Woven metal wire electrode
The woven metal wire electrodes are stabilized by coating with tin and using thermoplastic resin to enhance conductivity and fixation, addressing structural integrity and attachment issues, ensuring reliable performance in metal-air fuel cells.
Patent Information
- Application Number
- PCT/KR2024/006089
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-08
- Filing Date
- 2024-05-07
- Publication Date
- 2024-11-14
AI Technical Summary
Existing woven metal wire electrodes face challenges in maintaining fixation force, electrical conductivity, and structural integrity, particularly when used in metal-air fuel cells, where the woven structure is prone to breakage and requires secure attachment to the battery surface.
The solution involves weaving conductive metal wires coated with tin to enhance fixation, using a thermoplastic conductive resin to improve tension and conductivity, and incorporating melting yarns to bond the warp and weft wires, ensuring strong edge integrity through heat treatment and dense weaving patterns.
This approach maintains electrical conductivity and fixation force, prevents breakage during weaving, and ensures the electrode pattern remains intact and securely attached to the battery surface, even when punched out as a single pattern.
Smart Images

Figure KR2024006089_14112024_PF_FP_ABST
Abstract
Description
Woven metal wire electrode
[0001] The present invention relates to a technology for forming an electrode by weaving metal wires.
[0002] The invention that serves as the background is the invention of the Korean Intellectual Property Office Patent Registration No. 10-1650105 (August 16, 2016) and is illustrated in Figure 7.
[0003] The background technology is characterized by the metal cathode applied to the metal-air fuel cell being woven into a fiber form.
[0004] Here, the fiber-type metal cathode (1) is formed by weaving a warp (10) made of a conductive metal wire and a weft (20) made of an active metal wire, as shown in Fig. 7.
[0005] Therefore, electricity is conducted by the slope (10), and the weft (20) becomes fuel. For this purpose, the conductive metal wire forming the slope (10) is preferably made of copper, silver or gold, and the active metal wire forming the weft (20) is preferably made of magnesium, zinc or aluminum.
[0006] However, the materials of the conductive metal wire and the active metal wire are not limited to the materials listed above, and various materials can be used for the conductive metal wire under the premise that it has conductivity, and various materials can be used for the active metal wire under the premise that it becomes the fuel of the metal-air fuel cell.
[0007] Meanwhile, the warp yarn (10) and weft yarn (20) for forming the above-mentioned fiber-type metal cathode (1) are not particularly limited in their number of strands, but considering that the warp yarn (10) is intended to conduct electricity and the weft yarn (20) serves as fuel, it is preferable that the weft yarn (20) be woven with a number of strands greater than that of the warp yarn (10).
[0008] As shown in Fig. 7, when the warp yarn (10) is made up of 1 to 2 strands, the weft yarn (20) can be made up of 3 to 5 strands, but this is only an example, and both the warp yarn (10) and the weft yarn (20) can have various strand numbers. In addition, the fiber-type metal cathode (1) made up as described above can be used alone, or can be used by laminating multiple layers.
[0009] Therefore, the background technology is to weave a warp (10) made of a conductive metal wire such as copper and a weft (20) made of an active metal wire such as magnesium, zinc or aluminum to produce a fiber-shaped metal cathode (1), and apply this to a metal-air fuel cell, so that the surface area (reaction area) of the metal cathode (1) increases, thereby improving the energy density, power generation per hour, and charging capacity, and also ensuring flexibility to bend freely, so that it can be widely used without restrictions in fields of use such as military, outdoor, and emergency safety. In addition, as described above, when applying a plurality of layers of the fiber-shaped metal cathode (1) woven as described above, when a high-capacity power generation is generated, an electrolyte is impregnated into the woven pores, so that a stable structure can be maintained against external impact, etc.
[0010] However, the above-described conventional technology does not require fixing in a woven state, and the present invention configures a woven electrode that allows the woven metal to maintain fixing force.
[0011] The first task that the invention seeks to solve is to maintain the fixing strength and electrical conductivity of woven metal wires.
[0012] The second problem to be solved by the invention is to weave warp wire and weft wire, which are metal wires, while coating them with a soluble material, and to remove the soluble material after weaving to increase the tension during weaving and prevent wire breakage.
[0013] The third challenge that the invention seeks to address is to simultaneously secure electrical conductivity and maintain fixing force between the woven metal wire electrode and the battery surface layer.
[0014] The fourth problem to be solved by the invention is to ensure that the edge portion remains solid even when the electrode pattern is punched out and used as a single pattern.
[0015] In order to solve the above-mentioned problem, it has the following structure.
[0016] Weave the electrode pattern with warp wire and weft wire,
[0017] The above-mentioned inclined wire and the above-mentioned weft wire are each composed of conductive metal wires,
[0018] It has a woven metal wire electrode that constitutes a fixing means so as to fix the above electrode pattern.
[0019] Here, the fixing means comprises a tin-coated metal wire in which tin is coated on the surface of the metal wire, which is the inclined wire and the weft wire,
[0020] It is preferable to fix the electrode pattern by melting the tin coated on the woven electrode pattern through heat treatment to ensure electrical conductivity at the part where the tin-coated metal wires intersect.
[0021] Here, the fixing means is woven to surround the electrode pattern, and the circumference of the electrode pattern is woven with warp and weft yarns,
[0022] It is preferable to configure the electrode pattern so that the above-mentioned warp yarn and the above-mentioned warp yarn are woven so as to be in close contact with each other and thereby fix the periphery of the electrode pattern, thereby primarily fixing the electrode pattern.
[0023] Here, it is preferable to coat the tin-coated metal wire with an available material to increase the tension of the warp wire and the weft wire so that the warp wire and the weft wire can prevent breakage during weaving.
[0024] Here, it is preferable to configure the soluble material configured in the woven electrode pattern by melting the soluble material through at least one of chemical treatment, heat treatment, and water washing so that the warp wire and the weft wire are exposed.
[0025] It is preferable to configure the surface of the metal wire to be coated with a thermoplastic conductive resin so as to enhance the tension of the warp wire and the weft wire, the fixing force of the electrode pattern, the electrical conductivity between the warp and weft, and to exhibit a bonding function that secures electrical conductivity between the electrode and the solar cell.
[0026] Here, it is preferable that the thermoplastic conductive resin is composed of a resin containing nanopowder of any one of Ag, Cu, Sn, and Ni (it was written as nanowire, but I know it is a typo and will write it as nanopowder). Here, it is preferable that the melting yarn is included in some of the warp yarns and the weft yarns, and when heat-treated, the melting yarn included in the some of the warp yarns containing the melting yarn is melted and mutually bonded so that the warp yarns and the weft yarns maintain more fixing force, so that the periphery of the electrode pattern can be more fixed.
[0027] Here, the warp yarn and the weft yarn are preferably composed of one or more of rayon, silk, cotton, and polyester, and one or more of the warp yarn and the weft yarn is preferably composed of a composition in which melting yarn is partially mixed into one or more of the warp yarn and the weft yarn.
[0028] Here, when weaving the edge of the electrode pattern, it is preferable to increase the density by narrowing the weaving interval of the tin-coated copper wire or the copper thermoplastic resin wire in the edge, and then, by pressurized heating, fuse not only at the intersection of the copper warp wire and the copper weft wire but also at the edge so that the edge is firmly maintained even after the electrode pattern is punched out.
[0029] Here, as another embodiment, it is preferable to configure the edge portion of the electrode pattern to be woven with a metal film yarn.
[0030] In addition, it is preferable that the width of the metal film is configured to be 0.5 to 3.0 mm.
[0031] The first effect of the invention is that the woven metal wire has the effect of maintaining electrical conductivity and fixing force.
[0032] A second effect of the invention is that the fixing force of the electrode pattern is improved by weaving warp and weft yarns around the woven electrode pattern to maintain the fixing force of the woven metal wire.
[0033] The third effect of the invention is to prevent wire breakage when weaving warp wire and weft wire, which are metal wires, by weaving them together with a soluble material, thereby removing the soluble material after weaving, thereby increasing the tension of the wire during weaving.
[0034] The fourth effect of the invention is to secure electrical conductivity and maintain fixing force between the woven metal wire electrode and the battery surface layer by combining a thermoplastic resin with the warp wire and the warp wire.
[0035] The fifth effect of the invention is that the edge portion is maintained firmly even when the electrode pattern is punched out and used as a single pattern.
[0036] Figure 1a is a diagram showing an electrode pattern woven with copper wire and a configuration for adding fixing force using warp and weft yarns.
[0037] Fig. 1b is a diagram showing a configuration for adding fixing force by configuring melting yarn warp yarn and / or melting yarn weft yarn to some of the warp yarn and weft yarn in Fig. 1a.
[0038] Figure 2a is a diagram showing an electrode pattern woven with tin-coated copper wire and a configuration for adding fixing force using warp and weft yarns.
[0039] Figure 2b is a diagram showing a configuration for adding fixing force to an electrode pattern woven with tin-coated copper wire and a warp and weft yarn, and adding fixing force to some of the warp and weft yarns with melting yarn warp and weft yarn.
[0040] Figure 2c is a diagram of the melting yarn structure.
[0041] Figure 3a is a diagram showing an electrode pattern woven with copper wire coated with a tin-coated copper availability material and a configuration for adding fixing force with warp and weft yarns.
[0042] Figure 3b is a diagram showing a configuration for adding fixing force to an electrode pattern woven with a tin-coated copper-soluble material wire and a warp and weft yarn, and melting yarn warp and weft yarn and / or melting yarn weft yarn to some of the warp and weft yarns.
[0043] Figure 3c is a diagram showing a tin-coated copper-soluble material wire.
[0044] Figure 4a is a diagram showing that it is possible to attach an electrode pattern woven with copper thermoplastic resin wire and to add fixing force with warp and weft yarns, and to add fixing force and electrical conductivity through thermoplastic resin fusion, and to attach to a battery through thermoplastic resin fusion.
[0045] Figure 4b is a diagram showing a configuration for adding fixing force to the electrode pattern woven in Figure 4a and the warp and weft yarns, and adding fixing force to some warp yarns and melting yarn weft yarns.
[0046] Figure 4c is a diagram showing a copper thermoplastic resin wire.
[0047] Figure 5 is a diagram showing a weaving pattern in which two or three wires are woven with a narrow weaving interval at the edge of the electrode pattern.
[0048] Figure 6 is a diagram showing the edge of the electrode pattern woven with metal film yarn.
[0049] Figure 7 is a diagram showing the background technology.
[0050] There are eight embodiments in the detailed description of the present invention.
[0051] Although each embodiment has its own merits, and it is not possible to precisely describe which embodiment is the best, the applicant has decided to describe the fifth embodiment as the best embodiment.
[0052] The best example (fifth example) is as follows.
[0053] The explanation for Fig. 3a is as follows.
[0054] The woven electrode is configured to prevent wire breakage during weaving by coating the above tin-coated copper wire (200) with a soluble material (300a) to increase the tension of the tin-coated copper soluble material warp wire (310) and the tin-coated copper soluble material weft wire (320) with the tin-coated copper soluble material wire (300).
[0055] That is, in order to weave with finer sized copper wires, the tension is increased with a coated availability material.
[0056] After weaving, the soluble material is first melted through one or more of chemical treatment, heat treatment, and water washing to expose the warp wire and the weft wire.
[0057] After that, as a fixing means for fixing the electrode pattern, tin (200a) is melted through secondary heat treatment, and the intersections of the electrode pattern are melted and bonded to fix them.
[0058] The electrode pattern is composed of a tin-coated copper-soluble material wire (300), and the warp yarn (510) and the weft yarn (520) are woven in close contact to secure the periphery of the electrode pattern, thereby maintaining the fixing force of the electrode pattern.
[0059] In order to prevent the phenomenon of a fine tin-coated copper wire (200) being short-circuited due to insufficient tension, a tin-coated copper soluble material wire (300) is constructed by coating it with a soluble material (300a) to increase tension.
[0060] That is, the available material (300a) is formed on the above-mentioned inclined wire and the above-mentioned weft wire.
[0061] Since the four sides of the electrode pattern are wrapped with a dense density using the inclined side (510) and the oblique side (520), it can also play a role in maintaining the electrode pattern.
[0062] The warp yarn (510) and weft yarn (520) are rayon, silk, cotton, polyester, etc. and can also be used together with melting yarn.
[0063] The red square part marked as a product in the drawing is the state in which the available material applied to the metal wire has been removed.
[0064] The terms used in the specification are defined as follows.
[0065] Metal wire is a linear object made of metal, and is a term that includes all shapes including circular cross-sections.
[0066] Primary heat treatment refers to the heat treatment of melting yarn.
[0067] Secondary heat treatment means heat treatment at a melting point of the coated tin that is higher than the melting point of the melting yarn.
[0068] As a specific example in the detailed description of what is referred to as a metal wire, copper is used as the metal wire.
[0069] In drawings 1b, 2b, 3b, and 4b, only the melting yarn weft yarn (620) is indicated, and the weft yarn (520) with the specified range also includes the melting yarn weft yarn (620).
[0070] Since the number of false positives (520) is greater than that of the melting negative positives (620), it is written as the number of false positives (520) for convenience.
[0071] It is okay to configure it the other way around.
[0072] However, it is okay to make up only a portion of the melting yarn.
[0073] In addition, the melting pot syndrome (610) may also be included.
[0074] Additionally, the melting yarn slope changer (610) or the melting yarn width changer (620) can be optionally configured and both can be used.
[0075] Tin-coated copper wire (200) is a word that means a copper wire (100) in the form of tin coating or plating.
[0076] Tin-coated copper-soluble material wire (300) is a word that means coating a copper wire with tin or coating a soluble material on the surface of the tin in the form of plating.
[0077] Copper thermoplastic resin wire (400) is a word meaning a form of coating or plating of copper with thermoplastic resin wire (400a).
[0078] The term "byeonsa" refers to the use of dense weaving around an electrode pattern to add fixing force to the electrode pattern.
[0079] Melting yarn yarn (600) is a word that means using melting yarn and yarn together or using them in conjunction with the yarn.
[0080] 1. The first embodiment is a description of a woven electrode for manufacturing a basic electrode.
[0081] This is an explanation of Figure 1a.
[0082] An electrode pattern is woven by weaving a copper inclined wire (110) and a copper weft wire (120) with a copper wire (100).
[0083] The above-mentioned inclined wire and the above-mentioned weft wire are each composed of copper wire.
[0084] The purpose is to manufacture a woven electrode that constitutes a fixing means so as to maintain the above electrode pattern in a fixed state.
[0085] The above fixing means is to weave the warp yarn (520) and the warp yarn (510) surrounding the electrode pattern so that they are in close contact, thereby fixing the electrode pattern.
[0086] By weaving an electrode pattern with a copper inclined wire (110) and a copper weft wire (120) using a copper mesh, it is possible to weave an electrode pattern according to specifications while reducing the cost of the existing electrode pattern.
[0087] 2. This corresponds to the woven electrode of the second embodiment.
[0088] The description for Fig. 1b is as follows.
[0089] The above-mentioned warp yarn (510) and the weft yarn (520) are configured to include melting yarn in some of the warp yarns, and when heated to a temperature of 200°C for the first heat treatment, the melting yarn included in the some of the warp yarns including the melting yarn is melted and bonded to each other, so that the warp yarn (510) and the weft yarn (520) maintain more fixing force, so that the periphery of the electrode pattern can be secondarily fixed.
[0090] 3. Regarding the third embodiment.
[0091] The description for Fig. 2a is as follows.
[0092] Here, the fixing means is woven by coating or plating tin (200a) on the surface of the copper wire, which is the inclined wire and the weft wire, to form a tin-coated copper wire (200) for the bonding strength of the electrode pattern.
[0093] The above woven electrode pattern is heated to 300°C for secondary heat treatment, melting the tin (200a) and fixing it so that the copper wires are joined to each other at the intersection.
[0094] In addition to the above fixing means, the electrode pattern can be woven to surround the electrode pattern, thereby forming the electrode pattern with a warp yarn (510) and a weft yarn (520).
[0095] Secondary heat treatment refers to direct melting and bonding at the intersection of the warp and weft wires, and primary heat treatment is a term used to fix the warp and weft wires.
[0096] In other words, the term secondary heat treatment is not used as a prerequisite for primary heat treatment, but is used as a word to distinguish it.
[0097] 4. The description of the fourth embodiment is as follows.
[0098] The explanation for Fig. 2b is as follows.
[0099] Preferably, tin (200a) is melted and coated on copper wire or electroplated to weave the electrode, and then the tin (200a) is melted through secondary heat treatment to form a woven electrode in which the portions where the copper wires intersect in the electrode pattern are joined to each other, thereby fixing the electrode pattern.
[0100] Additionally, it is possible to construct a warp yarn (510) and a weft yarn (520) that are woven to surround the electrode pattern and fix the periphery of the electrode pattern to maintain the electrode pattern in a certain shape.
[0101] The above-mentioned warp yarn (510) and the weft yarn (520) are configured to include melting yarn in some of the warp yarns, and when the first heat treatment is performed, the melting yarn included in the some of the warp yarns including the melting yarn is melted, so that the warp yarn (510) and the weft yarn (520) are combined to further maintain fixing force, so that the periphery of the electrode pattern can be secondarily fixed.
[0102] 5. The sixth embodiment will be described as shown in Fig. 3b.
[0103] In the fifth embodiment described as the best example, when melting yarn is included in the weft yarn (520) or / and the warp yarn (510) or used by twisting the weft yarn (520) or / and the warp yarn (510) and heat-treating, the melting yarn weft yarn (620) and the melting yarn warp yarn (610) adhere to each other, thereby increasing the fixing force, thereby fixing the periphery of the electrode pattern and maintaining the electrode pattern in a constant shape.
[0104] Tin (200a) is coated on copper wire (100) so that the intersection of the warp wire and the weft wire can be melt-bonded to each other through heat treatment after weaving.
[0105] The following description is the same process in all embodiments where primary and secondary heat treatments are used.
[0106] In the first heat treatment, when melting yarn (600) is woven by twisting it with warp yarn and / or weft yarn, melting yarn is melted at 200°C to fix the periphery of the electrode pattern by fixing the yarn, thereby increasing the structural maintenance power of the electrode pattern.
[0107] When weaving by coating the above-mentioned inclined wire and the above-mentioned weft wire with a soluble material (300a), the soluble material (300a) is removed after weaving.
[0108] The available material (300a) is melted to expose the tin-coated copper wire (200), and care must be taken not to damage the melting yarn skein (620) and the melting yarn oblique (610).
[0109] That is, the soluble material (300a) configured in the woven electrode pattern is configured to expose the warp wire and the weft wire by melting the soluble material (300a) through one or more treatments such as chemical treatment, heat treatment, and water washing.
[0110] The secondary heat treatment is to melt tin (200a) at 300°C and connect the copper wires (100) at the intersections of the electrode patterns by melting them together.
[0111] This is a process of coating and weaving an available material (300a) to increase tension, and then removing the coating material, leaving only the target object.
[0112] The method of maintaining the pattern, such as the basic electrode, is the same.
[0113] 6. The seventh embodiment is as follows.
[0114] Let us explain in detail about Fig. 4a.
[0115] It relates to copper thermoplastic resin wire (400).
[0116] As a specific example of the present invention, a copper thermoplastic resin wire (400) is formed by coating Ag (nano powder) as a thermoplastic conductive resin on a copper wire.
[0117] Thermoplastic resin wire (400) increases the tension of copper wire to improve weaving properties and also enables connection of copper wires at intersections through subsequent heat treatment.
[0118] And it can simultaneously play the role of attaching the electrode to the battery.
[0119] Not only copper wire, but also tin-coated copper wire can be coated with a thermoplastic conductive resin.
[0120] Thermoplastic resin (400a) is composed of nanopowder made of any one metal such as silver, copper, tin, or nickel.
[0121] Additionally, to secure the electrode pattern, the four sides of the electrode pattern may be wrapped with a dense density of inclined side (510) and oblique side (520), thereby adding a role of maintaining the electrode pattern.
[0122] The warp yarn (510) and weft yarn (520) are rayon, silk, cotton, polyester, etc. and are used together with melting yarn.
[0123] 7. The eighth embodiment is a fabric in which some of the yarns of the seventh embodiment are partially made of melting yarn, as shown in Fig. 4b.
[0124] When melting yarn is included in the warp yarn (520) and / or warp yarn (510), or is woven using melting yarn warp yarn (610) and melting yarn weft yarn (620) by twisting the melting yarn into the warp yarn (520) and / or warp yarn (510), and then heat-treated, the warp yarn (520) and warp yarn (510) adhere to each other, increasing the fixing force, thereby having the effect of maintaining the electrode pattern.
[0125] The first heat treatment can increase the retention power of the electrode pattern structure by melting the melting yarn at 200℃ and increasing the fixing power by the warp yarn (520) and the warp yarn (510).
[0126] It is connected to each other at the intersection of the copper thermoplastic resin inclined wire (410) and the copper thermoplastic resin weft wire (420).
[0127] The thermoplastic resin wire (400a) is attached to the battery and contains nano Ag powder inside, enabling the flow of charge, so it can be attached to the desired battery through heat treatment.
[0128] It can even function to bond a woven electrode onto a solar cell, thereby simultaneously fixing and melting and bonding the cell.
[0129] Conventional electrodes are physically attached to the battery by using adhesives or by adding a film on top.
[0130] However, thermoplastic resins can be bonded directly because the electrodes are coated with an adhesive that enables electrical conductivity.
[0131] When the tension is increased by coating with thermoplastic resin (400a), it is also advantageous for manufacturing micro-electrodes of 100 micrometers or less.
[0132] In the role of maintaining the electrode pattern, the intersection of the melting yarn weft yam (620) and the melting yarn warp yam (610) can also be connected through heat treatment immediately after weaving.
[0133] The melting point of the melting yarn is 180℃ at the core and 140℃ at the outside, as shown in the drawing.
[0134] It can be used together with the fiber used for the change or by twisting it with the fiber.
[0135] When heat treatment is performed, the melting yarn slanting yarn (620) and the melting yarn oblique yarn (610) adhere to each other, increasing the fixing force and having the effect of maintaining the electrode pattern.
[0136] Tension is imparted to copper wire by coating it with thermoplastic resin.
[0137] It is to form a copper thermoplastic resin wire for melt connection and attachment to the battery at the intersection of the electrode pattern and the tension required for weaving.
[0138] The thermoplastic resin is composed of nanopowder made of one of the metals among silver, copper, tin, and nickel.
[0139] The copper thermoplastic resin wire (400) configured in this way can be connected to the copper wire at the intersection of the electrode pattern by heat treatment with the tension required for weaving, and also acts as an adhesive for attaching the woven electrode to the battery.
[0140] 8. The summary of the above explanation is as follows.
[0141] When woven with general copper wire, the electrode pattern is maintained when the weft wire and warp wire are composed of high density.
[0142] However, in the case where the density of the warp and warp wires in the electrode pattern is low (e.g., when a diameter of 100 micrometers is used and the spacing between wires is 5 millimeters), it is difficult to maintain the electrode pattern, so there is a possibility that the product will not maintain its shape and become disordered after weaving the woven electrode.
[0143] In order to physically connect the intersections of the warp and warp wires, a process of fusion bonding is required at each intersection.
[0144] A method for maintaining the electrode pattern after weaving a woven electrode is possible if the weft and warp wires are woven at a high density or if the weft and warp wires are physically connected at the intersections.
[0145] The fixation of the electrode pattern is achieved by fixing the periphery of the electrode pattern using a variable.
[0146] As an alternative to increasing density, if the fabric is woven at a high density at regular intervals, the force to maintain the pattern in that part is high, which is advantageous in maintaining the pattern overall.
[0147] Of course, in this case, it is helpful to maintain the electrode pattern that is actually used by weaving the warp yarn (510) and the weft yarn (520) so that a high density is maintained that can hold the electrode pattern in each direction on the surface of the electrode pattern.
[0148] A method for connecting the intersection of the warp yarn (520) and the oblique yarn (510), the first method for connecting the intersection is to add melting yarn to the warp yarn.
[0149] The melting point of melting yarn is 140℃ on the outside and 180℃ on the inside, so it is a thermoplastic resin that melts when a temperature higher than the melting point of 200℃ is applied.
[0150] As the melting yarn melts, it helps maintain the electrode pattern by connecting the warp yarn (510) and the weft yarn (520).
[0151] A second method for connecting cross-sections is to use tin (200a) plated on copper wire. Since tin (200a) has a melting point of 232°C, it melts when heat-treated above this temperature, and the two wires are fused and connected at the intersection of the warp and weft wires.
[0152] In the present invention, the temperature was set at 300°C.
[0153] The connection of the warp wire and the warp wire by the comment (200a) increases the electrical conductivity and enhances the function as an electrode.
[0154] Instead of a comment, it is possible to connect the cross points with an available material wire.
[0155] 9. About the electrode pattern border
[0156] This is explained as follows by Fig. 5.
[0157] A unit electrode pattern (750) is divided into a boundary between a circumferential and an oblique pattern surrounding the four sides.
[0158] As an example of using an electrode pattern (750), an electrode pattern (750) corresponding to one unit is configured so that when the electrode pattern (750) is blanked to fit the size of a solar cell unit cell, the edge of the electrode pattern (750) is firmly maintained so that the shape of the electrode pattern (750) can be maintained.
[0159] The edge of the electrode pattern (750) is woven by narrowing the weaving interval between two or three wires.
[0160] When weaving, a high-density warp yarn border (710) and a high-density weft yarn border (720) are formed so that the shape of the electrode pattern (750) is not disturbed when the electrode pattern (750) is punched out.
[0161] In the tin bonding process, tin is deposited not only at the intersection of the copper inclined wire and the copper weft wire but also at the edge portion, so that the edge portion of the unit electrode pattern can be implemented to more firmly maintain the shape of the electrode pattern.
[0162] 10. About the metal film frame
[0163] Another way to explain this is as follows, as shown in Figure 6.
[0164] In order to maintain the shape of the formed electrode pattern more firmly when stamping an electrode pattern (850), a metal film (800) having copper and tin deposited on the edge is formed and woven to maintain the edge of the electrode pattern more firmly than the fusion force of the copper inclined wire (110) and copper weft wire (120).
[0165] Metal film yarn (800) is used by depositing copper on a film and then depositing tin (200a) on the copper. Since tin (200a) has a melting point of 232°C, it melts when heat-treated above this temperature, and the two lines of the metal film yarn (800) are fused and connected at the intersection of the metal film slant edge portion (810) and the metal film weft edge portion (820).
[0166] Any flexible film such as PET will suffice.
[0167] Any conductive metal is sufficient as the deposited metal on the film.
[0168] Typically, Cu is used as a conductive metal.
[0169] In an embodiment of the present invention, tin is deposited after Cu is deposited on a film.
[0170] It is preferable that the thickness of the metal film (800) formed in this way be 0.2 to 1.2 mm and the line width be 0.5 to 3.0 mm.
[0171] As shown in Fig. 6, when weaving, a metal film inclined edge portion (810) and a metal film weft edge portion (820) are formed on the edge portion of the electrode pattern (850) so that the shape of the electrode pattern (850) is not distorted when the electrode pattern (850) is cut out.
[0172] Terms or words used in this specification and claims should not be interpreted as limited to their usual or dictionary meanings, but should be interpreted as meanings and concepts that conform to the technical idea of the present invention, based on the principle that the inventor can appropriately define the concept of the term to explain his or her own invention in the best way.
[0173] Accordingly, the embodiments described in this specification and the configurations illustrated in the drawings are only the most preferred embodiments of the present invention and do not represent all of the technical ideas of the present invention. Therefore, it should be understood that there may be various equivalents and modified examples that can be replaced at the time of filing this application.
[0174] The electrode of the present inventor configured in a woven form is currently being used in many technical fields.
[0175] Although it is difficult to maintain fixing force in a woven electrode, the present invention relates to a technology for providing fixing force to a woven electrode, which greatly contributes to the production and efficiency of woven electrodes and is thus industrially applicable.
[0176] The present invention has the effect of simultaneously securing electrical conductivity and maintaining fixing force between a woven metal wire electrode and a battery surface layer by combining a thermoplastic resin with a warp wire and a warp wire, and is thus industrially applicable.
Claims
1. Weave the electrode pattern with the warp wire and the weft wire. The above-mentioned inclined wire and the above-mentioned weft wire are each composed of conductive metal wires, A woven metal wire electrode characterized in that a fixing means is configured to secure electrical conductivity by fixing the above electrode pattern.
2. In the first paragraph, the fixing means comprises a tin-coated metal wire in which tin is coated on the surface of the metal wire, which is the inclined wire and the weft wire. A woven metal wire electrode characterized in that the electrode pattern is fixed by melting the tin coated on the woven electrode pattern through heat treatment to ensure electrical conductivity at the intersection of the tin-coated metal wires.
3. In the first paragraph, the fixing means is woven to surround the electrode pattern on all sides, and the circumference of the electrode pattern is woven with warp and weft yarns. A woven metal wire electrode characterized in that the electrode pattern is primarily fixed by weaving the above-mentioned warp yarn and the above-mentioned warp yarn so as to be in close contact with each other and fixing the periphery of the electrode pattern.
4. A woven metal wire electrode characterized in that, in the third paragraph, a soluble material is coated on the tin-coated metal wire to increase the tension of the warp wire and the weft wire, thereby preventing the warp wire and the weft wire from breaking during weaving.
5. A woven metal wire electrode characterized in that the soluble material configured in the woven electrode pattern in paragraph 4 is melted through at least one of chemical treatment, heat treatment, and water washing to expose the warp wire and the weft wire to secure electrical conductivity.
6. A woven metal wire electrode characterized in that, in the first paragraph, the surface of the metal wire is coated with a thermoplastic conductive resin to enhance the tension of the warp wire and the weft wire, the fixing force of the electrode pattern, and the electrical conductivity between the warp wire and the weft wire, and to exhibit a bonding function that secures electrical conductivity between the electrode pattern and the solar cell.
7. A woven metal wire electrode characterized in that the thermoplastic conductive resin in the 6th paragraph contains nanopowder of any one of silver, copper, tin, and nickel.
8. A woven metal wire electrode characterized in that, in the third paragraph, some of the warp yarns and the weft yarns are configured to include melting yarns, and when heat-treated, the melting yarns included in the some of the warp yarns including the melting yarns are melted and combined to further increase the fixing force of the warp yarns and the weft yarns, so that the periphery of the electrode pattern can be further fixed.
9. A woven metal wire electrode according to any one of claims 2 to 6, wherein the warp yarn and the weft yarn are composed of at least one of rayon, silk, cotton, and polyester, and wherein one or more of the warp yarns and the weft yarns are composed of a melting yarn mixed therein.
10. A woven metal wire electrode characterized in that, in any one of paragraphs 2 to 6, when weaving the edge of the electrode pattern, the interweaving interval of the tin-coated copper wire or the copper thermoplastic resin wire in the edge is narrowed to increase the density, and then the copper warp wire and the copper weft wire are fused by pressurized heating not only at the intersection but also at the edge, so that the edge is firmly maintained even after the electrode pattern is punched out.
11. A woven metal wire electrode characterized in that, in any one of the second to sixth paragraphs, the woven metal wire electrode is configured to weave a metal film yarn into the rim portion when weaving the rim portion of the electrode pattern.
12. A woven metal wire electrode characterized in that the width of the metal film yarn in the 11th paragraph is configured to be 0.5 to 3.0 mm.
Citation Information
Patent Citations
Lithium battery electrode, method of manufacturing the same, and lithium battery
JP2011034913A
PTFE fabric articles and their production methods
JP2012512770A
Element for electrode and secondary battery using the same
JP2013004179A
Textile electrode and accumulator containing such an electrode
KR1020090014304A
Electrode for Secondary Battery Comprising Electrode Wires and Method for Manufacturing the Same