A stabilization and arsenic removal technology, applied in the restoration of contaminated soil, etc., can solve the problems of poor leaching stability and low toxicity leaching concentration, and achieve the effect of inhibiting microorganisms, ensuring long-term effects, and better long-term stability effects
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2019-09-13
Smart Images

Figure 1 
Figure 2 
Figure 3
Abstract
Description
technical field
[0001] The invention belongs to the technical field of mineral arsenic fixation, and in particular relates to a compound stabilization agent for arsenic removal slag and its application. Background technique
[0002] Arsenic is a highly toxic element with high carcinogenicity, and is widely associated in various non-ferrous metal smelting process systems. In the past 30 years, with the rapid development of my country's nonferrous metal industry, the problem of arsenic pollution has become more and more serious, seriously threatening people's lives and health. Therefore, the research on arsenic pollution control is an urgent and significant topic.
[0003] At present, arsenic fixation technologies mainly include encapsulation and mineral arsenic fixation. Encapsulation is to use cement, glass and other materials to coat arsenic-containing materials so that they can be stored stably. This method has a large amount of solid waste and high cost, making it diff...
Examples
Embodiment 1
[0027] The composite stabilization agent for arsenic removal slag used in this embodiment includes the following components:
[0028]
[0029] Method of use: Take 2kg of arsenic removal slag with a pH of 12, add 8wt% compound stabilizing agent, stir for 15 minutes to mix evenly, and after standing, covering and curing for seven days, use the method specified in (GB18598-2001) to perform leaching toxicity Analysis showed that its arsenic leaching concentration was 0.13mg / L.
Embodiment 2
[0031] The composite stabilization agent for arsenic removal slag used in this embodiment includes the following components:
[0032]
[0033] Method of use: Take 2kg of arsenic removal slag whose pH has been adjusted to about 4, add 8wt% compound stabilizing agent, stir for 15 minutes to mix evenly, after standing, covering and curing for seven days, use the method specified in (GB18598-2001) The leaching toxicity analysis was carried out, and the arsenic leaching concentration was 0.67mg / L.