Manganese phosphate nanomaterials and their preparation method and application
By preparing manganese phosphate nanomaterials with a single valence state of manganese element, the problems of complex valence states and difficulty in preservation of nanomanganese materials are solved, achieving stable application in the field of vaccines and strong immune response effects.
Patent Information
- Application Number
- CN202211377526.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-11-04
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2042-11-04
AI Technical Summary
Existing nanomanganese materials have complex valence changes of manganese element, cumbersome preparation process and difficulty in long-term storage, which limits their application in the field of vaccines.
A specific method is used to prepare manganese phosphate nanomaterials with a single valence state of manganese element (+2 valence). The chemical composition is Mn3(PO4)2·nH2O. By controlling the dosage and pH value of dihydrogen phosphate and monohydrogen phosphate, Forming uniform nanoparticles ensures their stable degradation in acidic environments to release manganese ions and enhance immune response.
It achieves a high degree of uniformity and long-term stability of manganese phosphate nanomaterials, enhances the immunogenicity and cellular immune response of the antigen, is suitable as a vaccine adjuvant, can efficiently induce strong neutralizing antibody responses, and is suitable for large-scale production.
Smart Images

Figure CN115744853B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the fields of biomedicine technology and vaccine technology, and in particular to manganese phosphate nanomaterials and preparation methods and applications thereof. Background Art
[0002] Vaccination is the technology of inoculating vaccine preparations into humans or animals, so that the recipient can gain immunity against a specific pathogen or a pathogen similar to the vaccine. Through the recognition of foreign substances by the immune system, antibodies are screened and manufactured to produce antibodies against the pathogen or similar pathogens, thereby making the recipient have a stronger resistance to the disease. There are many types of vaccines, among which recombinant protein vaccines are vaccines prepared by constructing the target antigen gene on an expression vector, transforming the constructed expression protein vector into bacteria, yeast, mammalian or insect cells, and expressing a large amount of antigen protein under certain induction conditions, and then purifying it. Therefore, recombinant protein vaccines have the advantages of high yield, good biosafety, and high stability. However, the immunogenicity of protein antigens is weak, and suitable adjuvants are often required to enhance the immune response.
[0003] Aluminum adjuvants are the only adjuvants approved for widespread use in human vaccines due to their great safety. However, aluminum adjuvants mainly induce Th2-biased immune responses and are difficult to induce strong cellular immune responses. However, cellular immune responses are crucial for clearing virus-infected cells and cancerous cells. In addition, traditional aluminum adjuvants are often heterogeneous and difficult to form a uniform and stable structure, which also limits their medical applications to a certain extent.
[0004] Manganese is one of the most important essential trace elements involved in various physiological activities such as human bone development and metabolism. 2+ It can activate the cyclic GMP-AMP synthase-interferon gene stimulator (cGAS-STING) pathway and trigger a unique 2',3'-cyclic guanosine monophosphate-adenosine monophosphate (2,3'-c-GAMP) catalytic synthesis and induce type I interferon (IFN) response. 2+ It can be used as a potential STING agonist to induce a strong immune response. However, the direct administration of soluble manganese ions causes them to diffuse rapidly at the injection site, making it difficult to induce a local immune response, which greatly limits its effect. To overcome this limitation, nanomanganese materials are one of the best choices as manganese adjuvants. Compared with soluble manganese ions, nanomanganese materials can maintain the continuous release of manganese ions at the injection site to induce a local immune response, enhance the cellular uptake of antigens by dendritic cells (DCs), and promote the activation and maturation of DCs in vivo.
[0005] However, these nanomanganese materials may have some limitations, such as complex valence changes of manganese elements, complicated preparation process, and difficulty in long-term preservation. Summary of the invention
[0006] The purpose of the present invention is to overcome the problems of the existing technology that the valence state of nanomanganese materials is complex, it is difficult to preserve for a long time, and the preparation process is relatively cumbersome, and a manganese phosphate nanomaterial and its preparation method and application are provided. The present invention adopts a specific method to prepare a new manganese phosphate nanomaterial with a single manganese element valence state (+2 valence), and its chemical composition is Mn3(PO4)2·nH2O. The manganese phosphate nanomaterial prepared by this method has a high degree of uniformity, can be stored stably for a long time, and has good pH sensitivity. The material is stable under neutral conditions. After being taken up by cells, it can be degraded into free manganese ions in the acidic environment of the inclusion body and released into the cytoplasm to enhance the immune response by activating the STING pathway.
[0007] In order to achieve the above object, the present invention provides a method for preparing a manganese phosphate nanomaterial, the method comprising:
[0008] (1) adding dihydrogen phosphate solution to divalent manganese salt solution and stirring;
[0009] (2) adding a monohydrogen phosphate solution to the mixed solution obtained in step (1);
[0010] (3) Stirring the suspension obtained in step (2), and then centrifuging to obtain manganese phosphate nanomaterials.
[0011] Preferably, the molar ratio of the manganese element, dihydrogen phosphate and monohydrogen phosphate in the divalent manganese salt is 1:0.1-100:0.1-100, preferably 1:0.1-50:0.1-50, more preferably 1:0.5-20:0.5-20, further preferably 1:0.5-5:1-12.
[0012] Preferably, in step (1), the divalent manganese salt is selected from one or two of manganese chloride, manganese nitrate, manganese acetate, manganese sulfate and manganese oxalate, and their crystalline hydrates; preferably, the divalent manganese salt is manganese chloride tetrahydrate.
[0013] Preferably, the concentration of the divalent manganese salt is 0.1-10 mol / L.
[0014] Preferably, in step (1), the dihydrogen phosphate is selected from one or more of sodium dihydrogen phosphate, potassium dihydrogen phosphate, ammonium dihydrogen phosphate, aluminum dihydrogen phosphate and calcium dihydrogen phosphate, and their crystalline hydrates; preferably, the dihydrogen phosphate is sodium dihydrogen phosphate.
[0015] Preferably, in step (1), the concentration of the dihydrogen phosphate solution is 0.1 to 10 mol / L.
[0016] Preferably, in step (2), the monohydrogen phosphate is selected from one or more of disodium hydrogen phosphate, dipotassium hydrogen phosphate, diammonium hydrogen phosphate and calcium hydrogen phosphate, and their crystalline hydrates; preferably, the monohydrogen phosphate is disodium hydrogen phosphate.
[0017] Preferably, in step (2), the concentration of the monohydrogen phosphate solution is 0.1 to 10 mol / L.
[0018] Preferably, in step (1), the stirring time is 5 minutes to 200 hours, and the stirring time is 10 to 60 minutes.
[0019] Preferably, in step (3), the stirring conditions include: a stirring temperature of 10 to 37° C., a stirring time of 1 to 20 hours, and a stirring rate of 100 to 1000 r / min.
[0020] Preferably, in step (3), the centrifugal conditions include: a centrifugal rate of 50 to 5000 rpm, preferably 1000 to 3000 rpm; and a centrifugal time of 5 to 60 minutes, preferably 10 to 30 minutes.
[0021] The second aspect of the present invention provides a manganese phosphate nanomaterial prepared by the method described above, wherein the chemical formula of the manganese phosphate nanomaterial is Mn3(PO4)2·nH2O, wherein n is any integer between 0 and 10, and the Mn element has a valence of +2.
[0022] Preferably, the particle size of the manganese phosphate nanomaterial is 1 to 200 nm.
[0023] The third aspect of the present invention provides a manganese phosphate nanomaterial prepared by the method described above and use of the manganese phosphate nanomaterial described above in the preparation of a drug for treating immune-related diseases.
[0024] Preferably, the drug is an antiviral drug, an antifungal drug, an antibacterial drug, an antiparasitic drug, a drug for treating autoimmune diseases or a drug for treating cancer.
[0025] Preferably, the virus is a DNA virus or an RNA virus; preferably, it is from the family Herpesviridae, Rhabdoviridae, Filoviridae, Orthomyxoviridae, Paramyxoviridae, Coronaviridae, Hepadnaviridae, Flaviviridae, Papillomaviridae, Poxviridae or Retroviridae.
[0026] Preferably, the fungus is selected from the group consisting of Histoplasma, Coccidioides, Coccidioides, Blastomyces dermatitidis, Chromatid fungi, Mycetoma, Sporothrix, Candida albicans, Candida glabrata, Candida tropicalis, Cryptococcus, Aspergillus, Mucor, Actinomycetes, Nocardia asteroides, Nocardia brasiliensis, Nocardia caviae, Nocardia southafrica, Nocardia glanders or Nocardia novae.
[0027] Preferably, the bacterium is selected from Gram-negative bacteria or Gram-positive bacteria, more preferably, the bacterium is selected from Streptococcus pneumoniae, Haemophilus influenzae, Salmonella, Neisseria meningitidis, Staphylococcus epidermidis, Staphylococcus aureus, Escherichia coli, Klebsiella pneumoniae, Klebsiella oxytoca, Enterobacter cloacae, Citrobacter freundii, Pseudomonas aeruginosa or Acinetobacter baumannii.
[0028] Preferably, the parasite is selected from Plasmodium, Toxoplasma, Trypanosoma, Schistosoma, Filarial worm or Leishmania.
[0029] Preferably, the autoimmune disease is selected from type I diabetes, psoriasis, rheumatoid arthritis, systemic lupus erythematosus or multiple sclerosis.
[0030] Preferably, the cancer is selected from breast cancer, ovarian cancer, lung cancer, gastric cancer, liver cancer, pancreatic cancer, skin cancer, malignant melanoma, head and neck cancer, sarcoma, bile duct cancer, kidney cancer, colorectal cancer, placental choriocarcinoma, cervical cancer, testicular cancer, uterine cancer or leukemia.
[0031] The method of the present invention adopts a specific method to prepare a novel manganese phosphate nanoparticle with a single manganese element valence state, wherein the chemical composition of the novel manganese phosphate nanoparticle is Mn3(PO4)2·nH2O, while the manganese in the existing manganese phosphate nanoparticle has multiple valence states and the valence states are complex. The manganese phosphate nanoparticle prepared by the method has high uniformity, can be stored stably for a long time, is biodegradable, has good pH sensitivity, and can be degraded and release manganese ions under acidic conditions to enhance immune response. The nanomaterial can be used as a nanoreservoir of divalent manganese ions, can be degraded in a slightly acidic environment in tissues or cells, and releases free manganese ions to activate immune cells to enhance immune response.
[0032] The manganese phosphate nanoparticles of the present invention can be used alone as a component for stimulating innate immunity and / or adaptive immunity, or as an immune adjuvant. The manganese phosphate nanoparticles provided by the present invention are used as immune adjuvants to greatly enhance the immunogenicity of antigens, thereby enhancing antigen-specific humoral and cellular immune responses.
[0033] The manganese phosphate nanomaterial of the present invention is easy to synthesize and can effectively enhance the efficiency of antigen molecule lymph node delivery and antigen immunogenicity. The manganese nanoadjuvant in the constructed nanovaccine can stably and effectively carry antigen molecules and effectively enhance antigen-specific antibodies and T cell responses. The natural targeting properties of albumin and the size effect of the nanovaccine make the manganese nanoadjuvant suitable for effective drainage and retention in the lymph nodes, greatly increasing cell uptake and activation of immune cells, thereby enhancing antigen-specific immune responses.
[0034] The experimental results show that even after only two immunizations, the protein vaccine constructed using manganese nanoadjuvants in mice can effectively induce humoral and cellular immune responses. More importantly, the constructed protein vaccine can induce a strong neutralizing antibody response, which can cross-neutralize the new coronavirus and all of its five worrying variants (Alpha, Beta, Gamma, Delta and Omicron). Finally, the constructed manganese phosphate nanoparticles are low-cost, simple to prepare, and can adapt to large-scale production needs, greatly increasing the possibility of further clinical research.
[0035] In addition, the simple and clear characteristics of the nano manganese phosphate composition also help simplify its clinical transformation process. The biological test results show that nano manganese phosphate can be used as an adjuvant to induce the production of higher titers of specific and neutralizing antibodies and trigger a strong cellular immune response.
[0036] Compared with the prior art, the present invention has at least the following advantages:
[0037] 1) Manganese phosphate nanoparticles with uniform particle size and defined structural composition were prepared, ensuring the certainty of the adjuvant chemical structure and batch reproducibility.
[0038] 2) The prepared nano manganese phosphate particles can be stored for a long time at room temperature and will not deteriorate or precipitate even under high or low temperature conditions.
[0039] 3) The prepared nano manganese phosphate particles can effectively stimulate the activation and maturation of dendritic cells in vivo, and can induce the production of high-affinity antibody titers against antigen proteins and strong cellular immune responses.
[0040] 4) The prepared nano manganese phosphate particles have good biosafety and biocompatibility while enhancing immunostimulatory activity. BRIEF DESCRIPTION OF THE DRAWINGS
[0041] Figure 1 The change in turbidity and the Tyndall effect during the production of the manganese phosphate nanomaterial prepared in Example 1;
[0042] Figure 2The SEM and TEM images of the manganese phosphate nanomaterial prepared in Example 1 and the particle size distribution in the TEM image;
[0043] Figure 3 is an X-ray photoelectron spectrum data image of the manganese phosphate nanomaterial prepared in Example 1;
[0044] Figure 4 is a scanning electron microscope-X-ray energy spectrum diagram (surface scan) of the manganese phosphate nanomaterial prepared in Example 1;
[0045] Figure 5 is the thermogravimetric analysis data of the manganese phosphate nanomaterial prepared in Example 1;
[0046] Figure 6 It is a dynamic light scattering analysis and dispersion stability test diagram of the manganese phosphate nanomaterials prepared in Example 1, Comparative Example 1 and Comparative Example 2;
[0047] Figure 7 It is a dynamic light scattering analysis and dispersion stability test diagram of the manganese phosphate nanomaterials prepared in Example 2 and Example 3;
[0048] Figure 8 The long-term stability test of the manganese phosphate nanomaterial prepared in Example 1 and the stability test (dynamic light scattering analysis) stored under different temperature conditions;
[0049] Fig. 9 It is the acid sensitivity test of the manganese phosphate nanomaterial prepared in Example 1;
[0050] Fig.10 The flow cytometric analysis of the maturation and activation of dendritic cells in mice after two immunizations using the manganese phosphate nanomaterials prepared in Example 1 as an adjuvant to prepare a vaccine;
[0051] Fig.11 The flow cytometric analysis of the maturation and activation of dendritic cells in mice after two immunizations using the manganese materials prepared in Examples 1-3 and Comparative Examples 1-2 as adjuvants to make vaccines;
[0052] Fig.12 The specific IgM antibody titer in the serum of mice after two immunizations was evaluated after the manganese phosphate nanomaterials prepared in Example 1 were used as adjuvants to prepare vaccines;
[0053] Fig.13 The specific IgG antibody titer in the serum of mice after two immunizations was evaluated after the manganese phosphate nanomaterials prepared in Example 1 were used as adjuvants to prepare vaccines;
[0054] Fig.14The neutralizing antibody titer in the serum of mice after two immunizations was evaluated after the manganese phosphate nanomaterial prepared in Example 1 was used as an adjuvant to prepare a vaccine;
[0055] Fig.15 The manganese phosphate nanomaterial prepared in Example 1 was used as an adjuvant to prepare a vaccine, and the ELISPOT test of mouse spleen cells after two immunizations;
[0056] Fig.16 This is an experiment of intracellular cytokine staining of spleen cells of mice after two immunizations after the manganese phosphate nanomaterials prepared in Example 1 were used as adjuvants to make vaccines;
[0057] Fig.17 The blood biochemical analysis of mice after two immunizations with the manganese phosphate nanomaterials prepared in Example 1 as an adjuvant to make a vaccine;
[0058] Fig.18 This is a slice observation image of the main organs of mice after two immunizations after the manganese phosphate nanomaterial prepared in Example 1 was used as an adjuvant to make a vaccine;
[0059] Fig.19 It is a schematic diagram of the preparation process of the manganese phosphate nanomaterial of the present invention. DETAILED DESCRIPTION
[0060] The specific implementation of the present invention is described in detail below in conjunction with the accompanying drawings. It should be understood that the specific implementation described here is only used to illustrate and explain the present invention, and is not used to limit the present invention.
[0061] The endpoints and any values of the ranges disclosed in this article are not limited to the precise ranges or values, and these ranges or values should be understood to include values close to these ranges or values. For numerical ranges, the endpoint values of each range, the endpoint values of each range and the individual point values, and the individual point values can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed in this article.
[0062] The first aspect of the present invention provides a method for preparing a manganese phosphate nanomaterial, the method comprising:
[0063] (1) adding dihydrogen phosphate solution to divalent manganese salt solution and stirring;
[0064] (2) adding a monohydrogen phosphate solution to the mixed solution obtained in step (1);
[0065] (3) Stirring the suspension obtained in step (2), and then centrifuging to obtain manganese phosphate nanomaterials.
[0066] The method of the present invention adopts three raw materials of divalent manganese salt, dihydrogen phosphate and monohydrogen phosphate to prepare the material in a specific adding order, and the method is simple and easy to operate. In the present invention, after the manganese phosphate nano material is prepared, the manganese phosphate nano material can be resuspended in a PBS buffer solution for storage and use.
[0067] The inventors found that divalent manganese ions can form manganese dihydrogen phosphate, also known as acid manganese phosphate or Marib salt, in an acidic dihydrogen phosphate solution, which is completely soluble in water. With the increase of pH value, manganese dihydrogen phosphate is gradually converted into manganese phosphate precipitation that is insoluble in water, and the precipitation is completely generated when the solution reaches neutrality. However, when manganese ions are directly added to a neutral phosphate buffer, manganese ions quickly generate manganese phosphate precipitation, and this process is rapid and violent, so the generated precipitation particles are relatively large, reaching more than 1500nm, and this large particle form is not suitable for the preparation of vaccines. Using this principle, the inventors use a buffer pair of monohydrogen phosphate and dihydrogen phosphate, gradually add alkaline monohydrogen phosphate to acid manganese phosphate, and use the characteristics of the buffer pair to make the pH value gradually change, so that the conversion of precipitation is more gentle, thereby forming uniform and smaller (40nm) nanoparticles, which are of this size and are conducive to transport to lymph nodes to exert immune effects, and their uniform characteristics are also conducive to large-scale production and preparation of vaccines.
[0068] The method of the present invention is not limited thereto, and any method recognized by those skilled in the art that can form manganese phosphate nanomaterials by adjusting the pH value of phosphate buffer is within the protection scope of the present invention.
[0069] In the method of the present invention, in order to obtain manganese phosphate nanomaterials, it is necessary to control the dosage ratio of divalent manganese salt, dihydrogen phosphate and monohydrogen phosphate. In a specific embodiment, the molar ratio of the dosage of manganese element, dihydrogen phosphate and monohydrogen phosphate in the divalent manganese salt can be 1:0.1-100:0.1-100, preferably 1:0.1-50:0.1-50, more preferably 1:0.5-20:0.5-20, further preferably 1:0.5-5:1-12, for example 1:0.5:1, 1:5:12, 1:1:6, 1:1.5:8, 1:3:10, 1:4:2, 1:2:4 or 1:2.5:1. In a particularly preferred embodiment, the molar ratio of manganese element, dihydrogen phosphate and monohydrogen phosphate in the divalent manganese salt is 1:1.5:6.
[0070] In the method of the present invention, in step (2), after adding dihydrogen phosphate solution and monohydrogen phosphate solution to divalent manganese salt solution, the amount of substance of manganese element in raw material divalent manganese salt is calculated, and the total volume of divalent manganese salt solution, dihydrogen phosphate solution and monohydrogen phosphate solution is calculated to obtain the amount of substance concentration of manganese element in suspension at this time. In a preferred embodiment, the concentration of manganese element is 5-15mmol / L, for example, 5mmol / L, 10mmol / L and 15mmol / L. Similarly, the amount of substance of raw material dihydrogen phosphate and monohydrogen phosphate is calculated, and the total volume of divalent manganese salt solution, dihydrogen phosphate solution and monohydrogen phosphate solution is calculated to obtain the amount of substance concentration of dihydrogen phosphate and monohydrogen phosphate respectively. In a preferred embodiment, the concentration of NaH2PO4 is 5-50mmol / L, for example, 5mmol / L, 10mmol / L, 15mmol / L, 20mmol / L, 30mmol / L, 40mmol / L or 50mmol / L. In a preferred embodiment, the concentration of Na2HPO4 is 10 to 120 mmol / L, for example, 10 mmol / L, 20 mmol / L, 30 mmol / L, 40 mmol / L, 50 mmol / L, 60 mmol / L, 70 mmol / L, 80 mmol / L, 90 mmol / L, 100 mmol / L, 110 mmol / L or 120 mmol / L.
[0071] In the method of the present invention, the divalent manganese salt is a soluble salt that can provide divalent manganese, which is well known in the art, including anhydrous manganese salts and crystalline hydrates. In a specific embodiment, in step (1), the divalent manganese salt can be selected from one or two of manganese chloride, manganese nitrate, manganese acetate, manganese sulfate and manganese oxalate, and their crystalline hydrates. In a preferred embodiment, the divalent manganese salt is manganese chloride tetrahydrate. In the method of the present invention, in the divalent manganese salt solution, the concentration of the divalent manganese salt can be 0.1 to 10 mol / L, such as 0.1 mol / L, 0.5 mol / L, 1 mol / L, 2 mol / L, 3 mol / L, 4 mol / L, 5 mol / L, 6 mol / L, 7 mol / L, 8 mol / L, 9 mol / L or 10 mol / L.
[0072] In the method of the present invention, the dihydrogen phosphate can be a conventional choice in the art. In a specific embodiment, in step (1), the dihydrogen phosphate can be selected from one or more of sodium dihydrogen phosphate, potassium dihydrogen phosphate, ammonium dihydrogen phosphate, aluminum dihydrogen phosphate and calcium dihydrogen phosphate, and their crystalline hydrates. In a preferred embodiment, the dihydrogen phosphate is sodium dihydrogen phosphate. In a specific embodiment, in step (1), the concentration of the dihydrogen phosphate solution can be 0.1 to 10 mol / L, such as 0.1 mol / L, 0.5 mol / L, 1 mol / L, 2 mol / L, 3 mol / L, 4 mol / L, 5 mol / L, 6 mol / L, 7 mol / L, 8 mol / L, 9 mol / L or 10 mol / L.
[0073] In the method of the present invention, the monohydrogen phosphate can be a conventional choice in the art. In a specific embodiment, in step (2), the monohydrogen phosphate can be selected from one or more of disodium hydrogen phosphate, dipotassium hydrogen phosphate, diammonium hydrogen phosphate and calcium hydrogen phosphate, and their crystalline hydrates. In a preferred embodiment, the monohydrogen phosphate is disodium hydrogen phosphate. In the method of the present invention, in step (2), the concentration of the monohydrogen phosphate solution can be 0.1 to 10 mol / L, for example 0.1 mol / L, 0.5 mol / L, 1 mol / L, 2 mol / L, 3 mol / L, 4 mol / L, 5 mol / L, 6 mol / L, 7 mol / L, 8 mol / L, 9 mol / L or 10 mol / L.
[0074] In the method of the present invention, after adding the dihydrogen phosphate solution to the divalent manganese salt solution, stirring is required to allow the solution to be fully mixed and reacted. In a specific embodiment, in step (1), the stirring time is 5 minutes to 200 hours, preferably 10 to 60 minutes.
[0075] In the method of the present invention, in order to make the reaction fully proceed and obtain manganese phosphate nanoparticles with a single manganese valence state and uniform particle size, it is necessary to stir for a long time after adding the monohydrogen phosphate solution. In a specific embodiment, in step (3), the stirring conditions include: the stirring temperature can be 10-37°C, such as 10°C, 15°C, 20°C, 25°C, 30°C, 35°C or 37°C; the stirring time can be 1-20 hours, such as 1 hour, 1 hour, 3 hours, 5 hours, 8 hours, 10 hours, 12 hours, 15 hours, 18 hours or 20 hours; the stirring rate can be 100-1000r / min, such as 100r / min, 200r / min, 300r / min, 400r / min, 500r / min, 600r / min, 700r / min, 800r / min, 900r / min or 1000r / min.
[0076] In the method of the present invention, in order to obtain manganese phosphate nanoparticles, solid-liquid separation is required. In the present invention, the method for solid-liquid separation is centrifugation. In a specific embodiment, in step (3), the centrifugal conditions include: the centrifugal rate can be 50 to 5000 rpm, preferably 1000 to 3000 rpm, such as 1000 rpm, 1500 rpm, 2000 rpm, 2500 rpm or 3000 rpm; the centrifugal time can be 5 to 60 minutes, preferably 10 to 30 minutes, such as 10 minutes, 20 minutes or 30 minutes.
[0077] The second aspect of the present invention provides a manganese phosphate nanomaterial prepared by the method described above. The chemical formula of the manganese phosphate nanomaterial is Mn3(PO4)2·nH2O, wherein n can be any integer between 0 and 10, specifically, n can be, for example, 0, 1, 2, 3, 4, 5, 6, 7, 8, 9 or 10, preferably, n is 3. The Mn element in the manganese phosphate nanomaterial has a single valence state, which is +2.
[0078] The particle size of the manganese phosphate nanomaterial obtained by the present invention is uniform. The particle size of the manganese phosphate nanomaterial can be 1 to 200 nm, for example, 1 nm, 10 nm, 20 nm, 40 nm, 50 nm, 80 nm, 100 nm, 120 nm, 140 nm, 160 nm, 180 nm or 200 nm. Preferably, the particle size of the manganese phosphate nanomaterial is 1 to 100 nm.
[0079] The third aspect of the present invention provides a manganese phosphate nanomaterial prepared by the method described above and the use of the manganese phosphate nanomaterial described above in the preparation of a drug for treating immune-related diseases. The manganese phosphate nanomaterial can be used alone as a component to stimulate innate immunity and / or adaptive immunity, or as an immune adjuvant for preventive vaccines or therapeutic vaccines.
[0080] The method of the present invention is not limited thereto. The combined use of the manganese phosphate nanomaterial and other immunostimulants, including TLR agonists, NKT cell agonists, aluminum salt adjuvants, oil-in-water emulsions, cytokines, etc., are all within the scope of protection of the present invention.
[0081] In the application of the present invention, the drug can be an antiviral drug, an antifungal drug, an antibacterial drug, an antiparasitic drug, a drug for treating autoimmune diseases, or a drug for treating cancer.
[0082] In a specific embodiment, the virus is a DNA virus or an RNA virus; preferably, it is from the family Herpesviridae, Rhabdoviridae, Filoviridae, Orthomyxoviridae, Paramyxoviridae, Coronaviridae, Hepadnaviridae, Flaviviridae, Papillomaviridae, Poxviridae or Retroviridae.
[0083] In a specific embodiment, the fungus is selected from the group consisting of Histoplasma, Coccidioides, Coccidioides, Blastomyces dermatitidis, Chromatids, Mycetoma, Sporothrix, Candida albicans, Candida glabrata, Candida tropicalis, Cryptococcus, Aspergillus, Mucor, Actinomycetes, Nocardia asteroides, Nocardia brasiliensis, Nocardia caviae, Nocardia southafrica, Nocardia glanders, or Nocardia novae.
[0084] In a specific embodiment, the bacterium is selected from Gram-negative bacteria or Gram-positive bacteria, more preferably, the bacterium is selected from Streptococcus pneumoniae, Haemophilus influenzae, Salmonella, Neisseria meningitidis, Staphylococcus epidermidis, Staphylococcus aureus, Escherichia coli, Klebsiella pneumoniae, Klebsiella oxytoca, Enterobacter cloacae, Citrobacter freundii, Pseudomonas aeruginosa or Acinetobacter baumannii.
[0085] In a specific embodiment, the parasite is selected from Plasmodium, Toxoplasma, Trypanosoma, Schistosoma, Filarial worm or Leishmania.
[0086] In a specific embodiment, the autoimmune disease is selected from type I diabetes, psoriasis, rheumatoid arthritis, systemic lupus erythematosus or multiple sclerosis.
[0087] In a specific embodiment, the cancer is selected from breast cancer, ovarian cancer, lung cancer, gastric cancer, liver cancer, pancreatic cancer, skin cancer, malignant melanoma, head and neck cancer, sarcoma, bile duct cancer, kidney cancer, colorectal cancer, placental choriocarcinoma, cervical cancer, testicular cancer, uterine cancer or leukemia.
[0088] The present invention will be described in detail below through examples, but the method of the present invention is not limited thereto.
[0089] In the following examples, the test methods used are conventional methods unless otherwise specified. The materials, reagents, etc. used in the following examples are all commercially available unless otherwise specified.
[0090] Example 1
[0091] (1) Add 136.4 μL of 1.0 mol / L MnCl2·4H2O solution to 12.48 mL of deionized water and stir for 10 minutes until the mixture is uniform;
[0092] (2) adding 204.5 μL of 1.0 mol / L NaH2PO4 solution to the solution obtained in step (1), and stirring for 10 minutes until the mixture is uniform;
[0093] (3) quickly adding 818 μL of 1.0 mol / L Na2HPO4 solution to the MnCl2 / NaH2PO4 mixed solution obtained in step (2) to obtain a suspension, wherein the final concentrations of MnCl2, NaH2PO4 and Na2HPO4 are 10 mmol / L, 15 mmol / L and 60 mmol / L, respectively, and the final pH value of the supernatant is measured to be 7.4;
[0094] (4) The suspension obtained in step (3) was continuously stirred at a speed of 100 rpm for 8 hours. After the stirring, it was centrifuged at a speed of 1000 rpm for 10 minutes to collect the manganese phosphate nanoparticles in the suspension. Finally, the nano manganese phosphate was suspended in a PBS buffer solution with a pH of 7.4 for storage or use.
[0095] like Figure 1 As shown, during the preparation process, with the addition of disodium hydrogen phosphate, the pH of the supernatant gradually increased from 4.4 to 7.4. When disodium hydrogen phosphate was not added, the solution was acidic, with a pH of 4.4, and no obvious Tyndall effect was observed. With the addition of disodium hydrogen phosphate, when the pH reached 4.7, an obvious Tyndall effect could be observed in the solution, indicating that particles with a particle size of 1-100 nm were generated.
[0096] Example 2
[0097] (1) Add 136.4 μL of 1.0 mol / L MnCl2·4H2O solution to 12.82 mL of deionized water and stir for 10 minutes until the mixture is uniform;
[0098] (2) Add 136.4 μL of 1.0 mol / L NaH2PO4 solution to the solution obtained in step (1), and stir for 10 minutes until the mixture is uniform;
[0099] (3) quickly adding 545.6 μL of 1.0 mol / L Na2HPO4 solution to the MnCl2 / NaH2PO4 mixed solution obtained in step (2) to obtain a suspension, wherein the final concentrations of MnCl2, NaH2PO4 and Na2HPO4 are 10 mmol / L, 10 mmol / L and 40 mmol / L, respectively, and the final pH value of the supernatant is measured to be 7.3;
[0100] (4) The suspension obtained in step (3) was continuously stirred at a speed of 100 rpm for 8 hours. After the stirring, it was centrifuged at a speed of 1000 rpm for 10 minutes to collect the manganese phosphate nanoparticles in the suspension. Finally, the nano manganese phosphate was suspended in a PBS buffer solution with a pH of 7.4 for storage or use.
[0101] Example 3
[0102] (1) Add 136.4 μL of 1.0 mol / L MnCl2·4H2O solution to 12.14 mL of deionized water and stir for 10 minutes until the mixture is uniform;
[0103] (2) adding 272.8 μL of 1.0 mol / L NaH2PO4 solution to the solution obtained in step (1), and stirring for 10 minutes until the mixture is uniform;
[0104] (3) quickly adding 1091.2 μL of a 1.0 mol / L Na2HPO4 solution to the MnCl2 / NaH2PO4 mixed solution obtained in step (2) to obtain a suspension, wherein the final concentrations of MnCl2, NaH2PO4 and Na2HPO4 are 10 mmol / L, 20 mmol / L and 80 mmol / L, respectively, and the final pH value of the supernatant is measured to be 7.4;
[0105] (4) The suspension obtained in step (3) was continuously stirred at a speed of 100 rpm for 8 hours. After the stirring, it was centrifuged at a speed of 1000 rpm for 10 minutes to collect the manganese phosphate nanoparticles in the suspension. Finally, the nano manganese phosphate was suspended in a PBS buffer solution with a pH of 7.4 for storage or use.
[0106] Comparative Example 1
[0107] (1) Add 100 μL of 1.0 mol / L MnCl2·4H2O solution to 9.9 mL of PBS solution (pH = 7.4) and stir for 10 minutes until the mixture is well mixed;
[0108] (2) The suspension obtained in step (1) is continuously stirred at a speed of 100 rpm for 8 hours. After the stirring is completed, the suspension is centrifuged at a speed of 1000 rpm for 10 minutes. The manganese phosphate particles in the suspension are collected and suspended in a PBS buffer solution with a pH of 7.4 for storage or use.
[0109] Comparative Example 2
[0110] Directly add 100 μL of 1.0 mol / L MnCl2·4H2O solution to 9.9 mL of normal saline, stir for 10 min until well mixed, so that the final concentration of MnCl2 is 10 mmol / L, and store in a 4°C refrigerator.
[0111] Test Case
[0112] Test Example 1 Material Characterization and Composition Identification of Nano-Manganese Phosphate
[0113] The morphology of the manganese phosphate nanoparticles prepared in Example 1 was observed using a scanning electron microscope (SEM) and a transmission electron microscope (TEM), and the particle size of the nanoparticles was statistically analyzed using TEM images. The valence state of the manganese element in the prepared manganese phosphate nanomaterial was analyzed using X-ray electron spectroscopy (XPS), the ratio of manganese element to phosphorus element in the prepared manganese phosphate nanomaterial was analyzed using scanning electron microscope-X-ray energy spectrum (SEM-EDS), and the crystal water contained in the manganese phosphate nanomaterial was determined using thermogravimetric analysis. Figure 2 As shown in FIG. 1 , the manganese phosphate nanomaterials prepared by this method are distributed relatively uniformly, with an average particle diameter of 40 nm; Figure 3 As shown, the XPS analysis results show that the manganese element 2P 3 / 2 and 2P 1 / 2 The binding energies of 653.75eV and 641.25eV are consistent with the characteristics of divalent manganese, and are accompanied by a 2P 1 / 2 Satellite Peak (already in Figure 3 (in the logo); Figure 4 The SEM-EDX analysis results show that the material contains manganese, oxygen, and phosphorus (hydrogen cannot be detected in this experiment), and the molar ratio of manganese to phosphorus is close to 3:2. Figure 5 As shown, the thermogravimetric analysis results also show that the nano manganese phosphate material contains 12.7% of crystalline water. These results indicate that the chemical composition of the nano manganese phosphate material is Mn3(PO4)2·3H2O.
[0114] Test Example 2 Stability and pH sensitivity test of manganese phosphate nanomaterials
[0115] Dynamic light scattering analysis was used to test the stability of manganese phosphate nanomaterials; Figure 6As shown in the figure, compared with the large particles with a diameter of more than 1000 nm formed by directly adding manganese chloride solution to PBS solution (pH=7.4) (Comparative Example 1), the manganese phosphate nanomaterial prepared in Example 1 can form smaller and more uniform nanoparticles. 2+ The large particles formed (Comparative Example 1) quickly aggregated and precipitated within 1 hour, while the nano manganese phosphate material prepared in Example 1 could remain stable in the aqueous solution for at least 3 days without precipitation. In order to evaluate the stability of the nanoparticles, dynamic light scattering analysis was performed on the prepared nano manganese phosphate every 2 weeks. Figure 7 As shown in the figure, the hydrated particle size of the nano manganese phosphate material prepared in Example 2 and Example 3 is still about 120 nm and is evenly distributed. Figure 8 As shown, the nano manganese phosphate material prepared in Example 1 can remain stable for a long time without agglomeration or forming larger particles. In addition, the prepared nano manganese phosphate material still has good stability after being stored at different temperature conditions for 24 hours.
[0116] In order to verify the pH acid sensitivity of the prepared manganese phosphate nanoparticles, the nano manganese phosphate separated by centrifugation in Example 1 was added to phosphate buffer with a pH value of 4.5, 5.5 or 6.5. Fig. 9 As shown in the figure, as the pH decreases, the nanoparticles gradually dissolve, which indicates that the prepared nanomanganese phosphate particles are pH-sensitive, that is, they can be gradually degraded and release Mn under acidic conditions. 2+ .
[0117] Test Example 3 Mouse Immunization Experiment
[0118] The experimental mice of Test Examples 4 to 9 were immunized twice, on the 1st day and the 22nd day, and the injection method was subcutaneous injection. The blood was collected from the mice by tail cutting, and the blood collection time was 21st and 35th days. The blood was centrifuged to separate the serum and stored frozen at -80°C. In Test Example 4, lymphocytes were obtained by aseptically separating the lymph nodes and spleen of mice on the 25th day (three days after the second immunization), and lymphocytes were obtained by aseptically separating the lymph nodes and spleen of mice on the 35th day (fourteen days after the second immunization).
[0119] Table 1: Composition of vaccine preparations in each group in Test Example 3
[0120]
[0121] Test Example 4 Maturation and activation of dendritic cells in lymph nodes and spleen of immunized mice
[0122] The whole process must be carried out in a clean bench to maintain aseptic operation; on the 25th day of immunization (three days after the second immunization), the lymph nodes and spleens of the blank mice and immunized mice were taken, respectively ground through a cell sieve in 5 mL of cold PBS, centrifuged to collect the cells, and 2 mL of red blood cell lysis solution was added. After lysis for 3 minutes, the cells were centrifuged again. After the cells were collected, they were washed with cold PBS and culture medium 1640, respectively, and centrifuged; the cells were collected and resuspended in 2 mL of complete culture medium. In the clean bench, 300 μL of resuspended cell solution was added to a 1.5 mL centrifuge tube, and 300 μL of diluted CD11c, CD80 and CD86 cell staining solution (all purchased from Biolegend) were added to each tube. After mixing, they were placed in ice for staining for 40 minutes; then centrifuged, the supernatant was discarded, and the cells were washed twice with PBS. Finally, the cells were resuspended with 400 μL of PBS solution, and the cells were filtered through a cell sieve and tested on a flow cytometer. Fig.10 As shown, the nano manganese phosphate prepared in Example 1 can effectively promote the maturation and activation of dendritic cells in mice, so as to enhance their uptake and presentation of antigens and thus enhance the immune response. Then, the present invention compares the maturation of dendritic cells in the spleen of mice stimulated by Examples 1-3 and Comparative Examples 1-2 (such as Fig.11 The results show that the manganese phosphate nanomaterials prepared in Examples 1-3 can effectively induce the maturation and activation of dendritic cells in mice, and the effects are better than those of Comparative Examples 1 and 2. This may be because the manganese phosphate particles in Comparative Example 1 are too large to have an immune effect, while the free manganese ions in Comparative Example 2 are easy to diffuse at the injection site and are difficult to have a local immune effect.
[0123] Test Example 5 Determination of Antigen-Specific Antibody Content in Sera of Immunized Mice
[0124] In a 96-well ELISA plate (purchased from Corning), each well was coated with 100 μL of antigen (S1-WT protein or S1-Omicron protein, respectively), and incubated overnight at 4°C for 12 hours; the plate was washed 3 times with PBST (PBS buffer containing 0.05% Tween-20), and then blocked with PBS solution containing 3% bovine serum albumin (BSA), and incubated at 37°C for 1 hour; then the plate was washed 3 times with PBST, serum diluted in a gradient manner with 0.1% BSA in PBS solution was added, and incubated at 37°C for 1 hour; then the plate was washed 3 times with PBST again, and 100 μL of HRP-labeled goat anti-mouse secondary antibody IgM and IgG diluted 4000:1 with PBST solution were added respectively, and incubated at 37°C for 1 hour; then the plate was washed 5 times with PBST, freshly prepared TMB color development solution was added, and incubated in the dark for 5 minutes. After the color appeared, 50 μL of 2M sulfuric acid was added to each well to stop the color development. The absorbance at 450 nm was measured by an ELISA reader and the antibody titer was calculated. Fig.12 and Fig.13As shown, the nano manganese phosphate prepared in Example 1 mainly enhanced the antigen-specific IgG antibody titer and induced a strong humoral immune response.
[0125] Test Example 6 Determination of pseudovirus neutralizing antibody titer in immunized mouse serum
[0126] The sera of immunized mice from different groups were heat-inactivated (56°C water bath, 15-30min), and the treated serum samples were diluted with Opti-MEM according to different concentration gradients, and added to the 96-well plate after being blown evenly with a pipette. The pseudovirus was then taken out from -80°C and re-thawed at 4°C. The re-thawed pseudovirus was diluted with Opti-MEM (0.15μL pseudovirus / 25μL diluent) and added to the above 96-well plate, and incubated with the serum sample at room temperature for 1h. During the co-incubation period, ACE2-HEK293T cells were prepared, ACE2-HEK293T cells were counted, and the cell concentration was adjusted to 400,000 cells / mL with complete culture medium (without double antibody), and placed in a cell culture incubator for use. After the serum sample and pseudovirus co-incubation is completed, take out the prepared ACE2-HEK293T cells, blow evenly, add 50μL of cell suspension to each well, seal the edges with PBS, and then place the 96-well plate in a cell culture incubator for culture; after 24 hours, add 50μL of complete culture medium to each well and continue to culture for 24 hours. After the culture is completed, carefully remove the culture medium in the wells, wash once with PBS, add 100μL of cell lysis solution to each well, oscillate at room temperature for 15 minutes, and then add 80μL of luciferase detection agent, protect from light, mix well and measure the chemiluminescence value. Fig.14 As shown, the nano manganese phosphate prepared in Example 1 induced higher titers of neutralizing antibodies, and the induced neutralizing antibodies could cross-neutralize multiple mutants of the new coronavirus.
[0127] Test Example 7 Determination of the number of antigen-specific IFN-γ secreting cells in spleen cells of immunized mice
[0128] The whole process must be performed in a clean bench with sterile operation; spleens of blank mice and immunized mice were taken, ground in 5 mL of cold PBS through a cell sieve, centrifuged to collect cells, 2 mL of red blood cell lysis buffer was added, lysed for 3 minutes and centrifuged again, and the cells were collected and washed with cold PBS and culture medium 1640, respectively, and centrifuged; cells were collected and resuspended in 3 mL of complete culture medium. The steps of the ELISPOT kit instructions (Dakoway Company, Cat. No. 2210005) were followed: the ELISPOT plate pre-coated with capture antibody was activated with 200 μL of serum-free culture medium for 10 minutes in a clean bench, the culture medium was poured out, and 100 μL of the corresponding group of cell suspension (10 6cells / well), and stimulated by adding 2 μg of S1-WT or 2 μg of S1-Omicron, respectively, and incubated in a cell culture incubator for 24 h (movement or shaking is strictly prohibited during incubation). After the incubation, pour out the liquid, add 200 μL of cold deionized water, and place at 4°C for 10 minutes to lyse the cells; shake out the liquid, wash 6 times with the Washing Buffer provided in the kit, tap dry, add 100 μL of diluted biotin-labeled antibody, and incubate at 37°C for 1 hour; shake out the liquid, wash 6 times with Washing Buffer, tap dry, add 100 μL of diluted HRP-labeled avidin, and incubate at 37°C for 1 hour; shake out the liquid, wash 5 times with Washing Buffer, wash 2 times with deionized water, and tap dry; add 100 μL of freshly prepared AEC color development solution to each well, and incubate at 25°C for 20 minutes; shake out the liquid, wash 5 times with deionized water, stop color development, place the ELISPOT plate in a cool place to dry naturally, and use an ELISPOT analyzer for counting. Fig.15 As shown, the spleen cells of mice using the nano manganese phosphate prepared in Example 1 as an adjuvant showed more IFN-γ spots, indicating that nano manganese phosphate induced a stronger antigen-specific cellular immune response.
[0129] Test Example 8 Determination of Antigen-Specific CD4+ and CD8+ T Cell Levels in Spleen of Immunized Mice
[0130] The whole process must be carried out in a clean bench with sterile operation. The spleens of blank mice and immunized mice were taken, ground into 5 mL of cold PBS through a cell sieve, and the cells were collected by centrifugation. 2 mL of red blood cell lysis buffer was added, and the cells were lysed for 3 minutes and then centrifuged again. After the cells were collected, they were washed with cold PBS and culture medium 1640, respectively, and centrifuged. The cells were collected and 3 mL of complete culture medium was added to resuspend the cells. In the clean bench, the resuspended cell solution was added to a 24-well plate (400 μL complete medium and 200 μL cell suspension per well), and 2 μg of S1-WT or 2 μg of S1-Omicron was added for stimulation, and the plate was placed in a cell culture incubator for incubation; after 6 hours, 4 μL of protein transport inhibitors (2 μL monensin and 2 μL brefeldin A) were added to each well, and the plate was placed in a cell culture incubator for incubation for 12 hours; the cell solution was transferred to a 2mL EP tube, centrifuged, and the supernatant was discarded; the cells were washed with Stain Buffer (1% BSA, 1% FBS, 0.1% NaN3, PBS), centrifuged, and the supernatant was discarded; 500 μL of diluted CD3+, CD4+ and CD8+ cell staining solution was added to each tube, mixed well, and placed on ice for staining for 30 minutes; centrifuged, the supernatant was discarded, and the plate was washed twice with Stain Buffer; 250 μL of fixation and membrane permeabilization solution was added to each tube, fixed at 4°C for 10 minutes, and the supernatant was discarded. Wash twice with Buffer; add 250 μL of diluted IFN-γ and TNF-α cytokine staining solution to each tube, mix well and place at 4℃ in the dark for 30 minutes; centrifuge, discard the supernatant, wash twice with Washing Buffer, resuspend the cells with 400 μL 0.1% BSA PBS solution, filter the cells and use flow cytometer for testing. Fig.16 As shown, the spleen cells of mice using the nano manganese phosphate prepared in Example 1 as an adjuvant secreted more IFN-γ and TNF-α cytokines, indicating that nano manganese phosphate induced a stronger antigen-specific cellular immune response.
[0131] Test Example 9 Blood biochemical analysis of immunized mice and pathological section staining of important organs
[0132] On the 35th day after immunization, the blank mice and the immunized mice were euthanized, and the serum was collected for blood biochemical analysis to detect the levels of alanine aminotransferase (ALT), aspartate aminotransferase (AST), alkaline phosphatase (ALP) and urea (UREA) in the mouse serum. The heart, liver, spleen, lung, kidney and brain of the mice were fixed in 4% paraformaldehyde for 72 hours, then embedded in paraffin, sectioned, stained with hematoxylin and eosin, and images were taken with a Nikon Eclipse E100 microscope. Fig.17 and 18As shown, in the serum of mice immunized with nano manganese phosphate prepared in Example 1, aspartate alanine aminotransferase, aspartate aminotransferase, alkaline phosphatase and blood urea levels were the same as those in the PBS control group, without significant differences. In addition, compared with the PBS control group, the major organs such as the heart, liver, spleen, lung, kidney, brain of mice immunized with nano manganese phosphate had no obvious pathological changes. These results confirm that the nano manganese phosphate prepared does not cause obvious inflammation and organ damage in mice, indicating that it is a kind of adjuvant with good biocompatibility and biosafety.
[0133] The preferred embodiments of the present invention are described in detail above, but the present invention is not limited thereto. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications, including the combination of various technical features in any other suitable manner, and these simple modifications and combinations should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.
Claims
1. A method for preparing a manganese phosphate nanomaterial, characterized in that: The method includes: (1) Add dihydrogen phosphate solution to divalent manganese salt solution and stir; (2) adding a monohydrogen phosphate solution to the mixed solution obtained in step (1); (3) stirring the suspension obtained in step (2), and then centrifuging to obtain manganese phosphate nanomaterials; The molar ratio of the manganese element in the divalent manganese salt, the dihydrogen phosphate and the monohydrogen phosphate is 1:1-2:4-8.
2. The method according to claim 1, characterized in that In step (1), the divalent manganese salt is selected from one or two of manganese chloride, manganese nitrate, manganese acetate, manganese sulfate and manganese oxalate, and crystalline hydrates thereof.
3. The method according to claim 1, characterized in that The divalent manganese salt is manganese chloride tetrahydrate.
4. The method according to claim 1, characterized in that: The concentration of the divalent manganese salt is 0.1-10 mol / L.
5. The method according to any one of claims 1 to 4, characterized in that: In step (1), the dihydrogen phosphate is selected from one or more of sodium dihydrogen phosphate, potassium dihydrogen phosphate, ammonium dihydrogen phosphate, aluminum dihydrogen phosphate and calcium dihydrogen phosphate, and their crystalline hydrates.
6. The method according to claim 1, characterized in that In step (1), the concentration of the dihydrogen phosphate solution is 0.1-10 mol / L.
7. The method according to any one of claims 1 to 4, characterized in that: In step (2), the monohydrogen phosphate is selected from one or more of disodium hydrogen phosphate, dipotassium hydrogen phosphate, diammonium hydrogen phosphate and calcium hydrogen phosphate, and their crystalline hydrates.
8. The method according to claim 1, characterized in that In step (2), the concentration of the monohydrogen phosphate solution is 0.1-10 mol / L.
9. The method according to any one of claims 1 to 4, characterized in that: In step (1), the stirring time is 5 minutes to 200 hours.
10. The method according to claim 9, characterized in that In step (1), the stirring time is 10 to 60 minutes.
11. The method according to claim 1, characterized in that: In step (3), the stirring conditions include: stirring temperature of 10-37° C., stirring time of 1-20 hours, and stirring rate of 100-1000 r / min.
12. The method according to any one of claims 1 to 4, characterized in that: In step (3), the centrifugal conditions include: a centrifugal rate of 50 to 5000 rpm; and a centrifugal time of 5 to 60 minutes.
13. The method according to claim 12, characterized in that In step (3), the centrifugal speed is 1000-3000 rpm.
14. The method according to claim 12, characterized in that In step (3), the centrifugation time is 10 to 30 minutes.
Citation Information
Patent Citations
Application of divalent manganese in preparation of immunopotentiation drugs or antitumor drugs
CN112691120A