the carbon dioxide contained as bicarbonate ions in seawater is consumed in the precipitation of calcium carbonate, so that the seawater after primary electrolysis contains almost no bicarbonate ions (carbon dioxide), and even if the seawater is further electrolyzed, almost no calcium carbonate is precipitated, and it is possible to precipitate magnesium hydroxide by performing secondary electrolysis in a state in which almost no calcium carbonate is precipitated. Therefore, the primary electrolysis (degassing (calcium removal) step) of embodiment 2 corresponds to the carbon dioxide gas removal step of the present invention.
[0086] The seawater that has been subjected to the primary electrolysis is filtered in the first filtration device 40, and calcium carbonate and magnesium hydroxide precipitated in the primary electrolysis are separated from the seawater. The seawater that is the filtrate after separation is supplied to the cathode side tank 20b of the second electrolysis stack 22.
[0087] Then, in the second electrolysis stack 22, secondary electrolysis is performed at a unit volume electrical quantity of 8400 C / L as shown in Fig. 18. The reason for performing electrolysis at 8400 C / L is that, as described above in the first embodiment, when the total unit volume electrical quantity of the primary electrolysis and secondary electrolysis exceeds 12000 C / L, the precipitation of calcium hydroxide increases, causing calcium hydroxide to be mixed into the recovered magnesium hydroxide, thereby preventing a decrease in the purity of the recovered magnesium hydroxide. In addition, when calcium hydroxide is removed in a later process and magnesium hydroxide is refined, electrolysis may be performed at a total unit volume electricity quantity of 12000 C / L or more (for example, 14400 C / L) at which magnesium can be completely recovered from seawater. Even when electrolysis is performed at a total unit volume electricity quantity of 10800 C / L, as described in the first embodiment, a small amount of calcium (calcium hydroxide) is precipitated, so if it is desired to further increase the purity of magnesium hydroxide, electrolysis may be performed at a total unit volume electricity quantity of 7200 C / L before calcium (calcium hydroxide) begins to precipitate. In this case, the recovery rate of magnesium from seawater will be slightly lower than that in the case of a total unit volume electricity quantity of 10800 C / L, but magnesium can be recovered at a high purity.
[0088] In this manner, by filtering the seawater that has undergone secondary electrolysis in the second electrolysis stack 22 in the second filtration device 41, almost all of the magnesium contained in the seawater can be recovered as insoluble magnesium hydroxide, and since the recovered magnesium hydroxide contains almost no calcium carbonate or calcium hydroxide, high-purity magnesium hydroxide can be recovered.
[0089] After the secondary electrolysis, the seawater and the aqueous sodium sulfate solution are supplied to each compartment of the regeneration tank 30, as shown in FIG.
[0090] In this regeneration tank 30, as shown in FIG. 18, sodium ions that have migrated into the seawater by the first and second electrolysis pass through the cation exchange membrane and return to the aqueous sodium sulfate solution, thereby regenerating the aqueous sodium sulfate solution, and hydrogen ions in the aqueous sodium sulfate solution that has been made highly concentrated by the first and second electrolysis pass through the cation exchange membrane and migrate to the seawater side, where they react with and neutralize hydroxide ions in the seawater that has been made highly concentrated by the first and second electrolysis, thereby significantly lowering the pH value of the seawater, and the seawater with the lowered pH value can be discharged back into the sea with only magnesium having been recovered from the original seawater.
[0091] As described above, according to the embodiment, the cation exchange membrane 2b is used to separate the anode-side tank 20a having the anode 2a from the cathode-side tank 20b having the cathode 2c. Seawater, which is an aqueous solution containing magnesium ions, is introduced into the cathode-side tank 20b. Electrolysis is performed in a state in which the movement of hydroxide ions, which are anions, from the cathode-side tank 20b to the anode-side tank 20a is restricted. This makes it possible to efficiently increase the hydroxide ion concentration in the cathode-side tank 20b by electrolysis using less power, thereby improving the efficiency of magnesium hydroxide production.
[0092] Furthermore, it is possible to prevent hydroxide ions generated in the cathode side tank 20b from migrating to the anode side tank 20a and coming into contact with hydrogen ions, which are positive ions, generated in the anode side tank 20a, thereby preventing a decrease in the power efficiency of electrolysis. This improves the power efficiency of electrolysis, and since the generation of magnesium hydroxide depends on the electrical quantity per unit volume, it is also possible to accurately grasp the state of recovery (precipitation) by electrolysis based on the electrical quantity per unit volume.
[0093] Furthermore, according to the above-described embodiment, seawater, which is easily available and inexpensive, is used as the aqueous solution containing at least magnesium ions, so that magnesium can be recovered inexpensively.
[0094] Furthermore, according to the above-described embodiment, the use of a cation exchange membrane limits the movement of chlorine ions to the anode-side tank 20a, and the use of a sodium sulfate aqueous solution, which is non-chlorine-based electrolytic water that does not contain chlorine ions, in the anode-side tank 20a prevents harmful chlorine gas from being generated in the anode-side tank 20a. This makes it possible to suppress the increase in the cost of treating chlorine gas and the cost of recovering magnesium that would be caused by the use of non-chlorine-based electrolytic water.
[0095] Furthermore, according to the above-mentioned second embodiment, in the regeneration tank 30, sodium ions, which are cations reduced from the sodium sulfate aqueous solution by electrolysis, are returned from seawater to the sodium sulfate aqueous solution to be regenerated, and the regenerated sodium sulfate aqueous solution can be used repeatedly, thereby further reducing the cost of recovering magnesium.
[0096] Furthermore, according to the above-mentioned embodiment 1, the carbon dioxide contained in seawater as bicarbonate ions is removed in the degassing treatment device 12 by boiling degassing or acid-addition degassing, thereby reducing the amount of calcium carbonate that becomes mixed into the recovered magnesium hydroxide and increasing the purity of the recovered magnesium hydroxide.
[0097] Furthermore, according to the above-described first embodiment, dissolved carbon dioxide gas can be easily removed by performing boiling deaeration in which seawater is heated to boiling.
[0098] Furthermore, according to the above-mentioned second embodiment, carbon dioxide contained in seawater as bicarbonate ions is removed by performing the first electrolysis and recovering it as calcium carbonate, so that it is possible to recover high-purity magnesium hydroxide and also calcium carbonate.
[0099] Furthermore, according to the above-mentioned embodiment 2, the total unit volume electric energy applied to the electrolysis of seawater is 14,400 (3,600 + 10,800) C / L, so that it is possible to recover almost all of the magnesium ions contained in the seawater, and it is also possible to prevent calcium hydroxide contained in the seawater from being recovered together with magnesium hydroxide, which would result in a decrease in the purity of magnesium.
[0100] Furthermore, according to the embodiment described above, the electrodes constituting the anode 2a and the cathode 2c are titanium electrodes having a platinum layer on their surfaces. This makes it possible to prevent metal ions constituting the electrodes from being contained in seawater after magnesium recovery, which would have a significant impact on the environment.
[0101] Although the embodiments of the present invention have been described above with reference to the drawings, the specific configurations are not limited to these embodiments, and the present invention also includes modifications and additions that do not deviate from the gist of the present invention.
[0102] For example, in the above embodiment, an example is given of an aqueous solution containing at least magnesium ions in the form of seawater, but the present invention is not limited to this. The aqueous solution containing magnesium ions may be, for example, an aqueous solution containing magnesium ions obtained by processing magnesium minerals or the like, or may be, for example, an aqueous solution obtained by processing seawater into fresh water using a reverse osmosis membrane.
[0103] In addition, in the above embodiment, an example is given of a form in which seawater, which is an aqueous solution containing at least magnesium ions, is continuously treated, but the present invention is not limited to this. For example, these treatments may be performed in a batch form in which seawater is filled into the electrolysis stack 2 to perform electrolysis, and then the electrolyzed seawater is replaced with new seawater, and the seawater that can be stored in the electrolysis stack 2 is treated in a batch form.
[0104] In the above embodiment, in order to prevent harmful chlorine gas from being generated, an embodiment in which a sodium sulfate aqueous solution, which is non-chlorine-based electrolytic water, is introduced into the anode-side tank 20a, is exemplified. However, the present invention is not limited to this. In cases where chlorine gas can be treated or where it is desired to utilize the generated chlorine gas, seawater may be introduced into the anode-side tank 20a in the same manner as in the cathode-side tank 20b.
[0105] In the above embodiment, sodium sulfate, which is easy to obtain and inexpensive, is used as the non-chlorine electrolytic water that does not contain chlorine ions to prevent the generation of chlorine gas, but the present invention is not limited to this. The non-chlorine electrolytic water may be a sulfate other than sodium, or may be sodium nitrate or a nitrate other than sodium, and may be an aqueous solution of a water-soluble salt that does not generate chlorine gas when the aqueous solution is introduced into the anode side tank 20a and electrolyzed. When the aqueous solution introduced into the cathode side tank 20b contains a cation such as sodium ion in the case of seawater, a sulfate or nitrate containing a cation common to the cation may be used. Although an aqueous solution of these sulfates or nitrates is generally used, an aqueous solution of phosphates, oxalates, and chromates other than sulfates and nitrates may also be used. The cations that form salts with these acids can be of any type, and can be any ion such as sodium or potassium. However, when a monovalent cation exchange membrane is used, it is necessary to use monovalent cations.
[0106] In addition, in the above embodiment, the weight concentration of the sodium sulfate aqueous solution is 5%. However, these concentrations may be appropriately determined depending on the type of non-chlorine electrolyzed water used. The concentration may be such that almost no hydrogen ions generated in the anode side tank 20a move to the cathode side tank 20b, and only cations contained in the non-chlorine electrolyzed water move to the cathode side tank 20b.
[0107] In addition, in the above embodiment 2, an example is given in which seawater that has undergone secondary electrolysis is supplied to a tank other than the tank to which the sodium sulfate aqueous solution in the regeneration tank 30 is supplied, but the present invention is not limited to this. Instead of the seawater that has undergone secondary electrolysis, untreated seawater may be supplied, or an aqueous solution exclusively for regeneration may be supplied that contains a high concentration of cations, such as sodium ions, that have been reduced in the non-chlorine electrolyzed water by electrolysis.
[0108] In addition, in the above-mentioned second embodiment, the pH value of the discharged seawater is not adjusted. However, if the pH value is high, the pH value may be adjusted to a value close to that of actual seawater by adding an acid, for example.
[0109] In the above embodiment, a configuration in which both the anode 2a and the cathode 2c are platinum-plated titanium electrodes is illustrated, assuming that when deposits such as calcium carbonate or magnesium hydroxide adhere to the cathode 2c, the deposited deposits can be peeled off by switching the polarity. However, the present invention is not limited to this, and a metal electrode that does not have a platinum layer on its surface may be used for the cathode 2c.
[0110] Although not particularly implemented in the above embodiment, an additive capable of inhibiting adhesion of deposits to the electrodes may be added to the aqueous solution such as seawater supplied to the cathode side tank 20b.
[0111] Furthermore, although not specifically implemented in the above embodiment, a third electrolysis stack may be provided between the second electrolysis stack 22 and the regeneration tank 30, and the seawater after the second electrolysis and an aqueous sodium sulfate solution may be supplied to the third electrolysis stack and electrolyzed to recover calcium in the seawater as calcium hydroxide.
[0112] Furthermore, although not specifically implemented in the above embodiment, it goes without saying that hydrogen and oxygen generated by electrolysis may be recovered and utilized.
[0113] In addition, in the above embodiment, a form in which the degassing treatment device 16 is provided exclusively is exemplified, but the present invention is not limited to this, and for example, these degassing treatment devices may be provided separately, and for example, seawater used for cooling the power plant may be used as degassed seawater. [Industrial Applicability]
[0114] As an example of the application of the present invention, since seawater from which magnesium has been recovered by electrolysis does not contain carbon dioxide (bicarbonate ions), it is possible to use the seawater to absorb industrially produced carbon dioxide. [Explanation of symbols]
[0115] 1 DC power supply 2. Electrolytic stack 2a anode 2b Cation exchange membrane 2c cathode 3a flow meter 3c flow meter 4a Valve 4c Valves 6a Inverter power supply 6c Inverter power supply 7. Seawater Tank 8. Sodium sulfate solution tank 9 Anodic Solution Tank 10 Catholyte tank 11 Spare seawater tank 12 Deaeration treatment equipment 13a Inlet pipe 13c Inlet piping 14a Pump 14c Pump 16 Filtration device 20a Anode side tank 20b Cathode side tank 21 First electrolysis stack 22 No. 2 electrolysis stack 30 Regeneration tank 40 First filtration device 41 Second filtration device
Claims
[Claim 1] A method for recovering magnesium, comprising electrolyzing an aqueous solution containing at least magnesium ions to generate and recover magnesium hydroxide, which is poorly soluble in water, the method comprising the steps of: An electrolytic cell having an anode and a cathode is partitioned by a cation exchange membrane into an anode-side cell having the anode and a cathode-side cell having the cathode, and the aqueous solution is introduced into the cathode-side cell to perform electrolysis in a state in which the movement of anions from the cathode-side cell to the anode-side cell is restricted. A method for recovering magnesium.
Citation Information
Patent Citations
Method of making alkali matal carbonates
JP1979021997A
Electrolytic cation-exchange membrane and electrolytic method using the membrane
JP1995090666A
Method for reducing carbon dioxide in atmosphere and its device
JP2003326155A
Method and device for recovering magnesium
JP2012057230A