Electro-conductive contact pin

The contact pin design addresses the reliability issues of conventional MEMS contact pins by alternately stacking high elastic modulus and high conductivity metal layers, ensuring continuous material continuity and improved conductivity, thus enhancing connection reliability and reducing deformation.

WO2024219730A1PCT designated stage expired Publication Date: 2024-10-24POINT ENG
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/KR2024/004650
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-18
Filing Date
2024-04-08
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Conventional MEMS contact pins face limitations in improving connection reliability due to the difficulty in thinning the tip portion without forming nodes and reducing the continuity of the metal material, leading to increased electrical resistance and deformation issues.

Method used

The contact pin design alternately stacks first metal layers with high elastic modulus and second metal layers with high electrical conductivity, with specific thickness and content ratios in different regions, ensuring continuous material continuity from the body to the tip, and includes fine trenches for enhanced performance.

Benefits of technology

This design enhances connection reliability by maintaining material continuity, increasing rigidity, and improving electrical conductivity, while minimizing deformation and resistance issues.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure KR2024004650_24102024_PF_FP_ABST
    Figure KR2024004650_24102024_PF_FP_ABST
Patent Text Reader

Abstract

The present invention provides an electro-conductive contact pin with improved connection reliability. The electro-conductive contact pin includes: a body portion in which a plurality of first metal layers including a metal having a relatively high elastic modulus and a plurality of second metal layers including a metal having a relatively high electrical conductivity are alternately stacked in the thickness direction; and a tip portion provided at the front end portion of the body portion in the longitudinal direction. The body portion may include a first thickness area continuously connected to the tip portion in the longitudinal direction and a second thickness area provided on the upper portion of the first thickness area in the thickness direction, and the thickness of the first metal layer in the first thickness area is in the range of 1.1 to 50.0 times the thickness of the second metal layer.
Need to check novelty before this filing date? Find Prior Art

Description

electrically conductive contact pins

[0001] The present invention relates to an electrically conductive contact pin.

[0002] Electrical characteristic tests of semiconductor devices are performed by bringing a test object (semiconductor wafer or semiconductor package) close to a test device equipped with a plurality of electrically conductive contact pins and contacting the electrically conductive contact pins with corresponding electrode pads (or solder balls or bumps) on the test object.

[0003] When an electrically conductive contact pin is brought into contact with an electrode pad on an object to be inspected, after the two have reached a state where they begin to make contact, a process is performed to further bring the object to be inspected closer. This process is called overdrive. Overdrive is a process in which the electrically conductive contact pin is elastically deformed, and by performing overdrive, all the electrically conductive contact pins can be brought into secure contact with the electrode pad even if there is a deviation in the height of the electrode pad or the height of the electrically conductive contact pin. In addition, when the electrically conductive contact pin is elastically deformed during overdrive, and its tip moves on the electrode pad, thereby performing scrubbing. This scrubbing removes the oxide film on the surface of the electrode pad, which can reduce the contact resistance.

[0004] Electrically conductive contact pins can be manufactured using the MEMS process. The process of manufacturing electrically conductive contact pins using the MEMS process involves first applying a photoresist film to the surface of a conductive substrate and then patterning the photoresist film. Then, using the photoresist film as a mold, a metal material is deposited on the exposed surface of the conductive substrate within the opening via electroplating. The photoresist film and the conductive substrate are then removed to obtain a contact pin. Electrically conductive contact pins manufactured using the MEMS process are referred to herein as MEMS contact pins. The shape of the MEMS contact pin is identical to the shape of the opening formed in the mold of the photoresist film.

[0005] In this way, since the thickness of the photoresist film of the conventional MEMS contact pin is thin, such as about 30㎛, it is difficult to form the thickness of only the tip portion thinner than the thickness of the body portion using a single photoresist film. On the other hand, in order to form the tip portion of the contact pin thinner to a different thickness from the thickness of the body portion, the process of applying the photoresist film must be performed multiple times. In this case, there is a problem that deformation easily occurs because knots are formed like bamboo at each layer change portion on the side of the MEMS contact pin. In addition, since the tip portion is formed of a separate metal material different from the body portion, the continuity as the same material as the metal material of the body portion is reduced, which causes a problem of increased electrical resistance.

[0006] Therefore, conventional MEMS contact pins have limitations in improving connection reliability.

[0007] [Prior Art Literature]

[0008] [Patent Document]

[0009] (Patent Document 1) Republic of Korea Patent Publication No. 10-2018-0004753

[0010] The present invention has been devised to solve the problems of the above-described prior art, and its purpose is to provide an electrically conductive contact pin with improved connection reliability.

[0011] In order to achieve the above-described object of the present invention, an electrically conductive contact pin according to the present invention comprises a body portion in which a plurality of first metal layers made of a metal having a relatively large elastic modulus and a plurality of second metal layers made of a metal having a relatively large electrical conductivity are alternately laminated in a thickness direction; and a tip portion provided at a front end of the body portion in a lengthwise direction; wherein the body portion comprises a first thickness region continuously connected to the tip portion in a lengthwise direction; and a second thickness region provided on an upper portion of the first thickness region in a thicknesswise direction; wherein a thickness of the first metal layer in the first thickness region is in a range of 1.1 times or more and 50.0 times or less than a thickness of the second metal layer.

[0012] Additionally, in the first thickness region, the content of the first metal layer is greater than the content of the second metal layer.

[0013] In addition, the thickness direction dimensions and the length direction dimensions of the plurality of first metal layers in the first thickness region are the same, and the thickness direction dimensions and the length direction dimensions of the plurality of second metal layers in the first thickness region are the same.

[0014] In addition, the second thickness region includes a surface layer composed of one of the first metal layers; and an inner multilayer portion provided below the surface layer in the thickness direction and having a plurality of the first metal layers and a plurality of the second metal layers alternately laminated; and the inner multilayer portion is located between the surface layer and the first thickness region.

[0015] In addition, the content of the second metal layer in the inner multilayer portion is greater than the content of the first metal layer in the inner multilayer portion, and the thickness of the second metal layer in the inner multilayer portion has a range of 1.1 times or more and 50.0 times or less than the thickness of the first metal layer.

[0016] Additionally, the content of the first metal layer constituting the surface layer in the second thickness region is greater than the content of the first metal layer in the inner multilayer portion.

[0017] In addition, the thickness direction dimensions of the plurality of second metal layers in the inner multilayer portion are the same, and the thickness direction dimensions of the plurality of first metal layers in the inner multilayer portion are the same.

[0018] In addition, the plurality of first metal layers and the plurality of second metal layers in the second thickness region have a lengthwise dimension that increases from top to bottom in the thickness direction.

[0019] Additionally, micro trenches are provided on the side of the body portion and the side of the tip portion.

[0020] According to another feature of the present invention, an electrically conductive contact pin is provided in which a plurality of first metal layers and a plurality of second metal layers are alternately laminated in the thickness direction, wherein the first metal layer is a metal having a relatively large elastic modulus compared to the second metal layer, the second metal layer is a metal having a relatively large electrical conductivity compared to the first metal layer, and is divided into a first thickness region and a second thickness region in the thickness direction, and a tip portion is provided at an end in the longitudinal direction of the first thickness region that protrudes more than the second thickness region in the longitudinal direction, and a thickness of the first metal layer in the first thickness region is in a range of 1.1 times or more and 50.0 times or less than a thickness of the second metal layer.

[0021] In addition, the second thickness region is divided into a surface region formed by the first metal layer and an internal region formed by laminating the first metal layer and the second metal layer and positioned between the surface region and the first thickness region.

[0022] Additionally, in the inner region, the thickness of the second metal layer has a range of 1.1 times to 50.0 times the thickness of the first metal layer.

[0023] Additionally, the thickness of the first metal layer of the surface region has a range of 1.1 times to 100.0 times the thickness of the first metal layer of the inner region.

[0024] Additionally, the first thickness region excluding the tip portion matches the shape of the second thickness region.

[0025] Additionally, the total thickness of the plurality of first metal layers is the same as the total thickness of the plurality of second metal layers.

[0026] In addition, the side surfaces of the first thickness region and the second thickness region are provided with a plurality of fine trenches formed in a long fine groove along the thickness direction and formed in parallel along the entire side surface.

[0027] In addition, the electrically conductive contact pin includes a first surface and a second surface opposite the first surface, the side surface being a surface connecting the first surface and the second surface, and the micro-trench is not formed on the first surface and the second surface.

[0028] In addition, the thickness of the first metal layer provided on the surface of the second thickness region has a range of 1.1 times or more and 50.0 times or less than the thickness of the first metal layer provided on the surface of the first thickness region.

[0029] According to another feature of the present invention, an electrically conductive contact pin is provided in which a plurality of first metal layers and a plurality of second metal layers are laminated in the thickness direction, wherein the first metal layer is a metal having a relatively large elastic modulus compared to the second metal layer, the second metal layer is a metal having a relatively large electrical conductivity compared to the first metal layer, and the first metal layer is divided into a first thickness region and a second thickness region in the thickness direction, and a tip portion is provided at an end in the longitudinal direction of the first thickness region that protrudes more than the second thickness region in the longitudinal direction, and the second thickness region is divided into a surface region provided with the second metal layer, and an internal region provided by laminating the second metal layer and the second metal layer and positioned between the surface region and the first thickness region, and a content of the first metal layer in the first thickness region is greater than a content of the first metal layer in the internal region, and a content of the second metal layer in the first thickness region is less than a content of the second metal layer in the internal region.

[0030] According to another feature of the present invention, an electrically conductive contact pin is provided in which a plurality of first metal layers and a plurality of second metal layers are alternately laminated in the thickness direction, wherein the first metal layer is a metal having a relatively large elastic modulus compared to the second metal layer, the second metal layer is a metal having a relatively large electrical conductivity compared to the first metal layer, and is divided into a first thickness region and a second thickness region in the thickness direction, and a tip portion protruding more than the second thickness region in the length direction is provided at an end portion in the length direction of the first thickness region, and a thickness of the second metal layer in the second thickness region is in a range of 1.1 times or more and 50.0 times or less than a thickness of the second metal layer in the first thickness region.

[0031] The present invention provides an electrically conductive contact pin having improved connection reliability as a body portion and a tip portion have metal layers of the same material formed continuously in the longitudinal direction.

[0032] In addition, the present invention provides an electrically conductive contact pin having improved connection reliability by securing high rigidity by increasing the content of the first metal layer compared to the second metal layer in the first thickness region and by providing excellent electrical conductivity by increasing the content of the second metal layer compared to the first metal layer in the second thickness region.

[0033] Figure 1 is a plan view of an electrically conductive contact pin according to a preferred embodiment of the present invention.

[0034] Figure 2a is an enlarged view of part A of Figure 1, and Figure 2b is a perspective view of Figure 2a.

[0035] Figure 3 is an enlarged view of the tip of Figures 2a and 2b.

[0036] Figures 4a to 4d are side views of Figure 3 viewed in the width direction (±x direction).

[0037] Figure 5a is an enlarged view of part B of Figure 1, and Figure 5b is a perspective view of Figure 5a.

[0038] Fig. 6 is a side view of Fig. 5b viewed in the width direction (±x direction).

[0039] Figure 7a is an enlarged view of part C of Figure 1, and Figure 7b is a perspective view of Figure 7a.

[0040] Figure 8a is an enlarged view of part D of Figure 1, and Figure 8b is a perspective view of Figure 8a.

[0041] FIG. 9 is a drawing illustrating an inspection device having an electrically conductive contact pin installed according to a preferred embodiment of the present invention.

[0042] The following merely exemplifies the principles of the invention. Therefore, those skilled in the art will be able to implement the principles of the invention and invent various devices within the scope and spirit of the invention, even if not explicitly described or illustrated herein. Furthermore, all conditional terms and embodiments listed herein are expressly intended, in principle, to facilitate understanding of the invention's concepts and should be understood as being solely intended to facilitate understanding and are not intended to be limited to the specifically enumerated embodiments and conditions.

[0043] The above-described purposes, features and advantages will become clearer through the following detailed description with reference to the attached drawings, so that a person having ordinary skill in the art to which the invention pertains can easily practice the technical idea of ​​the invention.

[0044] Embodiments described herein will be described with reference to cross-sectional and / or perspective views, which are ideal illustrations of the present invention. The thicknesses of the membranes and regions depicted in these drawings are exaggerated for the purpose of effectively explaining the technical contents. The shapes of the illustrations may be modified due to manufacturing techniques and / or tolerances. Furthermore, the number of molded articles depicted in the drawings is only a partial example. Therefore, embodiments of the present invention are not limited to the specific shapes depicted, but also include variations in shapes resulting from the manufacturing process.

[0045] In describing various embodiments, components that perform the same function will be given the same names and reference numbers for convenience, even if the embodiments differ. Furthermore, configurations and operations already described in other embodiments will be omitted for convenience.

[0046] Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the drawings.

[0047] The width direction of the electrically conductive contact pin (100) described below is the ±x direction indicated in the drawing, the length direction of the electrically conductive contact pin (100) is the ±y direction indicated in the drawing, and the thickness direction of the electrically conductive contact pin (100) is the ±z direction indicated in the drawing.

[0048] An electrically conductive contact pin (100) is provided in an inspection device (10) and is used to transmit an electrical signal by making electrical and physical contact with an inspection target. The inspection device (10) includes an electrically conductive contact pin (100) that makes contact with the inspection target. The inspection device (10) may be an inspection device (10) used in a semiconductor manufacturing process, and may be, for example, a probe card or a test socket. The inspection device of the present invention is not limited thereto, and any device for applying electricity to check for defects in an inspection target is included.

[0049] FIG. 1 is a plan view of an electrically conductive contact pin (100), FIG. 2a is an enlarged view of part A of FIG. 1, FIG. 2b is a perspective view of FIG. 2a, FIG. 3 is an enlarged view of the tip of FIGS. 2a and 2b, FIGS. 4a to 4d are side views of FIG. 3 when viewed in the width direction (±x direction), FIG. 5a is an enlarged view of part B of FIG. 1, FIG. 5b is a perspective view of FIG. 5a, FIG. 6 is a side view of FIG. 5b when viewed in the width direction (±x direction), FIG. 7a is an enlarged view of part C of FIG. 1, FIG. 7b is a perspective view of FIG. 7a, FIG. 8a is an enlarged view of part D of FIG. 1, FIG. 8b is a perspective view of FIG. 8a, and FIG. 9 is a drawing showing an inspection device (10) in which an electrically conductive contact pin (100) is installed.

[0050] An electrically conductive contact pin (100) includes a body portion (BP) in which a plurality of first metal layers (101) and a plurality of second metal layers (102) are alternately laminated in the thickness direction (±z direction), and a tip portion (TP) provided at the tip end of the body portion (BP) in the length direction (±y direction).

[0051] An electrically conductive contact pin (100) has a first surface (upper surface in the +z direction) of the electrically conductive contact pin (100), a second surface (lower surface in the +z direction) of the electrically conductive contact pin (100) opposite to the first surface of the electrically conductive contact pin (100), and a side surface connecting the first surface of the electrically conductive contact pin (100) and the second surface of the electrically conductive contact pin (100). A tip portion of the electrically conductive contact pin (100) in the longitudinal direction (±y direction) is connected to a circuit board side, and a lower portion of the electrically conductive contact pin (100) in the longitudinal direction (±y direction) is connected to an inspection target side. Here, the inspection target may be a semiconductor wafer.

[0052] The body portion (BP) is a portion that is long in the longitudinal direction (±y direction) and is elastically deformable. The electrically conductive contact pin (100) is arranged perpendicular to the inspection object and is elastically deformable in the width direction (±x direction) during the overdrive process through the body portion (BP).

[0053] The cross-section of the body portion (BP) is formed as a square cross-section. In this case, the guide holes of the upper guide plate (GP1) and the lower guide plate (GP2) may be provided with a square cross-section corresponding to the cross-sectional shape of the body portion (BP). The electrically conductive contact pin (100) is prevented from rotating within the guide hole through the configuration of the body portion (BP) with a square cross-section and the guide hole with a square cross-section, so that the elastic deformation direction of the body portion (BP) becomes a constant direction. This prevents interference between each electrically conductive contact pin (100) provided corresponding to each of the plurality of guide holes, thereby enabling implementation of a narrow pitch of the electrically conductive contact pin (100).

[0054] The body portion (BP) is composed of a plurality of metal layers. Specifically, the body portion (BP) is composed of a plurality of first metal layers (101) composed of a metal having a relatively high elastic modulus, and a plurality of second metal layers (102) composed of a metal having a relatively high electrical conductivity, wherein the first and second metal layers (101, 102) are alternately laminated.

[0055] The first metal layer (101) is preferably formed of a metal having a relatively high elastic modulus or wear resistance compared to the second metal layer (102), and is preferably formed of a metal selected from among rhodium (Rd), platinum (Pt), iridium (Ir), palladium (Pd), nickel (Ni), manganese (Mn), tungsten (W), phosphorus (Ph), or an alloy thereof, or a palladium-cobalt (PdCo) alloy, a palladium-nickel (PdNi) alloy, a nickel-phosphorus (NiPh) alloy, a nickel-manganese (NiMn), nickel-cobalt (NiCo), or a nickel-tungsten (NiW) alloy. The plurality of first metal layers (101) may be of the same kind of metal or of different kinds of metal.

[0056] The second metal layer (102) is formed of a metal having a relatively high electrical conductivity compared to the first metal layer (101), and is preferably formed of a metal selected from among copper (Cu), silver (Ag), gold (Au), or an alloy thereof. The plurality of second metal layers (102) may be of the same type of metal or of different types of metal.

[0057] The first metal layer (101) is provided on the upper and lower surfaces in the thickness direction (±z direction) of the body portion (BP), and the second metal layer (102) is provided between the first metal layers (101). For example, the body portion (BP) may be provided by alternately stacking the first metal layer (101), the second metal layer (102), and the first metal layer (101) in that order from the bottom based on the thickness direction (±z direction). The number of stacked layers may be three or more, and preferably, the body portion (BP) may be provided by stacking 17 metal layers. The drawing illustrates a body portion (BP) provided by stacking 15 metal layers.

[0058] Referring to FIGS. 2 to 6, the body portion (BP) includes a first thickness region (F1) continuously connected to the tip portion (TP) in the longitudinal direction (±y direction) and a second thickness region (F2) provided on the upper portion of the first thickness region (F1) in the thickness direction (±z direction).

[0059] The body part (BP) has a plurality of first metal layers (101) and a plurality of second metal layers (102) located in a first thickness region (F1), and a plurality of first metal layers (101) and a plurality of second metal layers (102) located in a second thickness region (F2) having different thicknesses or contents.

[0060] Specifically, the body portion (BP) has a thickness of the first metal layer (101) greater than the thickness of the second metal layer (102) in the first thickness region (F1). More specifically, the thickness of the first metal layer (101) in the first thickness region (F1) has a range of 1.1 to 50.0 times greater than the thickness of the second metal layer (102). More preferably, the thickness of the first metal layer (101) may have a range of 1.5 to 3 times greater than the thickness of the second metal layer (102).

[0061] Accordingly, the content of the first metal layer (101) in the first thickness region (F1) is greater than the content of the second metal layer (102). The body portion (BP) has the thickness of the first metal layer (101) in the first thickness region (F1) to be greater than the thickness of the second metal layer (102), thereby increasing the content of the first metal layer (101) relative to the second metal layer (102), thereby increasing the rigidity of the first thickness region (F1).

[0062] Referring to FIGS. 3 to 4d, in the first thickness region (F1), a first metal layer (101), a second metal layer (102), a first metal layer (101), a second metal layer (102), a first metal layer (101), a second metal layer (102), and a first metal layer (101) are laminated from the bottom to the top in the thickness direction (±z direction).

[0063] In the first thickness region (F1), a plurality of first metal layers (101) are provided with the same dimensions in the thickness direction (±z direction). As an example, a plurality of first metal layers (101) may be provided with a thickness of 5 μm. One second metal layer (102) is provided between two adjacent first metal layers (101) in the first thickness region (F1). In the first thickness region (F1), the plurality of first metal layers (101) are also provided with the same dimensions in the longitudinal direction (±y direction).

[0064] In the first thickness region (F1), a plurality of second metal layers (102) are provided with the same dimensions in the thickness direction (±z direction). As an example, a plurality of second metal layers (102) may be provided with a thickness of 3 μm. In the first thickness region (F1), one first metal layer (101) is provided between two adjacent second metal layers (102). In the first thickness region (F1), the plurality of second metal layers (102) are also provided with the same dimensions in the longitudinal direction (±y direction).

[0065] The first thickness region (F1) of the body portion (BP) is continuously connected to the tip portion (TP) provided at the tip end of the body portion (BP) in the longitudinal direction (±y direction). Therefore, the tip portion (TP) is a portion formed by protruding longer than the second thickness region (F2) in the longitudinal direction (±y direction) by alternately stacking first and second metal layers (101, 102) located in the first thickness region (F1). The tip portion (TP) has the same thickness as the first thickness region (F1) of the body portion (BP), and the thickness of the first metal layer (101) is provided to be greater than the thickness of the second metal layer (102), so that the content of the first metal layer (101) is greater than that of the second metal layer (102). Accordingly, the tip portion (TP) can have high rigidity.

[0066] The second thickness region (F2) is located above the first thickness region (F1) in the thickness direction (±z direction).

[0067] The second thickness region (F2) is divided into a surface region (SF) formed by the first metal layer (101) and an internal region (IF) formed by laminating the first metal layer (101) and the second metal layer (102) and located between the surface region (SF) and the first thickness region (F1).

[0068] The surface region (SF) is provided with a surface layer (SL) composed of one first metal layer (101), and the internal region (IF) is provided with an internal multilayer portion (IL) provided below the surface layer (SL) in the thickness direction (±z direction) and in which a plurality of first metal layers (101) and a plurality of second metal layers (102) are alternately laminated.

[0069] The surface layer (SL) is located at the uppermost position in the thickness direction (±z direction) in the second thickness region (F2). Accordingly, the surface layer (SL) constitutes the upper surface of the body portion (BP) in the thickness direction (±z direction). In other words, the upper surface of the body portion (BP) in the thickness direction (±z direction), which is the first surface, is constituted by the surface layer (SL) of the second thickness region (F2). Since the surface layer (SL) is constituted by the first metal layer (101), the upper surface of the body portion (BP) in the thickness direction (±z direction) is constituted by the first metal layer (101). The thickness of the first metal layer (101) constituting the surface layer (SL) is preferably provided as 12.5 ㎛. The thickness of the first metal layer (101) of the surface layer (SL) is in a range of 1.1 times or more and 50.0 times or less than the thickness of the first metal layer (101) provided on the surface of the first thickness region (F1). More preferably, the thickness of the first metal layer (101) of the surface layer (SL) may have a range of 1.5 times or more and 3.0 times or less than the thickness of the first metal layer (101) provided on the surface of the first thickness region (F1). Here, the surface of the first thickness region (F1) may be at least one of the upper surface and the lower surface in the thickness direction (±z direction) of the first thickness region (F1) that protrudes more than the second thickness region (F2) in the longitudinal direction (±y direction) to form the tip portion (TP) and is exposed to the outside.

[0070] The electrically conductive contact pin (100) may have a CMP process performed on its first surface, which is an upper surface in the thickness direction (±z direction), during the manufacturing process. In other words, the upper surface in the thickness direction (±z direction) of the surface layer (SL) of the second thickness region (F2) is a surface on which the CMP process is performed. In the electrically conductive contact pin (100), in consideration of the CMP process, a first metal layer (101) having a high elastic modulus is provided on the metal layer corresponding to the surface layer (SL) during the manufacturing process, but the thickness thereof is larger than the thickness of the first metal layer (101) of the inner multilayer portion (IL) and larger than the thickness of the first metal layer (101) of the first thickness region (F1). As a result, the electrically conductive contact pin (100) in a manufactured state has a thickness in which the first metal layer (101) constituting the surface layer (SL) is larger than the thickness of the first metal layer (101) of the inner multilayer portion (IL) and larger than the thickness of the first metal layer (101) of the first thickness region (F1).

[0071] The electrically conductive contact pin (100) is manufactured in a state in which the shape is maintained without change by the CMP process performed during the manufacturing process, and the surface layer (SL) is provided as a first metal layer (101), but is provided with a thickness greater than the thickness of the first metal layer (101) of the inner multilayer part (IL) and the first metal layer (101) of the first thickness region (F1). Accordingly, even in the state in which the electrically conductive contact pin (100) is manufactured, the first metal layer (101) of the surface layer (SL) is provided with a thickness greater than the thickness of the first metal layer (101) of the inner multilayer part (IL) and the first metal layer (101) of the first thickness region (F1).

[0072] The body portion (BP) has an upper surface that constitutes a surface layer (SL) of a second thickness region (F2) and is composed of a first metal layer (101), and a lower surface that constitutes the lowest layer in the thickness direction (±z direction) of the first thickness region (F1) and is composed of a first metal layer (101). In other words, the body portion (BP) has a surface including an upper surface and a lower surface and is composed of a first metal layer (101) having a large elastic modulus and high rigidity.

[0073] The inner multilayer (IL) is provided by alternately stacking a plurality of first metal layers (101) and a plurality of second metal layers (102) below the surface layer (SL) in the thickness direction (±z direction). In the drawing, the inner multilayer (IL) is provided by stacking a second metal layer (102), a first metal layer (101), a second metal layer (102), a first metal layer (101), a second metal layer (102), a first metal layer (101), and a second metal layer (102) from the upper direction to the lower direction in the thickness direction (±z direction).

[0074] In the second thickness region (F2), the inner multilayer part (IL) is provided by alternately stacking a plurality of first metal layers (101) and a plurality of second metal layers (102), and the surface layer (SL) of the second thickness region (F2) is composed of the first metal layer (101). Accordingly, the uppermost layer in the thickness direction (±z direction) of the inner multilayer part (IL) is provided as the second metal layer (102), and the metal layer located below the thickness direction of the surface layer (SL) becomes the second metal layer (102).

[0075] The inner multilayer (IL) is located between the surface layer (SL) composed of one first metal layer (101) and the first thickness region (F1) in which the first metal layer (101) is located at the uppermost position in the thickness direction (±z direction). Accordingly, the inner multilayer (IL) is located between the first metal layer (101) of the surface layer (SL) and the first metal layer (101) of the first thickness region (F1).

[0076] In the inner multilayer (IL), the thickness of the second metal layer (102) is in a range of 1.1 times to 50.0 times the thickness of the first metal layer (101). More preferably, it may have a range of 5.0 times to 20.0 times the thickness. In the inner multilayer (IL), the plurality of first metal layers (101) have the same dimension in the thickness direction (±z direction), and the plurality of second metal layers (102) also have the same dimension in the thickness direction (±z direction). In the inner multilayer (IL), the second metal layer (102) is preferably provided with a thickness of 6.5 μm, and the first metal layer (101) is preferably provided with a thickness of 0.5 μm. Accordingly, in the inner multilayer (IL), the content of the second metal layer (102) is greater than the content of the first metal layer (101).

[0077] In the second thickness region (F2), only the first metal layer (101) is positioned in the surface layer (SL), which is the surface region (SF), and in the internal multilayer portion (IL), which is the internal region (IF), a plurality of first metal layers (101) and a plurality of second metal layers (102) are positioned alternately. At this time, the thickness of the second metal layer (102) in the second thickness region (specifically, the internal multilayer portion (IL)) has a range of 1.1 to 50.0 times greater than the thickness of the second metal layer (102) in the first thickness region (F1). More preferably, it may have a range of 1.5 to 3.0 times greater than the thickness of the second metal layer (102). The first thickness region (F1) is an advantageous region in terms of rigidity because the thickness of the first metal layer (101) is greater than the thickness of the second metal layer (102). The inner multilayer portion (IL) of the second thickness region (F2) is an advantageous region for improving the electrical conductivity of the electrically conductive contact pin (100) by providing the thickness of the second metal layer (102) to be greater than the thickness of the first metal layer (101).

[0078] The electrically conductive contact pin (100) has a thickness of the second metal layer (102) of the second thickness region (F2) that is relatively greater than the thickness of the second metal layer (102) of the first thickness region (F1).

[0079] The electrically conductive contact pin (100) can have excellent electrical conductivity by providing a thickness of the second metal layer (102) greater than the thickness of the first metal layer (101) in the inner multilayer portion (IL), thereby increasing the content of the second metal layer (102) compared to the first metal layer (101) in the second thickness region (F2), and providing a thickness of the second metal layer (102) of the inner multilayer portion (IL) greater than the thickness of the second metal layer (102) in the first thickness region (F1).

[0080] The electrically conductive contact pin (100) is provided with a thickness of a first metal layer (101) constituting a surface layer (SL) of a second thickness region (F2) that is greater than a thickness of the first metal layer (101) in an inner multilayer portion (IL), so that the content of the first metal layer (101) in the surface layer (SL) is greater than that in the inner multilayer portion (IL). The thickness of the first metal layer (101) in the surface layer (SL) is in a range of 1.1 times to 100.0 times greater than the thickness of the first metal layer (101) in the inner multilayer portion (IL). In addition, in the first thickness region (F1), the first metal layer (101) is provided to have a greater thickness than the second metal layer (102). Through this, the electrically conductive contact pin (100) can minimize damage to the electrically conductive contact pin (100) while increasing the rigidity of the upper surface and lower surface of the electrically conductive contact pin (100).

[0081] The electrically conductive contact pin (100) has an inner multilayer portion (IL) between the surface layer (SL) of the second thickness region (F2) having a relatively high content of the first metal layer (101) and the first thickness region (F1). The electrically conductive contact pin (100) has a thickness of the second metal layer (102) in the inner multilayer portion (IL) that is greater than the thickness of the first metal layer (101), so that the content of the second metal layer (102) is greater than that of the first metal layer (101). Accordingly, the content of the second metal layer (102) in the first thickness region (F1) is less than the content of the second metal layer (102) in the inner multilayer portion (IL), which is the inner region (IF).

[0082] Due to this, the electrically conductive contact pin (100) can secure high rigidity through the surface layer (SL) and the first thickness region (F1) and at the same time have excellent electrical conductivity through the inner multilayer portion (IL).

[0083] In the second thickness region (F2), the plurality of first metal layers (101) and the plurality of second metal layers (102) increase in length direction (±y direction) from top to bottom in the thickness direction (±z direction). Accordingly, the second metal layer (102), which forms the lowest layer in the thickness direction (±z direction) of the second thickness region (F2) and is in contact with the first metal layer (101) of the uppermost layer of the first thickness region (F1), has the largest length direction (±y direction) dimension among the metal layers located in the second thickness region (F2).

[0084] The electrically conductive contact pin (100) is provided with a plurality of first and second metal layers (101, 102) located in the second thickness region (F2) such that the dimensions in the length direction (±y direction) become larger from the top to the bottom in the thickness direction (±z direction), so that one side (end face) of the length direction (±y direction) of the second thickness region (F2) has a shape that is inclined and slanted.

[0085] The electrically conductive contact pin (100) has a shape in which the thickness gradually decreases when a thickness change occurs from the body portion (BP) side to the tip portion (TP) side through the inclined portion by the second thickness region (F2). In other words, the electrically conductive contact pin (100) has an inclined portion in the second thickness region (F2) so that the thickness of the body portion (BP) does not change abruptly but gradually decreases as it moves toward the tip portion (TP). This can alleviate the stress concentration phenomenon caused by the contact pressure applied to the tip portion (TP), and further minimize the problem of damage to the tip portion (TP).

[0086] In the electrically conductive contact pin (100), the body portion (BP) is divided into a first thickness region (F1) and a second thickness region (F2) in the thickness direction (±z direction), and a tip portion (TP) is provided so that the first thickness region (F1) protrudes further than the second thickness region (F2) in the longitudinal direction (±y direction). At this time, the first thickness region (F1) excluding the tip portion (TP) matches the cross-sectional shape in the width direction (±x direction) of the second thickness region (F2). However, due to the inclined portion of the second thickness region (F2), there may be a difference between the longitudinal direction (±y direction) dimension of the first thickness region (F1) excluding the tip portion (TP) and the longitudinal direction (±y direction) dimension of the second thickness region (F2).

[0087] The electrically conductive contact pin (100) may have a thin film layer (TL) on the longitudinal (±y direction) tip side. The thin film layer (TL) is illustrated only in FIGS. 4b, 4c, and 4d and is not illustrated in other drawings.

[0088] When the electrically conductive contact pin (100) is manufactured using a mold made of an anodic oxide material, an electroplating step is performed while the mold made of an anodic oxide material is provided on a seed layer (SD). The seed layer (SD) may be composed of, for example, gold (Au). The seed layer (SD) may be completely removed from the electrically conductive contact pin (100) during the manufacturing process of the electrically conductive contact pin (100) after the electroplating for forming the shape of the electrically conductive contact pin (100) is completed.

[0089] FIG. 4a is a diagram showing a state in which the seed layer (SD) bonded to one side (bottom) of the electrically conductive contact pin (100) in the thickness direction (±z direction) is completely removed and a thin film layer (TL) is not provided.

[0090] Fig. 4b is a diagram showing a state in which a thin film layer (TL) is formed by performing a flash plating process with gold (Au) on the longitudinal (±y direction) tip end side of an electrically conductive contact pin (100) in a state in which the seed layer (SD) has been completely removed from the electrically conductive contact pin (100). The thin film layer (TL) is composed of gold (Au).

[0091] An electrically conductive contact pin (100) is provided with a thin film layer (TL) by performing a flash plating process on one side (bottom) in the thickness direction (±z direction) of the longitudinal (±y direction) tip end, the other side (top) in the thickness direction (±z direction), the side in the width direction (±x direction), and the side in the longitudinal direction (±y direction). In this case, the thin film layer (TL) is formed to continuously wrap the entire tip end of the electrically conductive contact pin (100).

[0092] Due to this, the electrically conductive contact pin (100) can improve electrical conductivity when connected to the circuit board (300) side through the longitudinal (±y direction) tip side.

[0093] FIG. 4c is a diagram showing a state in which a thin film layer (TL) is provided on the longitudinal (±y direction) tip of an electrically conductive contact pin (100) provided on a seed layer (SD), and then the seed layer (SD) is completely removed from one surface (bottom surface) of the electrically conductive contact pin (100) in the thickness direction (±z direction).

[0094] Specifically, the electrically conductive contact pin (100) may be subjected to a flash plating process with gold (Au) to form a thin film layer (TL) on the longitudinal (±y direction) tip side while being provided on the seed layer (SD). Accordingly, the thin film layer (TL) may be composed of gold (Au) with high electrical conductivity.

[0095] The electrically conductive contact pin (100) may be subjected to flash plating treatment on a surface exposed to the outside, except for one surface (bottom) in the thickness direction (±z direction) combined with the seed layer (SD). More specifically, the flash plating treatment is performed on an exposed surface (including an exposed other surface (top surface) in the thickness direction (±z direction), a side surface in the width direction (±x direction), and a side surface in the length direction (±y direction)) of the tip portion (TP) and the front end side of the body portion (BP) of the electrically conductive contact pin (100), which includes a portion connected to the tip portion (TP).

[0096] At this time, the surface (one side (bottom side) in the thickness direction (±z direction)) combined with the seed layer (SD) of the electrically conductive contact pin (100) is not subjected to flash plating as it is a surface not exposed to the outside by the seed layer (SD).

[0097] Then, a process of removing the electrically conductive contact pin (100) that has been flash plated from the seed layer (SD) is performed. As a result, the electrically conductive contact pin (100) is provided with a thin film layer (TL) on the other surface (upper surface) in the thickness direction (±z direction), the side surface in the width direction (±x direction), and the side surface in the length direction (±y direction), except for one surface (bottom surface) in the thickness direction (±z direction) that is a bonding surface with the seed layer (SD) on the tip side in the length direction (±y direction).

[0098] The electrically conductive contact pin (100) can improve electrical conductivity when connected to the circuit board (300) side by having a thin film layer (TL) on the longitudinal (±y direction) tip side.

[0099] Meanwhile, the electrically conductive contact pin (100) may have a thin film layer (TL) on the other side (bottom) in the thickness direction (±z direction), the side in the width direction (±x direction), and the side in the length direction (±y direction), except for one side (top surface) in the thickness direction (±z direction) of the longitudinal (±y direction) tip end.

[0100] FIG. 4d is a diagram showing a state in which a thin film layer (TL) is provided on the thickness direction (±z direction) side surface (bottom surface), width direction (±x direction) side surface, and length direction (±y direction) side surface of the longitudinal direction (±y direction) tip side of the electrically conductive contact pin (100).

[0101] The electrically conductive contact pin (100) is a molded product in which a plurality of first and second metal layers (101, 102) are alternately laminated before the tip portion (TP) is formed and has the same dimensions in the thickness direction (±z direction). The electrically conductive contact pin (100) can be formed by laser processing one surface (top surface) in the thickness direction (±z direction) of the tip portion (±y direction) of the molded product so that the thickness becomes smaller.

[0102] The laser processing step of forming the tip portion (TP) can be performed after the seed layer (SD) is completely removed from the molded product, and then the process of flash plating the longitudinal (±y direction) tip end of the electrically conductive contact pin (100) with gold (Au) is performed.

[0103] Due to this, the electrically conductive contact pin (100) has the thin film layer (TL) formed on one surface (upper surface) in the thickness direction (±z direction) of the molded product removed. Accordingly, the electrically conductive contact pin (100) is provided in a state where the thin film layer (TL) is not formed on one inclined surface (upper surface) in the length direction (±y direction) of the second thickness region (F2) and one surface (upper surface) in the thickness direction (±z direction) of the tip portion (TP) and the metal layer is exposed, and the thin film layer (TL) can be provided on the other surface (lower surface) in the thickness direction (±z direction), the side surface in the width direction (±x direction), and the side surface in the length direction (±y direction).

[0104] Meanwhile, with the molded product on the seed layer (SD), laser processing can be performed after flash plating treatment on the longitudinal (±y direction) end of the molded product.

[0105] In this case, the electrically conductive contact pin (100) may be subjected to laser processing on the exposed one surface (top surface) in the thickness direction (±z direction) of the longitudinal (±y direction) tip end side while the thin film layer (TL) is formed on the externally exposed surface (including the exposed one surface (top surface) in the thickness direction (±z direction), the side surface in the width direction (±x direction), and the exposed side surface in the length direction (±y direction)) except for the other surface (bottom surface) in the thickness direction (±z direction) combined with the seed layer (SD). Then, the seed layer (SD) may be removed.

[0106] Accordingly, the electrically conductive contact pin (100) may be provided in a form in which the metal layer (first metal layer (101)) is exposed and the thin film layer (TL) is provided on the exposed side in the width direction (±x direction) and the side in the length direction (±y direction) since the thin film layer (TL) is not provided on one side (upper surface) in the thickness direction (±z direction) and the other side (lower surface) in the thickness direction (±z direction).

[0107] The electrically conductive contact pin (100) has a plurality of first metal layers (101) and a plurality of second metal layers (102) having different thicknesses in a first thickness region (F1), and has a plurality of first metal layers (101) and a plurality of second metal layers (102) having different thicknesses in a second thickness region (F2). The electrically conductive contact pin (100) can increase the rigidity of the tip portion (TP) side to which contact pressure is applied, and can secure not only the rigidity but also excellent electrical conductivity through the body portion (BP) side. The electrically conductive contact pin (100) has a plurality of first metal layers (101) and a plurality of second metal layers (102) having different thicknesses, but the total thickness of the plurality of first metal layers (101) constituting the electrically conductive contact pin (100) is the same as the total thickness of the plurality of second metal layers (102) constituting the electrically conductive contact pin (100). Through this, the electrically conductive contact pin (100) can have both high rigidity and excellent electrical conductivity in a shape in which the thicknesses of the body portion (BP) and the tip portion (TP) in the thickness direction (±z direction) are different.

[0108] Referring to FIGS. 1 and 2, the body portion (BP) includes a slit (211) formed in the form of an empty space inside the body portion (BP) by penetrating the first surface of the body portion (BP) in the thickness direction (±z direction) and the second surface of the body portion (BP). The slit (211) is formed long along the longitudinal direction (±y direction) of the body portion (BP). At least one slit (211) may be provided. As an example, three slits (211) are illustrated in FIGS. 1, 2, 5a, 5b, 7a, and 7b. The electrically conductive contact pin (100) includes a slit (211) formed inside the body portion (BP), thereby securing a desired overdrive amount and shortening the overall length while securing a desired stylus pressure or allowable time current characteristic. Since the electrically conductive contact pin (100) can have a shorter overall length, the inductance of the electrically conductive contact pin (100) can be reduced, thereby improving high-frequency characteristics.

[0109] The slit (211) is provided in a form in which the internal width direction (±x direction) dimension becomes smaller from the center to the ends in the longitudinal direction (±y direction). As a result, the beam portions provided on both sides of the slit (211) have a root portion whose width becomes larger from the center to the ends, thereby having the effect of relieving the stress concentration occurring at both ends of the slit (211) in the longitudinal direction (±y direction).

[0110] The tip portion (TP) has a dimension smaller than the width direction (±x direction) dimension of the body portion (BP) and a thickness smaller than the thickness of the body portion (BP) in the thickness direction (±z direction). Here, the thickness of the body portion (BP) is a value obtained by adding the dimensions of the first thickness region (F1) and the second thickness region (F2), and the tip portion (TP) is formed by protruding the first thickness region (F1) of the body portion (BP) longer than the second thickness region (F2) in the length direction, so that the tip portion (TP) has the same value as the dimension of the first thickness region (F1) of the body portion (BP).

[0111] The tip portion (TP) may be provided in a form in which the width direction (±x direction) dimension becomes smaller as it goes from the body portion (BP) side to one end of the tip portion (TP) in the length direction (±y direction). As a result, the width direction (±x direction) cross-sectional area of ​​the tip portion (TP) becomes smaller as it goes from the body portion (BP) side to one end of the tip portion (TP). One end of the tip portion (TP) is provided as a free end. At this time, one end of the tip portion (TP) is not pointed, but is provided as a flat surface having a cross-sectional area in the thickness direction (±z direction).

[0112] The surface in the thickness direction (±z direction) of the tip portion (TP) is flat and not inclined. More specifically, the first surface (one surface in the +z direction) of the tip portion (TP) and the second surface (the other surface in the +z direction) of the tip portion (TP) opposite to the first surface of the tip portion (TP) are parallel to each other and are provided flat and not inclined. The flat surface (first surface) in the thickness direction (±z direction) of the tip portion (TP) is positioned lower in the thickness direction (±z direction) than the surface (first surface) in the thickness direction (±z direction) of the body portion (BP) which is positioned in the same direction in the thickness direction (±z direction). At this time, the first surface of the body portion (BP) is inclined so that the leading end in the longitudinal direction (±y direction) is connected to the rear end in the longitudinal direction (±y direction) of the first surface of the tip portion (TP).

[0113] The second surface of the tip portion (TP) is positioned at the same position in the thickness direction (±z direction) as the second surface of the body portion (BP), and the first surface of the tip portion (TP) is positioned at a lower position in the thickness direction (±z direction) than the first surface of the body portion (BP), so that the center of the tip portion (TP) can be formed to be biased toward the second surface of the electrically conductive contact pin (100).

[0114] The tip portion (TP) can be formed by laser processing so that the thickness is reduced on one side (upper surface) in the thickness direction (±z direction) of the tip portion of a molded product in which a plurality of first and second metal layers (101, 102) are alternately laminated. Accordingly, the material of the tip portion (TP) and the material of the body portion (BP) are provided identically. As a result, the electrical conductivity of the electrically conductive contact pin (100) can be significantly improved. Conventionally, the material of the tip portion (TP) and the material of the body portion (BP) are different from each other, which causes resistance to the electric flow at the discontinuous boundary. However, in the electrically conductive contact pin (100), the body portion (BP) and the tip portion (TP) are formed of metal layers of the same material continuously in the longitudinal direction (±y direction), thereby eliminating the resistance element to the electric flow, thereby providing improved electrical conductivity.

[0115] The number of metal layers constituting the tip portion (TP) is less than the number of metal layers constituting the body portion (BP).

[0116] Specifically, the tip portion (TP) is configured by laminating a plurality of metal layers identical to the metal layers located in the first thickness region (F1) of the body portion (BP). In the drawing, the tip portion (TP) is provided by laminating seven metal layers.

[0117] More specifically, the tip portion (TP) is provided with a first metal layer (101), a second metal layer (102), a first metal layer (101), a second metal layer (102), a first metal layer (101), a second metal layer (102), and a first metal layer (101) laminated from the bottom to the top in the thickness direction (±z direction). As a result, the surface including the upper and lower surfaces of the tip portion (TP) in the thickness direction (±z direction) is composed of the first metal layer (101).

[0118] The tip portion (TP) has a first metal layer (101) having a thickness that is 1.1 times or more and 50.0 times or less than that of the second metal layer (102), and the content of the first metal layer (101) is greater than that of the second metal layer (102). The tip portion (TP) has a first metal layer (101) having a greater thickness and content than that of the second metal layer (102), and thus can have a relatively large elastic modulus, high rigidity, and excellent wear resistance.

[0119] The electrically conductive contact pin (100) is connected to the circuit board through the tip portion (TP). Therefore, contact pressure is applied to the tip portion (TP).

[0120] The tip portion (TP) of the electrically conductive contact pin (100) has a first metal layer (101) having a thickness greater than that of the second metal layer (102), so that the content of the first metal layer (101) in the tip portion (TP) is greater than that of the second metal layer (102). As a result, the electrically conductive contact pin (100) can minimize damage to the tip portion (TP) due to contact pressure applied to the tip portion (TP), thereby increasing durability and further improving connection reliability.

[0121] Referring to FIG. 3, the electrically conductive contact pin (100) has a micro-trench (88) on the side surface of the body portion (BP) and the side surface in the width direction (±x direction) of the tip portion (TP). Accordingly, the micro-trench (88) is provided on the side surface in the width direction (±x direction) of the first thickness region (F1) and the second thickness region (F2). The micro-trench (88) is only illustrated in the enlarged view of the tip portion of the electrically conductive contact pin (100) of FIG. 3, and is omitted in other drawings.

[0122] The micro trench (88) is formed as a long groove along the thickness direction (±z direction), and a plurality of them are formed in parallel along the entire side surface.

[0123] The micro trench (88) has a depth ranging from 20 nm to 1 μm, and a width ranging from 20 nm to 1 μm. The micro trench (88) can be formed by a mold made of an anodic oxide film material used to manufacture an electrically conductive contact pin (100).

[0124] Specifically, the electrically conductive contact pin (100) is manufactured by including a process of forming an opening space by etching at least a portion of a mold made of an anodic oxide material including numerous pores, and growing metal by electroplating inside the opening space. The electrically conductive contact pin (100) is provided by removing the metal grown inside the opening space from the mold made of the anodic oxide material, and a micro-trench (88) is formed when a side surface of the metal in the opening space contacts the pores of the mold made of the anodic oxide material. When the metal is separated from the mold made of the anodic oxide material, the electrically conductive contact pin (100) is provided with the micro-trench (88) on the side surface of the metal, thereby forming the micro-trench (88) on the side surface of the body portion (BP) and the tip portion (TP).

[0125] Here, since the micro trench (88) is due to the pores formed during the manufacturing of the mold made of the anodic oxide film material, the width and depth of the micro trench (88) have values ​​less than or equal to the range of the diameters of the pores of the mold made of the anodic oxide film material. Meanwhile, during the process of forming an opening space in the mold made of the anodic oxide film material, some of the pores of the mold made of the anodic oxide film material may be crushed together by the etching solution, thereby forming at least some micro trenches (88) having a depth greater than the range of the diameters of the pores formed during the anodic oxidation.

[0126] In a state where metal is provided in the opening space of a mold made of an anodic oxide film material, the upper and lower surfaces of the metal in the thickness direction (±z direction) correspond to the first and second surfaces of the electrically conductive contact pin (100), respectively. Since the upper and lower surfaces of the metal in the thickness direction (±z direction) are areas that do not come into contact with the pores of the mold, a micro-trench (88) is not formed. Accordingly, a micro-trench (88) is not formed on the first and second surfaces of the electrically conductive contact pin (100).

[0127] The micro trench (88) has the effect of increasing the surface area on the side surface of the electrically conductive contact pin (100). Through the configuration of the micro trench (88) formed on the side surface of the electrically conductive contact pin (100), heat generated in the electrically conductive contact pin (100) can be quickly released, thereby suppressing the temperature rise of the electrically conductive contact pin (100). In addition, through the configuration of the micro trench (88) formed on the side surface of the electrically conductive contact pin (100), the torsion resistance capability of the electrically conductive contact pin (100) can be improved when it is deformed.

[0128] Meanwhile, in the process of automatically inserting the electrically conductive contact pin (100) into the guide hole of the guide plate (GP1, GP2) using a robotic means, a process of confirming the position of the electrically conductive contact pin (100) by taking an image of the electrically conductive contact pin (200) is performed. At this time, the micro trench (88) formed on the side of the electrically conductive contact pin (100) functions as a diffuse reflection surface when taking an image with the imaging means, so that the imaging means can precisely determine the position of the electrically conductive contact pin (200).

[0129] Referring to Fig. 9, the tip portion (TP) of the electrically conductive contact pin (100) is connected to the pad (CP) of the circuit board (300). The circuit board (300) here is a part that constitutes a circuit portion for inspecting the inspection object, including a space converter. The base portion, which is opposite the tip portion (TP) of the electrically conductive contact pin (100), is connected to the terminal of the inspection object.

[0130] The electrically conductive contact pin (100) extends the first thickness region (F1) in the longitudinal direction (±y direction) to form a tip portion (TP), so that the thickness of the first metal layer (101) is large compared to the thickness of the second metal layer (102), and the content of the first metal layer (101) is large compared to the content of the second metal layer (102). This increases the rigidity and durability of the tip portion (TP).

[0131] In addition, the electrically conductive contact pin (100) secures rigidity by increasing the thickness of the first metal layer (101) compared to the second metal layer (102) in the first thickness region (F1) and thereby increasing its content, and increases electrical conductivity by increasing the thickness of the second metal layer (102) compared to the first metal layer (101) in the inner multilayer portion (IL) in the second thickness region (F2). As a result, the electrically conductive contact pin (100) can have durability due to high rigidity and excellent electrical conductivity.

[0132] In addition, the tip portion (TP), which is the leading end of the electrically conductive contact pin (100), has a smaller dimension than the dimension in the thickness direction (±z direction) of the body portion (BP) and has a smaller number of layers than the number of layers of metal layers constituting the body portion (BP). This increases the pinning pressure and provides high electrical conductivity and high strength, thereby improving the reliability of the connection.

[0133] An electrically conductive contact pin (100) is provided in an example inspection device (10) illustrated in FIG. 9 and is used to transmit an electrical signal by making electrical and physical contact with an inspection target. The inspection device (10) includes an electrically conductive contact pin (100) that is inserted into a guide hole of at least one guide plate (GP1, GP2) and installed in the guide plate (GP1, GP2). The inspection device (10) may be an inspection device used in a semiconductor manufacturing process, and may be, for example, a probe card or a test socket. The electrically conductive contact pin (100) may be an electrically conductive contact pin provided in a probe card to inspect a semiconductor chip, and may be a socket pin provided in a test socket to inspect a packaged semiconductor package to inspect the semiconductor package. The inspection devices (10) in which the electrically conductive contact pin (100) can be used are not limited thereto, and any inspection device that applies electricity to check for defects in an inspection target is included. The inspection object of the inspection device (10) may include a semiconductor element, a memory chip, a microprocessor chip, a logic chip, a light-emitting element, or a combination thereof.For example, inspection targets include logic LSIs (such as ASICs, FPGAs, and ASSPs), microprocessors (such as CPUs and GPUs), memories (such as DRAMs, HMCs (Hybrid Memory Cubes), MRAMs (Magnetic RAMs), PCMs (Phase-Change Memory), ReRAMs (Resistive RAMs), FeRAMs (Ferroelectric RAMs), and flash memories (NAND flashes)), semiconductor light-emitting devices (including LEDs, mini LEDs, and micro LEDs), power devices, analog ICs (such as DC-AC converters and insulated-gate bipolar transistors (IGBTs)), MEMS (such as accelerometers, pressure sensors, vibrators, and gyroscopes), wireless devices (such as GPS, FM, NFC, RFEM, MMIC, and WLAN), discrete devices, BSIs, CISs, camera modules, CMOSs, passive devices, GAW filters, RF filters, RF IPDs, APEs, and BBs.

[0134] As described above, the present invention has been described with reference to preferred embodiments thereof, but it will be apparent to those skilled in the art that various modifications or variations may be made to the present invention without departing from the spirit and scope of the present invention as set forth in the following claims.

[0135] [Explanation of symbols]

[0136] 10: Inspection device

[0137] 100: Electrically conductive contact pin

[0138] 101: First metal layer

[0139] 102: Second metal layer

[0140] BP: Body

[0141] TP: Tip section

[0142] F1: First thickness region

[0143] F2: Second thickness area

[0144] SL: Surface layer

[0145] IL: Internal multilayer

Claims

1. A body portion in which a plurality of first metal layers composed of a metal having a relatively large elastic modulus and a plurality of second metal layers composed of a metal having a relatively large electrical conductivity are alternately laminated in the thickness direction; and including a tip portion provided at the front end of the body portion in the longitudinal direction; The above body part, A first thickness region continuously connected to the tip portion in the longitudinal direction; and A second thickness region provided on the upper side of the first thickness region in the thickness direction; An electrically conductive contact pin, wherein the thickness of the first metal layer in the first thickness region is in a range of 1.1 times to 50.0 times the thickness of the second metal layer.

2. In paragraph 1, An electrically conductive contact pin, wherein the content of the first metal layer in the first thickness region is greater than the content of the second metal layer.

3. In paragraph 1, In the above first thickness region, the thickness direction dimension and the length direction dimension of the plurality of first metal layers are the same, An electrically conductive contact pin, wherein the thickness direction dimension and the length direction dimension of the plurality of second metal layers in the first thickness region are the same.

4. In paragraph 1, The above second thickness region is, a surface layer comprising one of the above first metal layers; and An inner multilayer portion is provided on the lower portion of the surface layer in the thickness direction and is provided by alternately stacking a plurality of the first metal layers and a plurality of the second metal layers; An electrically conductive contact pin, wherein the inner multilayer portion is positioned between the surface layer and the first thickness region.

5. In paragraph 4, In the above inner multilayer portion, the content of the second metal layer is greater than the content of the first metal layer in the above inner multilayer portion, An electrically conductive contact pin, wherein the thickness of the second metal layer in the inner multilayer portion is in a range of 1.1 times to 50.0 times the thickness of the first metal layer.

6. In paragraph 4, An electrically conductive contact pin, wherein the content of the first metal layer constituting the surface layer in the second thickness region is greater than the content of the first metal layer in the inner multilayer portion.

7. In paragraph 4, In the above inner multilayer portion, the thickness direction dimensions of the plurality of second metal layers are the same, An electrically conductive contact pin having the same thickness dimension of a plurality of the first metal layers in the above inner multilayer portion.

8. In paragraph 1, An electrically conductive contact pin, wherein a plurality of the first metal layers and a plurality of the second metal layers in the second thickness region have a lengthwise dimension that increases from top to bottom in the thickness direction.

9. In paragraph 1, An electrically conductive contact pin having micro-trench formed on the side of the body portion and the side of the tip portion.

10. In an electrically conductive contact pin in which a plurality of first metal layers and a plurality of second metal layers are alternately laminated in the thickness direction, The first metal layer is a metal having a relatively large elastic modulus compared to the second metal layer, and the second metal layer is a metal having a relatively large electrical conductivity compared to the first metal layer. It is divided into a first thickness region and a second thickness region in the thickness direction, and a tip portion protruding more than the second thickness region in the longitudinal direction is provided at an end portion in the longitudinal direction of the first thickness region. An electrically conductive contact pin, wherein the thickness of the first metal layer in the first thickness region is in a range of 1.1 times to 50.0 times the thickness of the second metal layer.

11. In paragraph 10, The above second thickness region is, A surface area provided with the first metal layer, An electrically conductive contact pin, which is provided by laminating the first metal layer and the second metal layer and is divided into an internal region located between the surface region and the first thickness region.

12. In paragraph 11, An electrically conductive contact pin, wherein the thickness of the second metal layer in the inner region is in a range of 1.1 times to 50.0 times the thickness of the first metal layer.

13. In paragraph 11, An electrically conductive contact pin, wherein the thickness of the first metal layer of the surface area is in a range of 1.1 times to 100.0 times the thickness of the first metal layer of the inner area.

14. In paragraph 10, An electrically conductive contact pin, wherein the first thickness region excluding the tip portion matches the shape of the second thickness region.

15. In paragraph 10, An electrically conductive contact pin, wherein the total thickness of the plurality of first metal layers is the same as the total thickness of the plurality of second metal layers.

16. In paragraph 10, An electrically conductive contact pin having a plurality of fine trenches formed in parallel along the entire side surface along the side surface, the fine trenches being formed as long grooves along the thickness direction on the side surface of the first thickness region and the second thickness region.

17. In paragraph 16, The electrically conductive contact pin includes a first surface and a second surface opposite to the first surface, The above side is a surface connecting the first surface and the second surface, An electrically conductive contact pin, wherein the micro-trench is not formed on the first surface and the second surface.

18. In paragraph 10, An electrically conductive contact pin, wherein the thickness of the first metal layer provided on the surface of the second thickness region is in a range of 1.1 times to 50.0 times the thickness of the first metal layer provided on the surface of the first thickness region.

19. In an electrically conductive contact pin having a plurality of first metal layers and a plurality of second metal layers laminated in the thickness direction, The first metal layer is a metal having a relatively large elastic modulus compared to the second metal layer, and the second metal layer is a metal having a relatively large electrical conductivity compared to the first metal layer. It is divided into a first thickness region and a second thickness region in the thickness direction, and a tip portion protruding more than the second thickness region in the longitudinal direction is provided at an end portion in the longitudinal direction of the first thickness region. The second thickness region is divided into a surface region formed by the first metal layer and an internal region formed by laminating the first metal layer and the second metal layer and positioned between the surface region and the first thickness region. The content of the first metal layer in the first thickness region is greater than the content of the first metal layer in the inner region, An electrically conductive contact pin, wherein the content of the second metal layer in the first thickness region is less than the content of the second metal layer in the inner region.

20. In an electrically conductive contact pin in which a plurality of first metal layers and a plurality of second metal layers are alternately laminated in the thickness direction, The first metal layer is a metal having a relatively large elastic modulus compared to the second metal layer, and the second metal layer is a metal having a relatively large electrical conductivity compared to the first metal layer. It is divided into a first thickness region and a second thickness region in the thickness direction, and a tip portion protruding more than the second thickness region in the longitudinal direction is provided at an end portion in the longitudinal direction of the first thickness region. An electrically conductive contact pin, wherein the thickness of the second metal layer in the second thickness region is in a range of 1.1 times to 50.0 times less than the thickness of the second metal layer in the first thickness region.

Citation Information

Patent Citations

  • Vertical probe pin and probe pin assembly with the same

    KR101769355B1

  • Electrically Conductive Pins For Microcircuit Tester

    KR1020120024541A

  • Heating wire using carbon

    KR1020240055316A

  • Probe pin and manufacturing method thereof

    KR102147699B1

  • KR20230032062A