Method for forming eDRAM device
By filling the dielectric and barrier layer materials during the formation of the eDRAM device and grinding on the surface of the liner oxide layer, the etching of the liner nitride layer is reduced, and the problem of loss of the liner nitride layer in the prior art is solved. Improves device quality and subsequent processes.
Patent Information
- Application Number
- CN202411495801.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-25
- Publication Date
- 2024-11-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In the existing eDRAM device formation method, etching the side walls of the polysilicon material layer will cause loss of the liner nitride layer, increasing the difficulty of subsequent STI or Fin patterning, and affecting device quality.
During the formation of the eDRAM device, the dielectric material layer, the barrier material layer and the polysilicon material layer are filled into the deep trench, and the surface of the liner oxide layer is ground to expose the liner nitride layer to reduce the liner nitrogen to the liner nitrogen. The etching of the decomposition layer avoids the etching of the side walls of the polysilicon layer, and forms a high-quality liner nitride layer.
It reduces the difficulty of subsequent STI or Fin patterning, improves the quality of the eDRAM device, and reduces the loss of the nitride layer of the liner.
Smart Images

Figure CN119053152A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a method for forming an eDRAM device. Background Art
[0002] Deep trench capacitors can be formed before MOSFETs without affecting the characteristics of MOSFETs, so DRAM (dynamic random access memory) and logic circuits using deep trench capacitors can be integrated on the same wafer, called eDRAM (embedded DRAM). The memory cell of eDRAM usually includes a deep trench capacitor and a traditional two-dimensional MOSFET or FinFET coupled thereto.
[0003] The prior art method for forming an eDRAM device includes: Figure 1 First, a substrate 110 is provided. The substrate 110 is SOI, including a bottom silicon 111, a buried oxide layer 112 and a top silicon 113 stacked in sequence. A pad nitride layer 120 is formed on the surface of the substrate 110, which can be formed by depositing silicon nitride. Next, a pad oxide layer 130 is formed on the surface of the pad nitride layer 120, which can be formed by depositing silicon oxide. Next, a hard mask layer is formed on the surface of the pad oxide layer 130, and the hard mask layer is etched to form a patterned hard mask layer. The pad oxide layer 130, the pad nitride layer 120 and a portion of the thickness of the substrate 110 are etched downward from the surface of the pad oxide layer 130 using the patterned hard mask layer to form a plurality of deep trenches 140 spaced apart from each other, and the substrate 110 is between adjacent deep trenches 140.
[0004] Next, please refer to Figure 2 , a titanium nitride (TiN) material layer 150 and a high-k dielectric layer 160 are sequentially deposited on the inner wall of the deep trench 140, and a polysilicon material layer 170 is continuously filled in the trench formed by the high-k dielectric layer 160. While filling the deep trench 140, the titanium nitride material layer 150, the high-k dielectric layer 160 and the polysilicon material layer 170 will sequentially cover the surface of the liner oxide layer 130 outside the deep trench 140.
[0005] Next, please refer to Figure 3 The polysilicon material layer 170 on the surface of the pad oxide layer 130 is ground for the first time. Then, the polysilicon material layer 170 on the surface of the pad oxide layer 130 is ground for the second time, and the grinding stops at the surface of the pad oxide layer 130 .
[0006] Next, please refer to Figure 4 and Figure 5, the pad oxide layer 130 is etched away to expose the surface of the pad nitride layer 120. Therefore, the titanium nitride material layer 150 originally located in the deep trench now exposes the sidewall. Next, the titanium nitride material layer 150 is etched away, and then the high-k dielectric layer 160 is etched away to expose the sidewall of the polysilicon material layer 170.
[0007] Next, the protruding polysilicon material layer 170 and part of the polysilicon material layer 170 in the deep trench are etched away, leaving only the polysilicon material layer 170 in the lower deep trench. At this time, a part of the thickness of the liner nitride layer 120 will be etched away. Next, the high-k dielectric layer 160 and the titanium nitride material layer 150 are etched away. Only the high-k dielectric layer 160 and the titanium nitride material layer 150 in the lower deep trench are left. The remaining high-k dielectric layer 160 and the titanium nitride material layer 150 are flush with the remaining polysilicon material layer 170. Next, the polysilicon material layer is continued to be filled into the deep trench. The newly filled polysilicon material layer and the remaining polysilicon material layer form a polysilicon layer, and the polysilicon layer fills the deep trench. Next, a groove is formed between adjacent deep trenches, and the groove exposes part of the polysilicon layer in the deep trench and the substrate between adjacent trenches. Next, a linear oxide layer and a dielectric layer are sequentially formed in the groove, and the dielectric layer is separated by the linear oxide layer and the polysilicon layer.
[0008] However, in the prior art, etching the high-k dielectric layer 160 and the titanium nitride material layer 150 as the sidewalls of the polysilicon material layer 170 will cause the pad nitride layer 120 to be damaged. In the subsequent high-performance logic process with embedded eDRAM, it is hoped that the pad nitride layer same as the deep trench process is shared as a hard mask for subsequent STI or Fin patterning. Therefore, after the pad nitride layer is damaged, it will increase the difficulty in forming the STI or Fin patterning later. Summary of the invention
[0009] The object of the present invention is to provide a method for forming an eDRAM device, which can form a high-quality liner nitride layer, thereby reducing the difficulty of subsequent STI or Fin patterning, and finally improving the quality of the eDRAM device.
[0010] In order to achieve the above object, the present invention provides a method for forming an eDRAM device, comprising: Providing a substrate, and sequentially forming a pad nitride layer and a pad oxide layer on the surface of the substrate; Etching the pad oxide layer, the pad nitride layer and a portion of the thickness of the substrate to form a plurality of deep trenches spaced apart from each other; Filling the deep trench with a dielectric material layer, a barrier material layer and a polysilicon material layer in sequence, wherein the dielectric material layer, the barrier material layer and the polysilicon material layer cover the surface of the liner oxide layer in sequence; Grinding the dielectric material layer, the barrier material layer, the polysilicon material layer and the pad oxide layer on the surface of the pad oxide layer to expose the pad nitride layer; removing the polysilicon material layer in the upper deep trench; Removing the dielectric material layer and the barrier material layer in the deep trench of the upper portion, the remaining dielectric material layer constitutes a dielectric layer, and the remaining barrier material layer serves as a barrier layer; A polysilicon material layer is filled in the upper portion of the deep trench, and all of the polysilicon material layer serves as a polysilicon layer.
[0011] Optionally, in the method for forming the eDRAM device, after the upper portion of the deep trench is filled with a polysilicon material layer and all the polysilicon material layers are used as polysilicon layers, the method further includes: forming grooves between adjacent deep trenches, wherein the grooves expose the polysilicon layer in a portion of the deep trenches and the substrate between adjacent deep trenches; A linear oxide layer and a dielectric layer are sequentially formed in the groove, and the dielectric layer is separated by the linear oxide layer and the polysilicon layer.
[0012] Optionally, in the method for forming the eDRAM device, the polysilicon material layer in the upper portion of the deep trench is etched away.
[0013] Optionally, in the method for forming the eDRAM device, the dielectric material layer and the barrier material layer in the upper portion of the deep trench are removed by etching, and the remaining dielectric material layer constitutes a dielectric layer, and the remaining barrier material layer serves as a barrier layer.
[0014] Optionally, in the method for forming the eDRAM device, the dielectric material layer, the barrier material layer, the polysilicon material layer and the pad oxide layer on the surface of the pad oxide layer are chemically mechanically polished to expose the pad nitride layer.
[0015] Optionally, in the method for forming the eDRAM device, the substrate includes a bottom silicon layer, a buried oxide layer, and a top silicon layer stacked in sequence.
[0016] Optionally, in the method for forming the eDRAM device, the pad nitride layer includes silicon nitride.
[0017] Optionally, in the method for forming the eDRAM device, the pad oxide layer includes silicon oxide.
[0018] Optionally, in the method for forming the eDRAM device, the dielectric layer includes a high-k dielectric layer.
[0019] Optionally, in the method for forming the eDRAM device, the barrier layer includes TiN.
[0020] The method for forming an eDRAM device provided by the present invention includes: providing a substrate, sequentially forming a liner nitride layer and a liner oxide layer on the surface of the substrate; etching the liner oxide layer, the liner nitride layer and a part of the thickness of the substrate to form a plurality of deep grooves spaced apart; sequentially filling a dielectric material layer, a barrier layer material layer and a polysilicon material layer into the deep grooves, wherein the dielectric material layer, the barrier layer material layer and the polysilicon material layer sequentially cover the surface of the liner oxide layer; grinding the dielectric material layer, the barrier layer material layer and the polysilicon material layer and the liner oxide layer on the surface of the liner oxide layer to expose the liner nitride layer; removing the polysilicon material layer in the upper deep trench; removing the dielectric material layer and the barrier layer material layer in the upper deep trench, wherein the remaining dielectric material layer constitutes a dielectric layer, and the remaining barrier layer material layer serves as a barrier layer; filling the upper deep trench with a polysilicon material layer, wherein all the polysilicon material layers serve as polysilicon layers. The present invention stops grinding to the nitrided surface of the pad, does not etch the dielectric material layer and the barrier material layer of the side wall of the polysilicon layer, and reduces the etching amount of the dielectric material layer and the barrier material layer. Thus, the amount of loss of the nitrided pad layer is reduced, the difficulty of subsequent STI or Fin patterning is reduced, and the quality of the eDRAM device is improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 is a schematic diagram of the structure of an eDRAM device after deep trenches are formed in the prior art; Figure 2 is a schematic diagram of the structure of an eDRAM device after a polysilicon material layer is formed in the prior art; Figure 3 It is a schematic diagram of the structure of an eDRAM device after grinding the titanium nitride material layer in the prior art; Figure 4 It is a schematic diagram of the structure of an eDRAM device after removing the titanium nitride material layer on the sidewall in the prior art; Figure 5 It is a schematic diagram of the structure of an eDRAM device after removing the sidewall high-k dielectric layer in the prior art; Figure 6 It is a schematic diagram of the structure of an eDRAM device after removing the polysilicon material layer in the upper deep trench of the prior art; Figure 7 It is a schematic diagram of the structure of an eDRAM device after removing the titanium nitride material layer and the high-k dielectric layer in the upper deep trench of the prior art; Figure 8 is a flow chart of a method for forming an eDRAM device according to an embodiment of the present invention; Fig. 9 is a schematic structural diagram of an eDRAM device after deep trenches are formed according to an embodiment of the present invention; Fig.10is a schematic structural diagram of an eDRAM device after a polysilicon material layer is formed according to an embodiment of the present invention; Fig.11 is a schematic structural diagram of an eDRAM device after removing the pad nitride layer according to an embodiment of the present invention; Fig.12 is a schematic structural diagram of an eDRAM device after removing the polysilicon material layer in the upper deep trench according to an embodiment of the present invention; Fig.13 is a schematic structural diagram of an eDRAM device after a polysilicon layer is formed according to an embodiment of the present invention; In the figure: 110-substrate, 111-bottom silicon, 112-buried oxide layer, 113-top silicon, 120-pad nitride layer, 130-pad oxide layer, 140-deep trench, 150-titanium nitride material layer, 160-high-k dielectric layer, 170-polysilicon material layer, 210-substrate, 211-bottom silicon, 212-buried oxide layer, 213-top silicon, 220-pad nitride layer, 230-pad oxide layer, 240-deep trench, 250-titanium nitride material layer, 260-high-k dielectric layer, 270-polysilicon material layer, 280-polysilicon layer. DETAILED DESCRIPTION
[0022] The specific implementation of the present invention will be described in more detail below in conjunction with the schematic diagram. The advantages and features of the present invention will become clearer based on the following description. It should be noted that the drawings are all in a very simplified form and are not in exact proportions, and are only used to facilitate and clearly assist in explaining the purpose of the embodiments of the present invention.
[0023] Hereinafter, the terms "first", "second", etc. are used to distinguish between similar elements and are not necessarily used to describe a particular order or chronological sequence. It is to be understood that these terms used in this manner are interchangeable where appropriate. Similarly, if the method described herein includes a series of steps, the order of these steps presented herein is not necessarily the only order in which these steps can be performed, and some of the steps described may be omitted and / or some other steps not described herein may be added to the method.
[0024] Furthermore, it should be understood that when a layer (or film), region, pattern or structure is referred to as being "on" a substrate, layer (or film), region and / or pattern, it can be directly on another layer or substrate, and / or there can be intervening layers. In addition, it should be understood that when a layer is referred to as being "under" another layer, it can be directly under another layer, and / or there can be one or more intervening layers. In addition, references to being "on" and "under" each layer can be made based on the accompanying drawings.
[0025] Please refer to Figure 8 The present invention provides a method for forming an eDRAM device, comprising: S11: providing a substrate, and sequentially forming a pad nitride layer and a pad oxide layer on a surface of the substrate; S12: etching the pad oxide layer, the pad nitride layer and a portion of the thickness of the substrate to form a plurality of deep trenches spaced apart; S13: filling the deep trench with a dielectric material layer, a barrier material layer, and a polysilicon material layer in sequence, and the dielectric material layer, the barrier material layer, and the polysilicon material layer cover the surface of the liner oxide layer in sequence; S14: grinding the dielectric material layer, the barrier material layer, the polysilicon material layer and the pad oxide layer on the surface of the pad oxide layer to expose the pad nitride layer; S15: removing the polysilicon material layer in the upper deep trench; S16: removing the dielectric material layer and the barrier layer material layer in the upper deep trench, the remaining dielectric material layer constitutes a dielectric layer, and the remaining barrier layer material layer serves as a barrier layer; S17: Filling the upper part of the deep trench with a polysilicon material layer, and all the polysilicon material layers serve as polysilicon layers.
[0026] Please refer to Fig. 9 First, a substrate 210 is provided. The substrate 210 is SOI, including a bottom silicon 211, a buried oxide layer 212 and a top silicon 213 stacked in sequence. A pad nitride layer 220 is formed on the surface of the substrate 210, which can be formed by depositing silicon nitride. Next, a pad oxide layer 230 is formed on the surface of the pad nitride layer 220, which can be formed by depositing silicon oxide. Next, a hard mask layer is formed on the surface of the pad oxide layer 230, and the hard mask layer is etched to form a patterned hard mask layer. The pad oxide layer 230, the pad nitride layer 220 and a partial thickness of the substrate 210 are etched downward from the surface of the pad oxide layer 230 using the patterned hard mask layer to form a plurality of deep trenches 240 spaced apart, and the substrate 210 is between adjacent deep trenches 240.
[0027] Next, please refer to Fig.10 , a titanium nitride (TiN) material layer 250 and a high-k dielectric layer 260 are sequentially deposited on the inner wall of the deep trench 240, and a polysilicon material layer 270 is continuously filled in the trench formed by the high-k dielectric layer 260. While filling the deep trench 240, the titanium nitride material layer 250, the high-k dielectric layer 260 and the polysilicon material layer 270 sequentially cover the surface of the liner oxide layer 230 outside the deep trench 240.
[0028] Next, please refer to Fig.11 The polysilicon material layer 270 , the high-k dielectric layer 260 , the titanium nitride material layer 250 and the pad oxide layer 130 on the surface of the pad nitride layer 120 are removed in sequence by one-time grinding to expose the surface of the pad nitride layer 220 .
[0029] Next, please refer to Fig.12 , the polysilicon material layer in the upper deep trench is etched, and then the high-k dielectric layer 260 and the titanium nitride material layer 250 in the upper deep trench are removed to expose the upper deep trench.
[0030] Next, please refer to Fig.13 , the remaining high-k dielectric layer 260 and the titanium nitride material layer 250 are flush with the remaining polysilicon material layer 270. Then, the polysilicon material layer is continued to be filled into the deep trench. The newly filled polysilicon material layer and the remaining polysilicon material layer form a polysilicon layer 280, and the polysilicon layer fills the deep trench. Then, grooves are formed between adjacent deep trenches, and the grooves expose part of the polysilicon layer in the deep trenches and the substrate between adjacent trenches. Then, a linear oxide layer and a dielectric layer are formed in sequence in the grooves, and the dielectric layer is separated by the linear oxide layer and the polysilicon layer.
[0031] In summary, the method for forming an eDRAM device provided in an embodiment of the present invention includes: providing a substrate, and sequentially forming a pad nitride layer and a pad oxide layer on the surface of the substrate; etching the pad oxide layer, the pad nitride layer and a portion of the thickness of the substrate to form a plurality of deep trenches at intervals; sequentially filling a dielectric material layer, a barrier layer material layer and a polysilicon material layer into the deep trenches, and the dielectric material layer, the barrier layer material layer and the polysilicon material layer sequentially cover the surface of the pad oxide layer; grinding the dielectric material layer, the barrier layer material layer and the polysilicon material layer and the pad oxide layer on the surface of the pad oxide layer to expose the pad nitride layer; removing the polysilicon material layer in the upper portion of the deep trench; removing the dielectric material layer and the barrier layer material layer in the upper portion of the deep trench, the remaining dielectric material layer constitutes a dielectric layer, and the remaining barrier layer material layer serves as a barrier layer; filling the polysilicon material layer into the upper portion of the deep trenches, and all the polysilicon material layers serve as polysilicon layers. The present invention stops grinding to the nitrided surface of the pad, does not etch the dielectric material layer and the barrier material layer of the side wall of the polysilicon layer, and reduces the etching amount of the dielectric material layer and the barrier material layer. Thus, the amount of loss of the nitrided pad layer is reduced, the difficulty of subsequent STI or Fin patterning is reduced, and the quality of the eDRAM device is improved.
[0032] The above is only a preferred embodiment of the present invention and does not limit the present invention in any way. Any technician in the relevant technical field, without departing from the scope of the technical solution of the present invention, makes any form of equivalent replacement or modification to the technical solution and technical content disclosed in the present invention, which does not depart from the content of the technical solution of the present invention and still falls within the protection scope of the present invention.
Claims
1. A method for forming an eDRAM device, characterized in that: include: Providing a substrate, and sequentially forming a pad nitride layer and a pad oxide layer on the surface of the substrate; Etching the pad oxide layer, the pad nitride layer and a portion of the thickness of the substrate to form a plurality of deep trenches spaced apart from each other; Filling the deep trench with a dielectric material layer, a barrier material layer and a polysilicon material layer in sequence, wherein the dielectric material layer, the barrier material layer and the polysilicon material layer cover the surface of the liner oxide layer in sequence; Grinding the dielectric material layer, the barrier material layer, the polysilicon material layer and the pad oxide layer on the surface of the pad oxide layer to expose the pad nitride layer; removing the polysilicon material layer in the upper deep trench; Removing the dielectric material layer and the barrier material layer in the deep trench of the upper portion, the remaining dielectric material layer constitutes a dielectric layer, and the remaining barrier material layer serves as a barrier layer; A polysilicon material layer is filled in the upper portion of the deep trench, and all of the polysilicon material layer serves as a polysilicon layer.
2. The method for forming an eDRAM device according to claim 1, wherein: After the upper part of the deep trenches is filled with a polysilicon material layer and all the polysilicon material layers are used as polysilicon layers, the method further includes: forming grooves between adjacent deep trenches, wherein the grooves expose the polysilicon layer in a part of the deep trenches and the substrate between adjacent deep trenches; A linear oxide layer and a dielectric layer are sequentially formed in the groove, and the dielectric layer is separated by the linear oxide layer and the polysilicon layer.
3. The method for forming an eDRAM device according to claim 1, wherein: The polysilicon material layer in the upper portion of the deep trench is removed by etching.
4. The method for forming an eDRAM device according to claim 1, wherein: The dielectric material layer and the barrier layer material layer in the upper portion of the deep trench are removed by etching, and the remaining dielectric material layer constitutes a dielectric layer, and the remaining barrier layer material layer serves as a barrier layer.
5. The method for forming an eDRAM device according to claim 1, wherein: The dielectric material layer, the barrier material layer, the polysilicon material layer and the pad oxide layer on the surface of the pad oxide layer are chemically and mechanically polished to expose the pad nitride layer.
6. The method for forming an eDRAM device according to claim 1, wherein: The substrate comprises a bottom silicon layer, a buried oxide layer and a top silicon layer which are stacked in sequence.
7. The method for forming an eDRAM device according to claim 1, wherein: The pad nitride layer includes silicon nitride.
8. The method for forming an eDRAM device according to claim 1, wherein: The pad oxide layer includes silicon oxide.
9. The method for forming an eDRAM device according to claim 1, wherein: The dielectric layer includes a high-k dielectric layer.
10. The method for forming an eDRAM device according to claim 1, wherein: The barrier layer includes TiN.
Citation Information
Patent Citations
Multi-sandwich structure for deep trench filling
CN115863250A
Preparation method of eDRAM
CN118382294A
Manufacturing method of semiconductor device
CN118658782A
IC with deep trench polysilicon oxidation
US20210134602A1
Multi-layer hard mask for deep trench silicon etch
US6440858B1