Preparation method of composite material for hyperbaric oxygen chamber

By combining the PU adhesive with a low boiling point solvent system with a high-modulus polyester clamp, a high-strength and high-tear TPU/cloth/TPU structure is formed, which solves the problem of the heavy weight of the traditional high-pressure oxygen chamber body. The high cost problem has achieved efficient and lightweight high-pressure oxygen chamber products.

CN118927655APending Publication Date: 2024-11-12FUJIAN AMITY NEW MATERIAL CO LTD
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202410837609.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-26
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The traditional hyperbaric oxygen chamber material is large in weight, large in size, high in manufacturing and high in maintenance, and cannot meet the needs of lightweight and efficient treatment.

Method used

The PU adhesive with a low boiling point solvent system is combined with a high-modulus polyester mesh, and is bonded with the TPU film through the casting process to form a composite material of TPU/cloth/TPU structure, which improves the stretching and tearing of the mesh. Strength and reduce elongation.

Benefits of technology

It realizes high strength, high tear and low elongation composite materials, meets the product needs of high-pressure oxygen chambers, and reduces the elongation and production costs of materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004913599710000011
    Figure BDA0004913599710000011
Patent Text Reader

Abstract

The invention discloses a preparation method of a composite material for a hyperbaric oxygen chamber. The method comprises the following steps: 1) uniformly mixing 100 parts of PU resin, 4-8 parts of a bridging agent and 4-6 parts of a diluent to obtain a PU adhesive, the diluent being a mixture of butanone and ethyl acetate in a weight ratio of 6: 4; 2) mixing 100 parts of TPU, 2-8 parts of color master batch and 2-8 parts of anti-UV agent to obtain a TPU casting mixture; (3) respectively coating the PU adhesive on the upper surface and the lower surface of the high-modulus polyester sandwich net to obtain a polyester sandwich net A with primer coating on both sides; 4) drying the polyester sandwich net A to obtain a polyester sandwich net B; 5) pre-drying the polyester sandwich net B to obtain a polyester sandwich net C; 6) attaching the TPU casting mixture to the upper surface of a polyester sandwich mesh C through a casting process, and 7) attaching the TPU casting mixture to the lower surface of the polyester sandwich mesh C through the casting process to form the composite material with a TPU / cloth / TPU structure for the hyperbaric oxygen chamber. The composite material for the hyperbaric oxygen chamber has high tensile strength, high tearing strength and low elongation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of composite materials, and in particular to a method for preparing a composite material for a hyperbaric oxygen chamber. Background Art

[0002] As people pay more attention to their health, hyperbaric oxygen chambers have begun to be promoted and applied to provide people with more comprehensive health care effects. Hyperbaric oxygen chambers can provide a high-concentration oxygen environment. By inhaling high-concentration oxygen, the blood oxygen content can be increased, the metabolism of body cells can be promoted, and the energy generation and utilization efficiency can be improved.

[0003] Hyperbaric oxygen chambers are of great significance for improving body functions, enhancing immunity and restoring health. They can help people improve sleep quality, relieve sleep problems and provide a better resting environment. At the same time, hyperbaric oxygen chambers can also reduce fatigue and relieve stress, and help people restore energy and vitality by relaxing the body and mind and relieving stress. In addition, hyperbaric oxygen chambers can also help promote wound healing. Inhalation of high-concentration oxygen can increase the oxygen content in the blood, improve the oxygen supply level of the wound, and accelerate the wound healing process. It can also promote the growth and repair of red blood cells and accelerate the tissue repair and regeneration process.

[0004] Traditional hyperbaric oxygen chambers use steel or aluminum to manufacture sealed cabins, and provide high-concentration oxygen therapy by increasing the air pressure in the cabin. However, these cabins are made of steel, aluminum, alloys and other materials, so they have disadvantages such as heavy weight, large volume, high manufacturing cost and high maintenance cost. In order to solve these defects, new TPU composite hyperbaric oxygen chambers have begun to be promoted in the market. TPU composite hyperbaric oxygen chambers use thermoplastic polyurethane (TPU) composite materials to manufacture sealed cabins, and also provide high-concentration oxygen therapy by increasing the air pressure in the cabin. This new material cabin has the advantages of light weight, small volume, low manufacturing cost and low maintenance cost. TPU composite hyperbaric oxygen chamber project requirements:

[0005] Summary of the invention

[0006] The object of the present invention is to provide a method for preparing a composite material for a hyperbaric oxygen chamber. The hyperbaric oxygen chamber prepared by the material has the advantages of high strength, high tear resistance and small product deformation.

[0007] A method for preparing a composite material for a hyperbaric oxygen chamber comprises the following steps:

[0008] 1) Preparation of PU adhesive

[0009] Mix 100 parts of PU resin, 4-8 parts of bridging agent and 4-6 parts of diluent evenly, and control the viscosity to 80,000-100,000 cps to obtain PU adhesive;

[0010] The solvent system used by the PU resin is a low-boiling point solvent system, the bridging agent is a mixture of TDI and MDI, and the diluent is a mixture of butanone and ethyl acetate in a weight ratio of 6:4;

[0011] 2) Preparation of TPU casting mixture

[0012] 100 parts of TPU, 2-8 parts of masterbatch and 2-8 parts of anti-UV agent are mixed to obtain a TPU casting mixture, wherein the anti-UV agent is composed of TPU, anti-UV powder and dispersant in a weight ratio of 100:25:5;

[0013] 3) The PU adhesive is applied to both sides of the high modulus polyester sandwich mesh to obtain a polyester sandwich mesh A with primer on both sides;

[0014] 4) Drying the polyester web A at a temperature of 80-120° C., a drying time of 1-3 min, and a drying speed of 10-15 m / min to obtain a polyester web B; this step can solidify the PU adhesive and improve the activation state of the primer;

[0015] 5) Pre-baking the polyester sandwich B at a temperature of 100-120° C. for 5-10 seconds to obtain a polyester sandwich C. The purpose of this step is to further improve the activation state of the primer to increase the subsequent bonding strength with the TPU film;

[0016] 6) bonding the TPU casting mixture to the upper surface of the polyester sandwich net C through a casting process;

[0017] 7) The TPU casting mixture is bonded to the lower surface of the polyester sandwich C through a casting process to form a composite material for a hyperbaric oxygen chamber with a TPU / cloth / TPU structure.

[0018] Furthermore, before casting, the TPU casting mixture is dried to a moisture content of less than 0.02%.

[0019] Furthermore, the casting temperature is 185-200° C., the casting speed is 5-10 m / min, the casting pressure is 10 MPa, and the laminating pressure is 30-60 kg.

[0020] The beneficial effects of the present invention are:

[0021] 1. Composite materials have high tensile and tear strength and low elongation.

[0022] Due to the influence of gram weight, only mesh cloth of 3000D and below can be used to make hyperbaric oxygen chambers. However, conventional processes can only make the tear strength of the mesh cloth about 300N, and the tensile strength can only reach less than 4000N. This obviously cannot meet the product demand of hyperbaric oxygen chambers. In order to solve this problem, it is necessary to improve the tensile and tear strength of the mesh cloth and reduce the elongation of the material by changing the base cloth, formula, and process. Therefore, the present invention selects high modulus, low elongation fiber materials to replace conventional fiber materials, such as using high modulus polyester fibers, which have higher strength and low elongation, and can improve the tear strength of the mesh cloth.

[0023] 2. The solvents in the traditional glue system are DMF solvent and toluene solvent. The solvent system of the PU adhesive of the present invention is a mixture of butanone and ethyl acetate in a weight ratio of 6:4. By adjusting the solvent in the glue, compared with the traditional process, the bridging agent in the PU adhesive formula can be reduced from 10-15 parts to 4-8 parts, the viscosity can be adjusted from 20,000-30,000 cps to 80,000-100,000 cps, the production process temperature of the coating can be reduced from 150°C to 80-120°C, and the casting machine needs to fully preheat the paste cloth before entering the cast film production. The preheating temperature is increased from 60-70°C of the traditional technology to 100-120°C.

[0024] 3. The hyperbaric oxygen chamber made of the composite material of the present invention has the advantages of high strength, high tearing and small product deformation. DETAILED DESCRIPTION

[0025] Example 1

[0026] A method for preparing a composite material for a hyperbaric oxygen chamber comprises the following steps:

[0027] 1) Preparation of PU adhesive

[0028] 100 parts of PU resin, 6 parts of bridging agent and 5 parts of diluent were mixed evenly, and the viscosity was controlled to be 90,000 cps to obtain PU adhesive;

[0029] The solvent system used by the PU resin is a low-boiling point solvent system, the bridging agent is a mixture of TDI and MDI, and the diluent is a mixture of butanone and ethyl acetate in a weight ratio of 6:4;

[0030] 2) Preparation of TPU casting mixture

[0031] 100 parts of TPU, 5 parts of masterbatch and 5 parts of anti-UV agent are mixed to obtain a TPU casting mixture, wherein the anti-UV agent is composed of TPU, anti-UV powder and dispersant in a weight ratio of 100:25:5;

[0032] 3) The PU adhesive is applied to both sides of the high modulus polyester sandwich mesh to obtain a polyester sandwich mesh A with primer on both sides;

[0033] 4) Drying the polyester web A at a drying temperature of 100° C., a drying time of 2 min, and a drying speed of 12.5 m / min to obtain a polyester web B; this step can solidify the PU adhesive and improve the activation state of the primer;

[0034] 5) Pre-baking the polyester sandwich B at a temperature of 110° C. for 8 seconds to obtain a polyester sandwich C. The purpose of this step is to further improve the activation state of the primer to increase the subsequent bonding strength with the TPU film;

[0035] 6) drying the TPU casting mixture until the moisture content is less than 0.02%, and then laminating the TPU casting mixture to the upper surface of the polyester sandwich C through a casting process;

[0036] 7) The TPU casting mixture is bonded to the lower surface of the polyester sandwich C through a casting process to form a composite material for a hyperbaric oxygen chamber with a TPU / cloth / TPU structure;

[0037] In the above casting process, the casting temperature is 190° C., the casting speed is 7.5 m / min, the casting pressure is 10 MPa, and the laminating pressure is 45 kg.

[0038] Example 2

[0039] A method for preparing a composite material for a hyperbaric oxygen chamber comprises the following steps:

[0040] 1) Preparation of PU adhesive

[0041] 100 parts of PU resin, 4 parts of bridging agent and 4 parts of diluent were mixed evenly, and the viscosity was controlled to be 82,000 cps to obtain PU adhesive;

[0042] The solvent system used by the PU resin is a low-boiling point solvent system, the bridging agent is a mixture of TDI and MDI, and the diluent is a mixture of butanone and ethyl acetate in a weight ratio of 6:4;

[0043] 2) Preparation of TPU casting mixture

[0044] 100 parts of TPU, 2 parts of masterbatch and 2 parts of anti-UV agent are mixed to obtain a TPU casting mixture, wherein the anti-UV agent is composed of TPU, anti-UV powder and dispersant in a weight ratio of 100:25:5;

[0045] 3) The PU adhesive is applied to both sides of the high modulus polyester sandwich mesh to obtain a polyester sandwich mesh A with primer on both sides;

[0046] 4) Drying the polyester web A at a temperature of 80° C., a drying time of 3 min, and a drying speed of 10 m / min to obtain a polyester web B; this step can solidify the PU adhesive and improve the activation state of the primer;

[0047] 5) Pre-baking the polyester sandwich B at a temperature of 100° C. for 10 seconds to obtain a polyester sandwich C. The purpose of this step is to further improve the activation state of the primer to increase the subsequent bonding strength with the TPU film;

[0048] 6) drying the TPU casting mixture until the moisture content is less than 0.02%, and then laminating the TPU casting mixture to the upper surface of the polyester sandwich C through a casting process;

[0049] 7) The TPU casting mixture is bonded to the lower surface of the polyester sandwich C through a casting process to form a composite material for a hyperbaric oxygen chamber with a TPU / cloth / TPU structure;

[0050] In the above casting process, the casting temperature is 185° C., the casting speed is 10 m / min, the casting pressure is 10 MPa, and the laminating pressure is 30 kg.

[0051] Example 3

[0052] A method for preparing a composite material for a hyperbaric oxygen chamber comprises the following steps:

[0053] 1) Preparation of PU adhesive

[0054] 100 parts of PU resin, 8 parts of bridging agent and 6 parts of diluent were mixed evenly, and the viscosity was controlled to be 100,000 cps to obtain PU adhesive;

[0055] The solvent system used by the PU resin is a low-boiling point solvent system, the bridging agent is a mixture of TDI and MDI, and the diluent is a mixture of butanone and ethyl acetate in a weight ratio of 6:4;

[0056] 2) Preparation of TPU casting mixture

[0057] 100 parts of TPU, 8 parts of masterbatch and 8 parts of anti-UV agent are mixed to obtain a TPU casting mixture, wherein the anti-UV agent is composed of TPU, anti-UV powder and dispersant in a weight ratio of 100:25:5;

[0058] 3) The PU adhesive is applied to both sides of the high modulus polyester sandwich mesh to obtain a polyester sandwich mesh A with primer on both sides;

[0059] 4) Drying the polyester web A at a drying temperature of 120° C., a drying time of 1 min, and a drying speed of 15 m / min to obtain a polyester web B; this step can solidify the PU adhesive and improve the activation state of the primer;

[0060] 5) Pre-baking the polyester sandwich B at a temperature of 120° C. for 5 seconds to obtain a polyester sandwich C. The purpose of this step is to further improve the activation state of the primer to increase the subsequent bonding strength with the TPU film;

[0061] 6) drying the TPU casting mixture until the moisture content is less than 0.02%, and then laminating the TPU casting mixture to the upper surface of the polyester sandwich C through a casting process;

[0062] 7) The TPU casting mixture is bonded to the lower surface of the polyester sandwich C through a casting process to form a composite material for a hyperbaric oxygen chamber with a TPU / cloth / TPU structure;

[0063] In the above casting process, the casting temperature is 200° C., the casting speed is 5 m / min, the casting pressure is 10 MPa, and the laminating pressure is 60 kg.

Claims

1. A method for preparing a composite material for a hyperbaric oxygen chamber, characterized in that: The following steps are involved: 1) Preparation of PU adhesive 100 parts of PU resin, 4-8 parts of bridging agent and 4-6 parts of diluent are mixed evenly, and the viscosity is controlled to be 80,000-100,000 cps to obtain PU adhesive; the diluent is a mixture of butanone and ethyl acetate in a weight ratio of 6:4; 2) Preparation of TPU casting mixture 100 parts of TPU, 2-8 parts of masterbatch and 2-8 parts of anti-UV agent are mixed to obtain a TPU casting mixture, wherein the anti-UV agent is composed of TPU, anti-UV powder and dispersant in a weight ratio of 100:25:5; 3) The PU adhesive is applied to the upper and lower surfaces of the high modulus polyester mesh to obtain a polyester mesh A with primer on both sides; 4) Drying the polyester web A at a temperature of 80-120°C, a drying time of 1-3 min, and a drying speed of 10-15 m / min to obtain a polyester web B; 5) Pre-drying the polyester sandwich B at a temperature of 100-120°C for 5-10 seconds to obtain a polyester sandwich C; 6) The TPU casting mixture is bonded to the upper surface of the polyester sandwich C through a casting process; 7) The TPU casting mixture is bonded to the lower surface of the polyester sandwich C through a casting process to form a composite material for a hyperbaric oxygen chamber with a TPU / cloth / TPU structure.

2. The method for preparing a composite material for a hyperbaric oxygen chamber according to claim 1, characterized in that: In step 1), the bridging agent is a mixture of TDI and MDI.

3. The method for preparing a composite material for a hyperbaric oxygen chamber according to claim 1, characterized in that: In steps 6) and 7), before casting, the TPU casting mixture is dried to a moisture content of less than 0.02%.

4. The method for preparing a composite material for a hyperbaric oxygen chamber according to claim 1, characterized in that: In steps 6) and 7), the casting temperature is 185-200°C, the casting speed is 5-10m / min, the casting pressure is 10mpa, and the laminating pressure is 30-60kg.

Citation Information

Cited By

  • High-tear material and preparation method thereof

    CN118186787A

  • A high tear material and a method for making the same

    CN118186787B