Negative electrode for zinc battery, and zinc battery

By designing a current collector with specific pore structure and material on the negative electrode of the zinc battery, the problem of shortening zinc battery life caused by dendrite growth is solved, and a more uniform reaction and extended battery life is achieved.

CN118974976APending Publication Date: 2024-11-15ANNEGIS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380030615.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-04-07
Filing Date
2023-02-10
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The zinc precipitation on the negative electrode of the zinc battery produces dendrites, resulting in a fast growth rate of dendrites, shortening the life of the zinc battery.

Method used

A negative electrode for zinc batteries is designed. The current collector has a plurality of holes penetrated along the thickness direction. The inner surface area and inner diameter of the hole are within a specific range. The pore opening rate of the current collector is high, including conductive substrates and plating. The tin film and the negative electrode material layer contain zinc components, and these structures slow down the growth of dendrites.

Benefits of technology

It effectively extends the life of the zinc battery, improves the fluidity of the electrolyte and the uniformity of the reaction, slows down the growth of dendrites, and significantly improves the cycle life of the zinc battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118974976A_ABST
    Figure CN118974976A_ABST
Patent Text Reader

Abstract

A negative electrode (1) for a zinc cell according to the present invention is provided with a current collector (2) and a negative electrode material layer (3) fixed to the current collector (2). The current collector (2) has a plurality of holes (6) that penetrate in the thickness direction and are filled with the negative electrode material layer (3). The inner surface area of each of the plurality of holes (6) in a cross-section perpendicular to the thickness direction is greater than 0.5 mm2 and less than 19.6 mm2.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field The invention relates to a negative electrode for a zinc battery and a zinc battery. Background Art As zinc batteries, nickel-zinc batteries, zinc-air batteries, silver-zinc batteries, etc. are known. For example, it is known that nickel-zinc batteries are aqueous batteries that use aqueous electrolytes such as potassium hydroxide aqueous solution, and therefore have high safety, and through the combination of zinc electrodes and nickel electrodes, have high electromotive force as aqueous batteries. In addition, nickel-zinc batteries not only have excellent input / output performance, but also have low costs, so the application possibilities of industrial uses (such as backup power supplies) and automotive uses (such as hybrid vehicles, etc.) are being studied. Patent document 1 discloses a technology related to nickel-zinc batteries. Previous technical literature Patent Literature Patent Document 1: Japanese Patent Application Laid-Open No. 58-126665 Summary of the invention Technical issues to be solved by the invention For example, as described in Patent Document 1, dendrites are generated on the negative electrode of a zinc battery due to the precipitation of zinc. During the repeated use of the zinc battery, the dendrites will grow significantly and will sooner or later cause a short circuit between the negative electrode and the positive electrode. Therefore, the faster the growth rate of the dendrites, the shorter the life of the zinc battery becomes. One aspect of the present invention is to provide a negative electrode for a zinc battery and a zinc battery that can slow down the growth rate of the dendrites to extend the life of the zinc battery. Means for solving technical problems

[0001] The negative electrode for zinc battery according to one aspect of the present invention comprises a current collector and a negative electrode material layer fixed to the current collector. The current collector has a plurality of holes penetrating in the thickness direction and filled with the negative electrode material layer. The plurality of holes include an inner surface area greater than 0.5 mm2 on a cross section perpendicular to the thickness direction. 2 And less than 19.6mm 2 hole.

[0002] In the zinc battery negative electrode of the above-mentioned [1], each of the plurality of holes has a circular cross-sectional shape, and the plurality of holes may include holes having an inner diameter in the cross section greater than 0.8 mm and less than 5 mm.

[0003] In the zinc battery negative electrode of [1] or [2] above, the open porosity of the current collector may be 35% or more.

[0004] In the zinc battery negative electrode according to any one of [1] to [3] above, the current collector may include a conductive substrate and a tin-plated film covering at least a portion of a surface of the substrate.

[0005] At this time, the base material may mainly include carbon steel.

[0006] In the zinc battery negative electrode according to any one of [1] to [5] above, the negative electrode material layer may contain a zinc-containing component and a binder.

[0007] A zinc battery according to one aspect of the present invention includes any one of the zinc battery negative electrode described in [1] to [6] above and a positive electrode. Effects of the Invention According to one aspect of the present invention, a negative electrode for a zinc battery and a zinc battery can be provided, which can slow down the growth rate of dendrites to extend the life of the zinc battery. BRIEF DESCRIPTION OF THE DRAWINGS Figure 1 It is a front view showing a negative electrode for zinc batteries according to one embodiment. Figure 2 is along Figure 1 Cross-sectional view taken along line II-II. Figure 3 Parts (a) to (c) are front views showing a negative electrode for a zinc battery according to a modification. Figure 4 This is a diagram schematically showing the structure of a nickel-zinc battery. DETAILED DESCRIPTION In the numerical range recorded in stages in this specification, the upper limit or lower limit of the numerical range of a certain stage can be arbitrarily combined with the upper limit or lower limit of the numerical range of other stages. In the numerical range recorded in this specification, the upper limit or lower limit of its numerical range can be replaced by the value shown in the embodiment. Unless otherwise specified, the material exemplified in this specification can be used alone or in combination with more than two kinds. In this specification, the words such as "film" or "layer" not only include the structure of the shape formed on the entire surface when observed as a top view, but also include the structure of the shape formed on a part. The following describes the embodiments of the present invention in detail. However, the present invention is not limited to the following embodiments, and can be implemented in various ways within the scope of the main purpose. The sizes of the structural elements in each figure are conceptual, and the relative relationship between the structural elements in terms of size is not limited to that shown in each figure. Figure 1 It is a front view showing the negative electrode 1 for zinc batteries according to the present embodiment. Figure 2 is along Figure 1 The cross-sectional view taken along the II-II line. Figure 1 and Figure 2 As shown, the zinc battery negative electrode 1 includes a current collector (negative electrode current collector) 2 and a negative electrode material layer 3. The current collector 2 forms a conductive path for current from the negative electrode material layer 3. The current collector 2 is composed of a substrate 4 and a tin-plated film 5. The substrate 4 is made of a conductive material, mainly copper or carbon steel. In one example, the substrate 4 is made of only copper or only carbon steel. The substrate 4 has a shape such as a flat plate. The substrate 4 can be a punched metal plate made of carbon steel. Carbon steel has conductivity and alkali resistance, and is also stable at the reaction potential of the negative electrode. The substrate 4 can be, for example, a cold-rolled steel plate or a part processed on a cold-rolled steel plate. Processing includes, for example, bending, stamping and / or drawing. The thickness of the substrate 4 can be, for example, greater than 0.01 mm, or less than 0.5 mm. The shape of the substrate 4 observed from the front can be, for example, various shapes such as a rectangle and a square. The area of ​​the substrate 4 observed from the front can be, for example, 2000 mm 2 Above, can also be 20000mm 2 the following. The tin-plated film (tin film) 5 covers the entire or a portion of the surface of the substrate 4. When at least a portion of the substrate 4 is covered with the tin-plated film 5, oxidation of the substrate 4 can be suppressed. In the negative electrode, as a side reaction, a decomposition reaction of the electrolyte is performed to generate hydrogen, but when at least a portion of the substrate 4 is covered with the tin-plated film 5, the progress of such a side reaction can be suppressed. The film thickness of the tin-plated film 5 can be, for example, greater than 0.1 μm or less than 5 μm. When the surface of the substrate 4 is composed of copper, the collector 2 may not have the tin-plated film 5. The current collector 2 has a plurality of holes 6 that penetrate the current collector 2 in the thickness direction. The plurality of holes 6 are dispersedly arranged in a two-dimensional shape according to a certain rule in a plane perpendicular to the thickness direction of the current collector 2. In one example, the plurality of holes 6 are arranged so that their centers of gravity coincide with the grid points of a square lattice or an equilateral triangle lattice. When a tin-plated film 5 is provided on the surface of the substrate 4, the tin-plated film 5 is also formed on the inner side of each of the plurality of holes 6. In the following description, when a tin-plated film 5 is provided on the surface of the substrate 4, the inner surface area and inner diameter of each of the plurality of holes 6 are specified as follows. That is, the inner surface area of ​​each of the plurality of holes 6 refers to the inner surface area of ​​each of the plurality of holes 6 specified by the surface of the tin-plated film 5 formed on the inner side of the hole 6. The inner diameter of each of the plurality of holes 6 refers to the inner diameter of each of the plurality of holes 6 specified by the surface of the tin-plated film 5 formed on the inner side of the hole 6. When a tin-plated film 5 is not provided on the surface of the substrate 4, the inner surface area and inner diameter of each of the plurality of holes 6 are specified as follows. That is, the inner surface area of ​​each of the plurality of holes 6 refers to the inner surface area of ​​each of the plurality of holes 6 defined by the surface of the substrate 4 inside the hole 6. The inner diameter of each of the plurality of holes 6 refers to the inner diameter of each of the plurality of holes 6 defined by the surface of the substrate 4 formed inside the hole 6. When the shape of the cross section of each of the plurality of holes 6 perpendicular to the thickness direction of the current collector 2 (in other words, the cross section parallel to the surface of the current collector 2) is a circle with an inner diameter R [mm], the inner surface area of ​​each of the plurality of holes 6 on the cross section perpendicular to the thickness direction of the current collector 2 is π (R / 2) 2 [mm 2] is calculated. When the inner surface area of ​​the hole 6 varies depending on the position in the thickness direction of the cross section perpendicular to the thickness direction of the collector 2, the inner surface area of ​​the hole 6 is defined by the smallest inner surface area. When the inner diameter of the hole 6 varies depending on the position in the thickness direction of the cross section perpendicular to the thickness direction of the collector 2, the inner diameter of the hole 6 is defined by the smallest inner diameter. In this embodiment, the plurality of holes 6 include at least one hole with an inner surface area greater than 0.5 mm 2 And less than 19.6mm 2 In other words, the plurality of holes 6 include at least one hole 6 having an inner diameter R greater than 0.8 mm and less than 5 mm. More preferably, the plurality of holes 6 include at least one hole 6 having an inner surface area of ​​1.7 mm. 2 Above and 7.0mm 2 In other words, the plurality of holes 6 include at least one hole 6 having an inner diameter R of 1.5 mm or more and 3 mm or less. More preferably, the plurality of holes 6 include at least one hole 6 having an inner surface area of ​​1.7 mm or less. 2 Above and 3.1mm 2 In other words, the plurality of holes 6 include one or more holes 6 having an inner diameter R of 1.5 mm or more and 2 mm or less. Two or more holes 6 among the plurality of holes 6 may satisfy any one of these numerical ranges, or all of the plurality of holes 6 may satisfy any one of these numerical ranges. The average value of all holes 6 may satisfy any one of these numerical ranges. The main holes 6 among the plurality of holes 6 may satisfy any one of these numerical ranges. The main holes 6 refer to, for example, two or more holes 6 of uniform size that account for a total of 80% or more of the open porosity of the collector 2. The porosity of the current collector 2 is defined as the ratio (B / A) of the area A defined by the outer edge of the portion of the current collector 2 covered by the negative electrode material layer 3 to the sum of the inner surface areas B of the plurality of holes 6. The porosity of the current collector 2 is, for example, 35% or more, preferably 40% or more, more preferably 45% or more, and further preferably 50% or more. The porosity of the current collector 2 is, for example, 70% or less. The shape of the cross section of each of the plurality of holes 6 that is perpendicular to the thickness direction of the current collector 2 is not limited to a circle. Figure 3Parts (a) to (c) in the figure respectively show the cases where the shape of the hole 6 in the cross section perpendicular to the thickness direction is a quadrilateral, an ellipse and a polygon. When the shape of the hole 6 is a quadrilateral, the quadrilateral includes a square, a rectangle, a parallelogram, a trapezoid and a rounded quadrilateral. When the shape of the hole 6 is a rectangle, the direction of its long side may be aligned between the multiple holes 6 or not. When the direction of the long side of the rectangle is aligned between the multiple holes 6, the direction of its long side may be along the vertical direction when the zinc battery is set, or along the horizontal direction. The shape of the hole 6 is not limited to an ellipse, and may be, for example, an oblong. The long axis direction of the ellipse or oblong may be aligned between the multiple holes 6 or not. When the long axis direction of the ellipse or oblong is aligned between the multiple holes 6, the direction of its long axis may be along the vertical direction when the zinc battery is set, or along the horizontal direction. When the shape of the hole 6 is a polygon, various numbers of sides such as triangles, hexagons, octagons, etc. may be used. The polygon may be a regular polygon. The negative electrode material layer 3 is a layer formed by the negative electrode material. The negative electrode material layer 3 is supported by the collector 2 by filling the negative electrode material between the multiple holes 6 of the collector 2, and is fixed to the collector 2. The negative electrode material layer 3 contains a zinc-containing component. As the zinc-containing component, for example, metallic zinc, zinc oxide and zinc hydroxide can be cited. The zinc-containing component acts as a negative electrode active material in the zinc battery, and can also be referred to as a raw material for the negative electrode active material. From the perspective of obtaining better life performance, the content of the zinc-containing component is preferably 50% by mass or more, more preferably 70% by mass or more, and further preferably 75% by mass or more, based on the total mass of the negative electrode material. From the perspective of obtaining better life performance, the content of the zinc-containing component is preferably 95% by mass or less, more preferably 90% by mass or less, and further preferably 85% by mass or less, based on the total mass of the negative electrode material. The negative electrode material layer 3 may also include additives such as a binder (adhesive) and a conductive material. As a binder, hydrophilic or hydrophobic polymers may be cited. Specifically, for example, polytetrafluoroethylene (PTFE), hydroxyethyl cellulose (HEC), carboxymethyl cellulose (CMC), polyethylene oxide, polyethylene, polypropylene, etc. may be used as a binder. The binder may be used alone or in combination. Regarding the viscosity of the binder, for example, in a 2% aqueous solution, it may be 3000 to 6000 cp at room temperature (25°C), and in a 60% aqueous solution, it may be about 25 cp at room temperature (25°C). The content of the binder is, for example, 0.5 to 10% by mass relative to 100% by mass of the zinc-containing component. As a conductive material, indium compounds such as indium oxide may be cited. The content of the conductive agent is, for example, 1 to 20% by mass relative to 100% by mass of the zinc-containing component. As a method for making the above-mentioned negative electrode 1 for zinc battery, there is, for example, a method of preparing a collector 2, and drying after placing a negative electrode material slurry on the collector 2. The negative electrode material slurry can be placed on the collector 2, for example, by rolling the negative electrode material slurry into a thin sheet and attaching it to the collector 2. The negative electrode material slurry can be placed on the collector 2 and on the inner side of the plurality of holes 6, for example, by coating or filling the negative electrode material slurry on the collector 2. The method of coating or filling the negative electrode material slurry is not particularly limited and can be appropriately selected according to the shape of the collector 2, the shape of the negative electrode material layer 3, etc. The negative electrode material layer 3 composed of the negative electrode material is formed by drying the negative electrode material slurry layer composed of the negative electrode material slurry. As needed, the density of the negative electrode material layer 3 can also be increased by stamping and other methods. The negative electrode material slurry contains a raw material of the negative electrode material and a solvent (such as water). The negative electrode material slurry can be obtained by adding a solvent (such as water) to the raw material of the negative electrode material and kneading it. Examples of the raw material of the negative electrode material include zinc-containing components and additives. Next, a nickel-zinc battery will be described as an example of the zinc battery of this embodiment using the zinc battery negative electrode 1. In the nickel-zinc battery, the negative electrode is a zinc (Zn) electrode, and the positive electrode is a nickel (Ni) electrode. Figure 4 1 is a diagram schematically showing the structure of a nickel-zinc battery 10 . The nickel-zinc battery 10 of this embodiment includes, for example, an electrolytic cell 11, an electrode group (e.g., an electrode plate group) 12 housed in the electrolytic cell 11, and an electrolyte 13. The nickel-zinc battery 10 may be either formed or unformed. When the nickel-zinc battery 10 is an unformed nickel-zinc battery, the electrodes (negative and positive electrodes) are unformed electrodes, and when the nickel-zinc battery 10 is a formed nickel-zinc battery, the electrodes are formed electrodes. The electrode group 12 includes, for example, a negative electrode (e.g., a negative electrode plate) 14, a positive electrode (e.g., a positive electrode plate) 15, and a separator 16 disposed between the negative electrode 14 and the positive electrode 15. The electrode group 12 may include a plurality of negative electrodes 14, a positive electrode 15, and a separator 16. The plurality of negative electrodes 14 and the plurality of positive electrodes 15 may be connected to each other, for example, by a ribbon. The negative electrode 14 has the structure of the negative electrode 1 for zinc battery described above. The separator 16 is, for example, a separator having a flat plate shape, a sheet shape, or the like. Examples of the separator 16 include polyolefin-based microporous membranes, nylon-based microporous membranes, oxidation-resistant ion exchange resin membranes, cellophane-based recycled resin membranes, inorganic-organic separators, polyolefin-based nonwoven fabrics, and the like. The positive electrode 15 has a positive electrode collector and a positive electrode material supported by the positive electrode collector. The positive electrode collector constitutes a conductive path for the current from the positive electrode material. The positive electrode collector has, for example, a flat plate shape, a sheet shape, etc. The positive electrode collector can be a collector of a three-dimensional mesh structure composed of a foamed metal, a porous metal plate, a punched metal plate, a felt-like object of a metal fiber, etc. The positive electrode collector is composed of a material having conductivity and alkali resistance. As such a material, for example, a material that can remain stable even at the reaction potential of the positive electrode can be used. Regarding materials that are still stable at the reaction potential of the positive electrode, for example, a material having a higher redox potential than the reaction potential of the positive electrode, or a material that forms a protective film such as an oxide film on the surface of the substrate in an alkaline aqueous solution and stabilizes the same. In the positive electrode, as a side reaction, a decomposition reaction of the electrolyte is carried out to produce oxygen. In terms of being able to suppress the progress of such a side reaction, a material with a high oxygen overvoltage is preferred. As specific examples of materials constituting the positive electrode collector, platinum, nickel (foamed nickel, etc.), metal materials (copper, brass, steel, etc.) on which metal plating is implemented, etc. can be cited. Among them, a positive electrode collector consisting of foamed nickel is preferably used. From the viewpoint of being able to further improve the high rate discharge performance, it is preferred that at least the portion (positive electrode material supporting portion) supporting the positive electrode material in the positive electrode collector is composed of foamed nickel. The positive electrode material is, for example, in a layered form. That is, the positive electrode may have a positive electrode material layer. The positive electrode material layer may be formed on a positive electrode collector. When the positive electrode material support portion of the positive electrode collector has a three-dimensional network structure, the positive electrode material may be filled between the grids of the positive electrode collector to form a positive electrode material layer. The positive electrode material contains a positive electrode active material containing nickel. Examples of the positive electrode active material include nickel oxyhydroxide (NiOOH), nickel hydroxide, and the like. The positive electrode material, for example, contains nickel oxyhydroxide in a fully charged state and contains nickel hydroxide in a discharge end state. For example, based on the total mass of the positive electrode material, the content of the positive electrode active material may be in the range of 50 mass % to 95 mass %. The positive electrode material may also contain other components other than the positive electrode active material as an additive. As additives, binders (adhesives), conductive agents, expansion inhibitors, etc. may be cited. As binders, hydrophilic or hydrophobic polymers may be cited. Specifically, for example, carboxymethyl cellulose (CMC), hydroxyethyl cellulose (HEC), hydroxypropyl methyl cellulose (HPMC), sodium polyacrylate (SPA), fluorine polymers (polytetrafluoroethylene (PTFE) etc.) etc. may be used as binders. The content of the binder is, for example, in the range of 0.01% to 5% by mass relative to 100% by mass of the positive electrode active material. As conductive agents, cobalt compounds (metallic cobalt, cobalt oxide, cobalt hydroxide etc.) may be cited. The content of the binder is, for example, in the range of 1% to 20% by mass relative to 100% by mass of the positive electrode active material. As expansion inhibitors, zinc oxide etc. may be cited. The content of the expansion inhibitor is, for example, in the range of 0.01% to 5% by mass relative to 100% by mass of the positive electrode active material. The electrolyte 13 contains, for example, a solvent and an electrolyte. As the solvent, water (for example, ion exchange water) and the like can be cited. As the electrolyte, alkaline compounds and the like can be cited, for example, alkali metal hydroxides such as potassium hydroxide (KOH), sodium hydroxide (NaOH), and lithium hydroxide (LiOH) and the like can be cited. The electrolyte can contain components other than the solvent and the electrolyte, such as potassium phosphate, potassium fluoride, potassium carbonate, sodium phosphate, sodium fluoride, zinc oxide, antimony oxide, titanium dioxide, nonionic surfactants, anionic surfactants and the like. The nickel-zinc battery 10 described above can be obtained, for example, by a method having an assembly process, wherein the components including the negative electrode 14 and the positive electrode 15 are assembled to obtain the nickel-zinc battery 10. In the assembly process, for example, the unformed positive electrode 15 and the unformed negative electrode 14 are alternately stacked via the separator 16, and the positive electrodes 15 and the negative electrodes 14 are connected to each other by a belt, thereby producing the electrode group 12. Next, after the electrode group 12 is arranged in the electrolytic cell 11, a cover is bonded to the upper surface of the electrolytic cell 11 to obtain the unformed nickel-zinc battery 10. Next, the electrolyte 13 is injected into the electrolytic cell 11 and left for a certain period of time. Next, the formation is performed by charging under prescribed conditions, thereby obtaining the nickel-zinc battery 10. In the above, the nickel-zinc battery 10 in which the positive electrode 15 is a nickel electrode is described, but the zinc battery may also be a zinc-air battery in which the positive electrode is an air electrode, or may be a silver-zinc battery in which the positive electrode is a silver oxide electrode. As the silver oxide electrode of the silver-zinc battery, a known silver oxide electrode used in a silver-zinc battery can be used. The silver oxide electrode contains, for example, silver (I) oxide. As the air electrode of the zinc-air battery, a known air electrode used in a zinc-air battery can be used. The air electrode contains, for example, an air electrode catalyst, an electronic conductive material, etc. As the air electrode catalyst, an air electrode catalyst that also functions as an electronic conductive material can be used. As the air electrode catalyst, a catalyst that functions as a positive electrode in a zinc-air battery can be used, and various air electrode catalysts that utilize oxygen as a positive electrode active material can be used. As the air electrode catalyst, carbon-based materials (graphite, etc.) having a redox catalyst function, metal materials (platinum, nickel, etc.) having a redox catalyst function, and inorganic oxide materials (perovskite oxides, manganese dioxide, nickel oxide, cobalt oxide, spinel oxide, etc.) having a redox catalyst function can be cited. The shape of the air electrode catalyst is not particularly limited, for example, it can be in the form of particles. The amount of the air electrode catalyst used in the air electrode can be in the range of 5% to 70% by volume, or in the range of 5% to 60% by volume, or in the range of 5% to 50% by volume relative to the total amount of the air electrode. As the electron conductive material, a material that has conductivity and can conduct electrons between the air electrode catalyst and the diaphragm can be used. As the electron conductive material, carbon blacks such as Ketjen black, acetylene black, channel black, furnace black, lamp black and thermal black can be cited; graphites such as natural graphite such as flake graphite, artificial graphite, expanded graphite, etc.; conductive fibers such as carbon fibers and metal fibers; metal powders such as copper, silver, nickel, and aluminum; organic electron conductive materials such as polyphenylene derivatives; any mixture thereof, etc. The shape of the electron conductive material can be particulate or other shapes. The electron conductive material is preferably used in the form of a continuous phase in the thickness direction in the air electrode. For example, the electron conductive material can be a porous material. The electron conductive material can be in the form of a mixture or a complex with the air electrode catalyst, as described above, or it can be an air electrode catalyst that acts as an electron conductive material. The amount of the electron conductive material used in the air electrode may be in the range of 10 to 80 volume %, 15 to 80 volume %, or 20 to 80 volume % relative to the total amount of the air electrode. The effects obtained by the zinc battery negative electrode 1 and the nickel-zinc battery 10 according to the present embodiment described above are described. As described above, in the zinc battery negative electrode 1 of the present embodiment, the current collector 2 has a plurality of holes 6 that penetrate along the thickness direction of the current collector 2 and are filled with the negative electrode material layer 3. In addition, the plurality of holes 6 include a plurality of holes having an inner surface area greater than 0.5 mm2 on a cross section perpendicular to the thickness direction of the current collector 2. 2 And less than 19.6mm 2 When the cross-sectional shape of each of the plurality of holes 6 is circular, the plurality of holes 6 include a hole 6 having an inner diameter R on the cross-section greater than 0.8 mm and less than 5 mm. When the inner surface area of ​​hole 6 is greater than 0.5 mm 2 And less than 19.6mm 2 When the inner diameter R of the hole 6 is greater than 0.8 mm and less than 5 mm, as shown in the examples described later, the life of the zinc battery in the cycle test can be extended. This result is believed to be due to the following effect. That is, when the inner surface area of ​​the hole 6 is greater than 0.5 mm 2 When the inner diameter R of the hole 6 is greater than 0.8 mm, the fluidity of the electrolyte 13 inside the zinc battery negative electrode 1 increases, thereby improving the uniformity of the reaction. 2 Or when the inner diameter R is less than 5 mm, the uneven coating of the negative electrode material slurry between the hole 6 and the surface of the substrate 4 other than the hole 6 becomes smaller, the thickness uniformity of the negative electrode material layer 3 is improved, and thus the uniformity of the reaction is improved. If the uniformity of the reaction is improved, the growth of dendrites based on the precipitation of zinc slows down, and the time until the negative electrode 14 and the positive electrode 15 are short-circuited due to dendrites is extended. As a result, the life of the zinc battery is extended. The growth of dendrites based on the precipitation of zinc is significant at high temperatures (e.g., 70°C), so the above effect is more effective at high temperatures. The inner surface area of ​​hole 6 can be 1.7 mm 2 Above and 7.0mm 2 Or, the inner diameter R of the hole 6 can be greater than 1.5 mm and less than 3 mm. In this case, as shown in the examples described below, the life of the zinc battery in the cycle test can be further extended. This result can also be considered to be due to the improved uniformity of the reaction, which slows down the growth of dendrites based on the precipitation of zinc, thereby extending the time until the negative electrode 14 and the positive electrode 15 are short-circuited due to dendrites. As in the present embodiment, the current collector 2 may have a conductive substrate 4 and a tin-plated film 5 covering at least a portion of the surface of the substrate 4. Thus, even when the resistivity of the substrate 4 is relatively high, the electrical performance of the current collector 2 can be fully utilized. Therefore, a material such as carbon steel having a relatively high resistivity can be used as the main constituent material of the current collector 2, and the options for the constituent materials of the current collector 2 can be increased. In this case, the substrate 4 may mainly contain carbon steel. Thus, compared to, for example, the case where copper is used as the material of the substrate 4, the manufacturing cost of the negative electrode 1 for a zinc battery can be reduced. As in this embodiment, the negative electrode material layer 3 may include a zinc-containing component and a binder. In this case, the negative electrode material layer 3 can be easily formed by applying the negative electrode material slurry. Example Hereinafter, the contents of the present invention will be described in more detail using examples, but the present invention is not limited to the following examples. [Production of negative electrode] As negative electrode current collectors, five samples A to E shown in Table 1 below were prepared. Specifically, samples A to E were prepared as tin-plated steel plate punching metal plates having respective pore diameters and porosity. Samples A to E differed only in the inner diameter and porosity of the circular hole 6, and the other structures were the same. The porosity of any sample was 50% or more. [Table 1] Next, zinc oxide, metallic zinc, surfactant, HEC and ion exchange water were weighed and mixed in a predetermined amount, and the negative electrode material slurry was prepared by stirring the obtained mixed solution. At this time, the mass ratio of the solid component was adjusted to "zinc oxide: metallic zinc: HEC: surfactant = 84.5: 11.5: 3.5: 0.5". The water content of the negative electrode material slurry was adjusted to 32.5% by mass based on the total mass of the negative electrode material slurry. Then, the negative electrode material slurry was applied to the negative electrode collector and dried at 80°C for 30 minutes. After that, the negative electrode having a negative electrode material layer was obtained by pressure forming by a roller press. [Preparation of electrolyte] Potassium hydroxide (KOH) and lithium hydroxide (LiOH) were added to ion exchange water and mixed to prepare an electrolyte solution (potassium hydroxide concentration: 30 mass %, lithium hydroxide concentration: 1 mass %). [Production of positive electrode] A lattice body composed of foamed nickel with a porosity of 95% was prepared, and a positive electrode collector was obtained by press-forming the lattice body. Next, cobalt-coated nickel hydroxide powder, metal cobalt, cobalt hydroxide, yttrium oxide, CMC, PTFE, and ion exchange water were weighed and mixed in a specified amount, and a positive electrode material slurry was prepared by stirring the mixed solution. At this time, the mass ratio of the solid component was adjusted to "nickel hydroxide: metal cobalt: yttrium oxide: cobalt hydroxide: CMC: PTFE = 88: 10.3: 1: 0.3: 0.3: 0.1". The moisture content of the positive electrode material slurry was adjusted to 27.5% by mass based on the total mass of the positive electrode material slurry. Then, after the positive electrode material slurry was applied to the positive electrode material support portion of the positive electrode collector, it was dried at 80°C for 30 minutes. After that, it was press-formed by a roller press to obtain an unformed positive electrode having a positive electrode material layer. [Preparation of diaphragm] In the separator, Celgard (registered trademark) 2500 was used as a microporous membrane, and VL100 (manufactured by Nippon Kodoshi Corporation) was used as a non-woven fabric. Before assembling the battery, the microporous membrane was hydrophilized with a surfactant Triton (registered trademark) -X100 (manufactured by The Dow Chemical Company). The hydrophilization treatment was carried out by immersing the microporous membrane in an aqueous solution containing 1% by mass of Triton-X100 for 24 hours and then drying it at room temperature for 1 hour. In addition, the microporous membrane was cut into a specified size, folded in half, and the sides were heat-welded to form a bag. In the microporous membrane processed into a bag, one unformed positive electrode and one unformed negative electrode were respectively contained. The non-woven fabric used was a non-woven fabric cut into a specified size. [Manufacturing of Nickel-Zinc Batteries] Two positive electrodes respectively contained in bag-shaped microporous membranes and three negative electrodes respectively contained in bag-shaped microporous membranes (sample A) are alternately stacked, non-woven fabric is sandwiched between the positive electrode and the negative electrode, and the plates of the same polarity are connected to each other with a belt to produce an electrode group (plate group). After the electrode group is arranged in the electrolytic cell, the cover is adhered to the upper surface of the electrolytic cell to obtain an unformed nickel-zinc battery. Then, the electrolyte is injected into the electrolytic cell of the unformed nickel-zinc battery and left for 24 hours. After that, it is charged at 20mA and 15 hours to produce a nickel-zinc battery with a nominal capacity of 320mAh. Nickel-zinc batteries having negative electrodes of samples B to E, respectively, are also produced in the same manner. [Cycle test] A nickel-zinc battery having negative electrode collectors of samples A to E was used, and the battery was charged at a constant voltage of 70°C, 105.7 mA (0.33C), and 1.88 V until the current value decayed to 16 mA (0.05C). The battery was then discharged at a constant current of 105.7 mA (0.33C) until the battery voltage reached 1.1 V. This was considered as one cycle in a cycle test. The above "C" relatively represents the current size when the rated capacity is discharged at a constant current from a fully charged state. The above "C" refers to "discharge current value (A) / battery capacity (Ah)". For example, the current that can discharge the rated capacity within 1 hour is represented as "1C", and the current that can discharge the rated capacity within 2 hours is represented as "0.5C". In the above cycle test, the short circuit resistance is evaluated by dividing the charge capacity by the discharge capacity in each cycle, and the number of cycles when the charge rate exceeds 110% is determined as the cycle at which a short circuit occurs and is taken as the life. Table 2 below shows the cycle life of the nickel-zinc battery having the negative electrode collectors of samples A to E, respectively. [Table 2] As shown in Table 2, the cycle life of the nickel-zinc battery with the negative electrode collector of sample B is the longest, followed by the cycle life of the nickel-zinc battery with the negative electrode collectors of samples C and D. The cycle life of the nickel-zinc battery with the negative electrode collectors of samples A and E is significantly shorter than that of samples B to D. Based on this result, it can be said that when the inner surface area of ​​pore 6 is larger than 0.5 mm 2 And less than 19.6mm 2 When the inner surface area of ​​hole 6 is 1.7mm 2 Above and 7.0mm 2 When the inner surface area of ​​hole 6 is 1.7 mm 2 Above and 3.1mm 2 When the value is below , the cycle life is further prolonged. The negative electrode for zinc battery and the zinc battery of the present invention are not limited to the above-mentioned embodiments, and various modifications are possible. For example, in the above-mentioned embodiments, copper and carbon steel are shown as examples of the material of the substrate, but various materials can be used for the substrate as long as they are conductive materials. Explanation of symbols 1-negative electrode for zinc battery, 2-current collector, 3-negative electrode material layer, 4-substrate, 5-tin-plated film, 6-pore.

Claims

1. A negative electrode for a zinc battery, comprising: current collector; and A negative electrode material layer is fixed to the current collector, The current collector has a plurality of holes penetrating in the thickness direction and filled with the negative electrode material layer, The plurality of holes include an inner surface area greater than 0.5 mm in a cross section perpendicular to the thickness direction. 2 And less than 19.6mm 2 hole.

2. The negative electrode for zinc battery according to claim 1, wherein The cross-section of each of the plurality of holes is circular in shape, The plurality of holes include holes having an inner diameter in the cross section greater than 0.8 mm and less than 5 mm.

3. The negative electrode for zinc battery according to claim 1 or 2, wherein: The open porosity of the current collector is greater than 35%.

4. The negative electrode for zinc battery according to claim 1 or 2, wherein: The current collector has: Conductive substrate; and The tin-plated film covers at least a portion of the surface of the substrate.

5. The negative electrode for zinc battery according to claim 4, wherein: The substrate primarily comprises carbon steel.

6. The negative electrode for zinc battery according to claim 1 or 2, wherein: The negative electrode material layer includes a zinc-containing component and a binder.

7. A zinc battery comprising: The negative electrode for zinc battery according to claim 1 or 2; and positive electrode.