Aluminum alloy profile and preparation method thereof

Through strict quality inspection and pretreatment of aluminum rods, extrusion into serrated profiles, aging and local annealing treatment, the problems of breaking and orange peel of aluminum alloy profiles during bending are solved, and the mechanical properties of the profiles are improved and bending performance, meet the high requirements of train windshield.

CN119187272APending Publication Date: 2024-12-27JIANGSU KAILUN ALUMINUM
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411521873.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-29
Publication Date
2024-12-27

AI Technical Summary

Technical Problem

Aluminum alloy profiles are prone to fracture and orange peel during bending, which is difficult to meet both strength and bending needs.

Method used

Through strict aluminum rod quality inspection and pretreatment, the profile with serrated cross-section is extruded into a profile with artificial aging and local annealing. Combined with comprehensive quality inspection and process parameter optimization, the mechanical and bending performance of the profile is ensured. .

Benefits of technology

The tensile strength, yield strength and fatigue life of the profile are improved, ensuring that there are no cracks or deformations in the bent parts, meeting the needs of complex application scenarios, and the stability and consistency of the product are achieved through refined control.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119187272A_ABST
    Figure CN119187272A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of aluminum profile machining, in particular to an aluminum alloy profile and a preparation method thereof.The preparation method comprises the following operation steps that S1, purchased aluminum bars are subjected to quality inspection including chemical component analysis, mechanical property testing and surface quality inspection, the aluminum bars with proper chemical components and subjected to basic quality control are selected, and the selected aluminum bars are subjected to surface quality inspection; the aluminum bar is pretreated; s2, the aluminum bar is placed in an extruding machine to be extruded, and a primary sectional material is obtained; checking that the appearance and the size meet the requirements; s3, the profile is subjected to artificial aging treatment; and then cutting a proper length according to application requirements, and bending at a corresponding position. S4, quality detection is conducted on the treated profile; and S5, surface treatment is conducted on the profile qualified through quality detection, and the aluminum alloy profile meeting the use standard is obtained.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of aluminum profile processing, and in particular to an aluminum alloy profile and a preparation method thereof. Background Art

[0002] With the continuous development of high-speed train technology and the increasing requirements of passengers for riding comfort, the design, manufacturing and process requirements of train windshields, as important components that connect various carriages and ensure the safety and comfort of passengers, are becoming increasingly higher. The train windshield is mainly composed of a pressure-resistant double-layer folding shed and a lip-shaped windshield frame fixed to the ends of the two carriages by spinning. This design not only requires the windshield to have good air tightness, sound insulation and weather resistance, but also to be able to withstand the strong vibration, wind pressure and complex and changeable environmental changes generated by high-speed trains during driving.

[0003] As the core part of the train windshield, the double-layer bellows is usually made of two layers of flexible materials (such as polyester fabric, polyethylene composite, etc.) connected by a specific process to form a light and strong structure. In order to ensure that the double-layer bellows can fit together tightly to form an integral structure and effectively resist the erosion of the external environment, aluminum alloy profiles are usually set between the double-layer bellows as support and connection parts.

[0004] Aluminum alloy profiles play a vital role in train windshields. Not only do they need to have sufficient strength and hardness to support the double-layer bellows and withstand various mechanical loads during train travel, they also need to have good bending performance to adapt to the special settings of the windshield structure. In particular, a 90° bend is required to meet the geometric shape and installation requirements of the windshield. However, the bending process of aluminum alloy profiles is not easy. Theoretically, the higher the strength, the greater the probability of fracture and orange peel during bending. Therefore, it is necessary to find a method that can ensure strength while meeting bending requirements.

[0005] The information disclosed in this background technology section is only intended to deepen the understanding of the overall background technology of the present invention, and should not be regarded as acknowledging or suggesting in any form that the information constitutes the prior art known to those skilled in the art. Summary of the invention

[0006] The technical problem to be solved by the present invention is to provide a method for preparing an aluminum alloy profile, which can ensure strength and meet bending requirements through process optimization.

[0007] In order to achieve the above object, the technical solution adopted by the present invention is: A method for preparing an aluminum alloy profile comprises the following steps: S1: Conduct quality inspection on purchased aluminum bars, including chemical composition analysis, mechanical property test and surface quality inspection, select aluminum bars with suitable chemical composition and basic quality control, and pre-treat the aluminum bars; S2: Place the aluminum rod in an extruder to extrude it to obtain a preliminary profile; and check that the appearance and size meet the requirements; S3: Perform artificial aging treatment on the profile; then cut the profile to a suitable length according to application requirements and bend it at the corresponding position; S4: Conduct quality inspection on the processed profiles; S5: Surface treatment is performed on the profiles that have passed the quality inspection to obtain aluminum alloy profiles that meet the use standards.

[0008] Furthermore, in step S1, the selection of aluminum rods with suitable chemical composition and basic quality control is dynamically adjusted based on the quality inspection information of the aluminum alloy profiles produced in the previous batch. The pretreatment includes removing the oxide layer, oil stains and impurities, which can be completed by pickling or alkali washing to ensure that no surface defects will occur during the extrusion process.

[0009] Furthermore, in step S2, the aluminum rod is heated to 400-500°C, cut and divided according to the amount of the profile, and then sent to the extruder for extrusion. During the extrusion process, the aluminum rod passes through the cavity of the mold and is extruded into a profile with a serrated cross-section; the extrusion speed and temperature are controlled to ensure the dimensional accuracy and surface quality of the profile.

[0010] Furthermore, in step S3, artificial aging treatment refers to: placing the profile in an environment of 180-200°C for 4-8 hours, and then cooling it. According to the specifications of the windshield, local annealing treatment is performed on the bending area at a temperature of 350-400°C, and then bending treatment is performed.

[0011] Furthermore, in step S4, the detection information obtained by the quality inspection is fed back to the terminal and associated with the process parameters, and the production process is continuously optimized through the feedback mechanism to achieve the best bending effect on the basis of ensuring the mechanical properties.

[0012] Furthermore, quality inspection includes dimension inspection, appearance inspection, mechanical property inspection, assembly and sealing inspection; dimension inspection includes the key dimensions of the profile, appearance inspection is to check whether there are cracks or deformations in the bent parts, mechanical property tests include tensile strength test, yield strength test and fatigue test, assembly and sealing inspection refers to trial installation of the profile and the dividing cloth to ensure that its clamping force and sealing effect meet the requirements.

[0013] Furthermore, the process parameters include the chemical composition data of each batch of aluminum bars; the extrusion temperature and extrusion speed during the extrusion process; the temperature, holding time and cooling rate of each aging treatment.

[0014] Furthermore, the processed profiles are subjected to quality inspection, and the process parameters are optimized according to the quality inspection results, including: Construct a profile quality prediction model, collect the process parameters of the current production batch and the chemical composition data of the new production batch of aluminum bars during the profile preparation process, input them into the profile quality prediction model, predict the new production batch of profiles, and obtain the profile quality prediction results; Analyze the profile quality prediction results and determine the process parameters that need to be adjusted through sensitivity analysis; Calculate the sensitivity index of each process parameter that needs to be adjusted, formulate the adjustment target value of the process parameter based on the sensitivity index, and adjust the process parameters of the new production batch.

[0015] Furthermore, when the initial production process parameters are set according to experience, the chemical composition of the aluminum rod includes: Si: 0.55%~0.6%, Fe≤0.3%, Cu: 0.15%~0.25%, Mn≤0.15%, Mg: 0.8%~0.95%, Cr: 0.05%~0.15%, Zn≤0.2%, Ti: 0.1%~0.15%, and the balance is Al; the extrusion temperature in the extrusion process is set to 400~500℃, and the extrusion speed is set to 1~10mm / s; the temperature of each aging treatment is set to 180~200℃, the holding time is set to 4~8h, and the cooling rate is set to 10~20℃ / s.

[0016] Furthermore, in step S5, the surface treatment includes anodizing, electrophoretic coating or powder spraying.

[0017] The second object of the present invention is to prepare an aluminum alloy profile that can fix a two-layer bellows based on the above-mentioned method for preparing the aluminum alloy profile.

[0018] In order to achieve the above object, the technical solution adopted by the present invention is: An aluminum alloy profile is prepared by the above preparation method. The cross section of the aluminum alloy profile is an n-type structure with one end open and axially symmetrically arranged. Saw teeth are arranged on the inner side of the open end of the aluminum alloy profile.

[0019] The beneficial effects of the present invention are: (1) The present invention ensures that the chemical composition, mechanical properties and surface quality of the raw materials meet high standards through strict aluminum rod quality inspection and pretreatment steps, laying a solid foundation for subsequent profile preparation. At the same time, by dynamically adjusting the selection of aluminum rods based on the quality inspection information of the previous batch of aluminum alloy profiles, the stability and consistency of the product are further improved.

[0020] (2) During the extrusion process, the present invention successfully prepared an aluminum alloy profile with a serrated cross-section by precisely controlling the heating temperature, extrusion speed and die design. This cross-sectional design not only enhances the structural strength of the profile, but also improves its connection stability and sealing with other components. At the same time, precise control also ensures the dimensional accuracy and surface quality of the profile. Through artificial aging treatment and local annealing treatment, the mechanical properties and bending properties of the profile are effectively improved. This treatment method not only improves the tensile strength, yield strength and fatigue life of the profile, but also ensures that the bent part will not crack or deform, thereby meeting the needs of complex application scenarios.

[0021] (3) The present invention ensures that all performance indicators of the product meet the use requirements through comprehensive quality inspection, including size inspection, appearance inspection, mechanical property inspection, and assembly and sealing inspection. At the same time, the inspection information obtained from the quality inspection is fed back to the terminal and associated with the process parameters. The production process is continuously optimized through the feedback mechanism, realizing intelligent and refined control of the production process. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0023] Figure 1 The following is a flow chart of the preparation of aluminum alloy profiles in an embodiment of the present invention; Figure 2 It is a structural schematic diagram of an aluminum alloy profile in an embodiment of the present invention; DETAILED DESCRIPTION

[0024] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.

[0025] It should be noted that when an element is referred to as being "fixed to" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only and do not represent the only implementation method.

[0026] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.

[0027] like Figure 1 As shown, a method for preparing an aluminum alloy profile comprises the following steps: S1: Conduct quality inspection on purchased aluminum bars, including chemical composition analysis, mechanical property test and surface quality inspection, select aluminum bars with suitable chemical composition and basic quality control, and pre-treat the aluminum bars; Specifically, the selection of aluminum rods with suitable chemical composition and basic quality control is dynamically adjusted based on the quality inspection information of the previous batch of aluminum alloy profiles. The pretreatment includes removing the oxide layer, oil stains and impurities, which can be completed by pickling or alkali washing to ensure that no surface defects will occur during the extrusion process.

[0028] In this application, aluminum bars are purchased products. During the process, the chemical compositions (Si, Fe, Cu, Mn, Mg, Cr, Zn, Ti, Al, etc.) of 6 series aluminum alloys (6061 or 6082) and 7 series aluminum alloys (such as 7075) are recorded for different grades and a database is formed. During the dynamic adjustment process, the grade and alloy system with the best performance are selected, and then the production process parameters are optimized according to the quality inspection information.

[0029] S2: Place the aluminum rod in an extruder to extrude it to obtain a preliminary profile; and check that the appearance and size meet the requirements; Specifically, the aluminum rod is heated to 400~500℃, cut and divided according to the amount of profile, and then sent to the extruder for extrusion. During the extrusion process, the aluminum rod passes through the cavity of the mold and is extruded into a profile with a serrated cross-section; the extrusion speed and temperature are controlled to ensure the dimensional accuracy and surface quality of the profile. After extrusion, residual stress will be generated inside the aluminum alloy profile, resulting in unstable material strength and durability. Through aging treatment, the organizational structure can be stabilized and the mechanical properties can be improved. The preliminary profile quality inspection not only includes dimensional and appearance inspection, but also non-destructive testing (such as ultrasonic testing) should be carried out to ensure that there are no defects such as pores and cracks inside. During the process, sensors and data acquisition systems record process parameters such as temperature, pressure, speed, time, and test results such as dimensional accuracy, mechanical properties, and surface quality of the product in real time. The collected data is stored in a cloud database or a local data server to form traceable historical data.

[0030] S3: Perform artificial aging treatment on the profile; place the profile in an environment of 180~200℃ for 4~8h to accelerate the precipitation of strengthening phase (such as Mg2Si) and improve the strength and hardness of the material, then cool it, cut it to a suitable length according to the windshield specifications, perform local annealing treatment on the bending area, the annealing temperature is 350~400℃, and then perform bending treatment.

[0031] The contradiction between the hardness and bending performance of aluminum alloys mainly stems from the strengthening mechanism of the material. Generally, an increase in hardness means a decrease in the plasticity of the material and a deterioration in the bending performance. The aluminum alloy profile produced by the present invention needs to adapt to the windshield structure, so it needs to be bent 90°. The bending needs to be performed on the profile after aging treatment, but it is necessary to ensure that the material has sufficient ductility. If the strength of the material is too high (after aging treatment), brittle fracture may occur. The present invention performs appropriate annealing treatment before bending to improve the balance between strength and ductility.

[0032] S4: Conduct quality inspection on the processed profiles; Furthermore, in step S4, the detection information obtained by the quality inspection is fed back to the terminal and associated with the process parameters, and the production process is continuously optimized through the feedback mechanism to achieve the best bending effect on the basis of ensuring the mechanical properties.

[0033] Furthermore, quality inspection includes dimension inspection, appearance inspection, mechanical property inspection, assembly and sealing inspection; dimension inspection includes the key dimensions of the profile, appearance inspection is to check whether there are cracks or deformations in the bent parts, mechanical property tests include tensile strength test, yield strength test and fatigue test, assembly and sealing inspection refers to trial installation of the profile and the dividing cloth to ensure that its clamping force and sealing effect meet the requirements.

[0034] Furthermore, the process parameters include the chemical composition data of each batch of aluminum bars; the extrusion temperature and extrusion speed during the extrusion process; the temperature, holding time and cooling rate of each aging treatment.

[0035] Furthermore, the processed profiles are subjected to quality inspection, and the process parameters are optimized according to the quality inspection results, including: Construct a profile quality prediction model, collect the process parameters of the current production batch and the chemical composition data of the new production batch of aluminum bars during the profile preparation process, input them into the profile quality prediction model, predict the new production batch of profiles, and obtain the profile quality prediction results, which specifically include: Collect the process parameters of the current production batch and the chemical composition data of the new production batch of aluminum bars during the profile preparation process; Preprocess the process parameters of the current production batch and the chemical composition data of the aluminum bars of the new production batch; In order to improve the quality of the data, the collected data can be preprocessed and cleaned. Interpolation or deletion methods can be used to deal with missing values ​​and outliers. The data can be standardized or normalized to eliminate the dimensional influence between different features. Feature selection can also be performed to identify features that have a greater impact on the prediction results and remove redundant features.

[0036] Collect the chemical composition data, process parameters and quality inspection information of several production batches of aluminum bars and store them in the database. When storing, the chemical composition data, process parameters and quality inspection information of the aluminum bars of each profile correspond one to one; Specifically, when collecting aluminum rod chemical composition data, process parameters and quality inspection information and storing them in a database, a variety of types of databases can be selected, including relational databases, NoSQL databases, data warehouses, cloud databases, etc. For example, relational databases can ensure data integrity and consistency through primary key and foreign key relationships and avoid isolated data. In relational databases, data can be represented in tables using rows and columns, which are suitable for structured data. Cloud databases are database services hosted on cloud platforms that support different data storage models. They can be traditional relational databases or NoSQL databases, and cloud databases provide on-demand expansion, automatic backup, high availability and other features. When storing data, data information can be matched one by one, which helps to effectively integrate information in subsequent data analysis and improve the prediction accuracy of the model.

[0037] Construct a profile quality prediction model, and use the data in the database to train and optimize the profile quality prediction model; Before building a prediction model, you can use tools such as association rules or regression analysis on the data in the database to understand the data characteristics and identify the key process parameters that affect the mechanical properties and bending effects as potentially important input variables. After selecting the features, you can use machine learning models such as linear regression, decision trees, neural networks, etc. for training. The model can further automatically adjust the feature weights during the training process, so as to gradually grasp the relationship between the input features and the output targets, so as to make more accurate predictions for new data. During the model training process, the data in the database can be divided into training sets and test sets. The model is trained with the training set. The model will randomly initialize parameters, including weights and biases, and input the training data into the model for forward propagation. The input features are passed through the model layer by layer to generate predicted values. At the same time, the loss between the predicted value and the true target value is calculated. The model parameters are updated to reduce the loss through gradient descent or other optimization algorithms. After the model training is completed, the test set can be used to evaluate the prediction performance of the model and calculate various performance indicators, including mean square error, determination coefficient, etc.

[0038] The pre-processed process parameters of the current production batch and the chemical composition data of the aluminum bars of the new production batch are input into the optimized profile quality prediction model, and the profiles of the new production batch are predicted to obtain the profile quality prediction results.

[0039] Analyze the profile quality prediction results and determine the process parameters that need to be adjusted through sensitivity analysis; Calculate the sensitivity index of each process parameter that needs to be adjusted, formulate the adjustment target value of the process parameter based on the sensitivity index, and adjust the process parameters of the new production batch.

[0040] On the basis of the above embodiments, the trained model is deployed to the production environment, and real-time prediction can be performed. For the obtained model prediction results, the influence of process parameters on the model prediction results can be evaluated through local sensitivity analysis or global sensitivity analysis. According to the results of the sensitivity analysis, the process parameters with the greatest impact on the performance are adjusted to reduce the number of tests and improve the optimization efficiency. After the sensitivity analysis, the influence of each process parameter on the model output can be calculated, that is, the sensitivity index. The sensitivity index can be used to guide the target setting. For example, the sensitivity analysis shows that the tensile strength is expected to increase by 5% when the extrusion temperature is increased from 500°C to 525°C. The target setting can be adjusted to increase the extrusion temperature by 5%. At the same time, the production conditions and material characteristics can be considered to formulate a reasonable adjustment range to ensure that it is within a safe and controllable range. In order to continuously optimize the production process, a closed-loop feedback mechanism can be established to use the adjusted process parameters for the next round of production. After the new production batch is completed, the performance test results of the product are fed back to the model and database again, so as to continuously update and optimize the model, improve the accuracy of the prediction, and ensure that the product has the best bending performance on the basis of ensuring mechanical properties.

[0041] Furthermore, when the initial production process parameters are set according to experience, the chemical composition of the aluminum rod includes: Si: 0.55%~0.6%, Fe≤0.3%, Cu: 0.15%~0.25%, Mn≤0.15%, Mg: 0.8%~0.95%, Cr: 0.05%~0.15%, Zn≤0.2%, Ti: 0.1%~0.15%, and the balance is Al; the extrusion temperature in the extrusion process is set to 400~500℃, and the extrusion speed is set to 1~10mm / s; the temperature of each aging treatment is set to 180~200℃, the holding time is set to 4~8h, and the cooling rate is set to 10~20℃ / s.

[0042] S5: Surface treatment is performed on the profiles that have passed the quality inspection, including anodizing, electrophoretic coating or powder spraying, to obtain aluminum alloy profiles that meet the use standards. Preferably, powder spraying is used to achieve corrosion protection on the outer surface of the aluminum alloy profile.

[0043] According to the above preparation method, the following Figure 2 The aluminum alloy profile shown has an n-shaped cross-section with one end open and axially symmetrically arranged. The inner side of the open end of the aluminum alloy profile is provided with saw teeth. It is used in the train windshield system. The windshield cloth is firmly combined with the cloth through the clamping action between the two layers of bellows. The inner side of the aluminum alloy profile is provided with a sawtooth shape, which can increase the friction force and ensure that the windshield system will not loosen or the material will not fall off due to vibration or pressure during the high-speed running of the train.

[0044] Those skilled in the art should understand that the present invention is not limited to the above embodiments, and the above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, and these changes and improvements fall within the scope of the present invention to be protected. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. A method for preparing an aluminum alloy profile, characterized in that: The steps are as follows: S1: Conduct quality inspection on the purchased aluminum bars, including chemical composition analysis, mechanical property test and surface quality inspection, select aluminum bars with suitable chemical composition and basic quality control, and pre-treat the aluminum bars; S2: placing the aluminum rod in an extruder for extrusion to obtain a preliminary profile; and checking that the appearance and size meet the requirements; S3: Perform artificial aging treatment on the profile; then cut the profile to a suitable length according to application requirements and bend it at the corresponding position; S4: Conduct quality inspection on the processed profiles; S5: Surface treatment is performed on the profiles that have passed the quality inspection to obtain aluminum alloy profiles that meet the use standards.

2. The method for preparing an aluminum alloy profile according to claim 1, characterized in that: In step S1, the selection of aluminum rods with suitable chemical composition and basic quality control is dynamically adjusted based on the quality inspection information of the aluminum alloy profiles produced in the previous batch. The pretreatment includes removing the oxide layer, oil stains and impurities, which can be completed by pickling or alkali washing to ensure that no surface defects will occur during the extrusion process.

3. The method for preparing an aluminum alloy profile according to claim 1, characterized in that: In step S2, the aluminum rod is heated to 400-500°C, cut and divided according to the amount of the profile, and then sent to the extruder for extrusion. During the extrusion process, the aluminum rod passes through the cavity of the mold and is extruded into a profile with a serrated cross-section; the extrusion speed and temperature are controlled to ensure the dimensional accuracy and surface quality of the profile.

4. The method for preparing an aluminum alloy profile according to claim 1, characterized in that: In step S3, artificial aging treatment refers to: placing the profile in an environment of 180-200°C for 4-8 hours, then cooling it, and performing local annealing treatment on the bending area according to the windshield specifications at an annealing temperature of 350-400°C, and then performing bending treatment.

5. The method for preparing an aluminum alloy profile according to claim 1, characterized in that: In step S4, the detection information obtained from the quality inspection is fed back to the terminal and associated with the process parameters. The production process is continuously optimized through the feedback mechanism to achieve the best bending effect while ensuring the mechanical properties.

6. The method for preparing an aluminum alloy profile according to claim 5, characterized in that: The quality inspection includes dimension inspection, appearance inspection, mechanical property inspection, assembly and sealing inspection; the dimension inspection includes the key dimensions of the profile, the appearance inspection is to check whether there are cracks or deformations in the bent part, the mechanical property test includes tensile strength test, yield strength test and fatigue test, and the assembly and sealing inspection refers to trial installation of the profile and the dividing cloth to ensure that the clamping force and sealing effect meet the requirements.

7. The method for preparing an aluminum alloy profile according to claim 6, characterized in that: The process parameters include the chemical composition data of each batch of aluminum bars; the extrusion temperature and extrusion speed during the extrusion process; the temperature, insulation time and cooling rate of each aging treatment.

8. The method for preparing an aluminum alloy profile according to claim 7, characterized in that: The step of performing quality inspection on the processed profile and optimizing the process parameters according to the quality inspection results includes: Constructing a profile quality prediction model, collecting process parameters of the current production batch and chemical composition data of aluminum bars of a new production batch during the profile preparation process and inputting them into the profile quality prediction model, predicting the profiles of the new production batch, and obtaining profile quality prediction results; Analyze the profile quality prediction results and determine the process parameters that need to be adjusted through sensitivity analysis; The sensitivity index of each process parameter that needs to be adjusted is calculated, and the adjustment target value of the process parameter is formulated according to the sensitivity index, and the process parameter of the new production batch is adjusted.

9. The method for preparing an aluminum alloy profile according to claim 1, characterized in that: In step S5, the surface treatment includes anodizing, electrophoretic coating or powder spraying.

10. An aluminum alloy profile, prepared by the preparation method according to any one of claims 1 to 9, characterized in that: The cross section of the aluminum alloy profile is an n-type structure with one end open and arranged axially symmetrically, and saw teeth are arranged on the inner side of the open end of the aluminum alloy profile.

Citation Information

Patent Citations

  • Passenger train rescue channel window

    CN101936114A

  • Serpent-shaped fin tube evaporator

    CN102121769A

  • Automotive aluminum alloy front auxiliary frame boundary beam forming method

    CN104646939A

  • Bent aluminum inflating valve body and treatment method thereof

    CN109944973A

  • Method for predicting online extrusion quenching mechanical property of aluminum alloy profile

    CN111916159A