Method for preparing ceramsite from waste manganese ore slag

By mixing manganese ore waste residue with materials such as clay, pulverized coal, and bentonite for pelletizing and roasting, high-strength ceramsite was successfully prepared, solving the problems of manganese ore waste residue pollution and resource waste, and achieving efficient ceramsite preparation and environmental protection. .

CN106365611AInactive Publication Date: 2017-02-01CENT SOUTH UNIV
7 Cites 3 Cited by

Patent Information

Application Number
CN201610750892.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2016-08-29
Publication Date
2017-02-01
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Manganese ore waste residue has not been properly processed, resulting in environmental pollution and resource waste. The domestic technology for preparing ceramsite from manganese slag is immature and the strength of the ceramsite is low.

Method used

Mix manganese ore waste residue with clay and coal powder, then dry and grind it, add bentonite and water for formation, pelletizing, drying and roasting to prepare high-strength ceramsite.

Benefits of technology

The process is simple and efficient, and high-strength ceramsite is prepared from waste manganese slag, which solves the problem of environmental pollution and has excellent performance and is suitable for industrial production.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to a method for preparing ceramsite from waste manganese ore slag. The method comprises the following steps that the waste manganese ore slag, clay and coal powder are mixed, dried and ground to obtain a preliminary mixture; bentonite and water are added into the preliminary mixture, mixing integration is conducted for a period of time, and a final mixture is obtained; the final mixture is pelletized to obtain wet pellets; the wet pellets are dried; the dried pellets are roasted to obtain the ceramsite. According to the method, the process is simple, operation is easy and convenient, the waste manganese ore slag is utilized, the problem that the waste manganese ore slag pollutes the environment is solved, waste materials are changed into things of value, the high-strength ceramsite is prepared by comprehensively utilizing the manganese ore slag resource, and the performance is greatly improved. The method is mature in technology, free of secondary pollution, low in cost and suitable for industrialized production.
Need to check novelty before this filing date? Find Prior Art