Extreme pressure anti-wear agent for lubricating oil and preparation method of extreme pressure anti-wear agent
Through the mixed preparation of composite organic molybdenum and modified wear-resistant agent, the problem that existing lubricant additives cannot meet environmental protection requirements is solved, and the wear resistance, corrosion and green environmental protection of lubricant is achieved, forming a stable oil film and chemical reaction. membrane, reduces wear and reduces environmental pollution.
Patent Information
- Application Number
- CN202411048432.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-08-01
AI Technical Summary
Existing lubricant additives such as ZDDP cannot meet environmental protection requirements and are difficult to achieve high-performance green friction reduction and anti-wear effects.
Compound organic molybdenum is prepared by the mixed preparation method of composite organic molybdenum and modified wear-resistant agent, and composite organic molybdenum is prepared by reaction of 2,4-dichlorobenzyl alcohol, diphosphate pentasulfide, sodium molybdate, graphene and other materials, and iodoacetamide is used, 3 -Chlobenzohydrazide, 2,5-dimercaptothiadiazole and other materials produce modified wear-resistant agents, combined with ultrasonic and physical mixing technology, to form extreme pressure anti-wear agents.
The wear resistance, corrosion resistance and green environmental protection of lubricating oil are achieved, and by forming a stable oil film and chemical reaction film, wear and environmental pollution are reduced.
Smart Images

Figure BDA0004974174940000061 
Figure BDA0004974174940000071
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of lubricating oil additives, in particular to an extreme pressure anti-wear agent for lubricating oil and a preparation method thereof. Background Art
[0002] With the gradual improvement of national environmental protection laws, the advancement of automobile engine and transmission system design, and the development of mechanical equipment, higher and higher requirements have been put forward for the formulation of lubricant industry standards. Lubricant additives are compounds added to base oils at corresponding concentrations. They can be a single compound or an interaction of multiple types of compounds.
[0003] Since traditional lubricant additives represented by zinc dialkyl dithiophosphate (ZDDP) can no longer meet environmental protection requirements, green anti-friction and anti-wear lubricant additives play an increasingly important role. In order to reduce environmental pollution, whether an excellent environmentally friendly lubricant extreme pressure anti-wear additive can be found to replace the most widely used ZDDP has become a hot spot in lubricant research and development. Summary of the invention
[0004] The object of the present invention is to provide an extreme pressure anti-wear agent for lubricating oil and a preparation method thereof, so as to solve the problems existing in the prior art.
[0005] In order to solve the above technical problems, the present invention provides the following technical solutions: an extreme pressure anti-wear agent for lubricating oil, wherein the extreme pressure anti-wear agent for lubricating oil is prepared by mixing composite organic molybdenum and modified anti-wear agent.
[0006] Furthermore, the composite organic molybdenum is prepared from 2,4-dichlorobenzyl alcohol, phosphorus pentasulfide, sodium molybdate and graphene.
[0007] Furthermore, the modified anti-wear agent is prepared from iodoacetamide, 3-chlorobenzoyl hydrazide and 2,5-dimercaptothiadiazole.
[0008] Furthermore, a method for preparing an extreme pressure anti-wear agent for lubricating oil comprises the following preparation steps:
[0009] (1) Dissolve 25-35 parts of 2,4-dichlorobenzyl alcohol in 32-46 parts of toluene, add 18-22 parts of phosphorus pentasulfide at 40-60°C, 600 rpm, and under nitrogen protection, raise the temperature to 85-95°C, and react for 2-4 hours to obtain a thiophosphoric acid solution;
[0010] (2) After 21 to 34 parts of sodium molybdate and 40 to 50 parts of water are stirred and dissolved, 16 to 32 parts of dilute sulfuric acid solution are added to adjust to acidity, and then 25 to 39 parts of thiophosphoric acid solution are added, the temperature is raised to 80 to 100° C., the reaction is performed for 4 to 6 hours, the temperature is cooled to 20 to 30° C., the filter is suctioned, and the filtrate is then rinsed with 57 to 73 parts of methanol, and the filtrate is dried at 50 to 60° C. for 2 to 6 hours to obtain modified organic molybdenum;
[0011] (3) dispersing 16 to 24 parts of modified organic molybdenum in 98 to 122 parts of ethanol, stirring at 500 rpm for 10 to 30 min, adding 34 to 56 parts of an aqueous solution of graphene, ultrasonicating at 40 to 60° C. and 20 to 100 kHz for 1 to 2 h, centrifuging, washing, and drying at 50 to 60° C. for 2 to 6 h to obtain composite organic molybdenum;
[0012] (4) Dissolve 7 to 15 parts of 3-chlorotoluhydrazide and 2 to 4 parts of potassium hydroxide solid in 56 to 144 parts of isopropanol, add 18 to 42 parts of iodoacetamide and 18 to 46 parts of toluene, react at 80 to 100° C. for 40 to 50 hours, add 55 to 141 parts of dichloromethane and 32 to 68 parts of saturated sodium bicarbonate solution after concentration, extract and separate three times, concentrate the organic phase, and obtain a composite hydrazide;
[0013] (5) Dissolve 0.8-2.4 parts of potassium iodide and 1.2-1.8 parts of potassium carbonate in 47-63 parts of dimethylformamide, add 7-13 parts of 2,5-dimercaptothiadiazole, stir at 600 rpm for 10-20 min, then add 17-23 parts of composite hydrazide, react at 100-120° C. for 3-6 h, cool naturally to 20-30° C., wash with 38-52 parts of water, filter and take the filter cake, rinse with 21-45 parts of acetone, and dry at 50-60° C. for 2-6 h to obtain a modified wear-resistant agent;
[0014] (6) 12 to 18 parts of composite organic molybdenum, 4 to 6 parts of modified anti-wear agent, 0.02 to 0.08 parts of defoaming agent, and 0.06 to 0.14 parts of anti-emulsifier are mixed to obtain an extreme pressure anti-wear agent for lubricating oil.
[0015] Furthermore, the concentration of the dilute sulfuric acid in step (2) is 35%, and the acidic pH is 1.5-2.0.
[0016] Furthermore, the concentration of the graphene aqueous solution in step (3) is 2 mg / mL.
[0017] Furthermore, the centrifugal speed in step (3) is 1800 rpm / min, and the centrifugal time is 10 to 20 min; the cleaning conditions are: 62 to 84 parts of deionized water and 62 to 84 parts of ethanol are alternately rinsed twice.
[0018] Furthermore, the concentration conditions in step (4) are: vacuum degree -0.1MPa to -0.04MPa, and concentration time: 1 to 3h.
[0019] Furthermore, the defoaming agent in step (6) is one or more of T921, DF667, and FS1265.
[0020] Furthermore, the anti-emulsifier in step (6) is one or more of D114, T1001, and T705.
[0021] Compared with the prior art, the beneficial effects achieved by the present invention are:
[0022] The invention prepares an extreme pressure anti-wear agent by mixing composite organic molybdenum with a modified anti-wear agent, so as to achieve the effects of wear resistance, corrosion resistance and green environmental protection.
[0023] Firstly, the composite organic molybdenum uses 2,4-dichlorobenzyl alcohol to react with phosphorus pentasulfide to generate di(β-2,4-dichlorobenzyl) dithiophosphoric acid, in which the sulfur, phosphorus and chlorine groups react by adsorption when in contact with the metal surface, initially forming a lubricating film on the surface to reduce wear; then, it reacts with sodium molybdate under acidic conditions to generate di(β-2,4-dichlorobenzyl) dithiophosphoric acid molybdenum, introducing molybdenum atoms to reduce the friction coefficient of the oil and improve wear resistance; then, it is physically mixed with graphene to make the organic molybdenum evenly adhere to the graphene surface, causing the graphene to be evenly dispersed inside the anti-wear agent in a network structure, and when friction occurs, it enters the secondary surface, fills and repairs the scratches after wear, and forms a stable oil film to increase wear resistance.
[0024] Secondly, the modified anti-wear agent is prepared from iodoacetamide, 3-chlorobenzohydrazide and thiadiazole; the iodine group of iodoacetamide reacts with the hydrazide structure of 3-chlorobenzohydrazide to make it have an amide bond, obtain hydrophobic properties, reduce liquid penetration, and improve the anti-corrosion effect. In addition, the hydrazide structure can effectively inhibit the migration of C elements from the base oil to the metal surface, has better stability and is green and environmentally friendly; then the chlorine group in the hydrazide combines with the thiol group of 2,5-dimercaptothiadiazole to form a CS bond, which is easy to form a reaction film with the metal surface to achieve an anti-wear effect. On this basis, thiadiazole is biodegradable and reduces environmental pollution. DETAILED DESCRIPTION
[0025] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0026] In order to more clearly illustrate the method provided by the present invention, the following examples are used to describe in detail the various index testing methods of the extreme pressure anti-wear agent for lubricating oil prepared in the following examples are as follows:
[0027] Load-bearing capacity: The composite additives of the embodiment and the comparative example were mixed evenly with the hydraulic oil and tested according to GB / T 3142-1982.
[0028] Corrosion resistance: The composite additives of the embodiment and the comparative example were mixed evenly with the hydraulic oil and tested according to GB / T 5096.
[0029] Biodegradation rate: The composite additives of the embodiments and comparative examples were mixed evenly with hydraulic oil and tested according to GB / T19277.1-2011.
[0030] Example 1
[0031] (1) Dissolve 25 parts of 2,4-dichlorobenzyl alcohol in 32 parts of toluene, add 18 parts of phosphorus pentasulfide at 40°C, 600 rpm, and under nitrogen protection, raise the temperature to 85°C, and react for 2 hours to obtain a thiophosphoric acid solution;
[0032] (2) After 21 parts of sodium molybdate and 40 parts of water are stirred and dissolved, 16 parts of 35% dilute sulfuric acid solution are added to adjust the pH to 1.5, and then 25 parts of thiophosphoric acid solution are added, the temperature is raised to 80° C., the reaction is carried out for 4 hours, the temperature is cooled to 20° C., the filter is sucked, and the filtrate is rinsed with 57 parts of methanol, and the filtrate is dried at 50° C. for 2 hours to obtain modified organic molybdenum;
[0033] (3) Dispersing 16 parts of modified organic molybdenum in 98 parts of ethanol, stirring at 500 rpm for 10 min, adding 34 parts of 2 mg / mL graphene aqueous solution, ultrasonicating at 40 ° C and 20 kHz for 1 h, centrifuging at 1800 rpm / min for 10 min, washing twice with 62 parts of water and 62 parts of ethanol alternately, and drying at 50 ° C for 2 h to obtain composite organic molybdenum;
[0034] (4) 7 parts of 3-chlorotoluene hydrazide and 2 parts of potassium hydroxide solid were dissolved in 56 parts of isopropanol, 18 parts of iodoacetamide and 18 parts of toluene were added, and the mixture was reacted at 80° C. for 40 hours. After concentration at -0.1 MPa for 1 hour, 55 parts of dichloromethane and 32 parts of saturated sodium bicarbonate solution were added for extraction and separation three times. The organic phase was concentrated at -0.1 MPa for 1 hour to obtain a composite hydrazide;
[0035] (5) 0.8 parts of potassium iodide and 1.2 parts of potassium carbonate were dissolved in 47 parts of dimethylformamide, 7 parts of 2,5-dimercaptothiadiazole were added, and the mixture was stirred at 600 rpm for 10 min, followed by adding 17 parts of composite hydrazide, reacting at 100° C. for 3 h, cooling naturally to 20° C., washing with 38 parts of water, filtering the filter cake, washing with 21 parts of acetone, and drying at 50° C. for 2 h to obtain a modified wear-resistant agent;
[0036] (6) 12 parts of composite organic molybdenum, 4 parts of modified anti-wear agent, 0.02 parts of T921 and 0.06 parts of D114 were mixed to obtain an extreme pressure anti-wear agent for lubricating oil.
[0037] Example 2
[0038] (1) 30 parts of 2,4-dichlorobenzyl alcohol were dissolved in 39 parts of toluene, 20 parts of phosphorus pentasulfide were added at 50°C, 600 rpm, and under nitrogen protection, the temperature was raised to 90°C, and the reaction was carried out for 3 hours to obtain a phosphoric acid solution;
[0039] (2) After 27.5 parts of sodium molybdate and 45 parts of water were stirred and dissolved, 24 parts of 35% dilute sulfuric acid solution were added to adjust the pH to 1.75, and then 32 parts of phosphoric acid solution were added, the temperature was raised to 90° C., the reaction was performed for 5 hours, the temperature was cooled to 25° C., the filter was suctioned, and the filtrate was rinsed with 65 parts of methanol, and the filtrate was dried at 55° C. for 4 hours to obtain modified organic molybdenum;
[0040] (3) Dispersing 20 parts of modified organic molybdenum in 110 parts of ethanol, stirring at 500 rpm for 20 min, adding 45 parts of 2 mg / mL graphene aqueous solution, ultrasonicating at 50 ° C and 60 kHz for 1.5 h, centrifuging at 1800 rpm / min for 15 min, washing twice with 73 parts of water and 73 parts of ethanol alternately, and drying at 55 ° C for 4 h to obtain composite organic molybdenum;
[0041] (4) 11 parts of 3-chlorotoluhydrazide and 3 parts of potassium hydroxide solid were dissolved in 100 parts of isopropanol, 30 parts of iodoacetamide and 32 parts of toluene were added, and the mixture was reacted at 90° C. for 45 hours. After concentrating at -0.07 MPa for 2 hours, 98 parts of dichloromethane and 50 parts of saturated sodium bicarbonate solution were added and extracted three times. The organic phase was concentrated at -0.07 MPa for 2 hours to obtain a composite hydrazide;
[0042] (5) 1.6 parts of potassium iodide and 1.5 parts of potassium carbonate were dissolved in 55 parts of dimethylformamide, 10 parts of 2,5-dimercaptothiadiazole were added, and the mixture was stirred at 600 rpm for 15 min, followed by adding 20 parts of composite hydrazide, reacting at 110° C. for 4.5 h, and naturally cooling to 25° C., washing with 45 parts of water, filtering the filter cake, washing with 33 parts of acetone, and drying at 55° C. for 4 h to obtain a modified wear-resistant agent;
[0043] (6) 15 parts of composite organic molybdenum, 5 parts of modified anti-wear agent, 0.05 parts of DF667 and 0.10 parts of T1001 were mixed to obtain an extreme pressure anti-wear agent for lubricating oil.
[0044] Example 3
[0045] (1) 35 parts of 2,4-dichlorobenzyl alcohol were dissolved in 46 parts of toluene, and 22 parts of phosphorus pentasulfide were added at 60° C., 600 rpm, and under nitrogen protection. The temperature was raised to 95° C. and the reaction was carried out for 4 hours to obtain a phosphoric acid solution;
[0046] (2) After 34 parts of sodium molybdate and 50 parts of water are stirred and dissolved, 32 parts of 35% dilute sulfuric acid solution are added to adjust the pH to 2.0, and then 39 parts of phosphoric acid solution are added, the temperature is raised to 100° C., the reaction is performed for 6 hours, the mixture is cooled to 30° C., filtered, and then rinsed with 73 parts of methanol, and dried at 60° C. for 6 hours to obtain modified organic molybdenum;
[0047] (3) Dispersing 24 parts of modified organic molybdenum in 122 parts of ethanol, stirring at 500 rpm for 30 min, adding 56 parts of 2 mg / mL graphene aqueous solution, ultrasonicating at 60 ° C and 100 kHz for 2 h, centrifuging at 1800 rpm / min for 20 min, washing twice with 84 parts of water and 84 parts of ethanol alternately, and drying at 60 ° C for 6 h to obtain composite organic molybdenum;
[0048] (4) 15 parts of 3-chlorotoluene hydrazide and 4 parts of potassium hydroxide solid were dissolved in 144 parts of isopropanol, 42 parts of iodoacetamide and 46 parts of toluene were added, and the mixture was reacted at 100° C. for 50 hours. After concentrating at -0.04 MPa for 3 hours, 141 parts of dichloromethane and 68 parts of saturated sodium bicarbonate solution were added and extracted three times. The organic phase was concentrated at -0.04 MPa for 3 hours to obtain a composite hydrazide;
[0049] (5) 2.4 parts of potassium iodide and 1.8 parts of potassium carbonate were dissolved in 63 parts of dimethylformamide, 13 parts of 2,5-dimercaptothiadiazole were added, and the mixture was stirred at 600 rpm for 20 min, followed by adding 23 parts of composite hydrazide, reacting at 120° C. for 6 h, and naturally cooling to 30° C., washing with 52 parts of water, filtering the filter cake, washing with 45 parts of acetone, and drying at 60° C. for 6 h to obtain a modified wear-resistant agent;
[0050] (6) 18 parts of composite organic molybdenum, 6 parts of modified anti-wear agent, 0.08 parts of FS1265 and 0.14 parts of T705 were mixed to obtain an extreme pressure anti-wear agent for lubricating oil.
[0051] Comparative Example 1
[0052] The difference between Comparative Example 1 and Example 2 is that there are no steps (1) and (2), and step (3) is changed to: 20 parts of sodium molybdate are dispersed in 110 parts of ethanol, stirred at 500 rpm for 20 min, 45 parts of 2 mg / mL graphene aqueous solution are added, ultrasonicated at 50° C. and 60 kHz for 1.5 h, centrifuged at 1800 rpm / min for 15 min, washed alternately with 73 parts of water and 73 parts of ethanol twice, and dried at 55° C. for 4 h to obtain composite organic molybdenum. The remaining steps are the same as those in Example 2.
[0053] Comparative Example 2
[0054] The difference between Comparative Example 2 and Example 2 is that there is no step (3). The remaining steps are the same as Example 2.
[0055] Comparative Example 3
[0056] The difference between Comparative Example 3 and Example 2 is that there is no step (1), and step (2) is changed to: 27.5 parts of sodium molybdate and 45 parts of water are stirred and dissolved, and then 24 parts of 35% dilute sulfuric acid solution are added to adjust the pH to 1.75, followed by adding 22 parts of phosphorus pentasulfide and 46 parts of toluene, heating to 90°C, reacting for 5h, cooling to 25°C, filtering, and then rinsing with 65 parts of methanol, and drying at 55°C for 4h to obtain modified organic molybdenum.
[0057] Comparative Example 4
[0058] The difference between Comparative Example 4 and Example 2 is that there is no step (4), and step (5) is changed to: 1.6 parts of potassium iodide and 1.5 parts of potassium carbonate are dissolved in 55 parts of dimethylformamide, 10 parts of 2,5-dimercaptothiadiazole are added, and stirred at 600 rpm for 15 minutes, followed by adding 20 parts of iodoacetamide, reacting at 110° C. for 4.5 hours, cooling naturally to 25° C., washing with 45 parts of water, filtering to obtain the filter cake, washing with 33 parts of acetone, and drying at 55° C. for 4 hours to obtain a modified anti-wear agent. The remaining steps are the same as those in Example 2.
[0059] Comparative Example 5
[0060] The difference between Comparative Example 5 and Example 2 is that there is no step (4), and step (5) is changed to: 1.6 parts of potassium iodide and 1.5 parts of potassium carbonate are dissolved in 55 parts of dimethylformamide, 10 parts of 2,5-dimercaptothiadiazole are added, and stirred at 600 rpm for 15 minutes, followed by adding 20 parts of 3-chlorotoluohydrazide, reacting at 110° C. for 4.5 hours, cooling naturally to 25° C., washing with 45 parts of water, filtering to obtain a filter cake, washing with 33 parts of acetone, and drying at 55° C. for 4 hours to obtain a modified anti-wear agent. The remaining steps are the same as those in Example 2.
[0061] Comparative Example 6
[0062] The difference between Comparative Example 6 and Example 2 is that there is no step (5). Step (6) is changed to: 15 parts of composite organic molybdenum, 5 parts of composite hydrazide, 0.05 parts of DF667, and 0.10 parts of T1001 are mixed to obtain an extreme pressure anti-wear agent for lubricating oil. The remaining steps are the same as those of Example 2.
[0063] Effect example
[0064] Table 1 below shows the performance analysis results of the extreme pressure antiwear agents for lubricating oils using Examples 1 to 3 of the present invention and Comparative Examples 1 to 6.
[0065]
[0066]
[0067] From the comparison of the experimental data of Examples 1, 2, and 3 with Comparative Example 1, it can be found that the introduction of sulfur and phosphorus elements by phosphorus pentasulfide can react with the metal surface to form a lubricating film and reduce wear; from the comparison of the experimental data of Examples 1, 2, and 3 with Comparative Example 2, it can be found that by physically mixing with graphene, organic molybdenum is uniformly attached to the graphene network structure, and when friction occurs, it enters the secondary surface to fill and repair the scratches after wear, and forms a stable oil film to increase wear resistance; from the comparison of the experimental data of Examples 1, 2, and 3 with Comparative Example 3, it can be found that the chlorine group in 2,4-dichlorobenzyl alcohol can react when in contact with the metal surface to form a chemical film to enhance wear resistance; from the comparison of the experimental data of Examples 1, 2, and 3 with Comparative Example 3, it can be found that the chlorine group in 2,4-dichlorobenzyl alcohol can react when in contact with the metal surface to form a chemical film to enhance wear resistance; By comparing the experimental data of Examples 1, 2, and 3 with those of Comparative Example 4, it can be found that 3-chlorotoluohydrazide can effectively inhibit the migration of C element from the base oil to the metal surface, has better stability and can increase the biodegradation rate, and is green and environmentally friendly; by comparing the experimental data of Examples 1, 2, and 3 with those of Comparative Example 5, it can be found that the iodine group of iodoacetamide reacts with the hydrazide structure of 3-chlorotoluohydrazide to form an amide bond, has hydrophobic properties, can reduce liquid penetration, and improve the anti-corrosion effect; by comparing the experimental data of Examples 1, 2, and 3 with those of Comparative Example 6, it can be found that thiadiazole has good biodegradability, and at the same time, the thiol group combines with the chlorine group in the hydrazide to form a CS bond, generates a reaction film with the metal, and improves the lubrication effect.
[0068] It is obvious to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the present invention can be implemented in other specific forms without departing from the spirit or essential features of the present invention. Therefore, the embodiments should be considered as exemplary and non-restrictive in all respects.
Claims
1. An extreme pressure anti-wear agent for lubricating oil, It is characterized in that The extreme pressure anti-wear agent for lubricating oil is prepared by mixing composite organic molybdenum and modified anti-wear agent.
2. The extreme pressure anti-wear agent for lubricating oil according to claim 1, It is characterized in that The composite organic molybdenum is prepared from 2,4-dichlorobenzyl alcohol, phosphorus pentasulfide, sodium molybdate and graphene.
3. The extreme pressure anti-wear agent for lubricating oil according to claim 1, It is characterized in that The modified anti-wear agent is prepared from iodoacetamide, 3-chlorobenzoyl hydrazide and 2,5-dimercaptothiadiazole.
4. A method for preparing an extreme pressure anti-wear agent for lubricating oil, It is characterized in that The method comprises the following preparation steps: (1) Dissolve 25-35 parts of 2,4-dichlorobenzyl alcohol in 32-46 parts of toluene, add 18-22 parts of phosphorus pentasulfide at 40-60°C, 600 rpm, and under nitrogen protection, raise the temperature to 85-95°C, and react for 2-4 hours to obtain a thiophosphoric acid solution; (2) After 21 to 34 parts of sodium molybdate and 40 to 50 parts of water are stirred and dissolved, 16 to 32 parts of dilute sulfuric acid solution are added to adjust to acidity, and then 25 to 39 parts of thiophosphoric acid solution are added, the temperature is raised to 80 to 100° C., the reaction is performed for 4 to 6 hours, the temperature is cooled to 20 to 30° C., the filter is suctioned, and the filtrate is then rinsed with 57 to 73 parts of methanol, and the filtrate is dried at 50 to 60° C. for 2 to 6 hours to obtain modified organic molybdenum; (3) dispersing 16 to 24 parts of modified organic molybdenum in 98 to 122 parts of ethanol, stirring at 500 rpm for 10 to 30 min, adding 34 to 56 parts of an aqueous solution of graphene, ultrasonicating at 40 to 60° C. and 20 to 100 kHz for 1 to 2 h, centrifuging, washing, and drying at 50 to 60° C. for 2 to 6 h to obtain composite organic molybdenum; (4) Dissolve 7 to 15 parts of 3-chlorotoluhydrazide and 2 to 4 parts of potassium hydroxide solid in 56 to 144 parts of isopropanol, add 18 to 42 parts of iodoacetamide and 18 to 46 parts of toluene, react at 80 to 100° C. for 40 to 50 hours, add 55 to 141 parts of dichloromethane and 32 to 68 parts of saturated sodium bicarbonate solution after concentration, extract and separate three times, concentrate the organic phase, and obtain a composite hydrazide; (5) Dissolve 0.8-2.4 parts of potassium iodide and 1.2-1.8 parts of potassium carbonate in 47-63 parts of dimethylformamide, add 7-13 parts of 2,5-dimercaptothiadiazole, stir at 600 rpm for 10-20 min, then add 17-23 parts of composite hydrazide, react at 100-120° C. for 3-6 h, cool naturally to 20-30° C., wash with 38-52 parts of water, filter and take the filter cake, rinse with 21-45 parts of acetone, and dry at 50-60° C. for 2-6 h to obtain a modified wear-resistant agent; (6) 12 to 18 parts of composite organic molybdenum, 4 to 6 parts of modified anti-wear agent, 0.02 to 0.08 parts of defoaming agent, and 0.06 to 0.14 parts of anti-emulsifier are mixed to obtain an extreme pressure anti-wear agent for lubricating oil.
5. A method for preparing an extreme pressure anti-wear agent for lubricating oil according to claim 4, It is characterized in that The concentration of the dilute sulfuric acid in step (2) is 35%, and the acidic pH is 1.5-2.
0.
6. The method for preparing an extreme pressure anti-wear agent for lubricating oil according to claim 4, It is characterized in that The concentration of the graphene aqueous solution in step (3) is 2 mg / mL.
7. The method for preparing an extreme pressure anti-wear agent for lubricating oil according to claim 4, It is characterized in that The centrifugal speed in step (3) is 1800 rpm / min, and the centrifugal time is 10 to 20 min; the cleaning conditions are: 62 to 84 parts of deionized water and 62 to 84 parts of ethanol are alternately rinsed twice.
8. The method for preparing an extreme pressure anti-wear agent for lubricating oil according to claim 4, It is characterized in that The concentration conditions of step (4) are: vacuum degree -0.1MPa to -0.04MPa, and concentration time: 1 to 3h.
9. The method for preparing an extreme pressure anti-wear agent for lubricating oil according to claim 4, It is characterized in that The defoaming agent in step (6) is one or more of T921, DF667, and FS1265.
10. The method for preparing an extreme pressure anti-wear agent for lubricating oil according to claim 4, It is characterized in that The anti-emulsifier in step (6) is one or more of D114, T1001, and T705.
Citation Information
Patent Citations
5-mercapto-1,2,3-thiadiazoles composition and process for preparing the same
CA1238329A
Environment-friendly thiazole compound as well as preparation and application thereof
CN102372681A
2,5-dialkylacetamide-1,3,4-thiadiazole for biodegradable lubricating oil additives, and preparation method thereof
CN106543099A
Preparation method for environmentally-friendly and wear-resistant lubricating oil
CN111088104A
Modified layered anti-wear additive for lubricating oil and preparation method
CN111979013A