Thin film for solving star explosion effect and preparation method thereof
By setting a non-periodic thin metal circuit layer on the surface of the conductive film and performing blackening treatment, the problem of star burst effect in the conductive film is solved, light diffraction interference is reduced, display effect is improved, and production efficiency is improved.
Patent Information
- Application Number
- CN202411251630.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-08
- Publication Date
- 2024-11-29
AI Technical Summary
During use, the diffraction pattern and dazzling cross light (star burst effect) generated by the light passing through the gaps of the metal grid during the use, interfering with vision, and the gentle slope of the metal grid lines will aggravate the light reflection phenomenon.
Set a non-periodic metal thin line layer on the surface of the conductive film, and form a blackened layer on its surface. The nanofiber web film is made by electrospinning technology, and a non-periodic pattern is formed using photoresist etching to fill metal particles , and finally blackening treatment is carried out to reduce the reflectivity of the metal.
Effectively reduce the cross-ray phenomenon caused by light diffraction, improve the display effect, and improve the production efficiency. Through the combination of thin line width and non-periodic patterns, it is difficult to detect the star burst effect, and it can be significantly reduced even under light diffraction conditions. Metal reflectivity.
Smart Images

Figure CN119049763A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of conductive films, and more specifically, to a film and a heating method for solving the starburst effect. Background Art
[0002] At present, conductive films, especially transparent metal mesh films, are widely used in touch screens, shielding film windows, and automobile windshield defoggers. In actual use, when light passes through the gaps in the metal mesh (micrometer level), a diffraction pattern will appear. The light on the diffraction pattern interferes with each other, and inevitably produces dazzling cross light (i.e., starburst effect); if there is a gentle slope on the metal mesh line, the light will be reflected on the metal mesh line, which will also cause the light phenomenon to intensify and interfere with vision. Therefore, in view of the above situation, how to improve the structure of the conductive film to solve the starburst effect has become an important technical problem that needs to be solved by technicians in this field. Summary of the invention
[0003] The present invention discloses a film for solving the starburst effect, comprising a conductive film and a metal circuit layer arranged on the surface of the conductive film; the metal circuit layer comprises a plurality of metal fine wires, and the plurality of metal fine wires are non-periodically distributed on the surface of the conductive film; a blackening layer is arranged on the surface of the metal circuit layer.
[0004] Preferably, the width of the metal fine wire is less than 5 microns.
[0005] Preferably, the blackened layer has a thickness of 1 to 5 micrometers.
[0006] Preferably, the material of the metal circuit layer is copper, silver, aluminum, chromium, nickel, tin or a composite material combination thereof.
[0007] Preferably, the method comprises the following steps:
[0008] Step S1: selecting a transparent substrate, and forming a non-periodically arranged nanofiber mesh on the transparent substrate by electrospinning technology;
[0009] Step S2: coating a layer of photoresist on the conductive film, using the nanofiber web as a mask, and exposing it under ultraviolet light;
[0010] Step S3: selectively etching the uncured photoresist to form grooves of a non-periodic pattern in the photoresist;
[0011] Step S4: filling the grooves with metal particles to form a metal circuit layer with a non-periodic pattern;
[0012] Step S5: washing away the photoresist to expose the metal circuit layer on the surface of the conductive film;
[0013] Step S6: performing a blackening treatment on the surface of the metal circuit layer to form a blackening layer.
[0014] Preferably, in step S4, the metal particles are filled in the grooves by using an electroplating process or a magnetron sputtering coating process.
[0015] The thin film for solving the starburst effect provided by the present invention is provided with a metal circuit layer on the surface of the conductive film. The metal fine wires in the metal circuit layer adopt a thinner line width, which is imperceptible to the human eye. At the same time, the metal fine wires adopt a non-periodic distribution structure to reduce the diffraction phenomenon. The present invention combines a fine line width with a non-periodic pattern, and performs a blackening treatment on the surface of the metal circuit layer. The blackening layer further reduces the metal reflectivity, and the starburst effect is difficult to detect even under the condition of light diffraction, thereby improving the display effect. The preparation method of the present invention is easy to implement, and can efficiently prepare a metal circuit layer with a non-periodic pattern on a conductive film, thereby improving production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0017] Figure 1 The structure of the film for solving the starburst effect of the present invention is schematically shown;
[0018] Figure 2 A schematic diagram of step S1 of the method for preparing a film for solving the starburst effect of the present invention;
[0019] Figure 3 A schematic diagram of step S2 of the method for preparing a film for solving the starburst effect of the present invention;
[0020] Figure 4 A schematic diagram of step S3 of the method for preparing a film for solving the starburst effect of the present invention;
[0021] Figure 5 A schematic diagram of step S4 of the method for preparing a film for solving the starburst effect of the present invention;
[0022] Figure 6 A schematic diagram of step S5 of the method for preparing a film for solving the starburst effect of the present invention;
[0023] Figure 7 A schematic diagram of step S6 of the method for preparing a film for solving the starburst effect of the present invention;
[0024] Figure 8A schematic diagram of each step of the method for preparing a film for solving the starburst effect of the present invention;
[0025] The marks in the drawings are as follows:
[0026] 1--conductive film, 2--metal circuit layer, 3--blackening layer, 4--transparent substrate, 5--nanofiber mesh, 6--photoresist, 7--grooves, 8--metal particles. DETAILED DESCRIPTION
[0027] The present invention discloses a film for solving the starburst effect and a preparation method thereof. A metal circuit layer is arranged on the surface of a conductive film. The metal fine wires in the metal circuit layer adopt a thinner line width, which is imperceptible to the human eye. At the same time, the metal fine wires adopt a non-periodic distribution structure to reduce diffraction. The present invention combines a fine line width with a non-periodic pattern, and performs a blackening treatment on the surface of the metal circuit layer. The blackening layer further reduces the metal reflectivity, and the starburst effect is difficult to detect even under the condition of light diffraction, thereby improving the display effect. In addition, the preparation method of the present invention is easy to implement, and can efficiently prepare a metal circuit layer with a non-periodic pattern on a conductive film, thereby improving production efficiency.
[0028] The following is a clear and detailed description of the technical solutions in the embodiments of the present invention in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0029] See also Figure 1 and Figure 8 The present invention provides a film for solving the starburst effect, comprising a conductive film 1 and a metal circuit layer 2 arranged on the surface of the conductive film 1; the metal circuit layer 2 comprises a plurality of metal fine wires, and the plurality of metal fine wires are non-periodically distributed on the surface of the conductive film 1; a blackening layer 3 is provided on the surface of the metal circuit layer 2.
[0030] In an embodiment of the present invention, a metal circuit layer 2 is prepared on the surface of a conductive film 1, wherein the metal circuit layer 2 is composed of a plurality of metal fine wires, and these metal fine wires are non-periodicly distributed, and the pattern formed by these metal fine wires is a non-periodic pattern. The non-periodic pattern can effectively reduce the mutual interference of light on the diffraction pattern when light passes through the gaps of the metal grid, avoid the generation of cross rays, and thus solve the problem of starburst effect. In addition, a blackening treatment is performed on the circuit surface to form a blackening layer 3 to further reduce the metal reflectivity.
[0031] Preferably, the line width of the metal thin wire is less than 5 micrometers. In order to improve the visual effect, the metal thin wire in this embodiment adopts a very thin line width that cannot be detected by human eyes.
[0032] Preferably, the blackened layer 3 has a thickness of 1 to 5 micrometers.
[0033] Preferably, the material of the metal circuit layer 2 is copper, silver, aluminum, chromium, nickel, tin or a composite material combination thereof.
[0034] Preferably, the method comprises the following steps:
[0035] Step S1: selecting a transparent substrate 4, and forming a non-periodically arranged nanofiber web 5 on the transparent substrate 4 by electrospinning technology;
[0036] Step S2: coating a layer of photoresist 6 on the conductive film 1, using the nanofiber web 5 as a mask, and exposing it under ultraviolet light;
[0037] Step S3: selectively etching the uncured photoresist 6 to form grooves 7 of a non-periodic pattern in the photoresist 6;
[0038] Step S4: filling the grooves 7 with metal particles 8 to form a metal circuit layer 2 with a non-periodic pattern;
[0039] Step S5: washing away the photoresist 6 to expose the metal circuit layer 2 on the surface of the conductive film 1;
[0040] Step S6: performing a blackening treatment on the surface of the metal circuit layer 2 to form a blackening layer 3 .
[0041] In the embodiment of the present invention, a transparent substrate 4 is first selected. The material of the transparent substrate 4 can be a transparent medium such as PET, COP, CPI, etc., and its thickness is usually 50um, 100um, 125um, etc. The nanofiber web 5 is made on the transparent substrate 4 using electrospinning technology, and the pattern formed by the nanofiber web 5 is a non-periodic pattern arranged non-periodically. The purpose of this step is to make a mask that can be used for photolithography;
[0042] Next, a layer of photoresist 6 is coated on the conductive film 1 to be processed, and the photoresist 6 is a photocurable resin. The mask obtained in the previous step is used for exposure. The transparent substrate 4 in the mask is used as a substrate, and the nanofiber mesh film 5 is a light shielding film. When ultraviolet light is used for exposure, the light shielding film blocks part of the ultraviolet light, and the ultraviolet light passing through the light shielding film is projected onto the photoresist 6 and solidifies the photoresist 6; the photoresist 6 is etched by an etching solution, and the uncured part of the photoresist 6 is etched by the etching solution, and after rinsing, a groove 7 showing a non-periodic pattern is obtained. By filling metal particles 8 on the groove 7, a metal circuit layer 2 with a non-periodic pattern has been formed; the residual photoresist 6 on the conductive film 1 is removed, and only the metal circuit layer 2 is left on the surface of the conductive film 1; finally, the metal circuit layer 2 is blackened to form a blackening layer 3 on the surface of the metal circuit layer 2, and the blackening layer 3 is used to further reduce the reflection of the metal surface.
[0043] Through the above steps, the metal circuit layer 2 can be efficiently prepared on the surface of the conductive film 1, and the metal circuit layer 2 can present a non-periodic pattern, effectively reducing the mutual interference of light on the diffraction pattern and avoiding the generation of dazzling cross light (starburst effect).
[0044] Preferably, in step S4 , the metal particles 8 are filled in the groove 7 by using an electroplating process or a magnetron sputtering coating process.
[0045] The thin film for solving the starburst effect provided by the present invention is provided with a metal circuit layer on the surface of the conductive film. The metal fine wires in the metal circuit layer adopt a thinner line width, which is imperceptible to the human eye. At the same time, the metal fine wires adopt a non-periodic distribution structure to reduce the diffraction phenomenon. The present invention combines a fine line width with a non-periodic pattern, and performs a blackening treatment on the surface of the metal circuit layer. The blackening layer further reduces the metal reflectivity, and the starburst effect is difficult to detect even under the condition of light diffraction, thereby improving the display effect. The preparation method of the present invention is easy to implement, and can efficiently prepare a metal circuit layer with a non-periodic pattern on a conductive film, thereby improving production efficiency.
[0046] The above is a detailed introduction to the film for solving the starburst effect provided by the present invention. For those skilled in the art, according to the concept of the embodiments of the present invention, there may be changes in the specific implementation methods and application scopes. In summary, the content of this specification should not be understood as limiting the present invention.
Claims
1. A film for solving the starburst effect, characterized in that: It comprises a conductive film (1) and a metal circuit layer (2) arranged on the surface of the conductive film; the metal circuit layer comprises a plurality of metal fine wires, and the plurality of metal fine wires are distributed non-periodically on the surface of the conductive film; and a blackening layer (3) is provided on the surface of the metal circuit layer.
2. The film for solving the starburst effect according to claim 1, characterized in that: The width of the metal fine wire is less than 5 microns.
3. The film for solving the starburst effect according to claim 2, characterized in that: The thickness of the blackened layer is 1 to 5 micrometers.
4. The film for solving the starburst effect according to claim 1, characterized in that: The material of the metal circuit layer is copper, silver, aluminum, chromium, nickel, tin or a composite material combination thereof.
5. The method for preparing a film for solving the starburst effect according to any one of claims 1 to 4, characterized in that: The following steps are included: Step S1: selecting a transparent substrate (4), and forming a non-periodically arranged nanofiber mesh (5) on the transparent substrate by electrospinning technology; Step S2: coating a layer of photoresist (6) on the conductive film, using the nanofiber web as a mask, and exposing it under ultraviolet light; Step S3: selectively etching the uncured photoresist to form grooves (7) of a non-periodic pattern in the photoresist; Step S4: filling the grooves with metal particles (8) to form a metal circuit layer with a non-periodic pattern; Step S5: washing away the photoresist to expose the metal circuit layer on the surface of the conductive film; Step S6: performing a blackening treatment on the surface of the metal circuit layer to form a blackening layer.
6. The method for preparing a film for solving the starburst effect according to claim 5, characterized in that: In step S4, metal particles are filled in the grooves by using an electroplating process or a magnetron sputtering coating process.