Method and system for recycling waste battery materials
The described method and system for recycling waste batteries through pressurized carbonation and specific gravity separation address inefficiencies in separating electrode materials and lithium recovery, enhancing metal recovery rates and environmental sustainability.
Patent Information
- Application Number
- PCT/KR2023/015218
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-20
- Filing Date
- 2023-10-04
- Publication Date
- 2024-10-24
AI Technical Summary
Current recycling methods for waste batteries face inefficiencies in separating positive and negative electrode materials and recovering lithium from black mass, leading to reduced metal recovery rates and potential environmental hazards due to lithium discharge into wastewater.
A method and system utilizing a pressurized carbonation step with carbon dioxide and specific gravity separation processes to recover lithium and distinguish between positive and negative electrode materials in black mass, enhancing dissolution efficiency and reducing environmental impact.
The method effectively increases the recovery rate of valuable metals like lithium, nickel, and cobalt, while minimizing environmental harm by utilizing carbon dioxide generated during recycling, thereby providing an eco-friendly recycling solution for waste batteries.
Smart Images

Figure KR2023015218_24102024_PF_FP_ABST
Abstract
Description
Method and system for recycling waste battery materials
[0001] The present disclosure relates to a method for recycling waste battery materials capable of separating not only lithium but also positive and negative electrode materials from black mass obtained from waste batteries, and comprises a pressurized carbonation step for recovering lithium in the black mass and a process for separating positive and negative electrode materials in the black mass through a difference in specific gravity, and relates to an environmentally friendly method and system for recycling waste battery materials that utilizes carbon dioxide generated during recycling of waste batteries in the separation process.
[0002] The secondary battery industry is increasingly important, positioning itself as a core technology in diverse applications ranging from smartphones and tablet PCs to electric vehicles and energy storage devices. Secondary batteries, primarily used in portable electronic devices, are undergoing active research and development amid growing concerns about the global environment and fossil fuel depletion. Demand for secondary batteries is expected to further increase with the expansion of the electric vehicle market.
[0003] In order to recover valuable metals such as nickel, cobalt, and lithium from medium and large-sized waste batteries, they are processed into a mixed powder form of positive and negative electrode materials called black mass through recycling stages such as discharging, crushing, grinding / classifying, and heat treatment.
[0004] In the process of separating and refining nickel, cobalt, and manganese from the processed black mass through the recycling process, the target metals are recovered in the form of metal compounds through a process technology commonly referred to as hydrometallurgy. Hydrometallurgy may include a step of dissolving the raw materials and a solvent extraction step that selectively extracts and purifies the target metal from the solution.
[0005] Black mass contains not only positive electrode materials (nickel, cobalt, and lithium) but also insoluble negative electrode materials (graphite), which reduces the efficiency of the dissolution process. Therefore, efforts are being made to increase the dissolution efficiency of the positive electrode materials contained in black mass by increasing the dissolution reaction time, adding additional dissolving and reducing agents, and redissolving insoluble residues to enhance the recovery of valuable metals.
[0006] In addition, if lithium contained in black mass is discharged into wastewater without a separate recovery process, it can cause environmental problems such as ecotoxicity. Therefore, various technologies for recovering lithium from spent batteries are currently being actively researched.
[0007] The present disclosure is intended to solve the aforementioned problems and to provide a method and system for recycling waste battery materials capable of separating positive and negative electrode materials as well as separating lithium from black mass obtained from waste batteries.
[0008] More specifically, the present disclosure comprises a pressurized carbonation step for recovering lithium within black mass and a process for separating positive and negative electrode materials within black mass through differences in specific gravity, and provides an environmentally friendly method and system for recycling waste battery materials that utilizes carbon dioxide generated during recycling of waste batteries in the separation process.
[0009] Other objects and advantages of the present disclosure will become more apparent from the detailed description of the invention, claims and drawings below.
[0010] The present disclosure, which aims to achieve the above-mentioned problem, relates to a method for recycling waste battery materials, which comprises a waste cathode material comprising a metal compound and a lithium compound and a waste anode material comprising graphite, comprising the steps of: a) performing a roasting process on the waste cathode material and the waste anode material of the waste battery material to produce black mass comprising the waste cathode material and the waste anode material; b) mixing and stirring the black mass with a mixing liquid to produce a black mass slurry; c) a pressurized carbonation step of introducing the black mass slurry into a carbonation reactor and reacting the black mass slurry with carbon dioxide in the carbonation reactor; and d) introducing the black mass slurry that has undergone the pressurized carbonation step into a first gravity separation device to separate the waste cathode material and the waste anode material of the black mass slurry into a first mixture and a second mixture having a specific gravity greater than that of the first mixture. It may include a first turbulent gravity separation step, e) a second turbulent gravity separation step of introducing the first mixture into a second gravity separation device and separating the first mixture into a third mixture and a fourth mixture having a greater specific gravity than the third mixture, and f) a solid / liquid separation step of separating the second mixture, the third mixture, and the fourth mixture into the metal compound, the lithium solution including the lithium compound, and the graphite.
[0011] In addition, the recycling system of waste battery materials according to the present disclosure utilizes black mass manufactured by roasting waste battery materials including waste positive electrode materials containing metal compounds and lithium compounds and waste negative electrode materials containing graphite, and may include a mixing reactor for manufacturing black mass slurry by mixing and stirring the black mass and a mixing liquid, a carbonation reactor for reacting the black mass slurry with carbon dioxide, a first gravity separation device for separating the waste positive electrode materials and the waste negative electrode materials of the black mass slurry into a first mixture and a second mixture having a greater specific gravity than the first mixture, a second gravity separation device for separating the first mixture into a third mixture and a fourth mixture having a greater specific gravity than the third mixture, and a solid-liquid separation device for separating the second mixture, the third mixture, and the fourth mixture into the metal compound, a lithium solution containing the lithium compound, and graphite.
[0012] According to the present disclosure, a method and system for recycling waste battery materials are provided, which can separate positive and negative electrode materials as well as lithium from black mass obtained from waste batteries.
[0013] More specifically, according to the present disclosure, an environmentally friendly recycling method and system for waste battery materials are provided, which comprises a pressurized carbonation step for recovering lithium in black mass and a process for separating positive and negative electrode materials in black mass through a difference in specific gravity, and utilizes carbon dioxide generated during recycling of waste batteries in the separation process.
[0014] Figure 1 is a flowchart showing a method for recycling waste battery materials according to an embodiment of the present disclosure.
[0015] Figure 2 illustrates the first gravity separation device used in the first turbulent gravity separation stage.
[0016] Figure 3 illustrates a second gravity separation device used in the second turbulent gravity separation stage.
[0017] Figure 4 illustrates a recycling system for waste battery materials according to an embodiment of the present disclosure.
[0018] The advantages and features of the present invention, and the methods for achieving them, will become clear with reference to the embodiments described in detail below together with the accompanying drawings. However, the present invention is not limited to the embodiments disclosed below, but may be implemented in various different forms. These embodiments are provided only to ensure that the disclosure of the present invention is complete and to fully inform those skilled in the art of the scope of the invention, and the present invention is defined only by the scope of the claims. Specific details for implementing the present invention will be described in detail with reference to the attached drawings. Regardless of the drawings, the same reference numerals refer to the same components, and "and / or" includes each and all combinations of one or more of the mentioned items.
[0019] The terminology used herein is for the purpose of describing embodiments and is not intended to limit the present invention. In this specification, singular forms also include plural forms, unless specifically stated otherwise. As used herein, the terms "comprises" and / or "comprising" do not exclude the presence or addition of one or more other components in addition to the components mentioned.
[0020] Unless otherwise defined, all terms (including technical and scientific terms) used herein may be used in their common sense to those of ordinary skill in the art to which the present invention pertains. Furthermore, terms defined in commonly used dictionaries are not to be interpreted ideally or excessively unless explicitly and specifically defined otherwise.
[0021] Hereinafter, a method and system for recycling waste battery materials according to an embodiment of the present invention will be described.
[0022] FIG. 1 is a flowchart showing a method for recycling waste battery materials according to an embodiment of the present invention, FIG. 2 shows a first gravity sorting device used in a first turbulent gravity sorting step, FIG. 3 shows a second gravity sorting device used in a second turbulent gravity sorting step, and FIG. 4 shows a recycling system for waste battery materials according to an embodiment of the present invention.
[0023] A method and system for recycling waste battery materials according to an embodiment of the present invention recycles waste battery materials including waste positive electrode materials containing metal compounds and lithium compounds and waste negative electrode materials containing graphite.
[0024] Referring to FIG. 1, the method for recycling waste battery materials of the present invention comprises: a) a step of performing a roasting process on the waste positive electrode material and the waste negative electrode material of the waste battery material to produce black mass including the waste positive electrode material and the waste negative electrode material; b) a step of mixing and stirring the black mass and a mixing liquid to produce a black mass slurry; c) a pressurized carbonation step of introducing the black mass slurry into a carbonation reactor and reacting the black mass slurry with carbon dioxide in the carbonation reactor; d) a first turbulent gravity separation step of introducing the black mass slurry that has undergone the pressurized carbonation step into a first gravity separation device and separating the waste positive electrode material and the waste negative electrode material of the black mass slurry into a first mixture and a second mixture having a higher specific gravity than the first mixture; and e) a second gravity separation device of introducing the first mixture into a second gravity separation device to separate the first mixture into a third mixture and a third mixture having a higher specific gravity than the third mixture. It may include a second turbulent gravity separation step for separating the large fourth mixture, and f) a solid-liquid separation step for separating the second mixture, the third mixture and the fourth mixture into the metal compound, the lithium solution including the lithium compound and the graphite.
[0025] In addition, referring to FIG. 4, the recycling system of waste battery materials according to an embodiment of the present invention to which the method is applied utilizes black mass manufactured by roasting waste battery materials including waste positive electrode materials including metal compounds and lithium compounds and waste negative electrode materials including graphite, and may include a mixing reactor for manufacturing black mass slurry by mixing and stirring the black mass and a mixing liquid, a carbonation reactor for reacting the black mass slurry with carbon dioxide, a first gravity separation device for separating the waste positive electrode materials and the waste negative electrode materials of the black mass slurry into a first mixture and a second mixture having a greater specific gravity than the first mixture, a second gravity separation device for separating the first mixture into a third mixture and a fourth mixture having a greater specific gravity than the third mixture, and a solid-liquid separation device for separating the second mixture, the third mixture, and the fourth mixture into the metal compound, a lithium solution including the lithium compound, and graphite. there is.
[0026] Black mass can be manufactured from waste battery material obtained by separating and crushing waste batteries.
[0027] More specifically, the provided waste batteries (S11) are separated, dismantled, and discharged (S12) so that they can be processed. From the separated and dismantled waste batteries, waste battery materials including waste positive and negative electrode materials are extracted.
[0028] The extracted waste battery material can be crushed and pulverized to improve the processability of the waste battery material to be processed in a subsequent process (S13).
[0029] Meanwhile, the waste battery material may include waste positive electrode material and waste negative electrode material. The waste positive electrode material may include a metal compound and a lithium compound, and the waste negative electrode material may include graphite.
[0030] The metal compound of the waste cathode material may be a compound or oxide combining nickel (Ni), cobalt (Co), manganese (Mn), etc., and may also be a composite metal thereof. In addition, the lithium compound may be an oxide or compound containing lithium (Li). The lithium compound may be, for example, lithium cobalt oxide (LiCoO2), lithium nickel cobalt manganese oxide (Li(Ni x Co y Mn z )O2), lithium manganese oxide (LiMnO2), lithium nickel cobalt aluminum oxide (Li(Ni x Co y Al z )O2) and lithium iron phosphate (LiFePO4) or a combination thereof.
[0031] A sintering process is performed on the waste cathode and anode materials obtained from waste batteries (S14). The sintering process is performed to combust or thermally decompose the binder, electrolyte, and separator materials contained within the waste batteries.
[0032] The roasting process is carried out at atmospheric pressure, and an inert gas atmosphere is generally used, but some air may be mixed in during the operation. The inert gas may be argon (Ar) or nitrogen (N₂), and air contains oxygen (O₂). That is, during the roasting process, some oxygen may also be supplied into the reactor, and the supplied oxygen may be converted into carbon dioxide (CO₂) during the roasting process. In addition, the exhaust gas discharged from the roasting process during the thermal decomposition or combustion of binders, electrolytes, and separators may contain carbon dioxide (CO2). The carbon dioxide in the exhaust gas may be supplied so that it can be used in subsequent processes such as the pressurized carbonation step, the first turbulent gravity separation step, and the second turbulent gravity separation step.
[0033] Black Mass is a battery in which nickel, cobalt, manganese, etc. exist in the form of oxides, and depending on the cathode material used, it is lithium cobalt oxide (LiCoO2), lithium nickel cobalt manganese oxide (Li(Nix Co y Mn z )O2), lithium manganese oxide (LiMnO2), lithium nickel cobalt aluminum oxide (Li(Ni x Co y Al z )O2) and lithium iron phosphate (LiFePO4) may be present alone or in combination.
[0034] Additionally, it contains approximately 3 wt% to 4 wt% of lithium, and may contain a large amount of crushed aluminum and copper, as well as graphite, the main material of the negative electrode material. The content of the negative electrode material varies depending on the recycling process used to process the black mass, and may account for approximately 20 wt% to 60 wt%.
[0035] The density of the cathode material can vary greatly depending on the true density, which is an inherent characteristic of the material. Cobalt-based cathode active material (LCO) has 5.05 g / cc, ternary cathode active material (NCM111) series has 4.7 g / cc, manganese-based cathode active material (LMO) has 4.15 g / cc, and iron phosphate-based cathode active material (LFP) has 3.6 g / cc, showing a large difference depending on the type of material. Carbon materials used as anode materials include soft carbon and graphite, and the true density of soft carbon is about 1.5 g / cc to 1.9 g / cc, and graphite can have a true density of 2.2 g / cc.
[0036] The present invention provides an eco-friendly waste battery recycling technology that separates a cathode from black mass, which is a mixture of anode and cathode with different specific gravity, by utilizing the difference in specific gravity between the two components, and recovers Li of a cathode material by utilizing carbon dioxide generated during the recycling process of waste batteries.
[0037] Next, the process for separating black mass will be described with reference to FIGS. 1 to 4.
[0038] Black mass and a mixing liquid are mixed and stirred to produce a black mass slurry (S21). This is a step of introducing black mass and a mixing liquid into a mixing reactor (30), which is a mixing facility, and mixing and stirring them to form a slurry. The mixing liquid contains water, and when the black mass and the mixing liquid are mixed, the weight ratio of the black mass and the mixing liquid may be 1:1 to 1:5.
[0039] When mixing black mass and mixing liquid, if the mixing liquid is less than the black mass, the viscosity of the slurry may increase, which may reduce processability during the process. On the other hand, if the mixing liquid is more than five times that of the black mass, the amount of liquid to be removed may increase, which may cause process delays.
[0040] After mixing the above black mass and the above mixing liquid, an additive is further added, and the additive may be MIBC (Methyl Iso Butyl Carbinol), kerosene, xylene, or sodium silicate.
[0041] The mixing reactor (30), which is a mixing facility, is not limited in its configuration, but can be used to manufacture black mass slurry using a reactor of the mortar mixer type or vessel type depending on the high-liquid ratio. The temperature inside the mixer can be operated in the range of 5°C to 50°C, and preferably, the range of 15°C to 30°C may be appropriate.
[0042] Next, the black mass slurry is introduced into a carbonation reactor (50), and a pressurized carbonation step is performed to react the black mass slurry with carbon dioxide within the carbonation reactor (50) (S22).
[0043] In this step, the lithium compound of the black mass slurry reacts with the carbon dioxide.
[0044] More specifically, this is a step of reacting carbon dioxide (CO2) gas with slurried black mass to react Li2CO3 contained in the cathode material in the black mass into LiHCO3. The solubility of Li2CO3 in water is 1.32g / 100ml at 20℃, and the solubility of Li2CO3 has the characteristic of decreasing as the temperature increases.
[0045] In comparison, the solubility of LiHCO3 in water is 5.7g / 100ml at 20℃, which is about 4.3 times higher. This can not only increase the recovery rate by improving the dissolution rate of lithium, but also reduce the energy cost incurred in the future process of purifying Li through concentration. In other words, the solubility of lithium compounds reacted with carbon dioxide in the mixing liquid increases.
[0046] The reaction between lithium compounds and carbon dioxide is illustrated / concretely as follows.
[0047] The reaction equation for generating Li2CO3 in the step of recycling black mass from waste batteries is as follows (Me = Ni, Co, Mn).
[0048] 1) 4LiMeO2+ C → 2Li2O + CO2+ 4MeO
[0049] 2) C + 2MeO + Li2O → 2Me + Li2CO3
[0050] Bicarbonate reaction equation: Li2CO3+ CO2+ H2O → 2LiHCO3
[0051] The carbon dioxide can be supplied from the exhaust gas emitted during the above-described combustion process. That is, the carbon dioxide utilized in the above-described step is contained in the exhaust gas generated during the process of manufacturing black mass from spent batteries. The exhaust gas is ultimately processed through an air quality reduction facility, including secondary combustion treatment, and the carbon dioxide contained in the processed exhaust gas is then supplied to a pressurized carbonation reaction.
[0052] The pressure within the carbonation reactor in which the reaction between the lithium compound and the carbon dioxide takes place may be 1.1 bar to 3 bar, and preferably 1.3 bar to 1.7 bar.
[0053] Next, the black mass slurry that has gone through the pressurized carbonation step is fed into a first gravity separation device (100), and a first turbulent gravity separation step is performed to separate the waste anode material and the waste cathode material of the black mass slurry into a first mixture and a second mixture having a higher specific gravity than the first mixture (S23). In the large-scale turbulent gravity separation step, the waste anode material and the waste cathode material in the black mass slurry are separated through gravity separation after the pressurized carbonation step, and in this step, the process can be performed by dividing it into a mixing section and a separation section.
[0054] Referring to Fig. 2, the first gravity separation device (100) may include a mixing unit (MX), a first separation unit (SP1), and a second separation unit (SP2). Here, the black mass slurry is introduced into the mixing unit through an inlet (103), and the first turbulent gravity separation step is initiated.
[0055] In the mixing section (MX), the black mass slurry can be moved to the upper part of the first gravity separation device (100). In the mixing section (MX), the introduced black mass slurry is rotated at a high speed to mix and simultaneously move the black mass slurry to the upper part of the first gravity separation device (100). There is no limitation on the shape of the first impeller (111) utilized in the mixing section (MX), but preferably, a turbine-type impeller or a paddle-type impeller can be applied. The first impeller (111) located in the mixing section (MX) can rotate at a first speed. The first speed is a high speed that is faster than the second speed of the second impeller of the first separation section to be described later.
[0056] Continuing, the black mass slurry at the top of the first gravity separation device (100) moves from the mixing unit (MX) to the first separation unit (SP1). In the first separation unit (SP1), the waste cathode material and waste anode material of the black mass slurry are separated by the difference in specific gravity. A portion of the first mixture and the second mixture may move to the top of the first gravity separation device, and another portion of the second mixture may settle to the bottom of the first gravity separation device.
[0057] More specifically, in the first separation section (SP1), a second impeller (112) that slowly stirs the slurry that has moved upwards can be placed to float low-density materials. That is, the second impeller (112) can rotate at a second speed that is lower than the first speed. The second impeller (112) utilized is not limited in form, but preferably, an anchor-type impeller can be utilized singly or in multiples.
[0058] Additionally, a screen (131) may be placed at the top of the lower sedimentation tank to ensure that only fine, heavy materials (i.e., other portions of the second mixture) ultimately move to the bottom. The screen size for particle size separation may be determined based on the particle size of the black mass processed in the recycling step, and may generally be configured in the range of 200 mesh to 40 mesh.
[0059] Subsequently, the first mixture and a portion of the second mixture move from the first separation unit (SP1) to the second separation unit (SP2). Thereafter, the first mixture remains in the upper portion of the first gravity separation device (100), and a portion of the second mixture settles downwards of the first gravity separation device (100).
[0060] A portion of the second mixture that has settled in the second separation unit (SP2) and another portion of the second mixture that has settled in the first separation unit (SP1) are collected at the bottom of the first gravity separation device (100) to form a second mixture. The second mixture is discharged through the outlet (141) of the first gravity separation device (100) and moves to the solid / liquid separation step.
[0061] Meanwhile, when separating the black mass slurry into the first mixture and the second mixture, carbon dioxide contained in the exhaust gas discharged from the combustion process can be injected into the first separation unit (SP1) and the second separation unit (SP2).
[0062] More specifically, the lower sedimentation tanks of the first separation unit (SP1) and the second separation unit (SP2) are configured to generate bubbles by injecting gas discharged from the roasting process in the same manner as the pressurized carbonation step. At this time, the smaller and more uniform the bubble size, the more effective it is, and preferably, it can be configured to generate ultra-small bubbles (microbubbles) of 50㎛ or less. Carbon dioxide injected from the bottom induces a bicarbonation reaction, and lithium bicarbonate generated after the reaction can be dissolved in a liquid phase.
[0063] The upper bubble layer can move to the next stage, the second turbulent gravity separation stage, through the upper discharge port (142, 143) consisting of two ports, and the flow rate and water level can be controlled by linking the control valve (151, 152) connected to the upper and lower ports (142, 143) through the water level gauge inside the first gravity separation device (100).
[0064] Subsequently, the first mixture is fed into the second gravity separation device (200), and a second turbulent gravity separation step is performed to separate the first mixture into a third mixture and a fourth mixture having a higher specific gravity than the third mixture (S24). In this step, the cathode materials floating together in the floating layer of the first turbulent gravity separation step are separated once more through the density difference. In the same way as the first turbulent gravity separation step, a screen (211) is placed at the top of the lower sedimentation tank so that only fine and heavy particles (i.e., the fourth mixture) fall to the bottom. The bottom of the sedimentation tank can be configured to induce an additional bicarbonation reaction by introducing a gas containing carbon dioxide.
[0065] Specifically, among the first mixtures fed into the second gravity sorting device (200), the fourth mixture with a relatively high specific gravity settles to the bottom of the second gravity sorting device, and the third mixture with a relatively low specific gravity moves to the top of the second gravity sorting device (200). Here, the screen size for particle size separation can be determined according to the particle size of the black mass processed in the recycling step, and can generally be configured in the range of 200 mesh to 40 mesh.
[0066] Meanwhile, when separating the first mixture into the third mixture and the fourth mixture, carbon dioxide contained in the exhaust gas discharged from the combustion process can be injected into the second gravity separation device (200). At this time, bubbles can be formed by the carbon dioxide, and the smaller and more uniform the bubble size, the more effective it is. Preferably, the bubbles can be configured to generate ultra-small bubbles (microbubbles) of 50㎛ or less.
[0067] The upper bubble layer can move to the next stage (solid / liquid separation stage) through the upper discharge port (222, 223) consisting of two ports, and the flow rate and water level can be controlled by linking the control valve (231, 232) connected to the upper and lower ports (222, 223) through the water level gauge inside the second specific gravity separation device (200).
[0068] Next, a solid / liquid separation step is performed to separate the second mixture, the third mixture, and the fourth mixture into a metal compound, a lithium solution containing a lithium compound, and graphite (S25, S26). Specifically, in the solid / liquid separation step, the remaining powder as an insoluble component and the liquid phase in which lithium is dissolved are separated using a solid-liquid separation device (301, 302), and a filter press is utilized, but the solid-liquid separation device (301, 302) is not limited thereto.
[0069] The second and fourth mixtures can be separated into metal compounds and a portion of the lithium solution through a solid / liquid separation step. Furthermore, the third mixture can be separated into graphite and another portion of the lithium solution through a solid / liquid separation step. That is, by separating the third mixture, which is the upper slurry collected in the second turbulent gravity separation step, into solid / liquid fractions, powders with a high content of negative electrode material (mainly graphite) can be recovered, and a lithium solution can be obtained.
[0070] A portion of the above lithium solution and another portion of the above lithium solution are collected in a liquid supply tank (401) and combined into a lithium solution.
[0071] The lithium solution can be recycled as process water. That is, the lithium solution obtained in the step can be recycled to the carbonation reactor (50), the first gravity separation device (100), or the second gravity separation device (200) described above. At this time, the lithium concentration in the lithium solution can be concentrated to about 20,000 ppm to 30,000 ppm through process circulation.
[0072] By the above recycling, when the lithium concentration in the lithium solution increases, the lithium solution can be stored in the liquid storage tank (402) without recycling. The separately stored lithium solution can be further concentrated through a crystallization process to crystallize lithium.
[0073] Hereinafter, the present invention will be described in more detail through examples. These examples are intended solely to illustrate the present invention more specifically, and it will be apparent to those skilled in the art that the scope of the present invention is not limited by these examples, in accordance with the gist of the present invention.
[0074] 1. Black Mass Slurry Preparation
[0075] In order to confirm the components of black mass containing Ni, Co, Li, and graphite, 1 g of raw material was dissolved in 10 ml of aqua regia, and the main composition and impurities were confirmed as follows using high-frequency inductively coupled plasma (ICP-OES) equipment and a C / S analyzer.
[0076] sampleNiCoMnLiCarbonwt%ppmWaste Battery MaterialBlack Mass18.905.985.4741,292432,000
[0077] 100 parts by weight of black mass, a waste battery material, and 300 parts by weight of a mixed liquid were stirred at room temperature at a stirring speed of 300 rpm to secure a uniform slurry. After stirring, the slurry was placed in a pressurized reactor, and CO2 gas was added at a speed of 50 cc / min under room temperature conditions, and the reaction was performed at a pressure of 1.5 bar for 30 minutes to obtain 400 parts by weight of a slurry for gravity separation.
[0078] 2. 1st turbulent gravity separation stage
[0079] For gravity separation, 400 parts by weight of slurry was added to a floating reactor containing 600 parts by weight of water, and before separation, 0.8 parts by weight of MIBC (Methyl Iso Butyl Carbinol) and 1.2 parts by weight of sodium silicate were added as additives.
[0080] The slurry that was floated to the top through high-speed stirring at 1000 rpm in the flotation reactor was collected, bubbled with CO2 gas, and injected into the upper part of the flotation reactor while being stirred at 200 rpm. The formed froth layer was collected and continuously injected into a flotation separation tank into which CO2 gas was being injected without stirring, and was ultimately separated into 627 parts by weight of settled slurry and 373 parts by weight of upper froth layer slurry.
[0081] After gravity sorting, slurry samples of the upper foam layer and sedimentation layer, which are intermediate separated materials, were collected and separated into solid and liquid phases, and the components were analyzed using an ICP-OES analyzer and a C / S analyzer for the liquid and solid phase samples.
[0082] sampleNiCoMnLiCarbonwt%ppm1st flotation slurry residue9.043.243.049,688661,0001st flotation slurry filtrate0.000.000.001,824-1st settling slurry residue24.817.887.1518,732231,0001st settling slurry filtrate0.000.000.001,883-
[0083] 3. Secondary turbulent gravity separation stage
[0084] CO2 gas was added without stirring to 373 parts by weight of the upper froth layer slurry recovered in the first turbulent gravity separation step, and the negative electrode material and positive electrode material were additionally separated through the density difference in the second gravity separation device. 291 parts by weight of slurry were recovered from the upper froth layer and 82 parts by weight of slurry from the sedimentation layer. After gravity separation, slurry samples from the upper froth layer and sedimentation layer, which are the separated materials, were collected and solid / liquid separated, and the components of the liquid and solid samples were analyzed using an ICP-OES analyzer and a C / S analyzer.
[0085] sampleNiCoMnLiCarbonwt%ppmSecondary flotation slurry residue7.292.662.4911,471826,000Secondary flotation slurry filtrate0.000.000.001,579-Secondary settling slurry residue10.043.523.3012,565239,000Secondary settling slurry filtrate0.000.000.001,557-
[0086] 4. High / Liquid Separation Stage
[0087] The upper froth layer slurry and the first and second sedimentation layer slurries obtained in the first and second turbulent gravity separation stages were filtered under reduced pressure to separate the solid and liquid phases. Finally, the filtered sedimentation layer residue was classified as a metal compound (high-grade black mass), the upper froth layer slurry residue as a spent cathode material (graphite), and the aqueous phase as a lithium solution. The components of the finally obtained materials were identified using an ICP-OES analyzer and a C / S analyzer.
[0088] sampleNiCoMnLiCarbonwt%ppmSpent cathode material7.292.662.4911,471826,000Metal compound (high-quality black mass)21.126.796.1817,192233,000Lithium solution0.000.000.001,773-
[0089] While the embodiments of the present invention have been described above, the present invention is not limited to the above embodiments, but can be manufactured in various different forms. Those skilled in the art will understand that the present invention can be implemented in other specific forms without altering the technical spirit or essential characteristics of the present invention. Therefore, the embodiments described above should be understood to be illustrative in all respects and not restrictive.
Claims
1. A method for recycling waste battery materials, including waste positive electrode materials containing metal compounds and lithium compounds and waste negative electrode materials containing graphite, a) A step of performing a sintering process on the waste positive electrode material and the waste negative electrode material of the waste battery material to produce a black mass including the waste positive electrode material and the waste negative electrode material; b) A step of mixing and stirring the black mass and the mixing liquid to prepare a black mass slurry; c) A pressurized carbonation step of introducing the black mass slurry into a carbonation reactor and reacting the black mass slurry with carbon dioxide in the carbonation reactor; d) A first turbulent gravity separation step in which the black mass slurry that has gone through the pressurized carbonation step is injected into a first gravity separation device to separate the waste anode material and the waste cathode material of the black mass slurry into a first mixture and a second mixture having a higher specific gravity than the first mixture; e) a second turbulent gravity separation step of introducing the first mixture into a second gravity separation device to separate the first mixture into a third mixture and a fourth mixture having a higher specific gravity than the third mixture; and f) A method for recycling waste battery materials, comprising a solid / liquid separation step of separating the second mixture, the third mixture, and the fourth mixture into the metal compound, the lithium solution containing the lithium compound, and the graphite.
2. In paragraph 1, The above mixing liquid contains water, and when the black mass and the mixing liquid are mixed, the weight ratio is 1:1 to 1:
5. A method for recycling waste battery materials, characterized in that after mixing the black mass and the mixing liquid, an additive is further added, wherein the additive is MIBC (Methyl Iso Butyl Carbinol), kerosene, xylene, or sodium silicate.
3. In paragraph 1, A method for recycling waste battery materials, characterized in that, in the pressurized carbonation step, the lithium compound of the black mass slurry reacts with the carbon dioxide.
4. In paragraph 3, The lithium compound reacted with the carbon dioxide has an increased solubility in the mixed liquid, The above carbon dioxide is supplied from the exhaust gas emitted during the above combustion process, A method for recycling waste battery materials, characterized in that the pressure within the carbonation reactor in which the lithium compound and the carbon dioxide react is 1.1 bar to 3 bar.
5. In paragraph 1, The above first gravity separation device includes a mixing unit, a first separation unit, and a second separation unit, A method for recycling waste battery materials, characterized in that the black mass slurry is introduced into the mixing unit and the first turbulent gravity separation step is initiated.
6. In paragraph 5, A method for recycling waste battery materials, characterized in that the black mass slurry in the above mixing unit is moved to the upper part of the first specific gravity sorting device.
7. In paragraph 6, The above black mass slurry moves from the mixing unit to the first separation unit, A method for recycling waste battery materials, characterized in that in the first separation unit, the waste positive electrode material and the waste negative electrode material of the black mass slurry are separated by a difference in specific gravity, wherein a part of the first mixture and the second mixture moves to the upper part of the first specific gravity separation device, and another part of the second mixture settles to the lower part of the first specific gravity separation device.
8. In paragraph 7, A portion of the first mixture and the second mixture are moved from the first separation unit to the second separation unit, A method for recycling waste battery materials, characterized in that the first mixture remains in the upper portion of the first gravity separation device, and a portion of the second mixture settles downwards of the first gravity separation device.
9. In paragraph 8, When separating the above black mass slurry into the first mixture and the second mixture, A method for recycling waste battery materials, characterized in that carbon dioxide contained in the exhaust gas discharged from the combustion process is injected into the first separating unit and the second separating unit.
10. In paragraph 1, Among the first mixtures fed into the second gravity sorting device, the fourth mixture having a relatively high specific gravity settles downwards of the second gravity sorting device, A method for recycling waste battery materials, characterized in that the third mixture having a relatively small specific gravity moves to the upper part of the second specific gravity sorting device.
11. In paragraph 10, When separating the first mixture into the third mixture and the fourth mixture, A method for recycling waste battery materials, characterized in that carbon dioxide contained in the exhaust gas discharged from the above-described combustion process is injected into the above-described second gravity sorting device.
12. In paragraph 1, The second mixture and the fourth mixture are separated into the metal compound and a portion of the lithium solution through the solid / liquid separation step, A method for recycling waste battery materials, characterized in that the third mixture is separated into the graphite and another portion of the lithium solution through the solid / liquid separation step.
13. In paragraph 1, A method for recycling waste battery materials, characterized in that the lithium solution obtained in the solid / liquid separation step is recycled to the carbonation reactor, the first gravity separation device, or the second gravity separation device.
14. In paragraph 13, A method for recycling waste battery materials, characterized in that when the lithium concentration in the lithium solution increases through the above recycling, the lithium solution is stored separately without being recycled.
15. In a recycling system for waste battery materials utilizing black mass manufactured by burning waste battery materials including waste positive electrode materials containing metal compounds and lithium compounds and waste negative electrode materials containing graphite, A mixing reactor for mixing and stirring the black mass and a mixing liquid to produce a black mass slurry; A carbonation reactor for reacting the above black mass slurry with carbon dioxide; A first gravity separation device for separating the waste anode material and the waste cathode material of the black mass slurry into a first mixture and a second mixture having a higher specific gravity than the first mixture; A second gravity separation device that separates the first mixture into a third mixture and a fourth mixture having a higher specific gravity than the third mixture; and A recycling system for waste battery materials, comprising a solid-liquid separation device that separates the second mixture, the third mixture, and the fourth mixture into the metal compound, a lithium solution containing the lithium compound, and graphite.
Citation Information
Patent Citations
Recycling method of waste lithium ion power battery
CN108400400A
Method for recovering lithium carbonate and nickel-cobalt-manganese mixed metal oxide from waste lithium battery of ternary positive electrode material
CN111960443A
Physical sorting and recycling method for positive and negative electrode materials of waste ternary lithium battery
CN112736314A
Method for pressurizing and roasting waste lithium battery black powder to fix fluorine and extract lithium
CN114132951A
Process for recovering values from batteries
WO2022032345A1
Cited By
Lithium and graphite recycled from black mass
WO2025125598A1