Method for eliminating flocculent carbon of lithium iron phosphate
Through metal ion solution soaking and high-temperature reduction treatment, floc carbon in lithium iron phosphate material is converted into graphitized carbon, solving the problems of low conductivity and floc carbon influence of lithium iron phosphate material, improving material performance and reducing Production cost.
Patent Information
- Application Number
- CN202411432736.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-14
- Publication Date
- 2024-11-22
AI Technical Summary
The low electronic conductivity and small lithium ion diffusion coefficient of lithium iron phosphate cathode material lead to limited performance in high-power applications, and the floc carbon generated during carbon coating affects the material's performance, and the prior art is not effective Solve the problem of graphitization of floc carbon.
By immersing the lithium iron phosphate material with a metal ion solution of 0.1 to 1 mol/L, combined with drying and high-temperature reduction treatment, floc carbon is converted into graphitized carbon, and the reaction conditions are controlled to achieve efficient graphitization.
It effectively improves the conductivity and electrochemical properties of lithium iron phosphate materials, reduces the impact of floc carbon, reduces production costs, and is suitable for large-scale production.
Smart Images

Figure CN118993016A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of lithium iron phosphate preparation, and more specifically, to a method for eliminating flocculent carbon of lithium iron phosphate. Background Art
[0002] Lithium iron phosphate cathode materials are widely used in the new energy vehicle market and energy storage field due to their safety, environmental protection, low raw material prices, and stable discharge platform. However, due to their low electronic conductivity and small lithium ion diffusion coefficient, their performance in high-power applications is limited, and the prepared lithium iron phosphate battery has a short cycle life and is prone to capacity decay. In order to improve its performance, a common method is to use carbon coating to improve the conductivity and rate performance of lithium iron phosphate cathode materials and the life of lithium iron phosphate batteries. However, during the carbon coating process, due to local temperature unevenness or improper atmosphere control during the carbonization process, fine flocculent carbon is sometimes produced on the surface of the material, and these generated flocculent carbons will have some adverse effects on the material, such as rough and uneven surface, gaps between the substrate and the coating layer, and voids or protrusions.
[0003] If we want to further make full use of the flocculent carbon and make it a beneficial part for lithium iron phosphate, we need to convert it into graphitized carbon. However, the process of converting it into graphitized carbon is the process of converting the flocculent carbon from an amorphous state to a crystalline state, which will inevitably encounter great resistance and easily form an unstable state, making graphitization difficult. Therefore, some power is needed to promote its graphitization process, such as high temperature or catalyst conditions. However, the high-temperature graphitization temperature of amorphous carbon is generally more than 2000°C. The carbonization equipment will work at high temperature for a long time, which will lead to a reduction in service life. At the same time, high energy consumption also increases the cost of production. Therefore, using a catalyst to convert low-temperature flocculent carbon is a more economical method.
[0004] The prior art also introduces catalysts, such as transition metal elements and their compounds, to promote the graphitization of carbon, thereby improving the electrochemical properties of the material as a whole and reducing the impact of flocculent carbon. This is to increase the degree of graphitization reaction during the carbon coating process to increase the carbon utilization rate and reduce the generation of flocculent carbon. However, there is no mention of graphitizing the flocculent carbon formed after carbon coating. Summary of the invention
[0005] In view of the above, the present invention provides a method for eliminating flocculent carbon in lithium iron phosphate, which converts the flocculent carbon into crystalline carbon, namely graphitized carbon, and effectively eliminates the flocculent carbon in lithium iron phosphate.
[0006] The present invention provides a method for eliminating flocculent carbon of lithium iron phosphate, comprising: (1) Preparing a metal ion solution: Preparing a metal ion solution containing metal ions at a concentration of 0.1 to 1 mol / L; (2) Soaking and drying: soaking the lithium iron phosphate material in a metal ion solution for 24 hours, and then drying the soaked lithium iron phosphate material at a drying temperature of 80° C. for 6 hours; High temperature reduction: The dried lithium iron phosphate material is subjected to high temperature reduction treatment, the reduction temperature is 350-650°C, and the reduction time is 1-3 hours.
[0007] A small amount of flocculent carbon will remain on the surface of the carbon-coated lithium iron phosphate material, which will affect the performance of the lithium iron phosphate material. Therefore, it is necessary to effectively eliminate the flocculent carbon and improve the performance of the lithium iron phosphate material, but also to pay attention to overreaction, which will affect the structure of the lithium iron phosphate material and reduce the performance of the lithium iron phosphate material. The present invention immerses the lithium iron phosphate material in a metal ion solution. At this time, the flocculent carbon on the surface of the lithium iron phosphate material will adsorb the metal ions in the solution. The concentration of the metal ions has a significant effect on the reaction of eliminating the flocculent carbon: within a certain range, as the metal ion concentration increases, the rate and amount of the flocculent carbon adsorbing the metal ions will increase. More metal ions are conducive to reducing the activation energy required for graphitization, thereby realizing the conversion of the flocculent carbon to graphite carbon at a lower temperature or in a shorter time. In this process, the metal ions themselves are not consumed, but participate in the reaction as a catalyst and can be recovered in the graphitized product. However, when the metal ion concentration exceeds a certain value, it may cause the flocculent carbon to adsorb too many metal ions, which in turn reduces the catalytic efficiency of the metal ions and reduces the conversion rate of the flocculent carbon to graphitized carbon. At the same time, it may also cause the lithium iron phosphate material to agglomerate and bring in impurities, thereby reducing the performance of the lithium iron phosphate material.
[0008] The metal ion solution includes iron ion solution, nickel ion solution, cobalt ion solution and copper ion solution. In order to control the content of other metal impurity elements in the lithium iron phosphate material, the iron ion solution is preferably used. The mass of metal ions in the metal ion solution is 0.01% to 0.1% of the total mass of the lithium iron phosphate.
[0009] The carbon content in lithium iron phosphate material is 1.3%, of which the content of flocculent carbon is less than 1%. Considering the three aspects of catalytic efficiency, cost and selectivity, too many metal ions may lead to an increase in side reactions, while inhibiting catalytic activity, affecting the conversion efficiency of flocculent carbon, increasing costs and possibly causing environmental pollution; too few metal ions are not enough to effectively catalyze the reaction, the reaction rate slows down, and the conversion of flocculent carbon is incomplete; therefore, the catalytic conversion is only 1% to 10% of this amount, and the amount of metal ions used is 0.01% to 0.1% of the total amount of lithium iron phosphate material.
[0010] The metal ion solution is a metal nitrate solution, because the decomposition temperature of nitrate is low, so it is suitable for low-temperature decomposition in subsequent treatment.
[0011] The method of the present invention uses a solution impregnation method to soak the lithium iron phosphate material with a solution containing metal ions such as iron, nickel, cobalt, and copper, and then converts the flocculent carbon into crystalline carbon, i.e., graphitized carbon, through drying and high-temperature reduction treatment, thereby improving the conductivity and electrochemical properties of the lithium iron phosphate material; at the same time, the method of the present invention does not change the synthesis process of lithium iron phosphate, will not change the crystal structure of lithium iron phosphate, and is simple and easy to implement, does not require special equipment, is conducive to large-scale production, and reduces production costs. Compared with changing the synthesis method, this method is more economical and more efficient. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Figure 1 This is a SEM picture of lithium iron phosphate that has not been subjected to the method of the present invention to eliminate flocculent carbon.
[0013] Figure 2 This is a SEM picture of lithium iron phosphate after the flocculent carbon is eliminated by the method of the present invention. DETAILED DESCRIPTION
[0014] The embodiments of the present application will be described in more detail below. The application can be implemented in various forms, and should not be construed as being limited to the embodiments set forth herein, but rather these embodiments are provided to provide a more thorough and complete understanding of the present application. It should be understood that the embodiments of the present application are only for exemplary purposes and are not intended to limit the scope of protection of the present application.
[0015] The embodiment of the present invention is implemented according to the following technical scheme, and the specific steps include: (1) preparing a metal ion solution: preparing a metal ion solution containing metal ions at a concentration of 0.1 to 1 mol / L, wherein the mass of the metal ions is 0.01% to 0.1% of the total mass of the lithium iron phosphate material; (2) Soaking and drying: soaking the lithium iron phosphate material in a metal ion solution for 24 hours, and then drying the soaked lithium iron phosphate material at a drying temperature of 80° C. for 6 hours; High temperature reduction: The dried lithium iron phosphate material is subjected to high temperature reduction treatment, the reduction temperature is 350-650°C, and the reduction time is 1-3 hours.
[0016] Table 1: Specific process conditions of the embodiments of the present invention and performance test results of lithium iron phosphate.
[0017] Attached Figure 1 is a SEM image of lithium iron phosphate without removing flocculent carbon by the method of the present invention, Figure 2This is a SEM picture of lithium iron phosphate after the flocculent carbon is eliminated by the method of the present invention. From the attached figure, it can be seen that the flocculent carbon in the lithium iron phosphate material after the flocculent carbon is eliminated by the method of the present invention is significantly reduced, which proves that the method of the present invention can effectively convert the flocculent carbon on the surface of the lithium iron phosphate material into graphitized carbon, thereby reducing the flocculent carbon on the surface of the lithium iron phosphate material.
[0018] Table 1 shows the specific process conditions of the embodiments of the present invention and the performance test results of the lithium iron phosphate material. The powder resistivity of the lithium iron phosphate material after the flocculent carbon is eliminated by the method of the present invention is significantly reduced, that is, its conductivity is significantly improved. At the same time, the charge and discharge specific capacity is significantly improved compared with the charge and discharge performance of the lithium iron phosphate material without eliminating the flocculent carbon. Figure 1 and attached Figure 2 This indicates that the method of the present invention not only effectively converts the flocculent carbon into graphitized carbon, thereby reducing the flocculent carbon on the surface of the lithium iron phosphate material, but also improves the conductivity and electrochemical properties of the lithium iron phosphate material.
[0019] The above description is only a specific implementation mode of the present invention, but the protection scope of the present invention is not limited thereto. For example, any technician familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed in this application, which should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.
Claims
1. A method for eliminating lithium iron phosphate flocculent carbon, characterized in that: include: (1) preparing a metal ion solution: preparing a metal ion solution having a metal ion concentration of 0.1 to 1 mol / L; (2) Soaking and drying: soaking the lithium iron phosphate material in a metal ion solution, and then drying the soaked lithium iron phosphate material; (3) High temperature reduction: The dried lithium iron phosphate material is subjected to high temperature reduction treatment, the reduction temperature is 350 to 650° C., and the reduction time is 1 to 3 hours.
2. The method for eliminating lithium iron phosphate flocculent carbon according to claim 1, characterized in that: The mass of the metal ions is 0.01% to 0.1% of the total mass of the lithium iron phosphate material.
3. The method for eliminating lithium iron phosphate flocculent carbon according to claim 1, characterized in that: The soaking time of the soaking and drying is 24 hours, and the drying is carried out at a temperature of 80° C. for 6 hours.
4. The method for eliminating lithium iron phosphate flocculent carbon according to claim 1, characterized in that: The metal ion solution includes iron ion solution, nickel ion solution, cobalt ion solution and copper ion solution.
5. The method for eliminating lithium iron phosphate flocculent carbon according to claim 1, characterized in that: The metal ion solution is a metal nitrate solution.
Citation Information
Patent Citations
Lithium iron phosphate / carbon composite anode material prepared by catalytic graphitization method, and preparation method thereof
CN102347476A
Synthesizing method of anode material lithium iron phosphate of lithium ion battery
CN102651475A
Secondary battery