Solar photovoltaic cell welding method
Through transparent pressing tools and laser local heating welding methods, the problem of low welding and welding accuracy in traditional welding is solved, and the repair of dummy welding after high-quality welding and packaging is achieved, which improves welding accuracy and quality.
Patent Information
- Application Number
- CN202411292389.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-14
- Publication Date
- 2024-12-03
AI Technical Summary
There are problems with false welding during welding of traditional solar photovoltaic cells, including misalignment of welding wire, untied bonding, expansion and twisting after heating, pulling and desoldering after cooling, and local temperature too low, resulting in low welding quality and false after packaging. The welding cannot be repaired by heating.
The local heating welding method is adopted that combines transparent pressing tools and laser. The transparent pressing tools cover the welding wire and apply pressure. The laser scans the welding wire along the welding wire to generate heat, so that the solder melts, ensuring that the welding wire and the battery are in full contact and maintaining pressure to achieve welding. .
It realizes full bonding contact between the welding wire and the battery cell during welding, avoids dummy welding, improves welding quality and accuracy, local heating reduces the expansion and cooling of the welding wire, and allows dummy welding and rework after lamination of the components without secondary heating, affecting the components. Function.
Smart Images

Figure CN119057165A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of photovoltaics, in particular to a solar photovoltaic cell welding method. Background Art
[0002] Solar photovoltaic cells have low voltage and high current characteristics. Cells are generally connected in series by tinned copper wire (also called welding wire). The base material of the welding wire is copper, and the outer surface is tin alloy. The welding wire is in contact with the metal electrode of the cell. The metal electrode material is generally silver. After heating, the tin alloy melts and infiltrates the surface of the metal electrode. After cooling, it fuses into one, forming a weld with strong welding adhesion and high reliability.
[0003] The conditions for achieving good welding are that the temperature is higher than the melting point of the tin alloy and the welding materials are in full contact. The welding process is a process of heating and then cooling. Infrared heating is generally used in photovoltaic cell welding. In addition, in order to make the welding wire fully contact with the battery cell electrode, a pressing tool such as a pressing block or a pressing mesh is generally added above the welding wire. However, the pressing tool will block part of the infrared light, so the pressing tool cannot be completely pressed on the welding wire. During the welding heating process, the welding wire is heated as a whole, and it will expand and stretch after heating, and shrink after cooling. The main causes of cold welding are misalignment, lack of compaction, expansion after heating causing the welding wire to twist and arch, cooling and shrinkage pulling and desoldering, and local temperature is too low. In addition, after the battery cell packaging and lamination, the cold welding inside the component cannot be heated and repaired. Summary of the invention
[0004] The purpose of the present invention is to provide a solar photovoltaic cell welding method to solve the above-mentioned problems existing in the traditional cell sheet welding process.
[0005] To achieve the above object, the present invention provides the following technical solutions: A solar photovoltaic cell welding method comprises the following steps: S1. Provide a battery cell and a welding wire, so that the welding surface of the welding wire is aligned with the surface to be welded of the battery cell, and there is sufficient solder between the welding surface of the welding wire and the surface to be welded of the battery cell; S2, providing a transparent pressing tool, wherein the transparent pressing tool is transparent to the laser used for welding; S3, making the transparent press at least partially cover the battery cell to which the welding wire has been attached from the direction of the welding wire layer, and applying pressure to the transparent press so that at least the welding wire and the battery cell in the area to be welded are compacted; S4, providing a laser, which can pass through the transparent press to reach the battery cell and generate heat at the irradiated part of the battery cell; S5, using the laser to scan the welding wire of the to-be-welded area of the battery cell from the direction of the press, so that the irradiated part of the welding wire generates heat sufficient to be conducted to the solder layer and melt the solder; S6. Maintaining the pressure at the welding position for at least the time required for the battery cell and the welding wire to be welded.
[0006] Preferably, the transparent pressing tool comprises a contact layer and a free layer, wherein the contact layer is in contact with the battery sheet, and the free layer faces the direction receiving laser irradiation.
[0007] Furthermore, the contact layer is a flexible layer, and the free layer is a hard layer.
[0008] More preferably, the contact layer is made of highly transparent plastic or transparent rubber, and the free layer is made of glass or organic glass.
[0009] In addition, preferably, the laser scanning is a local linear scanning along the direction of the welding wire.
[0010] Furthermore, the local linear scanning is single-beam laser point scanning or multi-beam laser combined area scanning.
[0011] Compared with the prior art, the present invention has the following beneficial effects: 1. The method of the present invention combines the method of local heating of the metal welding wire with the transparent pressing tool and the laser, so that the welding wire and the metal electrode of the battery cell are in a state of full contact during the entire welding process, so that there is no false welding during the welding process. The welding is completely heated under the condition of pressing. When the temperature reaches above the tinning temperature, welding can be achieved, thereby improving the welding quality; 2. The welding wire is heated locally instead of as a whole. Except for the high temperature at the welding point, other parts of the welding wire and other parts of the battery cell are at room temperature, which will not cause thermal effects, expansion and distortion, cooling and pulling off on the welding wire and other materials, and also improve the welding quality; 3. It can realize the repair of cold solder joints after component lamination without secondary heating of components and does not affect the normal function of components; 4. High welding precision. During the welding process, the welding wire is first aligned with the metal electrode of the battery cell and then pressed and welded. During the welding process, the battery cell does not produce mechanical displacement. The laser needs to heat the welding wire. The laser's travel path must be in a fixed position. The fixed welding position is not easy to shift after pressing and will not shift after welding. The welding precision is higher than that of traditional infrared welding methods. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Figure 1 It is a schematic diagram of the method of the present invention.
[0013] In the figure: 1. Battery cell; 2. Metal electrode; 3. Round welding wire; 4. Triangular welding wire; 5. Flexible layer; 6. Hard layer; 7. Laser. DETAILED DESCRIPTION
[0014] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0015] In the description of the present invention, it should be noted that the terms "upper", "lower", "inner", "outer", "front end", "rear end", "two ends", "one end", "the other end" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance.
[0016] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "provided with", "connected", etc. should be understood in a broad sense. For example, "connected" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0017] With regard to the many deficiencies existing in the traditional welding method mentioned in the background technology, this solution provides a method of laser local heating welding, which can solve the above problems.
[0018] In the method of the present invention, a transparent press is used above the battery cell 1 and the welding wire layer to compact the welding wire and the battery cell metal electrode 2 as a whole, and then a laser 7 is used to penetrate the upper transparent press layer directly onto the welding wire, and smoothly slides along the direction of the welding wire to heat it, so that the welding wire always maintains complete contact and fit with the battery cell metal electrode during the process of laser heating and cooling after the laser passes.
[0019] See also Figure 1 The welding wire used can be a round welding wire 3, a triangular welding wire 4 or a flat welding wire. Although only round welding wire and triangular welding wire are shown in the figure, it should be understood that the welding wire structure in the figure is only used as an example. In specific use, any welding wire that can be used for welding is within the protection scope of the present invention.
[0020] In the method of the present invention, laser welding is local high-temperature welding. During the welding process, only the part irradiated by the laser is at a high temperature, and the other parts of the welding wire are at room temperature. Therefore, the welding wire is not heated as a whole, and the heating process does not cause thermal expansion of the welding wire. Among them, the laser scanning method can be a single laser beam scanning back and forth multiple times or multiple laser beams scanning at the same time, and the welding point temperature and welding quality are adjusted by controlling the laser power output and scanning speed. For example, a single laser beam linear scanning can be used, which can be adjusted to a higher laser output power and a slower scanning speed to achieve one-time forming, or it can be adjusted to a lower laser output power and a higher scanning speed to scan back and forth multiple times. Multiple laser beams can also be used for linear scanning in sequence, and the intervals between the multiple laser beams can be designed in a certain configuration according to requirements to achieve higher production efficiency.
[0021] In the method of the present invention, in order to fully press the transparent pressing tool and the welding wire, the following steps can be performed: Figure 1 As shown, the transparent press is made into at least a double-layer structure, wherein the contact surface with the battery cell is designed to be a flexible layer 5 so that the welding wire can be pressed more fully. The material used for the flexible layer can be EVA, rubber and other flexible materials. The upper part of the transparent press is the free surface, which is a hard layer 6 to achieve better protection and light transmittance. The material used for the hard layer can be glass, acrylic and other hard materials.
[0022] By adopting the method of the present invention, during the welding process, the battery cell has no mechanical displacement, so the welding wire is in contact with the metal electrode of the battery cell and pressed without deviation. During the heating fusion and cooling solidification process, the welding wire does not deviate from the original fixed position. The welding accuracy is only determined by the placement position between the welding wire and the battery cell. The welding accuracy is higher than that of traditional welding methods.
[0023] In addition to being applied to the initial welding of photovoltaic cells, the method of the present invention can also be applied to the repair of cold solder joints after the cells are packaged into components. The component packaging materials are generally transparent hot melt adhesive films and tempered glass. If cold solder joints occur after the components are laminated, the cold solder joints can no longer be welded by heating the whole body. Through the method of the present invention, the component packaging materials are regarded as the transparent press used in the method of the present invention, and the cold solder joints can be heated locally by laser without contact, so that the tin alloy at the position of the cold solder joints is melted and then solidified and combined, so that the cold solder joints are reconnected.
[0024] In summary, by adopting the method of the present invention, combined with the method of local heating of the metal welding wire by a transparent press and laser, the welding wire and the metal electrode of the battery cell are in a state of full fitting contact during the entire welding process, thereby improving the welding quality; at the same time, the use of laser local heating, this non-traditional overall heating method, has little thermal impact on the welding wire, and basically no thermal expansion and contraction, expansion and distortion, etc.; this method can also be used to repair the cold solder joints of the components after laminated packaging without causing the impact of secondary heating of the components; this method can be applied to welding wires of various structures, such as circular, triangular and other structural welding wires.
[0025] The matters not described in detail in the present invention are all known technologies to those skilled in the art.
[0026] Finally, it should be noted that the above specific implementation methods are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified and replaced by equivalents without departing from the spirit and scope of the technical solution of the present invention, which should be included in the scope of the claims of the present invention.
Claims
1. A solar photovoltaic cell welding method, characterized in that: The method comprises the following steps: S1. Provide a battery cell and a welding wire, so that the welding surface of the welding wire is aligned with the surface to be welded of the battery cell, and there is sufficient solder between the welding surface of the welding wire and the surface to be welded of the battery cell; S2, providing a transparent pressing tool, wherein the transparent pressing tool is transparent to the laser used for welding; S3, making the transparent press at least partially cover the battery cell to which the welding wire has been attached from the direction of the welding wire layer, and applying pressure to the transparent press so that at least the welding wire and the battery cell in the area to be welded are compacted; S4, providing a laser, which can pass through the transparent press to reach the battery cell and generate heat at the irradiated part of the battery cell; S5, using the laser to scan the welding wire of the to-be-welded area of the battery cell from the direction of the press, so that the irradiated part of the welding wire generates heat sufficient to be conducted to the solder layer and melt the solder; S6. Maintaining the pressure at the welding position for at least the time required for the battery cell and the welding wire to be welded.
2. The solar photovoltaic cell welding method according to claim 1, characterized in that: The transparent pressing tool comprises a contact layer and a free layer, wherein the contact layer contacts the battery sheet, and the free layer faces the direction receiving laser irradiation.
3. The solar photovoltaic cell welding method according to claim 2, characterized in that: The contact layer is a flexible layer and the free layer is a hard layer.
4. The solar photovoltaic cell welding method according to claim 3, characterized in that: The contact layer is made of highly transparent plastic or transparent rubber, and the free layer is made of glass or organic glass.
5. The solar photovoltaic cell welding method according to claim 1, characterized in that: The laser scanning is a local linear scan along the direction of the welding wire.
6. The solar photovoltaic cell welding method according to claim 5, characterized in that: The local linear scanning is single-beam laser point scanning or multi-beam laser combined area scanning.
Citation Information
Cited By
Photovoltaic module manufacturing process
CN119767870A